Printing method and printing device for producing components

The method and device control light energy input based on optical parameters to prevent unwanted polymerization, addressing issues of fragments and delamination in stereolithography 3D printing, achieving precise and efficient component production.

CN119058098APending Publication Date: 2024-12-03IVOCLAR VIVADENT AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410456570.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-06-02
Filing Date
2024-04-16
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Stereolithography 3D printing faces issues with unwanted material fragments and layer delamination due to light scattering and improper exposure energy, leading to impaired fit and separation of components.

Method used

A method and device that calculate and dynamically control light energy input based on optical parameters of the photocurable material, using spatial and temporal adjustments to minimize unwanted polymerization outside intended areas, ensuring precise and uniform polymerization.

Benefits of technology

Prevents material fragments and delamination, enabling high-precision and accurate production of complex geometries with reduced exposure time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119058098A_ABST
    Figure CN119058098A_ABST
Patent Text Reader

Abstract

The invention relates to a printing method for producing a component, comprising the following steps: calculating an energy input for a spatial region of the component on the basis of an optical parameter of a photocurable material; and curing the region of the component by means of light which generates the calculated energy input into the material.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a printing method and a printing device for producing parts.

[0002] In stereolithography 3D printing, liquid materials polymerize under the action of light. The liquid material is usually located in a tank with a transparent bottom, into which the print bed is immersed from above and moves toward the bottom of the tank to the desired layer thickness. The liquid material in the intermediate gap is then exposed to light at the desired point through the transparent tank bottom by means of an exposure device, for example by means of point illumination using a laser beam raster or full-surface illumination using a micromirror array (DMD—digital micromirror device).

[0003] When sufficient exposure energy is above the polymerization threshold of the printing liquid, the printing liquid polymerizes at the exposure point, i.e. solidifies. Then, the print bed moves upward with the adhered solidified layer and forms the necessary intermediate gap between the solidified layer and the bottom of the groove for the next layer. Next comes the next exposure. In this way, three-dimensional parts can be stacked layer by layer.

[0004] The geometric shape of the specific layer to be polymerized is completely exposed. At the edges of the exposed shape, the light is scattered by the liquid material and also by the polymerized material, which has been continuously solidified during the exposure time.

[0005] As a result, unwanted fragments of solidified material are formed on the component or between the layers of the component, which on the one hand impairs the fit of the components and on the other hand leads to separation (delamination) of the individual layers of the component at the bottom of the groove. Delamination can also occur if the exposure energy is insufficient to completely cure the required layer thickness of the liquid material set according to the print job or if a previous layer polymerized too much.

[0006] Changes in the chemical composition of the material lead to negative changes in other properties (such as mechanical stability) and do not solve the underlying problem. The intensity of the light used also has an influence. If the total energy of the radiation remains constant, fragmentation increases at higher intensities. Higher intensities reduce the exposure time required per layer and therefore largely determine the overall duration of the printing process, which should be as short as possible.

[0007] The technical task of the present invention is to improve the printing process in such a way that the formation of material fragments and delamination of the layers are prevented.

[0008] This technical task is achieved by the subject matter according to the independent claim. Technically advantageous embodiments are the subject matter of the dependent claims, the description and the drawings.

[0009] According to a first aspect, the technical task is solved by a printing method for producing a component, the printing method comprising the steps of: calculating the energy input for a spatial region of the component based on optical parameters of a photocurable material; and curing the spatial region of the component by means of light, which generates the calculated energy input into the material. The calculation can be performed as a function of the degree of polymerization as a function of the exposure time. The light can vary dynamically with the exposure time. The region of the component can be formed by sub-regions, such as voxels. This allows each sub-region of the component to be selectively exposed. The optical parameters can include a scattering coefficient, an absorption coefficient and / or a transmission coefficient. The energy input to the region can be caused by direct irradiation from a light source and / or by indirect irradiation by scattering from adjacent regions. The method provides the technical advantage that components can be produced with greater precision.

[0010] In a technically advantageous embodiment of the printing method, the calculation is performed based on the geometry of the component. This provides technical advantages, for example, even narrow areas or sharp corners can be printed without debris.

[0011] In a further technically advantageous embodiment of the printing method, the time course of the energy input is calculated. This provides technical advantages, for example, further improving the production of components.

[0012] In a further technically advantageous embodiment of the printing method, the time course is calculated based on a temporal or spatial aggregation of regions. This provides technical advantages, for example, that the course of the polymerization during the exposure is taken into account and the polymerization in the layer is as uniform as possible in the cross-sectional area of ​​the object.

[0013] In a further technically advantageous embodiment of the printing method, the intensity of the exposure is varied based on the time course of the energy input. The intensity can thus be varied as a function of time. For example, the intensity of the exposure varies over time. This provides technical advantages, for example, reducing overexposure and thereby reducing debris formation, and enables components to be produced with high accuracy.

[0014] In a further technically advantageous embodiment of the printing method, the exposed area is changed based on the time course of the energy input. Thus, the exposed area can be changed as a function of time. This provides technical advantages, such as the energy input can be easily controlled.

[0015] In a further technically advantageous embodiment of the printing method, the repetition frequency of the periodic exposure is varied over time based on the time course. The periodic exposure uses individual light pulses or flashes to cure the light-curable material. This provides technical advantages, such as the energy input can be easily controlled.

[0016] In a further technically advantageous embodiment of the printing method, an optical parameter of the photocurable material is measured. The optical parameter can be measured in an uncured state and / or in a cured state. This provides technical advantages, for example, exposure parameters can be adjusted for different materials based on their optical properties.

[0017] In a further technically advantageous embodiment of the printing method, a laser or a micromirror array is used to generate the light. This provides technical advantages, for example, the use of a light source that is easily controllable.

[0018] In a further technically advantageous embodiment of the printing method, the region is a voxel. This provides the technical advantage that, for example, each voxel is exposed to a pre-calculated amount of energy.

[0019] According to a second aspect, the technical task is solved by a printing device for producing a component, the printing device comprising: a calculation device for calculating the energy input to a spatial region of the component based on optical parameters of a light-curable material; and an exposure device for curing the region of the component by means of light, the light generating the calculated energy input into the material. The printing device achieves the same technical advantages as the printing method according to the first aspect.

[0020] In a further technically advantageous embodiment of the printing device, the calculation device is configured to calculate the time course of the energy input. This also provides technical advantages, for example, further improving the production of components.

[0021] In a further technically advantageous embodiment of the printing device, the calculation device is configured to perform calculations based on the geometry of the component. This also offers technical advantages, for example, even complex geometries can be created without errors.

[0022] In a further technically advantageous embodiment of the printing device, the printing device comprises a measuring device for measuring the optical parameter. The measuring device comprises, for example, a spectrometer or a light sensor for measuring the transmission or absorption at a predetermined wavelength. In general, the optical parameters of the photocurable material can also be determined outside the printing device. This provides technical advantages, for example, narrow areas or sharp angles can be printed without debris.

[0023] In a further technically advantageous embodiment of the printing device, the exposure device comprises a laser or a micromirror array. This offers technical advantages, for example, that light can be introduced into the material in an easily controllable manner.

[0024] Exemplary embodiments of the invention are illustrated in the drawings and are described in more detail below, in which:

[0025] Figure 1 shows a graph of cure depth as a function of exposure energy;

[0026] Figure 2 A schematic diagram of a printing device is shown.

[0027] Figure 3 A schematic diagram of the exposure strategy is shown;

[0028] Figure 4 A schematic diagram showing another exposure strategy; and

[0029] Figure 5 A flow chart of a printing method is shown.

[0030] Figure 1 A graph showing the cure depth as a function of the exposure energy is shown. Cure depth (in μm) versus exposure energy E (in mJ / cm 2 The curing depth C D is an empirical value based on the amount of radiated energy E. The material-specific correlation between the curing depth and the radiated exposure energy E can be measured. The correlation is as follows:

[0031]

[0032] The logarithmic plot shows that there is a material-specific minimum polymerization energy E C , below the minimum aggregation energy E C No polymerization will occur. (Light) penetration depth D p Determined by the gradient of the straight line. Polymerization only occurs if the photoinitiator converts all available oxygen locally by light.

[0033] As long as this does not happen, the oxygen concentration increases and is locally balanced again by diffusion. The radiation energy that has accumulated locally is distributed over a larger volume of liquid at the expense of a reduced total oxygen content. This then leads to a total liquid aggregate energy E C In this way, the time available for compensation by diffusion is shortened, and the remaining accumulated energy exceeds the minimum polymerization energy E more quickly. C .

[0034] During exposure, an undetermined amount of energy is always introduced into the liquid outside the areas to be polymerized. Since the material is able to accumulate this energy, at a certain point in time the energy introduced is sufficient to polymerize the material undesirably also outside the exposed areas.

[0035] Finally, the intensity of the light used also has an influence. If the total energy of the radiation remains the same, more fragments will be formed at higher intensities. At higher intensities, the exposure time per layer is reduced. They are responsible for the overall duration of the printing process, which should be as short as possible.

[0036] The effect also depends on the material properties of the liquid starting material, for example optical properties such as opacity and pigmentation, i.e. absorption coefficient and scattering coefficient. A process window can be found for each material in which chip formation is suppressed and delamination of the individual layers is avoided. It is therefore technically advantageous if the exposure energy introduced due to light scattering outside the area to be cured is reduced or eliminated compared to full-surface exposure.

[0037] Figure 2 A schematic diagram of a printing device 200 for producing a component based on a photocurable material 103, the component being formed, for example, by a stereolithography device, is shown. The printing device 200 is used to stack a three-dimensional component 100 layer by layer from a photocurable material 103 (such as a curable dental material).

[0038] In order to prevent the photocurable material 103 from forming undesired fragments, the printing device 200 comprises a calculation device 201 for calculating the energy input for the spatial region 101 of the component 100 based on optical parameters of the photocurable material 103 .

[0039] Optical properties of the liquid and polymeric material 103, such as refractive index, absorption, scattering or optical anisotropy, may be measured for the wavelength used by the measuring device 205.

[0040] In addition, the kinetics of the polymerization process can also be measured. For this purpose, the measuring device 205 comprises a suitable sensor with which an optical parameter of the material 103 can be measured. The measuring device 205 comprises, for example, a spectrometer or a sensor with which the absorption or transmission at a predetermined wavelength can be calculated. The optical parameters are then transmitted to the computing device 201.

[0041] The optical parameters of the photocurable material 103 may also be determined outside of the printing device 200. The optical parameters may then be input into the printing device 200 so that the printing device 200 may perform additional processing on the optical parameters.

[0042] Then, for each area in the volume of the component 100 at a selected layer thickness, the computing device 201 calculates the light energy actually radiated at each point in time based on the optical parameters via the radiation transfer theory (e.g. based on variable transmission, absorption and / or scattering), taking into account the increase in the thickness of the polymer layer.

[0043] Furthermore, the radiated light energy is calculated not only for each region in the volume of the component 100 based on the optical parameters, but also for regions outside the volume that should not be cured and should be below the limit of the accumulated polymerization energy.

[0044] Thus, for each layer and each area 101 of the component 100 , the time course of the intensity of the radiation to be irradiated can be dynamically calculated to ensure focusing within the intended area 101 , while outside this area 101 , energy input is minimized by scattering.

[0045] The calculation device 201 comprises, for example, a digital memory and a microprocessor, which can calculate the energy input for the corresponding area to be exposed and the surrounding area according to the optical parameters and the radiation transfer equation of the material 103. The digital memory comprises a suitable computer program for this purpose and stores the obtained data.

[0046] In addition, the printing device 200 comprises an exposure device 203 for curing the regions 101 of the component 100 located below the grooves 105 by means of light, which generates the calculated energy input into the material 103. The exposure device 203 is capable of individually exposing each region 101. To this end, the exposure device 203 can be controlled by the computing device 201.

[0047] The exposure device 203 allows the energy input to be controlled with voxel precision via the grayscale values ​​of the micromirror device. If the laser is scanned over the area instead, this can be achieved by varying the dwell time of the laser beam per area 101. It is also possible to dynamically vary the intensity of the light source in synchronization with the temporal pixel-precise variation of the area 101 to be exposed.

[0048] Figure 3 A schematic diagram of the exposure strategy is shown. For example, if the scattering 109 in the polymerized material 103 is higher than the scattering 109 in the liquid material 103, the polymerization front starts from the transparent groove bottom 207 and travels through the exposed layer. The scattering 109 also increases at the edge of the part 100 in the direction of the non-exposed liquid as polymerization increases.

[0049] In this case, the exposure area 107 decreases continuously during exposure so that the increased scattering 109 is still sufficient to cure the entire volume of the component 100 but not the liquid areas outside the component 100 .

[0050] On the other hand, if the scattering 109 in the polymeric material 103 is less than the scattering 109 in the liquid material 103, then the scattering into the environment steadily decreases as the polymeric layer thickness increases. In this case, the exposure is initially performed with a reduced area 107. During the exposure process, the area 107 is expanded to the actual geometric size.

[0051] In this way, a variable exposure can be achieved using any number of different masks with different dwell times, shapes and transmittances. Physically correct calculation of the energy input allows the intensity in each area 101 to be adjusted so that fragmentation is minimized or even avoided completely. Nevertheless, sufficient polymerization can be ensured to prevent delamination of the layers in the part, and the exposure process can be faster or time optimized.

[0052] Figure 4 A schematic diagram of another exposure strategy is shown. In this exposure strategy, the exposure pattern does not change over time, but the intensity I of the irradiation decreases towards the edge of the component 100. In this way, it is also possible to prevent the energy input by scattering from entering areas of the liquid that are outside the component 100 and should not be cured.

[0053] Figure 5 A block diagram of a printing method for producing a component 100 is shown. The method comprises a step S101 of calculating an energy input to a spatial region 101 of a component 100 to be cured based on optical parameters of a light-curable material 103. This is followed by a step S102 of curing the spatial region 101 of the component 100 by means of light, the light generating the calculated energy input into the material 103. These steps may be performed for each spatial region 101 of a component 100.

[0054] In this way, suitable exposures can be calculated for multiple spatial regions of the component 100. The dynamic calculations performed by the computing device 201 ensure that even in the case of unusual geometries of the component 100, such as narrow areas, sharp or reflected angles, sharp protrusions or recesses, undesirable energy input into the surrounding liquid is minimized.

[0055] For this purpose, the illumination area can be changed dynamically or a dynamic adjustment of the selective exposure intensity or exposure can be performed or a combination of all possibilities. For example, the exposure can be ended early at a single point.

[0056] All features explained and shown in conjunction with the individual embodiments of the invention may be provided in different combinations in the subject matter according to the invention in order to achieve their advantageous effects simultaneously.

[0057] All method steps may be implemented by means suitable for carrying out the respective method step.All functions performed by features of the subject matter may be method steps of a method.

[0058] The scope of protection of the present invention is given by the claims and is not limited by the features explained in the description or shown in the drawings.

[0059] Reference numerals list

[0060] 100 parts

[0061] Area 101

[0062] 103 Photocurable materials

[0063] 105 slots

[0064] 107 exposure area

[0065] 109 Scattering

[0066] 200 Printing device

[0067] 201 Computing Device

[0068] 203 exposure device

[0069] 205 measuring device

[0070] 207 slot bottom.

Claims

1. A printing method for producing a component, the printing method comprising the following steps: - calculating the energy input for the spatial region of the component based on the optical parameters of the photocurable material; and - curing the spatial region of the component by means of light, which generates the calculated energy input into the material.

2. The printing method according to claim 1, wherein: The calculation is performed based on the geometry of the component.

3. A printing method according to any one of the preceding claims, wherein: The time course of the energy input is calculated.

4. The printing method according to claim 3, wherein: The time course is calculated based on the time aggregation or the spatial aggregation of the region.

5. The printing method according to claim 3 or 4, wherein: The intensity of the exposure is varied based on the time course of the energy input.

6. The printing method according to any one of claims 3 to 5, wherein: The exposed area is varied based on the time course of the energy input.

7. The printing method according to any one of claims 3 to 6, wherein: The repetition frequency of the periodic exposure is varied based on the time course.

8. The printing method according to any one of claims 3 to 7, wherein: The optical parameter of the photocurable material is measured.

9. A printing method according to any one of the preceding claims, wherein: The light is generated by means of a laser or a micromirror array.

10. A printing method according to any one of the preceding claims, wherein: The regions are voxels.

11. A printing device for producing a component, the printing device comprising: - calculation means for calculating the energy input for the spatial region of the component based on the optical parameters of the photocurable material; as well as - an exposure device for curing areas of the component by means of light, the light generating the calculated energy input into the material.

12. The printing device according to claim 11, wherein: The calculation device is configured to calculate the time course of the energy input.

13. The printing device according to claim 11 or 12, wherein: The calculation device is configured to perform the calculation based on the geometry of the component.

14. The printing device according to any one of claims 11 to 13, wherein: The printing device comprises a measuring device, and the measuring device is used to measure the optical parameters.

15. The printing device according to any one of claims 11 to 14, wherein: The exposure device includes a laser or a micromirror array.