Manufacturing method of insulated gate bipolar transistor
By introducing laser pre-treatment processes into the insulated gate bipolar transistor manufacturing process, the back defects of the substrate caused by the thinning process are solved, and the electrical characteristics stability and product quality consistency of the insulated gate bipolar transistor are significantly improved.
Patent Information
- Application Number
- CN202310651854.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-02
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing insulated gate bipolar transistor manufacturing methods, the thinning process causes defects on the back of the substrate, affecting the stability and consistency of electrical characteristics and product quality.
After the thinning process, the laser pretreatment process is added, and the defects caused by the thinning process on the back of the substrate are removed by using green lasers, a field cut-off layer is formed and annealed process is carried out to improve the stability of electrical characteristics.
Effectively remove defects such as microcracks and crystal dislocation caused by the thinning process, and improve the electrical characteristics stability of insulated gate bipolar transistors and the reproducibility and consistency of product quality.
Smart Images

Figure CN119069348A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing an insulated gate bipolar transistor, and more particularly to a method for manufacturing an insulated gate bipolar transistor with stable electrical characteristics. Background Art
[0002] Insulated Gate Bipolar Transistor (IGBT) is a power semiconductor component composed of a bipolar junction transistor (BJT) and a metal oxide semiconductor field-effect transistor (MOSFET). It has the advantages of both MOSFET and BJT and has been widely used in many fields.
[0003] See also Figure 1 , which shows a flow chart of a conventional insulated gate bipolar transistor manufacturing method. Figure 1 As shown, in the existing process of manufacturing an insulated gate bipolar transistor, first, as shown in step S101, a front element and a front metal layer are formed on the front side of the substrate, then, as shown in step S102, a thinning process is performed on the back side of the substrate, and then, as shown in step S103, an ion doping process is performed on the thinned back side of the substrate, and as shown in step S104, an annealing process is performed on the back side of the substrate, and finally, as shown in step S105, a collector metal layer is formed on the back side of the substrate to complete the manufacture of the insulated gate bipolar transistor.
[0004] In this process, the backside thinning process is a necessary and important procedure, which has a critical impact on the performance of the IGBT. The current thinning process mostly uses grinding to reduce the thickness of the substrate. However, since the grinding process applies stress to the back side of the substrate and performs grinding, many defects will still remain on the back side of the substrate after the stress is released. For example, the subsurface of the back side of the substrate will leave defects such as microcracks and crystal dislocations that can cause damage, and these defects will further affect the electrical characteristics of the final IGBT.
[0005] Therefore, it is necessary to develop a method for manufacturing an insulated gate bipolar transistor to improve the above-mentioned problems and disadvantages of the prior art. Summary of the invention
[0006] The purpose of this case is to provide a method for manufacturing an insulated gate bipolar transistor, which removes defects on the back side of the substrate caused by the thinning process by adding a laser pretreatment process after the thinning process, thereby enhancing the stability of the electrical characteristics of the insulated gate bipolar transistor and improving the product quality of the insulated gate bipolar transistor.
[0007] To achieve the above-mentioned purpose, the present invention provides a method for manufacturing an insulated gate bipolar transistor, comprising the following steps: (a) providing a substrate, wherein the substrate comprises a front side and a back side; (b) forming at least one front side element and at least one front side metal layer on the front side of the substrate; (c) performing a thinning process on the back side of the substrate; (d) performing a laser pretreatment process on the back side of the substrate; (e) performing at least one ion doping process on the back side of the substrate to form at least one ion doping layer; (f) performing an annealing process on the back side of the substrate; and (g) forming a collector metal layer on the back side of the substrate.
[0008] In one embodiment, the laser pre-treatment process is performed using a green laser.
[0009] In one embodiment, the laser pre-treatment process is performed at a temperature between about 1000-1500°C.
[0010] In one embodiment, the laser pre-treatment process may be performed for a period of time between about 60 seconds and about 150 seconds.
[0011] In one embodiment, at least one ion-doped layer comprises a field stop layer, and the insulated gate bipolar transistor is a field stop insulated gate bipolar transistor.
[0012] In one embodiment, the substrate is an N-type substrate or a P-type substrate. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 A flow chart showing a conventional method for manufacturing an insulated gate bipolar transistor is shown.
[0014] Figure 2 A flow chart showing a method for manufacturing an insulated gate bipolar transistor according to an embodiment of the present invention.
[0015] The reference numerals are described as follows:
[0016] S101, S102, S103, S104, S105: Steps
[0017] S201, S202, S203, S204, S205, S206, S207: Steps DETAILED DESCRIPTION
[0018] Some typical embodiments that embody the features and advantages of the present invention will be described in detail in the following description. It should be understood that the present invention can have various variations in different aspects, but they all do not depart from the scope of the present invention, and the descriptions and illustrations therein are essentially used for illustrative purposes rather than for limiting the present invention.
[0019] See also Figure 2, which shows a flow chart of a method for manufacturing an insulated gate bipolar transistor according to an embodiment of the present invention. Figure 2 As shown, in the process of manufacturing an insulated gate bipolar transistor in the present case, at the beginning, as shown in step S201, a substrate is provided, and the substrate has a front side and a back side; and as shown in step S202, a front element and a front metal layer are formed on the front side of the substrate. Next, the back side of the substrate is processed. First, as shown in step S203, a thinning process is performed on the back side of the substrate, and after reaching the required substrate thickness, as shown in step S204, a laser pretreatment process is performed on the back side of the substrate; then, as shown in step S205, at least one ion doping process is performed on the back side of the substrate to form at least one ion doping layer, and then as shown in step S206, an annealing process is performed on the back side of the substrate. Finally, as shown in step S207, a collector metal layer is formed on the back side of the substrate. Through the above steps, the manufacture of the insulated gate bipolar transistor with stable electrical characteristics in the present case can be completed.
[0020] In steps S201-S202, the substrate may be an N-type silicon substrate or a P-type silicon substrate without limitation, and the front element and the front metal layer on the front of the substrate may vary according to actual needs. In step S203, the thinning process is performed by grinding, but is not limited thereto. In step 205, the ion doping process may have different options depending on the type of insulated gate bipolar transistor to be manufactured. For example, in one embodiment, the ion doping layer of the field stop insulated gate bipolar transistor (FS IGBT) includes a field stop layer, and other insulated gate bipolar transistors, such as non-penetrating insulated gate bipolar transistors (NPTIGBT), trench insulated gate bipolar transistors (Trench IGBT) and field stop trench insulated gate bipolar transistors (FSTrench IGBT), also have corresponding ion doping layer distributions. In addition, the doped ions may be P-type silicon substrate or P-type silicon substrate depending on whether the substrate is an N-type silicon substrate or a P-type silicon substrate and the distribution of the ion doping layer. + and / or N + In step S206, the annealing process can be a laser annealing process or a gas annealing process, which is also not limited.
[0021] According to the above, compared with the prior art, the process of manufacturing the IGBT in the present case adds a laser pretreatment process shown in step S204. This laser pretreatment process is performed after the thinning process, and its function is to remove the defects left on the subsurface of the back side of the substrate during the thinning process. As is known, substrate thinning is a necessary and critical step for the IGBT. However, the thickness of the substrate after thinning is extremely thin, and it is easy to be damaged. The defects left on the substrate due to the thinning process further increase the probability of damage, for example, it may cause the substrate to be easily damaged in the subsequent process steps. On the other hand, even if the subsequent process steps have been completed, if there are still defects in the substrate, in addition to affecting the electrical characteristics of the IGBT, the product quality of the IGBT cannot be maintained consistently. In other words, since the location of the defects in the substrate is random, the impact on the IGBT is also random, so it is difficult to control and maintain the stability of the product quality. Therefore, after the thinning process, the back of the polished substrate is pre-treated to effectively remove defects generated in the substrate, which not only reduces the probability of substrate damage, but also improves the electrical characteristic stability of the insulated gate bipolar transistor and the consistency of product quality.
[0022] In the present embodiment, the laser pretreatment process uses a green laser, for example, a laser with a wavelength between about 495-570nm, and in a preferred embodiment, the wavelength of the green laser can be about 532nm; the laser pretreatment process is performed at a temperature between about 1000-1500°C, for example, in a preferred embodiment, the temperature can be performed between about 1200-1300°C; and the execution time of irradiating the back of the thinned substrate is about 60-150 seconds, for example, in a preferred embodiment, the execution time can be about 60-90 seconds. In this way, the effect of removing defects generated by the grinding and thinning process on the back of the substrate can be achieved, for example, micro cracks, crystal dislocations, etc. can be removed by this laser pretreatment process, greatly improving the damage to the back of the substrate. On the premise that the defects are removed, the insulated gate bipolar transistors made by executing the subsequent steps S205-S207 will provide more stable electrical characteristics and maintain the reproducibility and consistency of product quality. In addition, since the laser pretreatment process is performed in a very short exposure time, it will not affect the components and metal layers on the front side of the substrate. Therefore, this laser pretreatment process is a low-cost, easy-to-perform process that can achieve a specific defect removal effect.
[0023] In summary, the insulated gate bipolar transistor manufacturing method of the present invention is to add a laser pretreatment process after the thinning process of the back side of the substrate and before the further back-end process of the back side of the substrate to remove the defects on the sub-surface of the back side of the substrate generated during the thinning process, thereby greatly improving the stability of the electrical characteristics of the insulated gate bipolar transistor and effectively improving the reproducibility and consistency of the product quality of the insulated gate bipolar transistor.
[0024] It should be noted that the above is only a preferred embodiment for illustrating the present invention, and the present invention is not limited to the embodiment described. The scope of the present invention is determined by the attached claims. Moreover, the present invention may be modified in various ways by those skilled in the art, but all of them are within the scope of the protection intended by the attached claims.
Claims
1. A method for manufacturing an insulated gate bipolar transistor, comprising the following steps: (a) providing a substrate, the substrate comprising a front surface and a back surface; (b) forming at least one front element and at least one front metal layer on the front surface of the substrate; (c) performing a thinning process on the back side of the substrate; (d) performing a laser pretreatment process on the back side of the substrate; (e) performing at least one ion doping process on the back side of the substrate to form at least one ion doping layer; (f) performing an annealing process on the back side of the substrate; and (g) forming a collector metal layer on the back side of the substrate. 2 . The method for manufacturing an insulated gate bipolar transistor as claimed in claim 1 , wherein the laser pretreatment process is performed using a green laser. 3 . The method for manufacturing an insulated gate bipolar transistor as claimed in claim 1 , wherein a temperature of performing the laser pretreatment process is approximately between 1000° C. and 1500° C. 4 . The method for manufacturing an insulated gate bipolar transistor as claimed in claim 1 , wherein a execution time of the laser pretreatment process is approximately between 60-150 seconds. 5 . The method for manufacturing an insulated gate bipolar transistor as claimed in claim 1 , wherein the at least one ion-doped layer comprises a field-stop layer, and the insulated gate bipolar transistor is a field-stop insulated gate bipolar transistor. 6 . The method for manufacturing an insulated gate bipolar transistor as claimed in claim 1 , wherein the substrate is an N-type substrate or a P-type substrate.