Functional material for generating negative ion small molecule water through induction of precious metal, preparation method and application

The small molecule water functional material that induces negative ions through precious metals, uses the unique structural design and plasma resonance effect of composite fibers to solve the problems of poor stability and pollution of small molecule water, and achieves efficient production and stability improvement of negative ion small molecule water. It is suitable for Daily and outdoor use.

CN119080096AInactive Publication Date: 2024-12-06SUZHOU UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411194322.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The prior art has poor stability when converting macromolecular water into small molecule water, and it is easy to return to the macromolecular state after a long period of time, and there are problems of chemical contamination and microbial contamination in water.

Method used

Using small-molecule water functional materials that induce negative ions in precious metals, the preparation of zinc oxide and nano-precious metal composites with mesoporous structures to form composite fibers, and the use of its unique structural design and precious metal plasma resonance effect can achieve small water molecules. Moleculation and negative ionic small molecule water is generated through contact between fibers and water.

Benefits of technology

It has achieved the improvement of the stability of small molecule water, avoided contamination of chemical substances and microorganisms, simplified the preparation process without special devices, and is suitable for daily use and outdoor use, solving the problems of inconvenient portability and short shelf life of liquid canned water.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119080096A_ABST
    Figure CN119080096A_ABST
Patent Text Reader

Abstract

The invention discloses a functional material for generating negative ion small molecule water through induction of precious metal, a preparation method and application. A silicon oxide and zinc oxide composite polymer rich in a mesoporous structure is used as a hydrophilic layer, a polymer containing nano precious metal is used as a hydrophobic layer, composite long fibers are obtained, and the composite long fibers are made into a rod shape or a flat shape and used for treating water to obtain small molecule water containing negative ions. Unidirectional water conduction of a composite fiber interface is realized by utilizing the unique structural design of the fiber, charge separation at the interface is induced by utilizing a precious metal plasma resonance effect, and when a functional material is soaked in water, the water is dispersed into small molecular water with negative ions instantly by the metal plasma resonance effect. The invention overcomes the defects of poor stability, chemical pollution of water body, microbial pollution and the like of small molecule water obtained in the prior art, also solves the problems of invariable carrying, high transportation cost, short shelf life and the like of liquid canned water, and is suitable for daily use, outdoor use, business trip and other scenes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of negative ion small molecule water, and more specifically to the preparation of a functional material capable of generating small molecule water containing negative ions. Background Art

[0002] Water is omnipotent, therefore, functional water with water as the carrier has also come into being, such as disinfectant water, hydrogen-rich water, negative ion water, small molecule water, etc., but most of them enter the market in the form of liquid bottles, which is not only inconvenient to carry, but also has the problem of limited shelf life. The Bama area, which is known for its abundant small molecule water, has a lot of local natural water in a small molecule state due to the local magnetic field, air, geology and other reasons. However, once it leaves the area, the water quickly gathers together and becomes ordinary water.

[0003] The prior art uses magnetic field, electric field, ultrasound, far infrared, terahertz and other means to convert macromolecular water into small molecular water, but these methods usually require additional special devices. Chinese invention patent CN101624220B discloses a method for preparing small molecular water using a composite material, and the composite material provided contains substance A and substance B, substance A is one or more of tourmaline and CeO2-Fe2O3 composite oxide, and substance B is one or more of pyrophosphomolybdate, pyrophosphostanate, pyrophosphoferrate, and ferrate. Substance A and substance B are attached to the outer surface of a cylindrical structure, and water is directly passed through the outer surface of the cylindrical structure, so that macromolecular water can be converted into small molecular water. Chinese invention patent CN104230070B relates to a water treatment method and system for preparing small molecular cluster water, which includes a raw water pretreatment step, a small molecular cluster treatment step and a subsequent treatment step. The small molecular cluster treatment step performs small molecular cluster treatment on water through a water molecule cluster cutting reaction device. The device includes a tank body and a composite material filler located in the tank body. The composite material filler is a spherical material formed by activated sintering with tourmaline as the base material.

[0004] Chinese invention patent CN 115286870 A discloses a polypropylene composite material for preparing small molecule water and a preparation method thereof. The polypropylene composite material is prepared from the following components by weight: 70-80 parts of polypropylene resin; 15-25 parts of silicate minerals; 5-10 parts of terahertz wave generating materials; 1-5 parts of compatibilizers; 0.5-1 parts of antioxidants; and 0.5-1 parts of lubricants. After being evenly mixed, the mixture is melt-extruded and granulated through a twin-screw extruder. The prepared composite material has excellent water treatment performance. Water treated by short-term immersion in the composite material can be converted from large molecular cluster water to small molecular cluster water. The polypropylene composite material can be used in drinking water containers, filter bottles, filter elements, pipes and other devices in contact with water, or directly used in drinking water.

[0005] Although the existing technology can effectively convert macromolecular water into small molecule water, in actual use, the obtained small molecule water has poor stability and returns to the state of macromolecular clusters after being placed for a long time. In addition, there are problems such as chemical pollution and microbial pollution of water bodies. Summary of the invention

[0006] In view of the deficiencies in the prior art, the present invention provides a functional material, preparation method and application of a carrier material that can be in safe contact with water and has no water pollution caused by chemical substances, and produces abundant negative ions to ensure that small molecule water does not aggregate, and can effectively prevent water from being contaminated by microorganisms by inducing precious metals to produce negative ion small molecule water.

[0007] The technical solution to achieve the purpose of the present invention is to provide a method for preparing a functional material for generating anion small molecule water by inducing noble metals, comprising the following steps: (1) preparing spinning solutions of a P1 hydrophilic layer and a P2 hydrophobic layer respectively, wherein the P1 hydrophilic layer spinning solution comprises a composite of silicon oxide and zinc oxide rich in a mesoporous structure with a mass concentration of 0.01 to 0.1%, and the remainder is a hydrophilic polymer material of polyethylene, polylactic acid, and polyamide, and the P2 hydrophobic layer spinning solution comprises a nano-precious metal with a mass concentration of 0.01 to 0.1%, and the remainder is a hydrophobic polymer material of polyester and polypropylene; (2) adding the spinning solutions prepared in step (1) to the spinning pipelines respectively, heating and melting them, spraying them out through the spinneret assembly for compounding, and cooling them in the air for forming, thereby obtaining composite long fibers; (3) The prepared composite long fibers are drawn into bundles and cut into rods; or the prepared composite long fibers are cut into short pieces and formed into flat shapes by opening, spreading, hot air or hot pressing; thereby obtaining a rod-shaped or flat-shaped precious metal-induced functional material for generating negative ion small molecule water.

[0008] In the preferred technical solution, the nano noble metal is nano gold.

[0009] The preparation of the silicon oxide zinc oxide composite rich in mesoporous structure of the present invention comprises the following steps: adding 0.5 to 1.0% by mass of urea and 15 to 20% by mass of glycerol to a zinc acetate dihydrate solution with a concentration of 0.01 to 0.05 M, dissolving the mixture under high-speed mechanical stirring conditions, then adding 0.5 to 2.0% by mass of mesoporous silicon oxide, dispersing the mixture under ultrasonic and mechanical stirring conditions to obtain a mixed solution; placing the mixed solution in a microwave oven, and subjecting the mixed solution to microwave treatment for 10 to 30 minutes at a temperature of 155 to 175° C. to obtain the silicon oxide zinc oxide composite rich in mesoporous structure.

[0010] The technical solution of the present invention includes a functional material for producing negative ion small molecule water induced by noble metals obtained according to the above preparation method.

[0011] The technical solution of the present invention also provides an application of a functional material for inducing the production of negative ion small molecule water by precious metals, wherein the rod-shaped or flat functional material is immersed in water to treat the water, thereby obtaining small molecule water containing negative ions.

[0012] The invention provides an application of a functional material for inducing the production of negative ion small molecule water by noble metals. When treating water, the mass ratio of the functional material to water is 1:50-200; and the soaking treatment time is 10-60 minutes.

[0013] The present invention provides an application of a functional material for inducing the production of negative ion small molecule water by noble metals, wherein the small molecule water containing negative ions obtained after the treatment does not dissolve any chemical substance.

[0014] The technical solution of the present invention utilizes the unique structural design of the fabric to achieve unidirectional water conduction at the composite fiber interface, and utilizes the noble metal plasma resonance effect to induce charge separation at the interface. When water is immersed, the water is dispersed into small molecule water with negative ions. This solves the problems of poor stability of small molecule water prepared by the prior art, which returns to the state of large molecular clusters after long-term storage, as well as chemical pollution and microbial pollution of water bodies.

[0015] The functional material provided by the present invention is used as the main raw material, and after further processing, a functional device that can convert ordinary water into small molecule water containing negative ions within a few minutes can be prepared, which solves the problems of liquid bottled water being unchanged to carry, high transportation costs, and short shelf life. The device is suitable for use in daily use, outdoor use, business trips, and other scenarios.

[0016] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention utilizes the unique structural design of the fabric to overcome the problems of poor stability of small molecule water obtained in the prior art, recovery to a large molecular cluster state after long-term storage, and chemical pollution and microbial pollution of water bodies.

[0017] 2. Small molecule water containing negative ions can be obtained by simply soaking the fiber or the device made of the fiber in water, without the need for special preparation equipment and electric energy, etc. From preparation to application, it embodies the characteristics of safety, environmental protection and energy saving. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 , 2 The following are scanning electron microscope images of the cross section of the composite fiber prepared in Example 1 of the present invention before and after being soaked in water. DETAILED DESCRIPTION

[0019] The technical solution of the present invention will be clearly and completely described below in combination with the present embodiment and the accompanying drawings. Example 1

[0020] Preparation of a mesoporous silicon oxide-zinc oxide composite: 4.15 g of zinc acetate was dissolved in 100 ml of deionized water to prepare a clear solution, 0.55 g of urea and 15.0 g of glycerol were added to the zinc acetate aqueous solution, and dissolved by high-speed mechanical stirring, and then 1.0 g of mesoporous silicon oxide was dispersed in the above solution under ultrasonic action, and the mixed solution was placed in a microwave oven and microwaved at 160° C. for 30 min to obtain a mesoporous silicon oxide-zinc oxide composite, which was added to the HDPE material at a ratio of 10% in a slice modification device to obtain a modified PE material as the hydrophilic layer (outer layer) of the subsequent composite fiber.

[0021] Preparation of nano-gold: Add 5ml HAuCl4 and 5ml CTAB solution into a 20ml bottle, add 0.6ml 0.01M sodium borohydride solution, stir for 30min under ultrasound, let stand for 12h, centrifuge for 30min to obtain nano-gold solution. Dilute with glycerol to a certain concentration, add the prepared nano-gold dispersion to the PET material at a ratio of 5% in the slice modification device to obtain modified PET material, which will serve as the hydrophobic layer (inner layer) of the subsequent composite fiber.

[0022] In the composite fiber preparation device, the above two materials are added to the spinning melt pipe respectively, and after being heated and melted, they are extruded from the twin screws, and then sprayed out through the composite spinneret assembly, air-cooled and formed, and wound and stretched to obtain composite fibers.

[0023] See attached Figure 1 and 2 , are scanning electron micrographs of the cross sections of the composite fibers prepared in this embodiment before and after being immersed in water; Figure 1 It can be seen that the outer hydrophilic layer and the inner hydrophobic layer of the composite fiber present a uniform skin-core structure, forming a clearly visible interface; after the composite fiber is immersed for 10 minutes, Figure 2 The cross-sectional scanning electron micrograph shows that obvious peeling occurs at the interface between the hydrophilic layer and the hydrophobic layer after contacting water.

[0024] The obtained composite long fibers were drawn into bundles and cut into rods. A certain amount of the rods were taken and immersed in deionized water at a mass ratio of 1:50 to water for 0.5 h to obtain small molecule water with a half-peak width of 70.6.

[0025] The functional material samples prepared in this example were immersed in water at different mass ratios with water, and the water was treated. The obtained water was used for negative ion detection. The results are shown in Table 1.

[0026] Table 1 . Example 2

[0027] Preparation of a silicon oxide zinc oxide composite rich in mesoporous structure: dissolve 4.5 g of zinc acetate in 100 ml of deionized water to prepare a clear solution, add 0.55 g of urea and 18.0 g of glycerol to the zinc acetate aqueous solution, stir and dissolve it with a high-speed mechanical stirrer, then disperse 1.0 g of mesoporous silicon oxide in the above solution under ultrasonic action, put the above mixed solution into a microwave oven, microwave it at 170°C for 20 min, and obtain a silicon oxide zinc oxide composite rich in mesoporous structure, which is added to a PLA material at a ratio of 10% in a slice modification device to obtain a modified PLA material as a hydrophilic layer of the subsequent composite fiber.

[0028] Preparation of nano-gold: Add 5ml HAuCl4 and 5ml CTAB solution into a 20ml bottle, add 0.6ml 0.01M sodium borohydride solution, stir for 30min under ultrasound, let stand for 12h, centrifuge for 30min to obtain nano-gold solution. Dilute with glycerol to a certain concentration, add the prepared nano-gold dispersion to the PP material at a ratio of 5% in the slice modification device to obtain modified PP material, which will serve as the hydrophobic layer of the subsequent composite fiber.

[0029] In the composite fiber preparation device, the above two materials are added to the melt pipe of spinning respectively, extruded by a twin-screw, and then sprayed out by a composite spinneret assembly, cooled, formed, wound, stretched, curled and shaped, and finally the composite fiber is obtained. The prepared composite long fiber is drawn into bundles and sheared into rods. A certain amount of rods are taken at a mass ratio of 1:50 and immersed in deionized water for 0.5h to obtain small molecule water with a half-peak width of 78.2 and a negative ion number of 153500 ions / cm 3 . Example 3

[0030] Preparation of a silicon oxide zinc oxide composite rich in mesoporous structure: 5.0 g of zinc acetate was dissolved in 100 ml of deionized water to prepare a clear solution, 0.6 g of urea and 20.0 g of glycerol were added to the zinc acetate aqueous solution, and dissolved by high-speed mechanical stirring, and then 1.0 g of mesoporous silicon oxide was dispersed in the above solution under ultrasonic action, and the above mixed solution was placed in a microwave oven and microwaved at 175°C for 15 minutes to obtain a silicon oxide zinc oxide composite rich in mesoporous structure, which was added to the PA material at a ratio of 10% in a slice modification device to obtain a modified PA material as the hydrophilic layer of the subsequent composite fiber.

[0031] Preparation of nano-gold: Add 5ml HAuCl4 and 5ml CTAB solution into a 20ml bottle, add 0.6ml 0.01M sodium borohydride solution, stir for 30 minutes under ultrasound, let stand for 12h, and centrifuge for 30min to obtain nano-gold solution. Dilute with glycerol to a certain concentration, add the prepared nano-gold dispersion to the PET material at a ratio of 3.5% in the slice modification device to obtain a modified PET material as the hydrophobic layer of the subsequent composite fiber.

[0032] In the composite fiber preparation device, the above two materials are added to the melt pipe of spinning respectively, extruded by a twin screw, and then sprayed out by a composite spinneret assembly, cooled, formed, wound, stretched, curled and shaped, and finally the composite fiber is obtained. The obtained composite long fiber is drawn into bundles and sheared into rods. A certain amount of rods are taken at a mass ratio of 1:50 and immersed in deionized water for 0.5h to obtain small molecule water with a half-peak width of 88.5 and a negative ion number of 147000 ions / cm 3 .

Claims

1. A method for preparing a functional material for producing negative ion small molecule water induced by precious metals, Features The steps include: (1) preparing spinning solutions of a P1 hydrophilic layer and a P2 hydrophobic layer respectively, wherein the P1 hydrophilic layer spinning solution comprises a composite of silicon oxide and zinc oxide rich in a mesoporous structure with a mass concentration of 0.01 to 0.1%, and the remainder is a hydrophilic polymer material of polyethylene, polylactic acid, and polyamide, and the P2 hydrophobic layer spinning solution comprises a nano-precious metal with a mass concentration of 0.01 to 0.1%, and the remainder is a hydrophobic polymer material of polyester and polypropylene; (2) adding the spinning solution prepared in step (1) to the spinning pipeline respectively, heating and melting the solution and then ejecting the solution through the spinneret assembly, cooling the solution in the air and forming the composite long fiber; (3) The prepared composite long fibers are drawn into bundles and cut into rods; or the prepared composite long fibers are cut into short pieces and formed into flat shapes by opening, spreading, hot air or hot pressing; thereby obtaining a rod-shaped or flat-shaped precious metal-induced functional material for generating negative ion small molecule water.

2. The method for preparing a functional material for producing anionic small molecule water induced by noble metals according to claim 1, Features: The nano noble metal is nano gold.

3. The method for preparing a functional material for producing anionic small molecule water induced by noble metals according to claim 1, Features: The preparation of the silicon oxide zinc oxide composite rich in mesoporous structure comprises the following steps: adding 0.5 to 1.0% by mass of urea and 15 to 20% by mass of glycerol to a zinc acetate dihydrate solution with a concentration of 0.01 to 0.05 M, dissolving them under high-speed mechanical stirring conditions, then adding 0.5 to 2.0% by mass of mesoporous silicon oxide, dispersing them under ultrasonic and mechanical stirring conditions to obtain a mixed solution; placing the mixed solution in a microwave oven, and subjecting the mixed solution to microwave treatment for 10 to 30 minutes at a temperature of 155 to 175° C. to obtain the silicon oxide zinc oxide composite rich in mesoporous structure.

4. A functional material for producing negative ion small molecule water induced by noble metals obtained by the preparation method of claim 1.

5. Application of a functional material for producing negative ion small molecule water induced by noble metals as claimed in claim 4, Features: The rod-shaped or flat functional material is immersed in water to treat the water and obtain small molecule water containing negative ions.

6. Application of a functional material for producing negative ion small molecule water induced by noble metals according to claim 5, Features: When treating water, the mass ratio of the functional material to water is 1:50-200; the soaking treatment time is 10-60 minutes.

7. Application of a functional material for producing negative ion small molecule water induced by noble metals according to claim 5, Features: After treatment, the small molecule water containing negative ions does not contain any chemical substances dissolved.