Bearing component
Laser hardening non-functional surfaces in bearing components, combined with induction hardening of functional surfaces, addresses the challenges of cost and energy efficiency, enhancing wear resistance and reducing creep movements to extend bearing life.
Patent Information
- Application Number
- CN202410704429.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-05
- Filing Date
- 2024-06-03
- Publication Date
- 2024-12-06
AI Technical Summary
Existing bearing components face challenges in achieving cost-effective and energy-efficient production while minimizing warping and reworking, particularly in non-functional surfaces, which are prone to wear and creep movements, and existing technologies fail to address these issues effectively.
Laser hardening of non-functional surfaces in bearing components, combined with induction hardening of functional surfaces, to enhance wear resistance and reduce creep movements, while minimizing warping and reworking.
The combination of laser and induction hardening improves wear resistance, reduces creep movements, and extends the life of bearing components by optimizing friction and lubrication, thereby reducing material and energy costs.
Smart Images

Figure CN119084468A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a bearing component according to the preamble of claim 1 . Background Art
[0002] In order to have particularly good wear resistance and to resist the high loads to which the bearing components may be subjected, it is known practice to harden the bearing components specifically at their functional surfaces. In the context of the present application, a functional surface is understood to be in particular a raceway of a bearing component. In other words, a surface that is subject to high loads during bearing operation.
[0003] In order to save costs, in the case of selective hardening, for example in the case of induction hardening, non-functional surfaces, such as contact surfaces with the component receiving the bearing, are usually not hardened. Therefore, in the case of selective hardening, the non-functional surfaces have the initial hardness of the unhardened bearing component blank (for example 20HRC to 40HRC).
[0004] By contrast, if non-functional surfaces are hardened, for example in the case of through-hardening, the hardening can result in relatively pronounced warping, which then has to be compensated subsequently by hard machining.
[0005] It is therefore an object of the present invention to provide a bearing component which can be produced and hardened in an energy-efficient and cost-effective manner and which dispenses with laborious reworking. Summary of the invention
[0006] This object is achieved by the bearing component according to technical solution 1.
[0007] In the following, a bearing component is proposed, which has at least one raceway surface as a functional face and at least one further non-functional face different from the raceway surface.
[0008] In order to sufficiently protect the non-functional surfaces against wear, the present invention proposes that at least one non-functional surface has a first surface region which is laser-hardened.
[0009] In this case, the non-functional surface can in particular be the inside-diameter face of an inner ring, the outside-diameter face of an outer ring, a lateral face of a bearing ring, a shoulder of a bearing ring, an end face of a rolling element and / or a bore of a rolling element.
[0010] In some rolling bearings there may be rims which are necessary for retaining or guiding the rolling elements, such rims may be assigned both functional and non-functional surfaces and may therefore be induction hardened or laser hardened.
[0011] Due to the laser hardening of the non-functional surfaces, wear marks on the non-functional surfaces can be avoided during assembly of the bearing components. Likewise, due to the laser hardened non-functional surfaces, damage due to wear particles or damage to the bearing components can be avoided if creep movements occur between the bearing components and surrounding components. In addition, due to the laser hardened surface areas, wear can be reduced overall in the event of moving or sliding contacts between the bearing components and / or between the bearing components and the elements accommodating the bearing components, which extends the life of the bearing components and the bearing as a whole.
[0012] Furthermore, during laser hardening, microstructural phase changes occur, which lead to changes in the specific volume or density of the physical phases, for example during transformation into martensite and / or bainite. As a result, the hardened and transformed surface area has a larger volume than the initial phase and leads to a rise in the laser hardened surface in the micrometer range. As a result, interference fits and / or frictions can also be increased, in particular at contact surfaces with surrounding components, such as shafts or housings, with the result that the component is subject to less creep movements.
[0013] However, an increase in the coefficient of friction can also reduce the interference fit or force fit itself, because the high coefficient of friction ensures an equally good form fit between the components. Lower interference fit or lower force fit contributions in turn produce lower tensile stresses in the bearing components (e.g., an inner ring that is shrink-fitted to a shaft), which in turn results in longer component life.
[0014] Furthermore, the increase in the coefficient of friction between the bearing components and the surroundings (eg seat / shaft) due to the texturing of the surface can help to avoid movement (eg ring creep), thereby extending the life of the bearing components.
[0015] Furthermore, laser hardening is a relatively cost-effective hardening process. However, for raceways or functional surfaces, laser hardening can only be used to a limited extent, since the hardness penetration depth that can be achieved by laser hardening is generally not sufficient to cover the Hertzian stresses. However, for the loads to be expected at non-functional surfaces, the hardness penetration depth that can be achieved by laser hardening is completely sufficient.
[0016] Another advantage of laser hardening is that during laser hardening, if any warping occurs in the bearing component, only very little warping occurs, so that expensive reworking, especially laborious hard machining, can be partially or completely dispensed with. This also has the advantage that less material needs to be added, since less deformation occurs, which represents better material utilization and likewise saves costs.
[0017] Furthermore, the laser hardening process can be integrated into a reworking procedure (turning, grinding, honing, etc.), wherein even integration into existing machines is possible.
[0018] Laser hardening can be performed with one or more laser heads.
[0019] Furthermore, laser hardening has other advantages; in particular, laser hardening has low energy consumption and low CO2 emissions. In addition, laser hardening exhibits a high energy density and short processing times. It is also advantageous that only small volumes are affected, or only a small part of the workpiece cross section is processed, and that no process gases are required. Furthermore, during laser hardening, the workpiece does not need to be quenched after heating, since quenching occurs by heat conduction in the constituent components. This has the advantage that no quenching medium is required and therefore no pumps are required for quenching or cooling the plant. Moreover, the same laser source and optical unit are used for different workpiece geometries, so that part-specific tooling can be omitted.
[0020] Laser hardening of non-functional surfaces also enables the use of lower alloy steels, which in turn reduces CO2 emissions during steel production.
[0021] According to a further preferred exemplary embodiment, the non-functional surface is subjected to sliding contact with an element that accommodates a bearing component and / or to sliding contact with another bearing component in the assembled state. In the case of sliding contact, a smaller hardness penetration depth is generally sufficient, since the maximum stress (stress maximum) generally forms closer to the surface than in the case of rolling contact. Therefore, in the case of sliding contact, hardening by means of a laser is sufficient, which can only achieve a small hardness penetration depth (down to about 2 mm) in order to produce a sufficiently hard and wear-resistant volume on the corresponding surface.
[0022] Preferably, the functional surfaces (particularly the raceway surfaces) are induction hardened. This can ensure that these surfaces withstand ( / withstand) high loads, particularly in the case of rolling contact. As a result of the combination of induction hardening and laser hardening, less warping can be introduced into the component parts compared to a comparable ( / effectively comparable / comparable) through-hardening process ( / through-hardening process), which can lead to less hard machining, thereby saving costs / energy. In this case, laser hardening of non-functional surfaces can be carried out before or after the induction hardening process. Laser hardening can even be carried out in an induction hardening machine. As a further option, laser hardening can be carried out before induction hardening, particularly during soft machining (e.g. on a lathe, special machine tool), or after induction hardening (e.g. on a hard lathe, a grinding machine, eddy current testing, etc., or on a special machine tool).
[0023] According to a further preferred exemplary embodiment, the bearing component is a bearing component of a rolling bearing (eg a bearing ring or a rolling element) in which the raceway surfaces are subject to rolling contact.
[0024] According to a further preferred exemplary embodiment, the non-functional surface has at least one second surface region which is not laser hardened.
[0025] As mentioned above, during laser hardening, microstructural phase transformations occur, which lead to changes in the specific volume or changes in the density of the physical phase, for example during the transformation to martensite and / or bainite. As a result, the hardened and transformed areas have a larger volume than the initial phase and lead to a rise in the laser hardened surface in the micrometer range. In combination with the unhardened surface areas, this allows the application of specific surface textures.
[0026] Thus, as shown in another preferred exemplary embodiment, a laser-hardened first surface area can have a first coefficient of friction and a non-laser-hardened second surface area can have a second coefficient of friction, wherein the first coefficient of friction is higher than the second coefficient of friction.
[0027] Because the bearing component has a targeted increase in the coefficient of friction at specific points, the bearing component and the counterpart (e.g., shaft / seat) may be more difficult to move relative to each other during use. The increase in the coefficient of friction and the specific configuration of the surface texture may allow for a lower interference fit or a lower force fit contribution, which in turn produces lower tensile stresses in the bearing component and extends component life.
[0028] Alternatively or additionally, the first surface area and the second surface area can be configured such that the second surface area forms a lubricant reservoir and / or a lubricant channel delimited by the first surface area. This advantageously contributes to reducing wear in the event of sliding contact. Furthermore, this can ensure that the lubricant can be retained at a specific point on the bearing component and / or can be directed to a specific point in the bearing component.
[0029] According to a further advantageous exemplary embodiment, the first surface area is formed so as to be continuous.
[0030] Thus, the bearing component can be realized without weak points over the entire circumferential surface, which ensures, for example, a uniform increase in the coefficient of friction and thus a uniform force transmission. This can be achieved with one or more laser heads.
[0031] Alternatively, it may of course be advantageous to form the first surface region as discrete surface region portions.
[0032] Thus, for example, a soft, non-laser-hardened area can be provided over the entire circumferential surface between the start and end position of the scanning operation, or even a plurality of soft areas allowing a specific pattern to be formed. Thus, for example, the hardening can be in the form of a plurality of rectangles / squares, a plurality of circular / elliptical points, a plurality of triangles, or in the form of a sawtooth, optionally with different angles.
[0033] In this case, the patterns may contain other functions, such as the lubricant reservoirs or channels mentioned above. However, the patterns may also be configured as just a specific design, for example, visually assigning the bearing to the applicant as manufacturer by these patterns themselves.
[0034] Another aspect of the present application relates to a bearing having the bearing component as described above.
[0035] Further advantages and advantageous embodiments are specified in the description, the drawings and the claims. In particular, the combinations of features specified in the description and the drawings are by way of example only, so that these features may also exist alone or in some other combination. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Hereinafter, the present invention will be described in more detail with reference to the exemplary embodiments shown in the accompanying drawings. The exemplary embodiments and the combinations shown in the exemplary embodiments are only examples and are not intended to determine the scope of protection of the present invention. The scope of protection of the present invention is limited only by the attached claims.
[0037] In the attached picture:
[0038] Figure 1 : shows a schematic cross-sectional view through a first exemplary embodiment of a bearing component;
[0039] Figure 2 : shows a schematic cross-sectional view through a second exemplary embodiment of a bearing component;
[0040] Figure 3 : shows a schematic cross-sectional view through a third exemplary embodiment of a bearing component;
[0041] Figure 4 : A schematic perspective view showing a fourth exemplary embodiment of a bearing component;
[0042] Figure 5 : A schematic perspective view showing a fifth exemplary embodiment of a bearing component;
[0043] Figure 6 : A schematic perspective view showing a sixth exemplary embodiment of a bearing component;
[0044] Figure 7 : A schematic perspective view showing a seventh exemplary embodiment of a bearing component;
[0045] Figure 8 : A schematic perspective view showing an eighth exemplary embodiment of a bearing component;
[0046] Fig. 9 : A schematic perspective view showing a ninth exemplary embodiment of a bearing component;
[0047] Fig.10 : A schematic perspective view showing a tenth exemplary embodiment of a bearing component;
[0048] Fig.11 : A schematic perspective view showing an eleventh exemplary embodiment of a bearing component.
[0049] Reference numerals list
[0050] 1 Bearing ring
[0051] 2 Outer ring
[0052] 4 Inner ring
[0053] 6, 7 rolling tracks
[0054] 8 Hardness layer
[0055] t Hardness penetration depth
[0056] 9.10 Rim faces
[0057] 12, 13 shoulder surface
[0058] 14, 15 lateral surface
[0059] 16 inner diameter surface
[0060] 17 Outer diameter surface
[0061] 20 Laser hardened surface area
[0062] 22 Surface area not laser hardened
[0063] 24 End area
[0064] 26 Gap
[0065] 30 Rolling elements
[0066] 36 Rolling element raceway
[0067] 34, 35 rolling element end faces DETAILED DESCRIPTION
[0068] In the following, the same elements or elements having the same function are denoted by the same reference numerals.
[0069] Figure 1 A cross section through a bearing ring of a ball bearing is schematically shown, wherein the bearing ring 1 can represent the outer ring 2 or the inner ring 4. In addition, Figure 1The bearing ring 1 is shown with a raceway 6 which is subjected to rolling contact with rolling elements, in this case balls, during operation. The raceway 6 therefore represents a functional surface for the ball bearing, since this surface represents a function that is important for the operation of the bearing, namely a rolling surface for the rolling elements. In order to withstand loads arising, for example, due to rolling contact with the rolling elements, the raceway 6 is usually hardened, in particular induction hardened. This produces a hardness layer 8 which usually has a hardness penetration depth t suitable for covering the Hertzian stresses arising due to rolling contact with the rolling elements at this surface.
[0070] In the exemplary embodiment shown, the secondary or non-functional faces of the bearing rings are respectively the shoulder faces 12, 13, the end faces 14, 15 and the inside-diameter face 16 (in the case of the bearing inner ring 2) and the outside-diameter face 17 (in the case of the bearing outer ring 4). These non-functional faces 12 to 17 are usually not hardened. The reason for this is that, firstly, during the induction hardening or through-hardening ( / through-hardening) of the bearing components, relatively significant warping can be expected, which requires reworking to give the bearing components the appropriate dimensions. However, this reworking must be carried out on a particularly hardened material, which places higher demands on the corresponding tools than for processing unhardened bearing components. In addition, hardening is very expensive and energy-intensive, so it is usually only used at points where hardening is critical to the function of the bearing.
[0071] In contrast, the non-functional surfaces 12 to 17 are usually not subjected to significant loads during the operation of the bearing, so that no special hardening is required here. However, it has been found that in particular in the case of non-functional surfaces that are subject to sliding contact (for example by contact with an element that accommodates a bearing component), such as a shaft to which the inner ring is fastened for joint rotation, or a housing connected to the outer ring for joint rotation, and also in the case of surfaces that serve, for example, as sealing contact surfaces or as cage guides, such as shoulders 12, 13, increased wear may be found. Therefore, in particular during the assembly of the bearing ring 1 in or on the housing component (shaft; housing), increased wear or wear signs may be found, which limits the operation and life of the bearing.
[0072] Furthermore, so-called ring creep (i.e. a movement of the ring relative to the accommodating component) can occur at the connection between the bearing component and the accommodating element, which is in fact intended for conjoint rotation, which should be avoided. In order to avoid such ring creep, the bearing component is usually attached to the accommodating component with a very high interference fit, which requires a relatively large overlap, but which in turn leads to very high tensile stresses in the bearing and the accommodating component. Therefore, as an alternative or in addition, it is known to apply a friction coating or other mechanical fastening elements, such as twist-prevention means, at the corresponding faces, such as at the inner circumferential face or at the outer circumferential face, at the outer diameter.
[0073] In order to solve these problems, it is proposed to make at least one of the secondary surfaces 12 to 16 also hardened, which reduces wear. Laser hardening causes a phase change, which leads to a change in the volume of the hardened material, so that the hardened point protrudes slightly from the surface. This fact can be used to locally increase the friction coefficient at the laser-hardened surface area, or to provide the surface with a specific texture, which ensures, for example, that lubricant is retained at a specific point or guided to a specific position. In this case, the friction area increase property of laser hardening is preferred, especially at the surfaces in contact with the surrounding components, such as the inner diameter surface 16 or the outer diameter surface 17 of the bearing ring 1, because as a result a smaller overlap can be selected, but a connection for joint rotation between the bearing component and the surrounding components can still be achieved that is comparable (if not better). This in turn reduces the tensile stresses in the bearing itself and thereby extends the service life.
[0074] In contrast, at the shoulder surfaces 12 and 13, for example, a lubricant reservoir structure or a lubricant channel structure can be particularly preferably applied, which guides the lubricant in the direction of ( / towards) the rolling elements or ensures that the lubricant remains at this point and is not transported away.
[0075] Figure 2 and Figure 3 Each shows another example of a bearing component, wherein: Figure 2 The inner ring 2 and the outer ring 4 of the tapered roller bearing are shown. Figure 3 A tapered roller 30 is shown for use in such a bearing. Figure 2It is evident that in the case of tapered roller bearings, the raceway 6 of the inner ring 2 and the raceway 7 of the outer ring 4 are also hardened by means of induction, wherein the hardness penetration depth is again selected such that the Hertzian stresses are covered or such that the set fatigue strength profile satisfies the stress distribution. In the case of tapered roller bearings, in addition to the raceways, the rims are also considered to be functional surfaces, since the rims are also subject to high loads during bearing operation. Therefore, the rim faces 9 and 10 on which the tapered rollers run are usually also induction hardened.
[0076] also, Figure 2 It is shown that the inner diameter surface 16 (ie, the bore) of the bearing inner ring 2, the bearing outer diameter surface 17 of the bearing outer ring 4, and the end surfaces 14 and 15 of the respective bearing rings 2; 4 exhibit laser hardening.
[0077] Figure 3 A tapered roller 30 is schematically shown, the raceway 36 of which is induction hardened, while the end faces 34 , 35 or a possibly present bore (not shown) of the tapered roller 30 are laser hardened.
[0078] Figures 4 to 11 Different laser-hardened outer circumferential surfaces 17 are schematically illustrated by way of the example of a bearing outer ring 4 .
[0079] So, for example, Figure 4 The entire surface of the outer side 17 of the bearing ring is shown to be laser hardened in a slip-free manner. Figure 5 It is shown that not all of the surface 17 is laser hardened, but only a portion of the surface 17, in this case the ring portion 20, can be laser hardened. Thus, in the exemplary embodiment shown, the outer circumferential face 17 has a laser-hardened region 20 and two regions 22-1, 22-2 arranged adjacent to the region 20, which have not yet been subjected to laser hardening and therefore have the softness of untreated material. In addition, Figure 5 It is shown that the laser-hardened surface region 20 extends continuously around the entire bearing ring 4 .
[0080] In contrast, Figure 6 In the exemplary embodiment of the laser hardened surface area 20 does not extend around the entire circumference, so that a gap 26 remains in the end area 24. Such a gap 26 can occur, for example, during the scanning of the bearing ring. However, since the laser hardened surface 20 is a secondary or non-functional surface, the small unhardened area 26 is uncritical even with regard to the wear characteristics of the bearing ring.
[0081] Figure 7 Two laser-hardened surface areas 20-1, 20-2 are shown, each of which has a non-laser-hardened area 22-1, 22-2, 22-3 laterally and centrally. These areas can be used, for example, as lubricant channels in order to retain lubricant on the non-laser-hardened area 22 in a targeted manner. Figures 4 to 7 In addition to the further extended exemplary embodiments, it is also possible to laser harden only discrete points, such as in Figures 8 to 11 Of course, other patterns are conceivable, and thus specific patterns, for example for assigning bearing rings to specific manufacturers, are also possible.
[0082] Overall, as a result of the laser hardening of non-functional surfaces, bearing components can be provided which exhibit greater wear resistance. At the same time, as a result of the laser hardening of non-functional surfaces, a surface texture can be applied, which reduces the relative movement between the bearing component and the component in which it is accommodated. In particular, laser hardening also makes it possible to harden bores, such as inner ring bores or bores in rolling elements, thereby significantly improving the bearing component properties. The laser hardening itself can be carried out with one or more laser heads and can preferably be integrated into existing machining processes, with the result that no additional expensive machining steps are required.
Claims
1. A bearing component (1; 30) having at least one raceway surface (6; 7; 36) as a functional surface and at least one further non-functional surface (12; 13; 14; 15; 16; 17) different from the raceway surface (6; 7; 36), characterized in that: At least one non-functional surface (12; 13; 14; 15; 16; 17) has a laser-hardened first surface region (20).
2. The bearing component (1; 30) according to claim 1, characterized in that The non-functional surface (12; 13; 14; 15; 16; 17) is in sliding contact with another bearing component and / or in the assembled state is in sliding contact with an element that accommodates the bearing component, or is in contact with an element that accommodates the bearing component.
3. The bearing component (1; 30) according to claim 1 or 2, characterized in that: The raceway surface (6; 7; 36) is induction hardened.
4. Bearing component (1; 30) according to any one of the preceding claims, characterized in that The bearing component is a bearing component of a rolling bearing, and the raceway surface (6; 7; 36) is subject to rolling contact.
5. Bearing component (1; 30) according to any one of the preceding claims, characterized in that The non-functional surface (12; 13; 14; 15; 16; 17) has at least one second surface area (22) which is not laser hardened.
6. The bearing component (1; 30) according to claim 5, characterized in that The laser-hardened first surface area (20) has a first friction coefficient and the non-laser-hardened second surface area (22) has a second friction coefficient, wherein the first friction coefficient is different from the second friction coefficient, in particular, the first friction coefficient is higher than the second friction coefficient.
7. The bearing component (1; 30) according to claim 5 or 6, characterized in that: The first surface area (20) and the second surface area (22) are configured such that the second surface area (22) forms a lubricant reservoir and / or a lubricant channel (26) delimited by the first surface area (20).
8. Bearing component (1; 30) according to any one of the preceding claims, characterized in that The first surface area (20) is formed to be continuous.
9. The bearing component (1; 30) according to any one of claims 1 to 7, characterized in that The first surface area (20) is formed as discrete surface area portions.
10. Bearing component (1; 30) according to any one of the preceding claims, characterized in that The non-functional surface (12; 13; 14; 15; 16; 17) is the inner diameter surface (16) of the inner ring (4), the outer diameter surface (17) of the outer ring (2), the lateral surface (14; 15) of the bearing ring (1), the shoulder (12; 13) of the bearing ring (1), the edge (9; 10) of the bearing ring (1), the end surface (34; 35) of the rolling element (30) and / or the hole of the rolling element (30).
11. A bearing having a bearing component (1; 30) according to any one of the preceding claims.