Method for producing a sealing for a semiconductor module and housing for a semiconductor module

A pre-seal method using a matrix material and delayed adhesion promoter activation forms a strong, bubble-free seal between the housing and substrate, addressing contamination issues and reducing production costs in semiconductor modules.

CN119092418APending Publication Date: 2024-12-06INFINEON TECHNOLOGIES AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410705160.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-06-06
Filing Date
2024-06-03
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing semiconductor module seals face challenges in forming strong, bubble-free adhesions between the housing and substrate due to contamination and incompatible curing processes, leading to reduced sealing effectiveness and increased production costs.

Method used

A method involving a pre-seal composed of a matrix material and adhesion promoter, where the adhesion promoter is activated at a higher temperature after initial curing, ensuring a strong adhesive bond without additional fasteners, and a housing design with a pre-seal on its lower surface to facilitate this process.

Benefits of technology

The solution provides a robust, bubble-free seal with enhanced adhesion, reducing production costs and extending the lifetime of semiconductor modules by preventing environmental contaminants from entering the housing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092418A_ABST
    Figure CN119092418A_ABST
Patent Text Reader

Abstract

A method for manufacturing a seal for a semiconductor module includes applying a first material to a first surface, the first material including a matrix material and an adhesion promoter, where the matrix material is configured to cure when heated to a defined temperature for a defined period of time, and wherein the adhesion promoter is configured to be activated when heated to a temperature above a defined temperature and / or for a period of time longer than a defined period of time, and heating the first material to the defined temperature for the defined period of time such that the matrix material cures and the adhesion promoter remains inactive, thereby forming the pre-seal.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a method for producing a seal for a semiconductor module and to a housing for a semiconductor module. Background Art

[0002] The power semiconductor module device generally includes at least one semiconductor substrate arranged in a housing. A semiconductor device including a plurality of controllable semiconductor elements (e.g., two IGBTs in a half-bridge configuration) is arranged on each of the at least one substrate. Each substrate generally includes a substrate layer (e.g., a ceramic layer), a first metallization layer deposited on a first side of the substrate layer, and a second metallization layer deposited on a second side of the substrate layer. The controllable semiconductor elements are mounted on, for example, the first metallization layer. The second metallization layer can be optionally attached to a substrate. The controllable semiconductor device is generally mounted on the semiconductor substrate by welding or sintering techniques.

[0003] The components of the semiconductor module device are usually protected from mechanical damage or other environmental influences by means of a housing. For example, the housing needs to be securely mounted to a substrate or base plate. A seal can be arranged between the housing and the substrate or base plate to prevent particles or gases from entering the interior of the housing.

[0004] There is a need for a semiconductor module arrangement that provides protection for semiconductor components arranged therein such that the overall lifetime of the power semiconductor module arrangement is increased. Summary of the invention

[0005] A method includes applying a first material to a first surface, the first material including a matrix material and an adhesion promoter, wherein the matrix material is configured to cure when heated to a defined temperature for a defined period of time, and wherein the adhesion promoter is configured to be activated when heated to a temperature above the defined temperature and / or for a period of time longer than the defined period of time, and heating the first material to the defined temperature for a defined period of time such that the matrix material cures and the adhesion promoter remains inactive, thereby forming a pre-seal.

[0006] A housing for a power semiconductor module device includes a side wall and a cover, and a pre-seal arranged on a lower surface of the side wall, wherein the pre-seal includes a cured matrix material and an adhesion promoter, wherein the adhesion promoter is configured to be activated at or above a second temperature.

[0007] The present invention can be better understood with reference to the following drawings and descriptions. The components in the drawings are not necessarily drawn to scale, but emphasis is placed on illustrating the principles of the present invention. In addition, in the drawings, the same reference numerals represent corresponding parts in all different views. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figure 1is a cross-sectional view of a power semiconductor module device.

[0009] Figure 2 is a cross-sectional view of another power semiconductor module device.

[0010] Figure 3A and 3B A conventional method for forming a seal and a method for forming a seal according to one example are shown.

[0011] Figure 4 , 5 6 schematically illustrate a method for manufacturing a seal for a semiconductor module according to an example.

[0012] Figure 7 is a top view of an exemplary seal for a power semiconductor module arrangement.

[0013] Fig. 8A and Figure 8B is a cross-sectional view of a housing for a power semiconductor module device, with a seal formed on the housing.

[0014] Fig.9A and 9B is a cross-sectional view of a side wall of a housing with a seal formed thereon. DETAILED DESCRIPTION

[0015] In the following detailed description, reference is made to the accompanying drawings. The accompanying drawings show specific examples in which the present invention can be implemented. It should be understood that, unless otherwise specifically stated, the features and principles described with respect to the various examples can be combined with each other. In the specification and the claims, naming certain elements as "first element", "second element", "third element", etc. should not be understood as enumerable. On the contrary, such names are only used to express different "elements". That is, for example, the presence of a "third element" does not require the presence of a "first element" and a "second element". The wire or electrical connection as described herein can be a single conductive element, or include at least two separate conductive elements connected in series and / or in parallel. The wire and the electrical connection can include metal and / or semiconductor material, and can be permanently conductive (i.e., non-switchable). The semiconductor body as described herein can be made of (doped) semiconductor material, and can be a semiconductor chip or included in a semiconductor chip. The semiconductor body has an electrical connection pad and includes at least one semiconductor element having an electrode.

[0016] refer to Figure 1, a cross-sectional view of a power semiconductor module device 100 is shown. The power semiconductor module device 100 comprises a housing 7 and a substrate 10. The substrate 10 comprises a dielectric insulating layer 11, a (structured) first metallization layer 111 attached to the dielectric insulating layer 11, and a (structured) second metallization layer 112 attached to the dielectric insulating layer 11. The dielectric insulating layer 11 is arranged between the first metallization layer 111 and the second metallization layer 112.

[0017] Each of the first metallization layer 111 and the second metallization layer 112 may be composed of or include one of the following materials: copper; copper alloy; aluminum; aluminum alloy; any other metal or alloy that remains solid during operation of the power semiconductor module device. The substrate 10 may be a ceramic substrate, i.e., a substrate in which the dielectric insulating layer 11 is a ceramic (e.g., a thin ceramic layer). The ceramic may be composed of or include one of the following materials: aluminum oxide; aluminum nitride; zirconium oxide; silicon nitride; boron nitride; or any other dielectric ceramic. For example, the dielectric insulating layer 11 may be composed of or include one of the following materials: Al2O3, AlN, SiC, BeO, or Si3N4. For example, the substrate 10 may be, for example, a direct copper bonding (DCB) substrate, a direct aluminum bonding (DAB) substrate, or an active metal brazing (AMB) substrate. In addition, the substrate 10 may be an insulated metal substrate (IMS). The insulated metal substrate typically includes a dielectric insulating layer 11, which includes a (filled) material, such as an epoxy resin or a polyimide. For example, the material of the dielectric insulating layer 11 can be filled with ceramic particles. Such particles can include, for example, SiO2, Al2O3, AlN or BN, and can have a diameter between about 1 μm and about 50 μm. The substrate 10 can also be a conventional printed circuit board (PCB) with a non-ceramic dielectric insulating layer 11. For example, the non-ceramic dielectric insulating layer 11 can consist of or include a cured resin.

[0018] The substrate 10 is arranged in the housing 7. Figure 1 In the example shown, the substrate 10 forms the ground surface of the housing 7, while the housing 7 itself only includes side walls and a cover. However, this is only an example. The substrate 10 can also be mounted on a base plate. In some power semiconductor module devices 100, more than one substrate 10 is arranged on a single base plate. For example, the base plate can form the ground surface of the housing 7. That is, the side walls of the housing 7 can be attached to the base plate, thereby covering at least one substrate 10.

[0019] One or more semiconductor bodies 20 may be arranged on at least one substrate 10. Each of the semiconductor bodies 20 arranged on at least one substrate 10 may include a diode, an IGBT (insulated gate bipolar transistor), a MOSFET (metal oxide semiconductor field effect transistor), a JFET (junction field effect transistor), a HEMT (high electron mobility transistor), or any other suitable controllable or uncontrollable semiconductor element.

[0020] One or more semiconductor bodies 20 may form a semiconductor device on the substrate 10. Figure 1 In FIG. 2 , only two semiconductor bodies 20 are shown by way of example. Figure 1 The second metallization layer 112 of the semiconductor substrate 10 in the embodiment is a continuous layer. However, the second metallization layer 112 may also be omitted. The second metallization layer 112 may also be a structured layer. Figure 1 In the example shown, the first metallization layer 111 is a structured layer. In this context, "structured layer" means that the first metallization layer 111 is not a continuous layer, but includes recesses between different sections of the layer. Such recesses are Figure 1 . In this example, the first metallization layer 111 includes three different sections. Different semiconductor bodies 20 can be mounted on the same or different sections of the first metallization layer 111. Different sections of the first metallization layer may not have an electrical connection, or may be electrically connected to one or more other sections using, for example, a bonding wire 3. For example, the electrical connection 3 may also include a bonding tape, a connecting plate, or a conductor track, to name a few. One or more semiconductor bodies 20 can be electrically and mechanically connected to the substrate 10 via a conductive connection layer 30. For example, such a conductive connection layer can be a solder layer, a conductive adhesive layer, or a sintered metal powder (e.g., sintered silver powder) layer.

[0021] The power semiconductor module device 100 also includes a terminal element 4. The terminal element 4 is electrically connected to the first metallization layer 111 and provides an electrical connection between the inside and the outside of the housing 7. The terminal element 4 can be electrically connected to the first metallization layer 111 through a first end, while the second end 41 of the terminal element 4 protrudes from the housing 7. The terminal element 4 can be electrically contacted from the outside at its second end 41. However, such a terminal element 4 is only an example. The components inside the housing 7 can be electrically contacted from the outside of the housing 7 in any other appropriate manner. For example, the terminal element 4 can be arranged closer to the side wall of the housing 7 or adjacent to the side wall of the housing 7. The terminal element 4 can also protrude vertically or horizontally through the side wall of the housing 7. It is even possible that the terminal element 4 protrudes through the ground surface of the housing 7.

[0022] The semiconductor bodies 20 may each include chip pad metallization, such as source, drain, anode, cathode or gate metallization. The chip pad metallization generally provides a contact surface for electrically connecting the semiconductor body 20. For example, the chip pad metallization may electrically contact the connection layer 30, the terminal element 4 or the electrical connection 3. The chip pad metallization may consist of or include a metal such as aluminum, copper, gold or silver. For example, the electrical connection 3 and the terminal element 4 may also consist of or include a metal such as copper, aluminum, gold or silver.

[0023] The power semiconductor module device 100 also includes a casting compound 5. For example, the casting compound 5 may be composed of or include silicone gel, silicone, polyurethane, epoxy resin or polyacrylate-based isolation material, or may be a rigid molding compound. The casting compound 5 may at least partially fill the interior of the housing 7, thereby covering the components and electrical connections arranged on the substrate 10. The terminal element 4 may be partially embedded in the casting compound 5. However, at least its second end 41 is not covered by the casting compound 5, and protrudes from the casting compound 5 through the housing 7 to the outside of the housing 7. The casting compound 5 is configured to protect the components and electrical connections inside the power semiconductor module 100 (particularly inside the housing 7) from certain environmental conditions and mechanical damage. The casting compound 5 can be formed by dispensing a material (e.g., an uncured dielectric gel) into the housing 7 after the housing 7 has been mounted to the substrate 10 or base plate, and then curing the material.

[0024] The housing 7 surrounds the device and provides further protection from certain environmental conditions and mechanical damage. As described above, for example, the housing 7 can be attached to the substrate 10, or if the substrate 10 is arranged on a base plate, the housing 7 can be attached to the base plate. In order to prevent the casting compound 5 from escaping between the housing 7 and the substrate 10 or the base plate, and to prevent contaminants or gases (e.g., corrosive gases) from entering the interior of the housing 7, a seal 8 can be arranged between the housing 7 and the substrate 10 (or between the housing 7 and the base plate). Reference Figure 2 , schematically shows a semiconductor module arrangement 100 including a seal 8 between a substrate 10 and a housing 7 .

[0025] In order to form the seal 8, the material of the seal 8 can be applied in liquid or viscous form on the substrate 10 (or base plate) or to the housing 7. The housing 7 can then be arranged on the substrate 10 (or base plate), wherein the material of the seal 8 is arranged between the housing 7 and the substrate 10 (or base plate). The material of the seal 8 can then be cured, for example by heating the device. During the curing process, the presence of contaminants may lead to the formation of bubbles and unwanted cavities in the seal 8, which may reduce the sealing ability of the seal 8. Measures to avoid unwanted bubble formation lead to higher costs due to additional process steps and / or longer cycle times. In addition, components of the viscous seal 8 may interact with other module components, in particular during heating until curing, which may have an adverse effect on the module, for example, by reduced cycle times.

[0026] Additionally, there is a risk that contaminants in the material forming the seal will interfere with the curing process so that uncured (unsolidified) material remains between the housing and the cured portion of the seal 8. This may also result in a reduction in the sealing ability of the seal 8. For example, corrosive gases may be able to enter the housing 7 through a non-cured layer of sealing material.

[0027] Therefore, it is important to prevent air from penetrating into the material 90 so that the seal 8 is free of any unwanted bubbles or cavities. Furthermore, any fluid or moisture that may be present in the housing 7 should be prevented from penetrating into the seal 8. Therefore, the seal 8 should also be free of any unwanted bubbles and uncured material. Measures to avoid the formation of unwanted bubbles lead to higher costs due to additional process steps and / or longer cycle times.

[0028] Reference now Figure 3A , schematically illustrates a conventional process for forming a seal. A liquid or viscous material 90 (in Figure 3AThe material 90 is disposed on the substrate 10 or substrate with the material 90 disposed therebetween (step 302A). The material 90 typically includes a matrix material 82 (e.g., a silicone-based matrix material) and an adhesion promoter 84. An adhesion promoter (also commonly referred to as a coupling agent) is a chemical that acts at the interface between two different materials (e.g., an organic polymer such as a matrix material and an inorganic material such as a shell, substrate, and substrate) to enhance the adhesion between the two materials. Organic and inorganic materials are very different in many respects, such as compatibility, chemical reactivity, surface characteristics, and thermal expansion coefficients, making it difficult to form a strong adhesive bond between each of the two different materials and the matrix material 82. The adhesion promoter 84 effectively acts at the interface between the matrix material 82 and each of the organic material and the inorganic material (for example, the interface between the matrix material 82 and the shell 7, and the interface between the matrix material 82 and the substrate 10 or baseplate) to chemically and physically bond each of these different materials to the matrix material 82 via a strong adhesive bonding structure.

[0029] The curing process is typically conducted at a sufficiently high temperature and applied for a sufficient duration to solidify (cure) the matrix material 82 and activate the adhesion promoter 84. That is, during the curing process, a cross-linking process occurs and the adhesion promoter 84 is activated, resulting in certain adhesive properties of the resulting seal 8. Once activated, the adhesion promoter is consumed, such that it becomes unreactive, i.e., it cannot be activated again at a later time.

[0030] Reference now Figure 3B , schematically illustrating a method according to an example. A material 90 including a silicone-based matrix material 82 and an adhesion promoter 84 may be provided. The material 90 may be provided with respect to Figure 3A The material 90 described is the same or similar. In a first step (step 301B), the material 90 is heated to a first temperature. However, the first temperature is lower than the temperature required to activate the adhesion promoter 84, or the duration of application of the first temperature is too short (insufficient) to completely consume the adhesion promoter 84. That is, the material 90 (matrix material 82) is cured (a cross-linking process occurs) while ensuring that a sufficient amount of the adhesion promoter 84 remains in the pre-seal 92 after curing. The resulting intermediate product (pre-seal 92) is solid (cured / hardened), but has limited adhesive properties, that is, although it may be slightly sticky, it cannot be permanently attached to a surface. This makes the pre-seal 92 easy to handle. For example, in Figure 3BStep 301B shown above the dashed line may be performed at the supplier of the pre-seal 92. The pre-seal 92 may then be shipped to the manufacturer of the power semiconductor module device 100. Thus, the surface on which the pre-seal 92 is formed may be a suitable working surface, and the resulting pre-seal 92 may be removed from the working surface for further processing.

[0031] Different adhesion promoters 84 are generally applicable to seals 8. Each adhesion promoter 84 can have different specific activation time-temperature budgets. In other words, heating a given adhesion promoter 84 at a given temperature for a given period of time will result in activation and consumption of the adhesion promoter 84. On the other hand, heating the adhesion promoter 84 for a shorter time at a higher temperature, or heating the adhesion promoter 84 for a longer time at a lower temperature, can also result in activation and consumption of the adhesion promoter 84. The activation temperature of many adhesion promoters 84 is between 130°C and 150°C, and the activation time is between 20 minutes and 120 minutes. That is, the temperature and time of performing the first step 301B depend on the specific activation time-temperature budget of the adhesion promoter 84 present in the material 90. However, in any case, the first step 301B is performed at a duration and temperature lower than the activation time-temperature budget of the adhesion promoter 84 used for the seal 8. For example, the matrix material 82 used for the silicone-based seal 8 is usually cured at a temperature significantly lower than the activation temperature of the adhesion promoter 84. Curing can even occur at relatively low temperatures (e.g., between 50° C. and 100° C.). According to one example, the curing step (step 301B) can be performed at 50° C. for 2 hours, at 60° C. for 1 hour, or at 80° C. for 30 minutes. However, as described above, the specific temperature and duration are generally dependent on the specific material and can vary.

[0032] The resulting pre-seal 92 can be transported and then can be arranged on the surface of the substrate 10, base plate or housing 7, and the housing 7 can be arranged on the substrate 10 or base plate with the pre-seal 92 arranged between them (step 302B). A second heating step can then be performed, during which the device, in particular the pre-seal 92, is heated to a temperature corresponding to or even higher than the activation temperature of the adhesion promoter 84 (step 303B). For example, heat can be applied to the side of the substrate 10 or base plate opposite to the side on which the pre-seal 92 is installed, to achieve activation of the adhesion promoter 84 and to securely attach the resulting seal 8 to both the housing 7 and the substrate 10 or base plate. That is, the resulting seal 8 securely attaches the housing 7 to the substrate 10 or base plate and additionally seals the interior of the housing 7.

[0033] Conventional non-adhesive seals such as gaskets and O-rings may also be used to seal the power module. However, such gaskets and O-rings require the use of external fasteners to provide compression forces to maintain the seal between the housing 7 and the substrate 10 or baseplate at all times before and after the casting compound 5 is cured. Likewise, the adhesive properties of the adhesive seal 8 according to embodiments of the present disclosure mean that no additional fasteners are required after the adhesion promoter is activated in order to secure the housing 7 to the substrate 10 or baseplate.

[0034] As mentioned above Figure 3B Steps 302B and 303B are described again by Figure 4 , 5 and 6. Figure 4 As schematically shown in FIG. 1 , the prefabricated pre-seal 92 may be arranged on the substrate 10. The housing 7 may be arranged on the substrate 10, wherein the pre-seal 92 is arranged between the substrate 10 and the housing 7, as shown in FIG. Figure 5 As shown. A heating step may then be performed, during which the adhesion promoter present in the pre-seal 92 (but not yet activated) is activated, thereby producing a seal 8 having both sealing properties and adhesive properties. That is, the resulting seal 8 has a strong adhesive force and firmly attaches the housing 7 to the substrate 10.

[0035] The pre-seal 92 may have any suitable form. According to one example, the pre-seal 92 forms a closed loop, e.g. Figure 7 Schematically shown in . For example, the shape and size of the pre-seal 92 can depend on the shape and size of the housing 7. The pre-seal 92 can have exactly the same shape and size as the housing 7, so that it can be arranged between the housing 7 and the substrate 10 or base plate to attach the housing 7 to the substrate 10 or base plate and seal the interior of the housing 7. Many substrates 10, substrates and housings 7 have a rectangular or square shape. However, other shapes are generally possible. The size of the pre-seal 92 can be slightly smaller than the size of the corresponding substrate 10 or base plate, so that when it is arranged on the substrate 10 or base plate, it extends along its edge. When the housing 7 is arranged on the pre-seal 92, the pre-seal 92 extends along the entire periphery of the housing 7 (i.e., along the lower surface of the side wall of the housing 7 facing the substrate 10 or base plate).

[0036] Alternatively, the pre-seal 92 may be first arranged on the surface of the housing 7. Then, the housing 7 with the pre-seal 92 arranged thereon may be arranged on the substrate 10. The heating step may be as described above with respect to Figure 6 This is done as described to form the final seal 8. If the substrate 10 is arranged on a base plate, the housing 7 can be arranged on the base plate, wherein the pre-seal 92 is arranged between the base plate and the housing 7.

[0037] The pre-seal 92 may be manufactured and shipped independently. However, according to another example, the pre-seal 92 may be formed on the housing 7 and the housing 7 may be shipped together with the pre-seal 92 formed thereon. Fig. 8A and 8B In a first step, a material 90 comprising a (silicone-based) matrix material and an adhesion promoter may be applied to the housing 7 (e.g., on the lower surface of the side wall of the housing 7 facing the substrate 10 or substrate when the housing 7 is arranged on the substrate 10 or substrate). Fig. 8A The heating step is performed to cure the matrix material without activating or completely consuming the adhesion promoter, thereby forming a pre-seal 92 ( Figure 8B ). The housing 7 with the pre-seal 92 formed thereon may then be arranged on the substrate 10 or base plate, and the final seal 8 may be formed by performing the second heating step as described above.

[0038] The lower surface of the side wall of the housing 7 may be a flat or substantially flat surface, for example Fig. 8A and 8B In this case, the pre-seal 92 needs to have certain adhesive properties in order to remain attached to the flat lower surface. However, the lower surface of the side wall can also be formed to have, for example, at least one recess or undercut 72. This Fig.9A . When the material 90 is applied to the lower surface of the housing 7, the material 90 fills the recess 72 formed in the side wall of the housing 7 and further forms a layer of the material 90 extending from the lower surface in the vertical direction y. Once the material 90 has cured and the pre-seal 92 is solid, it is firmly attached to the lower surface of the housing 7 without any adhesive properties, or only with limited adhesive properties. Fig.9A The specific form of the recess 72 shown in is only an example. The recess or undercut 72 can generally have any suitable form. In this case, the pre-seal 92 remains attached to the side wall of the housing without any adhesive properties.

[0039] If the lower surface of the housing 7 comprises a protrusion 74 and the material 90 is applied to the lower surface of the housing 7 such that it forms a layer of material 90 extending from the lower surface in the vertical direction y and completely surrounding the protrusion 74, such as Fig. 9B As shown in FIG. 7 , a similar effect can be achieved. The recess 72 or protrusion 74 can be a continuous recess 72 or protrusion 74 along the entire periphery of the housing 7. However, a plurality of recesses 72 and / or protrusions 74 can also be arranged along the periphery of the housing 7.

[0040] When forming the pre-seal 92 (e.g., independently or on the lower surface of the housing), the curing step at a temperature below the activation temperature of the adhesion promoter 84 can be performed, for example, in a vacuum chamber. This prevents air from penetrating into the material 90. Thus, the resulting pre-seal 92, as well as the final seal 8, is free of any unwanted bubbles or cavities. Furthermore, any fluid or moisture that may be present in the housing 7 can be prevented from penetrating into the material 90. Thus, the resulting pre-seal 92, as well as the final seal 8, is also free of any unwanted fluids.

[0041] According to another example, the housing 7 with the pre-attached pre-seal 92 can be formed, for example, in a two-shot (2K) injection molding process. The technology known as 2K injection molding allows injection molded parts containing two different materials to be formed in the same mold. A first material (e.g., a material forming the housing 7) can be filled into the mold by at least one injection. A second material (e.g., a material 90 forming the pre-seal 92) is filled into a mold containing the housing 7 using at least one second injection, wherein the mold has a defined position adjacent to the housing 7. In this way, the two materials can be connected to each other. It is important that during the second step of the 2K process, for example, during the formation of the pre-seal 92, the temperature is kept high enough and for a sufficient time to allow the second material 90 to cure, but at a sufficiently low temperature and / or for a sufficiently short time to prevent the adhesion promoter from being completely consumed during the curing process. For example, the 2K injection molding process can be a manual two-step process, or a fully automatic process in the form of rotational injection molding. The two materials may be filled into the mold in any suitable order, as long as the temperature can be kept low enough or for an amount of time insufficient to allow the adhesion promoter in the pre-seal material 90 to be completely consumed.

[0042] According to this example, the housing / pre-seal assembly 7, 92 can be placed on the substrate 10, wherein the pre-seal 92 is 2022P00784 CN

[0043] The pre-seal 92 is placed between the housing 7 and the substrate 10 and mounted to the substrate 10 by pressing the housing 7 toward the substrate. The pre-seal 92 is then heated to activate the adhesion promoter remaining in the pre-seal material 90, for example, by heating the other side of the substrate 10. Once the adhesion promoter is fully activated and the pre-seal 92 is fully bonded to the substrate 10, the pressure can be removed from the housing 7 and the heat can be removed.

[0044] A pre-seal 92 may also be formed generally on the substrate 10 or base plate, similar to what is described above with respect to the housing 7. The housing 7 may then be arranged on the substrate 10 or base plate, with the pre-seal 92 arranged between the housing 7 and the substrate 10 or base plate. The final seal 8 may be formed by performing the second heating step as described above.

Claims

1. A method, include: applying a first material (90) to the first surface, the first material (90) comprising a matrix material (82) and an adhesion promoter (84), wherein the matrix material (82) is configured to cure when heated to a defined temperature for a defined period of time, and wherein the adhesion promoter (84) is configured to be activated when heated to a temperature above the defined temperature and / or for a period of time longer than the defined period of time, and The first material (90) is heated to the defined temperature for the defined period of time such that the matrix material (82) cures and the adhesion promoter (84) remains inactive, thereby forming a pre-seal (92).

2. The method according to claim 1, further comprising: include: removing the pre-seal (92) from the first surface; The pre-seal (92) is arranged between a housing (7) and a substrate (10) or base plate of a power semiconductor module; as well as The pre-seal (92) is heated to a temperature equal to the defined temperature for a period of time longer than the defined time period, or is heated to a temperature greater than the defined temperature for a period of time equal to or longer than the defined time period, thereby activating the adhesion promoter (84) and forming a seal (8) between the shell (7) and the substrate (10) or baseplate, wherein the seal (8) forms an adhesive bond with the shell (7) and the substrate (10) or baseplate.

3. The method according to claim 1, in, The first surface is a surface of a housing (7), and the method further comprises: Arranging the housing (7) with the pre-seal (92) arranged thereon on a substrate (10) or base plate; and The pre-seal (92) is heated to a temperature equal to the defined temperature for a period of time longer than the defined time period, or is heated to a temperature greater than the defined temperature for a period of time equal to or longer than the defined time period, thereby activating the adhesion promoter (84) and forming a seal (8) between the shell (7) and the substrate (10) or baseplate, wherein the seal (8) forms an adhesive bond with the shell (7) and the substrate (10) or baseplate.

4. The method according to claim 3, further comprising: include: A material different from the first material (90) is filled into the mold to form the housing (7), wherein: Applying the first material (90) to the first surface includes subsequently filling the first material (90) into the mold.

5. The method according to claim 3 or 4, in, The surface of the housing (7) comprises at least one recess (72), and the first material (90) is applied to the surface such that the first material (90) fills the at least one recess (72) and forms a layer of material (90) extending from the surface in a vertical direction (y); and / or The surface of the shell (7) includes at least one protrusion (74), and the first material (90) is applied to the surface so that the first material (90) forms a layer of material (90) that extends from the surface in a vertical direction (y) and completely surrounds the at least one protrusion (74).

6. The method according to claim 1, in, The first surface is a surface of a substrate (10) or base plate, and the method further comprises: Arranging a housing (7) on the substrate (10) or base plate such that the pre-seal (92) is arranged between the housing (7) and the substrate (10) or base plate; and The pre-seal (92) is heated to a temperature equal to the defined temperature for a period of time longer than the defined time period, or is heated to a temperature greater than the defined temperature for a period of time equal to or longer than the defined time period, thereby activating the adhesion promoter (84) and forming a seal (8) between the shell (7) and the substrate (10) or baseplate, wherein the seal (8) forms an adhesive bond with the shell (7) and the substrate (10) or baseplate.

7. The method according to any one of claims 1 to 6, in, The matrix material (82) is a silicone-based matrix material.

8. The method according to any one of the preceding claims, in, The limiting temperature is between 50°C and 100°C; and Heating the pre-seal (92) to a temperature greater than the defined temperature includes heating the pre-seal (92) to a temperature between 130°C and 150°C.

9. The method according to any one of claims 2 to 8, in, The pre-seal (92) is arranged between the shell (7) and the substrate (10) or base plate, so that the pre-seal (92) extends along the entire periphery of the shell (7) and along the lower surface of the side wall of the shell (7) facing the substrate (10) or base plate.

10. The method according to any one of the preceding claims, in, The pre-seal (92) forms a closed loop.

11. A housing (7) for a power semiconductor module device (100), the housing include: side walls and covers; as well as A pre-seal (92) is disposed on a lower surface of the sidewall, wherein the pre-seal (92) includes a cured matrix material (82) and an uncured adhesion promoter (84).

12. The housing (7) according to claim 11, in, The lower surface of the housing (7) includes at least one recess (72), and the pre-seal (92) fills the at least one recess (72) and forms a layer extending from the lower surface in a vertical direction (y); and / or The surface of the housing (7) includes at least one protrusion (74), and the pre-seal (92) forms a layer extending from the lower surface in the vertical direction (y) and completely surrounding the at least one protrusion (74).