Displacement pre-treatment of laser surfaces and passivation devices formed using same material

Through the shift process, using an external energy source to quickly process the passivation layer of the laser diode, solving the problem of long processing time in the prior art, improving process efficiency and the stability of the laser diode, and achieving more efficient mass production.

CN119093151APending Publication Date: 2024-12-06II VI DELAWARE INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411209901.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2018-06-04
Filing Date
2019-06-04
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The passivation layer processing process of laser diodes in the prior art takes a long time and needs to be performed one by one, resulting in an increase in manufacturing process time and cost.

Method used

The passivation layer is quickly processed through external energy sources (such as lasers, flashes, electron beams) using a shift process, instead of the traditional low-current operation method, and a stable passivation layer and reflective coating are formed.

Benefits of technology

It significantly shortens the processing time, takes only a few seconds or minutes, improves process efficiency, reduces the possibility of mirror damage, and improves the stability and mass production capacity of laser diodes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119093151A_ABST
    Figure CN119093151A_ABST
Patent Text Reader

Abstract

The invention relates to displacement pre-treatment of laser surfaces and passivation devices formed using the same material. An edge emitting laser diode with a mirror surface includes a passivation coating that is treated using a shift process to treat an insulating material used to form the passivation layer. The material is irradiated with an external energy source (laser, flash, electron beam) at a given dose and for sufficient time to treat the entire thickness of the passivation layer. This displacement laser treatment is applied to a layer (possibly including a passivation layer and a coating) covering both end faces of a laser diode to stabilize the entire end face coating. Importantly, when the device is still in the strip-shaped state, the displacement process can be performed.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of an application with an application date of June 4, 2019, application number 201910479237.5, and invention name “Shift pretreatment of laser surface and passivation device formed using the same material”. Technical Field

[0002] The present invention relates to laser devices, and more particularly to edge emitting laser diodes having mirror surfaces processed by a shifting process. Background Art

[0003] High-power semiconductor laser diodes have become an important component of optical communication technology, especially because such laser diodes can be used for fiber pumping (amplification of optical signals) and other high-power applications. In most cases, laser diodes are usually required to have long life, reliable and stable output, high output power, high photoelectric efficiency, and good beam quality. One key to the long-term reliability of modern high-power laser diodes lies in the stability of the laser cut facets, which form the two opposing mirrors of the laser cavity.

[0004] The physical degradation of a laser facet is a complex reaction that can be driven by light, current, and heat, leading to power degradation and, in severe cases, catastrophic optical damage (COD) of the mirror itself. A process developed by IBM and known as "E2 passivation" has been used to address these issues and minimize the potential for COD. As described in IBM's U.S. Patent 5,063,173, entitled "Method for Passivating Mirrors of Semiconductor Laser Diodes" published by M. Gasser et al., the E2 process involves depositing a layer of silicon (or possibly germanium or antimony) as a coating on the surface of the exposed facet (mirror). The presence of the coating acts as a passivation layer to prevent the diffusion of impurities that could react with the mirror interface.

[0005] Today’s laser diodes operate at relatively high powers, and these prior art passivation layers, which are deposited, have been found to decompose, potentially causing damage to the mirror. Therefore, in order to obtain stable mirrors for infrared high-power laser diodes, it has become standard practice to “treat” the passivation layer. In today’s operations, treatment is a very time-consuming process that requires operating the laser diode at a reduced current level for a long period of time (e.g., tens to hundreds of hours) in order to form a crystalline structure within the deposited amorphous passivation layer, thereby forming a stable interface between the passivation layer and the mirror. In addition to the time required for this treatment process, it must also be performed on a device-by-device basis, further extending the time and expense of the manufacturing process. Summary of the invention

[0006] This disclosure provides the following:

[0007] 1). A method for passivating an end face of an edge emitting laser diode, comprising:

[0008] a) depositing one or more passivation layers on the surface of the exposed face of the edge emitting laser diode in a reaction chamber to form an end face coating of a predetermined thickness;

[0009] b) removing the edge emitting laser diode from the reaction chamber; and

[0010] c) irradiating the end face coating with an energy source sufficient to treat the end face coating through the predetermined thickness.

[0011] 2). The method as described in 1), wherein when performing step c), a laser source is used to irradiate the end face coating.

[0012] 3). The method as described in 1), wherein when performing step c), a flash lamp is used to irradiate the end face coating.

[0013] 4). The method as described in 1), wherein when performing step c), the end face coating is irradiated with an electron beam.

[0014] 5). The method as described in 1), wherein the method is applied before the laser diode is cut into individual devices.

[0015] 6) The method as described in 1), wherein the one or more passivation layers are composed of a material selected from silicon, germanium, antimony, and oxides, nitrides or combinations thereof.

[0016] 7). The method as described in 1), wherein pulses are used as energy sources.

[0017] 8). The method as described in 1), wherein a continuous wave is used as the energy source.

[0018] 9) The method as described in 1), wherein when performing step a) and before performing the irradiation of step c), a coating is deposited on each of the passivation layers.

[0019] 10) The method as described in 9), wherein the coating comprises a material selected from silicon, germanium, gallium arsenide, silicon oxide, silicon nitride, aluminum oxide, titanium oxide, aluminum nitride, tantalum oxide or a combination thereof.

[0020] 11). An edge-emitting laser diode, comprising

[0021] a semiconductor substrate having a waveguide structure formed thereon for generating light at an operating wavelength;

[0022] a pair of cut surfaces formed on opposite surfaces of the waveguide structure;

[0023] a passivation layer of a predetermined thickness formed to cover the pair of cut faces, wherein the passivation layer is sufficiently processed throughout the predetermined thickness; and

[0024] A reflective coating is formed directly on at least one of the passivation layers.

[0025] 12) An edge emitting laser diode as described in 11), wherein the reflective coating is fully processed together with the passivation layer.

[0026] 13). The edge emitting laser diode as described in 11), wherein the passivation layer comprises a laser irradiation material selected from silicon, germanium, antimony and their oxides, nitrides or combinations thereof.

[0027] 14). An edge-emitting laser diode as described in 11), wherein the reflective coating is formed of silicon, germanium, gallium arsenide, silicon oxide, silicon nitride, aluminum oxide, titanium oxide, aluminum nitride, tantalum oxide or a combination thereof.

[0028] The present invention addresses the need to reduce the time required for laser end face processing and relates to laser devices, and more particularly to edge emitting laser diodes having a mirror-like passivation coating that is processed using a "shifted" irradiation process instead of the traditional reduced current operation method.

[0029] According to the teachings and principles of the present invention, an external energy source is used to irradiate the material used as the end face passivation layer. Preferably, the passivation layer is insulating (or low conductivity). In particular, it can be formed using materials such as silicon, germanium or antimony. Compared with the extended time required for the "aging" treatment process in the prior art, the irradiation process itself only takes a few seconds or minutes.

[0030] The external energy source may include a laser, a flash lamp, an electron beam, or other suitable radiation source. The energy source may be operated in a continuous wave (CW) or pulsed mode, wherein the passivation layer is irradiated with an irradiation dose sufficient to treat the entire thickness of the passivation material layer. This shift processing method is applicable to the end face of the laser diode and is preferably performed when the device is in a bar shape (i.e., before cutting). However, it should be understood that the shift processing process of the present invention can also be applied to a single device after cutting, and the shift processing is performed on a single unmounted mold or a mounted mold (e.g., a device mounted on a card, a carrier, or a sub-substrate).

[0031] An exemplary method of shifting the end face of a passivated edge emitting laser diode according to one or more embodiments of the present invention includes the following steps: a) depositing one or more layers of passivation material on the surface of the exposed face of the edge emitting laser diode in a reaction chamber to form an end face coating of a predetermined thickness; b) removing the laser diode from the reaction chamber; and c) irradiating the end face coating with a beam from an energy source for a period of time sufficient for the beam to penetrate the predetermined thickness to treat the end face coating. In an alternative method, an external coating can be deposited on the passivation layer before performing the irradiation step (so as to fully treat and provide stability of the passivation layer and the coating combination).

[0032] Another embodiment of the present invention takes the form of an edge-emitting laser diode, which includes a semiconductor substrate on which a waveguide structure for generating light at an operating wavelength is formed; a pair of cut faces are formed on opposite surfaces of the waveguide structure; a passivation layer of a predetermined thickness is formed to cover the pair of cut faces, wherein the passivation layer is fully processed throughout the predetermined thickness, and a reflective coating is directly formed on at least one of the passivation layers.

[0033] Other and further embodiments and aspects of the present invention will become apparent during the following discussion and by reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 is a schematic plan view of an edge-emitting semiconductor laser diode;

[0035] Figure 2 An exemplary arrangement for performing a shifting process of a laser diode passivation layer according to one or more embodiments of the present invention is shown;

[0036] Figure 3 An alternative arrangement for performing the displacement treatment is shown, in which case adequate treatment or stabilization of the passivation layer and the cover coating is provided; and

[0037] Figure 4 A set of graphs are included showing the improvement in COD by using a translocation process according to the invention. DETAILED DESCRIPTION

[0038] As will be described in detail below, it is an object of the present invention to fully condition a passivation layer used as a coating on an exposed face of a laser diode using a shift process. The term "shift" as used herein is intended to emphasize the distinction between treatments formed in accordance with the principles of the present invention (i.e., treatments provided using an external energy source) and prior art "in situ" treatments which are accomplished by operating the laser diode device itself (typically at reduced current levels for long periods of time (e.g., extended times). For purposes of the present invention, the phrase "fully treated" refers primarily to treating a material comprising a passivation layer (e.g., silicon, germanium, antimony) throughout the entire thickness of that layer. For purposes of the present invention, "fully conditioned" may also be described as providing shift stabilization of the entire face covering, including the passivation layer and a standard coating overlying the passivation layer (and all interfaces therebetween, such as the passivation film-chip interface).

[0039] As will be discussed below, the shifting method of the present invention allows for the process to be performed on a strip of laser diodes (before being cut into individual devices), thereby significantly improving the efficiency of the process relative to the prior art process of processing each product one by one. In addition, depending on the size / area to be processed, the shifting process of the present invention only needs to be performed in a few seconds or minutes, rather than the time required by traditional equipment operation processing methods.

[0040] Now turning to the figure, Figure 1 An exemplary laser diode is schematically illustrated in plan view of FIG. The laser is formed in a semiconductor optoelectronic chip (or "bar") 10 having a front facet 12 and an opposing rear facet 14. Bar 10 includes a vertical structure (not shown in detail) that is typically composed of layers of AlGaAs, GaAs, and related III-V semiconductor materials epitaxially deposited on a GaAs substrate. However, it should be understood that other material combinations are possible within the scope of the present invention.

[0041] In the commercial production of these devices, a large number of such bars are formed simultaneously on a single gallium arsenide wafer (GaAs wafer), and the wafer is subsequently cut along natural cleavage planes to form a large number of individual bars 10 having front facets 12, rear facets 14 and vertically aligned side faces 16, 18, such as Figure 1 As shown. Semiconductor processing performed on the wafer also forms a waveguide structure 20 extending between and perpendicular to the front facets 12 and 14. Although in most cases the waveguide structure 20 is a ridge waveguide, other configurations are possible (e.g., a buried heterostructure waveguide, which is preferred in high power applications). In many high power applications, the waveguide structure 20 has a width substantially greater than the wavelength of the laser emission to form a wide area laser.

[0042] As part of the manufacturing process, the cut faces 12, 14 are subjected to a conventional E2 passivation process. That is, the strip 10 is loaded into a reaction chamber and a passivation material is deposited to a predetermined thickness to provide a coating on the mirror surfaces of the faces 12 and 14. The passivation material needs to be insulating (or of low conductivity), preferably comprising silicon, germanium or antimony, and may also comprise any oxide or nitride of these materials. Figure 1 In FIG. 1 , the deposited material is shown as passivation layers 22, 24. At this time, the shift processing method of the present invention can be used.

[0043] According to one or more embodiments of the present invention, the processing of the passivation layers 22, 24 is provided by an external system 30, such as Figure 2 The external system 30 includes an energy source 32 for generating a light beam 34, which is typically in the visible light range (e.g., 532 nm), but may also include UV or IR light beams. The energy source 32 may emit in a continuous wave (CW) or pulsed mode. Figure 2 In the specific embodiment shown in , the light beam 34 from the energy source 32 then passes through a focusing lens 36 and is scanned along a portion 38 of the passivation layer 22 overlying the active area of ​​the laser diode bar 10. The laser diode bar 10 can be mounted on a conventional submount fixture 40 and moved relative to the radiation from the energy source 32 so that the focused light beam is scanned across the lateral extent of the passivation layer 22. The energy source 32 can include any radiation source capable of radiating sufficient energy to uniformly treat the passivation material. Specifically, the energy source 32 can include a laser source, a flash lamp, an electron beam source, or any other system that produces a beam with sufficient energy to treat the entire thickness of the passivation layer 22.

[0044] like Figure 2 The spectrometer 42 shown can be used to monitor the progress of the treatment. For example, the scattered / redirected radiation of the passivation layer 22 can be analyzed in the spectrometer 42 using conventional methods to determine the point in time when complete treatment is achieved. Once the monitoring signal stabilizes, the external energy system can be deactivated.

[0045] It will be appreciated that the same shifted irradiation process can be used to fully treat the passivation layer 24 along the opposite end facets of the laser diode. In fact, the system can be configured to treat both end faces simultaneously. It has been found that such a shifted irradiation process provides treatment that achieves uniform treatment of the passivation material throughout the thickness of the passivation layer. This is a significant advantage over prior art methods of activating the device and performing the treatment at a reduced power level, which can sometimes result in partially non-uniform conditions of the passivation material.

[0046] As mentioned above, the treatment process of the present invention can also be performed after both the passivation layer and the reflective coating are applied to the laser facet. Figure 3An exemplary laser diode is shown, which has a structure similar to Figure 1 In this case, further processing is performed to deposit a first coating 26 on the passivation layer 22, and a second coating 28 on the passivation layer 24. In most cases, silicon nitride is used as the coatings 26, 28. Other suitable coating materials include, but are not limited to, silicon, germanium, gallium arsenide, silicon oxide, aluminum oxide, titanium oxide, aluminum nitride, and tantalum oxide.

[0047] and Figure 1 Similar to the embodiment of the present invention, the coating layer 26 and the underlying passivation layer 22 are irradiated using an energy source 30 to fully treat and stabilize the laser diode structure. Under irradiation, the structure of both the coating and the passivation layer will change in a manner that stabilizes the device and causes the desired high COD level to be produced. For example, when silicon nitride is used as the coating material, the silicon nitride remains amorphous (as opposed to crystalline) during irradiation, but the atomic configuration in the nitride material does change. At the same time, this irradiation causes the passivation layer to crystallize and form an interface between the passivation layer and the chip.

[0048] Therefore, according to the present invention Figure 3 In one embodiment, the phrase "substantially treat" refers to structurally changing the coating, crystallizing the passivation layer, and forming an interface between the laser chip and the passivation layer. Thus, the shift treatment process of the present invention can be considered to "stabilize" the laser diode itself through the changes made to these layers.

[0049] The COD current of the device formed according to the present invention was compared with the device using the conventional aging process. It should be noted that the "COD current" refers to the current at which the laser face suffers catastrophic optical damage (COD). Figure 4 The results of this comparison are shown. In particular, Figure 4 A set of Figures I is included, which shows the COD power as a function of current for devices subjected only to a conventional E2 process (without any post-processing). Figure II relates to devices created using the same prior art E2 process, followed by a conventional "in-situ" treatment process operating the device at a low current / power level. Clearly, the performance of these treated devices exceeds those of the first set, which have higher COD levels. Figure III relates to devices formed according to the present invention; that is, using a shift treatment process to provide complete treatment of the passivation layer. In particular, Figure 4 The results shown in Figure 3 The formed device wherein a shift treatment process is formed to stabilize the coating and passivation layers.

[0050] It can be seen that the COD level of the device formed according to the present invention is slightly higher than that of the prior art device. While this is obviously a goal of the present invention, the fact that the complete treatment can be performed on the entire laser bar (rather than at the individual device level) is also important and a significant improvement over the prior art. In addition, the shift treatment process of the present invention is several orders of magnitude more efficient than standard burn-in processes, being able to fully treat / stabilize the structure in seconds or minutes, as opposed to the tens to hundreds of hours required for low current level burn-in.

[0051] In summary, it has been found that the method of the present invention can uniformly and fully process the standard E2 passivation layer (and the cover coating, when present), eliminating the vertical and lateral processing non-uniformities found in the prior art. The method of the present invention has been demonstrated to maximize the current level (i.e., COD current / optical power) at which mirror damage occurs without burning. This eliminates the need for chip training through chip operation in the prior art. The distribution of COD current within a production batch is also reduced.

[0052] Furthermore, as described above, the laser facets can be fully processed in-place at the bar level (i.e., before chip separation). This allows a large number of bars to be fully processed in a short time, which is preferred for mass production situations. In fact, the method of the present invention also eliminates the need for the customer to perform any processing steps on the device, as was the case in some cases in the past.

[0053] It should be understood that the principles of the present invention may be implemented in other specific forms without departing from the spirit or essential features of the present invention. The embodiments described are to be considered in all respects as merely illustrative and non-restrictive. Therefore, the scope of the present invention is indicated by the appended claims rather than by the above description. All changes within the equivalent meaning and scope of the claims are included within their scope.

Claims

1. An edge emitting laser diode, comprising: a semiconductor substrate having a waveguide structure formed thereon for generating light at an operating wavelength; a pair of cut facets formed on opposite sides of the waveguide structure; a pair of irradiation passivation layers, each irradiation passivation layer comprising a uniform material selected from the group consisting of silicon, germanium, antimony, and oxides and nitrides thereof, each irradiation passivation layer formed to have a predetermined thickness and arranged to cover associated cut faces of a pair of cut faces, each irradiation passivation layer exhibiting a uniform structure over said predetermined thickness thereof, providing a pair of conditioned irradiation passivation layers; as well as A reflective coating is formed directly on at least one of the pair of radiation passivating layers.

2. The edge emitting laser diode of claim 1, wherein the reflective coating is a radiation reflective coating.

3. The edge emitting laser diode of claim 1, wherein the reflective coating is formed of a material selected from the group consisting of silicon, germanium, gallium arsenide, silicon oxide, silicon nitride, aluminum oxide, titanium oxide, aluminum nitride, and tantalum oxide.

4. The edge emitting laser diode of claim 1, wherein the waveguide structure comprises a ridge waveguide configuration.

5. The edge emitting laser diode of claim 1, wherein the waveguide structure comprises a buried heterostructure configuration.

6. A laser diode bar comprising a semiconductor substrate having a waveguide structure formed thereon, the waveguide structure extending a width sufficient to allow the laser diode bar to be subsequently cut into individual edge emitting laser diode devices; a pair of cut faces formed on opposite faces of the laser diode bar; a pair of irradiation passivation layers, each irradiation passivation layer comprising a uniform material selected from the group consisting of silicon, germanium, antimony, and oxides and nitrides thereof, each irradiation passivation layer formed to have a predetermined thickness and arranged to cover associated cut faces of a pair of cut faces, each irradiation passivation layer exhibiting a uniform structure over its predetermined thickness, providing a pair of conditioned irradiation passivation layers; as well as A reflective coating is formed directly on at least one of the pair of radiation passivating layers.

7. The laser diode bar of claim 6, wherein the reflective coating is a radiation reflective coating.

8. The laser diode bar of claim 6, wherein the reflective coating is formed of a material selected from the group consisting of silicon, germanium, gallium arsenide, silicon oxide, silicon nitride, aluminum oxide, titanium oxide, aluminum nitride, and tantalum oxide.

9. The laser diode bar of claim 6, wherein the waveguide structure comprises a ridge waveguide configuration.

10. The laser diode bar of claim 6, wherein the waveguide structure comprises a buried heterostructure configuration.

Citation Information

Patent Citations