Edge structure and filter
By using a superimposed layer structure of high dielectric constant material and high acoustic resistance material in the edge structure, the impedance curve bulging problem caused by edge structure in semiconductor devices is solved, and a high parallel impedance and smooth impedance curve are achieved.
Patent Information
- Application Number
- CN202411278246.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-12-06
AI Technical Summary
The existing edge structures cause the bulge of spurious impedance curves in semiconductor devices, which is mainly due to the high edge electric field strength, causing the sub-resonance to increase, making it difficult to achieve high parallel impedance Rp and smooth impedance curves at the same time.
The first raised layer of high dielectric constant material and the second raised layer superposition structure of high acoustic resistance material are adopted, the non-metallic material is located near the piezoelectric layer, and the metal material is located near the top electrode. The acoustic impedance is improved through this laminated structure. and suppress sub-resonance.
A high parallel impedance Rp is achieved while suppressing sub-resonance, resulting in a relatively smooth impedance curve, solving the impedance curve bulging problem caused by edge structure.
Smart Images

Figure CN119093891A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of bulk acoustic wave resonators, and in particular to an edge structure and a filter. Background Art
[0002] The edge structure refers to the structure corresponding to the edge part. In some semiconductor devices, the edge structure usually includes an edge protrusion structure. The edge protrusion structure OB usually selects a metal material that is the same or similar to the upper and lower electrodes. This structure can improve the parallel impedance Rp of the resonator. However, due to this structure, the electric field strength at the edge is higher, causing the secondary resonance outside the main resonance to be larger, and ultimately leading to a bulge in the impedance curve below the spurious. Summary of the invention
[0003] In view of this, the embodiments of the present application are directed to providing an edge structure and a filter to solve the problem of bulging of the impedance curve below the spurious.
[0004] The present application provides an edge structure, comprising: an edge protrusion structure is arranged between a bottom electrode and a top electrode of the edge structure;
[0005] The edge protrusion structure comprises a first protrusion layer and a second protrusion layer stacked in a direction away from the substrate;
[0006] Wherein, the material of the first protrusion layer is a material with a high dielectric constant; wherein, the material of the second protrusion layer is a material with a high acoustic resistance.
[0007] In some embodiments, the material of the first protrusion layer is a non-metallic material.
[0008] In some embodiments, the material of the second protrusion layer is a metal material.
[0009] In some embodiments, the edge structure includes a substrate, a bottom electrode, a piezoelectric layer, a top electrode, and a top electrode surface protection layer arranged along a stack;
[0010] The edge structure also includes an acoustic mirror.
[0011] In some embodiments, an edge recess structure is disposed on the top electrode surface protection layer.
[0012] In some embodiments, the bottom electrode comprises: a first bottom electrode layer and a second bottom electrode layer stacked;
[0013] The acoustic mirror is disposed between the first bottom electrode layer and the second bottom electrode layer.
[0014] In some embodiments, the method further includes: a top electrode thickening layer disposed on a side of the top electrode layer away from the substrate.
[0015] In some embodiments, the method further includes: a top electrode thickening layer surface protection layer disposed on a side of the top electrode thickening layer away from the substrate.
[0016] In some embodiments, the first protrusion layer and the second protrusion layer of the edge protrusion structure are stacked in a stepped structure.
[0017] In some embodiments, the first convex layer and the upper surface structure wrap the second convex layer, or the second convex layer and the lower surface structure wrap the first convex layer;
[0018] Wherein, the upper surface structure is: a structure in the edge structure that is in close contact with the edge protrusion structure and is farther away from the substrate than the edge protrusion structure;
[0019] The lower surface structure is: a structure in the edge structure that is in close contact with the edge protrusion structure and is closer to the substrate than the edge protrusion structure.
[0020] In some embodiments, the edge protrusion structure is disposed between the piezoelectric layer and the top electrode.
[0021] In some embodiments, the edge protrusion structure is disposed between the bottom electrode and the piezoelectric layer.
[0022] In some embodiments, the piezoelectric layer includes a first piezoelectric layer and a second piezoelectric layer that are stacked.
[0023] In some embodiments, a sound wave reflection structure is disposed in a region corresponding to an edge between the first piezoelectric layer and the second piezoelectric layer.
[0024] In some embodiments, the sound wave reflecting structure is a cavity.
[0025] In some embodiments, the sound wave reflecting structural material is a non-metallic material.
[0026] In some embodiments, the first raised layer
[0027] The first piezoelectric layer is disposed between the first piezoelectric layer and the second piezoelectric layer; and the second protrusion layer is disposed between the piezoelectric layer and the top electrode.
[0028] In some embodiments, the ratio of the thickness of the first protrusion layer to the thickness of the second protrusion layer is 0.01-100.
[0029] In some embodiments, the ratio of the thickness of the first protrusion layer to the thickness of the second protrusion layer is 0.5-20.
[0030] An edge structure provided by the present application includes: an edge protrusion structure is arranged between the bottom electrode and the top electrode of the edge structure; the edge protrusion structure includes a first protrusion layer and a second protrusion layer stacked in a direction away from the substrate; wherein the material of the first protrusion layer is a material with a high dielectric constant; wherein the material of the second protrusion layer is a material with a high acoustic impedance. In this arrangement, the first protrusion layer of the material with a high dielectric constant is located on the side close to the bottom electrode, and the second protrusion layer of the material with a high acoustic impedance is located on the side close to the top electrode. Due to the presence of the second protrusion layer of the material with a high acoustic impedance, a higher acoustic impedance can be achieved and Rp can be improved. At the same time, due to the presence of the first protrusion layer of the material with a high dielectric constant, the secondary resonance is suppressed, making the curve below the spurious smoother. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] By describing the embodiments of the present application in more detail in conjunction with the accompanying drawings, the above and other purposes, features and advantages of the present application will become more apparent. The accompanying drawings are used to provide a further understanding of the embodiments of the present application and constitute a part of the specification. Together with the embodiments of the present application, they are used to explain the present application and do not constitute a limitation of the present application. In the accompanying drawings, the same reference numerals generally represent the same components or steps.
[0032] Figure 1 It is a structural diagram of a traditional edge structure.
[0033] Figure 2 It is the impedance curve of the traditional edge structure.
[0034] Figure 3 is the impedance curve of another traditional edge structure.
[0035] Figure 4 It is a structural schematic diagram of an edge structure provided by an embodiment of the present application.
[0036] Figures 5 to 11 It is a schematic diagram of preparing an edge structure provided in one embodiment of the present application.
[0037] Fig.12 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0038] Fig.13 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0039] Fig.14 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0040] Fig.15 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0041] Fig.16 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0042] Fig.17 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0043] Fig.18 It is a structural schematic diagram of an edge structure provided in another embodiment of the present application.
[0044] Reference numerals:
[0045] 10. Substrate; 20. Acoustic mirror; 30. Bottom electrode layer; 31. First bottom electrode layer; 32. Second bottom electrode layer; 40. Piezoelectric layer; 41. First piezoelectric layer; 42. Second piezoelectric layer; 50. Top electrode; 51. Top electrode thickening layer; 60. Top electrode surface protection layer; 61. Top electrode thickening layer surface protection layer; 70. Edge protrusion structure; 71. First protrusion layer; 72. Second protrusion layer; 80. Release hole; 90. Sound wave reflection structure; 91. Edge recess structure; 100. Photoresist. DETAILED DESCRIPTION
[0046] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0047] Application Overview
[0048] The edge structure refers to the structure corresponding to the edge part. In some semiconductor devices, the edge structure usually includes an edge convex structure. The edge convex structure OB is usually made of the same or similar metal material as the upper and lower electrodes, such as Figure 1 As shown, the edge structure is divided into three areas: the first effective area 1, also called the main resonance area, the second functional area 2 and the third functional area 3 are formed outside the first effective area 1. This structure can improve the parallel impedance Rp of the resonator, such as Figure 2 As shown, A1 corresponds to Rp. However, due to this structure, the electric field strength at the edge is higher, causing the secondary resonance outside the main resonance to be larger, and ultimately leading to a bulge in the impedance curve below the spurious, such as Figure 2 The B1 position in the middle corresponds to the bulge below the spurious. The reason for this phenomenon is that the introduction of the metal OB structure is equivalent to introducing a parasitic resonator with thickened electrodes into the original resonator. The internal electric field strength of this parasitic resonator is high. In this case, the vibration of the particles is intensified, which eventually leads to the formation of a bulge below the spurious.
[0049] If the edge protrusion structure is simply changed to non-metallic material, the bulge of the curve can be suppressed, such as Figure 3 The disadvantage is that Rp is reduced, corresponding to point A2, the value is Figure 2 The Rp point is half as low. This is because the edge protrusion structure composed of non-metallic materials (i.e., the second functional area 2 and the third functional area 3) reduces the electric field here and suppresses the sub-resonance, but the acoustic impedance of non-metallic materials is low and it is impossible to achieve a high acoustic impedance mismatch at the edge, which makes it easy for sound waves to leak out of the resonator and reduce Rp. Therefore, it is difficult for a single edge protrusion structure to achieve a high Rp while also ensuring that the impedance curve below the spurious does not have a bulge.
[0050] The present invention changes the traditional OB structure into a layer of non-metallic material with low acoustic impedance and a layer of metal material with high acoustic impedance. In this case, the non-metallic material should be located on the side close to the piezoelectric layer, and the metal material should be located on the side close to the electrode (such as Figure 4 As shown in the embodiment, 71 should be non-metallic and 72 should be metal). Thus, due to the presence of metal material with high acoustic impedance, a higher acoustic impedance mismatch can be achieved, thereby improving Rp. At the same time, due to the presence of non-metallic material, the electric field strength of the second and third functional areas outside the main resonance area can be reduced, and the secondary resonance can be suppressed, so that the curve below the spurious is smoother.
[0051] After introducing the basic principles of the present application, various non-limiting embodiments of the present application will be described in detail with reference to the accompanying drawings.
[0052] Exemplary edge structures
[0053] Reference Figure 4 The present application provides an edge structure, including: an edge protrusion structure 70 is arranged between the bottom electrode and the top electrode 50 of the edge structure; the edge protrusion structure 70 includes a first protrusion layer 71 and a second protrusion layer 72 stacked in a direction away from the substrate 10; wherein the material of the first protrusion layer 71 is a material with a high dielectric constant; wherein the material of the second protrusion layer 72 is a material with a high acoustic impedance.
[0054] Specifically, the material of the first protrusion layer 71 may be a non-metal material, and the material of the second protrusion layer 72 may be a metal material.
[0055] Thus, the non-metallic material should be located close to the bottom electrode ( Figure 4On the side close to the piezoelectric layer 40), the metal material should be located on the side close to the top electrode 50. In this way, due to the presence of the metal material with high acoustic impedance, a higher acoustic impedance mismatch can be achieved, thereby improving Rp. At the same time, due to the presence of the non-metallic material, the electric field strength of the second and third functional areas outside the main resonance area can be reduced, the secondary resonance can be suppressed, and the curve below the spurious can be smoother.
[0056] In some embodiments, the edge structure includes a substrate 10 , a bottom electrode, a piezoelectric layer 40 , a top electrode 50 , and a top electrode surface protection layer 60 arranged along a stack; the edge structure also includes an acoustic mirror 20 .
[0057] Furthermore, an edge recess structure is provided on the top electrode surface protection layer 60 .
[0058] Reference Figures 5 to 11 , the processing steps corresponding to the solution provided in this application are as follows:
[0059] First refer to Figure 5 , the FBAR acoustic mirror 20 filling structure is prepared on the preset substrate 10 as described above.
[0060] Specifically, the acoustic mirror 20 filling structure of the FBAR (film bulk acoustic resonator) is a key part in the resonator design. The acoustic mirror 20 is usually used to reflect sound waves to enhance the resonant characteristics of the resonator. The following is relevant information about the acoustic mirror 20 filling structure:
[0061] Acoustic mirror 20: It can be a cavity, or a Bragg reflection layer or other equivalent forms. The main function of the acoustic mirror 20 is to reflect sound waves to enhance the resonant frequency of the resonator.
[0062] Substrate 10: is the basis for constructing the acoustic mirror 20. Optional materials include single crystal silicon, gallium nitride, gallium arsenide, sapphire, quartz, silicon carbide, diamond, etc.
[0063] The design of the acoustic mirror 20 needs to consider its ability to reflect sound waves, which is usually achieved by selecting appropriate materials and structural design. In the actual preparation process, it is necessary to accurately control parameters such as material selection, layer thickness, etching depth, etc. to ensure that the filling structure of the acoustic mirror 20 can meet the expected performance requirements.
[0064] Reference Figure 6 , preparing a bottom electrode and depositing a piezoelectric layer 40;
[0065] The bottom electrode is usually made of metal materials, such as molybdenum, gold or other conductive materials. A piezoelectric layer 40 is deposited on the bottom electrode. The piezoelectric layer 40 is the core part of the FBAR and can convert electrical signals into mechanical vibrations.
[0066] Reference Figure 7 , prepare an edge protrusion structure 70 formed by stacking a first protrusion layer 71 made of a non-metallic material with low acoustic impedance and a second protrusion layer 72 made of a metal material with high acoustic impedance.
[0067] Specifically, a first protruding layer 71 is prepared, which is composed of a non-metallic material with low acoustic impedance, such as SiO2, PSG, AlN or SiN. Then, a second protruding layer 72 is prepared, which is composed of a metal material with high acoustic impedance, such as molybdenum, gold or other high acoustic impedance metals. The first protruding layer 71 and the second protruding layer 72 are superimposed to form an edge protruding structure 70, which helps to increase the parallel impedance Rp of the resonator and reduce sub-resonance.
[0068] Reference Figure 8 , prepare the top electrode 50 and the protective layer, and etch out the top electrode 50 structure.
[0069] That is, a top electrode 50 is prepared on the edge protrusion structure 70. The top electrode 50 is usually made of a metal material, which may be the same as or different from the bottom electrode material. A protective layer is prepared to protect the top electrode 50 from being affected by subsequent process steps.
[0070] Reference Fig. 9 , and a release hole 80 is etched.
[0071] Specifically, release holes 80 are etched in the acoustic mirror 20 structure, and these holes will be used to release the sacrificial material in the acoustic mirror 20 in subsequent steps.
[0072] Reference Fig.10 , making a photolithography pattern, except for the release hole 80, all are covered by the photoresist 100. The sacrificial material of the acoustic mirror 20 is released.
[0073] In practical applications, photolithography patterns are made, which include coating photoresist 100 on different layers of the FBAR, and performing exposure and development to form the desired pattern. Except for the release hole 80, all other parts are covered by the photoresist 100, which helps to protect the material in the subsequent etching step. The sacrificial material in the acoustic mirror 20 is removed by etching or other appropriate methods, which usually involves using chemical or physical methods to remove the material, thereby forming a cavity or a reflective layer of the acoustic mirror 20.
[0074] Reference Fig.11 , remove the photoresist 100 to obtain the final resonator.
[0075] The specific method of removing all the remaining photoresist 100 can be achieved by chemical cleaning or plasma ashing. After completing these steps, the final resonator is obtained, which has an improved edge protrusion structure 70 and optimized acoustic performance.
[0076] In some embodiments, the top electrode surface protection layer 60 is provided with an edge recess structure 91. Fig.12 The edge recess structure 91 may be disposed between the first effective region and the second functional region, and between the second functional region and the third functional region.
[0077] The edge recessed structure can be used to reduce the parasitic capacitance of the resonator and increase the resonant frequency, and can also be used to adjust the electrical and mechanical properties of the resonator, for example, by changing the vibration mode of the resonator. The edge recessed structure is arranged on the top electrode surface protection layer 60, and the groove can be formed by performing specific photolithography and etching techniques on the dielectric layer. The etching process needs to be precisely controlled to ensure that the size and shape of the recessed structure meet the design requirements. The edge recessed structure can reduce the parasitic effects of the resonator and improve the quality factor (Q value) of the resonator. They can also help suppress or reduce the subharmonic response of the resonator, thereby improving the passband performance of the filter.
[0078] Reference Fig.13 In order to reduce Rs (series impedance) and parasitic impedance, the bottom electrode thickness is increased, and the cavity is wrapped by the lower electrode: that is, the bottom electrode includes: a first bottom electrode layer 31 and a second bottom electrode layer 32 stacked together; the acoustic mirror 20 is arranged between the first bottom electrode layer 31 and the second bottom electrode layer 32.
[0079] Reference Fig.14 In order to reduce Rs (series impedance) and parasitic impedance, the thickness of the top electrode 50 is increased; specifically, it also includes: a top electrode thickening layer 51 disposed on a side of the top electrode 50 layer away from the substrate 10. The top electrode thickening layer 51 is in direct contact with the top electrode 50.
[0080] The top electrode thickening layer 51 is only arranged outside the first effective area to form a third functional area; correspondingly, there is no need to arrange the top electrode surface protection layer 60 in the area where the top electrode thickening layer 51 is arranged. Correspondingly, in order to protect the top electrode thickening layer 51, a top electrode thickening layer surface protection layer 61 needs to be arranged on the side of the top electrode thickening layer 51 away from the substrate 10.
[0081] The top electrode thickening layer 51 can increase the mass and rigidity of the top electrode 50, thereby affecting the vibration mode and frequency characteristics of the resonator. It can also be used to adjust the electrical properties of the resonator, reduce Rs (series impedance) and parasitic impedance, and the material of the top electrode thickening layer 51 can be molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite or alloy of these metals. These materials have good electrical conductivity and mechanical strength. The preparation of the top electrode thickening layer 51 usually involves an additional deposition process on the top electrode 50 layer to increase its thickness. The deposition technology may include physical vapor deposition (PVD), chemical vapor deposition (CVD) or other suitable thin film deposition technology.
[0082] Reference Fig.15 , the edge protrusion structure 70 formed by a layer of non-metallic material with lower acoustic impedance and a layer of metal material with higher acoustic impedance can be stepped, not necessarily flush: in some embodiments, the edge protrusion structure 70 is a trapezoidal structure in a cross section perpendicular to the substrate 10. The lower bottom of the edge protrusion structure 70 is close to the substrate 10. In the design of FBAR (film bulk acoustic resonator), the morphology of the edge protrusion structure 70 has an important influence on its performance. Specifically, the first protrusion layer 71 and the upper surface structure wrap the second protrusion layer 72, or the second protrusion layer 72 and the lower surface structure wrap the first protrusion layer 71; wherein the upper surface structure is: in the edge structure, the structure that is in close contact with the edge protrusion structure and is farther away from the substrate than the edge protrusion structure; the lower surface structure is: in the edge structure, the structure that is in close contact with the edge protrusion structure and is closer to the substrate than the edge protrusion structure. The edge protrusion structure 70 can be designed to be stepped, which provides more flexibility to adjust the acoustic and electrical characteristics of the resonator. By adjusting the size and shape of the stepped or trapezoidal edge protrusion structure 70, the vibration mode of the resonator can be optimized, parasitic effects can be reduced, and the quality factor (Q value) of the resonator can be improved. In some embodiments, the edge protrusion structure 70 may be designed to have different number of steps or trapezoidal sizes to adapt to different performance requirements and application scenarios.
[0083] Reference Fig.16 , the edge protrusion structure 70 is arranged between the bottom electrode and the piezoelectric layer 40. Specifically, at this time, the edge protrusion structure 70 is located between the piezoelectric layer 40 and the bottom electrode, at this time the metal material is in a layer close to the bottom electrode, and the non-metal material is in a layer close to the piezoelectric layer 40: In some embodiments, the edge protrusion structure 70 is arranged between the piezoelectric layer 40 and the top electrode 50.
[0084] Reference Fig.17In order to further improve Rp, an edge structure is added between the piezoelectric layers 40: the piezoelectric layer 40 includes a first piezoelectric layer 41 and a second piezoelectric layer 42 stacked. An acoustic wave reflection structure 90 is provided in the area corresponding to the edge between the first piezoelectric layer 41 and the second piezoelectric layer 42. The acoustic wave reflection structure 90 is a cavity. Furthermore, the acoustic impedance of the material of the acoustic wave reflection structure 90 is less than or equal to the acoustic impedance of air. In some embodiments, the acoustic wave reflection structure 90 may correspond to the first effective area and the third functional area.
[0085] The piezoelectric layer 40 is composed of at least two layers, namely the first piezoelectric layer 41 and the second piezoelectric layer 42, which are the core parts of the FBAR and are responsible for converting electrical energy into mechanical vibrations. Between the first piezoelectric layer 41 and the second piezoelectric layer 42, corresponding to the edge area, an acoustic wave reflection structure 90 is provided, which helps to enhance the reflection and propagation of acoustic waves inside the resonator. The acoustic wave reflection structure 90 is designed as a cavity, and this cavity structure can effectively reflect acoustic waves, thereby enhancing the resonant characteristics of the resonator. The material of the acoustic wave reflection structure 90 should have a low acoustic impedance, less than or equal to the acoustic impedance of air, for example, it can be a non-metallic material, which helps the propagation and reflection of acoustic waves in the structure. Materials with low acoustic impedance can reduce the energy loss of acoustic waves when entering and leaving the reflection structure, thereby improving the Q value and Rp of the resonator.
[0086] In some embodiments, the first protruding layer 71 is disposed between the first piezoelectric layer 41 and the second piezoelectric layer 42; the second protruding layer 72 is disposed between the piezoelectric layer 40 and the top electrode 50. The first protruding layer 71 is composed of a non-metallic material with low acoustic impedance and is disposed between the first piezoelectric layer 41 and the second piezoelectric layer 42. This configuration helps to form a region with low acoustic impedance between the two piezoelectric layers 40, which can help the propagation of sound waves between the piezoelectric layers 40 while reducing the reflection of sound waves between these layers. The second protruding layer 72 is composed of a metal material with high acoustic impedance and is disposed between the piezoelectric layer 40 (including the first and second piezoelectric layers 42) and the top electrode 50. This configuration helps to form a region with high acoustic impedance between the piezoelectric layer 40 and the top electrode 50, which can enhance the reflection of sound waves inside the resonator, thereby improving the resonant performance of the resonator.
[0087] In some embodiments, the ratio of the thickness between the first raised layer 71 and the second raised layer 72 is 0.01 to 100. Furthermore, the ratio of the thickness between the first raised layer 71 and the second raised layer 72 is 0.5 to 20. In the design, the thickness ratio of the first raised layer 71 and the second raised layer 72 of the edge raised structure 70 is a key parameter, which has a significant impact on the performance of the resonator. The thickness ratio of the first raised layer 71 and the second raised layer 72 affects the propagation and reflection of sound waves inside the resonator, and thus affects the resonant frequency, quality factor (Q value) and parallel impedance (Rp) of the resonator. In some embodiments, the thickness of the first raised layer 71 and the second raised layer 72 can be adjusted based on actual needs.
[0088] Example Filters
[0089] The present application also provides a filter, comprising the edge structure provided by any of the above embodiments.
[0090] Specifically, the materials of each component in the filter are described as follows:
[0091] Substrate 10, optional materials include single crystal silicon, gallium nitride, gallium arsenide, sapphire, quartz, silicon carbide, diamond, etc.
[0092] The acoustic mirror 20 may be a cavity, or may be a Bragg reflection layer or other equivalent forms.
[0093] The bottom electrode layer 30 may be made of molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof.
[0094] The first bottom electrode layer 31 may be made of molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof.
[0095] The second bottom electrode layer 32 may be made of molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof.
[0096] The piezoelectric layer 40 may be a single crystal piezoelectric material, such as single crystal aluminum nitride, single crystal gallium nitride, single crystal lithium niobate, single crystal lead zirconate titanate (PZT), single crystal potassium niobate, single crystal quartz film, or single crystal lithium tantalate, etc. It may also be a polycrystalline piezoelectric material (corresponding to a single crystal, a non-single crystal material), such as polycrystalline aluminum nitride, zinc oxide, PZT, etc., or may be a rare earth element doped with a certain atomic ratio of the above materials. The material, for example, can be doped aluminum nitride, which contains at least one rare earth element, such as scandium (Sc), yttrium (Y), magnesium (Mg), titanium (Ti), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), etc.
[0097] The first piezoelectric layer 41 may be a single crystal piezoelectric material, such as single crystal aluminum nitride, single crystal gallium nitride, single crystal lithium niobate, single crystal lead zirconate titanate (PZT), single crystal potassium niobate, single crystal quartz film, or single crystal lithium tantalate, etc. It may also be a polycrystalline piezoelectric material (corresponding to a single crystal, a non-single crystal material), such as polycrystalline aluminum nitride, zinc oxide, PZT, etc., or may be a rare earth element doped with a certain atomic ratio of the above materials. The impurity material may be, for example, doped aluminum nitride, which contains at least one rare earth element, such as scandium (Sc), yttrium (Y), magnesium (Mg), titanium (Ti), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), etc.
[0098] The second piezoelectric layer 42 may be a single crystal piezoelectric material, such as single crystal aluminum nitride, single crystal gallium nitride, single crystal lithium niobate, single crystal lead zirconate titanate (PZT), single crystal potassium niobate, single crystal quartz film, or single crystal lithium tantalate, etc. It may also be a polycrystalline piezoelectric material (corresponding to a single crystal, a non-single crystal material), such as polycrystalline aluminum nitride, zinc oxide, PZT, etc., or may be a rare earth element doped with a certain atomic ratio of the above materials. The impurity material may be, for example, doped aluminum nitride, which contains at least one rare earth element, such as scandium (Sc), yttrium (Y), magnesium (Mg), titanium (Ti), lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), etc.
[0099] The material of the top electrode 50 can be selected from molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof. The materials of the top electrode 50 and the bottom electrode are generally the same, but can also be different.
[0100] The top electrode thickening layer 51 may be made of molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof.
[0101] The top electrode surface protection layer 60 may be made of AlN, SiN, SiO2, or Al2O3.
[0102] The top electrode thickening layer surface protection layer 61 can be made of AlN, SiN, SiO2, or Al2O3.
[0103] The edge protrusion structure 70 includes a layer of non-metal material with low acoustic impedance and a layer of metal material with high acoustic impedance.
[0104] The first protruding layer 71 is made of non-metallic material with low acoustic impedance, including SiO2, PSG, AlN, SiN and the like.
[0105] The second protruding layer 72 is made of a metal material with high acoustic impedance, including molybdenum, ruthenium, gold, aluminum, magnesium, tungsten, copper, titanium, iridium, osmium, chromium or a composite of the above metals or an alloy thereof.
[0106] The sound wave reflecting structure 90 is made of air or a functional material for reflecting sound waves, wherein the acoustic impedance of the functional material is less than or equal to the acoustic impedance of air.
[0107] The above description has been given for the purpose of illustration and description. In addition, this description is not intended to limit the embodiments of the present application to the forms disclosed herein. Although multiple example aspects and embodiments have been discussed above, those skilled in the art will recognize certain variations, modifications, changes, additions and sub-combinations thereof.
Claims
1. An edge structure, characterized in that: include: An edge protrusion structure is provided between the bottom electrode and the top electrode of the edge structure; The edge protrusion structure comprises a first protrusion layer and a second protrusion layer stacked in a direction away from the substrate; Wherein, the material of the first protrusion layer is a material with a high dielectric constant; wherein, the material of the second protrusion layer is a material with a high acoustic resistance.
2. The edge structure according to claim 1, characterized in that: The material of the first protrusion layer is a non-metallic material.
3. The edge structure according to claim 1, characterized in that: The second protrusion layer is made of metal material.
4. The edge structure according to claim 1, characterized in that: The edge structure includes a substrate, a bottom electrode, a piezoelectric layer, a top electrode, and a top electrode surface protection layer arranged along the stack; The edge structure also includes an acoustic mirror.
5. The edge structure according to claim 4, characterized in that: An edge recessed structure is arranged on the top electrode surface protection layer.
6. The edge structure according to claim 4, characterized in that: The bottom electrode comprises: a first bottom electrode layer and a second bottom electrode layer which are stacked; The acoustic mirror is disposed between the first bottom electrode layer and the second bottom electrode layer.
7. The edge structure according to claim 4, characterized in that: Also includes: A top electrode thickening layer is arranged on a side of the top electrode layer away from the substrate.
8. The edge structure according to claim 4, characterized in that: Also includes: A surface protection layer of the top electrode thickening layer is arranged on a side of the top electrode thickening layer away from the substrate.
9. The edge structure according to claim 4, characterized in that: The first protrusion layer and the second protrusion layer of the edge protrusion structure are stacked in a stepped structure.
10. The edge structure according to claim 9, characterized in that: The first convex layer and the upper surface structure wrap the second convex layer, or the second convex layer and the lower surface structure wrap the first convex layer; Wherein, the upper surface structure is: a structure in the edge structure that is in close contact with the edge protrusion structure and is farther away from the substrate than the edge protrusion structure; The lower surface structure is: a structure in the edge structure that is in close contact with the edge protrusion structure and is closer to the substrate than the edge protrusion structure.
11. The edge structure according to claim 4, characterized in that: The edge protrusion structure is arranged between the piezoelectric layer and the top electrode.
12. The edge structure according to claim 4, characterized in that: The edge protrusion structure is arranged between the bottom electrode and the piezoelectric layer.
13. The edge structure according to claim 4, characterized in that: The piezoelectric layer includes a first piezoelectric layer and a second piezoelectric layer which are stacked.
14. The edge structure according to claim 13, characterized in that: An acoustic wave reflection structure is arranged in a region corresponding to the edge between the first piezoelectric layer and the second piezoelectric layer.
15. The edge structure according to claim 14, characterized in that: The sound wave reflecting structure is a cavity.
16. The edge structure according to claim 14, characterized in that: The sound wave reflecting structural material is a non-metallic material.
17. The edge structure according to claim 14, characterized in that: The first protrusion layer is arranged between the first piezoelectric layer and the second piezoelectric layer; and the second protrusion layer is arranged between the piezoelectric layer and the top electrode.
18. The edge structure according to claim 14, characterized in that: The ratio of the thickness of the first protrusion layer to the thickness of the second protrusion layer is 0.01-100.
19. The edge structure according to claim 14, characterized in that: The ratio of the thickness of the first protrusion layer to the thickness of the second protrusion layer is 0.5-20.
20. A filter, characterized in that: Comprising the edge structure as claimed in claims 1 to 19.
Citation Information
Cited By
Edge structure and filter
WO2026056374A1