Additively produced magnetic sheet, method for producing magnetic sheet, laminated core and electric machine
Through the multi-layer structural design and the symmetrical arrangement of material components, the problems of insufficient mechanical strength and high inherent stress during high-speed operation of the magnetic sheet are solved, and higher mechanical stability and performance improvement are achieved.
Patent Information
- Application Number
- CN202380036117.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-27
- Filing Date
- 2023-04-19
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing magnetic sheets are insufficient in mechanical strength and have high inherent stresses when operating at high speed, resulting in problems such as warping and cracks. Especially when the thermal expansion coefficients of different material components do not match, the mechanical stresses seriously damage performance.
A magnetic sheet design adopts a multi-layer structure, in which each layer contains different material components, the first material component is radially inner and the second material component is radially outer and the material share varies in the layer order and exists in the transition area. The dispersed sub-regions are used to adapt to the difference in thermal expansion coefficients, and strength and stability are formed by sintering connections.
The mechanical strength and stability of the magnetic sheet are improved, the stress caused by the difference in thermal expansion coefficient is reduced, the bending of the magnetic sheet is reduced, and the overall performance of the magnetic sheet is enhanced.
Smart Images

Figure CN119095683A_ABST
Abstract
Description
[0001] The invention relates to an additively manufactured magnet sheet according to claim 1 , a method for producing a magnet sheet according to claim 11 , a laminated core according to claim 14 and an electric machine according to claim 15 .
[0002] Screen or silk screen printing is a new process for manufacturing magnetic sheets for electric motors. Here, a printing paste is printed onto a substrate using a silk screen, and the opening areas in the silk screen can also use the screen. This is called screen printing or screen printing, where silk screen printing is a superordinate term for screen printing. In addition to solvents and / or binders, the printing paste also contains metal powder, which has a functional influence on the subsequent components. The green body is produced by screen printing technology. After further heat treatment, the green body is usually first deburred and then sintered at a higher temperature, where the metal powder particles sinter together to form a structured sheet, i.e. the magnetic sheet.
[0003] In order to improve the mechanical strength of such magnetic sheets, especially when the rotor of the motor is running at high speed, the manufacturability of two-component magnetic sheets is becoming increasingly important. For this purpose, an embodiment is described in document EP 3723249 A1. The basic problem of producing such two-component magnetic sheets using screen printing technology is that different materials, if they have good magnetic properties on the one hand and high strength on the other hand, usually have different thermal expansion coefficients. Thus, for example, the expansion coefficient of the high-strength steel used for the mechanical strength of the magnetic sheet is 16x10 -6 K -1 The thermal expansion coefficient of another soft magnetic material in the temperature range of 0 to 100°C is 10-12x10 -6 K -1 When these different material components or material pairs are sintered together into a magnetic sheet in a green body, high mechanical stress will be formed in the connection or seam area between these material components due to these different thermal expansion coefficients, especially when cooling from the sintering temperature to room temperature. This may cause warping, cracks or overall mechanical stress in the magnetic sheet, which will seriously damage the mechanical or magnetic properties.
[0004] The technical problem to be solved by the present invention is to provide a magnetic sheet and a method for manufacturing the magnetic sheet, as well as a laminated plate group and a motor produced thereby, wherein when at least two material components are used in the magnetic sheet, the magnetic sheet has higher strength and lower inherent stress than the prior art.
[0005] This object is achieved according to the invention by a magnet lamination having the features of claim 1 , a method for producing a magnet lamination having the features of claim 11 , a laminated core having the features of claim 14 and an electric machine having the features of claim 15 .
[0006] The additively manufactured magnetic sheet of the lamination stack for an electric machine according to claim 1 comprises at least three layers connected by sintering, wherein in each layer there are at least two material components separated from each other in the plane extension direction. According to the present invention, the arrangement of the material components in the plane extension direction in each layer is symmetrical relative to the center plane of the magnetic sheet, wherein the ratio of the material share of the first material component and the second material component changes according to the layer sequence. Here, the first material component is arranged in the radial inner region of each layer, and the second material component is arranged in the radial outer region of each layer. The first material component includes an iron alloy having an austenitic structure of at least 25% by volume.
[0007] Compared with the prior art, the magnetic sheet has the advantage that the magnetic sheet itself is constructed as a laminate from a plurality of different layers, wherein the plurality of layers are firmly connected to one another by sintering, and the material proportions of the plurality of material components in each layer are different, thereby compensating for stresses caused by different thermal expansion coefficients of the individual material components.
[0008] The magnetic disc produced in this way also has a higher mechanical stability, because the material components located radially inside have an austenitic structure and therefore have a higher mechanical strength. In order to reduce the stress caused by different expansion coefficients, the symmetry of the individual layers is also important. Thus, the reference magnetic disc props up a symmetry plane on the magnetic disc plane, which is exactly at half the height of the magnetic disc. The material proportions of the individual material components above and below the symmetry plane are the same. This is mainly aimed not only to reduce the stress caused by the expansion coefficient, but also to make the magnetic disc less arched.
[0009] In a further embodiment of the invention, the second material component comprises an iron alloy comprising at least 95% by weight, in particular at least 97% by weight and particularly preferably at least 99% by weight of iron. Ideally, it is pure iron, since pure iron has an optimal ferrite structure or martensite structure and has very good soft magnetic properties, which are advantageous for corresponding alternating magnetization in the electric machine.
[0010] The first material component should preferably be designed in the radially inner region of the magnetic disk in such a way that it has the highest possible strength and can withstand mechanical loads acting on the magnetic disk. For this purpose, a chromium-nickel alloy is particularly suitable as a starting material for the first material component. The chromium-nickel alloy preferably has a chromium component, wherein the chromium content is between 22% and 28% by weight, in particular between 24% and 26% by weight.
[0011] In a suitable embodiment of the invention, the nickel content is between 4% and 10% by weight, in particular between 6% and 8% by weight, wherein the end points are contained in the specified range.
[0012] In another preferred embodiment of the present invention, it is provided that at least one layer is provided with a transition region between a radially inner region and a radially outer region. In the transition region, the first material component and the second material component are present in dispersed sub-regions. Dispersed sub-regions should be understood here as meaning that the individual material components are not mixed in the transition region, but that the region having the first material component and the region having the second material component are present in sections, i.e. dispersedly, in the transition region.
[0013] Here, each material component in the transition region can be arranged adjacent to the inner region or the outer region, or it can exist as an island within each other material component. Each material component in the transition region has the dispersed sub-regions described, which is particularly suitable for adapting different thermal expansion coefficients to each other. Compared with larger regions, smaller dispersed sub-regions have smaller absolute expansion during heating or sintering shrinkage during operation. For example, by finite element calculation, the appropriate structure of the dispersed sub-regions in the transition region can be determined, and thus by applying the finite element method, the stress in the magnetic sheet can also be minimized.
[0014] However, when using the transition region, it is appropriate to design the upper and lower covering layers of the magnetic sheet to have no transition region and to consist only of a radially inner region and a radially outer region. The advantage of this is that the magnetic shielding of the transition region located inside can be ensured, so that the magnetic region in the radially inner non-magnetic region itself does not cause eddy current loss.
[0015] In order to better match the thermal expansion coefficient in the magnetic sheet, it is also suitable that the individual layers can have different layer thicknesses. The layer thickness of the individual layers can have a layer thickness between 10 μm and 80 μm, especially between 20 μm and 50 μm, depending on the number of layers, which respectively form the magnetic sheet, and the number of layers is usually advantageously between three layers and nine layers.
[0016] Another aspect of the invention is a method for producing rotationally symmetrical magnetic segments of a lamination stack for an electric machine, the method comprising the following steps:
[0017] a) applying a first printing paste on the substrate by screen printing for structuring a first region of the first layer,
[0018] b) applying a second region of the first layer onto the substrate using a second printing paste, such that radially inner and radially outer printing regions are formed in the layer,
[0019] c) repeating steps a) to c) to produce at least three layers, which constitute the green body of the magnetic sheet, wherein:
[0020] d) said first printing paste and said second printing paste comprise different functional material precomponents, and these functional material precomponents of both printing pastes comprise iron particles in different alloy compositions, and
[0021] e) the arrangement of the printing areas in the individual layers is designed in such a way that they are symmetrical with respect to a central plane which extends parallel to the substrate and through the center of the green body, and the material proportions of the printing paste are different in the individual layers,
[0022] f) In order to form a magnet sheet, the green body is subjected to a sintering process, so that the radially inner printed area of the green body is converted into an iron-based material component in the magnet sheet, which material component has an austenitic structure at least in some areas.
[0023] It is usually appropriate, but not necessary in all cases, to insert a drying step between steps b) and c), depending on the viscosity and water content of the printing paste.
[0024] The method or the magnetic sheet produced thereby has the same advantageous properties as the magnetic sheet according to claim 1. In order to analyze the metallographic proportions, in particular to determine the austenitic structural proportion, the material is planarly sliced and evaluated by incident light microscopy using image processing software. For example, Zeiss microscopes and ZEN software can be used for image processing. Here, the favorable structural proportion of the austenitic structure is at least 25% by volume. In the structural proportions, since the evaluation is carried out by planar microsections and two-dimensional images, the volume fraction is used as the measured variable. When specifying the alloy composition, the weight percentage is used because the incorporation amount of the individual components can be measured by weight.
[0025] In a further advantageous embodiment of the method, a transitional printing region is created in at least two layers next to the radially inner printing region and next to the radially outer printing region, in which the first material precomponent and the second material precomponent are present in discrete sub-regions. This advantageous embodiment has also been described in relation to magnetic sheets and further reduces the influence of different expansion coefficients of the individual material components.
[0026] In particular, when island-shaped, dispersed sub-regions are depicted in the transitional printing region, printing a material component into the printed material component may be very complex in terms of process technology. In this case, it is expedient to use a printing-free additive manufacturing process, in particular a spraying process, to produce the second printing material precomponent, in particular in the island-shaped region.
[0027] Another aspect of the present invention is a lamination stack for a rotor of an electric machine, comprising a plurality of magnetic sheets according to any one of claims 1 to 10 or magnetic sheets manufactured according to the method of claim 11. In addition, one aspect of the present invention is an electric machine, comprising the lamination stack according to claim 14.
[0028] Other designs and other technical features of the present invention are further described with reference to the following figures. These figures are only schematic diagrams and do not constitute a limitation on the scope of protection. In each figure, the same figure number is used for features with different designs but the same name. In the figures:
[0029] Figure 1 The invention shows an exploded schematic diagram of an electrical machine, in particular an electric machine, mounted on a shaft, comprising a housing, a stator and a rotor,
[0030] Figure 2 shows a typical lamination stack for a rotor of an electrical machine,
[0031] Figure 3 An example of the layer structure of each layer of the magnetic sheet is shown,
[0032] Figure 4 Shown in relation to Figure 3 The layer structure of the magnetic sheet in the alternative design scheme is
[0033] Figure 5 Shown with respect to Figure 3 and 4 The layer structure of the magnetic sheet of the alternative design,
[0034] Figure 6 A top view of a magnetic sheet and a cross-sectional view of a magnetic sheet are shown, wherein the magnetic sheet has three material component regions.
[0035] Figure 7 Shown as Figure 6 A cross-sectional view of a magnetic sheet having an alternative design is shown,
[0036] Figure 8 A flow chart of a method for manufacturing a magnetic sheet is shown.
[0037] Figure 1 The figure shows an exploded view of an electric machine 6, which is in the form of an electric motor for an electric vehicle, for example. The individual components of the electric machine 6 are not described in detail here. However, the figure shows a rotor 48 mounted on a shaft 50. The rotor 48 here comprises a lamination stack 4, Figure 2 4 shows a laminated core 4 in more detail, wherein the laminated core 4 is composed of a stack of individual magnetic laminations 2. When installed in a rotor 48, the laminated core 4 is surrounded by a winding (not shown).
[0038] Figure 2As can be seen in the figure, the magnetic sheet 2 is a structured planar structure, where "planar" should be understood as a flat extension, and the extension of the magnetic sheet on the lamination plane is much larger than the height 64 of the magnetic sheet 2. The planar extension, that is, the diameter of the magnetic sheet 2 is preferably at least five times larger than the height 64.
[0039] Figure 3 2 shows a schematic cross-sectional view of a magnetic sheet 2. Only one surface of the rotationally symmetrical magnetic sheet 2 is shown here.
[0040] In addition, the description Figure 2 The magnetic sheet 2 and Figure 8 The characteristics of the magnetic sheet 2, especially the layered structure and the material components used, will be described in detail in the following. Figures 3 to 7 Detailed description in. Figures 3 to 7 Based on the finished magnetic sheet 2, but also with the corresponding layer structure and the characteristics of the individual material components during the production process, which only become the final characteristics during the manufacturing process. Different names are used here. Figures 3 to 5 In the description, the names associated with the magnetic sheet are used, and the reference numerals corresponding to these final features in the green body as a preliminary stage in the production process of the magnetic sheet 2 are marked in brackets. Figure 3 The magnetic sheet 2 shown has a total of seven layers 8-1 to 8-7. These layers 8-1 to 8-7 correspond to the layers in the production process of the magnetic sheet 2, which are marked in brackets as 32-1 to 32-7. Therefore, the bottom layer 8-1 has a radially inner area 10-1, which corresponds to the radially inner printing area 36 in the screen printing method 28. In addition, the layer 8-1 also has a second material component 10-2, which corresponds to the radially outer printing area 38. The thickness 24 of the layer 8-1 is about 30μm. Typically, the layer thickness 24 is between 10μm and 8μm.
[0041] The second layer 8-2 has a first material component 10-1 and a second material component 10-2. This applies continuously to the other layers 8-3 to 8-7. A symmetry plane 12 is defined here, which is parallel to the plane of the magnet sheet extending in the center of the magnet sheet 2. The center of the magnet sheet 2 is halfway up the height 64 of the magnet sheet 2 and is parallel to the plane of the magnet sheet, i.e. the surface of the magnet sheet or the substrate surface (see Figure 8) are parallel. The arrangement of the first material component 10-1 and the second material component 10-2 is symmetrically arranged above and below the symmetry plane 12. In addition, the proportion of the first material components 10-1 and 10-2 in each layer 8-1 to 8-7 is variable. Through these two measures, on the one hand, symmetry along the symmetry axis 12 is achieved, and on the other hand, each layer 8-1 to 8.7 is variable, which makes the various thermal expansion coefficients of the various material components 10-1 and 10-2 adapt to each other, thereby significantly reducing the material stress generated, especially during the sintering shrinkage process. In addition, the symmetrical arrangement of layers 8-1 to 8-7 means that the magnetic sheet will hardly curl, so that the magnetic sheet 2 has a higher flatness.
[0042] In addition, a transition region 18 (marked as a transition printing region in the green body) is provided, in which the first material component 10-1 and the second material component 10-2 are present on the entire magnetic sheet 2. As mentioned above, the transition region also plays a buffering role and minimizes the influence of the different expansion coefficients of the material components 10-1 and 10-2.
[0043] The material component 10-1 is preferably a chromium-nickel alloy, but it is not necessary, for example, the chromium content is 25% by weight and the nickel content is 7% by weight. This alloy is a stainless steel alloy with very high strength. This material component 10-1 constitutes the radial inner region 14 of the magnetic sheet 2, and serves as a supporting structure for the strength of the magnetic sheet 2, especially during high-speed rotation. In contrast, the material component 10-2 is designed as a magnetic material component, especially a soft magnetic component. Its iron content is very high, preferably exceeding 95% by weight, and particularly preferably exceeding 99% by weight. Such a high iron content, ideally pure iron, can form a ferrite material structure, which has particularly good soft magnetic properties. This pure iron structure is very easy to be alternatingly magnetized, wherein the hysteresis loss during the alternating magnetization of the material is very low.
[0044] exist Figure 4 and Figure 5 Shown in Figure 3 The magnetic sheet 2 described in detail has alternative designs for magnetic sheets with different structures. Figure 4 and Figure 5 and Figure 3 The main difference in the structural design of the magnetic sheet 2 shown is that the transition area 18 is larger than Figure 3 The second material component 10-2 having soft magnetic properties is embedded in the material region of the material component 10-1. Figure 6 and Figure 7 It can also be seen in another view in which a top view of the magnetic sheet 2 is shown. Figure 7In the embodiment, the dispersed sub-regions 20 of the material component 10-2 are embedded in the material component 10-1 in the shape of islands. These dispersed sub-regions 20 are located in the transition region 18, and different thermal expansion coefficients can be considered in the transition region 18 through these sub-regions 20. When designing the magnetic sheet 2, the corresponding distribution of the dispersed sub-regions 20 in the transition region 18 can be calculated using the finite element method, so as to optimize the adjustment of the thermal expansion coefficient between the material components 10-1 and 10-2.
[0045] Figure 5 The view of the middle magnetic piece 2 and Figure 4 The difference of the view is that there is a lower cover layer 22-1 and an upper cover layer 22-2, in which only the radially inner region 14 and the radially outer region 16 are present, while the transition region 18 is present in the middle layer, that is, in the present case, in the layers 8-2 to 8-8. It is covered by the first material component 10-1 and the soft magnetic material component 10-2, thereby forming a magnetic shield. This can reduce eddy current losses.
[0046] As mentioned earlier, Figure 6 and Figure 7 A top view of the magnetic disk 2 is shown, wherein in particular the transition region 18 is Figure 6 and Figure 7 Here, the magnet piece 2 has a hole 52, which is located in the center of the magnet piece 2 and through which the shaft 50 passes in the installed position.
[0047] Figure 8 Here, a method or possibility of manufacturing a magnetic sheet 2 having the described layer structure is shown. This is a very simplified schematic diagram, only to better illustrate the individual process steps. First, from Figure 8 Starting from the upper left of the figure, the first layer 32-1 of the green body 40 to be produced is produced by screen printing 28. In this embodiment, the printing screen 56 is designed as a screen printing template, and the first layer of printing paste 26-1 is printed on the substrate 30 by means of the printing screen 56 and the doctor blade 54. In the upper right part, it can be seen how the first printing paste 26-1 on the substrate 30 is dried in the drying device 58. The drying device 58 can be a drying box, for example, it can be designed in the form of a roller-guided continuous drying box, but it can also be a chamber for drying by infrared irradiation.
[0048] In the next step, a second printing paste 26-2 is printed onto the same substrate using another screen 56'. The two printing pastes 26-1 and 26-2 form a first printing area 34-1 and a second printing area 34-2, respectively. These printing areas 34-1 and 34-2 together form the first layer 32-1 of the green body 40. Excluding process errors, these printing areas 34-1 and 34-2 are directly adjacent to each other without overlapping. Figure 8In the pure schematic diagram, Figures 3 to 5 The detailed structure of the layers 32-1 to 32-7 shown will not be described here. Only the first printing area 34-1 and the second printing area 34-2 are shown here. Only the radially inner printing area 36 and the radially outer printing area 38 are marked in this simplified diagram. Figure 8 A further similar process is shown for stacking a plurality of layers 32-1 until finally 32-5 using this printing process. The drying process in the drying device 58 can be carried out after the individual partial printing of each area 34-1 or 34-2, or after the double printing of each layer 32-n, for example 32-1. This can reduce the process cost because drying does not need to be carried out after each individual printing.
[0049] Here, for example, the green compact 40 having five layers 32-1 to 32-5 is now removed from the substrate 30 and subjected to further heat treatment. First of all, there is a debinding step, in which the organic binder is thermally removed from the printing pastes 26-1 and 26-2 in a debinding device 60. In the next method step, the green compact 40 thus prepared is sintered in a sintering device 62 at a temperature between 1000° C. and 1350° C. to form the final magnetic sheet 2. During the sintering process, the individual grains of the iron alloy, which are not shown here, are bonded together by diffusion processes in the grain boundary region and to a lesser extent by melting processes, thus forming an integral structure. The magnetic sheet 2 thus produced is as shown in FIG. Figure 3-7 shown and with a correspondingly characterized layer sequence and the resulting mechanical advantage.
[0050] Reference numerals list
[0051] 2 Magnetic disk
[0052] 4 lamination pack
[0053] 6 Electrical machinery
[0054] Floors 8-1–8-9
[0055] 10-1–10-2 Material composition
[0056] 12 Middle plane
[0057] 14 Radially inner area
[0058] 16 Radially outer area
[0059] 18 Transition Zone
[0060] 20 Scattered sub-regions
[0061] 22-1, 2 Lower covering layer, upper covering layer
[0062] 24 layers thickness
[0063] 26-1 First Printing Paste
[0064] 26-2 Second printing paste
[0065] 28 Screen printing
[0066] 30 substrate
[0067] 32-1–32-9 Green layer
[0068] 34-1, 2 First printing area, second printing area
[0069] 36 Printing area located radially inward
[0070] 38 Printing area located radially outside
[0071] 40 Green
[0072] 42 Sintering process
[0073] 44 Transition Zone
[0074] 46 Dispersed sub-regions of the green body
[0075] 48 Rotor
[0076] 50 Axis
[0077] 52 holes
[0078] 54 Scraper
[0079] 56 Printing Screen
[0080] 58 Drying device
[0081] 60 Debonding device
[0082] 62 Sintering device
[0083] 64 Disk height
Claims
1. An additively manufactured magnetic sheet (2) for a laminated core (4) of an electric machine (6), the magnetic sheet comprising at least three layers (8-1, 8-2, 8-3 . . . 8-n) connected by sintering, wherein: In each layer (8-1, 8-2, 8-3 ... 8-n) there are at least two material components (10-1), (10-2) separated from each other in the plane extension direction, characterized in that: - the arrangement of the material components (10-1), (10-2) in the plane extension direction in each layer (8-1, 8-2, 8-3 ... 8-n) is symmetrical with respect to the center plane of the magnetic sheet (2), wherein: - the ratio of the material proportions of the first material component and the second material component changes depending on the layer sequence, and - the first material component (10-1) is arranged in a radially inner region (14) of each layer (8-1, 8-2, 8-3 ... 8-n), and the second material component (10-2) is arranged in a radially outer region (16) of each layer (8-1, 8-2, 8-3 ... 8-n), and - The first material component (10-1) comprises an iron alloy having an austenitic structure of at least 25% by volume.
2. The magnetic sheet according to claim 1, characterized in that: The second material component (10-2) comprises an iron alloy comprising at least 95% by weight, in particular at least 97% by weight, of iron.
3. The magnetic sheet according to claim 2, characterized in that: The second material component (10-2) has a ferrite structure or a martensitic structure.
4. The magnetic sheet according to any one of claims 1 to 3, characterized in that: The first material component (10-1) is a chromium-nickel alloy.
5. The magnetic sheet according to claim 4, characterized in that: The first material component (10-1) is an iron-chromium alloy, wherein the proportion of chromium is 22% to 28% by weight, in particular 24% to 26% by weight.
6. The magnetic sheet according to claim 4 or 5, characterized in that: The first material component (10-1) has a nickel content of 4 to 10% by weight, in particular 6 to 8% by weight.
7. The magnetic sheet according to any one of the preceding claims, characterized in that At least one layer (8-1, 8-2, 8-3 . . . 8-n) has a transition region (18) between a radially inner region (14) and a radially outer region (16), in which the first material component (10-1) and the second material component (10-2) are present in dispersed sub-regions (20).
8. The magnetic sheet according to claim 7, characterized in that: The lower cover layer (22-1) and the upper cover layer (22-2) of the magnetic sheet are respectively composed of only a radially inner region (14) and a radially outer region (16).
9. The magnetic sheet according to any one of the preceding claims, characterized in that The individual layers (8-1, 8-2, 8-3 . . . 8-n) of the magnetic sheet (2) have different layer thicknesses (24).
10. The magnetic sheet according to any one of the preceding claims, characterized in that The individual layers (8-1, 8-2, 8-3 . . . 8-n) have a layer thickness (24) of 10 μm to 80 μm.
11. A method for producing a rotationally symmetrical magnetic segment (2) for a lamination stack (4) of an electric machine (6), the method comprising the following steps: a) applying a first printing paste (26-1) on a substrate (30) by screen printing (28) for forming a first region (34-1) of a first layer (32-1), b) applying a second region (34-2) of the first layer (32-1) onto the substrate (30) using a second printing paste (26-2) such that a radially inner printing region (36) and a radially outer printing region (38) are formed in the layer, c) repeating steps a) to c) to produce at least three layers (32-1, 32-2, 32-3, ..., 32-n), which constitute the green body (40) of the magnetic sheet (2), wherein: d) the first printing paste (26-1) and the second printing paste (26-2) comprise different functional material precomponents, and these functional material precomponents of the two printing pastes comprise iron particles in different alloy compositions, and e) the arrangement of the printing areas (34-1, 34-2) in the individual layers (32-1, 32-2, 32-3, ..., 32-n) is designed in such a way that the areas (34-1, 34-2) are symmetrical with respect to a center plane (12) extending parallel to the substrate (30) and through the center of the green body (40), and the material proportions of the printing paste are different in the individual layers, f) In order to form the magnetic sheet (2), the green sheet (40) is subjected to a sintering process (42) so that the radially inner printed area (36) of the green sheet (40) is transformed into an iron-based material component (10-1) in the magnetic sheet (2), which material component at least partially has an austenitic structure.
12. The method according to claim 11, characterized in that A transition printing area is established in at least two layers (32-1, 32-2, 32-3, ..., 32-n) next to a radially inner printing area (36) and next to a radially outer printing area (38), in which the first material precomponent and the second material precomponent are present in dispersed sub-areas (46).
13. The method according to claim 11 or 12, characterized in that: In the transitional printing region, at least one material component is applied by a printing-free additive manufacturing method, in particular a spraying method.
14. A lamination stack for a rotor (48) of an electric machine (6), comprising a plurality of magnetic laminations (2) according to any one of claims 1 to 10.
15. An electric machine comprising the lamination stack (4) according to claim 14.
Citation Information
Patent Citations
Electric machine with locally-tuned properties
CN110880841A
Method for manufacturing a magnetic sheet and a stack of magnetic sheets and electric machine and electric vehicle
CN113678352A
Graded magnetic component and method of forming
EP3231888A1
Electric machine with locally-tuned properties
US20200083788A1
Magnetic sheet stack and method for producing a magnetic sheet stack
WO2020216645A1