System for marking and tracking hot section runner component in assembled state by using high-temperature material

By using dielectric substrate material and etched refractive film marks in the hot section runner of the turbine engine, combined with optical interference and thickness modulation technology, the problem of marking recognizability and visibility in high temperature environments is solved, and above 1350℃ is achieved Stability and efficient component tracking at temperature improve the maintenance efficiency of components on the wing.

CN119096003APending Publication Date: 2024-12-06INDIAN ACAD OF SCI +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280079292.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2021-11-29
Filing Date
2022-11-28
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing high-temperature markings are difficult to maintain recognizability and visibility in the hot section runners of turbine engines, and cannot effectively track and maintain components, affecting the maintenance efficiency of components on the wings.

Method used

Using marks made of dielectric substrate material and etched refractive film, the identification pattern is generated by optical interference and thickness modulation technology, and remains visible and readable by etching and heat treatment in high temperature environments, combined with thermal barrier coating protection , fixed to the surface of the component for long-term stability.

Benefits of technology

The stability and visibility of marking at temperatures above 1350°C are achieved, which reduces component inspection time, improves component tracking and maintenance efficiency on the wings, and ensures correct assembly and maintenance of components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119096003A_ABST
    Figure CN119096003A_ABST
Patent Text Reader

Abstract

A marker, a system, and a method of creating and utilizing a marker containing identification information are provided. Embodiments include an identification mark composed of a high temperature material for tracking a component in a high temperature environment. The indicia may be disposed on the component such that the indicia is secured to the component while undergoing a high temperature. Markers may provide for tracking a history of components attached to the marker for maintenance.
Need to check novelty before this filing date? Find Prior Art

Description

CROSS-REFERENCE TO RELATED APPLICATIONS

[0001] This application claims the benefit of Indian Provisional Application No. 202141055216 filed on November 29, 2021, which is incorporated herein by reference in its entirety. Technical Field

[0002] The present subject matter relates to identification markers and, more particularly, to high temperature markers for tracking components used in high temperature environments, such as turbine engines. Background Art

[0003] Components in the hot section of a turbine engine must be able to withstand thermal cycling and temperatures in excess of 1000°C. Markings used to track components within the hot section must also be able to withstand these temperatures and remain identifiable, visible, and / or readable after such exposure. Maintaining information about components aids in the proper maintenance of the assembly. Tracking and maintaining components on-wing aids in more efficient and effective repairs.

[0004] It is desirable to improve tracking of components in hot section flow paths to improve tracking of components on a wing and / or assembly. BRIEF DESCRIPTION OF THE DRAWINGS

[0005] Various needs are at least partially met by providing the identification marks described in the following detailed description (especially when studied in conjunction with the accompanying drawings). This specification, in conjunction with the accompanying drawings, provides a complete and enabling disclosure of various aspects of the description (including the best mode) to those of ordinary skill in the art, wherein:

[0006] Figure 1 is a cross-sectional view of an aircraft gas turbine engine;

[0007] Figure 2A is a schematic diagram of optical interference on a silicon dioxide film in some embodiments;

[0008] Figure 2B is a schematic diagram of a colorimetric diagram of different silicon dioxide thicknesses in some embodiments;

[0009] Figure 3A is a front view of a mark in some embodiments;

[0010] Figure 3B is a front view of a mark in some embodiments;

[0011] Figure 4 is a flowchart of an exemplary method of forming a mark in some embodiments;

[0012] Figure 5A A top view of the markings in the test tray;

[0013] Figure 5B FIG. 4 is a side view of a test tray disposed in a quartz tube.

[0014] Figure 5C is a perspective view of a quartz tube and a test tray disposed in a furnace;

[0015] Figure 6 is a top view of a pattern in some embodiments;

[0016] Fig. 7A is a top view of a pattern in some embodiments;

[0017] Figure 7B for Fig. 7A A top view of a pattern after thermal cycling in some embodiments;

[0018] Fig. 8A is a top view of a pattern in some embodiments;

[0019] Figure 8B for Fig. 8A A top view of a pattern after thermal cycling in some embodiments;

[0020] Fig. 9A is a top view of a pattern in some embodiments;

[0021] Fig. 9B for Fig. 9A A top view of a pattern after thermal cycling in some embodiments;

[0022] Fig. 10A is a top view of a pattern in some embodiments;

[0023] Fig. 10B for Fig. 10A A top view of a pattern after thermal cycling in some embodiments;

[0024] Fig.11A is a top view of a pattern in some embodiments;

[0025] Fig. 11B for Fig.11A A top view of a pattern after thermal cycling in some embodiments;

[0026] Fig. 12A is a top view of a pattern in some embodiments;

[0027] Fig. 12B for Fig. 12A Top view of the pattern after 15 hours of thermal cycling;

[0028] Fig. 12C for Fig. 12ATop view of the pattern after 40 hours of thermal cycling;

[0029] Fig.13 is a graph showing the relationship between etch depth and thermal cycle in some embodiments;

[0030] Fig.14 is a graph showing visibility versus thermal cycling in some embodiments;

[0031] Fig.15 is a block diagram of a system for scanning a tag in some embodiments;

[0032] Fig.16 is a front view of a system for scanning a mark in some embodiments;

[0033] Fig.17A A top view of a mark disposed on a surface of a component in some embodiments;

[0034] Fig. 17B is a front view of a marking provided on a surface of a component in some embodiments; and

[0035] Fig.18 A flow chart of an exemplary method of part tracking in some implementations.

[0036] The elements shown in the figures are shown for simplicity and clarity and are not necessarily drawn to scale. For example, the size and / or relative position of certain elements in the figures may be exaggerated relative to other elements to help improve the understanding of various embodiments of the present invention. In addition, common but easy to understand elements that are useful or necessary in commercially feasible embodiments are often not shown to facilitate a clearer view of these various embodiments of the present invention. Certain actions and / or steps may be illustrated or described in a specific order of occurrence, and those skilled in the art will understand that such specificity about the order is not actually required. DETAILED DESCRIPTION

[0037] The following embodiments illustrate the construction of a tag that can be used to track components that are subjected to high temperature environments, such as components in the hot section flow path of a turbine engine. More specifically, one or more benefits of tracking components in the hot section flow path is the increase of historical information about the components. In addition, another benefit is the ability to track the components when they are in an assembled state within the turbine engine, which reduces inspection time. These benefits can be achieved by tags that can withstand temperatures above 1350°C. The above and other benefits may become more apparent after a thorough review and study of the following specific embodiments.

[0038] Unless otherwise specifically defined herein, the terms and expressions used herein have the ordinary technical meanings given to these terms and expressions by those skilled in the art as described above. Unless otherwise explicitly stated, the word "or" used herein should be interpreted as having a separate structure rather than a connected structure. Unless otherwise specified herein, the terms "coupled", "fixed", "attached to", etc. refer to both direct coupling, fixing or attachment and indirect coupling, fixing or attachment through one or more intermediate components or features.

[0039] The singular forms "a," "an," and "the" include plural references unless the context clearly dictates otherwise.

[0040] Approximate expressions used in the specification and claims are used to modify a quantitative representation to allow for variations without resulting in a change in the basic function to which it is related. Thus, values ​​modified by terms such as "about," "approximately," and "substantially" are not limited to the precise values ​​specified. In at least some cases, an approximate expression may correspond to the precision of an instrument used to measure the value, or the precision of a method or machine used to construct or manufacture a component and / or system. For example, an approximate expression may refer to within a 10% margin.

[0041] Now refer to the drawings. In the drawings, like numbers represent like elements throughout the drawings. Figure 1 1 is a cross-sectional view of a gas turbine engine. The gas turbine engine is a high bypass turbofan jet engine, referred to herein as a "turbofan engine 10". The turbofan engine 10 defines an axial direction A (extending parallel to a longitudinal centerline 12 as a reference) and a radial direction R. Generally, the turbofan engine 10 includes a fan section 14 and a core turbine engine 16 located downstream of the fan section 14.

[0042] The illustrated exemplary core turbine engine 16 generally includes a generally tubular outer casing 18 defining an annular inlet 20. The tubular outer casing 18 encloses, in series flow relationship, a compressor section having a low pressure (LP) compressor 22 and a high pressure (HP) compressor 24; a combustion section 26; a turbine section having a high pressure (HP) turbine 28 and a low pressure (LP) turbine 30; and an ejection exhaust nozzle section 32. A high pressure (HP) shaft or spool 34 drivingly connects the HP turbine 28 to the HP compressor 24. A low pressure (LP) spool 36 drivingly connects the LP turbine 30 to the LP compressor 22.

[0043] The fan section 14 includes a variable pitch fan 38 having a plurality of fan blades 40 coupled to a disk 42 in an interval manner. As shown, the fan blades 40 extend outwardly from the disk 42 in a radial direction R as a whole. Each fan blade 40 can rotate about a blade axis P relative to the disk 42 by operably coupling the fan blades 40 to an actuating member 44, and the actuating member 44 is configured to change the pitch of the fan blades 40 in unison. The fan blades 40, the disk 42, and the actuating member 44 rotate together about the longitudinal centerline 12 through the low pressure shaft 36 across the power gear box 46. The power gear box 46 includes a plurality of gears for gradually reducing the rotational speed of the LP shaft 36 to a more efficient fan rotational speed.

[0044] Continue to see Figure 1 . The disk 42 is covered by a rotatable forward impeller hub 48 having an aerodynamic profile to facilitate airflow through the plurality of fan blades 40. In addition, the exemplary fan section 14 includes an annular fan casing or outer nacelle 50 that circumferentially surrounds at least a portion of the variable pitch fan 38 and / or the core turbine engine 16. It should be understood that the outer nacelle 50 may be configured to be supported by a plurality of circumferentially spaced outlet guide vanes 52, opposite the core turbine engine 16. A downstream portion 54 of the outer nacelle 50 may extend above the exterior of the core turbine engine 16 to define a bypass airflow passage 56 therebetween.

[0045] During operation of the turbofan engine 10, a volume of air 58 enters the turbofan engine 10 through the outer nacelle 50 and / or the associated inlet 60 of the fan section 14. As the volume of air 58 passes through the fan blades 40, a first portion 62 of the air 58 (as indicated by the arrow) is directed or routed into the bypass airflow passage 56, while a second portion 64 of the air 58 (as indicated by the arrow) is directed or routed into the LP compressor 22. The ratio between the first portion 62 of the air 58 and the second portion 64 of the air 58 is generally referred to as the bypass ratio. The pressure of the second portion 64 of the air 58 is then increased as it is directed through the HP compressor 24 and into the combustion section 26, where the air 58 is mixed with fuel and combusted to provide combustion gases 66. The combustion gases 66 are then directed through the hot runners or hot section runners of the HP turbine 28 and the LP turbine 30, where a portion of the thermal energy and / or kinetic energy is extracted from the combustion gases 66.

[0046] The combustion gases 66 are then directed through the jet exhaust nozzle portion 32 of the core turbine engine 16 to provide propulsive thrust. At the same time, the pressure of the first portion 62 of the air 58 is significantly increased as it is directed through the bypass airflow passage 56 before being discharged from the fan nozzle exhaust portion 76 of the turbofan engine 10, thereby also providing propulsive thrust.

[0047] However, it should be understood that Figure 1 The exemplary turbofan engine 10 shown in is for example only, and in other exemplary embodiments, aspects of the present invention may be applied additionally or alternatively to any other suitable gas turbine engine. For example, in other exemplary embodiments, the turbofan engine 10 may be any other suitable aviation gas turbine engine, such as a turbojet engine, a turboshaft engine, a turboprop engine, etc. In addition, in other exemplary embodiments, the exemplary turbofan engine 10 may include or be operably connected to any other suitable accessory system. In addition, the exemplary turbofan engine 10 may also not include or be operably connected to more than one of the above-mentioned accessory systems.

[0048] See also Figure 2A and 2B . It shows an optical interference pattern on a silicon dioxide film 90 and a colorimetric diagram of different silicon dioxide thicknesses. Crystalline silicon usually oxidizes when in contact with oxygen and water to form an oxide layer containing silicon dioxide. At room temperature, the thickness of the oxide layer is about 1.5 nm. Therefore, it is difficult to avoid the presence of an oxide layer when using silicon wafers. For this purpose, commercially available silicon wafers are processed into silicon wafers with a known oxide thickness (the oxide is grown in a controlled environment).

[0049] The silicon dioxide film 94 on top of the silicon substrate 96 surface behaves as a semi-transparent layer to minimize contact with the air 92. Therefore, when viewed under a microscope, light 102 is reflected from at least the air and silicon dioxide interface 98 (between the air 92 and the silicon dioxide film 94), and from the silicon dioxide and silicon interface 100 (between the silicon dioxide film 94 and the silicon substrate 96). The reflected light 104 from the air and silicon dioxide interface 98 and the reflected light 106 from the silicon dioxide and silicon interface 100 undergo a phase change of about 180 degrees compared to the light 102. The reflected light 104 and 106 may be reflected into a medium with a lower refractive index.

[0050] Reflected light rays 104 and 106 may interfere with each other and add to each other. Although the refractive index of silica can be considered constant, it can vary with the wavelength of the incident light as well as the angle of incidence. To determine the intensity of the reflected light, the angle and wavelength need to be considered, as well as the type of light source and microscope settings.

[0051] like Figure 2B As shown, the wavelengths of visible light that interfere constructively for a given angle and oxide thickness can determine the dominant colors in the reflection spectrum. Figure 2BThe color variation for different silicon dioxide thicknesses is shown. The reflectance spectrum, which depends on the thickness of the oxide layer, can be used to generate patterns visible through an optical microscope.

[0052] See also Figure 3A . It shows a mark 110 in some embodiments. The mark 110 includes a dielectric substrate material 112, and a refractive film 114 is provided on its top surface. The refractive film 114 of the mark 110 has not yet been etched with an identification pattern. The dielectric substrate material 112 may be composed of silicon, germanium, titanium, doped silicon, doped germanium, and doped titanium, and / or a combination thereof. The refractive film 114 may be composed of oxides, carbides, nitrides, fluorides, and / or a combination thereof. The refractive film 114 may have a thickness of about 50 angstroms to 3900 angstroms. In some other embodiments, the refractive film 114 may have a thickness of about 100 angstroms to 900 angstroms.

[0053] See also Figure 3B . It shows a mark 116 of a refractive film 114 with an etched identification pattern in some embodiments. Figure 3A The thickness modulated film 118 is obtained by etching the refractive film 114 in the dielectric substrate material 112. The refractive film 114 is similar to the silicon dioxide film 94, and can be etched to different depths to provide different reflective colors. The thickness modulated film 118 can be etched in the refractive film 114, and the thickness of the etching pattern can be less than that of the refractive film 114. The thickness modulated film 118 can include an etching pattern so that the surface of the thickness modulated film 118 is modulated on the refractive film 114. The thickness of the thickness modulated film 118 can be equal to the thickness of the refractive film 114, so that the thickness modulated film 118 can be disposed on the surface of the dielectric substrate material 112. The thickness modulated film 118 and the refractive film 114 can be the same material, so that the etching depth is defined as from the surface of the dielectric substrate material 112 to the top of the thickness modulated film 118 layer.

[0054] The refractive film 114 may be etched using a dry etching process, a wet etching process, and / or a combination thereof. The thickness modulated film 118 may have a thickness of about 5 nanometers to 390 nanometers. The thickness modulated film 118 or the etching depth may be determined using the different refractive properties (e.g., dielectric constant) of the dielectric substrate material 112 and the refractive film 114, as described above with reference to Figure 2A and Figure 2B This allows for the spectral distribution of the reflected light from the refractive film 114 or thickness modulated film 118 on the dielectric substrate material 112. The spectral distribution may be highly sensitive to the thickness of the refractive film layer 114 or thickness modulated film 118 due to optical interference effects.

[0055] A refractive material coating 120 may be disposed on the surface of the thickness modulated film 118. The refractive material 120 may be composed of barium fluoride, calcium fluoride, lanthanum fluoride, magnesium fluoride, hafnium oxide, silicon dioxide, aluminum oxide, titanium nitride, and / or combinations thereof to protect the etched pattern.

[0056] The refractive film 114 may be etched to achieve or create at least one pattern. In some embodiments, a pattern may be printed onto the refractive film 114 prior to etching to depict the pattern to be etched. A thickness modulated film 118 may be created that includes, contains, or has a pattern printed onto the refractive film 114 prior to etching, similar to the above in conjunction with Figure 2A and 2B The etched pattern may be contained within the thickness modulated film 118, or may be the result of a contrast between the thickness modulated film 118 and the remaining, i.e., unetched, refractive film 114. The pattern may include features that allow the pattern to be tracked, such that the pattern is an identification pattern. The etching process may further create a pattern that is readable, visible, and / or sensed by an optical sensor. This may occur by the contrast created by the etching process that etches the refractive film 114 to create the thickness modulated film 118.

[0057] The dry etching process may include sputtering or dissolving at least a portion of the refractive film 114 using a reactive ion or vapor phase etchant, while the wet etching process may include dissolving at least a portion of the refractive film 114 in a chemical solution. In some embodiments, the etching process may be performed using micron or nano-fabrication techniques, optical lithography techniques, or photon-based techniques. In an illustrative embodiment, etching may utilize an isotropic etching process, which includes projecting an image or shadow onto a photosensitive emulsion or a substrate coated with a photoresist coating. In yet another embodiment, the etching process may be selected to allow control of the size of the channel created for patterning. The selection of the etching process may also allow patterns to be manufactured on areas as large as submicron scales. This may enable patterns to be arranged on components of many different sizes. The pattern may be predefined by a user or machine to track components and / or pair with components.

[0058] See also Figure 4. It shows a flow chart of an exemplary method 122 for forming a mark 116 in some embodiments. For example, method 122 and / or more than one step of method 122 may be applicable to more than one embodiment described herein. Method 122 includes step 124 of etching a refractive film 114 disposed on a surface of a dielectric substrate material 112. In addition, method 122 includes step 126 of obtaining a thickness modulated film 118. The thickness modulated film 118 may be etched into the refractive film 114 or etched outside the refractive film 114, as described above. Therefore, the thickness modulated film 118 and the refractive film 114 may be composed of the same layer / material. For illustrative purposes, in the accompanying drawings, the thickness modulated film 118 or the etching depth is shown as a layer separated from the refractive film 114, however, as previously described, the two layers may be a single layer / single material, wherein the thickness modulated film 118 is etched into the refractive film 114 or etched outside the refractive film 114. In addition, the etching depth can have a depth extending from the dielectric base material 112 to the top of the thickness modulated film 118, where the thickness modulated film 118 and the refractive material 120 are joined. The method 122 also includes a step 128 of coating the thickness modulated film 118 and the refractive film 114 with the refractive material 120. In some embodiments, the thickness modulated film 118 can be coated but not cover the entire surface of the refractive film 114, or the refractive film 114 is exposed through the thickness modulated film 118. In addition, the method 122 includes a step 130 of obtaining an optically readable recognition pattern. The optically readable pattern discussed in more detail below can be the result of etching the refractive film 114 and subsequently creating the thickness modulated film 118.

[0059] In an illustrative embodiment, a dielectric substrate material 112 (e.g., a silicon substrate) has a refractive film 114 (e.g., silicon dioxide) disposed on a surface of the dielectric substrate material 112, which are collectively referred to as a substrate. The refractive film 114 may have a thickness of approximately 280 nm. The substrate may be subjected to a standard wafer cleaning procedure, which may include sonicating the substrate in acetone and then rinsing in isopropyl alcohol and deionized water.

[0060] The identification pattern can be printed onto the refractive film 114 using optical lithography and buffered HF processing. The identification pattern can be drawn using AutoCAD software and then converted to an appropriate format. The size of the identification pattern can be selected to ensure easy optical imaging through a microscope and surface profile measurement by an atomic force microscope (AFM) and a Dektak surface profiler. Lithography can be completed in a Microtech LW-405 instrument. A laser writer using rasterization can be used to write the identification pattern onto the refractive film 114. The sample wavelength used is 405nm, which is in the ultraviolet (UV) spectrum. A positive photoresist (S1813) can be spin-coated onto the refractive film 114 and then preheated. Positive photoresists are sensitive to the ultraviolet spectrum but not to the visible light range. MF26A is a chemical commonly used in photoresist developers for optical lithography, used to develop the identification pattern after exposure.

[0061] After exposure and development, a post-heat treatment may be performed to ensure that the buffered HF selectively etches the refractive film 114 to obtain the thickness modulated film 118. During etching, the mark 116 may be immersed in buffered HF and then rinsed with deionized water to wash off the acid and stop the etching process. After etching, the mark 116 with the thickness modulated film 118 may be immersed in isopropyl alcohol to remove organic residues. This step may remove the photoresist. A nitrogen gun may be used to dry the mark 116. Atomic layer deposition (ALD) may be used to deposit a refractive material 120 (e.g., aluminum oxide) on the mark 116, specifically, the refractive material 120 is deposited on the thickness modulated film 118 as a mask layer and / or coating.

[0062] See also FIG. 5A to FIG. 5C . With reference Figure 3B The marks described are similar, showing the marks in the heat treatment. Test setup 132 is shown with marks 136 loaded into tray 134. Tray 134 can then be loaded into test tube 138. Tray 134 and test tube 138 can be placed in furnace 140 for heating mark 136. Test tube 138 can remain open to ensure that heat treatment is performed under atmospheric conditions. Furnace 140 can be operated in proportional-integral-differential (PID) control mode. The automatic adjustment of PID can be set to activation, that is, the PID value is optimized by the temperature controller of furnace 140 to ensure that overshoot is minimized and the temperature is stable at the set point. The temperature rise rate can be set to 24°C per minute. Ramp-down is naturally allowed. Heat treatment can be performed at a temperature of about 1000°C for one hour or longer. This can be regarded as a heat treatment.

[0063] See also Figure 6 . Combined with Figure 3BThe recognition pattern described is similar, which shows an image of pattern 142. The image of pattern 142 was taken using an Olympus UC30 camera mounted on an Olympus BX51 microscope at 20x optical magnification.

[0064] See also Fig. 7A and Figure 7B . It shows the image before the pattern thermal cycle ( Fig. 7A ), and the image after thermal cycling of the pattern. Similarly, FIG. 8A to FIG. 11B Images of patterns 144, 146, 148, 150, 152 are shown before (A) and after (B) thermal cycling. Figures 7A to 11B The thermal cycle was repeated 6 times at one hour intervals. Figure 3B The pattern described is similar, and undergoes a similar process to that of bonding FIG. 5A to FIG. 5C Some patterns are coated with a layer of aluminum oxide. In one illustrative embodiment, a 20 nm aluminum oxide mask layer is deposited on its surface using ALD, as shown in FIG. Fig.13 As shown in sample E.

[0065] like Fig. 7A As shown, Figure 7B In contrast, pattern 144 may change color after thermal cycling. This may be due to the small change in the thickness of the refractive film. However, if Figure 7B As shown, pattern 144 remains intact and at least partially discernible after thermal cycling.

[0066] See also Figures 12A to 12C . Similar to the above, pattern 154 is etched into the refractive film, thereby creating a thickness modulated film. In this illustrative embodiment, pattern 154 is printed and etched so that pattern 154 is a quick response (QR) code. Pattern 154 can be etched in such a way that pattern 154 can be scanned, sensed and / or read using an optical sensor. This can include a barcode, a printed microscopic pattern, a QR code, or an identification number. These patterns can be traced back to the component to which they are fixed.

[0067] Fig. 12A A QR code etched into the refractive film is shown. Fig. 12B Pattern 154 is shown after fifteen hours of thermal cycling. Fig. 12C The pattern 154 is shown after forty hours of thermal cycling. In some embodiments, the pattern 154 can be optically readable after forty hours of thermal cycling. Optical readability or optical visibility is a method of quantifying how the intensity of reflected light depends on various factors, such as the spectrum of the light source, the thickness of the oxide, and the refractive index of the oxide. As used and discussed herein, the optical readability of a pattern can be imaged by an instrument utilizing visible light, which is quantified using a visibility parameter obtained from the following formula.

[0068] Visibility can be determined using the Michelson contrast equation: Visibility = (I max -I min ) / (I max +I min )

[0069] Here, I max and I min It can be determined by the light intensity from the background (e.g., unetched refractive film) and the reflected light intensity from the pattern (e.g., thickness modulated film). max It can be defined by the larger intensity measured between the background intensity and the pattern intensity. min It can be defined by the smaller intensity measured between the background intensity and the pattern intensity. In some embodiments, if the intensity of the reflected light from the pattern is greater than the background, the pattern is visible and readable. In other embodiments, if the light intensity from the pattern is different from the background light intensity, and the pattern is visible and readable, the background intensity may be higher.

[0070] As described in this article, Fig.14 As shown on the x-axis, if the visibility parameter is greater than or equal to 0.01, the pattern can be captured using a visible light instrument.

[0071] In some embodiments, the pattern can be stable such that the pattern is visible and / or readable at a temperature of about -273.14°C to 1350°C for a period of at least forty hours. In other embodiments, the pattern can be stable such that the pattern is visible and / or readable at a temperature of about -273.14°C to 1350°C and a pressure range of about 1 micro Pascal to about 100 Giga Pascal for a period of at least forty hours. In other embodiments, the pattern can be stable such that the pattern is visible and / or readable at a temperature of about -273.14°C to 1350°C and a pressure range of about 1 micro Pascal to about 100 Giga Pascal for a period of at least forty hours. -10 The pressure and / or humidity range of the torr is visible and / or readable under extreme humidity conditions from 0% to 100%.

[0072] For example, the markings may be used in and / or on turbine engines, automobiles, research instruments, jet engines, gas turbines, steam turbines, and other applications where harsh high temperature environments may exist.

[0073] See also Fig.13. It is shown in Figure 156. The figure shows samples D, E, F and G, with the y-axis representing the etching depth of the pattern and the x-axis representing the thermal cycle at 1000°C (in hours). Samples D and E have the same etching depth, which is about 40.1nm. The etching depth of sample F is about 49.4nm. The etching depth of sample G is about 90.3nm. Figure 156 shows how thermal cycling affects the etching depth. Figure 156 shows that the etching depth decreases slightly at the beginning of the thermal cycle and seems to stabilize after about ten thermal cycles.

[0074] See also Fig.14 . It is shown in Figure 158. Samples D, E, F and G are shown in the figure, the y-axis represents visibility and the x-axis represents thermal cycles in hours. The y-axis is plotted on a logarithmic scale. The samples have the above combined Fig.13 The pattern etch depth described above is approximately the same. Fifty thermal cycles were performed at 1000°C. Visibility was calculated using the Michelson contrast equation as explained above. Figure 158 shows that the visibility of the sample generally decreases with successive thermal cycles, but the sample is still visible after fifty thermal cycles, and combined with the above Figure 2A and 2B Similar to what has been discussed, in some cases it may become more visible due to color changes associated with changes in etch depth.

[0075] More specifically, FIG. 158 shows that the visibility parameter fluctuates around a visibility parameter of about 0.1. As shown, after fifty thermal cycles, the visibility parameters of samples D, E, F, and G remain above zero. As described above, if the visibility parameter is greater than or equal to 0.01 (a-axis), the pattern can be captured using an instrument using visible light. Therefore, FIG. 158 shows that the pattern can be captured by an instrument using visible light after at least 50 thermal cycles.

[0076] See also Fig.15 . It shows a system for scanning a tag in some embodiments. The system 160 includes a sensor 162 and a tag 116 (refer to Figure 3B ). The marking 116 is composed of a dielectric base material 112, a refractive film 114, a thickness modulated film 118, and a refractive coating 120. The sensor 162 can scan a pattern on or created by the thickness modulated film 118 and the refractive film 114. As described in more detail below, the system includes a database 186 for storing the sensed or scanned patterns to link the patterns to the parts.

[0077] refer to Fig.16 , which shows a system for scanning a tag according to some embodiments. The system 164 includes a sensor 162 and a tag 116 (refer to Figure 3B). The marking 116 is composed of a dielectric base material 112, a refractive film 114, a thickness modulated film 118, and a refractive coating 120. The sensor 162 can scan a pattern (e.g., patterns 144, 146, 148, 150, 152) created on or by the thickness modulated film 118 and the refractive film 114. As described in more detail below, the system includes a database 186 for storing the sensed or scanned patterns to link the patterns to the parts.

[0078] In some embodiments, the marker 116 can be coated with a thermal barrier coating 166. The thermal barrier coating 166 can be deposited on the marker 116 to protect the marker 116 from excessive heat of the environment. The thermal barrier coating 166 can also help protect the marker 116 from dust and debris in the environment that may contact and / or deposit on the surface of the marker 116. In addition, the thermal barrier coating 166 can allow the marker 116 to remain visible for a longer period of time and more thermal cycles.

[0079] See also Fig.17A . It shows a mark set on the surface of a component in some embodiments. The component 168 (e.g., a turbine blade) is shown as having a base metal material 170, a mark 116, and an adhesive layer 172. The adhesive layer 172 can fix the mark 116 to the base metal material 170. The adhesive layer 182 may include one or more high-temperature adhesives, glues, or cements. Fixing the mark 116 to the base metal material 170 can be achieved by one or more electrodeposition, brazing, cladding, welding, spraying, coating, or embedding, which methods can be combined with or replace the adhesive layer 182.

[0080] See also Fig. 17B . It shows the markings provided on the surface of the component in some embodiments. Fig.17A Similarly, the indicia 116 is secured to the base metal material 170 via the adhesive layer 182. The indicia 116 can be coated with a thermal barrier coating 166. In some embodiments, the base metal material 170 can also be coated with a thermal barrier coating 166. In some embodiments, the indicia 116 can be exposed through the thermal barrier coating 166. The thermal barrier coating 166 provides and / or acts as a barrier to oxygen diffusion, which can change the overall thickness of the pattern created on or by the thickness modulated film 118 and the refractive film 114, which can reduce visibility parameters. Aluminum oxide can be used as the thermal barrier coating 166, but other materials can also be used, such as different oxides, including those similar to the aluminum oxide contemplated herein.

[0081] See also Fig.18. It shows an exemplary tracking method 174 of components in some embodiments. For example, method 174 and / or more than one step of method 174 may be applied to more than one embodiment described herein. Method 174 includes step 176 of fixing a tag having identification information to a component. In addition, method 174 includes step 178 of pairing the identification information with the component (e.g., component information). Method 174 also includes step 180 of maintaining a database 186 of component information. In addition, method 174 includes step 182 of sensing the identification information using sensor 162. In addition, method 174 includes step 184 of retrieving a component history based on the sensed identification information. The method also includes step 186 of updating a database 186 of component information in response to the sensed identification information.

[0082] The marker 116 may be affixed to the component 168 prior to assembling the system (e.g., a turbine engine). After the marker 116 is affixed and the system is assembled, the sensor 162 may then be used to scan the marker 116. This may be accomplished using a borescope opening in the turbine engine casing, into which the sensor 162 may be inserted to scan the marker 116. The sensor 162 may be optically sensed using an optical sensor (e.g., a camera) to visually inspect the marker 116. In some embodiments, the sensor 162 may use optical, ultraviolet, infrared scanning, or acoustic scanning. In some embodiments using a thermal barrier coating 166, acoustic scanning may be used. In some embodiments, magnetic scanning may be used. In some embodiments, the pattern may be provided on the component 168 itself.

[0083] The sensor 162 may include more than one processor. The processor may be configured to communicate with the sensor 162 via a communication network (e.g., LAN, WAN, Internet). The sensor 162 may scan the tag 116 to sense, parse, or read the identification pattern or information contained on the surface of the tag 116 from the thickness modulated film 118. The processor may transmit the sensed identification information to the processor, and the processor may communicate with and reference the database 186. The database 186 may map or pair the identification pattern to the component to which the tag 116 is fixed. After pairing, subsequent scans may allow the database 186 to record, track, or maintain a scan record or scan history of the sensed identification information, thereby tracking the component scan. The mapping or pairing of the identification pattern to the component may be performed before or after the tag 116 is fixed to the component 168. Similarly, the application of the thermal barrier coating 166 may be performed before or after the tag 116 is fixed; therefore, the tag 116 may be attached to the component 168 that already includes the thermal barrier coating 166.

[0084] An image of component 168 including marker 116 may be captured using an inspection device, such as an optical sensor inserted through a borescope opening. A pattern may be scanned, read, and / or sensed from the image. This may allow the component to be tracked during an inspection image of component 168. Securing marker 116 to component 168 in an exposed position allows the marker to be scanned, read, and / or sensed in an assembled state and / or in an on-wing state. Marker 116 may include a pattern that is unique to component 168, such that different components within a turbine engine have patterns that are different from one another.

[0085] Marker 116 can be used in high or low temperature and / or pressure environments. High and low temperature environments can be, for example, about -273.14°C to 1350°C. In one illustrative embodiment, the high temperature environment in the hot runner of a turbine engine can be about 1200°C. High and low pressure environments can be, for example, about 1 micropascal to 100 gigapascals.

[0086] Mark 116 can be used for parts in these high or low temperature and / or high pressure environments. In one illustrative embodiment, mark 116 can be used for parts of turbine engines. Mark 116 can also be used in automotive applications, such as for parts in and throughout engines and exhaust systems. Other applications of mark 116 can be heavy machinery industries, such as turbines for power applications, such as turbines used in wind turbines and hydroelectric dams. Mark 116 can also be used in low temperature industries and / or applications. Other industries including high temperature environments that can use mark 116 can be, for example, nuclear reactors, boilers and chimneys. Finally, mark 116 can be used in the entire aerospace industry, including space vehicles, such as rockets.

[0087] Further aspects of the invention are provided by the subject matter of the following clauses:

[0088] A marker (object) includes: a dielectric substrate material; a refractive film, which is arranged on the dielectric substrate material and is etched to obtain a thickness modulated film; and a refractive material coating, which is arranged on the thickness modulated film to obtain an identification pattern.

[0089] The marking of any of the preceding items, wherein the identification pattern is stable at a temperature of about -273.14°C to 1350°C for a period of at least 40 hours.

[0090] The marking of any of the preceding items, wherein the identification pattern is stable over a pressure range of about 1 microPascal to 100 gigapascals.

[0091] The marking of any of the preceding items, wherein the identification pattern comprises one or more of a barcode, a printed micro pattern, and a QR code.

[0092] The marking of any of the preceding items, wherein the etching of the refractive film comprises one or more of a dry etching process and a wet etching process.

[0093] The marking of any of the preceding items, wherein the refractive film comprises one or more of oxides, carbides, nitrides and fluorides.

[0094] The marking of any of the preceding items, wherein the refractive film has a thickness of about 500 angstroms to 3900 angstroms.

[0095] The marking of any of the preceding items, wherein the dielectric substrate material comprises one or more of silicon, germanium, titanium, doped silicon, doped germanium, and doped titanium.

[0096] The marker of any of the preceding items, wherein the thickness modulation amount of the thickness modulated film is about 5 nanometers to 390 nanometers.

[0097] The marking of any of the preceding items, wherein the refractive material comprises one or more of barium fluoride, calcium fluoride, lanthanum fluoride, magnesium fluoride, hafnium oxide, silicon dioxide, aluminum oxide or titanium nitride.

[0098] The marker of any preceding clause, wherein the marker is secured to a component used in a hot runner of a gas turbine engine.

[0099] A method includes: fixing a marker to a component, wherein a refractive film has an identification pattern; and pairing the identification pattern of the marker with the component.

[0100] The method of any of the preceding items, wherein the recognition pattern is stable at a temperature of about -273.14°C to 1350°C.

[0101] The method of any of the foregoing items further includes the following steps: maintaining a component pattern database for components; sensing a recognition pattern of a marking on a component; retrieving a component history from the component pattern database; and updating the component pattern database for the component in response to sensing the recognition pattern of the marking on the component.

[0102] The method of any of the preceding claims, wherein the marker is secured to the component by at least one of electrodeposition, brazing, cladding, welding, spraying, coating, and embedding.

[0103] The method of any of the preceding claims, further comprising securing a marker to a component used in a hot runner of a gas turbine engine.

[0104] The method of any of the preceding items, further comprising coating the marking with a thermal barrier material.

[0105] The method of any of the preceding items, further comprising coating the component with a thermal barrier material.

[0106] The method of any of the preceding items, wherein sensing the identification pattern of the marker comprises at least one of optical, ultraviolet, infrared scanning, and acoustic scanning.

[0107] The method of any of the preceding items, wherein sensing the marking comprises visually inspecting the marking with a camera.

[0108] A method as in any preceding claim, wherein the marking comprises a pattern traceable to an identification number.

[0109] The method of any of the foregoing items, wherein the identification pattern comprises one or more of a barcode, a printed micro pattern, and a QR code.

[0110] A method for making a mark, comprising: etching a refractive film on a dielectric substrate material to obtain a thickness modulated film; coating a refractive material on the thickness modulated film to obtain an identification pattern; wherein the identification pattern is stable at a temperature of about -273.14 degrees Celsius to about 1350 degrees Celsius for a period of at least 40 hours.

[0111] The method of any of the preceding items, wherein the recognition pattern is stable at pressures in the range of about 1 microPascal (μPa) to about 100 gigapascals (GPa).

[0112] The method of any of the preceding items, wherein the identification pattern comprises at least one of a barcode, a printed micro pattern, and a QR code.

[0113] Any of the above methods, wherein etching the refractive film is selected from at least one of a dry etching process and a wet etching process.

[0114] The method of any of the preceding items, wherein the refractive film is selected from the group consisting of at least one of oxides, nitrides, and fluorides.

[0115] The method of any of the preceding items, wherein the refractive film has a thickness of about 50 angstroms to about 3900 angstroms.

[0116] The method of any of the preceding items, wherein the dielectric substrate material comprises at least one of silicon, germanium, titanium, doped silicon, doped germanium, and doped titanium.

[0117] The method of any of the foregoing, wherein the thickness modulation amount of the thickness modulated film is from about 5 nanometers to about 390 nanometers.

[0118] The method of any of the preceding items, wherein the refractive material comprises at least one of barium fluoride, calcium fluoride, lanthanum fluoride, magnesium fluoride, hafnium oxide, silicon dioxide, aluminum oxide, and titanium nitride.

[0119] A method as in any preceding claim, wherein the dielectric substrate material is secured to a component for use in a hot runner of a gas turbine engine.

[0120] Those skilled in the art will appreciate that various modifications, changes and combinations may be made to the above-described embodiments without departing from the scope of the present invention, and these modifications, changes and combinations should be understood to be within the scope of the inventive concept.

[0121] This written description uses examples to disclose the invention, including its best mode, and to enable those skilled in the art to practice the invention, including making and using any devices or systems and performing any incorporated methods. The patentable scope of the invention is defined by the claims, and may include other examples that occur to those skilled in the art. Such other examples are intended to be within the scope of the claims if they include structural elements that do not differ from the literal language of the claims, or if they include equivalent structural elements that do not differ substantially from the literal language of the claims.

Claims

1. A label, comprising: Dielectric substrate materials; A refractive film, wherein the refractive film is disposed on a dielectric substrate material and a thickness modulated film is obtained after etching; and A refractive material coating is provided on the thickness modulated film to obtain a recognition pattern.

2. The marking according to claim 1, wherein: The recognition pattern is stable at a temperature of about -273.14°C to 1350°C for a period of at least 40 hours.

3. The marking according to claim 1, wherein: The recognition pattern is stable over a pressure range of about 1 micropascal to 100 gigapascals.

4. The marking according to claim 1, wherein: The identification pattern includes one or more of a barcode, a printed micro pattern and a QR code.

5. The marking according to claim 1, wherein: The etching of the refractive film includes one or more of a dry etching process and a wet etching process.

6. The marking according to claim 1, wherein: The refractive film includes one or more of oxide, carbide, nitride and fluoride.

7. The marking according to claim 1, wherein: The thickness of the refractive film is about 500 angstroms to 3900 angstroms.

8. The marking according to claim 1, wherein: The dielectric substrate material includes one or more of silicon, germanium, titanium, doped silicon, doped germanium and doped titanium.

9. The marking according to claim 1, wherein: The thickness modulation amount of the thickness modulated film is about 5 nanometers to 390 nanometers.

10. The marking according to claim 1, wherein: The refractive material includes at least one of barium fluoride, calcium fluoride, lanthanum fluoride, magnesium fluoride, hafnium oxide, silicon dioxide, aluminum oxide or titanium nitride.

11. The marking according to claim 1, wherein: The marker is secured to a component used in a hot runner of a gas turbine engine.

12. A method comprising: fixing the marking of claim 1 to a component, wherein the refractive film has an identification pattern; and Match the marked identification pattern to the part.

13. The method according to claim 12, wherein: The recognition pattern is stable at temperatures between about -273.14°C and 1350°C.

14. The method according to claim 12, further comprising the steps of: maintaining a database of component patterns for the components; sensing a recognition pattern of a marking of a component; retrieving a part history from a part pattern database; and In response to sensing the identification pattern of the indicia of the component, a component pattern database is updated for the component.

15. The method according to claim 12, wherein: The marker is fixed to the component by at least one of electrodeposition, brazing, cladding, welding, spraying, coating and embedding.

16. The method of claim 12, further comprising securing a marker to a component used in a hot runner of a gas turbine engine.

17. The method of claim 16, further comprising coating the marking with a thermal barrier material.

18. The method of claim 17, further comprising coating the component with a thermal barrier material.

19. The method according to claim 12, wherein: The recognition pattern of the sensing mark includes at least one of optical, ultraviolet, infrared scanning and acoustic scanning.

20. The method according to claim 12, wherein: Sensing the marking includes visually inspecting the marking with a camera.

21. The method according to claim 12, wherein: The marking has a pattern traceable to an identification number.

22. The method according to claim 12, wherein: The identification pattern includes one or more of a barcode, a printed micro pattern and a QR code.

23. A method of making the marking of claim 1, the method comprising: etching the refractive film on the dielectric substrate material to obtain a thickness modulated film; coating a refractive material on a thickness modulated film to obtain a recognition pattern; Wherein the recognition pattern is stable at a temperature of about -273.14 degrees Celsius to about 1350 degrees Celsius for a period of at least 40 hours.

24. The method according to claim 23, wherein: The recognition pattern is stable at pressures ranging from about 1 microPascal (μPa) to about 100 gigapascals (GPa).

25. The method according to claim 23, wherein: The identification pattern includes at least one of a barcode, a printed micro pattern, and a QR code.

26. The method of claim 23, wherein: The etching of the refractive film is selected from at least one of a dry etching process and a wet etching process.

27. The method according to claim 23, wherein: The refractive film is selected from the group consisting of at least one of oxides, nitrides, and fluorides.

28. The method of claim 23, wherein: The refractive film has a thickness of about 50 angstroms to about 3900 angstroms.

29. The method of claim 23, wherein: The dielectric substrate material includes at least one of silicon, germanium, titanium, doped silicon, doped germanium, and doped titanium.

30. The method of claim 23, wherein: The thickness modulated film has a thickness modulation amount of about 5 nanometers to about 390 nanometers.

31. The method of claim 23, wherein: The refractive material includes at least one of barium fluoride, calcium fluoride, lanthanum fluoride, magnesium fluoride, hafnium oxide, silicon dioxide, aluminum oxide, and titanium nitride.

32. The method of claim 23, wherein: The dielectric base material is secured to a component used in a hot runner of a gas turbine engine.