High-precision radiator brazing tool

By designing high-precision radiator brazing tooling, using positioning components and fixed components to match the shape of the nozzle and runner, the problem of low accuracy of the existing tooling is solved, and high-precision radiator welding is achieved to meet mass production needs and simplify the process flow.

CN119658061APending Publication Date: 2025-03-21SHENZHEN FRD SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411993256.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-31
Publication Date
2025-03-21

AI Technical Summary

Technical Problem

The brazing tooling accuracy of existing radiators is not high, and cannot meet the radiator assembly requirements of special-shaped structures and the mass-production brazing needs of radiators with high accuracy requirements.

Method used

A high-precision radiator brazing tool is designed, including support components, fixing components and positioning components. The positioning components achieve the matching of the nozzle and the runner in the horizontal direction, and the fixing components achieve the matching of the nozzle and the runner in the vertical direction, ensuring the position accuracy between the nozzle and the runner during welding processing.

Benefits of technology

It realizes the high precision of welding processing in the case of irregularly shaped nozzles and runners, and meets the production requirements of radiator with high dimensional accuracy requirements, and simplifies the process flow and reduces the production cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119658061A_ABST
    Figure CN119658061A_ABST
Patent Text Reader

Abstract

The invention discloses a high-precision radiator brazing tool which is characterized in that a radiator comprises a water nozzle and a flow channel which are fixed through brazing, the high-precision radiator brazing tool comprises a supporting assembly, a fixing assembly and a positioning assembly, and the fixing assembly and the positioning assembly are fixed to the supporting assembly; wherein the water nozzle and the flow channel are matched in the horizontal direction through the positioning assembly, and then the water nozzle and the flow channel are matched in the vertical direction through the fixing assembly, so that the position precision between the water nozzle and the flow channel in the welding machining process can still be guaranteed under the condition that the water nozzle and the flow channel are in irregular shapes; after all parts of a product are positioned and clamped, the radiator meeting the requirement for high dimensional accuracy can be welded.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of brazing, and in particular to a high-precision radiator brazing tool. Background Art

[0002] The car radiator includes a core and water chambers on both sides of the core. The core is welded by a water pipe, a main plate and a heat dissipation belt. Before welding the core, the core needs to be plugged and assembled. After the assembly is completed, the two sides of the core are clamped and positioned by a brazing tool. Brazing refers to a welding method in which the brazing material below the melting point of the weldment and the weldment are heated to the melting temperature of the brazing material at the same time, and the gap between the solid workpieces is filled with liquid brazing material to connect the metals. When brazing the core, the core is generally clamped and fixed by a tool to facilitate the brazing of the core.

[0003] Conventional brazing tooling in the prior art can currently ensure the following shape errors: 1) the radiator diagonal error is more than 1 mm; 2) the radiator height error is more than 1 mm; 3) the radiator length error is more than 1 mm.

[0004] The above are only the appearance errors that can be directly detected after the radiator brazing is completed. The radiator brazed by conventional tooling has certain rules: First, the radiator has a relatively regular appearance, usually a three-dimensional regular structure composed of six planes, so the usage of conventional assembly tooling is relatively simple, and conventional brazing tooling has the following problems: 1) The accuracy is not high; 2) It cannot meet the assembly requirements of radiators with special-shaped structures; 3) It cannot meet the mass production brazing requirements of radiators with high precision requirements;

[0005] Therefore, when the actual production of high-precision mass production brazing tooling requires irregular shapes, high tooling flatness and verticality errors, and upper and lower plane parallelism and other technical indicators, the current conventional radiator brazing tooling is unable to meet and achieve its high technical requirements.

[0006] In view of this, the high-precision heat sink brazing tooling that can be mass-produced still needs to be further improved. Summary of the invention

[0007] In view of the deficiencies in the prior art, the present invention proposes a high-precision radiator brazing tooling, which solves the technical problems that the existing radiator brazing tooling has low precision, cannot meet the assembly requirements of radiators with special-shaped structures, and cannot meet the mass production brazing requirements of radiators with high precision requirements.

[0008] The technical solution of the present invention is achieved in this way:

[0009] The present invention provides a high-precision radiator brazing tool, wherein the radiator comprises a water nozzle and a flow channel fixed by brazing, wherein the high-precision radiator brazing tool comprises a supporting component, a fixing component and a positioning component, wherein the fixing component and the positioning component are fixed on the supporting component;

[0010] Among them, the water nozzle and the flow channel are clamped on the positioning component to achieve the matching of the water nozzle and the flow channel in the horizontal direction, and the fixing component cooperates with the supporting component to fix the water nozzle and the flow channel on the supporting component to achieve the matching of the water nozzle and the flow channel in the vertical direction.

[0011] In one embodiment, the fixing assembly and the positioning assembly are positioned and welded on the supporting assembly, and are subjected to a heat treatment at 600° C. for 12 hours after welding to ensure the matching accuracy of the water nozzle and the flow channel.

[0012] In one embodiment, the positioning assembly comprises:

[0013] A faucet clamp, which is fixed on the supporting assembly and clamps the faucet to achieve positioning and fixing of the faucet;

[0014] A flow channel clamp is fixed on the support assembly and clamps the flow channel to achieve positioning and fixation of the flow channel.

[0015] In one embodiment, the faucet clamp comprises:

[0016] A fixing plate, the fixing plate being vertically welded and fixed on the supporting assembly;

[0017] A movable plate is vertically arranged on the support assembly and relative to the fixed plate. The movable plate can slide on the support assembly relative to the fixed plate to clamp the water nozzle, thereby achieving horizontal positioning and fixation of the water nozzle.

[0018] In one embodiment, the flow channel clamp comprises:

[0019] A fixing block, the fixing block is welded and fixed on the supporting assembly;

[0020] A clamping block, the clamping block is arranged relative to the fixing block and is slidably fixed on the supporting assembly;

[0021] A push rod is arranged on the other side of the clamping block relative to the fixing block, and the distance between the clamping block and the fixing block is adjusted by the push rod to clamp the flow channel, thereby realizing the positioning and fixing of the flow channel in the horizontal direction.

[0022] In one embodiment, the fixing assembly comprises:

[0023] A plurality of fixing seats, which are welded and fixed on the supporting assembly and symmetrically arranged around the flow channel, and the top of the fixing seat is provided with a pin hole;

[0024] A pressing plate, the pressing plate is arranged on the other side of the flow channel relative to the support assembly, pressing the flow channel onto the support assembly;

[0025] A plurality of C-shaped clips are arranged corresponding to the fixing seat, the C-shaped clips are fixed to the fixing seat by pins, and the pressure plate, the flow channel and the fixing seat are clamped to clamp the flow channel between the fixing seat and the pressure plate, so as to realize the positioning and fixation of the flow channel in the vertical direction.

[0026] In one embodiment, the top surfaces of several of the fixing seats and the top surface of the fixing block are located in the same plane, and the flow channel is placed on the top surfaces of the fixing seats and the fixing block on one side opposite to the supporting assembly to ensure that the flow channel matches the faucet in the vertical direction.

[0027] In one embodiment, the fixing assembly includes four symmetrically arranged fixing seats, and the top surfaces of the four fixing seats are equal to the top surface of the fixing block and are arranged corresponding to the height of the water nozzle, so that the top surfaces of the four fixing seats and the top surface of the fixing block are located in the same plane, and it is ensured that after the flow channel is placed on the fixing seat and the fixing block, the flow channel matches the water nozzle in the vertical direction.

[0028] In one embodiment, the pressing plate comprises:

[0029] A graphite block, wherein the graphite block is arranged above the flow channel to provide a heat conduction function for the flow channel during the brazing process;

[0030] A stainless steel pressing plate is arranged above the graphite pressing block, the pin passes through the stainless steel pressing plate, and cooperates with the C-type clamp to fix the stainless steel pressing plate, the graphite pressing block and the flow channel on the fixing seat to ensure the flatness of the flow channel.

[0031] In one embodiment, the support assembly further comprises a graphite pad, which is fixed on the support assembly and disposed below the water nozzle and the flow channel to provide a heat conduction function for the water nozzle and the flow channel during the brazing process.

[0032] The high-precision heat sink brazing tool proposed in the present invention has the following beneficial effects compared with the prior art:

[0033] The present invention respectively arranges a fixing component and a positioning component on the brazing tool, wherein the positioning component realizes the matching of the water nozzle and the flow channel in the horizontal direction, and then the fixing component realizes the matching of the water nozzle and the flow channel in the vertical direction. Thus, when the water nozzle and the flow channel are of irregular shapes, the position accuracy between the water nozzle and the flow channel during the welding process can still be guaranteed. After the various components of the product are positioned and clamped, a radiator that meets high dimensional accuracy requirements can be welded. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0035] Figure 1 This is a schematic diagram of the explosion and decomposition of the high-precision heat sink brazing tooling of the present invention;

[0036] Figure 2 It is a schematic diagram of the base frame in the high-precision radiator brazing tooling of the present invention;

[0037] Figure 3 A top view of the high-precision heat sink brazing tooling of the present invention;

[0038] Figure 4 It is a left view of the high-precision heat sink brazing tooling of the present invention;

[0039] 100-support assembly; 110-graphite pad; 200-positioning assembly; 210-faucet clamp; 211-fixed plate; 212-movable plate; 213-movable pin; 220-flow channel clamp; 221-fixed block; 222-clamping block; 223-push rod; 300-fixing assembly; 310-fixing seat; 311-pin hole; 320-pressure plate; 321-graphite pressure block; 322-stainless steel pressure plate; 330-C-type clamp; 331-pin; 400-faucet; 500-flow channel. DETAILED DESCRIPTION

[0040] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0041] It should be understood that the terms used in this description of the embodiments of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the embodiments of the present invention. As used in the description of the embodiments of the present invention and the appended claims, unless the context clearly indicates otherwise, the singular forms of "a", "an" and "the" are intended to include plural forms.

[0042] In order to ensure the position accuracy between the water nozzle and the flow channel during the welding process when the water nozzle and the flow channel of the radiator are irregular in shape, the present invention provides a high-precision radiator brazing tool, the radiator includes a water nozzle and a flow channel fixed by brazing, wherein, Figure 1 As shown, the high-precision heat sink brazing tooling includes a support assembly 100, a fixing assembly 300 and a positioning assembly 200, wherein the fixing assembly 300 and the positioning assembly 200 are fixed on the support assembly 100. The water nozzle 400 and the flow channel 500 are clamped on the positioning assembly 200 to achieve the matching of the water nozzle 400 and the flow channel 500 in the horizontal direction, and the fixing assembly 300 cooperates with the support assembly 100 to fix the water nozzle 400 and the flow channel 500 on the support assembly 100 to achieve the matching of the water nozzle 400 and the flow channel 500 in the vertical direction.

[0043] In one embodiment, the fixing assembly 300 and the positioning assembly 200 are positioned and welded on the supporting assembly 100 , and are subjected to a heat treatment at 600° C. for 12 hours after welding to ensure the matching accuracy of the faucet 400 and the flow channel 500 .

[0044] In one embodiment, if Figure 3 As shown, the positioning assembly 200 includes a faucet clamp 210 and a flow channel clamp 220. The faucet clamp 210 is fixed to the support assembly 100 and clamps the faucet 400 to achieve positioning and fixing of the faucet 400; the flow channel clamp 220 is fixed to the support assembly 100 and clamps the flow channel 500 to achieve positioning and fixing of the flow channel 500.

[0045] In one embodiment, the faucet clamp 210 includes a fixed plate 211 and a movable plate 212, wherein the fixed plate 211 is vertically welded and fixed on the support assembly 100; the movable plate 212 is vertically arranged on the support assembly 100 and is arranged relative to the fixed plate 211, and the movable plate 212 can slide on the support assembly 100 relative to the fixed plate 211 to clamp the faucet 400, thereby realizing the positioning and fixation of the faucet 400 in the horizontal direction.

[0046] In one embodiment, if Figure 1As shown, the flow channel clamp 220 includes a fixing block 221, a clamping block 222 and a push rod 223. The fixing block 221 is welded and fixed on the support assembly 100; the clamping block 222 is arranged relative to the fixing block 221 and slidably fixed on the support assembly 100; the push rod 223 is arranged on the other side of the clamping block 222 relative to the fixing block 221, and the distance between the clamping block 222 and the fixing block 221 is adjusted by the push rod 223 to clamp the flow channel 500, so as to realize the positioning and fixing of the flow channel 500 in the horizontal direction.

[0047] In one embodiment, if Figure 1 As shown, the fixing assembly 300 includes a plurality of fixing seats 310, a pressing plate 320 and a C-type clamp 330. The fixing seats 310 are welded and fixed on the supporting assembly 100 and are symmetrically arranged around the flow channel 500. A pin hole 311 is provided on the top of the fixing seat 310. The pressing plate 320 is arranged on the other side of the flow channel 500 relative to the supporting assembly 100 to press the flow channel 500 onto the supporting assembly 100. The C-type clamp 330 is arranged corresponding to the fixing seat 310. The C-type clamp 330 is fixed to the fixing seat 310 by the cooperation of the pin 331 and the pin hole 311, and the pressing plate 320, the flow channel 500 and the fixing seat 310 are clamped to clamp the flow channel 500 between the fixing seat 310 and the pressing plate 320, so as to realize the positioning and fixing of the flow channel 500 in the vertical direction.

[0048] In one embodiment, the top surfaces of several of the fixing seats 310 and the top surface of the fixing block 221 are located in the same plane, and the flow channel 500 is placed on the top surfaces of the fixing seat 310 and the fixing block 221 relative to a side of the support assembly 100 to ensure that the flow channel 500 matches the faucet 400 in the vertical direction.

[0049] In one embodiment, if Figure 2 As shown, the fixing assembly 300 includes four symmetrically arranged fixing seats 310, and the top surfaces of the four fixing seats 310 are equal to the top surface height of the fixing block 221 and are arranged corresponding to the height of the water nozzle 400, so that the top surfaces of the four fixing seats 310 and the top surface of the fixing block 221 are located in the same plane, and it is ensured that after the flow channel 500 is placed on the fixing seat 310 and the fixing block 221, the flow channel 500 matches the water nozzle 400 in the vertical direction.

[0050] In one embodiment, if Figure 1 and Figure 4As shown, the pressing plate 320 includes a graphite pressing block 321 and a stainless steel pressing plate 322, wherein the graphite pressing block 321 is arranged above the flow channel 500 to provide a heat conduction function for the flow channel 500 during the brazing process; the stainless steel pressing plate 322 is arranged above the graphite pressing block 321, and the pin 331 passes through the stainless steel pressing plate 322, and cooperates with the C-type clamp 330 to fix the stainless steel pressing plate 322, the graphite pressing block 321 and the flow channel 500 on the fixing seat 310 to ensure the flatness of the flow channel 500.

[0051] In one embodiment, if Figure 1 and Figure 4 As shown, the support assembly 100 further includes a graphite pad 110, which is fixed on the support assembly 100 and disposed below the water nozzle 400 and the flow channel 500 to provide a heat conduction function for the water nozzle 400 and the flow channel 500 during the brazing process.

[0052] The following is a description of a high-precision heat sink brazing tool in one embodiment of the present invention with reference to the accompanying drawings.

[0053] like Figure 1 As shown, the high-precision radiator brazing fixture includes a support component 100, a positioning component 200 and a fixing component 300. By respectively arranging the fixing component 300 and the positioning component 200 on the brazing fixture, the positioning component 200 realizes the matching of the water nozzle 400 and the flow channel 500 in the horizontal direction, and then the fixing component 300 realizes the matching of the water nozzle 400 and the flow channel 500 in the vertical direction. Therefore, when the water nozzle and the flow channel in the radiator are irregular shapes, the position accuracy between the water nozzle and the flow channel during the welding process can still be guaranteed. After the positioning and clamping of each component of the product, a radiator that meets the high dimensional accuracy requirements can be welded. Specifically, the flatness of the flow channel can meet the requirement of not more than 0.2mm, and the distance tolerance between the flow channel and the water nozzle can meet the requirement of 0-0.3mm.

[0054] From a process perspective, the high-precision radiator brazing tooling needs to arrange regular (one month) re-measurement of dimensions to prevent deformation caused by long-term thermal expansion and contraction in the chain furnace. The corresponding components can be reworked after mechanical processing to ensure the consistency of the welded radiator products and meet the relevant requirements of existing radiator products for high-precision technical indicators such as flatness, verticality, parallelism and coplanarity, namely: 1) The radiator diagonal error is less than 1mm; 2) The radiator height error is less than 1mm; 3) The radiator length error is less than 1mm; at the same time, the high-precision radiator brazing tooling only needs one welding process to obtain the radiator product, which greatly simplifies the existing process flow and reduces production costs.

[0055] In this embodiment, the positioning component 200 and the fixing component 300 are fixed to the support component 100 by positioning welding, and after the welding process, the high-precision radiator brazing tooling is placed in a brazing furnace for heat treatment at 600°C for 12 hours to ensure subsequent processing accuracy.

[0056] Furthermore, if Figure 4 As shown, a graphite pad 110 is provided on the support assembly 100 to provide a heat conduction function for the water nozzle 400 and the flow channel 500 during the brazing process to avoid heat accumulation affecting the processing accuracy.

[0057] Furthermore, if Figure 1 and Figure 3 As shown, the positioning assembly 200 is fixedly mounted on the support assembly 100, wherein the positioning assembly 200 includes a faucet clamp 210 corresponding to the faucet 400 and a flow channel clamp 220 corresponding to the flow channel 500. Figure 3 and Figure 4 As shown, the faucet clamp 210 includes a fixed plate 211, a movable plate 212 and a movable pin 213, wherein the fixed plate 211 is vertically fixed on the support assembly 100, and the movable plate 212 can be moved relative to the fixed plate 211 through the movable pin 213 to adjust the distance between the movable plate 212 and the fixed plate 211, thereby clamping and fixing the faucet 400, ensuring the position of the faucet 400 in the horizontal direction, and ensuring the matching accuracy between the faucet 400 and the flow channel 500 in the horizontal plane.

[0058] Further, the flow channel clamp 220 includes a fixed block 221, a clamping block 222 and a push rod 223, wherein the fixed block 221 and the clamping block 222 are both arranged in a long strip shape to correspond to the two opposite sides of the flow channel 500. The fixed block 221 is fixed to the support assembly 100, and the clamping block 222 can move relative to the fixed block 221 along the support assembly 100 to adjust the distance between the fixed block 221 and the clamping block 222, so as to clamp and fix the flow channel 500. Specifically, the fixed block 221 and the clamping block 222 are arranged in parallel to achieve stable clamping of the flow channel 500. Furthermore, the push rod 223 is provided on the side of the clamping block 222 away from the fixing block 221, and three push rods 223 are provided in parallel, corresponding to the two ends and the middle position of the clamping block 222 respectively, and the distance between the clamping block 222 and the fixing block 221 is adjusted by the push rod 223 to achieve the clamping and fixing of the flow channel 500. Specifically, the posture of the clamping block 222 is adjusted by the three push rods 223 to match the corresponding flow channel shape, thereby achieving stable clamping of the flow channel 500, ensuring the position of the flow channel 500 in the horizontal direction, and ensuring the matching accuracy between the flow channel 500 and the faucet 400 on the horizontal plane.

[0059] Furthermore, if Figure 1 and Figure 3 As shown, the fixing assembly 300 is fixed on the surface of the supporting assembly 100 and is arranged corresponding to the flow channel 500. Specifically, the fixing assembly 300 includes a fixing seat 310, a pressing plate 320 and a C-type clamp 330 to cooperate to achieve clamping and fixing of the flow channel 500. Figure 2 and Figure 3 As shown, there are four fixing seats 310, and the fixing seats 310 are symmetrically arranged on both sides of the flow channel 500 in groups of two, and a horizontal plane is formed by matching the four fixing seats 310 and the fixing block 221 to ensure the height of the flow channel 500 in the vertical direction. Specifically, the top surfaces of the four fixing seats 310 and the top surface of the fixing block 221 are at the same height and fall on the same plane, and the heights of the fixing seats 310 and the fixing block 221 match the height setting of the water nozzle 400, so as to ensure that after the flow channel 500 is placed on the fixing seats 310 and the fixing block 221, the flow channel 500 matches the height setting of the water nozzle 400, ensuring the matching accuracy of the flow channel 500 and the water nozzle 400 in the vertical direction, thereby ensuring the accuracy of the final brazing effect.

[0060] Furthermore, if Figure 1 and Figure 2As shown, a pin hole 311 is provided on the top surface of the fixing seat 310, and the C-type clamp 330 is fixed to the fixing seat 310 by the pin 331 cooperating with the pin hole 311. Further, the C-type clamp 330 clamps the pressing plate 320 and the flow channel 500, and the pin 331 passes through both ends of the C-type clamp 330 to fix the pressing plate 320 and the flow channel 500 to the fixing seat 310, thereby ensuring the flatness of the flow channel 500 and the processing accuracy of the flow channel 500 and the faucet 400 during the brazing process.

[0061] Specifically, Figure 3 and Figure 4 As shown, the pressing plate 320 includes a graphite pressing block 321 and a stainless steel pressing plate 322, wherein the graphite pressing block 321 is placed on the flow channel 500, and the stainless steel pressing plate 322 is arranged on the graphite pressing block 321, and the pin 331 passes through the stainless steel pressing plate 322 to fix the graphite pressing block 321 and the flow channel 500 in the C-type clamp 330 and clamp them, thereby ensuring the flatness of the flow channel 500.

[0062] Specifically, through the arrangement of the fixing assembly 300 and the positioning assembly 200, the high-precision radiator brazing fixture in this embodiment can achieve a flatness of less than 0.2 mm and a distance tolerance of 0-0.3 mm between the nozzle and the flow channel. Compared with the existing radiator brazing fixture, the addition of heat treatment can effectively ensure the reliability of the stainless steel bracket and enhance the performance characteristics of the material, and can also ensure that the fixture does not deform or slightly deforms after multiple brazings, so as not to affect the precision requirements of the finished product after brazing.

[0063] The present invention provides a high-precision radiator brazing tool. The stainless steel pipe is positioned by the tool and then welded. The stainless steel frame is heat-treated to enhance the material strength and reduce the deformation caused by thermal expansion and contraction. The position accuracy is ensured by machining. After the various components of the product are positioned and clamped, a brazing quality that meets the high dimensional accuracy requirements of the product can be welded.

[0064] The high-precision radiator brazing tooling provided by the present invention will undergo deformation due to thermal expansion and contraction in the furnace for a long time, so it is necessary to remeasure the dimensions once a month. After machining and reworking the corresponding parts, the consistency of the welded products can be guaranteed, meeting the high-precision technical indicators requirements of the entire product for flatness, verticality, parallelism, coplanarity, etc.

[0065] In summary, the present invention discloses a high-precision radiator brazing tool, the radiator includes a water nozzle and a flow channel fixed by brazing, wherein the high-precision radiator brazing tool includes a supporting component, a fixing component and a positioning component, the fixing component and the positioning component are fixed on the supporting component; wherein the water nozzle and the flow channel are clamped on the positioning component to achieve the matching of the water nozzle and the flow channel in the horizontal direction, and the fixing component cooperates with the supporting component to fix the water nozzle and the flow channel on the supporting component to achieve the matching of the water nozzle and the flow channel in the vertical direction. By respectively arranging the fixing component and the positioning component on the brazing tool, the matching of the water nozzle and the flow channel in the horizontal direction is achieved by the positioning component, and then the matching of the water nozzle and the flow channel in the vertical direction is achieved by the fixing component, so that when the water nozzle and the flow channel are irregular shapes, the position accuracy between the water nozzle and the flow channel during the welding process can still be guaranteed, and after the positioning and clamping of the various components of the product, a radiator that meets the high dimensional accuracy requirements can be welded.

[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A high-precision radiator brazing tool, the radiator includes a water nozzle and a flow channel fixed by brazing, characterized in that: The high-precision heat sink brazing tooling comprises a supporting component, a fixing component and a positioning component, wherein the fixing component and the positioning component are fixed on the supporting component; Among them, the water nozzle and the flow channel are clamped on the positioning component to achieve the matching of the water nozzle and the flow channel in the horizontal direction, and the fixing component cooperates with the supporting component to fix the water nozzle and the flow channel on the supporting component to achieve the matching of the water nozzle and the flow channel in the vertical direction.

2. The high-precision heat sink brazing tool as claimed in claim 1, characterized in that: The fixing assembly and the positioning assembly are positioned and welded on the supporting assembly, and are subjected to a heat treatment at 600° C. for 12 hours after welding to ensure the matching accuracy of the water nozzle and the flow channel.

3. The high-precision heat sink brazing tool as claimed in claim 2, characterized in that: The positioning component comprises: A faucet clamp, which is fixed on the supporting assembly and clamps the faucet to achieve positioning and fixing of the faucet; A flow channel clamp is fixed on the support assembly and clamps the flow channel to achieve positioning and fixation of the flow channel.

4. The high-precision heat sink brazing tool as claimed in claim 3, characterized in that: The faucet clamp comprises: A fixing plate, the fixing plate being vertically welded and fixed on the supporting assembly; A movable plate is vertically arranged on the support assembly and relative to the fixed plate. The movable plate can slide on the support assembly relative to the fixed plate to clamp the water nozzle, thereby achieving horizontal positioning and fixation of the water nozzle.

5. The high-precision heat sink brazing tool as claimed in claim 3, characterized in that: The flow channel clamp comprises: A fixing block, the fixing block is welded and fixed on the supporting assembly; A clamping block, the clamping block is arranged relative to the fixing block and is slidably fixed on the supporting assembly; A push rod is arranged on the other side of the clamping block relative to the fixing block, and the distance between the clamping block and the fixing block is adjusted by the push rod to clamp the flow channel, thereby realizing the positioning and fixing of the flow channel in the horizontal direction.

6. The high-precision heat sink brazing tool as claimed in claim 5, characterized in that: The fixing assembly comprises: A plurality of fixing seats, which are welded and fixed on the supporting assembly and symmetrically arranged around the flow channel, and the top of the fixing seat is provided with a pin hole; A pressing plate, the pressing plate is arranged on the other side of the flow channel relative to the support assembly, pressing the flow channel onto the support assembly; A plurality of C-shaped clips are arranged corresponding to the fixing seat, the C-shaped clips are fixed to the fixing seat by pins, and the pressure plate, the flow channel and the fixing seat are clamped to clamp the flow channel between the fixing seat and the pressure plate, so as to realize the positioning and fixation of the flow channel in the vertical direction.

7. The high-precision heat sink brazing tool as claimed in claim 6, characterized in that: The top surfaces of several of the fixing seats and the top surface of the fixing block are located in the same plane, and the flow channel is placed on the top surfaces of the fixing seats and the fixing block on one side opposite to the support assembly to ensure that the flow channel matches the faucet in the vertical direction.

8. The high-precision heat sink brazing tool as claimed in claim 7, characterized in that: The fixing assembly includes four symmetrically arranged fixing seats, and the top surfaces of the four fixing seats are equal to the top surface of the fixing block and are arranged corresponding to the height of the water nozzle, so that the top surfaces of the four fixing seats and the top surface of the fixing block are located in the same plane, and it is ensured that after the flow channel is placed on the fixing seat and the fixing block, the flow channel matches the water nozzle in the vertical direction.

9. The high-precision heat sink brazing tool as claimed in claim 6, characterized in that: The pressing plate comprises: A graphite block, wherein the graphite block is arranged above the flow channel to provide a heat conduction function for the flow channel during the brazing process; A stainless steel pressing plate is arranged above the graphite pressing block, the pin passes through the stainless steel pressing plate, and cooperates with the C-type clamp to fix the stainless steel pressing plate, the graphite pressing block and the flow channel on the fixing seat to ensure the flatness of the flow channel.

10. The high-precision heat sink brazing tool as claimed in claim 1, characterized in that: The support assembly further comprises a graphite pad, which is fixed on the support assembly and arranged below the water nozzle and the flow channel to provide a heat conduction function for the water nozzle and the flow channel during the brazing process.