Colorful rubbing paper-plastic texture picture adopting novel plastic paper process
By adding water-based shaping curing agent to the paper and using silicone and polyacrylate blend emulsion for modification, the problem of traditional rubbing paper lacking waterproofness and three-dimensional effect is solved, and a harder and better waterproofing effect is achieved.
Patent Information
- Application Number
- CN202311358354.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-19
- Publication Date
- 2025-04-22
AI Technical Summary
The rice paper used in traditional rubbing paintings is highly absorbent but lacks waterproofness, resulting in poor rubbing effect, single three-dimensional effect and easy to wear and deform.
The new plastic paper process is adopted to increase the surface strength, wear resistance and water resistance of the paper by adding water-based shaping curing agent to the paper and physically modifying it with silicone and polyacrylate blend emulsion.
The hard and waterproof performance of the paper is improved, so that the rubbings printed have a hard and waterproof effect, good waterproof performance and a long storage service life, while enhancing the three-dimensional effect and multi-layer color texture.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of decorative paintings, and in particular discloses a color rubbing paper plastic texture painting using a novel paper plastic process. Background Art
[0002] The traditional method of rubbing woodblock prints is to spread rubbing paper flat on the engraved block, wet it, brush it with white hyacinth water, and then gently beat it with a brush so that the image is clearly visible on the back of the paper, and then use a homemade rubbing bag to add color.
[0003] Since the paper material currently required for rubbing paintings is mostly rice paper, which is mainly made of plant fiber and has high water absorption, is not waterproof, and is easily corrupted after being soaked in water. Although the rubbing paintings produced have undulations, the three-dimensional effect is not strong, the three-dimensional height is single, and the surface texture is easily worn and deformed during extrusion and friction, the present invention proposes a color rubbing paper plastic texture painting using a new plastic paper process. Summary of the invention
[0004] The present invention is designed to address the deficiencies of the prior art and provides a color rubbing paper plastic texture painting using a new paper plastic process.
[0005] The technical solution adopted by the present invention to solve the above problems is as follows:
[0006] The present invention provides a color rubbing paper plastic texture painting using a novel paper plastic process, comprising the following specific steps:
[0007] S1. Papermaking: adding a water-based plastic curing agent into the paper to shape it and obtain a wet stretchable plastic material;
[0008] S2, paper processing: using polyacrylate emulsion as a stiffening agent, adding silicone solution and magnesium chloride to blend for physical modification, forming silicone and polyacrylate blended emulsion, spraying the emulsion on the surface of the paper in S1, increasing its surface strength, wear resistance, solvent resistance and improving the water resistance of the paper, thereby obtaining drawing paper;
[0009] S3, plate making: Use plastic paste to draw the texture template and place it in a ventilated and cool place to dry for 30-70 hours;
[0010] S4, core creasing: spray the drawing paper obtained in S2 to make the paper reach 40-80% humidity, gently hammer with a brush to make the wet paper adhere to the texture template, and continue to hammer out three-dimensional texture with concave and convex texture;
[0011] S5, picture making: after the wet paper in step S4 is slightly dry, a proper amount of ink or cinnabar is dipped into a puff, applied evenly on the puff surface, and lightly patted on the paper, and the picture is modified by dyeing, spraying, etc. to form a rubbing;
[0012] S6, picture modification: repeat step S5, tear the processed paper into small pieces to modify the picture, and repeatedly paste the pieces to obtain the picture core;
[0013] S7. Drying of the painting core: Place the modified painting core in an environment ≥28℃ and dry it for 1-3 hours to avoid bulging of the paper during drying.
[0014] Furthermore, the paper in S1 is Yunlong paper.
[0015] Furthermore, in S3, a plastic paste is used to draw a texture template, which is placed in a ventilated and cool place to dry for 48 hours.
[0016] Furthermore, in S4, the humidity of the paper reaches 60%.
[0017] Furthermore, the drying time in S7 is 2 hours.
[0018] In summary, the beneficial effects of the present invention are as follows: the technical scheme provided by the present invention improves the performance of paper, avoiding the shortcomings of poor waterproofness and poor rubbing effect of traditional rice paper; and the silicone and polyacrylate blended emulsion is sprayed on the surface of the paper to increase its surface strength, wear resistance, and solvent resistance, and improve the water resistance of the paper. The prepared paper also has excellent stiffening and waterproof effects, so that the rubbings prepared by rubbing the paper have strong stiffening effect, good waterproof performance, and long storage life; in addition, the technical scheme innovates the traditional rubbing process, making up for the shortcomings of single rubbing color and weak three-dimensional effect; specially treated paper is used for rubbing to make three-dimensional patterns, and a variety of color spray painting methods are used, and multiple layers of color texture are attached to form a finished decorative painting, and its production effect is more three-dimensional and beautiful, which can be derived and applied to a variety of picture innovations. DETAILED DESCRIPTION
[0019] The following specifically illustrates the implementation modes of the present invention, which does not constitute a limitation on the patent protection scope of the present invention.
[0020] The technical solution adopted by the present invention to solve the above problems is as follows:
[0021] A color rubbing paper plastic texture painting using a new paper plastic process includes the following specific steps:
[0022] S1. Papermaking: Add water-based plastic curing agent to the paper for shaping to obtain wet stretchable plastic material, wherein the paper color is pure color, and pigments can also be added to it; after air drying, various patterns can be sprayed, and the tension of the color and the three-dimensional sense of the structure are very prominent, and the style has a certain plasticity;
[0023] S2, paper processing: using polyacrylate emulsion as a stiffening agent, adding silicone solution and magnesium chloride to blend for physical modification, forming silicone and polyacrylate blended emulsion, spraying the emulsion on the surface of the paper in S1, increasing its surface strength, wear resistance, solvent resistance and improving the water resistance of the paper, thereby obtaining drawing paper;
[0024] S3, plate making: Use plastic paste to draw the texture template and place it in a ventilated and cool place to dry for 30-70 hours;
[0025] S4, core creasing: spray the drawing paper obtained in S2 to make the paper reach 40-80% humidity, gently hammer with a brush to make the wet paper adhere to the texture template, and continue to hammer out three-dimensional texture with concave and convex texture;
[0026] S5, picture making: after the wet paper in step S4 is slightly dry, a proper amount of ink or cinnabar is dipped into a puff, applied evenly on the puff surface, and lightly patted on the paper, and the picture is modified by dyeing, spraying, etc. to form a rubbing;
[0027] S6, picture modification: repeat step S5, tear the processed paper into small pieces to modify the picture, and repeatedly paste the pieces several times, and use methods such as pasting foil and adding brushstrokes to increase the three-dimensional layering of the picture to obtain the picture core;
[0028] S7. Drying of the painting core: Place the modified painting core in an environment ≥28℃ and dry it for 1-3 hours to avoid bulging of the paper during drying.
[0029] As a preferred implementation of this embodiment, the paper in S1 is Yunlong paper.
[0030] Preferably, the number of layers of Yunlong paper is three.
[0031] Specifically, in S3, a plastic paste is used to draw a texture template, and the template is placed in a ventilated and cool place to dry for 48 hours.
[0032] As another preferred implementation of this embodiment, the paper reaches 60% humidity in S4.
[0033] In addition, the drying time in S7 is 2 hours.
[0034] From the above description, it can be seen that the above embodiments of the present invention achieve the following technical effects:
[0035] The technical solution provided by the present invention improves the performance of paper, avoiding the shortcomings of poor waterproofness and poor rubbing effect of traditional rice paper; and a silicone and polyacrylate blended emulsion is sprayed on the surface of the paper to increase its surface strength, wear resistance, and solvent resistance and improve the water resistance of the paper. The prepared paper also has excellent stiffening and waterproof effects, so that the rubbings prepared by rubbing the paper have strong stiffening effect, good waterproof performance and long storage life; in addition, the technical solution innovates the traditional rubbing process to make up for the shortcomings of single rubbing color and weak three-dimensional effect; specially treated paper is used for rubbing to make three-dimensional patterns, and a multi-color spray painting method is used to form a finished decorative painting with multiple layers of color texture. The production effect is more three-dimensional and beautiful, and can be derived and applied to a variety of picture innovations.
[0036] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited to the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications that do not violate the spirit and principles of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. A color rubbing paper plastic texture painting using a new paper plastic process, characterized in that: The specific steps include: S1. Papermaking: adding a water-based plastic curing agent into the paper to shape it and obtain a wet stretchable plastic material; S2, paper processing: using polyacrylate emulsion as a stiffening agent, adding silicone solution and magnesium chloride to blend for physical modification, forming silicone and polyacrylate blended emulsion, spraying the emulsion on the surface of the paper in S1, increasing its surface strength, wear resistance, solvent resistance and improving the water resistance of the paper, thereby obtaining drawing paper; S3, plate making: Use plastic paste to draw the texture template and place it in a ventilated and cool place to dry for 30-70 hours; S4, core creasing: spray the drawing paper obtained in S2 to make the paper reach 40-80% humidity, gently hammer with a brush to make the wet paper adhere to the texture template, and continue to hammer out three-dimensional texture with concave and convex texture; S5, picture making: after the wet paper in step S4 is slightly dry, a proper amount of ink or cinnabar is dipped into a puff, applied evenly on the puff surface, and lightly patted on the paper, and the picture is modified by dyeing, spraying, etc. to form a rubbing; S6, picture modification: repeat step S5, tear the processed paper into small pieces to modify the picture, and repeatedly paste the pieces to obtain the picture core; S7. Drying of the painting core: Place the modified painting core in an environment ≥28℃ and dry it for 1-3 hours to avoid bulging of the paper during drying.
2. The color rubbing paper plastic texture painting using the new paper plastic process according to claim 1, characterized in that: The paper in S1 is Yunlong paper.
3. The color rubbing paper plastic texture painting using the new paper plastic process according to claim 1, characterized in that: In the S3, a plastic paste is used to draw a texture template, which is placed in a ventilated and cool place to dry for 48 hours.
4. The color rubbing paper plastic texture painting using the new paper plastic process according to claim 1, characterized in that: In S4, the paper reaches 60% humidity.
5. The color rubbing paper plastic texture painting using the new paper plastic process according to claim 1, characterized in that: The drying time in S7 is 2 hours.
Citation Information
Patent Citations
Method for manufacturing three-dimensional craft painting
CN103407319A
Preparation method for negative ion organosilicon modified polyacrylate paper reinforcing agent
CN103554345A
Environmentally-friendly cationic polyacrylate, and preparation method and application thereof
CN103993502A
Production method of three-dimensional simulation oil painting
CN104589898A
Fabrication process for high relief rubbing with stereoscopic effect
CN107175988A