Processing device and method for anti-corrosion coating of table top side plate
By designing a ceramic anticorrosion coating processing device that uses a driving motor and a ball screw, the problem of difficulty in mixing high-viscosity ceramic raw materials in existing equipment is solved, and the full mixing of ceramic anticorrosion coatings is achieved, and the performance and quality of the coating are improved.
Patent Information
- Application Number
- CN202510280809.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-11
- Publication Date
- 2025-05-02
AI Technical Summary
It is difficult for existing mixing equipment to fully mix high viscosity and high density raw materials of ceramic anticorrosion coatings, resulting in slurry delamination, agglomeration or local concentration uneven, affecting the performance and quality of the coating.
A processing device for anti-corrosion coating on the side panel of the desktop was designed. The ball screw was driven to rotate by a driving motor, and the bearing plate slid back and forth along the guide rail, so that the raw materials of the ceramic anti-corrosion coating repeatedly impacted in the mixing box through inertia, achieving full mixing.
It effectively avoids precipitation or agglomeration during the mixing process, ensures full mixing of ceramic anticorrosion coating raw materials, and is suitable for high viscosity and high density ceramic slurries, improving the performance and quality of the coating.
Smart Images

Figure CN119910766A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of side panel anti-corrosion coating processing, and specifically relates to a processing device and method for a desktop side panel anti-corrosion coating. Background Art
[0002] Ceramic anti-corrosion coating has multiple functions on the side panels of metal desktops, including excellent anti-corrosion performance, effectively isolating oxygen, moisture and chemical media to prevent oxidation and corrosion; excellent wear resistance, significantly reducing damage caused by friction and impact; high temperature resistance, protecting the metal surface from high temperature oxidation; insulation and heat insulation performance, providing electrical insulation and thermal insulation protection; and aesthetic effect, enhancing decorativeness through diversified colors and smooth surfaces. These characteristics make it widely used in industrial equipment, laboratory tables, outdoor facilities, architectural decoration, and home and commercial furniture, ensuring long-term protection and aesthetics of metal surfaces, and becoming an indispensable advanced protective technology in modern manufacturing. The production steps of ceramic anti-corrosion coating mainly include five key links: raw material preparation, ingredient mixing, coating construction, curing maintenance and quality inspection. Raw materials such as ceramic powder (such as alumina, zirconium oxide), binders, solvents and additives must be prepared according to the formula requirements, and their quality and performance must meet the standards. Secondly, the various component materials are fully mixed through precise metering and stirring equipment to prepare a uniform and delicate ceramic coating slurry.
[0003] The raw materials of ceramic anti-corrosion coatings have complex and diverse characteristics, including high-density fine-grained ceramic powders, high-viscosity binders, solvents with good fluidity, and a variety of functional additives. These materials are prone to difficulty in fully mixing during the mixing process. First, ceramic powders (such as alumina and zirconia) have high density and fine particles, and are prone to sedimentation during the mixing process, resulting in slurry stratification; secondly, binders (such as silicates and organic resins) usually have high viscosity and a large difference in fluidity with solvents (such as water and alcohol), which easily leads to uneven mixing; in addition, there are many types of additives (such as dispersants, plasticizers, coupling agents, etc.), and there may be compatibility issues between different additives, resulting in precipitation or agglomeration during the mixing process. The stirring speed and blade design of existing stirring equipment may not be able to effectively cope with high-viscosity and high-density ceramic slurries, further exacerbating the problem of uneven mixing. These problems make it difficult for existing stirring equipment to fully mix the raw materials of ceramic anti-corrosion coatings, resulting in slurry stratification, agglomeration or local uneven concentration, which in turn affects the performance and quality of the coating.
[0004] Therefore, a processing device and method for the anti-corrosion coating of the desktop side panel are now proposed. Summary of the invention
[0005] In order to solve the problems raised in the above background technology, the present invention provides a processing device and method for the anti-corrosion coating of the desktop side panel, which solves the problem that the existing equipment is difficult to fully mix the ceramic anti-corrosion coating material.
[0006] To achieve the above object, the present invention provides the following technical solution: a processing device for a desktop side panel anti-corrosion coating, comprising a support base, and also comprising: A driving assembly, wherein the driving assembly is disposed on the supporting base; A mixing assembly, the mixing assembly is installed on the driving assembly, and the mixing assembly is used to store ceramic anti-corrosion coating raw materials; A cross frame assembly, the cross frame assembly is installed on the top of the driving assembly; A limiting assembly, wherein the limiting assembly slides on the cross frame assembly; Wherein, the driving assembly comprises a guide rail and a ball screw fixed on the supporting base, a receiving plate is slidably arranged on the guide rail through a sliding block, the bottom of the receiving plate is connected to the ball screw through a docking piece, and one end of the ball screw is equipped with a driving motor; Both ends of the receiving plate are fixed with vertical fixing plates, and a mixing assembly is arranged between the two vertical fixing plates, and the mixing assembly is used to store ceramic anti-corrosion coating raw materials; The ceramic anti-corrosion coating is injected into the mixing component, and the driving motor drives the vertical fixed plate, the receiving plate and the mixing component to slide back and forth along the guide rail. During the sliding process, the ceramic raw materials inside the mixing component collide under the action of inertia.
[0007] Preferably, the mixing assembly comprises a mixing box fixed between two of the vertical fixed plates via a docking frame; A receiving frame for supporting the mixing box is fixedly installed between the two vertical fixing plates.
[0008] Preferably, the mixing box is made of soft plastic; The raw materials of the ceramic anti-corrosion coating are injected into the mixing box, and the ceramic anti-corrosion coating gathers in the middle of the mixing box and is supported by a receiving frame.
[0009] Preferably, a circular hole is opened in the middle of one of the vertical fixing plates, and a feed pipe is fixedly installed in the circular hole; A circular hole is formed at one end of the mixing box, and the mixing box is installed between the two vertical fixing plates, and the circular hole is connected with the feeding pipe.
[0010] Preferably, the cross frame assembly includes a fixed cross beam fixedly mounted on the top of the vertical fixed plate, a guide cross groove is provided on the top of the fixed cross beam, and limiting holes are provided on both sides of the guide cross groove at the top of the fixed cross beam.
[0011] Preferably, the limiting assembly comprises a sliding docking frame sliding inside the guide transverse groove, and the sliding docking frame is provided with a spring latch; The spring latch is engaged with the interior of the limiting hole.
[0012] Preferably, a supporting cross frame is fixedly mounted at the bottom of the sliding docking frame, transmission threaded rods are movably mounted at both ends of the supporting cross frame, a first arc plate is movably mounted at the lower end of the transmission threaded rod, and a second arc plate is mounted on the outer thread sleeve of the transmission threaded rod; The first arc plate and the second arc plate are sleeved on the outside of the mixing box.
[0013] Preferably, an arc-shaped through groove is provided in the middle of the first arc-shaped plate, and two ends of the second arc-shaped plate pass through the arc-shaped through groove and are connected to the transmission threaded rod; The first arc plate and the second arc plate are located in the middle of the mixing box, so that the middle of the mixing box is in a contracted state.
[0014] The present invention also provides a method for processing the anti-corrosion coating of the desktop side panel, comprising the following steps: S1. The ceramic anti-corrosion coating raw materials are injected into the interior of the mixing box through the feed pipe. The ceramic anti-corrosion coating raw materials gather in the middle of the mixing box under the action of gravity, and the middle of the mixing box is in a falling state, so that the mixing box is supported by the receiving frame; S2. The driving motor drives the ball screw to rotate. The receiving plate slides back and forth along the guide rail through the sliding block under the cooperation of the docking piece and the ball screw. When the receiving plate slides to one end of the guide rail, the ceramic anti-corrosion coating raw materials in the mixing box gather to one end of the mixing box under the action of inertia and hit one end of the mixing box. S3. At this time, the ceramic anti-corrosion coating raw materials gather toward the middle along the curvature of the mixing box, and the driving motor drives the receiving plate to move in the opposite direction, so that the ceramic anti-corrosion coating raw materials hit the other end of the mixing box. In this way, the ceramic anti-corrosion coating raw materials repeatedly hit the two ends of the mixing box to achieve mixing of the ceramic anti-corrosion coating raw materials.
[0015] Compared with the prior art, the present invention has the following beneficial effects: The present invention injects ceramic anti-corrosion coating raw materials into the interior of the mixing box through a feeding pipe. The ceramic anti-corrosion coating raw materials gather in the middle of the mixing box under the action of gravity, and the middle of the mixing box is in a falling state, so that the mixing box is supported by a receiving frame, and the ball screw is rotated by a driving motor. The receiving plate slides back and forth along the guide rail through a sliding block under the cooperation of a docking piece and the ball screw. When the receiving plate slides to one end of the guide rail, the ceramic anti-corrosion coating raw materials in the mixing box gather toward one end of the mixing box under the action of inertia, and collide with one end of the mixing box to gather toward the middle. The driving motor drives the receiving plate to move in the opposite direction, so that the ceramic anti-corrosion coating raw materials collide with the other end of the mixing box. In this way, the ceramic anti-corrosion coating raw materials repeatedly collide with the two ends of the mixing box through reciprocating, so as to achieve full mixing of the ceramic anti-corrosion coating raw materials, avoid precipitation or agglomeration during the mixing process, and at the same time be able to cope with high-viscosity and high-density ceramic slurry; After the ceramic anti-corrosion coating raw materials are mixed, the supporting cross frame slides away from the open end of the mixing box, and the second arc plate is moved up by rotating the transmission threaded rod to narrow the gap between the second arc plate and the first arc plate, so that one end of the mixing box is squeezed by the second arc plate and the first arc plate, so that the mixing box is in a tightened state. At the same time, during the upward movement of the second arc plate, one end of the mixing box can be driven higher than the other end, and the ceramic anti-corrosion coating raw materials inside can be discharged through the circular hole and the feed pipe. The mixing box is in a gathered state under the action of the first arc plate and the second arc plate, and the limit assembly is pushed to move toward the open end of the mixing box, so that the ceramic anti-corrosion coating raw materials in the mixing box can be discharged. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the overall appearance structure of the present invention; Figure 2 It is a schematic diagram of the plane structure of the present invention; Figure 3 This is a schematic diagram of the disassembled structure of the drive assembly and the mixing assembly of the present invention; Figure 4 It is a schematic diagram of the internal cross-sectional structure of the present invention; Figure 5 It is a schematic diagram of the coordination structure of the limit assembly and the mixing assembly of the present invention; Figure 6 This is a schematic diagram of the disassembled structure of the cross frame assembly, the limit assembly and the mixing assembly of the present invention; Figure 7 This is a schematic diagram of the disassembled structure of the cross frame assembly and the limit assembly of the present invention; Figure 8 It is a schematic diagram of the coordination structure of the limit assembly and the mixing assembly of the present invention; Fig. 9 This is a schematic diagram of the appearance structure of the limit assembly of the present invention; Fig.10It is a schematic diagram of the deformation of the limit component and the coordination structure of the mixing component of the present invention.
[0017] In the figure: 1. Support base; 2. Drive assembly; 21. Vertical fixed plate; 22. Feed pipe; 23. Sliding block; 24. Guide rail; 25. Adapter plate; 26. Ball screw; 27. Docking piece; 3. Frame assembly; 31. Fixed beam; 32. Limiting hole; 33. Guide groove; 4. Limiting assembly; 41. Support frame; 42. Sliding docking frame; 43. Spring latch; 44. Transmission threaded rod; 45. First arc plate; 46. Second arc plate; 47. Arc through groove; 5. Mixing assembly; 51. Mixing box; 52. Docking frame; 53. Adapter frame. DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] like Figures 1 to 10 As shown, the present invention provides a processing device for a desktop side plate anti-corrosion coating, comprising a support base 1, and also comprising: A driving assembly 2, wherein the driving assembly 2 is disposed on the supporting base 1; A mixing assembly 5, the mixing assembly 5 is installed on the driving assembly 2, and the mixing assembly 5 is used to store ceramic anti-corrosion coating raw materials; A cross frame assembly 3, the cross frame assembly 3 is installed on the top of the driving assembly 2; A limit assembly 4, the limit assembly 4 slides on the cross frame assembly 3; The driving assembly 2 includes a guide rail 24 and a ball screw 26 fixedly mounted on the supporting base 1. A receiving plate 25 is slidably arranged on the guide rail 24 through a sliding block 23. The bottom of the receiving plate 25 is connected to the ball screw 26 through a docking piece 27. One end of the ball screw 26 is equipped with a driving motor. The feeding speed of the ball screw 26 and the docking piece 27 is 30-70 m / min; Both ends of the receiving plate 25 are fixed with vertical fixing plates 21, and a mixing assembly 5 is arranged between the two vertical fixing plates 21, and the mixing assembly 5 is used to store ceramic anti-corrosion coating raw materials; The ceramic anti-corrosion coating is injected into the mixing assembly 5, and the driving motor drives the vertical fixing plate 21, the receiving plate 25 and the mixing assembly 5 to slide back and forth along the guide rail 24. During the sliding process, the ceramic raw materials inside the mixing assembly 5 collide under the action of inertia; The mixing assembly 5 comprises a mixing box 51 fixed between two vertical fixing plates 21 via a docking frame 52; A support frame 53 for supporting the mixing box 51 is fixedly installed between the two vertical fixed plates 21; The mixing box 51 is made of soft plastic; The ceramic anti-corrosion coating raw material is injected into the mixing box 51, and the ceramic anti-corrosion coating is gathered in the middle of the mixing box 51 and supported by the receiving frame 53; A circular hole is formed in the middle of one of the vertical fixing plates 21, and a feed pipe 22 is fixedly installed in the circular hole; A circular hole is formed at one end of the mixing box 51 . The mixing box 51 is installed between two vertical fixing plates 21 , and the circular hole is connected to the feed pipe 22 .
[0020] The ceramic anti-corrosion coating raw material is injected into the mixing box 51 through the feed pipe 22. The ceramic anti-corrosion coating raw material gathers in the middle of the mixing box 51 under the action of gravity, and the middle of the mixing box 51 is in a falling state, so that the mixing box 51 is supported by the receiving frame 53, and the ball screw 26 is driven to rotate by the driving motor. The receiving plate 25 slides back and forth along the guide rail 24 through the sliding block 23 under the cooperation of the docking piece 27 and the ball screw 26. When the receiving plate 25 slides to one end of the guide rail 24, the ceramic anti-corrosion coating raw material in the mixing box 51 is moved to the mixing box 51 under the action of inertia. One end of the mixing box 51 gathers and hits the other end of the mixing box 51. At this time, the ceramic anti-corrosion coating raw materials gather toward the middle along the curvature of the mixing box 51. The driving motor drives the receiving plate 25 to move in the opposite direction, so that the ceramic anti-corrosion coating raw materials hit the other end of the mixing box 51. In this way, the ceramic anti-corrosion coating raw materials repeatedly hit the two ends of the mixing box 51 through reciprocation, so as to achieve sufficient mixing of the ceramic anti-corrosion coating raw materials and avoid precipitation or agglomeration during the mixing process. At the same time, it can cope with high-viscosity and high-density ceramic slurry. After the raw materials are mixed, they can be discharged and sprayed on the metal desktop side panels.
[0021] like Figure 2-Figure 10 As shown, the cross frame assembly 3 includes a fixed cross beam 31 fixedly mounted on the top of the vertical fixed plate 21, a guide cross groove 33 is provided on the top of the fixed cross beam 31, and limiting holes 32 are provided on both sides of the guide cross groove 33 at the top of the fixed cross beam 31; The limiting assembly 4 includes a sliding docking frame 42 that slides inside the guide transverse groove 33, and a spring latch 43 is provided on the sliding docking frame 42; The spring latch 43 is engaged with the interior of the limiting hole 32; A supporting cross frame 41 is fixedly mounted at the bottom of the sliding docking frame 42, transmission threaded rods 44 are movably mounted at both ends of the supporting cross frame 41, a first arc plate 45 is movably mounted at the lower end of the transmission threaded rod 44, and a second arc plate 46 is sleeved on the outer thread of the transmission threaded rod 44; The first arc plate 45 and the second arc plate 46 are sleeved on the outside of the mixing box 51; An arc-shaped through slot 47 is formed in the middle of the first arc-shaped plate 45, and both ends of the second arc-shaped plate 46 pass through the arc-shaped through slot 47 and are connected to the transmission threaded rod 44; The first arc plate 45 and the second arc plate 46 are located in the middle of the mixing box 51, so that the middle of the mixing box 51 is in a contracted state.
[0022] By lifting the spring latch 43 and disengaging it from the inside of the limiting hole 32, the supporting cross frame 41 and the sliding docking frame 42 are pushed to slide along the fixed cross beam 31 to the middle of the mixing box 51. The middle of the mixing box 51 is gathered toward the middle under the action of the first arc plate 45 and the second arc plate 46. During the movement of the receiving plate 25, the ceramic anti-corrosion coating raw materials in the mixing box 51 move toward one end of the mixing box 51 under the action of inertia. During the movement, the raw materials are blocked by the second arc plate 46. When the raw materials pass through the gathering part in the middle of the mixing box 51, the ceramic anti-corrosion coating raw materials are wavy, thereby further improving the mixing effect of the ceramic anti-corrosion coating raw materials. At the same time, after the ceramic anti-corrosion coating raw materials are mixed, the supporting cross frame 41 slides away from the open end of the mixing box 51, and the second arc plate 46 is moved up by rotating the transmission threaded rod 44 to narrow the gap with the first arc plate 45, so that one end of the mixing box 51 is squeezed by the second arc plate 46 and the first arc plate 45, so that the mixing box 51 is in a tightened state. At the same time, the second arc plate 46 can drive one end of the mixing box 51 to be higher than the other end during the upward movement, and the internal ceramic anti-corrosion coating raw materials can be discharged through the circular hole and the feed pipe 22, and the mixing box 51 is in a gathered state under the action of the first arc plate 45 and the second arc plate 46, pushing the limit assembly 4 to move toward the open end of the mixing box 51, so that the ceramic anti-corrosion coating raw materials in the mixing box 51 can be discharged, and the metal desktop side panels can be sprayed.
[0023] The present invention also provides a method for processing the anti-corrosion coating of the desktop side panel, comprising the following steps: S1. The ceramic anti-corrosion coating raw material is injected into the interior of the mixing box 51 through the feed pipe 22. The ceramic anti-corrosion coating raw material gathers in the middle of the mixing box 51 under the action of gravity, and the middle of the mixing box 51 is in a falling state, so that the mixing box 51 is supported by the receiving frame 53; S2, the driving motor drives the ball screw 26 to rotate, and the receiving plate 25 slides back and forth along the guide rail 24 through the sliding block 23 under the cooperation of the docking piece 27 and the ball screw 26. When the receiving plate 25 slides to one end of the guide rail 24, the ceramic anti-corrosion coating raw materials in the mixing box 51 gather to one end of the mixing box 51 under the action of inertia and hit one end of the mixing box 51; S3. At this time, the ceramic anti-corrosion coating raw materials gather toward the middle along the curvature of the mixing box 51, and the driving motor drives the receiving plate 25 to move in the opposite direction, so that the ceramic anti-corrosion coating raw materials hit the other end of the mixing box 51. In this way, the ceramic anti-corrosion coating raw materials repeatedly hit the two ends of the mixing box 51 back and forth to achieve mixing of the ceramic anti-corrosion coating raw materials.
[0024] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0025] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A processing device for a desktop side panel anti-corrosion coating, comprising a support base (1), characterized in that: Also includes: A driving assembly (2), wherein the driving assembly (2) is arranged on the supporting base (1); A mixing assembly (5), the mixing assembly (5) being mounted on the driving assembly (2), the mixing assembly (5) being used to store ceramic anti-corrosion coating raw materials; A cross frame assembly (3), wherein the cross frame assembly (3) is mounted on the top of the driving assembly (2); A limiting assembly (4), wherein the limiting assembly (4) slides on the cross frame assembly (3); The driving assembly (2) comprises a guide rail (24) and a ball screw (26) fixedly mounted on the supporting base (1); a receiving plate (25) is slidably arranged on the guide rail (24) via a sliding block (23); the bottom of the receiving plate (25) is connected to the ball screw (26) via a docking piece (27); and one end of the ball screw (26) is equipped with a driving motor; Both ends of the receiving plate (25) are fixedly mounted with vertical fixing plates (21), and a mixing assembly (5) is arranged between the two vertical fixing plates (21), wherein the mixing assembly (5) is used to store ceramic anti-corrosion coating raw materials; The ceramic anti-corrosion coating is injected into the mixing component (5), and the driving motor drives the vertical fixing plate (21), the receiving plate (25), and the mixing component (5) to slide back and forth along the guide rail (24). During the sliding process, the ceramic raw materials inside the mixing component (5) collide under the action of inertia.
2. The processing device for the anti-corrosion coating of the desktop side panel according to claim 1 is characterized in that: The mixing assembly (5) comprises a mixing box (51) fixed between the two vertical fixing plates (21) via a docking frame (52); A supporting frame (53) for supporting the mixing box (51) is fixedly installed between the two vertical fixing plates (21).
3. The processing device for the anti-corrosion coating of the desktop side panel according to claim 2 is characterized in that: The mixing box (51) is made of soft plastic; The ceramic anti-corrosion coating raw material is injected into the mixing box (51), and the ceramic anti-corrosion coating is gathered in the middle of the mixing box (51) and supported by the receiving frame (53).
4. The processing device for the anti-corrosion coating of the desktop side panel according to claim 3 is characterized in that: A circular hole is formed in the middle of one of the vertical fixing plates (21), and a feed pipe (22) is fixedly installed in the circular hole; A circular hole is formed at one end of the mixing box (51); the mixing box (51) is installed between the two vertical fixing plates (21), and the circular hole is connected to the feed pipe (22).
5. The processing device for the anti-corrosion coating of the desktop side panel according to claim 2 is characterized in that: The cross frame assembly (3) comprises a fixed cross beam (31) fixedly mounted on the top of the vertical fixed plate (21), a guide cross groove (33) being provided on the top of the fixed cross beam (31), and limiting holes (32) being provided on both sides of the guide cross groove (33) on the top of the fixed cross beam (31).
6. The processing device for the anti-corrosion coating of the desktop side panel according to claim 5 is characterized in that: The limiting assembly (4) comprises a sliding docking frame (42) that slides inside the guide transverse groove (33), and a spring latch (43) is provided on the sliding docking frame (42); The spring latch (43) is engaged with the interior of the limiting hole (32).
7. The processing device for the anti-corrosion coating of the desktop side panel according to claim 6 is characterized in that: A supporting cross frame (41) is fixedly mounted at the bottom of the sliding docking frame (42), transmission threaded rods (44) are movably mounted at both ends of the supporting cross frame (41), a first arc-shaped plate (45) is movably mounted at the lower end of the transmission threaded rod (44), and a second arc-shaped plate (46) is provided on the outer thread sleeve of the transmission threaded rod (44); The first arc-shaped plate (45) and the second arc-shaped plate (46) are sleeved on the outside of the mixing box (51).
8. The processing device for the anti-corrosion coating of the desktop side panel according to claim 7 is characterized in that: An arc-shaped through groove (47) is formed in the middle of the first arc-shaped plate (45), and two ends of the second arc-shaped plate (46) pass through the arc-shaped through groove (47) to be connected to the transmission threaded rod (44); The first arc-shaped plate (45) and the second arc-shaped plate (46) are located in the middle of the mixing box (51), so that the middle of the mixing box (51) is in a contracted state.
9. A method for processing an anti-corrosion coating on a desktop side panel, using the processing device for the anti-corrosion coating on a desktop side panel as claimed in claim 4, characterized in that: The following steps are involved: S1, the ceramic anti-corrosion coating raw material is injected into the interior of the mixing box (51) through the feed pipe (22), and the ceramic anti-corrosion coating raw material is gathered in the middle of the mixing box (51) under the action of gravity, and the middle of the mixing box (51) is in a falling state, so that the mixing box (51) is supported by the receiving frame (53); S2, the driving motor drives the ball screw (26) to rotate, and the receiving plate (25) slides back and forth along the guide rail (24) through the sliding block (23) under the cooperation of the docking piece (27) and the ball screw (26). When the receiving plate (25) slides to one end of the guide rail (24), the ceramic anti-corrosion coating raw materials in the mixing box (51) gather toward one end of the mixing box (51) under the action of inertia and collide with the other end of the mixing box (51); S3. At this time, the ceramic anti-corrosion coating raw materials gather toward the middle along the arc of the mixing box (51), and the driving motor drives the receiving plate (25) to move in the opposite direction, so that the ceramic anti-corrosion coating raw materials hit the other end of the mixing box (51). In this way, the ceramic anti-corrosion coating raw materials repeatedly hit the two ends of the mixing box (51) through reciprocating motion, thereby achieving mixing of the ceramic anti-corrosion coating raw materials.