Secondary battery and electric device

By combining a sealant and an adhesive in the gap between the side walls of the secondary battery casing, the problem of sealing failure caused by casing torsion is solved, thereby improving the battery's encapsulation strength and energy density.

CN120453595BActive Publication Date: 2026-11-10NINGDE AMPEREX TECHNOLOGY LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202510779536.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-06-11
Publication Date
2026-11-10
Estimated Expiration
2045-06-11

AI Technical Summary

Technical Problem

The casing of existing secondary batteries is prone to relative torsion under conditions such as drops, which increases the risk of seal failure.

Method used

The design employs a combination of seals and adhesives. The seals are arranged around the gaps in the side walls of the housing, while the adhesives are fixed to the seals and side walls through adhesive parts, which enhances the sealing strength and reduces the possibility of housing torsion.

Benefits of technology

It improves the sealing of the secondary battery, reduces the risk of casing torsion, and enhances the battery's energy density and lifespan.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120453595B_ABST
    Figure CN120453595B_ABST
Patent Text Reader

Abstract

The application discloses a secondary battery and an electric device. The secondary battery comprises a shell, an electrode assembly, a sealing member and a first adhesive member. The electrode assembly is arranged in the shell. The shell comprises a first shell body with a first wall and a first side wall, and a second shell body with a second wall and a second side wall. The first side wall is provided with a first surface. The first surface is directed to the second side wall along the extension direction of the first side wall. The second side wall is provided with a second surface. The second surface is directed to the first side wall along the extension direction of the second side wall. The first surface and the second surface are oppositely arranged and have a gap. The sealing member seals the gap and comprises a filling part arranged in the gap. The first adhesive member is arranged on the first side wall and comprises a first adhesive part arranged on the first surface and a second adhesive part arranged on the inner wall of the first side wall. The first adhesive part is integrally arranged with the second adhesive part and is fixedly arranged with the filling part. The packaging strength of the sealing member and the shell can be improved, and the possibility of relative torsion of the first shell body and the second shell body can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of energy storage technology, and in particular to a secondary battery and electrical equipment. Background Technology

[0002] Current secondary batteries include steel-cased batteries and pouch batteries. Generally, both steel-cased and pouch batteries include a casing and electrode components housed within the casing. The casing of a steel-cased battery comprises a first housing and a second housing, which are sealed together by welding or a sealing element. Summary of the Invention

[0003] Regarding existing secondary batteries, the inventors discovered that if the first and second shells are sealed together by a sealing element, when the secondary battery is dropped, the first and second shells are prone to relative torsion, causing the outer shell to deform. This results in a high risk of failure of the outer shell and the sealing element.

[0004] In view of the above situation, it is necessary to provide a secondary battery that helps to reduce the possibility of relative torsion between the first and second casings.

[0005] This application provides a secondary battery, including a casing, an electrode assembly, a seal, and a first adhesive. The casing includes a first housing and a second housing, which together form a receiving cavity filled with an electrolyte. The electrode assembly is disposed within the receiving cavity. The first housing includes a first wall and a first sidewall connecting to the periphery of the first wall. The second housing includes a second wall and a second sidewall connecting to the periphery of the second wall. The first sidewall has a first surface extending towards the second sidewall, and the second sidewall has a second surface extending towards the first sidewall. The first and second surfaces face each other and have a gap. The seal is disposed around the outer periphery of the first and second sidewalls and seals the gap. The seal includes a filling portion disposed in the gap. The first adhesive is disposed on the first sidewall and includes a first adhesive portion and a second adhesive portion. The first adhesive portion is disposed on the first surface of the first sidewall, and the second adhesive portion is disposed on the inner wall of the first sidewall. The first adhesive portion and the second adhesive portion are integrally disposed. The first adhesive portion and the filling portion are fixedly disposed together.

[0006] The first adhesive portion is disposed on the first surface of the first sidewall, and the second adhesive portion is disposed on the inner wall of the first sidewall. The first adhesive portion and the second adhesive portion are integrally disposed, which enables the adhesive to be stably fixed to the first sidewall. Furthermore, the first adhesive portion is fixedly disposed with the filling portion, and the cooperation between the first adhesive portion and the sealing element can improve the sealing strength between the sealing element and the shell, which helps to reduce the possibility of relative torsion between the first shell and the second shell.

[0007] In one or more of the above embodiments, the secondary battery further includes a second adhesive member disposed on the second sidewall. The second adhesive member includes a third adhesive portion and a fourth adhesive portion. The third adhesive portion is disposed on the second surface of the second sidewall, and the fourth adhesive portion is disposed on the inner wall of the second sidewall. The third adhesive portion and the fourth adhesive portion are integrally disposed, which enables the second adhesive member to be more stably fixed to the second sidewall. Furthermore, the third adhesive portion is fixedly disposed with the filling portion. The cooperation between the second adhesive member and the sealing member can further improve the sealing strength between the sealing member and the shell, which is beneficial to further reduce the possibility of relative torsion between the first shell and the second shell.

[0008] In one or more of the above embodiments, the distance between the first surface and the second surface is D, where 20μm ≤ D ≤ 5000μm. By setting D to 20μm ≤ D, the distance between the first surface and the second surface is not too small, which helps to reduce the possibility of short circuits caused by burr contact between the first and second housings. By setting D ≤ 5000μm, the distance between the first surface and the second surface is not too large, which helps to improve the energy density of the secondary battery.

[0009] In one or more of the above embodiments, 40μm≤D≤3000μm. By setting 40μm≤D, it is beneficial to further reduce the possibility of short circuits caused by burr contact between the first and second housings. By setting D≤3000μm, it is beneficial to further improve the energy density of the secondary battery.

[0010] In one or more of the above embodiments, the thickness of the first adhesive portion is H1, the thickness of the second adhesive portion is H2, 3μm≤H1≤500μm, and 90%H1≤H2≤110%H1. Setting 3μm≤H1 helps reduce the risk of short circuits caused by burrs piercing the first adhesive portion after the filler melts. Setting H1≤500μm helps improve the energy density of the secondary battery. Considering the precision of the processing technology, setting 90%H1≤H2≤110%H1 facilitates the integral installation of the first and second adhesive portions. The thickness of the third adhesive portion is H3, the thickness of the fourth adhesive portion is H4, 3μm≤H3≤500μm, and 90%H3≤H4≤110%H3. Setting 3μm≤H3 helps reduce the risk of short circuits caused by burrs piercing the third adhesive portion after the filler melts. Setting H3≤500μm helps improve the energy density of the secondary battery. Considering the precision of the processing technology, by setting 90%H3≤H4≤110%H3, it is easy to integrate the third and fourth bonding parts.

[0011] In one or more of the above embodiments, 6μm ≤ H1 ≤ 200μm. Setting 6μm ≤ H1 helps to further reduce the risk of short circuits caused by burrs piercing the first bonding portion after the filler melts. Setting H1 ≤ 200μm helps to further improve the energy density of the secondary battery. 6μm ≤ H3 ≤ 200μm. Setting 6μm ≤ H3 helps to further reduce the risk of short circuits caused by burrs piercing the third bonding portion after the filler melts. Setting H1 ≤ 200μm helps to further improve the energy density of the secondary battery.

[0012] In one or more of the above embodiments, the first adhesive portion and the filler portion are integrally formed. This helps to improve the stability of the connection between the first adhesive portion and the filler portion. The third adhesive portion and the filler portion are integrally formed. This helps to improve the stability of the connection between the third adhesive portion and the filler portion.

[0013] In one or more of the above embodiments, the width of the second adhesive portion is W2, where 30μm ≤ W2 ≤ 3000μm. By setting 30μm ≤ W2, the bonding area between the second adhesive portion and the inner wall of the sidewall is not too small, which helps to improve the stability of the second adhesive portion on the inner wall of the first sidewall. Furthermore, when the first adhesive portion and the filling portion are integrally formed, setting 30μm ≤ W2 also helps to reduce the possibility of electrolyte erosion at the interface between the second adhesive portion and the first sidewall. By setting W2 ≤ 3000μm, the bonding area between the second adhesive portion and the inner wall of the first sidewall is not too large. When the polarity of the electrode assembly is led out through the first sidewall, the first sidewall can have a larger area for connection, which helps to improve the convenience of connecting the electrode assembly to the first sidewall. The width of the fourth adhesive portion is W4, where 30μm ≤ W4 ≤ 3000μm. By setting W4 to 30μm ≤ W4, the bonding area between the fourth adhesive portion and the inner wall of the second sidewall is not too small, which helps improve the stability of the fourth adhesive portion on the inner wall of the second sidewall. Furthermore, when the third adhesive portion and the filling portion are integrally formed, setting W4 to 30μm ≤ W4 also helps reduce the possibility of electrolyte erosion at the interface between the fourth adhesive portion and the second sidewall. By setting W4 ≤ 3000μm, the bonding area between the fourth adhesive portion and the inner wall of the second sidewall is not too large. When the polarity of the electrode assembly is led out through the second sidewall, the second sidewall has a larger area for connection, which helps improve the ease of connection between the electrode assembly and the second sidewall.

[0014] In one or more of the above embodiments, 100μm ≤ W2 ≤ 1500μm. Setting 100μm ≤ W2 helps to further improve the stability of the second adhesive portion on the inner wall of the first sidewall. Furthermore, when the first adhesive portion and the filling portion are integrally formed, setting 100μm ≤ W2 also helps to further reduce the possibility of electrolyte erosion at the interface between the second adhesive portion and the first sidewall. Setting W2 ≤ 1500μm helps to further improve the ease of connection between the electrode assembly and the first sidewall. 100μm ≤ W4 ≤ 1500μm. Setting 100μm ≤ W4 helps to further improve the stability of the fourth adhesive portion on the inner wall of the second sidewall. Furthermore, when the third adhesive portion and the filling portion are integrally formed, setting 100μm ≤ W4 helps to further reduce the possibility of electrolyte erosion at the interface between the fourth adhesive portion and the second sidewall. Setting W4 ≤ 1500μm helps to further improve the ease of connection between the electrode assembly and the second sidewall.

[0015] In one or more of the above embodiments, the sealing element includes a first adhesive layer, a metal layer, and a second adhesive layer. Along the thickness direction of the metal layer, the first and second adhesive layers are respectively disposed on both sides of the metal layer. The first adhesive layer is adhered to the outer periphery of the first and second sidewalls, and the filling portion is integrally formed with the first adhesive layer. The sealing element includes a first adhesive layer, which is bonded to the first and second sidewalls. The first adhesive layer helps improve the stability of the bond between the sealing element and the outer shell. The sealing element includes a metal layer, which is disposed on the side of the first adhesive layer away from the outer shell. The water resistance of the metal layer is superior to that of the first adhesive layer, which helps improve the sealing performance of the sealing element to the first and second shells. The sealing element includes a second adhesive layer, which is disposed on the side of the metal layer away from the first adhesive layer. The second adhesive layer can protect the metal layer, which helps reduce the risk of metal layer failure. Therefore, during the long-term use of the secondary battery, it is beneficial to maintain the sealing performance of the sealing element to the first and second shells.

[0016] In one or more of the above embodiments, along the thickness direction of the seal, the thickness of the first adhesive layer is d1, the thickness of the metal layer is d2, and the thickness of the second adhesive layer is d3, with 7μm≤d1≤500μm, 7μm≤d2≤250μm, and 6μm≤d3≤500μm. By setting 7μm≤d1, 7μm≤d2, and 6μm≤d3, the first adhesive layer, the metal layer, and the second adhesive layer are not too thin, which helps reduce the risk of the first adhesive layer failing due to electrolyte corrosion and reduces the risk of the second adhesive layer breaking after the secondary battery is dropped, leading to metal layer failure or corrosion. By setting d1≤500μm, d2≤250μm, and d3≤500μm, the first adhesive layer, the metal layer, and the second adhesive layer are not too thick, which helps improve the energy density of the secondary battery.

[0017] In one or more of the above embodiments, 10μm≤d1≤200μm, 10μm≤d2≤150μm, and 8μm≤d3≤200μm. By setting 10μm≤d1, 10μm≤d2, and 8μm≤d3, the first adhesive layer, the metal layer, and the second adhesive layer can be made thicker. This helps to further reduce the risk of the first adhesive layer failing due to electrolyte corrosion, and further reduces the risk of the second adhesive layer breaking after a drop, leading to metal layer failure or corrosion. By setting d1≤200μm, d2≤150μm, and d3≤200μm, the energy density of the secondary battery can be further improved while ensuring that the thickness of the first adhesive layer is basically sufficient to prevent electrolyte corrosion, the thickness of the second adhesive layer is sufficient for most drop scenarios, and the thickness of the metal layer is basically sufficient to prevent failure due to breakage or corrosion.

[0018] The second aspect of this application provides an electrical device, including the secondary battery of the first aspect of this application. The secondary battery has better sealing performance, and the electrolyte is less prone to leakage, which helps to extend the service life of the electrical device. Attached Figure Description

[0019] Figure 1 This is a top view of a secondary battery provided in an embodiment of this application.

[0020] Figure 2 This is a front view of a secondary battery provided in an embodiment of this application.

[0021] Figure 3 An exploded view of a secondary battery provided in an embodiment of this application.

[0022] Figure 4 The first embodiment of this application is along Figure 1 Cross-sectional view of the mid-section line AA.

[0023] Figure 5 The second embodiment of this application is along Figure 1 Cross-sectional view of the mid-section line AA.

[0024] Figure 6 This is a cross-sectional schematic diagram of a first adhesive member provided in an embodiment of this application.

[0025] Figure 7 This is a schematic diagram of an electrical device provided in an embodiment of this application.

[0026] Explanation of main component symbols 1000 Electrical equipment; 100 Secondary battery; 10 Outer casing; 101 Receiving cavity; 11 First housing; 111 First wall; 112 First side wall; 1121 First surface; 12 Second housing; 121 Second wall; 122 Second side wall; 1221 Second surface; 20 Electrode assembly; 201 First electrode bundle; 202 Second electrode bundle; 21 First electrode; 22 Second electrode; 23 Separator; 30 Sealing element; 301 Filler portion; 31 First adhesive layer; 32 Metal layer; 33 Second adhesive layer; 40 Adhesive element; 41 First adhesive portion; 42 Second adhesive portion; 50 Second adhesive element; 51 Third adhesive portion; 52 Fourth adhesive portion; 60 Fixing element. Detailed Implementation

[0027] The technical solutions of the embodiments of this application will be described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments.

[0028] It should be noted that when a component is considered to be "connected" to another component, it can be directly connected to the other component or may also have a component that is centrally located. When a component is considered to be "set" on another component, it can be directly set on the other component or may also have a component that is centrally located.

[0029] Unless otherwise stated, the term "multiple" as used herein refers to two or more.

[0030] The terms “first”, “second”, etc., are used only to distinguish different objects and should not be construed as indicating or implying relative importance or implying the quantity, specific order, or primary and secondary relationship of the indicated technical features.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0032] It should be understood that, considering the actual machining tolerances, in the technical solution of this application, when the two components are arranged in parallel / perpendicular positions, the included angle between the two components is allowed to have a tolerance within 10% of the included angle corresponding to the parallel / perpendicular arrangement.

[0033] This application provides a secondary battery, including a casing, an electrode assembly, a seal, and a first adhesive. The casing includes a first housing and a second housing, which together form a receiving cavity filled with electrolyte. The electrode assembly is disposed within the receiving cavity. The first housing includes a first wall and a first sidewall connecting to the periphery of the first wall. The second housing includes a second wall and a second sidewall connecting to the periphery of the second wall. The first sidewall has a first surface extending towards the second sidewall along its extension direction. The second sidewall has a second surface extending towards the first sidewall along its extension direction. The first and second surfaces face each other and have a gap. The seal is disposed around the outer periphery of the first and second sidewalls and seals the gap. The seal includes a filling portion disposed in the gap. The first adhesive is disposed on the first sidewall and includes a first adhesive portion and a second adhesive portion. The first adhesive portion is disposed on the first surface of the first sidewall, and the second adhesive portion is disposed on the inner wall of the first sidewall. The first adhesive portion and the second adhesive portion are integrally disposed. The first adhesive portion and the filling portion are fixedly disposed together.

[0034] In the secondary battery of this application, a first adhesive portion is disposed on the first surface of the first sidewall, and a second adhesive portion is disposed on the inner wall of the first sidewall. The first adhesive portion and the second adhesive portion are integrally disposed, which enables the first adhesive portion to be stably fixed to the first sidewall. Furthermore, the first adhesive portion and the filling portion are fixedly disposed, and the cooperation between the first adhesive portion and the sealing member can improve the sealing strength between the sealing member and the shell, which helps to reduce the possibility of relative torsion between the first shell and the second shell.

[0035] Some embodiments of this application will now be described with reference to the accompanying drawings. Unless otherwise specified, the following embodiments and features can be combined with each other.

[0036] Please see Figures 1 to 6 An embodiment of this application provides a secondary battery 100, including a housing 10, an electrode assembly 20, a sealing member 30, and a first adhesive member 40. The electrode assembly 20 is housed within the housing 10. The sealing member 30 is disposed on the outer wall of the housing 10 and is used to seal the housing 10. The first adhesive member 40 is disposed on the side wall of the housing 10 and is connected to the sealing member 30.

[0037] In some embodiments, please refer to Figure 2 and Figure 3 The outer casing 10 includes a first casing 11 and a second casing 12. In some embodiments, the first casing 11 and the second casing 12 are disposed facing each other. In some embodiments, the first casing 11 and the second casing 12 are insulated from each other.

[0038] In some embodiments, the outer casing 10 is a metal casing, and the material of the outer casing 10 includes at least one selected from steel alloy, aluminum alloy, and copper alloy. The materials of the first casing 11 and the second casing 12 may be the same or different.

[0039] In some embodiments, please refer to Figure 3 The first housing 11 includes a first wall 111 and a first side wall 112, and the second housing 12 includes a second wall 121 and a second side wall 122. The first side wall 112 connects to the periphery of the first wall 111, and the second side wall 122 connects to the periphery of the second wall 121. Along a direction perpendicular to the second side wall 122, the projection of the second side wall 122 is separate from the projection of the first side wall 112. The first side wall 112 may be inclined or perpendicular to the first wall 111, and the second side wall 122 may be inclined or perpendicular to the second wall 121; this application does not impose any limitations on this. The first side wall 112 has a first surface 1121, which extends towards the second side wall 122 along the extension direction of the first side wall 112. The second side wall 122 has a second surface 1221, which extends towards the first side wall 112 along the extension direction of the second side wall 122. The first surface 1121 and the second surface 1221 are arranged facing each other and have a gap. Wherein, the extension direction of the first sidewall 112 refers to the direction in which it extends away from the side connected to the periphery of the first wall 111, and the extension direction of the second sidewall 122 refers to the direction in which it extends away from the side connected to the periphery of the second wall 121. It should be understood that the first surface 1121 and the second surface 1221 can be either a plane or a curved surface, and this application does not limit them.

[0040] Please see Figure 4 and Figure 5 The first housing 11 and the second housing 12 together form a receiving cavity 101, which is filled with electrolyte. The electrode assembly 20 is disposed in the receiving cavity 101. Please refer to... Figure 3 The electrode assembly 20 includes a first electrode 21, a second electrode 22, and a diaphragm 23. The second electrode 22 has the opposite polarity to the first electrode 21, and the diaphragm 23 separates the first electrode 21 from the second electrode 22.

[0041] In some embodiments, please refer to Figure 4 and Figure 5 The electrode assembly 20 has a stacked structure, with first electrode 21 and second electrode 22 alternately stacked, and a diaphragm 23 disposed between adjacent first electrode 21 and second electrode 22. In some embodiments, the electrode assembly 20 has a wound structure, with first electrode 21 and second electrode 22 alternately wound, and a diaphragm 23 disposed between adjacent first electrode 21 and second electrode 22.

[0042] In some embodiments, the first electrode 21 is a negative electrode and the second electrode 22 is a positive electrode. In some embodiments, the first electrode 21 is a positive electrode and the second electrode 22 is a negative electrode. Wherein, along the thickness direction of the electrode assembly 20, the projection of the negative electrode overlaps the projection of the positive electrode.

[0043] In some embodiments, the first electrode 21 includes a first current collector and a first active material layer, the first active material layer being disposed on two opposing sides of the first current collector along its thickness direction. The second electrode 22 includes a second current collector and a second active material layer, the second active material layer being disposed on two opposing sides of the second current collector along its thickness direction. In some embodiments, when the first electrode 21 or the second electrode 22 is the outermost electrode of the electrode assembly 20, the side of the current collector facing away from the interior of the electrode assembly 20 may not have an active material layer.

[0044] In some embodiments, the material of the first current collector includes at least one of copper, nickel, tantalum, and titanium, and the material of the second current collector includes at least one of aluminum, nickel, tantalum, and titanium.

[0045] In some embodiments, the first active material layer is made of at least one of graphite, hard carbon, soft carbon, silicon, silicon-oxygen materials, and silicon-carbon materials. The second active material layer is made of at least one of lithium cobalt oxide, lithium nickel cobalt manganese oxide, lithium nickel cobalt aluminum oxide, lithium iron phosphate, lithium manganese iron phosphate, or lithium manganese oxide.

[0046] In some embodiments, the diaphragm 23 is an insulating membrane material such as a polyethylene membrane, a polypropylene membrane, a polyester membrane, or a polyimide membrane.

[0047] In some embodiments, the first current collector and the second current collector each have an empty foil area. One of the empty foil areas of the first current collector and the second current collector is directly connected to the first housing 11, and the other of the empty foil areas of the first current collector and the second current collector is directly connected to the second housing 12. The first housing 11 and the second housing 12 are insulated from each other. In some embodiments, the empty foil area is indirectly connected to the first housing 11 and / or the second housing 12 through a conductive element (not shown). The conductive element includes, but is not limited to, conductive protrusions, metal springs, and conductive adhesives. The conductive protrusions may be formed by laser texturing of the outer shell 10.

[0048] In some embodiments, please refer to Figure 3The secondary battery 100 also includes a plurality of first tabs connected to the first electrode 21, the plurality of first tabs being gathered together to form a first tab bundle 201. The secondary battery 100 also includes a plurality of second tabs connected to the second electrode 22, the plurality of second tabs being gathered together to form a second tab bundle 202. One of the first tab bundle 201 and the second tab bundle 202 is electrically connected to the first housing 11, and the other of the first tab bundle 201 and the second tab bundle 202 is electrically connected to the second housing 12, the first housing 11 and the second housing 12 being insulated from each other. In some embodiments, one of the first tab bundle 201 and the second tab bundle 202 is connected to the first sidewall 112, and the other of the first tab bundle 201 and the second tab bundle 202 is connected to the second sidewall 122.

[0049] In some embodiments, the seal 30 is used to separate and seal the first housing 11 and the second housing 12. See also Figure 1 and Figure 2 The sealing element 30 is disposed around the outer periphery of the first sidewall 112 and the second sidewall 122. Along the thickness direction of the sealing element 30, the projection of the sealing element 30 at least partially overlaps with the projection of the first housing 11 and the second housing 12. The sealing element 30 includes a filling portion 301 disposed in the gap between the first surface 1121 and the second surface 1221. The filling portion 301 can separate the first housing 11 and the second housing 12, facilitating the insulation of the first housing 11 and the second housing 12.

[0050] Please see Figure 4 and Figure 5 The first adhesive member 40 is disposed on the first sidewall 112 and connected to the sealing member 30. The first adhesive member 40 includes a first adhesive portion 41 and a second adhesive portion 42 (see...). Figure 6 The first adhesive portion 41 is disposed on the first surface 1121 of the first sidewall 112, and the second adhesive portion 42 is disposed on the inner wall of the first sidewall 112. The first adhesive portion 41 and the second adhesive portion 42 are integrally disposed. This allows the adhesive member 40 to be fixedly fixed to the first sidewall 112. In some embodiments, the first adhesive portion 41 is fixedly disposed with the filling portion 301. The cooperation between the first adhesive member 40 and the sealing member 30 can improve the sealing strength between the sealing member 30 and the outer shell 10, which helps to reduce the possibility of relative torsion between the first shell 11 and the second shell 12.

[0051] In some embodiments, the first adhesive portion 41 is bonded and fixed to the filling portion 301. In some embodiments, the first adhesive portion 41 is fused and fixed to the filling portion 301.

[0052] In some embodiments, the first adhesive portion 41 and the filler portion 301 are integrally formed. This improves the stability of the connection between the first adhesive portion 41 and the filler portion 301. In some embodiments, before assembling the first housing 11 and the second housing 12, a first adhesive member 40 is pre-attached to the first sidewall 112 to form the first adhesive portion 41 and the second adhesive portion 42, so that the filler portion 301 is fused with the first adhesive portion 41 in a molten state, and after cooling, the filler portion 301 and the first adhesive portion 41 are integrally formed.

[0053] In some embodiments, please refer to Figure 6 The thickness of the first adhesive portion 41 is H1, where 3μm ≤ H1 ≤ 500μm. For example, H1 can be 3μm, 6μm, 10μm, 20μm, 50μm, 100μm, 200μm, 300μm, 500μm, or any value between the listed endpoints. By setting 3μm ≤ H1, it is beneficial to reduce the risk of short circuits caused by burrs piercing the first adhesive portion 41 after the filling portion 301 melts. By setting H1 ≤ 500μm, it is beneficial to improve the energy density of the secondary battery 100. The thickness of the first adhesive portion 41 is the dimension of the first adhesive portion 41 along the direction perpendicular to the first surface 1121.

[0054] In some embodiments, 6μm ≤ H1 ≤ 200μm. By setting 6μm ≤ H1, it is beneficial to further reduce the risk of short circuits caused by burrs piercing the first adhesive portion 41 after the filler portion 301 melts. By setting H1 ≤ 200μm, it is beneficial to further improve the energy density of the secondary battery 100.

[0055] In some embodiments, please refer to Figure 6 The thickness of the second adhesive portion 42 is H2, where 90%H1≤H2≤110%H1. Considering the precision of the processing technology, setting 90%H1≤H2≤110%H1 facilitates the integral installation of the first adhesive portion 41 and the second adhesive portion 42. The thickness of the second adhesive portion 42 is its dimension along the direction perpendicular to the first sidewall 112.

[0056] In some embodiments, please refer to Figure 6 The width of the first adhesive portion 41 is W1, which is less than or equal to the wall thickness of the first sidewall 112. Considering the precision of the processing technology, when W1 is greater than the wall thickness of the first sidewall 112 within a 10% error range, W1 can also be considered equal to the wall thickness of the first sidewall 112. The width of the first adhesive portion 41 is the dimension of the first adhesive portion 41 along a direction parallel to the first surface 1121.

[0057] In some embodiments, please refer to Figure 6The width of the second adhesive portion 42 is W2, where 30μm ≤ W2 ≤ 3000μm. For example, W2 can be 30μm, 50μm, 100μm, 200μm, 500μm, 1000μm, 1500μm, 3000μm, or any value between the listed endpoints. By setting 30μm ≤ W2, the bonding area between the second adhesive portion 42 and the inner wall of the first sidewall 112 is not too small, which helps to improve the stability of the second adhesive portion 42 on the inner wall of the first sidewall 112. Furthermore, when the first adhesive portion 41 and the filling portion 301 are integrally formed, setting 30μm ≤ W2 also helps to reduce the possibility of electrolyte erosion at the interface between the second adhesive portion 42 and the first sidewall 112. By setting W2 ≤ 3000μm, the bonding area between the second adhesive portion 42 and the inner wall of the first sidewall 112 is not too large. When the polarity of the electrode assembly 20 is led out through the first sidewall 112, the first sidewall 112 can have a larger area for connection, which is beneficial to improving the convenience of connecting the electrode assembly 20 and the first sidewall 112. The width of the second adhesive portion 42 is the dimension along the extending direction of the first sidewall 112.

[0058] In some embodiments, 100μm ≤ W2 ≤ 1500μm. Setting 100μm ≤ W2 helps to further improve the stability of the second adhesive portion 42 on the inner wall of the first sidewall 112. Furthermore, when the first adhesive portion 41 and the filling portion 301 are integrally formed, setting 100μm ≤ W2 also helps to further reduce the possibility of electrolyte erosion at the interface between the second adhesive portion 42 and the first sidewall 112. Setting W2 ≤ 1500μm helps to further improve the ease of connection between the electrode assembly 20 and the first sidewall 112.

[0059] In some embodiments, the melting point of the first adhesive 40 is between 95°C and 130°C. For example, the melting point of the first adhesive 40 is 95°C, 100°C, 110°C, 130°C, or a range between the listed endpoint values, or any value between the listed endpoint values. In some embodiments, the melting point of the first adhesive 40 is between 150°C and 500°C. For example, the melting point of the first adhesive 40 is 150°C, 200°C, 250°C, 300°C, 500°C, or a range between the listed endpoint values, or any value between the listed endpoint values.

[0060] In some embodiments, the secondary battery 100 further includes a second adhesive member 50 disposed on the second sidewall 122. The second adhesive member 50 includes a third adhesive portion 51 and a fourth adhesive portion 52. The third adhesive portion 51 is disposed on the second surface 1221 of the second sidewall 122, and the fourth adhesive portion 52 is disposed on the inner wall of the second sidewall 122. The third adhesive portion 51 and the fourth adhesive portion 52 are integrally disposed, which enables the second adhesive member 50 to be more stably fixed to the second sidewall 122. In some embodiments, the third adhesive portion 51 is fixedly disposed with the filling portion 301. The cooperation between the second adhesive member 50 and the sealing member 30 can further improve the sealing strength between the sealing member 30 and the outer shell 10, which is beneficial to further reduce the possibility of relative torsion between the first shell 11 and the second shell 12.

[0061] In some embodiments, the third adhesive portion 51 is bonded and fixed to the filling portion 301. In some embodiments, the third adhesive portion 51 is fused and fixed to the filling portion 301.

[0062] In some embodiments, the third adhesive portion 51 is integrally formed with the filler portion 301. This improves the stability of the connection between the third adhesive portion 51 and the filler portion 301. In some embodiments, before assembling the first housing 11 and the second housing 12, a second adhesive member 50 is pre-attached to the second sidewall 122 to form the third adhesive portion 51 and the fourth adhesive portion 52, so that the filler portion 301 is fused with the third adhesive portion 51 in a molten state, and after cooling, the filler portion 301 is integrally formed with the third adhesive portion 51.

[0063] In some embodiments, the thickness of the third adhesive portion 51 is H3, where 3μm ≤ H3 ≤ 500μm. For example, H3 is 3μm, 6μm, 10μm, 20μm, 50μm, 100μm, 200μm, 300μm, 500μm, or a range between the listed endpoint values, or any value between the listed endpoint values. By setting 3μm ≤ H3, it is beneficial to reduce the risk of short circuits caused by burrs piercing the third adhesive portion 51 after the filling portion 301 melts. By setting H3 ≤ 500μm, it is beneficial to improve the energy density of the secondary battery 100. The thickness of the third adhesive portion 51 is the dimension of the third adhesive portion 51 along the direction perpendicular to the second surface 1221.

[0064] In some embodiments, 6μm ≤ H3 ≤ 200μm. Setting 6μm ≤ H3 helps to further reduce the risk of short circuits caused by burrs piercing the third adhesive portion 51 after the filler portion 301 melts. Setting H3 ≤ 200μm helps to further improve the energy density of the secondary battery 100.

[0065] In some embodiments, the thickness of the fourth adhesive portion 52 is H4, where 90%H3≤H4≤110%H3. Considering the precision of the processing technology, setting 90%H3≤H4≤110%H3 facilitates the integral installation of the third adhesive portion 51 and the fourth adhesive portion 52. The thickness of the fourth adhesive portion 52 is a dimension along a direction perpendicular to the second sidewall 122.

[0066] In some embodiments, the width of the third adhesive portion 51 is W3, where W3 is less than or equal to the wall thickness of the second sidewall 122. Considering the precision of the manufacturing process, when W3 is greater than the wall thickness of the second sidewall 122 within a 10% error range, W3 can also be considered equal to the wall thickness of the second sidewall 122. The width of the third adhesive portion 51 is the dimension of the third adhesive portion 51 along a direction parallel to the second surface 1221.

[0067] In some embodiments, the width of the fourth adhesive portion 52 is W4, where 30μm ≤ W4 ≤ 3000μm. For example, W4 can be 30μm, 50μm, 100μm, 200μm, 500μm, 1000μm, 1500μm, 3000μm, or any value between the listed endpoint values. By setting 30μm ≤ W4, the bonding area between the fourth adhesive portion 52 and the inner wall of the second sidewall 122 is not too small, which helps to improve the stability of the fourth adhesive portion 52 on the inner wall of the second sidewall 122. Furthermore, when the third adhesive portion 51 and the filling portion 301 are integrally provided, setting 30μm ≤ W4 also helps to reduce the possibility of electrolyte erosion at the interface between the fourth adhesive portion 52 and the second sidewall 122. By setting W4 ≤ 3000 μm, the bonding area between the fourth adhesive portion 52 and the inner wall of the second sidewall 122 is not too large. When the polarity of the electrode assembly 20 is led out through the second sidewall 122, the second sidewall 122 can have a larger area for connection, which is beneficial to improving the convenience of connecting the electrode assembly 20 and the second sidewall 122. The width of the fourth adhesive portion 52 is the dimension of the fourth adhesive portion 52 along the extending direction of the second sidewall 122.

[0068] In some embodiments, 100μm ≤ W4 ≤ 1500μm. Setting 100μm ≤ W4 helps to further improve the stability of the fourth adhesive portion 52 on the inner wall of the second sidewall 122. Furthermore, when the third adhesive portion 51 and the filling portion 301 are integrally formed, setting 100μm ≤ W4 also helps to further reduce the possibility of electrolyte erosion at the interface between the fourth adhesive portion 52 and the second sidewall 122. Setting W4 ≤ 1500μm further improves the ease of connection between the electrode assembly 20 and the second sidewall 122.

[0069] In some embodiments, the melting point of the second adhesive 50 is between 95°C and 130°C. For example, the melting point of the second adhesive 50 is 95°C, 100°C, 110°C, 130°C, or a range between the listed endpoint values, or any value between the listed endpoint values. In some embodiments, the melting point of the second adhesive 50 is between 150°C and 500°C. For example, the melting point of the second adhesive 50 is 150°C, 200°C, 250°C, 300°C, 500°C, or a range between the listed endpoint values, or any value between the listed endpoint values.

[0070] In some embodiments, the distance between the first surface 1121 and the second surface 1221 is D, where 20 μm ≤ D ≤ 5000 μm. For example, D can be 20 μm, 40 μm, 100 μm, 200 μm, 500 μm, 1000 μm, 2000 μm, 3000 μm, 5000 μm, or any value between the listed endpoints. By setting D to 20 μm ≤ D, the distance between the first surface 1121 and the second surface 1221 is not too small, which helps to reduce the possibility of short circuits caused by burr contact between the first housing 11 and the second housing 12. By setting D ≤ 5000 μm, the distance between the first surface 1121 and the second surface 1221 is not too large, which helps to improve the energy density of the secondary battery 100.

[0071] In some embodiments, 40 μm ≤ D ≤ 3000 μm. By setting 40 μm ≤ D, it is beneficial to further reduce the possibility of short circuits caused by burr contact between the first housing 11 and the second housing 12. By setting D ≤ 3000 μm, it is beneficial to further improve the energy density of the secondary battery 100.

[0072] In some embodiments, please refer to Figure 4 and Figure 5 The sealing element 30 includes a first adhesive layer 31, which is bonded to the outer periphery of the first sidewall 112 and the second sidewall 122. The filling part 301 is connected to the first adhesive layer 31. The bonding of the first adhesive layer 31 to the first sidewall 112 and the second sidewall 122 helps to improve the stability of the bonding between the sealing element 30 and the outer shell 10.

[0073] In some embodiments, the filler portion 301 is integrally formed with the first adhesive layer 31. The filler portion 301 can be formed directly by melting a portion of the first adhesive layer 31 and then cooling it into the gap between the first surface 1121 and the second surface 1221. This simplifies the assembly process of the secondary battery 100 and streamlines the manufacturing process. Furthermore, the integral formation of the filler portion 301 with the first adhesive layer 31 ensures a tight fit between the first surface 1121 and the second surface 1221, improving the sealing performance of the sealant 30 on the first housing 11 and the second housing 12. In other embodiments, the filler portion 301 and the first adhesive layer 31 are separate components.

[0074] In some embodiments, the first adhesive layer 31 can be heated to melt or de-adhere, forming part of a pressure relief channel communicating with the receiving cavity 101. When the secondary battery 100 experiences thermal runaway, the melting or de-adhesion of the first adhesive layer 31 can promptly relieve pressure in the receiving cavity 101, which helps improve the safety of the secondary battery 100.

[0075] In some embodiments, the melting point of the first adhesive layer 31 is between 95°C and 130°C. For example, the melting point of the first adhesive layer 31 is 95°C, 100°C, 110°C, 130°C, or a range between the listed endpoints or any value between the listed endpoints. By setting the melting point of the first adhesive layer 31 to between 95°C and 130°C, the possibility of the first adhesive layer 31 melting or losing adhesion before the secondary battery 100 experiences thermal runaway can be reduced, which is beneficial for maintaining the sealing effect of the sealant 30 on the outer casing 10. Furthermore, it can ensure that the first adhesive layer 31 melts or loses adhesion in a timely manner when the secondary battery 100 experiences thermal runaway, thereby relieving pressure in the receiving cavity 101 and improving the safety of the secondary battery 100. It should be understood that when the filler 301 is integrally formed with the first adhesive layer 31, and the filler 301 is formed directly by melting a portion of the first adhesive layer 31 and entering the gap between the first surface 1121 and the second surface 1221 and then cooling, the melting point of the filler 301 is basically the same as the melting point of the first adhesive layer 31.

[0076] In some embodiments, the first housing 11 and the second housing 12 have the same polarity, and at least one of the first adhesive 40 and the filler 301 has a melting point of 95°C to 130°C, and the first adhesive layer 31 has a melting point of 95°C to 130°C. This reduces the possibility that at least one of the first adhesive 40 and the filler 301 may melt or lose adhesion before the secondary battery 100 experiences thermal runaway, which is beneficial for maintaining the sealing effect of the sealant 30 on the outer casing 10. Furthermore, it facilitates the timely melting or loss of adhesion of at least one of the first adhesive 40, the filler 301, and the first adhesive layer 31 in the event of thermal runaway of the secondary battery 100, thereby depressurizing the receiving cavity 101 and improving the safety of the secondary battery 100.

[0077] In some embodiments, the first housing 11 and the second housing 12 have the same polarity, and at least one of the second adhesive 50 and the filler 301 has a melting point of 95°C to 130°C, and the first adhesive layer 31 has a melting point of 95°C to 130°C. This reduces the possibility that at least one of the second adhesive 50 and the filler 301 may melt or lose adhesion before the secondary battery 100 experiences thermal runaway, which is beneficial for maintaining the sealing effect of the sealant 30 on the outer casing 10. Furthermore, it facilitates the timely melting or loss of adhesion of at least one of the second adhesive 50, the filler 301, and the first adhesive layer 31 in the event of thermal runaway of the secondary battery 100, thereby depressurizing the receiving cavity 101 and improving the safety of the secondary battery 100.

[0078] In some embodiments, the first housing 11 and the second housing 12 have different polarities, the melting point of the first adhesive layer 31 is 95°C to 130°C, the melting point of the filler 301 is 95°C to 130°C, and the melting point of the first adhesive 40 is 150°C to 500°C. When the secondary battery 100 experiences thermal runaway, it is possible to facilitate the timely melting or loss of adhesion of the first adhesive layer 31 and the filler 301 to relieve pressure in the receiving cavity 101, while reducing the possibility of the first adhesive 40 melting or losing adhesion. This helps to reduce the risk of short circuits between the first housing 11 and the second housing 12. Alternatively, the melting point of the first adhesive layer 31 is 95°C to 130°C, the melting point of the filling part 301 is 150°C to 500°C, and the melting point of the first adhesive member 40 is 95°C to 130°C. When the secondary battery 100 experiences thermal runaway, the first adhesive layer 31 and the first adhesive member 40 can melt or lose adhesion in time to relieve pressure in the receiving cavity 101, while reducing the possibility of the filling part 301 melting. This helps to reduce the risk of short circuit between the first housing 11 and the second housing 12.

[0079] In some embodiments, the first housing 11 and the second housing 12 have different polarities. The melting point of the first adhesive layer 31 is 95°C to 130°C, the melting point of the filler 301 is 95°C to 130°C, and the melting point of the second adhesive 50 is 150°C to 500°C. When the secondary battery 100 experiences thermal runaway, the first adhesive layer 31 and the filler 301 can melt or lose adhesion in time to relieve pressure in the receiving cavity 101, while reducing the possibility of the second adhesive 50 melting or losing adhesion. This helps to reduce the risk of short circuit between the first housing 11 and the second housing 12. Alternatively, the melting point of the first adhesive layer 31 is 95°C to 130°C, the melting point of the filler 301 is 150°C to 500°C, and the melting point of the second adhesive 50 is 95°C to 130°C. When the secondary battery 100 experiences thermal runaway, the first adhesive layer 31 and the second adhesive 50 can melt or lose adhesion in time to relieve pressure in the receiving cavity 101, while reducing the possibility of the filler 301 melting. This helps to reduce the risk of short circuit between the first housing 11 and the second housing 12.

[0080] In some embodiments, the material of the first adhesive layer 31 includes an electrolyte-resistant polymer, and the polymer of the first adhesive layer 31 includes at least one selected from polyolefins, fluororubber, and polyurethane. The polyolefin may include polypropylene and polyethylene, etc. This allows the first adhesive layer 31 to have high resistance to electrolyte corrosion. In some embodiments, the first adhesive layer 31 comprises a single layer or multiple layers of polymer.

[0081] In some embodiments, please refer to Figure 4 and Figure 5 The sealing element 30 includes a metal layer 32, which is disposed on the side of the first adhesive layer 31 away from the outer shell 10. The water resistance of the metal layer 32 is better than that of the first adhesive layer 31, which is beneficial to improving the sealing performance of the sealing element 30 to the first shell 11 and the second shell 12.

[0082] In some embodiments, the material of the metal layer 32 includes at least one selected from steel, aluminum, nickel, silver, copper, and alloys thereof. In some embodiments, the metal layer 32 is a single-layer or multi-layer structure. For example, a multi-layer structure is a steel layer plus an aluminum layer or a nickel layer plus a copper layer, etc.

[0083] In some embodiments, please refer to Figure 4 and Figure 5 The seal 30 includes a second adhesive layer 33, which is disposed on the side of the metal layer 32 opposite to the first adhesive layer 31. The second adhesive layer 33 can protect the metal layer 32, which helps to reduce the risk of failure of the metal layer 32.

[0084] In some embodiments, the melting point of the second adhesive layer 33 is greater than that of the first adhesive layer 31. In some embodiments, the melting point difference between the second adhesive layer 33 and the first adhesive layer 31 is greater than 10°C.

[0085] In some embodiments, the melting point of the second adhesive layer 33 is between 140°C and 500°C. For example, the melting point of the second adhesive layer 33 is 140°C, 160°C, 200°C, 250°C, 300°C, 500°C, or any value between the listed endpoints.

[0086] In some embodiments, the material of the second adhesive layer 33 includes an electrolyte-resistant polymer, and the polymer of the second adhesive layer 33 includes at least one selected from polyolefins, fluoropolymers, polyetheretherketones, fluororubber, and polyurethanes. The polyolefins may include polypropylene and polyethylene, and the fluoropolymers may be, for example, polytetrafluoroethylene. This allows the second adhesive layer 33 to have high resistance to electrolyte corrosion. In some embodiments, the second adhesive layer 33 comprises a single layer or multiple layers of polymer.

[0087] It should be understood that when the sealing element 30 simultaneously includes a first adhesive layer 31, a metal layer 32, and a second adhesive layer 33, the first adhesive layer 31 and the second adhesive layer 33 are respectively disposed on both sides of the metal layer 32 along the thickness direction of the metal layer 32. In some embodiments, the first adhesive layer 31 is fixed to the metal layer 32, and the second adhesive layer 33 is fixed to the metal layer 32 by adhesive bonding, so that the first adhesive layer 31, the metal layer 32, and the second adhesive layer 33 are combined into a whole. In some embodiments, the first adhesive layer 31 is fixed to the metal layer 32, and the second adhesive layer 33 is fixed to the metal layer 32 by hot pressing, so that the first adhesive layer 31, the metal layer 32, and the second adhesive layer 33 are combined into a whole. During the long-term use of the secondary battery 100, it is beneficial to maintain the sealing performance of the sealing element 30 to the first housing 11 and the second housing 12.

[0088] In some embodiments, along the thickness direction of the seal 30, the thickness of the first adhesive layer 31 is d1, the thickness of the metal layer 32 is d2, and the thickness of the second adhesive layer 33 is d3, where 7μm≤d1≤500μm, 7μm≤d2≤250μm, and 6μm≤d3≤500μm. For example, d1 is any value between 7μm, 10μm, 20μm, 50μm, 100μm, 200μm, 500μm, or any of the listed endpoint values; d2 is any value between 7μm, 10μm, 20μm, 50μm, 100μm, 150μm, 250μm, or any of the listed endpoint values; and d3 is any value between 6μm, 8μm, 20μm, 50μm, 100μm, 200μm, 500μm, or any of the listed endpoint values. By setting 7μm≤d1, 7μm≤d2, and 6μm≤d3, the first adhesive layer 31, metal layer 32, and second adhesive layer 33 are not too thin, which helps reduce the risk of the first adhesive layer 31 being corroded and failing by the electrolyte. It also helps reduce the risk of the second adhesive layer 33 breaking after the secondary battery 100 is dropped, leading to the failure of the metal layer 32 or its erosion. By setting d1≤500μm, d2≤250μm, and d3≤500μm, the first adhesive layer 31, metal layer 32, and second adhesive layer 33 are not too thick, which helps improve the energy density of the secondary battery 100.

[0089] In some embodiments, 10μm≤d1≤200μm, 10μm≤d2≤150μm, and 8μm≤d3≤200μm. By setting 10μm≤d1, 10μm≤d2, and 8μm≤d3, the first adhesive layer 31, the metal layer 32, and the second adhesive layer 33 can be made thicker. This helps to further reduce the risk of the first adhesive layer 31 being corroded and failed by the electrolyte, and further reduces the risk of the second adhesive layer 33 breaking after the secondary battery 100 is dropped, leading to the failure of the metal layer 32 or its corrosion failure. By setting d1≤200μm, d2≤150μm, and d3≤200μm, the energy density of the secondary battery 100 can be further improved while ensuring that the thickness of the first adhesive layer 31 is basically sufficient to prevent corrosion failure by the electrolyte, the thickness of the second adhesive layer 33 is sufficient for most drop scenarios, and the thickness of the metal layer 32 is basically sufficient to prevent failure due to breakage or corrosion.

[0090] In some embodiments, the thickness of the first adhesive layer 31 may be uniform or non-uniform. In some embodiments, the thickness of the metal layer 32 may be uniform or non-uniform. In some embodiments, the thickness of the second adhesive layer 33 may be uniform or non-uniform. In some embodiments, the thickness of the seal 30 may be uniform or non-uniform, and the thickness of the seal 30 is equal to the sum of the thicknesses of the first adhesive layer 31, the metal layer 32, and the second adhesive layer 33.

[0091] In some embodiments, please refer to Figure 4 and Figure 5 The secondary battery 100 also includes a retainer 60, which adheres to the outer casing 10 and the electrode assembly 20. This helps reduce the risk of the electrode assembly 20 shifting within the receiving cavity 101, causing the first casing 11 and / or the second casing 12 to detach from the seal 30. In some embodiments, the retainer 60 is disposed between the outer casing 10 and the electrode assembly 20 along the thickness direction of the electrode assembly 20. In some embodiments, the retainer 60 is a hot melt adhesive.

[0092] Please see Figure 7 One embodiment of this application provides an electrical device 1000, including the secondary battery 100 as described above. The secondary battery 100 has good sealing performance, and the electrolyte is not easily leaked, which helps to extend the service life of the electrical device 1000. The electrical device 1000 includes, but is not limited to, electronic devices such as e-book players, mobile phones, fax machines, copiers, printers, headphones, video recorders, LCD TVs, tape recorders, radios, cameras, tablet computers, and laptop computers.

[0093] Furthermore, those skilled in the art should recognize that the above embodiments are merely illustrative of this application and are not intended to limit this application. Any appropriate changes and modifications made to the above embodiments within the substantive scope of this application fall within the scope of this application's disclosure.

Claims

1. A secondary battery, characterized in that, include: The outer casing includes a first casing and a second casing, the first casing and the second casing together forming a receiving cavity, the receiving cavity being filled with an electrolyte; the first casing includes a first wall and a first sidewall connecting the periphery of the first wall, the second casing includes a second wall and a second sidewall connecting the periphery of the second wall, the first sidewall has a first surface facing the second sidewall along the extending direction of the first sidewall, the second sidewall has a second surface facing the first sidewall along the extending direction of the second sidewall, the first surface and the second surface are disposed facing each other and have a gap; The electrode assembly is disposed within the receiving cavity; A sealing element is disposed around the outer periphery of the first sidewall and the second sidewall, and seals the gap; the sealing element includes a filling portion disposed in the gap; as well as A first adhesive component is disposed on the first sidewall. The first adhesive component includes a first adhesive portion and a second adhesive portion. The first adhesive portion is disposed on a first surface of the first sidewall, and the second adhesive portion is disposed on an inner wall of the first sidewall. The first adhesive portion and the second adhesive portion are integrally disposed together. The first adhesive portion is fixedly disposed with the filling portion.

2. The secondary battery according to claim 1, characterized in that, The secondary battery further includes a second adhesive component, which is disposed on the second sidewall. The second adhesive component includes a third adhesive portion and a fourth adhesive portion. The third adhesive portion is disposed on the second surface of the second sidewall, and the fourth adhesive portion is disposed on the inner wall of the second sidewall. The third adhesive portion and the fourth adhesive portion are integrally disposed together. The third adhesive portion is fixedly disposed with the filling portion.

3. The secondary battery according to claim 1, characterized in that, The distance between the first surface and the second surface is D, where 20μm≤D≤5000μm.

4. The secondary battery according to claim 3, characterized in that, 40μm≤D≤3000μm.

5. The secondary battery according to claim 2, characterized in that, The thickness of the first adhesive portion is H1, the thickness of the second adhesive portion is H2, 3μm≤H1≤500μm, 90%H1≤H2≤110%H1; the thickness of the third adhesive portion is H3, the thickness of the fourth adhesive portion is H4, 3μm≤H3≤500μm, 90%H3≤H4≤110%H3.

6. The secondary battery according to claim 5, characterized in that, 6μm≤H1≤200μm; 6μm≤H3≤200μm.

7. The secondary battery according to claim 2, characterized in that, The first adhesive portion is integrally formed with the filling portion, and the third adhesive portion is integrally formed with the filling portion.

8. The secondary battery according to claim 2 or 7, characterized in that, The width of the second adhesive part is W2, 30μm≤W2≤3000μm, and the width of the fourth adhesive part is W4, 30μm≤W4≤3000μm.

9. The secondary battery according to claim 8, characterized in that, 100μm≤W2≤1500μm, 100μm≤W4≤1500μm.

10. The secondary battery according to claim 1, characterized in that, The sealing element includes a first adhesive layer, a metal layer, and a second adhesive layer. Along the thickness direction of the metal layer, the first adhesive layer and the second adhesive layer are respectively disposed on both sides of the metal layer. The first adhesive layer is adhered to the outer periphery of the first sidewall and the second sidewall. The filling part is integrally disposed with the first adhesive layer.

11. The secondary battery according to claim 10, characterized in that, Along the thickness direction of the seal, the thickness of the first adhesive layer is d1, the thickness of the metal layer is d2, and the thickness of the second adhesive layer is d3, where 7μm≤d1≤500μm, 7μm≤d2≤250μm, and 6μm≤d3≤500μm.

12. The secondary battery according to claim 11, characterized in that, 10μm≤d1≤200μm, 10μm≤d2≤150μm, 8μm≤d3≤200μm.

13. An electrical appliance, characterized in that, Includes the secondary battery as described in any one of claims 1 to 12.

Citation Information

Patent Citations

  • Secondary battery

    CN106207244A

  • Secondary battery and electric device

    CN119674379A