Concealer composition, preparation method thereof and concealer pen

By using a mixture of polysiloxane and plant oils, synthetic waxes and specific film-forming agents in concealer products, a concealer composition with high coverage, long-lasting effect and good skin feel is formed, solving the problems of insufficient long-lasting effect and skin feel of existing concealer products and improving the user experience.

CN121370667APending Publication Date: 2026-01-23JOTM DAILY CHEM HANGZHOU CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202511862619.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-12-11
Publication Date
2026-01-23

AI Technical Summary

Technical Problem

Existing concealer products are inadequate in terms of staying power, skin feel, and user experience, and are prone to problems such as makeup smudging, creasing, or skin irritation.

Method used

A concealer composition with high coverage, long-lasting effect and good skin feel is formed by using a mixture of polysiloxane and plant oil as a moisturizer, synthetic wax as a plasticizer, and organosilicone ester and polysiloxane-silicone-organic hydrocarbon copolymer as a film-forming agent.

Benefits of technology

It achieves high coverage, long-lasting wear, stability, and a pleasant skin feel in concealer products, solving problems such as makeup fading, creasing, and skin irritation, and improving the user experience.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of cosmetics, and discloses a concealer composition, a preparation method thereof and a concealer pen. The concealer composition comprises the following raw material components: an emollient I, an emollient II, a plasticizer, a film-forming agent I, a film-forming agent II, a thickening agent, an antioxidant I, an antioxidant II, a dispersing agent, a preservative and a coloring agent, the emollient I is a mixture of polysiloxane and vegetable fat; the emollient II is a mixture of at least two kinds of polysiloxane; the plasticizer is synthetic wax; the film-forming agent I is organic silicate ester; and the film-forming agent II is a mixture of polysiloxane and a silicone-organic alkyl copolymer. The preparation method is simple, efficient and controllable in condition, the prepared concealer composition has high covering power, durability, stability and good skin feeling, and the problems that an existing concealer product is prone to makeup removal, powder blocking or skin irritation are solved.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present application relates to the technical field of cosmetics, in particular to a concealer composition, a preparation method thereof and a concealer pen. BACKGROUND

[0002] As an important category in the field of cosmetics, the concealer product is mainly used to cover up facial dark circles, acne marks, redness, and other blemishes, helping to improve the completeness and delicacy of makeup, and has become an essential product in daily makeup and professional makeup scenes. With the acceleration of consumers' life pace and the continuous improvement of the demand for long-lasting makeup, a large number of concealer products claiming long-lasting makeup have emerged in the market, and the types of concealer products are becoming more and more diverse.

[0003] In the prior art, in order to achieve the long-lasting effect of the concealer product, the industry mainly adopts the following methods: one is to add a high-adhesion acrylic film-forming agent to form a film on the skin surface to lock the makeup, which to some extent prolongs the makeup time, but the film has poor extensibility and insufficient air permeability, which can easily cause skin tightness and dryness; two is to rely on oil-absorbing powders such as silica and nylon powder to delay makeup removal by adsorbing facial sebum, but this can make the product texture heavy and the makeup feel rough, and can easily cause problems such as lines and powder floating; three is to increase the content of waxy base to increase the melting point of the product and enhance the anti-sweating performance, but a high proportion of wax can cause the product to be difficult to apply, and repeated application is required to evenly cover up the blemishes, which can cause a rough skin feel and affect the user experience. Moreover, most products can still cause obvious makeup removal under conditions such as intense exercise or long-term wearing of a mask. SUMMARY

[0004] In order to at least overcome one of the problems existing in the prior art, one of the purposes of the present application is to provide a concealer composition, which has high hiding power, durability, stability and good skin feel through the synergistic cooperation between the raw material components, solving the problem of easy makeup removal, powder blocking or skin irritation of existing concealer products. The second purpose of the present application is to provide a preparation method of the concealer composition. The third purpose of the present application is to provide a concealer pen.

[0005] To this end, the present application adopts the following technical solutions: The first aspect of the present application provides a concealer composition, the raw material components of which include: emollient I, emollient II, plasticizer, film-forming agent I, film-forming agent II, thickening agent, antioxidant I, antioxidant II, dispersant, preservative and colorant; wherein the emollient I is a mixture of polysiloxane and vegetable oil; the emollient II is a mixture of at least two or more polysiloxanes; the plasticizer is a synthetic wax; the film-forming agent I is an organosilicate; and the film-forming agent II is a mixture of polysiloxane and silicone-organic hydrocarbon copolymer.

[0006] In the raw material components of the concealer composition of the present application, the emollient I adopts a mixture of polysiloxane and vegetable oil, the polysiloxane gives the skin a smooth touch and has good spreadability, which can make the product more uniform and easy to push when applying; the vegetable oil is rich in various nutrients, which can nourish the skin, supplement nutrients to the skin, enhance the moisturizing ability of the skin, keep the skin moist while concealing, and reduce the dryness and powder sticking phenomenon of the skin; the emollient II selects a mixture of at least two kinds of polysiloxane, the different types of polysiloxane are matched with each other, which can further optimize the skin feel of the product, improve the stability and compatibility of the product, and keep the product in good condition during storage and use; the plasticizer is a synthetic wax, which can increase the hardness and formability of the product, ensure that the concealer composition has a suitable texture, and is convenient to apply and maintain; the film former I is an organosilicon ester, which helps to form a uniform and breathable film on the skin surface, enhances the durability and water resistance of the product, and makes the concealing effect more durable and less affected by sweat, oil and other factors; the film former II is a mixture of polysiloxane and silicone-organic hydrocarbon copolymer, which not only has a film forming effect, but also improves the affinity of the product to the skin, makes the product more conformable to the skin, further improves the adhesion of the product, makes the concealing effect more uniform and resistant to friction, and reduces the makeup removal. The mutual cooperation between the components makes the concealer composition of the present application have high hiding power, durability, stability and good skin feel, which meets the market demand for concealer products in the cosmetic field.

[0007] Preferably, the weight ratio of polysiloxane to vegetable oil in the emollient I is (5-7):(1.5-3.5). Further preferably, the weight ratio of polysiloxane to vegetable oil in the emollient I is (5.5-7):(1.5-3.5). Still further preferably, the weight ratio of polysiloxane to vegetable oil in the emollient I is (5.9-7):(1.5-3.5).

[0008] Preferably, the weight ratio of polysiloxane to silicone-organic hydrocarbon copolymer in the film former II is (12-15):(5-8). Further preferably, the weight ratio of polysiloxane to silicone-organic hydrocarbon copolymer in the film former II is (13-15):(5-8). Still further preferably, the weight ratio of polysiloxane to silicone-organic hydrocarbon copolymer in the film former II is (13.5-15):(6-8).

[0009] The weight ratio of the polysiloxane and the plant oil in the emollient I is (5-7):(1.5-3.5), which optimizes the balance between smoothness and nourishment, avoids being too oily or dry, provides a more comfortable application experience for the user, and also enhances the stability of the composition. The weight ratio of the polysiloxane and the silicone-organic hydrocarbon copolymer in the film former II is (12-15):(5-8), the polysiloxane helps to form a thin film with certain flexibility and air permeability, and the silicone-organic hydrocarbon copolymer can enhance the adhesion of the thin film to the skin. The combination of the two makes the thin film less likely to crack or fall off when the user's facial expression changes, thereby further improving the durability and stability of the concealing effect.

[0010] Preferably, the polysiloxane is selected from at least one of dimethicone, methyl trimethicone, octyl methicone, phenyl trimethicone, lauryl dimethicone. Further preferably, the polysiloxane is selected from at least one of dimethicone, methyl trimethicone, octyl methicone, phenyl trimethicone.

[0011] Preferably, the emollient II is a mixture of methyl trimethicone and octyl methicone. Further preferably, the weight ratio of methyl trimethicone and octyl methicone in the emollient II is (20-24):(1-3). Still further preferably, the weight ratio of methyl trimethicone and octyl methicone in the emollient II is (21-24):(2-3).

[0012] Preferably, the plant oil is selected from at least one of camellia (CAMELLIA JAPONICA) seed oil, jojoba (SIMMONDSIA CHINENSIS) seed oil, sunflower (HELIANTHUS ANNUUS) seed oil, meadowfoam (LIMNANTHES ALBA) seed oil, shea (BUTYROSPERMUM PARKII) butter. Further preferably, the plant oil is selected from at least one of camellia (CAMELLIA JAPONICA) seed oil, jojoba (SIMMONDSIA CHINENSIS) seed oil, sunflower (HELIANTHUS ANNUUS) seed oil, meadowfoam (LIMNANTHES ALBA) seed oil. Still further preferably, the plant oil is selected from at least one of camellia (CAMELLIA JAPONICA) seed oil, jojoba (SIMMONDSIA CHINENSIS) seed oil, sunflower (HELIANTHUS ANNUUS) seed oil.

[0013] Preferably, the synthetic wax is a polyolefin-based synthetic wax or an ester-based synthetic wax. Further preferably, the synthetic wax is a polyolefin-based synthetic wax. Still further preferably, the synthetic wax is at least one of a polyethylene wax, a polypropylene wax, a microcrystalline wax, an ethylene-vinyl acetate copolymer wax.

[0014] Preferably, the organosiliconate is at least one of trimethylsiloxysilicate, polymethylsilicate, triisostearyl polymethylsilicate, perfluoropolyisopropyl methyl silicate. Further preferably, the organosiliconate is at least one of trimethylsiloxysilicate, polymethylsilicate, triisostearyl polymethylsilicate.

[0015] Preferably, the silicone-organic hydrocarbon copolymer is at least one of an acrylate / polydimethylsiloxane copolymer, an acrylate / polytrimethylsiloxane methacrylate copolymer, an acrylate / polydimethylsiloxane crosspolymer. Further preferably, the silicone-organic hydrocarbon copolymer is at least one of an acrylate / polydimethylsiloxane copolymer, an acrylate / polytrimethylsiloxane methacrylate copolymer.

[0016] In the above technical solution, each of the selected polysiloxanes has unique performance advantages. For example, polydimethylsiloxane has good lubricity and air permeability, can form a light, breathable protective film on the skin surface, making the product more smooth when applied, without causing a heavy feeling on the skin, and allowing the skin to breathe freely; methyl polytrimethylsiloxane has low volatility, which helps to prolong the product's persistence on the skin and maintain the integrity of the makeup. By selecting at least one of these polysiloxanes as a raw material, the skin feel, stability and persistence of the concealer composition can be optimized, meeting the diverse needs of users for product performance.

[0017] Plant oils are rich in various nutrients such as unsaturated fatty acids, vitamins, minerals, etc., and have excellent moisturizing and hydrating properties. For example, camellia (CAMELLIA JAPONICA) seed oil contains rich oleic acid, which can penetrate deep into the skin, nourish the skin, enhance the skin's barrier function, prevent water loss, and keep the skin moist and smooth; the molecular structure of jojoba seed oil is similar to human sebum, has good skin affinity, can regulate the water-oil balance of the skin, and also has good conditioning effect on oily skin, while also supplying nutrients to the skin and improving the dry and rough condition of the skin. Incorporating these plant oils as one of the components of the emollient I not only provides sufficient nourishment and nutrients to the skin, but also enhances the affinity of the product to the skin, making the concealer composition more conformable to the skin, improving the comfort and naturalness of the concealing effect.

[0018] The synthetic wax is a polyolefin synthetic wax or an ester synthetic wax, which has high hardness and melting point, can effectively increase the formability and stability of the product, ensure that the concealer composition can maintain good texture and shape under different storage conditions and use environments, facilitate application and use, and also improve the heat resistance of the product to prevent deformation or melting of the product in a high-temperature environment.

[0019] The organosilicate is selected from at least one of trimethylsiloxysilicate, polymethylsilicate, triisostearyl polymethylsilicate, perfluoropolyisopropyl silicate, and the organosilicate has good film-forming property and water resistance, can form a tight and uniform film on the skin surface, effectively locks in moisture and pigments, enhances the durability and water resistance of the concealing effect, makes the product less likely to be washed away by sweat, and helps maintain the integrity of the makeup.

[0020] The silicone-organic hydrocarbon copolymer is selected from at least one of acrylate / polydimethylsiloxane copolymer, acrylate / polytrimethylsiloxane methacrylate copolymer, and acrylate / polydimethylsiloxane crosslinked polymer, can significantly improve the affinity of the product to the skin, makes the film formed by the film-forming agent II more closely adhere to the skin and less likely to fall off, and further improves the stability and durability of the concealing effect.

[0021] Preferably, the thickening agent is selected from at least one of bis-diglyceryl polyacyladipate-2, polyglyceryl-2 stearate, polyglyceryl-2 dipolyhydroxystearate, and isononyl isononanoate. Further preferably, the thickening agent is selected from at least one of bis-diglyceryl polyacyladipate-2, polyglyceryl-2 stearate, and polyglyceryl-2 dipolyhydroxystearate. More preferably, the thickening agent is selected from at least one of bis-diglyceryl polyacyladipate-2 and polyglyceryl-2 stearate.

[0022] Preferably, the antioxidant I is selected from at least one of tetrahexyldecyl ascorbate, ascorbyl palmitate, propyl gallate, and pentaerythrityl tetra-di-t-butyl hydroxyhydrocinnamate. Further preferably, the antioxidant I is selected from at least one of tetrahexyldecyl ascorbate, propyl gallate, and pentaerythrityl tetra-di-t-butyl hydroxyhydrocinnamate. More preferably, the antioxidant I is selected from at least one of tetrahexyldecyl ascorbate and pentaerythrityl tetra-di-t-butyl hydroxyhydrocinnamate.

[0023] Preferably, the antioxidant II is selected from at least one of ascorbyl glucoside, tea polyphenols, and tocopheryl acetate. Further preferably, the antioxidant II is selected from at least one of ascorbyl glucoside and tocopheryl acetate.

[0024] Preferably, the dispersing agent is selected from at least one of polyhydroxystearic acid, polyhydroxystearic acid ethyl ester, octyldodecyl polyhydroxystearate, polyhydroxystearic acid glyceryl ester. Further preferably, the dispersing agent is selected from at least one of polyhydroxystearic acid, polyhydroxystearic acid ethyl ester, octyldodecyl polyhydroxystearate.

[0025] Preferably, the preservative is selected from at least one of phenoxyethanol, ethylhexylglycerin, p-hydroxyacetophenone, sodium dehydroacetate. Further preferably, the preservative is selected from at least one of phenoxyethanol, ethylhexylglycerin, p-hydroxyacetophenone.

[0026] Preferably, the colorant is a mixture of CI 77491, CI 77492, CI 77499, CI 77891, triethoxyoctylsilane, aluminum hydroxide. Further preferably, the colorant is a mixture of CI 77891-aluminum hydroxide-triethoxyoctylsilane, CI 77491-triethoxyoctylsilane, CI 77492-triethoxyoctylsilane, CI 77499-triethoxyoctylsilane. Still further preferably, in the colorant, the weight ratio of the mixture of CI 77891-aluminum hydroxide-triethoxyoctylsilane, CI 77491-triethoxyoctylsilane, CI 77492-triethoxyoctylsilane, CI 77499-triethoxyoctylsilane is (25-30):(0.7-1):(6-8):(0.4-0.7).

[0027] Preferably, in the colorant, the CI 77891-aluminum hydroxide-triethoxyoctylsilane is a mixture of CI 77891, aluminum hydroxide, triethoxyoctylsilane with mass fractions of 96.5%, 2.5% and 1% respectively, the CI 77491-triethoxyoctylsilane is a mixture of CI 77491 and triethoxyoctylsilane with mass fractions of 99% and 1% respectively, the CI 77492-triethoxyoctylsilane is a mixture of CI 77492 and triethoxyoctylsilane with mass fractions of 99% and 1% respectively, and the CI 77499-triethoxyoctylsilane is a mixture of CI 77499 and triethoxyoctylsilane with mass fractions of 99% and 1% respectively.

[0028] In the above technical solution, the specific selection of the thickening agent controls the viscosity and texture of the composition, making it easy to apply but not easy to flow, reducing the phenomenon of easy flow of the product or the product being too thick to push away. The combination of antioxidants I and II provides a synergistic antioxidant effect, prevents the oxidation of the composition, and protects the skin from free radical damage. The specific type of dispersing agent ensures uniform dispersion of the powder such as colorant, avoids clumping or settling, and improves the uniformity of the hiding power. The specific selection of the preservative provides broad-spectrum antibacterial protection, inhibits the growth and reproduction of microorganisms, and ensures the safety and hygiene of the product during storage and use. The mixture of colorants provides a natural skin color covering effect, improves the adhesion and stability of the colorants, and makes the concealer more durable and less likely to fall off.

[0029] Preferably, in the raw materials of the concealer composition, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5).

[0030] Preferably, in the raw materials of the concealer composition, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6).

[0031] Preferably, in the raw materials of the concealer composition, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent, antioxidant I is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6):(0.2-0.7).

[0032] Preferably, in the raw materials of the concealer composition, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent, antioxidant I, antioxidant II is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6):(0.2-0.7):(0.1-0.4).

[0033] Preferably, in the raw materials of the concealer composition, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent, antioxidant I, antioxidant II, dispersing agent is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6):(0.2-0.7):(0.1-0.4):(3.2-6.5).

[0034] Preferably, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent, antioxidant I, antioxidant II, dispersant, preservative, colorant in the raw materials of the concealer composition is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6):(0.2-0.7):(0.1-0.4):(3.2-6.5):(0.4-0.8):(30-37.5).

[0035] Preferably, the weight ratio of emollient I, emollient II, plasticizer, film former I, film former II, thickening agent, antioxidant I, antioxidant II, dispersant, preservative, colorant in the raw materials of the concealer composition is (7-12):(21-27):(10-16):(7.5-11):(2.8-4.5):(3-6):(0.2-0.7):(0.1-0.4):(3.2-6.5):(0.4-0.8):(30-37.5).

[0036] The colorant is the core component for achieving the concealing function in the raw materials of the concealer composition of the present application. An appropriate amount of colorant effectively covers various skin imperfections and, through absorption and reflection of light, makes the skin appear uniform, smooth and delicate. The emollient I and the emollient II provide a good dispersion medium for the colorant, ensuring that the colorant is evenly distributed in the product system and avoiding uneven color, thereby ensuring the stability and reliability of the concealing effect. At the same time, they enhance the skin barrier function, prevent water loss and keep the skin moist and smooth. The plasticizer increases the hardness and formability of the product, ensuring that the concealer composition has a suitable texture for easy application and use, and also helps the product to maintain a specific shape for easy carrying and storage. The film former I and the film former II help to form a uniform and breathable film on the skin surface, enhancing the durability and water resistance of the product and making the concealing effect more durable and less likely to be removed.

[0037] The second aspect of the present application provides a preparation method of the concealer composition according to the first aspect of the present application, comprising the following steps: S1, mixing emollient I, plasticizer, antioxidant I, thickening agent, stirring to obtain pre-made material I; S2, adding emollient II, film former I, film former II to the pre-made material I, heating and stirring to obtain pre-made material II; S3, adding dispersant and colorant to the pre-made material II, grinding and stirring to obtain a semi-finished material; S4, adding preservative, antioxidant II to the semi-finished product, stirring, vacuum degassing to obtain the concealer composition.

[0038] Preferably, in step S1, the temperature of the stirring is 90-105℃, the stirring speed is 20-50rpm, and the stirring time is 20-35min. Further preferably, in step S1, the temperature of the stirring is 95-105℃, the stirring speed is 30-50rpm, and the stirring time is 20-35min. Still further preferably, in step S1, the temperature of the stirring is 98-105℃, the stirring speed is 30-50rpm, and the stirring time is 25-35min.

[0039] Preferably, in step S2, the temperature of the stirring is 70-80℃, the stirring speed is 20-50rpm, and the stirring time is 15-25min. Further preferably, in step S2, the temperature of the stirring is 72-80℃, the stirring speed is 25-50rpm, and the stirring time is 15-25min. Still further preferably, in step S2, the temperature of the stirring is 75-80℃, the stirring speed is 30-50rpm, and the stirring time is 15-25min.

[0040] Preferably, in step S3, the grinding speed is 800-1100rpm, the grinding time is 25-40min, the stirring temperature is 80-90℃, the stirring speed is 20-50rpm, and the stirring time is 8-15min. Further preferably, in step S3, the grinding speed is 850-1100rpm, the grinding time is 30-40min, the stirring temperature is 85-90℃, the stirring speed is 20-50rpm, and the stirring time is 8-15min.

[0041] Preferably, in step S4, the stirring temperature is 55-70℃, the stirring speed is 20-50rpm, the stirring time is 3-5min, the vacuum degree of the vacuum degassing is -0.1--0.06MPa, and the vacuum degassing time is 5-15min. Further preferably, in step S4, the stirring temperature is 60-70℃, the stirring speed is 30-50rpm, the stirring time is 3.5-5min, the vacuum degree of the vacuum degassing is -0.08--0.06Mpa, and the vacuum degassing time is 8-15min.

[0042] In the preparation method, the step-by-step mixing method is adopted, step S1 mixes the base components such as emollient I, plasticizer, etc. uniformly to lay the foundation for the subsequent steps; step S2 promotes the dissolution and fusion of the film-forming agent by heating to enhance the film-forming property; step S3 ensures the uniform dispersion of the colorant by grinding to avoid color difference or caking; and step S4 adds the sensitive components preservative and antioxidant II at the end to avoid degradation at high temperature, and removes bubbles through vacuum degassing to prevent the product from having voids or rough surface, and improve the smoothness and quality of the product. The method ensures that the concealer composition has stable performance and excellent skin feel.

[0043] The third aspect of the present application provides a concealer pen, which comprises a pen barrel and a pen core assembly arranged in the pen barrel, and the filling material of the pen core assembly is the concealer composition described above.

[0044] The concealer pen using the concealer composition described above as the filling material also has high hiding power, durability, good skin feel, etc. The concealer pen of the present application is suitable for local concealing and carrying use, and improves the user experience.

[0045] Compared with the prior art, the present application has at least the following beneficial effects: 1) The raw material components of the concealer composition of the present application include emollient I, emollient II, plasticizer, film-forming agent I, film-forming agent II, thickening agent, antioxidant I, antioxidant II, dispersant, preservative and colorant; wherein the emollient I is a mixture of polysiloxane and vegetable oil; the emollient II is a mixture of at least two or more polysiloxanes; the plasticizer is synthetic wax; the film-forming agent I is organosilicate; and the film-forming agent II is a mixture of polysiloxane and silicone-organic hydrocarbon copolymer. Through reasonable proportioning of each raw material component, the prepared concealer composition has high hiding power, durability, stability and good skin feel, and solves the problems of easy makeup removal, powder sticking or skin irritation of existing concealer products.

[0046] 2) In the preparation method of the concealer composition of the present application, the step-by-step mixing method is adopted, and the mixing process is carried out through heating stirring, grinding, vacuum degassing and other ways, which is helpful to form a uniform and stable concealer composition with high hiding power.

[0047] 3) The concealer composition of the present application is used as the filling material of the pen core assembly of a concealer pen, which is convenient to carry, has high hiding power and is not easy to fall off, and has good use comfort. DETAILED DESCRIPTION

[0048] The content of the present application is further described in detail through specific examples, comparative examples and tables, but is not limited to all the discussions and data.

[0049] The raw material components of the concealer composition, polydimethylsiloxane is purchased from Shin-Etsu Silicone International Trade (Shanghai) Co., Ltd., Camellia (CAMELLIA JAPONICA) seed oil is purchased from Laozhixing (Fujian) Biotechnology Co., Ltd., methyl polytrimethylsiloxane, octyl polymethylsiloxane are purchased from Momentive (Shanghai) Trading Co., Ltd., synthetic wax is purchased from U.S. New-Syn Wax Co., Ltd., the model is PERFORMA SW-88 Synthetic Wax polyethylene wax of U.S. New-Syn Wax Co., Ltd., Cirebelle Fine Chemicals (Pty) Ltd., synthetic wax polyethylene wax, trimethylsiloxy silicate is purchased from Wacker Chemical (China) Co., Ltd., acrylate / polydimethylsiloxane copolymer is purchased from Hangzhou Shenhu Technology Co., Ltd., bis-diglyceryl polyacyladipate-2 is purchased from IOI Oleochemicals Sdn Bhd, pentaerythrityl tetra-di-t-butyl hydroxyhydrocinnamate is purchased from BASF (China) Co., Ltd., tocopheryl acetate is purchased from DSM Vitamin (Shanghai) Co., Ltd., polyhydroxystearic acid is purchased from Nisshin OilliO Group, Ltd., phenoxyethanol is purchased from Clariant Chemicals (Shanghai) Co., Ltd., CI 77491, CI 77492, CI 77499, CI 77891, triethoxysilane, aluminum hydroxide are purchased from Sanhe Cosmetics Material (Suzhou) Co., Ltd.

[0050] It is particularly emphasized that, unless otherwise specified, the raw materials, reagents or devices in the present application can be obtained from conventional commercial channels, unless otherwise specified.

[0051] Preparation Example of Emollient I: Preparation Example 1: A preparation method of an emollient I is as follows: 5g of polydimethylsiloxane and 2.8g of Camellia (CAMELLIA JAPONICA) seed oil are uniformly mixed to prepare the emollient I.

[0052] Preparation Example 2: A preparation method of an emollient I is as follows: 5g of polydimethylsiloxane and 1.5g of Camellia (CAMELLIA JAPONICA) seed oil are uniformly mixed to prepare the emollient I.

[0053] Preparation Example 3: A preparation method of an emollient I is as follows: 7g of polydimethylsiloxane and 1.5g of Camellia (CAMELLIA JAPONICA) seed oil are uniformly mixed to prepare the emollient I.

[0054] Preparation Example of Emollient II: Preparation Example 4: A method of making a moisturizer II, the steps of which are as follows: Mixing 21.3 g of methyl methicone, 1.9 g of octyl methicone uniformly to make the moisturizer II.

[0055] Preparation Example 5: A method of making a moisturizer II, the steps of which are as follows: Mixing 20 g of methyl methicone, 1 g of octyl methicone uniformly to make the moisturizer II.

[0056] Preparation Example 6: A method of making a moisturizer II, the steps of which are as follows: Mixing 23.5 g of methyl methicone, 2.8 g of octyl methicone uniformly to make the moisturizer II.

[0057] Preparation Example of a film former II: Preparation Example 7: A method of making a film former II, the steps of which are as follows: Mixing 1.8 g of methyl methicone, 1.2 g of acrylates / dimethicone copolymer uniformly to make the film former II.

[0058] Preparation Example of a plasticizer: Preparation Example 8: A method of making a plasticizer, the steps of which are as follows: Mixing 8 g of polyethylene wax of type PERFORMA SW-88 Synthetic Wax of Nu-White Wax Co. Ltd., 4.2 g of polyethylene wax of type Synthetic Wax of Cirebelle Fine Chemicals (Pty) Ltd. uniformly to make the plasticizer.

[0059] Preparation Example of a colorant: Preparation Example 9: A method of making a colorant, the steps of which are as follows: Mixing 27.6 g of CI 77891-aluminium hydroxide-triethoxyl octyl silane mixture of mass fractions 96.5%, 2.5% and 1% respectively, 0.8 g of CI 77491-triethoxyl octyl silane mixture of mass fractions 99% and 1% respectively, 7.1 g of CI 77492-triethoxyl octyl silane mixture of mass fractions 99% and 1% respectively, 0.6 g of CI 77499-triethoxyl octyl silane mixture of mass fractions 99% and 1% respectively, uniformly to make the colorant.

[0060] Preparation Comparative Example of a moisturizer I: Preparation Comparative Example 1: A preparation method of a skin emollient I is as follows: 8g of polydimethylsiloxane and 1g of Camellia japonica seed oil are mixed uniformly to prepare the skin emollient I.

[0061] Embodiment of a concealer composition: A concealer composition is prepared by the following steps: S1, 7-12g of the skin emollient I, 10-16g of the plasticizer, 0.2-0.7g of the antioxidant I, and 3-6g of the thickening agent are mixed, and stirred at a temperature of 90-105℃ and a speed of 20-50rpm for 20-35min to obtain a pre-preparation I.

[0062] S2, 21-27g of the skin emollient II, 7.5-11g of the film-forming agent I, and 2.8-4.5g of the film-forming agent II are added to the pre-preparation I, and stirred at a temperature of 70-80℃ and a speed of 20-50rpm for 15-25min to obtain a pre-preparation II.

[0063] S3, 3.2-6.5g of the dispersing agent and 30-37.5g of the colorant are added to the pre-preparation II, and ground at a speed of 800-1100rpm for 25-40min, and stirred at a temperature of 80-90℃ and a speed of 20-50rpm for 8-15min to obtain a semi-finished product.

[0064] S4, the temperature is lowered to 55-70℃, 0.4-0.8g of the preservative and 0.1-0.4g of the antioxidant II are added to the semi-finished product, and stirred at a speed of 20-50rpm for 3-5min, and vacuumized to a vacuum degree of -0.1--0.06MPa, and vacuum defoamed for 5-15min to obtain the concealer composition.

[0065] For step S1, in some embodiments, the emollient I is a mixture of polysiloxane and vegetable oil, the weight ratio of polysiloxane to vegetable oil in the emollient I is (5-7):(1.5-3.5), wherein the polysiloxane can be at least one selected from polydimethylsiloxane, methyl polytrimethylsiloxane, octyl polymethylsiloxane, phenyl polytrimethylsiloxane, lauryl polydimethylsiloxane, and the vegetable oil can be at least one selected from CAMELLIA JAPONICA seed oil, SIMMONDSIA CHINENSIS seed oil, HELIANTHUS ANNUUS seed oil, LIMNANTHES ALBA seed oil, and BUTYROSPERMUM PARKII butter. The plasticizer is a synthetic wax, which can be a polyolefin synthetic wax or an ester synthetic wax, and can be at least one polyolefin synthetic wax selected from polyethylene wax, polypropylene wax, microcrystalline wax, and ethylene-vinyl acetate copolymer wax, or can be polyethylene wax produced by different manufacturers. The antioxidant I can be at least one selected from pentaerythritol tetra(bis-tert-butylhydroxyhydrocinnamate), propyl gallate, tetrahexyldecyl ascorbate, and ascorbyl palmitate. The thickening agent can be at least one selected from bis-diglyceryl polyacyladipate-2, polyglyceryl-2 stearate, polyglyceryl-2 dipolyhydroxystearate, and isononyl isononanoate. The amount of the emollient I can be 7 g, 8 g, 10 g, or 12 g, the amount of the plasticizer can be 10 g, 12 g, 14 g, 15 g, or 16 g, the amount of the antioxidant I can be 0.2 g, 0.4 g, 0.5 g, 0.6 g, or 0.7 g, and the amount of the thickening agent can be 3 g, 4 g, 5 g, or 6 g. The stirring temperature can be 90℃, 95℃, 100℃, or 105℃, the stirring speed can be 20 rpm, 30 rpm, 40 rpm, 45 rpm, or 50 rpm, and the stirring time can be 20 min, 25 min, 30 min, or 35 min.

[0066] For step S2, in some embodiments, the emollient II is a mixture of at least two polysiloxanes, which can be a mixture of methyl trimethicone and octyl methicone in a weight ratio of (20-24):(1-3). The film former I can be at least one organosilicate selected from trimethyl siloxy silicate, polymethyl silicate, triisostearyl polymethyl silicate, perfluoro polymethyl isopropyl silicate. The film former II is a mixture of polysiloxane and silicone-organic hydrocarbon copolymer in a weight ratio of (12-15):(5-8), the polysiloxane can be at least one selected from dimethicone, methyl trimethicone, octyl methicone, phenyl trimethicone, lauryl dimethicone, and the silicone-organic hydrocarbon copolymer is at least one selected from acrylate / dimethicone copolymer, acrylate / polytrimethylsiloxymethacrylate copolymer, acrylate / polydimethylsiloxane crosspolymer. The amount of emollient II can be 21 g, 22 g, 25 g, or 27 g, the amount of film former I can be 7.5 g, 8.5 g, 10 g, or 11 g, and the amount of film former II can be 2.8 g, 3.2 g, 4.1 g, or 4.5 g. The stirring temperature can be 70 °C, 72 °C, 76 °C, or 80 °C, the stirring speed can be 20 rpm, 30 rpm, 40 rpm, 45 rpm, or 50 rpm, and the stirring time can be 15 min, 18 min, 20 min, or 25 min.

[0067] For step S3, in some embodiments, the dispersant can be selected from at least one of polyhydroxystearic acid, polyhydroxystearic acid ethyl ester, octyldodecyl polyhydroxystearate, polyhydroxystearic acid glyceryl ester. The colorant can be a mixture of CI 77491, CI 77492, CI 77499, CI 77891, triethoxysilane octyl, aluminum hydroxide, and the colorant can also be a mixture of CI 77891-aluminum hydroxide-triethoxysilane octyl, CI 77491-triethoxysilane octyl, CI 77492-triethoxysilane octyl, CI 77499-triethoxysilane octyl, wherein the weight ratio of the mixture of CI 77891-aluminum hydroxide-triethoxysilane octyl, CI 77491-triethoxysilane octyl, CI 77492-triethoxysilane octyl, CI 77499-triethoxysilane octyl is (25-30):(0.7-1):(6-8):(0.4-0.7), the mixture of CI 77891-aluminum hydroxide-triethoxysilane octyl is a mixture of CI 77891, aluminum hydroxide, and triethoxysilane octyl with mass fractions of 96.5%, 2.5%, and 1% respectively, the mixture of CI 77491-triethoxysilane octyl is a mixture of CI 77491 and triethoxysilane octyl with mass fractions of 99% and 1% respectively, the mixture of CI 77492-triethoxysilane octyl is a mixture of CI 77492 and triethoxysilane octyl with mass fractions of 99% and 1% respectively, and the mixture of CI 77499-triethoxysilane octyl is a mixture of CI 77499 and triethoxysilane octyl with mass fractions of 99% and 1% respectively. The amount of dispersant can be 3.2g, 4g, 5g, 5.5g, or 6.5g, the amount of colorant can be 30g, 32g, 35g, 36g, or 37.5g, the colorant can be a mixture of 27.6g of CI 77891-aluminum hydroxide-triethoxysilane octyl with mass fractions of 96.5%, 2.5%, and 1% respectively, 0.8g of CI 77491-triethoxysilane octyl with mass fractions of 99% and 1% respectively, 7.1g of CI 77492-triethoxysilane octyl with mass fractions of 99% and 1% respectively, and 0.6g of CI 77499-triethoxysilane octyl with mass fractions of 99% and 1% respectively, the colorant can be a mixture of 25g of CI 77891-aluminum hydroxide-triethoxysilane octyl with mass fractions of 96.5%, 2.5%, and 1% respectively, 0.9g of CI 77491-triethoxysilane octyl with mass fractions of 99% and 1% respectively, 6.3g of CI 77492-triethoxysilane octyl with mass fractions of 99% and 1% respectively, and 0.7g of CI 77499-triethoxysilane octyl with mass fractions of 99% and 1% respectively.The speed of grinding can be 800 rpm, 900 rpm, 1000 rpm or 1100 rpm, the time of grinding can be 25 min, 30 min, 35 min or 40 min, the temperature can be 80℃, 82℃, 85℃ or 90℃, the stirring speed can be 20 rpm, 30 rpm, 40 rpm, 45 rpm or 50 rpm, and the stirring time can be 8 min, 10 min, 13 min or 15 min.

[0068] For step S4, in some embodiments, the preservative can be selected from at least one of phenoxyethanol, ethylhexylglycerin, p-hydroxyacetophenone, sodium dehydroacetate. The antioxidant II can be selected from at least one of tocopheryl acetate, ascorbyl glucoside, tea polyphenol. The amount of preservative can be 0.4 g, 0.5 g, 0.6 g or 0.8 g, and the amount of antioxidant II can be 0.1 g, 0.2 g or 0.4 g. The temperature of cooling can be reduced to 55℃, 60℃, 65℃ or 70℃, the stirring speed can be 20 rpm, 30 rpm, 40 rpm, 45 rpm or 50 rpm, the stirring time can be 3 min, 4 min or 5 min, the vacuum degree can be -0.1 MPa, -0.8 MPa, -0.5 MPa, -0.2 MPa or -0.06 MPa, and the vacuum defoaming time can be 5 min, 10 min, 12 min or 15 min.

[0069] Example 1: A concealer composition is prepared by the following steps: S1, 7.8 g of emollient I of Preparation Example 1, 12.2 g of plasticizer of Preparation Example 8, 0.48 g of pentaerythritol tetra(bis-tert-butylhydroxyhydrocinnamate) ester, 4 g of bis-diglyceryl polyacyladipate-2 are mixed, stirred at a temperature of 95℃ and a speed of 50 rpm for 30 min to obtain a preformed material I.

[0070] S2, 23.2 g of emollient II of Preparation Example 4, 8.2 g of trimethylsiloxy silicate, 3 g of film former II of Preparation Example 7 are added to the preformed material I, stirred at a temperature of 75℃ and a speed of 50 rpm for 20 min to obtain a preformed material II.

[0071] S3, 3.9 g of polyhydroxy stearic acid, 36.1 g of colorant of Preparation Example 9 are added to the preformed material II, ground at a speed of 1000 rpm for 35 min, the temperature is adjusted to 85℃, and stirred at a speed of 50 rpm for 10 min to obtain a semi-finished product.

[0072] S4. When the temperature drops to 60℃, add 0.5g phenoxyethanol and 0.28g tocopheryl acetate to the semi-finished material, stir at 40rpm for 5min, evacuate to a vacuum degree of -0.06MPa, and degas under vacuum for 10min to obtain the concealer composition.

[0073] Example 2: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient I in Example 2 is the same as the emollient I prepared in Example 2.

[0074] Example 3: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient I in Example 3 is the same as the emollient I prepared in Example 3.

[0075] Example 4: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient II in Example 4 is the same as the emollient II in Example 5.

[0076] Example 5: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient II in Example 5 is the same as the emollient II prepared in Example 6.

[0077] Comparative Example 1: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient I in Comparative Example 1 is prepared using the same emollient I as in Comparative Example 1.

[0078] Comparative Example 2: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient II in Comparative Example 2 is an equal amount of methyl polytrimethylsiloxane.

[0079] Comparative Example 3: The preparation method and the amount of each raw material in a concealer composition are the same as in Example 1, except that the emollient II in Comparative Example 3 is an equal amount of octyl polymethylsiloxane.

[0080] Material performance testing: The concealer compositions obtained in Examples 1-5 and Comparative Examples 1-3 were subjected to various performance tests, and the test methods are as follows: 1. Covering power: Take 0.1g of each group of samples and coat them evenly on the black and white masking cards using a 5mm diameter coater to form a uniform film layer of 10cm×2cm. Dry at room temperature (25±2℃, RH50±5%) for 30min. Measure the reflectance of the black and white areas after coating using a spectrophotometer (referred to as Y). b and Y w ), Calculate the shading force: Shading force = Yb / Y w The lower the ratio, the stronger the covering power.

[0081] 2. Durability: 20 female evaluators aged 25-45 years old were randomly selected to apply the same amount of sample to the easy-to-bleed area of the cheekbone, and after 8 hours of normal activity, the makeup was photographed with a high-definition camera. The score was decreased from 10 points for complete coverage without bleeding to 0 points for obvious nakedness in the central area. The average value was taken.

[0082] 3. Heat resistance: the sample was sealed and placed in a constant temperature oven at 45±2℃ for 30 days. After recovery to room temperature, there was no change and it could be used normally. This was used as the judgment standard.

[0083] 4. Cold resistance: the sample was sealed and placed in a low temperature box at -10±2℃ for 30 days. After recovery to room temperature, there was no change and it could be used normally. This was used as the judgment standard.

[0084] 5. Cold and heat cycle: freeze for 24 hours at -10±2℃, and place for 24 hours at 45±2℃, cycle for 3 times. Observe whether the product melts, cracks, and whether it returns to its original shape after cooling.

[0085] 6. Skin adhesion and water feeling: 20 female evaluators aged 25-45 years old were randomly selected to apply the same amount of sample to their faces, and the skin adhesion and water feeling of the sample were scored. A 10-point system was used, with 10 points being the best skin adhesion and water feeling, 9 points being the second best, and 1 point being the worst. The scores of all evaluators were recorded and the average value was taken.

[0086] The test performance of the concealer compositions of Examples 1-5 and Comparative Examples 1-3 is shown in Table 1 below: Table 1 Test results of the properties of Examples 1-5 and Comparative Examples 1-3 Covering power Durability Heat resistance Cold resistance Cold and hot cycle Skin adhesion Moisturizing feeling Example 1 0.17 9.2 No abnormality No abnormality No abnormality 9.3 8.8 Example 2 0.19 8.9 No abnormality No abnormality No abnormality 9.1 8.9 Example 3 0.22 9.1 No abnormality No abnormality No abnormality 9.0 8.7 Example 4 0.18 8.7 No abnormality No abnormality No abnormality 9.2 8.5 Example 5 0.19 8.9 No abnormality No abnormality No abnormality 9.4 8.7 Comparative example 1 0.28 6.5 Obvious oiling No abnormality Slight cracking 7.5 7.3 Comparative example 2 0.25 6.9 No abnormality No abnormality No abnormality 8.1 7.8 Comparative example 3 0.27 7.2 Slight oiling Slight oozing No abnormality 8.3 7.9 The concealer compositions of Examples 1-5 have a strong covering power, with a value less than 0.22, good durability, stability, strong heat and cold resistance, comfortable skin feel, good skin adhesion and water feeling, and solve the problem of easy bleeding, powder accumulation or skin irritation of existing concealer products, by reasonable proportioning of the raw material components such as emollient I, emollient II, plasticizer, film former I, film former II, and especially the specific components and proportions of emollient I, emollient II, colorant, etc.

[0087] Comparative Example 1 was prepared in the same way as Example 1 except that the emollient I used in Comparative Example 1 was prepared according to the method of Comparative Example 1. The results showed that the heat resistance test of Comparative Example 1 showed obvious oiling, the cold and hot cycle test showed slight cracking, and the water-wet feeling and skin adhesion were significantly reduced. This proved that the balance between the polysiloxane and the vegetable oil in the emollient I was crucial to the stability, skin feel and moisturizing degree.

[0088] Comparative Example 2 used only methyl trimethicone in the emollient II, and removed the octyl methicone. The results showed that the coverage and durability of the concealer composition of Comparative Example 2 were better than those of Comparative Example 1, but significantly lower than all the examples. Methyl trimethicone could provide a smooth feeling, but lacked the better affinity with other raw materials and skin that octyl methicone had, resulting in a decrease in film-forming property and adhesion, thus leading to poor coverage and durability of the product. In addition, a single silicone oil could not provide the level and delicacy brought by the composite silicone oil system, so that the skin adhesion of the product was not ideal, resulting in a decrease in skin adhesion and water-wet feeling.

[0089] Comparative Example 3 used only octyl methicone in the emollient II, and removed the methyl trimethicone. The octyl methicone had a large molecular weight and low polarity, and a large amount of octyl methicone alone might not be compatible with other raw material components, so that the product showed a slight oiling phenomenon after the heat resistance test; its solubility changed at low temperature, causing some raw material components to precipitate slightly; the product might be too greasy without the refreshing and volatile assistance of methyl trimethicone, thus the water-wet feeling was reduced.

[0090] Obviously, the above examples of the present application are only examples for clearly illustrating the present application, and are not a limitation on the embodiments of the present application. For those skilled in the art, other different forms of changes or variations can be made on the basis of the above description, and any obvious changes or variations within the technical solution of the present application still fall within the protection scope of the present application.

Claims

1. A concealing composition characterized in that, The raw material components include: emollient I, emollient II, plasticizer, film former I, film former II, thickener, antioxidant I, antioxidant II, dispersant, preservative and colorant; The emollient I is a mixture of polysiloxane and vegetable oil; The emollient II is a mixture of at least two polysiloxanes; The plasticizer is synthetic wax; The film former I is organosilicon ester; The film former II is a mixture of polysiloxane and silicone-organic hydrocarbon copolymer.

2. The concealing composition according to claim 1, characterized in that, The weight ratio of polysiloxane to vegetable oil in the emollient I is (5-7):(1.5-3.5); And / or, the weight ratio of polysiloxane to silicone-organic hydrocarbon copolymer in the film former II is (12-15):(5-8).

3. The concealing composition according to claim 1, wherein The polysiloxane is at least one selected from polydimethylsiloxane, methyl polytrimethylsiloxane, octyl polymethylsiloxane, phenyl polytrimethylsiloxane, lauryl polydimethylsiloxane.

4. The concealing composition according to claim 1, wherein The vegetable oil is at least one selected from Camellia japonica seed oil, Simmondsia chinensis seed oil, Helianthus annuus seed oil, Limnanthes alba seed oil, Butyrospermum parkii butter.

5. The concealing composition according to claim 1, wherein The synthetic wax is polyolefin synthetic wax or ester synthetic wax; And / or, the organosilicon ester is at least one selected from trimethylsiloxysilicate, polymethylsilicate, triisostearyl polymethylsilicate, perfluoropolyisopropyl methyl silicate; And / or, the silicone-organic hydrocarbon copolymer is at least one selected from acrylate / polydimethylsiloxane copolymer, acrylate / polytrimethylsiloxane methacrylate copolymer, acrylate / polydimethylsiloxane cross-linked polymer.

6. The concealing composition according to claim 1, wherein The thickener is at least one selected from bis-diglyceryl polyacyladipate-2, polyglyceryl-2 stearate, polyglyceryl-2 dipolyhydroxystearate, isononyl isononanoate; And / or, the antioxidant I is at least one selected from pentaerythrityl tetra-di-t-butyl hydroxyhydrocinnamate, propyl gallate, tetrahexyldecyl ascorbate, ascorbyl palmitate; And / or, the antioxidant II is at least one selected from tocopheryl acetate, ascorbyl glucoside, tea polyphenol; And / or, the dispersant is at least one selected from polyhydroxystearic acid, polyhydroxystearic acid ethyl ester, octyldodecyl polyhydroxystearate, polyhydroxystearic acid glyceryl ester; And / or, the preservative is at least one selected from phenoxyethanol, ethylhexylglycerin, p-hydroxyacetophenone, sodium dehydroacetate; And / or, the colorant is a mixture of CI 77491, CI 77492, CI 77499, CI 77891, triethoxysilane, aluminum hydroxide.

7. The concealing composition according to claim 1, wherein The raw materials include the following components by weight: Emollient I 7-12 parts; Emollient II 21-27 parts; Plasticizer 10-16 parts; Film forming agent I 7.5~11 parts; Film forming agent II 2.8~4.5 parts; Thickening agent 3~6 parts; Antioxidant I 0.2~0.7 parts; Antioxidant II 0.1~0.4 parts; Dispersing agent 3.2~6.5 parts; Preservative 0.4~0.8 parts; Coloring agent 30~37.5 parts.

8. A process for the preparation of a concealer composition according to any one of claims 1 to 7, characterized in that, Comprising the following steps: S1, mixing emollient I, plasticizer, antioxidant I, thickening agent, stirring, to obtain pre-material I; S2, adding emollient II, film forming agent I, film forming agent II to pre-material I, heating and stirring, to obtain pre-material II; S3, adding dispersing agent, coloring agent to pre-material II, grinding, stirring, to obtain semi-finished material; S4, adding preservative, antioxidant II to semi-finished material, stirring, vacuum degassing, to obtain the concealer composition.

9. The method for preparing a concealer composition according to claim 8, wherein In step S1, the temperature of the stirring is 90~105℃, the stirring speed is 20~50rpm, and the stirring time is 20~35min; In step S2, the temperature of the stirring is 70~80℃, the stirring speed is 20~50rpm, and the stirring time is 15~25min; In step S4, the vacuum degree of the vacuum degassing is-0.1~-0.06MPa.

10. A concealer pen, characterized by A pen comprising a pen barrel and a refill assembly arranged in the pen barrel, wherein the filling material of the refill assembly is the concealer composition according to any one of claims 1~7.