A harmless resource utilization process for halogenated organic waste salt

By employing adiabatic bubbling reforming technology and a closed-loop design for gas-fired heat recovery, the problems of secondary pollution, high energy consumption, and low resource utilization in the treatment of halogenated organic waste salts have been solved, achieving harmless, resource-efficient, and low-carbon energy-saving treatment results.

CN122184050BActive Publication Date: 2026-11-10EAST CHINA UNIV OF SCI & TECH +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202610352194.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-03-20
Publication Date
2026-11-10
Estimated Expiration
2046-03-20

AI Technical Summary

Technical Problem

Existing processes for treating halogenated organic waste salts have problems such as high risk of secondary pollution, high energy consumption, high carbon emissions, and low resource utilization rate. In particular, high-temperature incineration is prone to producing toxic and harmful gases such as hydrogen halides and dioxins, and the equipment is severely corroded. Molten salt method has high energy consumption and the equipment is prone to clumping. Chemical oxidation method is ineffective and cannot completely render the waste harmless.

Method used

The adiabatic bubbling reforming technology is used to reform preheated halogenated organic waste salt and purified organic gaseous products in a high-temperature turbulent environment, converting organic matter into combustible gas and halogens into hydrogen halides. Energy recycling is achieved through the gas reuse and heat closed-loop coupling design, and complete separation and resource recovery are achieved by combining the halogen removal unit.

Benefits of technology

It achieves zero secondary pollution, low carbon and energy saving in the harmless treatment process, stable equipment operation, dual recycling of waste salt resources and energy, high product purity, and a resource utilization rate of over 95%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122184050B_ABST
    Figure CN122184050B_ABST
Patent Text Reader

Abstract

This invention discloses a harmless resource-based treatment process for halogenated organic waste salt, relating to the field of organic solid waste resource utilization technology. This invention achieves the directional conversion and separation of organic matter and halogens through adiabatic bubbling reforming. Preheated hot waste salt particles and purified organic gaseous products are fed together into an adiabatic bubbling bed reactor, while high-temperature reforming gas is introduced. Under a high-temperature and turbulent bubbling environment of 500-700℃, the residual carbon carried by the waste salt particles undergoes a reforming reaction with the organic gaseous products. This not only completely converts complex organic matter into combustible gas but also converts halogen pollutants existing in solid or complex states in the waste salt into gaseous hydrogen halides, which are discharged from the reactor with the gas flow. This mechanism allows halogens to be completely stripped from the solid salt particles and transferred to the gas phase, avoiding equipment corrosion and product purity defects caused by halogen residues in the salt phase in traditional processes. It also creates conditions for the subsequent centralized removal of hydrogen halides.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of organic solid waste resource utilization technology, specifically a harmless resource utilization process for halogenated organic waste salts. Background Technology

[0002] In the production processes of industries such as chemicals, pesticides, pharmaceuticals, and dyes, a large amount of halogenated organic waste salts are generated. These waste salts contain a large number of organic pollutants and are also rich in halogen elements such as fluorine, chlorine, and bromine. They are classified as hazardous wastes. If they are discharged directly without proper treatment, they will cause serious pollution to the soil, water bodies, and atmospheric environment, and at the same time, cause a large waste of salt resources.

[0003] Currently, the main treatment processes for halogenated organic waste salts include high-temperature incineration, molten salt method, chemical oxidation method, and salt washing method. Among these, high-temperature incineration is the most widely used process. It oxidizes and decomposes the organic pollutants in the waste salt into carbon dioxide and water through high-temperature incineration, achieving harmless treatment. However, this process has significant drawbacks:

[0004] First, halogenated organic compounds produce large amounts of toxic and harmful gases such as hydrogen halides and dioxins during incineration, making exhaust gas treatment difficult, costly, and prone to causing secondary pollution.

[0005] Secondly, the incineration process requires a large amount of auxiliary fuels such as natural gas, resulting in high energy consumption and large carbon emissions, creating a sharp conflict between environmental governance and energy consumption.

[0006] Third, waste salt is prone to melting and agglomeration during the incineration process, which can lead to coking and blockage of equipment, affecting the continuous and stable operation of the system. At the same time, organic pollutants are still likely to remain in the waste salt after incineration, resulting in low resource utilization rate.

[0007] The molten salt method requires heating the waste salt to a high temperature of over 800°C to melt the salt matrix and decompose the organic matter. However, it consumes more energy, causes severe equipment corrosion, and has high operating and maintenance costs, making it difficult to promote and apply on a large scale.

[0008] Chemical oxidation and salt washing methods are only suitable for waste salt with low organic pollutant content and simple composition. They are ineffective in treating high-concentration, difficult-to-degrade halogenated organic waste salt, cannot achieve complete harmlessness, and will generate a large amount of secondary pollutants in wastewater.

[0009] Therefore, developing a treatment process that can achieve complete harmlessness, high-value resource utilization, and low-carbon energy saving of halogenated organic waste salt has become a technical problem that urgently needs to be solved in this field. Summary of the Invention

[0010] The purpose of this invention is to overcome the shortcomings of existing technologies and provide a harmless resource-based treatment process for halogenated organic waste salt. This process achieves the directional conversion and separation of organic matter and halogens through adiabatic bubbling reforming. Preheated hot waste salt particles and purified organic gaseous products are fed together into an adiabatic bubbling bed reactor, while high-temperature reforming gas is introduced. Under the high-temperature and turbulent bubbling environment of 500-700℃, the residual carbon carried by the waste salt particles undergoes a reforming reaction with the organic gaseous products. This not only completely converts complex organic matter into combustible gas, but also converts halogen pollutants existing in solid or complex states in the waste salt into gaseous hydrogen halides, which are discharged from the reactor with the gas flow. This mechanism allows halogens to be completely stripped from the solid salt particles and transferred to the gas phase, avoiding equipment corrosion and product purity defects caused by halogen residues in the salt phase in traditional processes. It also creates conditions for the subsequent centralized removal of hydrogen halides.

[0011] To solve the above-mentioned technical problems, the present invention provides the following technical solution: a harmless resource utilization process for halogen-containing organic waste salt, the steps of which are as follows:

[0012] S100. The halogenated organic waste salt particles are fed into the waste salt heater for preheating treatment to obtain preheated halogenated waste salt solid material. At the same time, the preheated gaseous products generated by the decomposition of organic matter during the preheating process of the halogenated organic waste salt particles are collected. The preheated gaseous products are sent to the first dust collector for purification treatment to obtain purified pyrolysis gaseous products.

[0013] S200: Natural gas is used as auxiliary fuel in the burner, and the recycled purified combustible gas is used for combustion reaction to produce high temperature flue gas with a temperature of 600℃-800℃. The high temperature flue gas is sent to the second dust collector for dust removal and purification to obtain reformed gas of the components.

[0014] S300. The preheated halogenated waste salt solid material, the purified pyrolysis gas phase product, and the reforming gas are fed into an adiabatic bubbling bed reactor. The reforming reaction is carried out in a high temperature and turbulent environment, so that the halogenated organic matter and residual carbon are converted into combustible gas, and the halogens in the halogenated organic waste salt particles are converted into hydrogen halides, to obtain the reformed high temperature salt solid material and the reformed halogenated combustible gas phase material.

[0015] S400: The reformed halogen-containing combustible phase material is sent to the halogen removal unit for hydrogen halide removal treatment to obtain purified combustible gas and halogen enrichment by-products. The purified combustible gas is then transported to the burner as combustion fuel to achieve energy recycling.

[0016] S500. The reformed high-temperature salt solid material is fed into the waste salt heat recovery unit, so that the reformed high-temperature salt solid material and the cold air fed into the waste salt heat recovery unit can exchange heat indirectly to obtain preheated combustion air and cooled purified salt solid material. The preheated combustion air is delivered to the burner as a combustion medium to realize the system heat circulation coupling. The cooled purified salt solid material is discharged as finished salt.

[0017] Furthermore, in S100, the preheating temperature of the waste salt preheater is controlled at 400℃-500℃, so that the organic matter in the halogen-containing organic waste salt particles decomposes and vaporizes, forming the preheated halogen-containing waste salt solid material and the preheated gaseous product.

[0018] The halogenated organic waste salt particles fed into the waste salt heater are uniform particles that have been crushed and screened, with a particle size of 0.1mm-5mm and a moisture content of 0.5%-5%.

[0019] Furthermore, in S200, the oxygen content of the high-temperature flue gas generated by the burner is controlled at 0.5%-3% to avoid excessive oxygen in the high-temperature flue gas causing premature oxidation of combustible components in the adiabatic bubbling bed reactor, thus ensuring a reducing atmosphere for the reforming reaction. The main components of the reforming gas are carbon dioxide and water vapor, which provide a reaction medium for the reforming reaction.

[0020] Furthermore, in the S300, the reaction temperature in the adiabatic bubbling bed reactor is controlled at 500-700℃. Under high temperature and turbulent bubbling conditions, the residual organic pollutants and carbon residues in the preheated halogen-containing waste salt solid phase material undergo a reforming reaction with the pyrolysis organic matter in the purified pyrolysis gas phase products and the carbon dioxide and water vapor in the reformed gas, converting them into combustible gases with hydrogen and carbon monoxide as the main components. The core reaction equations include: C + CO2 = 2CO, C + H2O = CO + H2, C n H m +nH2O=nCO+(n+m / 2)H2, through the reforming reaction, organic pollutants are completely converted into combustible gas, and at the same time, organically bound halogens are completely converted into gaseous hydrogen halides, thus achieving complete separation of organic pollutants from the matrix.

[0021] Meanwhile, the halogen components in the halogen-containing organic waste salt particles are converted into hydrogen halide gas during the reforming reaction and discharged with the gaseous products. After the reforming reaction is completed, the top of the adiabatic bubbling bed reactor yields reformed gaseous material containing combustible gas and hydrogen halide, and the bottom of the adiabatic bubbling bed reactor yields reformed high-temperature salt solid material.

[0022] Furthermore, the reforming gas is a gaseous medium obtained by purifying the high-temperature flue gas generated by the burner through a second dust collector. The temperature of the high-temperature flue gas is 600-800℃, and the dust collection rate after dust removal is >99.9%. When the reforming gas is fed into the adiabatic bubbling bed reactor, it simultaneously provides the heat and reaction medium required for the reforming reaction, maintaining the adiabatic reaction temperature in the adiabatic bubbling bed reactor.

[0023] Furthermore, in S300, the reaction system inside the adiabatic bubbling bed reactor is a slightly positive pressure system with a pressure of 500Pa-2000Pa. The solid phase residence time of the preheated halogen-containing waste salt solid material in the adiabatic bubbling bed reactor is controlled at 30min-120min. The gas phase residence time of the purified pyrolysis gaseous products and reformed gas in the adiabatic bubbling bed reactor is controlled at 2s-10s, which is used to fully reform and convert the halogen-containing organic matter and residual carbon.

[0024] Furthermore, in S400, the halogen removal unit employs a multi-stage alkaline washing and absorption process, using sodium hydroxide solution as the absorbent, controlling the pH of the absorbent to be 8-12, and the absorption temperature to be 30℃-60℃. After treatment by the halogen removal unit, the hydrogen halide content in the purified combustible gas is ≤10mg / m³. 3 The hydrogen halide removal rate is ≥99%, and the halogen enrichment byproduct is a sodium halide salt solution, which is recycled after evaporation and crystallization.

[0025] Furthermore, in S500, after the cold air exchanges heat with the reformed high-temperature salt solid material in the waste salt heat recovery unit, its temperature rises to 300℃-400℃, forming the preheated combustion air which is then sent into the burner to improve the combustion efficiency and energy utilization efficiency of the burner.

[0026] Furthermore, in S500, the total organic carbon content of the finished salt is ≤50ppm, the sodium chloride purity is ≥98.5%, the resource utilization rate of halogenated organic waste salt particles is ≥95%, and the organic pollutant removal rate is ≥99%.

[0027] Compared with existing technologies, this harmless resource utilization process for halogenated organic waste salt has the following beneficial effects:

[0028] I. This process achieves the directional conversion and separation of organic matter and halogens through adiabatic bubbling reforming. Preheated hot waste salt particles and purified organic gaseous products are fed together into an adiabatic bubbling bed reactor, while high-temperature reforming gas is introduced. Under the high temperature and turbulent bubbling environment of 500-700℃, the residual carbon carried by the waste salt particles undergoes a reforming reaction with the organic gaseous products. This not only completely converts complex organic matter into combustible gas, but also converts halogen pollutants in solid or complexed state in the waste salt into gaseous hydrogen halides, which are discharged from the reactor with the gas flow. This mechanism allows halogens to be completely stripped from the solid salt particles and transferred to the gas phase, avoiding equipment corrosion and product purity defects caused by halogen residues in the salt phase in traditional processes. It also creates conditions for the subsequent centralized removal of hydrogen halides.

[0029] II. This process, through a combination of preheating pyrolysis and adiabatic bubbling bed reforming, solves the problems of secondary pollution and equipment clogging caused by high-temperature incineration and molten salt methods. The preheating stage at a low temperature of 400-500℃ achieves preliminary pyrolysis of organic matter, avoiding melting of the salt matrix. The reforming temperature of 500-700℃ in the adiabatic bubbling bed is much lower than the melting temperature of salt, and the turbulent environment ensures full contact between the solid and gas phases, preventing local overheating and agglomeration of salt materials and ensuring continuous and stable operation of the equipment. At the same time, the reforming reaction converts organically bound halogens into hydrogen halides, which are efficiently captured by a dedicated halogen removal unit, avoiding the generation of toxic gases such as hydrogen halides and dioxins during incineration. This solves the technical defects of traditional processes, such as the difficulty in treating tail gas and the risk of secondary pollution, and achieves zero risk of secondary pollution throughout the waste salt treatment process.

[0030] Third, this process relies on a dual-energy cycle design of combustible gas recycling and heat closed-loop coupling to solve the pain points of high energy consumption and low resource utilization rate of traditional halogenated organic waste salt treatment processes. The reforming reaction converts organic pollutants in waste salt into combustible gas, which is recycled in the burner to replace part of the natural gas. It converts hazardous pollutants into system heating energy, changing the traditional process that only consumes energy without energy recovery. At the same time, the high-temperature salt solid phase sensible heat is recovered through the waste salt heat recovery unit to preheat the combustion air, realizing a closed-loop supply from incineration waste heat to reforming heat. This allows for the cascade utilization of energy within the system, and the purity of the finished salt can be directly reused. This solves the problems of residual organic matter and low resource utilization rate of waste salt in traditional processes, and realizes the dual recycling of energy and salt resources.

[0031] Other advantages, objectives and features of the invention will be set forth in part in the description which follows, and in part will be apparent to those skilled in the art from the following examination or study, or may be learned from the practice of the invention. Attached Figure Description

[0032] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without any creative effort.

[0033] Figure 1 A flowchart of a harmless resource utilization process for halogenated organic waste salt;

[0034] Figure 2 This is a flowchart illustrating the steps of a harmless resource recovery process for halogenated organic waste salt. Detailed Implementation

[0035] To better understand the above technical solutions, a detailed description of the solutions will be provided below in conjunction with the accompanying drawings and specific embodiments. Obviously, the described embodiments are merely some, not all, of the embodiments of the present invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.

[0036] To address the problems of high secondary pollution risk, high energy consumption, high carbon emissions, and low resource utilization rate in existing halogenated organic waste salt treatment processes, this invention first describes its application scenarios. This invention is mainly applied to the harmless resource utilization of halogenated organic waste salt generated in industries such as chemicals, pesticides, pharmaceuticals, and dyes. In these scenarios, traditional treatment methods such as high-temperature incineration, molten salt methods, chemical oxidation methods, and salt washing methods suffer from drawbacks: they easily generate toxic and harmful gases such as hydrogen halides and dioxins; they have high energy consumption and severe equipment corrosion; they are only suitable for low-concentration, simple-component waste salts and easily generate secondary wastewater pollution; at the same time, the waste salt easily melts and clumps, leading to unstable equipment operation and residual organic pollutants in the treated waste salt, severely restricting the complete harmlessness and high-value resource utilization of halogenated organic waste salts.

[0037] This invention utilizes a combined reaction method of preheating pyrolysis and adiabatic bubbling bed reforming, a dual-energy cycle design of combustible gas recycling and heat closed-loop coupling, and a halogen-directed conversion, separation and efficient removal process. The aim is to achieve a harmless resource-based treatment process for halogen-containing organic waste salt that is free from secondary pollution, low-carbon and energy-saving, ensures stable equipment operation, and achieves dual recycling of salt resources and energy.

[0038] In the specific implementation process, such as Figure 1 and Figure 2 As shown, this invention provides a harmless resource utilization process for halogenated organic waste salt, the steps of which are as follows:

[0039] S100. The halogenated organic waste salt particles are fed into the waste salt heater for preheating treatment to obtain the preheated halogenated waste salt solid material. At the same time, the preheated gaseous products generated by the decomposition of organic matter during the preheating process of the halogenated organic waste salt particles are collected. The preheated gaseous products are sent to the first dust collector for purification treatment to obtain the purified pyrolysis gaseous products.

[0040] S200: Natural gas is used as auxiliary fuel in the burner, and the recycled purified combustible gas is used for combustion reaction to produce high temperature flue gas with a temperature of 600℃-800℃. The high temperature flue gas is sent to the second dust collector for dust removal and purification to obtain reformed gas of the components.

[0041] S300: The preheated halogenated waste salt solid material and the purified pyrolysis gas phase product are fed together with the reforming gas into the adiabatic bubbling bed reactor. The reforming reaction is carried out in a high temperature and turbulent environment, so that the halogenated organic matter and residual carbon are converted into combustible gas, and the halogen in the halogenated organic waste salt particles are converted into hydrogen halides, to obtain the reformed high temperature salt solid material and the reformed halogenated combustible gas phase material.

[0042] S400: The reformed halogen-containing combustible phase material is sent to the halogen removal unit for hydrogen halide removal treatment to obtain purified combustible gas and halogen enrichment by-products. The purified combustible gas is then transported to the burner as combustion fuel to achieve energy recycling.

[0043] S500: The reformed high-temperature salt solid material is sent to the waste salt heat recovery unit, so that the reformed high-temperature salt solid material and the cold air sent to the waste salt heat recovery unit can exchange heat indirectly to obtain preheated combustion air and cooled purified salt solid material. The preheated combustion air is sent to the burner as a combustion medium to realize the system heat circulation coupling. The cooled purified salt solid material is discharged as finished salt.

[0044] The harmless resource utilization process for halogenated organic waste salt disclosed in this invention comprises the following steps: raw material preheating and dust removal purification, combustion to prepare reformed gas, adiabatic bubble bed reforming reaction, gas-phase dehalogenation and energy recovery, solid-phase waste heat recovery and finished salt production. These steps are described in detail below through specific embodiments:

[0045] Example 1

[0046] This embodiment addresses the harmless and resource-based treatment of high-chlorine-content organic waste salt generated in the pesticide industry. The waste salt raw material contains 92% sodium chloride, 3.5% total organic carbon, 1.2% organic chlorine, and 2% moisture. This embodiment controls the preheating temperature to 450℃, the reforming reaction temperature to 600℃, and the combustion flue gas temperature to 700℃. Organic matter conversion is achieved through adiabatic bubbling bed reforming. A closed-loop coupling design for fuel gas reuse and heat recovery is incorporated to achieve the harmless disposal of waste salt and the recycling of salt resources and energy. The specific implementation steps are as follows:

[0047] S100. Raw material preheating and dust removal purification: High-chlorine organic waste salt is crushed and screened to obtain uniform particles with a particle size of 0.5mm-2mm. These particles are then fed into a waste salt heater for preheating treatment, with the preheating temperature controlled at 450℃, to obtain preheated halogen-containing waste salt solid material. Simultaneously, preheated gaseous products generated by the decomposition of organic matter during the preheating process of the halogen-containing organic waste salt particles are collected. These preheated gaseous products are then sent to the first dust collector for purification treatment. The first dust collector is a high-temperature resistant bag filter with a dust removal accuracy of 1μm, to obtain purified pyrolysis gaseous products. The dust content in the purified pyrolysis gaseous products is 8mg / m³.

[0048] S200, Combustion to Prepare Reformed Gas: Natural gas is used as auxiliary fuel in a burner, along with recycled purified combustible gas, to produce high-temperature flue gas at 700℃. The oxygen content of the high-temperature flue gas is controlled at 1% to avoid excessive oxygen from disrupting the reducing atmosphere for subsequent reforming reactions. The high-temperature flue gas is then sent to a second dust collector for dust removal and purification. The second dust collector is a high-temperature resistant ceramic multi-tube dust collector with a dust removal accuracy of 5μm, resulting in reformed gas with carbon dioxide and water vapor as the main components and a dust content of 30mg / m³.

[0049] S300, Adiabatic Bubbling Bed Reforming Reaction: Preheated halogen-containing waste salt solid material, purified pyrolysis gaseous products, and reforming gas are fed into an adiabatic bubbling bed reactor. The reaction temperature inside the reactor is controlled at 600℃, the reaction system is a slightly positive pressure system, and the pressure is controlled at 1000Pa. The solid phase residence time of the preheated halogen-containing waste salt solid material in the reactor is 60min, and the gaseous material residence time is 5s. Under the high temperature and turbulent bubbling environment, the residual organic pollutants and carbon residues in the preheated halogen-containing waste salt solid material undergo reforming reactions with the pyrolysis organic matter in the purified pyrolysis gaseous products, carbon dioxide, and water vapor in the reforming gas. The core reactions include C + CO2 = 2CO, C + H2O = CO + H2, and C n H m +nH2O=nCO+(n+m / 2)H2, which completely converts organic pollutants into combustible gas with hydrogen and carbon monoxide as the main components, and at the same time completely converts organically bound chlorine into gaseous hydrogen chloride; after the reaction is completed, the top of the reactor obtains reformed halogen-containing combustible gas phase material, and the bottom of the reactor obtains reformed high-temperature salt solid phase material.

[0050] S400, Gas-phase Dehalogenation and Energy Recovery: The reformed halogen-containing combustible gas phase material is fed into a halogen removal unit for hydrogen halide removal. The halogen removal unit adopts a three-stage alkaline washing absorption process, using a 10% sodium hydroxide solution as the absorbent, controlling the pH of the absorbent to 10, and the absorption temperature to 40℃. After treatment, purified combustible gas and sodium chloride enriched by-products are obtained. The hydrogen chloride content in the purified combustible gas is 5 mg / m³, and the hydrogen halide removal rate reaches 99.5%. The purified combustible gas is transported to the burner as combustion fuel, replacing 30% of the natural gas consumption, realizing energy recycling. The halogen enriched by-products can be evaporated and crystallized to recover halogen resources.

[0051] S500, Solid-phase waste heat recovery and finished salt production: The reformed high-temperature salt solid material is sent to the waste salt heat recovery unit, where it undergoes indirect heat exchange with the cold air fed into the unit. After heat exchange, the cold air temperature rises to 350°C, forming preheated combustion air. This preheated combustion air is then delivered to the burner as a combustion medium, improving combustion efficiency and energy utilization efficiency, and achieving system heat circulation coupling. After cooling through heat exchange, the purified salt solid material is obtained and discharged as finished salt at a discharge temperature of 80°C.

[0052] After processing in this embodiment, the sodium chloride purity of the finished salt is 99.1%, the total organic carbon content is 22 ppm, the organic pollutant removal rate of the whole process reaches 99.92%, and the resource utilization rate of halogenated organic waste salt particles reaches 96.2%.

[0053] Example 2

[0054] This embodiment addresses the treatment of high-concentration chlorine-containing organic waste salts generated in the pharmaceutical industry. The waste salt raw material contains 90% sodium chloride, 5.2% total organic carbon, 2.1% organic chlorine, and 3% moisture. Based on the process route of this invention, this embodiment adapts to the treatment requirements of high-organic-content waste salts by adjusting the preheating temperature to 420℃, the reforming reaction temperature to 650℃, and the combustion flue gas temperature to 750℃, extending the material residence time to ensure complete conversion of organic matter, achieving deep harmlessness and high-value resource utilization of the waste salts. The specific implementation steps are as follows:

[0055] S100. Raw material preheating and dust removal purification: The above-mentioned high-concentration chlorine-containing organic waste salt is crushed and screened to obtain uniform particles with a particle size of 1mm-3mm. These particles are then fed into a waste salt heater for preheating treatment. The preheating temperature is controlled at 420℃ to fully decompose and gasify the volatile organic compounds in the waste salt, resulting in preheated halogen-containing waste salt solid material and preheated gaseous products. The preheated gaseous products are then sent to a first dust collector for purification treatment. The first dust collector is a high-temperature resistant bag filter with a dust removal accuracy of 0.5μm, resulting in purified pyrolysis gaseous products with a dust content of 5mg / m³.

[0056] S200, Combustion to Prepare Reformed Gas: Natural gas is used as auxiliary fuel in a burner, along with recycled purified combustible gas, to produce high-temperature flue gas at 750℃. The oxygen content of the high-temperature flue gas is controlled at 2%. The high-temperature flue gas is then sent to a second dust collector for dust removal and purification. The second dust collector is a high-temperature resistant ceramic multi-tube dust collector with a dust removal accuracy of 3μm. The resulting reformed gas is mainly composed of carbon dioxide and water vapor, with a dust content of 20mg / m³, which simultaneously provides the reaction medium and heat for subsequent reforming reactions.

[0057] S300, Adiabatic Bubbling Bed Reforming Reaction: Preheated halogenated waste salt solid material and purified pyrolysis gaseous products are fed into an adiabatic bubbling bed reactor along with reforming gas. The reaction temperature inside the reactor is controlled at 650℃, and the reaction system is a slightly positive pressure system with a pressure controlled at 1500Pa. The solid phase residence time of the preheated halogenated waste salt solid material in the reactor is 90min, and the gaseous material residence time is 8s. Under the high temperature and turbulent bubbling environment, the residual organic pollutants and carbon residues in the waste salt undergo a full reforming reaction with the pyrolysis organic matter and reforming gas, completely converting the organic pollutants into combustible gas. At the same time, the organically bound chlorine is completely converted into gaseous hydrogen chloride, achieving complete separation of organic pollutants from the salt matrix. After the reaction is completed, the top of the reactor yields reformed halogenated combustible gaseous material, and the bottom of the reactor yields reformed high-temperature salt solid material.

[0058] S400, Gas-phase Dehalogenation and Energy Recovery: The reformed halogen-containing combustible gas phase material is fed into a halogen removal unit for hydrogen halide removal. The halogen removal unit adopts a four-stage alkaline washing absorption process, using a 15% sodium hydroxide solution as the absorbent, controlling the pH value of the absorbent to 11, and the absorption temperature to 45℃. After treatment, purified combustible gas and sodium chloride enriched by-products are obtained. The hydrogen chloride content in the purified combustible gas is 3 mg / m³, and the hydrogen halide removal rate reaches 99.7%. The purified combustible gas is then transported to a burner as combustion fuel, replacing 38% of the natural gas consumption, thus achieving energy recycling.

[0059] S500, Solid-phase waste heat recovery and finished salt production: The reformed high-temperature salt solid material is sent to the waste salt heat recovery unit and undergoes indirect heat exchange with the incoming cold air. After heat exchange, the temperature of the cold air rises to 380°C, forming preheated combustion air that is then sent to the burner, realizing the system's heat circulation coupling. After cooling through heat exchange, the cooled purified salt solid material is obtained and discharged as finished salt at a temperature of 70°C.

[0060] After processing in this embodiment, the sodium chloride purity of the finished salt is 98.8%, the total organic carbon content is 35 ppm, the organic pollutant removal rate of the whole process reaches 99.93%, and the resource utilization rate of halogenated organic waste salt particles reaches 95.7%, achieving stable and compliant disposal of high-concentration halogenated organic waste salt.

[0061] Example 3

[0062] This embodiment addresses the harmless treatment of bromine-containing organic waste salts generated in the dye industry. The waste salt raw material contains 88% sodium bromide, 4.5% total organic carbon, 1.8% organic bromine, and 1.5% moisture. Based on the process route of this invention, this embodiment adapts to the treatment characteristics of bromine-containing organic waste salts, controlling the preheating temperature at 480℃, the reforming reaction temperature at 580℃, and the combustion flue gas temperature at 680℃ to achieve the directional conversion and efficient removal of organic bromine, while simultaneously completing the recycling of salt resources and energy. The specific implementation steps are as follows:

[0063] S100. Raw material preheating and dust removal purification: The above-mentioned bromine-containing organic waste salt is crushed and screened to obtain uniform particles with a particle size of 0.2mm-2mm. These particles are then fed into a waste salt heater for preheating treatment, with the preheating temperature controlled at 480℃. This yields preheated halogen-containing waste salt solid material, while simultaneously collecting the preheated gaseous products generated during the preheating process. The preheated gaseous products are then sent to a first dust collector for purification treatment. The first dust collector is a high-temperature resistant bag filter with a dust removal accuracy of 1μm. This yields purified pyrolysis gaseous products with a dust content of 7mg / m³.

[0064] S200, Combustion to produce reformed gas: Natural gas is used as auxiliary fuel in a burner, along with recycled purified combustible gas, to produce high-temperature flue gas at 680℃. The oxygen content of the high-temperature flue gas is controlled at 0.8%. The high-temperature flue gas is then sent to a second dust collector for dust removal and purification. The second dust collector is a high-temperature resistant ceramic multi-tube dust collector with a dust removal accuracy of 5μm, resulting in reformed gas with carbon dioxide and water vapor as the main components. The dust content in the reformed gas is 35mg / m³.

[0065] S300, Adiabatic Bubbling Bed Reforming Reaction: Preheated halogenated waste salt solid material and purified pyrolysis gaseous products are fed into an adiabatic bubbling bed reactor along with reformed gas. The reaction temperature inside the reactor is controlled at 580℃, and the reaction system is a slightly positive pressure system with a pressure controlled at 800Pa. The solid phase residence time of the preheated halogenated waste salt solid material in the reactor is 80min, and the gaseous material residence time is 6s. Under the high temperature and turbulent bubbling environment, the organic pollutants and residual carbon in the waste salt undergo a complete reforming reaction and are converted into combustible gas. At the same time, the organically bound bromine is completely converted into gaseous hydrogen bromide, achieving complete separation of organic pollutants from the salt matrix. After the reaction is completed, the top of the reactor yields reformed halogenated combustible gaseous material, and the bottom of the reactor yields reformed high-temperature salt solid material.

[0066] S400, Gas-phase Dehalogenation and Energy Recovery: The reformed halogen-containing combustible gas phase material is fed into a halogen removal unit for hydrogen bromide removal. The halogen removal unit adopts a three-stage alkaline washing absorption process, using a 12% sodium hydroxide solution as the absorbent, controlling the pH of the absorbent to 9.5, and the absorption temperature to 35℃. After treatment, purified combustible gas and sodium bromide enriched byproducts are obtained. The hydrogen bromide content in the purified combustible gas is 6 mg / m³, and the hydrogen bromide removal rate reaches 99.4%. The purified combustible gas is then transported to a burner as combustion fuel, replacing 32% of the natural gas consumption, thus achieving energy recycling.

[0067] S500, Solid-phase waste heat recovery and finished salt production: The reformed high-temperature salt solid material is sent to the waste salt heat recovery unit and undergoes indirect heat exchange with the incoming cold air. After heat exchange, the temperature of the cold air rises to 320°C, forming preheated combustion air that is then sent to the burner, realizing the system's heat circulation coupling. After cooling through heat exchange, the cooled purified salt solid material is obtained and discharged as finished salt at a discharge temperature of 90°C.

[0068] After processing in this embodiment, the sodium bromide purity of the finished salt is 98.7%, and the total organic carbon content is 28 ppm, which can be directly recycled in the dye production process; the organic pollutant removal rate of the whole process reaches 99.91%, and the resource utilization rate of halogenated organic waste salt particles reaches 95.8%, which is suitable for the treatment needs of organic waste salt of different halogen types.

[0069] Comparative Example 1

[0070] This comparative example uses a conventional high-temperature incineration process commonly used in the industry to treat chlorine-containing organic waste salts from the pesticide industry, which is exactly the same as in Example 1. A rotary kiln incinerator is used as the core equipment, and organic matter is decomposed through high-temperature incineration. The comparison verifies the advantages of the process of this invention in terms of harmlessness, resource utilization rate, energy consumption control, and operational stability. The comparative implementation steps are as follows:

[0071] The batch of chlorinated organic waste salts, the same as those in the example, was fed into a rotary kiln incinerator. Natural gas was used as the sole fuel. The furnace temperature was controlled at 850°C and the flue gas residence time was ≥2s. The waste salts were discharged after being cooled by water. The high-temperature flue gas generated by incineration was treated in sequence by a quench tower, a deacidification tower, a bag filter, and an activated carbon adsorption tower before being discharged through a chimney in compliance with emission standards.

[0072] Compared with Example 1, this comparative example has poor harmlessness. The total organic carbon content of the waste salt after incineration is 1200ppm, and the purity of sodium chloride is only 93.2%, which cannot meet the industrial salt standard. An additional refining process is required to achieve resource recovery. Moreover, the initial concentration of hydrogen chloride in the incineration flue gas is high, and the tail gas treatment cost is 60% higher than that of Example 1. At the same time, there is an environmental risk of dioxin generation, which can easily cause secondary pollution. The energy consumption and carbon emissions are high. The natural gas consumption is 2.1 times that of Example 1, and the carbon emissions are 42% higher than those of Example 1. There is no energy recovery and recycling process, highlighting the contradiction between environmental protection and energy consumption. The operational stability is poor. During the incineration process, the waste salt is prone to local melting and agglomeration, causing coking of the furnace body and blockage of the slag outlet, making it impossible to achieve long-term continuous and stable operation, which is in stark contrast to the advantages of the process of this invention.

[0073] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the present invention. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A harmless resource utilization process for halogenated organic waste salt, characterized in that, The steps of this process are as follows: S100. The halogenated organic waste salt particles are fed into the waste salt heater for preheating treatment to obtain preheated halogenated waste salt solid material. At the same time, the preheated gaseous products generated by the decomposition of organic matter during the preheating process of the halogenated organic waste salt particles are collected. The preheated gaseous products are sent to the first dust collector for purification treatment to obtain purified pyrolysis gaseous products. S200: Natural gas is used as auxiliary fuel in the burner, and the recycled purified combustible gas is used for combustion reaction to produce high temperature flue gas with a temperature of 600℃-800℃. The high temperature flue gas is sent to the second dust collector for dust removal and purification to obtain reformed gas of the components. S300. The preheated halogenated waste salt solid material, the purified pyrolysis gas phase product, and the reforming gas are fed into an adiabatic bubbling bed reactor. The reforming reaction is carried out in a high temperature and turbulent environment, so that the halogenated organic matter and residual carbon are converted into combustible gas, and the halogens in the halogenated organic waste salt particles are converted into hydrogen halides, to obtain the reformed high temperature salt solid material and the reformed halogenated combustible gas phase material. S400: The reformed halogen-containing combustible phase material is sent to the halogen removal unit for hydrogen halide removal treatment to obtain purified combustible gas and halogen enrichment by-products. The purified combustible gas is then transported to the burner as combustion fuel to achieve energy recycling. S500. The reformed high-temperature salt solid material is fed into the waste salt heat recovery unit, so that the reformed high-temperature salt solid material and the cold air fed into the waste salt heat recovery unit can exchange heat indirectly to obtain preheated combustion air and cooled purified salt solid material. The preheated combustion air is delivered to the burner as a combustion medium to realize the system heat circulation coupling. The cooled purified salt solid material is discharged as finished salt.

2. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 1, characterized in that, In S100, the preheating temperature of the waste salt preheater is controlled at 400℃-500℃ so that the organic matter in the halogen-containing organic waste salt particles decomposes and gasifies, forming the preheated halogen-containing waste salt solid material and the preheated gaseous product. The halogenated organic waste salt particles fed into the waste salt heater are uniform particles that have been crushed and screened, with a particle size of 0.1mm-5mm and a moisture content of 0.5%-5%.

3. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 1, characterized in that, In S200, the oxygen content of the high-temperature flue gas generated by the burner is controlled at 0.5%-3%, and the main components of the reforming gas are carbon dioxide and water vapor, which provide a reaction medium for the reforming reaction.

4. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 1, characterized in that, In the S300, the reaction temperature in the adiabatic bubbling bed reactor is controlled at 500-700℃. Under high temperature and turbulent bubbling conditions, the organic pollutants and residual carbon in the preheated halogenated waste salt solid material undergo a reforming reaction with the pyrolysis organic matter in the purified pyrolysis gas phase product and the carbon dioxide and water vapor in the reformed gas, and are converted into combustible gas with hydrogen and carbon monoxide as the main components. During the reforming reaction, the halogen components in the halogen-containing organic waste salt particles are converted into hydrogen halide gas and discharged with the gaseous products. After the reforming reaction is completed, the top of the adiabatic bubbling bed reactor yields reformed gaseous material containing combustible gas and hydrogen halide, and the bottom of the adiabatic bubbling bed reactor yields reformed high-temperature salt solid material.

5. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 3, characterized in that, The reforming gas is a gaseous medium obtained by removing dust and purifying the high-temperature flue gas generated by the burner through a second dust collector. The temperature of the high-temperature flue gas is 600-800℃, and the dust collection rate after dust removal is >99.9%. When the reforming gas is sent into the adiabatic bubbling bed reactor, it simultaneously provides the heat and reaction medium required for the reforming reaction, maintaining the adiabatic reaction temperature in the adiabatic bubbling bed reactor.

6. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 1, characterized in that, In the S300, the reaction system in the adiabatic bubbling bed reactor is a slightly positive pressure system with a pressure of 500Pa-2000Pa. The solid phase residence time of the preheated halogen-containing waste salt solid material in the adiabatic bubbling bed reactor is controlled at 30min-120min. The gas phase residence time of the purified pyrolysis gaseous products and reformed gas in the adiabatic bubbling bed reactor is controlled at 2s-10s, which is used to fully reform and convert the halogen-containing organic matter and residual carbon.

7. The harmless resource utilization process for halogenated organic waste salt according to claim 1, characterized in that, In the S400, the halogen removal unit adopts a multi-stage alkaline washing absorption process, using sodium hydroxide solution as the absorbent, controlling the pH value of the absorbent to be 8-12, and the absorption temperature to be 30℃-60℃. After treatment by the halogen removal unit, the hydrogen halide content in the purified combustible gas is ≤10mg / m³, and the hydrogen halide removal rate is ≥99%. The halogen enrichment byproduct is a sodium halide salt solution, which is used to recover halogen resources after evaporation and crystallization.

8. The harmless resource utilization process for halogenated organic waste salt according to claim 1, characterized in that, In S500, the cold air exchanges heat with the reformed high-temperature salt solid material in the waste salt heat recovery unit, and its temperature rises to 300℃-400℃, forming the preheated combustion air which is then sent into the burner.

9. The harmless resource utilization treatment process for halogenated organic waste salt according to claim 1, characterized in that, In the S500 process, the total organic carbon content of the finished salt is ≤50ppm, the sodium chloride purity is ≥98.5%, the resource utilization rate of halogenated organic waste salt particles is ≥95%, and the organic pollutant removal rate is ≥99%.

Citation Information

Patent Citations

  • Dechlorination method for chlorine-containing material

    CN107413815A