Method, device and apparatus for improving process parameters of a continuous casting machine
By using fiber optic grating temperature sensors in the continuous casting machine crystallizer to identify the air gap and protective slag, the problem of uneven heat transfer caused by inaccurate air gap position was solved, enabling precise adjustment of process parameters and improving production reliability and efficiency.
Patent Information
- Application Number
- CN202611382535.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-08
- Publication Date
- 2026-11-10
AI Technical Summary
During the continuous casting process, the peritectic reaction of peritectic steel causes changes in the air gap between the initial solidified billet shell and the crystallizer, resulting in uneven heat transfer and local temperature drops in the crystallizer, which affects the growth of the billet shell. It is necessary to accurately determine the location of the air gap in order to carry out targeted process improvements.
A fiber optic temperature sensor is installed through drilled holes on the narrow and wide copper plates of the crystallizer. By detecting temperature information, the air gap and protective slag are identified. The location of the air gap is determined based on the temperature change characteristics, and the process parameters of the continuous casting machine are adjusted according to the location information.
This enabled accurate determination of the air gap location, improved the reliability and heat transfer efficiency of continuous casting machine production, avoided incorrect process parameter adjustments, and enhanced production stability.
Smart Images

Figure CN123060069A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of continuous casting technology, and particularly relates to a method, apparatus and equipment for improving the process parameters of a continuous casting machine. Background Technology
[0002] During continuous casting, when peritectic steel undergoes a peritectic reaction, the austenite phase transformation from the liquid phase and the subsequent ferrite transformation lead to significant volume shrinkage. This causes changes in the local air gap between the initially solidified billet shell and the mold. The location of these air gaps can result in uneven heat transfer and localized temperature drops in the mold, leading to billet shell warping and uneven growth. Therefore, accurately determining the air gap location is crucial for targeted process improvements. Thus, accurately determining the air gap location is a pressing technical problem that needs to be solved. Summary of the Invention
[0003] This invention provides an improved method, apparatus, and equipment for the process parameters of a continuous casting machine, solving the technical problem of how to accurately determine the air gap position.
[0004] In a first aspect, embodiments of the present invention provide a method for improving the process parameters of a continuous casting machine. The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow and wide copper plates are provided with drilled holes, the extension direction of which is from the top to the bottom of the crystallizer. A chain-structured fiber optic grating temperature sensor is disposed through the drilled holes. The method includes: acquiring temperature information obtained by the fiber optic grating temperature sensor detecting molten steel in the crystallizer; if the temperature information indicates the presence of an air gap in the molten steel, determining the location information of the air gap based on the temperature information; and improving the process parameters of the continuous casting machine based on the location information of the air gap.
[0005] In conjunction with the first aspect of the present invention, in some embodiments, each of the fiber optic temperature sensors includes multiple detection points, and the temperature information includes temperature sub-information of each of the multiple detection points, wherein the temperature sub-information of the detection point includes the temperature of the molten steel at different times at that detection point; the method further includes: if the temperature sub-information of each of the multiple detection points contains first target temperature sub-information that meets a first preset requirement, determining that the temperature information indicates the presence of an air gap in the molten steel; wherein the first preset requirement is that, in the first target temperature sub-information, the temperature of the molten steel decreases by a first temperature in a first time period, and the temperature of the molten steel increases by a second temperature in a second time period immediately following the first time period.
[0006] In conjunction with the first aspect of the present invention, in some embodiments, the first time period includes 5s to 50s, the first temperature includes 10℃ to 40℃, the second time period includes 10s to 60s, and the second temperature includes 10℃ to 40℃.
[0007] In conjunction with the first aspect of the present invention, in some embodiments, determining the position information of the air gap based on the temperature information includes: obtaining at least one detection point based on the detection point corresponding to the first target temperature sub-information; among the at least one detection point, taking the detection point closest to the top of the crystallizer as the first starting detection point and the detection point farthest from the top of the crystallizer as the first ending detection point; determining the starting position of the air gap based on the position of the first starting detection point, determining the ending position of the air gap based on the position of the first ending detection point, and determining the distribution length of the air gap based on the distance between the first starting detection point and the first ending detection point; the position information includes the starting position, ending position, and distribution length of the air gap.
[0008] In conjunction with the first aspect of the present invention, in some embodiments, the method further includes: if the temperature information indicates the presence of a protective slag in the molten steel, determining the flow rate of the protective slag based on the temperature information; and improving the process parameters of the continuous casting machine based on the flow rate of the protective slag.
[0009] In conjunction with the first aspect of the present invention, in some embodiments, the method further includes: if the temperature sub-information of each of the plurality of detection points contains second target temperature sub-information that meets a second preset requirement, determining that the temperature information indicates the presence of the protective slag in the molten steel; wherein, the second preset requirement is that, in the second target temperature sub-information, the temperature of the molten steel decreases by a third temperature during a third time period, and the temperature of the molten steel increases by a fourth temperature during a fourth time period immediately following the third time period; wherein, the third temperature is less than the first temperature.
[0010] In conjunction with the first aspect of the present invention, in some embodiments, the third time period includes 1s to 10s, the third temperature includes 0℃ to 10℃, the fourth time period includes 1s to 5s, and the fourth temperature includes 0℃ to 15℃.
[0011] In conjunction with the first aspect of the present invention, in some embodiments, the fiber Bragg grating temperature sensor has 15 to 20 detection points, and the spacing between different detection points on the fiber Bragg grating temperature sensor is 10 mm to 20 mm; the fiber Bragg grating temperature sensor has a reflectivity greater than or equal to 80%, a temperature resolution of 0.01 ℃, a temperature accuracy of 0.5 ℃ to 2 ℃, a temperature range of 50 ℃ to 300 ℃, and is packaged in ceramic with a diameter of 0.2 mm to 0.5 mm; the fiber Bragg grating temperature sensor measures the Bragg wavelength range of reflected light from 1400 nm to 1800 nm.
[0012] Secondly, embodiments of the present invention provide an apparatus for improving the process parameters of a continuous casting machine. The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow and wide copper plates are provided with drilled holes, the extension direction of which is from the top to the bottom of the crystallizer. A chain-structured fiber optic grating temperature sensor is disposed through the drilled holes. The apparatus includes: an information acquisition unit for acquiring temperature information obtained by the fiber optic grating temperature sensor from the molten steel in the crystallizer; a position determination unit for determining the position information of the air gap based on the temperature information if the temperature information indicates the presence of an air gap in the molten steel; and an improvement unit for improving the process parameters of the continuous casting machine based on the position information of the air gap.
[0013] Thirdly, embodiments of the present invention provide an electronic device, including: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the method described in any of the first aspects.
[0014] The embodiments of the present invention provide one or more technical solutions that achieve at least the following technical effects or advantages: This invention utilizes temperature information obtained from the detection of molten steel within the crystallizer by a fiber optic grating temperature sensor. If the temperature information indicates the presence of an air gap in the molten steel, the location of the air gap is determined based on the temperature information. Based on the location of the air gap, the process parameters of the continuous casting machine are improved. By drilling holes in both the narrow and wide copper plates and embedding the fiber optic grating temperature sensor within these holes, the temperature field within the crystallizer can be measured. Since the presence of an air gap affects the temperature field, the existence and location of the air gap can be determined based on the temperature detection results from the fiber optic grating temperature sensor. Therefore, the invention achieves the beneficial effect of accurately determining the location of the air gap. Attached Figure Description
[0015] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a front view of the crystallizer in an embodiment of the present invention; Figure 2 This is a top view of the crystallizer in an embodiment of the present invention; Figure 3 This is a flowchart of a method for improving the process parameters of a continuous casting machine in an embodiment of the present invention; Figure 4 This is a functional block diagram of the device for improving the process parameters of a continuous casting machine in an embodiment of the present invention; Figure 5 This is a schematic diagram of the structure of the electronic device in an embodiment of the present invention; Among them, 1 is the crystallizer, 2 is the immersion nozzle, 3 is the narrow copper plate, 4 is the drill hole, 5 is the fiber optic temperature sensor, and 6 is the wide copper plate. Detailed Implementation
[0017] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0018] In this invention, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. Furthermore, the technical solutions of the various embodiments can be combined with each other, but only on the basis of being achievable by those skilled in the art. If the combination of technical solutions is contradictory or impossible to implement, such a combination of technical solutions should be considered non-existent and not within the scope of protection claimed by this invention.
[0019] This invention provides a method for improving the process parameters of a continuous casting machine, with reference to... Figure 1 and Figure 2 As shown, Figure 1 This is a front view of the crystallizer in an embodiment of the present invention. Figure 2This is a top view of the crystallizer in an embodiment of the present invention. The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow and wide copper plates have drilled holes extending from the top to the bottom of the crystallizer. A chain-structured fiber optic grating temperature sensor is disposed through one of the drilled holes. It should be noted that... Figure 1 and Figure 2 The drawing only shows the drill holes for the narrow copper plate and the fiber Bragg grating temperature sensor; the drill holes for the wide copper plate and the fiber Bragg grating temperature sensor are not shown. The top of the crystallizer is the end with the open casting inlet, and the immersion gate extends into the crystallizer cavity from the casting inlet to inject molten steel. The bottom of the crystallizer is the end with the billet exit.
[0020] refer to Figure 3 As shown, Figure 3 This is a flowchart of a method for improving the process parameters of a continuous casting machine in an embodiment of the present invention; the method includes the following steps S101 to S103: S101: Acquire temperature information obtained by the fiber optic grating temperature sensor from detecting the molten steel in the crystallizer.
[0021] It should be noted that the fiber Bragg grating temperature sensor may include a temperature sensor body and a fiber Bragg grating demodulator. The temperature sensor body measures the temperature change of the molten steel and outputs a wavelength signal. The temperature measurement time of the temperature sensor body can be 0.04s / time. The wavelength signal output by the temperature sensor body is demodulated by the fiber Bragg grating demodulator. The temperature information output by the fiber Bragg grating demodulator after demodulation enables the detection of temperature changes on the inner wall of the copper plate of the crystallizer.
[0022] It should be noted that the fiber Bragg grating temperature sensor has 15 to 20 detection points, and the spacing between different detection points on the fiber Bragg grating temperature sensor is 10 mm to 20 mm; the reflectivity of the fiber Bragg grating temperature sensor is greater than or equal to 80%, the temperature resolution is 0.01 ℃, the temperature accuracy is 0.5 ℃ to 2 ℃, the temperature range is 50 ℃ to 300 ℃, the packaging method is ceramic packaging, and the diameter is 0.2 mm to 0.5 mm; the fiber Bragg wavelength range for measuring reflected light is 1400 nm to 1800 nm.
[0023] It should be noted that the diameter of the drilled hole needs to be determined based on the diameter of the fiber Bragg grating temperature sensor to ensure that the sensor can be installed throughout the hole. Assuming the narrow-face copper plate has two rows of drilled holes and the wide-face copper plate has three rows, the narrow-face copper plate can have fiber Bragg grating temperature sensors a and b, while the wide-face copper plate can have fiber Bragg grating temperature sensors c, d, and e. Each fiber Bragg grating temperature sensor will detect its own temperature information.
[0024] S102: If the temperature information indicates the presence of an air gap in the molten steel, determine the location information of the air gap based on the temperature information.
[0025] In some embodiments, each fiber Bragg grating temperature sensor includes multiple detection points, and the temperature information includes temperature sub-information for each of the multiple detection points, wherein the temperature sub-information for each detection point includes the temperature of the molten steel at different times at that detection point; the method further includes: if the temperature sub-information for each of the multiple detection points contains first target temperature sub-information that meets a first preset requirement, determining that the temperature information indicates the presence of an air gap in the molten steel; wherein the first preset requirement is that in the first target temperature sub-information, the temperature of the molten steel decreases by a first temperature in a first time period, and the temperature of the molten steel increases by a second temperature in a second time period immediately following the first time period.
[0026] It should be noted that during the peritectic reaction of peritectic steel, the solidified billet shell detaches from the copper plate of the crystallizer due to volume shrinkage, forming an air gap. The high thermal resistance of the air gap hinders heat transfer to the copper plate, causing a sharp drop in temperature. As the billet moves downward, the shell thickens and re-adheres to the copper plate, the air gap closes, heat transfer resumes, and the copper plate temperature rises accordingly. Therefore, if a temperature sub-information meets the first preset requirement, an air gap exists at the detection point corresponding to that temperature sub-information.
[0027] In some implementations, the first time period includes 5s to 50s, the first temperature includes 10℃ to 40℃, the second time period includes 10s to 60s, and the second temperature includes 10℃ to 40℃.
[0028] In some implementations, determining the location information of the air gap based on temperature information includes: obtaining at least one detection point based on the detection point corresponding to the first target temperature sub-information; among the at least one detection point, taking the detection point closest to the top of the crystallizer as the first starting detection point and the detection point farthest from the top of the crystallizer as the first ending detection point; determining the starting position of the air gap based on the position of the first starting detection point, determining the ending position of the air gap based on the position of the first ending detection point, and determining the distribution length of the air gap based on the distance between the first starting detection point and the first ending detection point; the location information includes the starting position, ending position, and distribution length of the air gap.
[0029] It should be noted that obtaining at least one detection point based on the detection point corresponding to the first target temperature sub-information can be achieved by using the detection point corresponding to the first target temperature sub-information as at least one detection point. Determining the starting position of the air gap based on the position of the first starting detection point can be achieved by using the position of the first starting detection point as the starting position of the air gap. Determining the ending position of the air gap based on the position of the first ending detection point can be achieved by using the position of the first ending detection point as the ending position of the air gap. Determining the distribution length of the air gap based on the distance between the first starting detection point and the first ending detection point can be achieved by using the distance between the first starting detection point and the first ending detection point as the distribution length of the air gap.
[0030] S103: Based on the location information of the air gap, the process parameters of the continuous casting machine are improved.
[0031] For example, the casting speed can be adjusted based on the starting position of the air gap. If the starting position of the air gap is too high (close to the meniscus), it indicates that the initial billet shell undergoes peritectic reaction and volume shrinkage too early. A process parameter improvement measure could be to reduce the casting speed to prolong the residence time of the molten steel in the upper part of the crystallizer, thereby thickening the initial billet shell, increasing its strength, delaying the occurrence of peritectic reaction, and moving the starting point of the air gap downwards in the crystallizer. As another example, the cooling intensity of the crystallizer can be adjusted based on the distribution length of the air gap. If the distribution length of the air gap is too long, it indicates that the heat transfer between the billet shell and the copper plate is continuously deteriorating and shrinkage is uneven. A process parameter improvement measure could be to optimize the cooling water flow rate and cooling distribution in the crystallizer, appropriately enhancing cooling in the corresponding area of the air gap to accelerate billet shell solidification, reduce volume shrinkage, and thus shorten the air gap length.
[0032] In some embodiments, the method for improving the process parameters of the continuous casting machine further includes: if the temperature information indicates the presence of protective slag in the molten steel, determining the flow rate of the protective slag based on the temperature information; and improving the process parameters of the continuous casting machine based on the flow rate of the protective slag.
[0033] In some embodiments, the method for improving the process parameters of the continuous casting machine further includes: if the temperature sub-information of each of the multiple detection points contains a second target temperature sub-information that meets a second preset requirement, it is determined that the temperature information indicates the presence of protective slag in the molten steel; wherein, the second preset requirement is that, in the second target temperature sub-information, the molten steel temperature decreases by a third temperature during a third time period, and the molten steel temperature increases by a fourth temperature during a fourth time period immediately following the third time period; wherein, the third temperature is less than the first temperature.
[0034] It should be noted that the temperature of the newly added mold flux is much lower than that of the copper plate and molten steel in the mold. When the flux flows to the corresponding detection point area of the sensor, it quickly absorbs local heat from the copper plate, causing a brief drop in the temperature of the inner wall of the copper plate. Then, the flux rapidly melts at high temperature, forming a continuous and uniform liquid slag film between the billet shell and the copper plate of the mold. This slag film fills the tiny gaps between the billet shell and the copper plate, significantly improving heat transfer efficiency. The heat from the billet is transferred to the copper plate more smoothly, increasing the heat received by the copper plate and causing its temperature to rise rapidly. However, it should be noted that the temperature change caused by the flux is less than the temperature change caused by the air gap, i.e., the third temperature is less than the first temperature. Therefore, if the temperature sub-information meets the second preset requirement, then flux is present at the detection point corresponding to that temperature sub-information.
[0035] In some implementations, the third time period includes 1s to 10s, the third temperature includes 0℃ to 10℃, the fourth time period includes 1s to 5s, and the fourth temperature includes 0℃ to 15℃.
[0036] It should be noted that both protective slag and air gaps can cause localized temperature changes. If not distinguished, protective slag might be mistaken for an air gap, leading to incorrect process parameter adjustments and reduced production reliability of the continuous casting machine. Therefore, this embodiment of the invention distinguishes between protective slag and air gaps by limiting different temperature changes at different times. When protective slag is identified, the process parameters of the continuous casting machine are improved based on its flow velocity. When an air gap is identified, the process parameters are improved based on the air gap's location information. Thus, targeted process adjustments are achieved, improving the production reliability of the continuous casting machine.
[0037] In some implementations, determining the flow velocity of the protective slag based on temperature information includes: obtaining at least two detection points based on the detection points corresponding to the second target temperature sub-information; selecting a first detection point and a second detection point from the at least two detection points; determining a first moment when the protective slag flows through the first detection point and a second moment when the protective slag flows through the second detection point; obtaining the flow duration based on the difference between the first moment and the second moment; and using the quotient of the distance between the first detection point and the second detection point divided by the flow duration as the flow velocity of the protective slag.
[0038] The following examples illustrate how to improve the process parameters of a continuous casting machine based on the flow rate of the protective slag: First, adjust the billet casting speed. When the protective slag flow rate is significantly lower than the billet casting speed, appropriately reduce the billet casting speed to extend the spreading and flow time of the protective slag in the upper part of the crystallizer, allowing the protective slag to flow downwards synchronously with the billet and eliminating flow rate lag. Second, optimize the physicochemical properties of the protective slag. To address the problem of excessively slow flow rate, adjust the viscosity, melting rate, and spreading properties of the protective slag: reduce the viscosity, increase the melting rate and spreading ability, and accelerate the downward flow speed of the protective slag, making its flow rate close to or match the billet casting speed. Third, optimize the protective slag addition process. Adopt a continuous, quantitative, and uniform addition method instead of intermittent addition to avoid flow rate fluctuations caused by protective slag interruption and accumulation, ensuring that the slag film continuously and stably flows into the gap between the billet shell and the copper plate.
[0039] It should be noted that, in addition to using fiber Bragg grating temperature sensors to measure temperature, embedded thermocouples can also be used to measure the temperature field distribution within the crystallizer. Thermocouple temperature measurement offers advantages such as providing fast and stable temperature measurement, along with high accuracy and high-temperature resolution. However, thermocouples can only provide single-point temperature measurements and are not suitable for detecting very dense temperature fluctuations, such as the formation of the solidified billet shell during the peritectic transformation in peritectic steel. If a large number of thermocouples were embedded in the crystallizer to generate a thermal image, this would not only require extensive machining but also interfere with the material being measured. This conduction blockage is usually caused by the numerous cavities machined to accommodate the thermocouple sensors. Therefore, this embodiment of the invention uses fiber Bragg grating temperature sensors, avoiding the use of thermocouples for temperature measurement and thus avoiding extensive machining, achieving the beneficial effect of improved temperature measurement convenience. Simultaneously, it avoids interference with the material being measured, improving the production reliability of the continuous casting machine.
[0040] It should be noted that, with two rows of drilled holes in the narrow-face copper plate, based on continuous temperature measurement results and the known location of the fiber optic temperature sensor, temperature change curves for the two parallel channels at different casting times can be obtained. By observing the trend of the densely distributed temperature curves as casting time increases, the formation characteristics of the billet shell during the initial solidification stage along the height of the narrow-face copper plate in the crystallizer can be displayed. This allows for accurate measurement of the location of the local air gap between the initial solidified billet shell and the crystallizer caused by volume shrinkage during the peritectic reaction.
[0041] It should be noted that the location information of the air gap is determined based on the location of the detection point. Furthermore, the location of the detection point can be determined based on the meniscus, which is the free liquid surface of the molten steel at the very top of the crystallizer. It is the starting point where the molten steel begins to solidify into a billet shell.
[0042] The following example illustrates the air gap issue. An industrial test was conducted on a slab continuous casting machine at a steel plant, with thermocouples and fiber Bragg grating temperature sensors installed respectively for temperature comparison and analysis. The ladle tonnage was 80 t, the steel grade was SPA-H, the casting cross-section was 1000 mm × 237 mm, the casting speed was 1.45 m / min, and the depth of the submerged entry nozzle into the liquid surface was 150 mm. A total of 7 heats were cast in this test, and temperature data measured by thermocouples and fiber Bragg grating temperature sensors were obtained for different casting cycles. The measurement data from both thermocouples and fiber Bragg grating temperature sensors showed relatively consistent trends in their respective systems, indicating that the temperature changes in the molten steel were effectively reflected. However, the temperature change curve measured by the fiber Bragg sensor showed more pronounced fluctuations. At a distance of 248 mm from the meniscus, the temperature dropped sharply from 162 ℃ to 125 ℃, and then rose again to 141 ℃. This reflects the change in the local air gap between the initial solidified slab shell and the crystallizer during the peritectic reaction in peritectic steel solidification. In addition, based on the analysis of temperature information, the starting position of the air gap was determined to be 248 mm from the meniscus, and the ending position of the air gap was determined to be 351 mm from the meniscus. The distribution length of the air gap can be estimated to be 103 mm.
[0043] The following example illustrates the use of mold flux. A comparative analysis experiment was conducted on a slab continuous casting machine at a steel plant, using both thermocouples and fiber Bragg grating temperature sensors for continuous addition of mold flux. The ladle tonnage was 80 t, the steel grade was 590CL, the casting cross-section was 1300 mm × 237 mm, the casting speed was 1.4 m / min, and the submerged entry nozzle was inserted to a depth of 180 mm into the liquid surface. A total of 5 heats were cast, with mold flux added 5 times consecutively during normal production. At the moment of mold flux addition, the temperature change curve measured by the thermocouple was flat with no significant fluctuations. However, the temperature change curve measured by the fiber Bragg grating temperature sensor first decreased and then rose sharply by about 12 °C, followed by a slow decrease. The same temperature change pattern was observed the next time mold flux was added. Based on the data, the downward flow velocity of the mold flux was determined to be approximately 0.96 m / min, lower than the slab casting speed of 1.4 m / min. This indicates that the physical and chemical properties of the current protective slag need to be optimized and improved to enhance its lubrication performance and better promote heat transfer between the solidified billet shell and the copper plate of the crystallizer.
[0044] This invention utilizes temperature information obtained from the detection of molten steel within the crystallizer by a fiber optic grating temperature sensor. If the temperature information indicates the presence of an air gap in the molten steel, the location of the air gap is determined based on the temperature information. Based on the location of the air gap, the process parameters of the continuous casting machine are improved. By drilling holes in both the narrow and wide copper plates and embedding the fiber optic grating temperature sensor within these holes, the temperature field within the crystallizer can be measured. Since the presence of an air gap affects the temperature field, the existence and location of the air gap can be determined based on the temperature detection results from the fiber optic grating temperature sensor. Therefore, the invention achieves the beneficial effect of accurately determining the location of the air gap.
[0045] Based on the same inventive concept, and referring to Figure 4 As shown, this embodiment of the invention provides a device 10 for improving the process parameters of a continuous casting machine. The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow and wide copper plates are provided with drilled holes, the extension direction of which is from the top to the bottom of the crystallizer. A chain-structured fiber optic grating temperature sensor is disposed through the drilled holes. The device 10 for improving the process parameters of the continuous casting machine includes: an information acquisition unit 110, used to acquire temperature information obtained by the fiber optic grating temperature sensor from the molten steel in the crystallizer; a position determination unit 120, used to determine the position information of the air gap based on the temperature information if the temperature information indicates the presence of an air gap in the molten steel; and an improvement unit 130, used to improve the process parameters of the continuous casting machine based on the position information of the air gap.
[0046] It is understood that each fiber optic temperature sensor includes multiple detection points, and the temperature information includes temperature sub-information for each of the multiple detection points. This temperature sub-information for each detection point includes the temperature of the molten steel at different times at that detection point. The continuous casting machine process parameter improvement device 10 further includes: a first determination unit, used to determine that if the temperature sub-information for each of the multiple detection points contains a first target temperature sub-information that meets a first preset requirement, the temperature information indicates the presence of an air gap in the molten steel. The first preset requirement is that, in the first target temperature sub-information, the molten steel temperature decreases by a first temperature within a first time period, and then increases by a second temperature within a second time period immediately following the first time period. The first time period includes 5s to 50s, and the first temperature includes 10℃ to 40℃; the second time period includes 10s to 60s, and the second temperature includes 10℃ to 40℃.
[0047] Understandably, the position determination unit 120 is specifically used for: obtaining at least one detection point based on the detection point corresponding to the first target temperature sub-information; among the at least one detection point, taking the detection point closest to the top of the crystallizer as the first starting detection point and the detection point farthest from the top of the crystallizer as the first ending detection point; determining the starting position of the air gap based on the position of the first starting detection point, determining the ending position of the air gap based on the position of the first ending detection point, and determining the distribution length of the air gap based on the distance between the first starting detection point and the first ending detection point; the position information includes the starting position, ending position, and distribution length of the air gap.
[0048] Understandably, the process parameter improvement device 10 for the continuous casting machine also includes: a flow rate determination unit, used to determine the flow rate of the protective slag based on the temperature information indicating the presence of protective slag in the molten steel; and a parameter improvement unit, used to improve the process parameters of the continuous casting machine based on the flow rate of the protective slag.
[0049] It is understandable that the process parameter improvement device 10 for the continuous casting machine further includes: a second determination unit, used to determine that if the temperature sub-information of each of the multiple detection points contains second target temperature sub-information that meets the second preset requirement, the temperature information indicates the presence of protective slag in the molten steel; wherein, the second preset requirement is that, in the second target temperature sub-information, the molten steel temperature decreases by a third temperature during the third time period, and the molten steel temperature rises by a fourth temperature during the fourth time period immediately following the third time period; wherein, the third temperature is lower than the first temperature. The third time period includes 1s to 10s, and the third temperature includes 0℃ to 10℃; the fourth time period includes 1s to 5s, and the fourth temperature includes 0℃ to 15℃.
[0050] The fiber Bragg grating temperature sensor has 15 to 20 detection points, with a spacing of 10 mm to 20 mm between different detection points. The sensor has a reflectivity greater than or equal to 80%, a temperature resolution of 0.01 ℃, a temperature accuracy of 0.5 ℃ to 2 ℃, a temperature range of 50 ℃ to 300 ℃, and is packaged in ceramic with a diameter of 0.2 mm to 0.5 mm. The sensor measures the Bragg wavelength of reflected light in the range of 1400 nm to 1800 nm.
[0051] It should be understood that further implementation details of the continuous casting machine process parameter improvement device 10 in the embodiments of the present invention are as described in the aforementioned method for improving the process parameters of the continuous casting machine, and will not be repeated here for the sake of brevity.
[0052] Based on the same inventive concept, embodiments of the present invention also provide an electronic device, such as... Figure 5As shown, it includes a memory 304, a processor 302, and a computer program stored in the memory 304 and executable on the processor 302. The processor 302 executes the program to implement the steps described in any embodiment of the method for improving the process parameters of the continuous casting machine.
[0053] Among them, Figure 5 In this document, a bus architecture (represented by bus 300) is used. Bus 300 may include any number of interconnected buses and bridges, linking various circuits including one or more processors represented by processor 302 and memory represented by memory 304. Bus 300 may also link various other circuits such as peripheral devices, voltage regulators, and power management circuits, which are well known in the art and therefore will not be described further herein. Bus interface 305 provides an interface between bus 300 and receiver 301 and transmitter 303. Receiver 301 and transmitter 303 may be the same element, i.e., a transceiver, providing a unit for communicating with various other devices over a transmission medium. Processor 302 is responsible for managing bus 300 and general processing, while memory 304 can be used to store data used by processor 302 during operation.
[0054] The functions described herein can be implemented in hardware, software executed by a processor, firmware, or any combination thereof. If implemented in software executed by a processor, the functions can be stored as one or more instructions or codes on or transmitted via a computer-readable medium. Other examples and embodiments are within the scope and spirit of this invention and the appended claims. For example, due to the nature of software, the functions described above can be implemented using software executed by a processor, hardware, firmware, hardwired, or any combination thereof. Furthermore, the functional units can be integrated into a single processing unit, or each unit can exist physically separately, or two or more units can be integrated into a single unit.
[0055] In the several embodiments provided in this application, it should be understood that the disclosed technical content can be implemented in other ways. The device embodiments described above are merely illustrative; for example, the division of units can be a logical functional division, and in actual implementation, there may be other division methods. For instance, multiple units or components may be combined or integrated into another system, or some features may be ignored or not executed. Furthermore, the displayed or discussed mutual coupling, direct coupling, or communication connection may be through some interfaces; the indirect coupling or communication connection between units or modules may be electrical or other forms.
[0056] The units described as separate components may or may not be physically separate. Similarly, the components of the control device may or may not be physical units; they may be located in one place or distributed across multiple units. Some or all of the units can be selected to achieve the purpose of this embodiment, depending on actual needs.
[0057] If the integrated unit is implemented as a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of the present invention, in essence, or the part that contributes to the prior art, or all or part of the technical solution, can be embodied in the form of a software product. This computer software product is stored in a storage medium and includes several instructions to cause a computer device (which may be a personal computer, server, or network device, etc.) to execute all or part of the steps of the methods described in the various embodiments of the present invention. The aforementioned storage medium includes various media capable of storing program code, such as USB flash drives, read-only memory (ROM), random access memory (RAM), portable hard drives, magnetic disks, or optical disks.
[0058] The above description is merely an embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of the claims of the present invention.
Claims
1. A method for improving the process parameters of a continuous casting machine, characterized in that, The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow copper plate and the wide copper plate are provided with drill holes, and the extension direction of the drill holes is from the top of the crystallizer to the bottom of the crystallizer. A chain-structured fiber optic temperature sensor is disposed throughout the borehole; the method includes: The temperature information obtained by the fiber optic temperature sensor from the molten steel in the crystallizer is acquired. If the temperature information indicates the presence of an air gap in the molten steel, the location information of the air gap is determined based on the temperature information. Based on the location information of the air gap, the process parameters of the continuous casting machine are improved.
2. The method for improving the process parameters of a continuous casting machine according to claim 1, characterized in that, Each fiber Bragg grating temperature sensor includes multiple detection points, and the temperature information includes temperature sub-information of each of the multiple detection points, which includes the temperature of the molten steel at different times at that detection point. The method further includes: If the temperature sub-information of each of the plurality of detection points contains a first target temperature sub-information that meets the first preset requirement, it is determined that the temperature information indicates that the molten steel has an air gap; wherein, the first preset requirement is that in the first target temperature sub-information, the temperature of the molten steel decreases by a first temperature in a first time period, and the temperature of the molten steel increases by a second temperature in a second time period immediately following the first time period.
3. The method for improving the process parameters of a continuous casting machine according to claim 2, characterized in that, The first time period includes 5s to 50s, and the first temperature includes 10℃ to 40℃. The second time period includes 10s to 60s, and the second temperature includes 10℃ to 40℃.
4. The method for improving the process parameters of a continuous casting machine according to claim 2, characterized in that, Determining the location information of the air gap based on the temperature information includes: Based on the detection points corresponding to the first target temperature sub-information, at least one detection point is obtained; In the at least one detection point, the detection point closest to the top of the crystallizer is taken as the first starting detection point, and the detection point farthest from the top of the crystallizer is taken as the first ending detection point; The starting position of the air gap is determined based on the position of the first starting detection point, the ending position of the air gap is determined based on the position of the first ending detection point, and the distribution length of the air gap is determined based on the distance between the first starting detection point and the first ending detection point; the position information includes the starting position, ending position, and distribution length of the air gap.
5. The method for improving the process parameters of a continuous casting machine according to claim 2, characterized in that, Also includes: If the temperature information indicates the presence of protective slag in the molten steel, the flow rate of the protective slag is determined based on the temperature information; Based on the flow rate of the protective slag, the process parameters of the continuous casting machine are improved.
6. The method for improving the process parameters of a continuous casting machine according to claim 5, characterized in that, Also includes: If the temperature sub-information of each of the plurality of detection points contains a second target temperature sub-information that meets the second preset requirement, it is determined that the temperature information indicates that the molten steel contains the protective slag; wherein, the second preset requirement is that, in the second target temperature sub-information, the temperature of the molten steel decreases by a third temperature during the third time period, and the temperature of the molten steel increases by a fourth temperature during the fourth time period immediately following the third time period; wherein, the third temperature is less than the first temperature.
7. The method for improving the process parameters of a continuous casting machine according to claim 6, characterized in that, The third time period includes 1s to 10s, the third temperature includes 0℃ to 10℃, the fourth time period includes 1s to 5s, and the fourth temperature includes 0℃ to 15℃.
8. The method for improving the process parameters of the continuous casting machine according to any one of claims 1-7, characterized in that, The fiber Bragg grating temperature sensor has 15 to 20 detection points, and the spacing between different detection points on the fiber Bragg grating temperature sensor is 10 mm to 20 mm. The fiber Bragg grating temperature sensor has a reflectivity greater than or equal to 80%, a temperature resolution of 0.01 ℃, a temperature accuracy of 0.5 ℃ to 2 ℃, a temperature range of 50 ℃ to 300 ℃, and is packaged in ceramic with a diameter of 0.2 mm to 0.5 mm. The fiber Bragg grating temperature sensor measures the Bragg wavelength range of reflected light from 1400 nm to 1800 nm.
9. A device for improving the process parameters of a continuous casting machine, characterized in that, The continuous casting machine includes a crystallizer, which includes a narrow copper plate and a wide copper plate. Both the narrow copper plate and the wide copper plate are provided with drill holes, and the extension direction of the drill holes is from the top of the crystallizer to the bottom of the crystallizer. A chain-structured fiber optic temperature sensor is disposed throughout the borehole; the device includes: The information acquisition unit is used to acquire the temperature information obtained by the fiber optic grating temperature sensor from the molten steel in the crystallizer; A position determination unit is used to determine the position information of the air gap based on the temperature information if the temperature information indicates that an air gap exists in the molten steel. An improvement unit is used to improve the process parameters of the continuous casting machine based on the location information of the air gap.
10. An electronic device, characterized in that, include: A memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor, when executing the computer program, implements the method of any one of claims 1-8.