Methods, systems, and trains for assessing the safety of component defects.

By reconstructing the true geometric shape of defects in metal components and performing node-level analysis, the problem of bias in safety assessment results in existing technologies has been solved, enabling more accurate safety assessments and risk judgments under multiple working conditions.

CN123069764APending Publication Date: 2026-11-10CRRC QINGDAO SIFANG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611290048.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-24
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing technologies, when assessing defects in metal components, simplify them into regular shapes, leading to deviations between safety assessment results and actual conditions. They fail to reflect the true geometric characteristics of defects, ignore differences in leading edge nodes, lack criteria for short crack propagation, and cannot uniformly evaluate risks under multiple operating conditions.

Method used

By reconstructing the true geometric shape from the defect contour data, a sequence of target defect contour nodes is generated. Leading edge curves and cutting lines are generated in the baseline structural model, mesh elements are configured, the stress intensity factor of the defect structural model is analyzed, and the safety assessment results are determined by combining stress eigenvalues ​​and safety assessment indicators.

Benefits of technology

It improves the accuracy of safety assessments, reflects the true geometric characteristics of defects, provides node-level assessments, and is adaptable to risk assessments under multiple operating conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123069764A_ABST
    Figure CN123069764A_ABST
Patent Text Reader

Abstract

This application provides a method, system, and train for evaluating the safety of defects in structural components, applied in the field of safety assessment technology for engineering structural metal components based on fracture mechanics. The method includes: processing contour detection data of the defect region on the component to be evaluated to obtain a target defect contour node sequence; generating a leading-edge curve and cutting lines on both sides of the leading-edge curve based on the target defect contour node sequence in a reference structural model; configuring multiple mesh elements in the region between the cutting lines, and replacing the mesh elements traversed by the leading-edge curve with defect elements to obtain a defect structural model; analyzing the defect structural model to obtain the stress intensity factor of the leading-edge nodes on the leading-edge curve of the defect structural model under the analysis step; determining the stress characteristic value and safety assessment index of the leading-edge nodes based on the stress intensity factor of the leading-edge nodes under the analysis step; and determining the safety assessment result based on the stress characteristic value and the safety assessment index.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of safety assessment technology for engineering structural metal components based on fracture mechanics, and specifically to a method, system, and train for assessing the safety of component defects. Background Technology

[0002] With the expansion of engineering structural equipment and the increase in service load levels, the safety and reliability requirements for metal components are rising, leading to a corresponding increase in the demand for metal component inspection. Various inspection methods can detect various manufacturing or service defects in metal components, which are relatively common in metal components of rail transit vehicles.

[0003] Currently, safety assessments for such defects typically involve simplifying the actual defect into a regular semi-elliptical or elliptical outline based on its length and width, so that traditional analytical models can be applied for analysis. However, due to the variations in shape, depth, local depressions, and sharp features of real defects, the standardization process loses these key details, causing the safety assessment results to deviate from the actual situation and reducing the accuracy of the assessment results. Summary of the Invention

[0004] In view of the above problems, this application provides a method, system and train for assessing the safety of component defects to improve the accuracy of assessment results.

[0005] One aspect of this application provides a method for evaluating the safety of defects in a component. The method includes: processing contour detection data of a defect region on the component to be evaluated to obtain a target defect contour node sequence; generating a leading edge curve and cutting lines on both sides of the leading edge curve in a reference structural model based on the target defect contour node sequence, wherein the leading edge curve represents the boundary of the defect region on the reference structural model, and the reference structural model is constructed by the component to be evaluated in a defect-free state; configuring multiple mesh elements in the region between the cutting lines, and replacing the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structural model; analyzing the defect structural model to obtain the stress intensity factor of each leading edge node on the leading edge curve of the defect structural model at each analysis step during the analysis process; determining the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node at each analysis step; and determining the safety assessment result based on the stress characteristic value and the safety assessment index.

[0006] According to an embodiment of this application, the reference structural model is constructed as follows: based on the identification information of the component to be evaluated, an initial reference structural model of the component to be evaluated in a defect-free state is obtained; the actual usage conditions of the component to be evaluated are applied to the initial reference structural model and analyzed to obtain the first stress field data of the initial reference structural model; if the first stress field data passes the verification, the initial reference structural model is used as the reference structural model.

[0007] According to an embodiment of this application, the first stress field data includes the direction of the maximum principal stress; processing the contour detection data of the defect region on the component to be evaluated to obtain a target defect contour node sequence includes: processing the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence; interpolating the initial discrete node sequence to obtain an interpolated contour node sequence, and generating an initial contour based on the interpolated contour node sequence; smoothing the initial contour to obtain a smooth contour; reconstructing the peak and valley regions of the smooth contour to obtain a reconstructed contour; and outputting the target defect contour node sequence based on the reconstructed contour.

[0008] According to an embodiment of this application, the contour detection data is processed based on the direction of the maximum principal stress to obtain an initial discrete node sequence, including: locating the direction of the maximum principal stress at the location of the defect region in the reference structural model based on the contour detection data of the defect region; establishing a reference coordinate system with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; placing the contour detection data in the reference coordinate system; projecting the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress to obtain multiple initial discrete nodes; and cleaning and sorting the initial discrete nodes to obtain an initial discrete node sequence.

[0009] According to an embodiment of this application, the reference coordinate system further includes a second coordinate axis for representing the defect length direction and a third coordinate axis for representing the defect depth direction; each initial discrete node in the initial discrete node sequence has a second coordinate value in the defect length direction and a third coordinate value in the defect depth direction; interpolating the initial discrete node sequence to obtain an interpolated contour node sequence includes: determining the defect length range of the initial discrete node sequence based on the second coordinate value of each initial discrete node in the defect length direction; constructing interpolated coordinate values ​​evenly distributed on the second coordinate axis in the defect length direction within the defect length range; and interpolating the initial discrete node sequence using the interpolated coordinate values ​​to obtain the interpolated contour node sequence.

[0010] According to an embodiment of this application, the peak region includes peak points, and the valley region includes valley points. Reconstructing the peak and valley regions of the smooth contour to obtain a reconstructed contour includes: constructing peak windows and valley windows of predetermined lengths centered on the peak points and valley points, respectively; extracting data within the peak and valley windows to obtain peak window data and valley window data; inputting the peak and valley window data into a contour reconstruction function to obtain initial reconstructed contours of the peak and valley windows, respectively, where the contour reconstruction function is constructed with the peak or valley point as the center of symmetry; fusing the initial reconstructed contours of the peak and valley windows with the original smooth contours within the peak and valley windows, respectively, to obtain local reconstructed contours of the peak and valley windows; and replacing the original smooth contours within the peak and valley windows according to the local reconstructed contours of the peak and valley windows, respectively, to obtain the reconstructed contours.

[0011] According to an embodiment of this application, the reconstructed contour further includes a smooth region, which together with the peak region and the valley region constitutes the reconstructed contour. Based on the reconstructed contour, a target defect contour node sequence is output, including: determining the total number of contour nodes to be output based on the contour length of the reconstructed contour and a preset node spacing; for each of the smooth region, peak region, and valley region: determining the number of nodes in the region based on the total number of contour nodes to be output and a preset weight for the region; within the region, determining encrypted nodes based on the number of nodes in the region and nodes at the region's endpoints; constructing a node set for the region based on the encrypted nodes in the region and nodes at the region's endpoints; and processing the node sets of the smooth region, peak region, and valley region to obtain the target defect contour node sequence.

[0012] According to an embodiment of this application, in a reference structural model, generating a leading edge curve and cutting lines located on both sides of the leading edge curve based on a target defect contour node sequence includes: in the reference structural model, generating a leading edge curve in a plane perpendicular to the direction of the maximum principal stress based on the target defect contour node sequence; and generating cutting lines with the leading edge curve as the center, offset by a predetermined distance on both sides of the leading edge curve.

[0013] According to an embodiment of this application, multiple mesh elements are configured in the region between cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structure model. This includes: configuring multiple mesh elements between cutting lines, wherein the number of mesh elements in the region between cutting lines is odd in the defect length direction, and the number of nodes in the mesh elements in the defect depth direction is greater than or equal to the total number of contour nodes; verifying the baseline structure model configured with mesh elements; and if the verification passes, replacing the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structure model.

[0014] According to an embodiment of this application, the verification of a reference structural model configured with mesh elements includes: applying actual usage conditions of the component to be evaluated to the reference structural model configured with mesh elements and analyzing the results to obtain second stress field data of the reference structural model under the condition of configuring mesh elements; and verifying the reference structural model configured with mesh elements based on the error between the second stress field data and the first stress field data.

[0015] According to an embodiment of this application, the defective structure model is analyzed to obtain the stress intensity factor of each leading node on the leading curve of the defective structure model at each analysis step during the analysis process. This includes: applying the actual usage conditions of the component to be evaluated to the defective structure model, and analyzing the defective structure model to obtain the stress field, strain energy density, and displacement field distribution of each leading node on the leading curve of the defective structure model at each analysis step during the analysis process; and obtaining the stress intensity factor of each leading node at each analysis step based on the stress field, strain energy density, and displacement field distribution of each leading node at each analysis step.

[0016] According to an embodiment of this application, the stress characteristic value and safety assessment index of each leading edge node are determined based on the stress intensity factor of each leading edge node in each analysis step, including: for each leading edge node: extracting the maximum stress intensity factor and minimum stress intensity factor of the leading edge node from the stress intensity factor of the leading edge node in each analysis step; determining the stress intensity factor range and stress ratio of the leading edge node based on the maximum stress intensity factor and minimum stress intensity factor; obtaining the stress characteristic value based on the maximum stress intensity factor, minimum stress intensity factor, stress intensity factor range and stress ratio; and obtaining the safety assessment index based on the stress ratio and multiple assessment parameters.

[0017] According to embodiments of this application, a safety assessment index is obtained based on the stress ratio and multiple evaluation parameters, including: for each leading-edge node: querying a baseline fatigue crack propagation threshold value from a standard file based on the material properties corresponding to the leading-edge node; determining a target fatigue crack propagation threshold value for the leading-edge node based on the stress ratio and the baseline fatigue crack propagation threshold value; determining the material characteristic crack length corresponding to the leading-edge node based on the target fatigue crack propagation threshold value, tensile strength, and stress ratio; and obtaining a node-level defect propagation threshold for the leading-edge node as a safety assessment index based on the defect feature size, the target fatigue crack propagation threshold value, and the material characteristic crack length. The defect feature size of the leading-edge node is determined according to the defect type of the defect region.

[0018] According to embodiments of this application, a safety assessment result is determined based on stress characteristic values ​​and safety assessment indicators, including: obtaining a safety factor for each leading edge node based on the ratio of the node-level defect propagation threshold to the stress intensity factor range; extracting the minimum value of the safety factor from the safety factors of each leading edge node to obtain a target safety factor; obtaining an assessment result indicating the safety of the defect area when the target safety factor is greater than a predetermined value; and obtaining an assessment result indicating the danger of the defect area when the target safety factor is less than or equal to a predetermined value.

[0019] Another aspect of this application provides a system for evaluating the safety of defects in a component. The system includes: a processing module for processing contour detection data of a defect region on the component to be evaluated to obtain a target defect contour node sequence; a generation module for generating a leading edge curve and cutting lines on both sides of the leading edge curve in a reference structural model based on the target defect contour node sequence, wherein the leading edge curve represents the boundary of the defect region on the reference structural model, and the reference structural model is constructed by the component to be evaluated in a defect-free state; a configuration module for configuring multiple mesh elements in the region between the cutting lines and replacing the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structural model; an analysis module for analyzing the defect structural model to obtain the stress intensity factor of each leading edge node on the leading edge curve of the defect structural model at each analysis step during the analysis process; a first determination module for determining the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node at each analysis step; and a second determination module for determining the safety assessment result based on the stress characteristic value and the safety assessment index.

[0020] According to an embodiment of this application, a system for evaluating the safety of component defects further includes: an acquisition module for acquiring an initial reference structural model of the component to be evaluated in a defect-free state based on the identification information of the component to be evaluated; an application module for applying the actual usage conditions of the component to be evaluated to the initial reference structural model and performing analysis to obtain first stress field data of the initial reference structural model; and a verification module for using the initial reference structural model as a reference structural model if the first stress field data passes verification.

[0021] According to an embodiment of this application, the first stress field data includes the direction of the maximum principal stress; the processing module includes: a first processing submodule, used to process the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence; an interpolation submodule, used to interpolate the initial discrete node sequence to obtain an interpolated contour node sequence, and generate an initial contour based on the interpolated contour node sequence; a second processing submodule, used to smooth the initial contour to obtain a smooth contour; a reconstruction submodule, used to reconstruct the peak and valley regions of the smooth contour to obtain a reconstructed contour; and an output submodule, used to output a target defect contour node sequence based on the reconstructed contour.

[0022] According to an embodiment of this application, the first processing submodule includes: a positioning unit, used to locate the direction of the maximum principal stress at the location of the defect region in a reference structural model based on the contour detection data of the defect region; an establishment unit, used to establish a reference coordinate system with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; a first processing unit, used to place the contour detection data in the reference coordinate system; a projection unit, used to project the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress, to obtain multiple initial discrete nodes; and a second processing unit, used to clean and sort the initial discrete nodes to obtain an initial discrete node sequence.

[0023] This application also provides a train, including a memory and a processor; the memory stores a computer program, which, when executed by the processor, is configured to: process contour detection data of a defect region on a component to be evaluated to obtain a target defect contour node sequence; in a reference structural model, generate a leading edge curve and cutting lines on both sides of the leading edge curve based on the target defect contour node sequence, the leading edge curve representing the boundary of the defect region on the reference structural model, the reference structural model being constructed by the component to be evaluated in a defect-free state; configure multiple mesh elements in the region between the cutting lines, and replace the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structural model; analyze the defect structural model to obtain the stress intensity factor of each leading edge node on the leading edge curve of the defect structural model at each analysis step during the analysis process; determine the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node at each analysis step; and determine the safety assessment result based on the stress characteristic value and safety assessment index.

[0024] According to an embodiment of this application, the processor is further configured to: obtain an initial reference structural model of the component to be evaluated in a defect-free state based on the identification information of the component to be evaluated; apply the actual usage conditions of the component to be evaluated to the initial reference structural model and perform analysis to obtain first stress field data of the initial reference structural model; and, if the first stress field data passes the verification, use the initial reference structural model as the reference structural model.

[0025] According to an embodiment of this application, the first stress field data includes the direction of the maximum principal stress, and the processor is further configured to: process the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence; perform interpolation processing on the initial discrete node sequence to obtain an interpolated contour node sequence, and generate an initial contour based on the interpolated contour node sequence; perform smoothing processing on the initial contour to obtain a smooth contour; reconstruct the peak and valley regions of the smooth contour to obtain a reconstructed contour; and output the target defect contour node sequence based on the reconstructed contour.

[0026] According to an embodiment of this application, the processor is further configured to: locate the direction of the maximum principal stress at the location of the defect region in the reference structural model based on the contour detection data of the defect region; establish a reference coordinate system with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; place the contour detection data in the reference coordinate system; project the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress to obtain multiple initial discrete nodes; and perform data cleaning and sorting on the initial discrete nodes to obtain an initial discrete node sequence.

[0027] According to an embodiment of this application, a target defect contour node sequence is obtained by processing the contour detection data of the defect area on the component to be evaluated; in the reference structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve are generated based on the target defect contour node sequence; multiple mesh elements are configured in the area between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structural model; the defect structural model is analyzed to obtain the stress intensity factor of each leading edge node on the leading edge curve of the defect structural model under each analysis step; based on the stress intensity factor of each leading edge node under each analysis step, the stress characteristic value and safety assessment index of each leading edge node are determined; based on the stress characteristic value and safety assessment index, the safety assessment result is determined. During the evaluation process, the contour detection data of the defect area on the component to be evaluated is processed to obtain the target defect contour node sequence, which preserves the true geometric features of the defect. Based on the target defect contour node sequence, a leading edge curve is generated on the benchmark structural model in a defect-free state. Using the leading edge nodes on the leading edge curve as units, the stress characteristic value and safety assessment index of each leading edge node on the defective structural model are determined, thus realizing node-level evaluation of the defect area and improving the accuracy of safety assessment. Attached Figure Description

[0028] The above-mentioned contents, other objects, features and advantages of this application will become clearer from the following description of embodiments with reference to the accompanying drawings, in which:

[0029] Figure 1 This illustration schematically depicts an application scenario of a method for assessing the safety of component defects according to an embodiment of this application.

[0030] Figure 2 A flowchart illustrating a method for assessing the safety of component defects according to an embodiment of this application is shown schematically.

[0031] Figure 3 A schematic diagram illustrating the projection of contour detection data is shown.

[0032] Figure 4 A schematic diagram illustrating a target defect contour node sequence according to an embodiment of this application is shown.

[0033] Figure 5 A schematic diagram illustrating a target defect contour node sequence according to another embodiment of this application is shown.

[0034] Figure 6 This illustration schematically shows a model of a defective structure constructed according to an embodiment of this application;

[0035] Figure 7A schematic diagram illustrating the construction of a defect structure model according to another embodiment of this application is shown;

[0036] Figure 8 A schematic diagram of the resulting document according to an embodiment of this application is shown;

[0037] Figure 9 A schematic diagram illustrating stress characteristic values ​​according to an embodiment of this application is shown.

[0038] Figure 10A A schematic diagram illustrating the determination of defect feature size according to an embodiment of this application is shown;

[0039] Figure 10B A schematic diagram illustrating the determination of defect feature size according to another embodiment of this application is shown;

[0040] Figure 11 A schematic diagram illustrating the variation of the defect propagation threshold with defect feature size and stress ratio according to an embodiment of this application is shown in a three-dimensional example.

[0041] Figure 12 A schematic diagram illustrating the security assessment results according to an embodiment of this application is shown.

[0042] Figure 13 A flowchart illustrating a method for assessing the safety of component defects according to another embodiment of this application is shown schematically;

[0043] Figure 14 This schematic diagram illustrates a structural block diagram of a system for assessing the safety of component defects according to an embodiment of this application;

[0044] Figure 15 A schematic diagram of a train according to an embodiment of this application is shown. Detailed Implementation

[0045] The embodiments of this application will now be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of this application. In the following detailed description, numerous specific details are set forth to provide a thorough understanding of the embodiments of this application for ease of explanation. However, it will be apparent that one or more embodiments may be implemented without these specific details. Furthermore, descriptions of well-known structures and technologies are omitted in the following description to avoid unnecessarily obscuring the concepts of this application.

[0046] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. The terms “comprising,” “including,” etc., as used herein indicate the presence of features, steps, operations, and / or components, but do not exclude the presence or addition of one or more other features, steps, operations, or components.

[0047] All terms used herein (including technical and scientific terms) have the meanings commonly understood by those skilled in the art, unless otherwise defined. It should be noted that the terms used herein are to be interpreted in a manner consistent with the context of this specification, and not in an idealized or overly rigid way.

[0048] When using expressions such as "at least one of A, B and C", they should generally be interpreted in accordance with the meaning that is commonly understood by those skilled in the art (e.g., "a system having at least one of A, B and C" should include, but is not limited to, a system having A alone, a system having B alone, a system having C alone, a system having A and B, a system having A and C, a system having B and C, and / or a system having A, B and C, etc.).

[0049] With the expansion of engineering structural equipment scale and the increase in service load levels, the number of minute abnormal defects found in metal components during manufacturing and service through various inspection methods has increased significantly. Rail transit vehicle components are a typical application scenario for this type of problem. These defects generally have the following characteristics: small size but diverse locations, not cracks, irregular morphology, located in complex multiaxial stress fields, making it difficult to determine their hazard level using simple size limits. Currently, the assessment of this type of defect faces the following challenges:

[0050] The main problems are as follows:

[0051] (1) The defect morphology model is oversimplified and cannot reflect the true geometric features.

[0052] Existing methods typically simplify real-world defects into regular semi-elliptical or elliptical profiles based on their length and width, allowing for analysis using traditional analytical models or finite element fracture mechanics methods. However, real-world defects are significantly more complex in terms of shape variations, depth changes, local depressions, and sharp features; regularization loses these crucial details. Since the crack propagation driving force (stress intensity factor range) is highly dependent on the true geometry of the defect front, simplified models struggle to accurately reflect the actual stress state at the defect front, leading to discrepancies between safety assessments and reality.

[0053] (2) It cannot reflect the non-uniformity of the defect leading edge and lacks the ability to make node-level expansion judgments.

[0054] Existing methods simplify the defect leading edge into a regularized profile and assume the deepest point or surface point as the danger point. However, the actual defect leading edge has significant differences in local geometry, stress state, stress ratio, and equivalent defect size. Such assumptions ignore the real differences between nodes at the leading edge, resulting in the obtained propagation driving force not matching the actual situation, and making it difficult to maintain the accuracy of the evaluation results.

[0055] (3) Existing fatigue crack propagation threshold criteria are not suitable for evaluating the risk of early defect propagation.

[0056] Existing technologies rely on long crack fatigue propagation thresholds as a criterion when determining whether a defect will propagate into a crack. However, long crack thresholds are derived from stable long crack conditions and cannot reflect the short crack behavior of defect propagation in actual engineering, easily underestimating the risk of defect propagation in the early stages. On the other hand, while short crack thresholds can more realistically reflect defect initiation and early propagation behavior, their acquisition relies on specialized short crack fatigue tests, which are demanding, complex, costly, and have poor repeatability, making them difficult to implement in engineering fields. Furthermore, existing short crack threshold models fail to systematically consider the influence of mean stress (stress ratio) under fatigue loads, making it difficult to correspond to actual service loads. Due to the lack of a short crack propagation criterion that is both physically meaningful and easily obtainable in engineering, existing technologies use long crack criteria and lack a defect propagation threshold based on short crack behavior that is available in engineering, resulting in inaccurate judgments on whether a defect will propagate under propagation driving forces.

[0057] (4) There is a lack of a unified evaluation framework for complex and diverse service conditions, making it impossible to achieve consistency judgment across multiple service conditions.

[0058] Engineering components undergo various operating states during actual service, with significant differences in stress amplitude and stress ratio under different conditions. This causes the driving force for defect propagation to continuously change with the changing conditions. Existing methods often only assess one or a few typical conditions, lacking an evaluation framework that can uniformly incorporate all service conditions into a single judgment system. This leads to inconsistent evaluation results and fails to fully reflect the true propagation risk of defects throughout their entire service life.

[0059] In view of this, embodiments of this application provide a method for evaluating the safety of component defects, avoiding the simplistic approach of using only standard regular cracks and single stress levels for defect analysis in the prior art. This method reconstructs the true geometric shape of irregular defects based on defect contour data and discretizes it into a sequence of target defect contour nodes suitable for fracture mechanics analysis. Based on a baseline structural model, defects determined by the target defect contour node sequence are introduced and analyzed to obtain the stress intensity factor of each node at the defect leading edge. Then, based on multi-dimensional evaluation parameters such as defect size, stress ratio, and material characteristic crack length at each node at the defect leading edge, an engineering-applicable defect safety assessment conclusion is obtained, improving the accuracy of the safety assessment results. This application is applicable to the determination of allowable defect sizes and safety assessments of metal components in engineering structures, and is particularly suitable for application scenarios where critical load-bearing metal components such as rail transit vehicles are sensitive to defects and have complex service loads.

[0060] Figure 1The illustration shows an application scenario diagram of a method for assessing the safety of component defects according to an embodiment of this application.

[0061] like Figure 1 As shown, application scenario 100 according to this embodiment may include detection device 101, network 102, server 103, and terminal device 104. Network 102 is used as a medium to provide a communication link between detection device 101, terminal device 104, and server 103. Network 102 may include various connection types, such as wired or wireless communication links or fiber optic cables, etc.

[0062] The detection device 101 can detect defect areas on the component to be evaluated and obtain contour detection data. The contour detection data can be sent to the server 103 via the network 102. The server 103 can process the contour detection data to obtain a safety assessment result. The safety assessment result can be sent to the terminal device 104 via the network 102 so that the user can view the safety assessment result through the terminal device 104.

[0063] The inspection equipment 101 may include a contour inspector, an industrial CT (Computed Tomography) scanner, etc.

[0064] The terminal device 104 can be equipped with various communication client applications, such as result display applications, web browser applications, search applications, instant messaging tools, email clients, social media platform software, etc. (for example only). The terminal device 104 can be various electronic devices with a display screen that support web browsing, including but not limited to smartphones, tablets, laptops, and desktop computers.

[0065] Server 103 can be a server that provides various services, such as a back-end management server that supports the contour detection data sent by the detection device 101 (for example only). The back-end management server can analyze and process data such as contour detection data, and feed back the processing results (such as security assessment results, web pages, information, or data) to the terminal device.

[0066] It should be noted that the method for assessing the safety of component defects provided in this application embodiment can generally be executed by server 103. Correspondingly, the system for assessing the safety of component defects provided in this application embodiment can generally be located in server 103. The method for assessing the safety of component defects provided in this application embodiment can also be executed by a server or server cluster that is different from server 103 and capable of communicating with detection device 101, terminal device 104, and / or server 103. Correspondingly, the system for assessing the safety of component defects provided in this application embodiment can also be located in a server or server cluster that is different from server 103 and capable of communicating with detection device 101, terminal device 104, and / or server 103.

[0067] It should be understood that Figure 1 The number of testing devices, terminal devices, networks, and servers shown is merely illustrative. Depending on implementation needs, any number of testing devices, terminal devices, networks, and servers can be included.

[0068] The following will be based on Figure 1 The described scene, through Figures 2-13 The method for evaluating the safety of component defects according to embodiments of this application will be described in detail.

[0069] Figure 2 A flowchart illustrating a method for assessing the safety of component defects according to an embodiment of this application is shown schematically.

[0070] like Figure 2 As shown, the method for assessing the safety of component defects in this embodiment includes operations S210 to S260.

[0071] In operation S210, the contour detection data of the defect area on the component to be evaluated is processed to obtain the target defect contour node sequence.

[0072] In operation S220, in the reference structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve are generated based on the target defect contour node sequence. The leading edge curve is used to represent the boundary of the defect region on the reference structural model, which is constructed by the component to be evaluated in a defect-free state.

[0073] In operation S230, multiple mesh elements are configured in the area between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain the defect structure model.

[0074] In operation S240, the defect structure model is analyzed to obtain the stress intensity factor of each leading node on the leading edge curve of the defect structure model at each analysis step during the analysis process.

[0075] In operation S250, the stress characteristic value and safety assessment index of each leading edge node are determined based on the stress intensity factor of each leading edge node in each analysis step.

[0076] During operation of S260, the safety assessment results are determined based on stress characteristic values ​​and safety assessment indicators.

[0077] In some embodiments, the component to be evaluated may be an engineering structural metal component that requires defect safety assessment, such as a bearing, wheel, axle, tie rod, axle box, or other component on a vehicle.

[0078] The defective area can be, for example, the area corresponding to manufacturing defects such as inclusions, pores, cracks, lack of fusion, and incomplete penetration on the component to be evaluated, or the area corresponding to service defects such as dents and scratches.

[0079] Contour detection data can be raw data that characterizes the boundary shape of a defect region after the contour of the defect region is detected by non-destructive testing equipment.

[0080] For example, for surface defects of the component to be evaluated, a contour inspection instrument can be used to obtain the shape data of the defect. One type of inspection instrument is a contour inspection instrument that uses a contact probe. First, the defect is replicated, and then discrete contour points are obtained by scanning along the replicated surface with a mechanical probe. Another type of inspection instrument is a non-contact contour inspection instrument that uses laser scanning. It obtains the contour data of the defect surface through a laser displacement sensor and outputs the discrete coordinate points of the defect contour.

[0081] For internal defects in the component to be evaluated, industrial CT can be used to image the structure, and the spatial contour of the internal defects can be obtained through data reconstruction.

[0082] The target defect contour node sequence can be a set of discrete nodes arranged in sequence after processing the contour detection data, used to describe the true geometric boundary shape of the defect region.

[0083] The benchmark structural model can be a finite element model of the component to be evaluated in a defect-free state. When constructing the benchmark structural model, an initial benchmark structural model of the component to be evaluated can be obtained first, and the actual usage conditions of the component to be evaluated can be applied to the initial benchmark structural model to obtain the benchmark structural model. The initial benchmark structural model can be constructed using general finite element analysis software based on the geometric information of the component to be evaluated, such as the component's three-dimensional dimensional data (e.g., length, width, height, thickness, diameter, etc.), geometric topological relationships (e.g., the connection relationships and relative positions between the constituent faces, edges, and vertices), and design benchmark information (e.g., coordinate origin, reference plane, reference axis, etc.).

[0084] The leading edge curve can be a continuous curve generated based on the target defect contour node sequence in the reference structure model. It is used to represent the boundary of the defect region on the reference structure model and serves as a reference for subsequent set cutting.

[0085] Cutting lines can be parallel auxiliary lines located on both sides of the leading edge curve, used to define the extent of a local area on the reference structural model.

[0086] Mesh elements are basic computational units used for finite element analysis, which can be configured in the region between cutting lines, such as quadrilateral elements or hexahedral elements.

[0087] The defect element can be a mesh element used to simulate defects, such as a crack-specific element composed of wedge elements and hexahedral elements.

[0088] A defective structural model can be a finite element model containing defects obtained by replacing the mesh elements traversed by the leading edge curve with defective elements, based on a baseline structural model.

[0089] An analysis step can be any of the calculation steps performed sequentially when performing finite element analysis (i.e. solving the defective structural model) on a defective structural model. Each analysis step can correspond to a load condition.

[0090] Leading nodes can be discrete nodes located on the leading curve.

[0091] The stress intensity factor is a fracture mechanics parameter extracted from the calculation results of each analysis step during the analysis of the defect structure model, used to characterize the stress field intensity at the crack tip at the leading edge node.

[0092] Stress eigenvalues ​​can be statistics determined based on the stress intensity factor of each leading edge node in each analysis step, such as the maximum stress intensity factor, minimum stress intensity factor, stress intensity factor range, and the stress ratio of the minimum stress intensity factor to the maximum stress intensity factor.

[0093] Safety assessment indicators can be node-level defect propagation thresholds determined based on the stress characteristic values ​​and material parameters of each leading-edge node. These thresholds are used to determine the critical resistance to whether a defect at the leading-edge node will propagate. For example, if the stress intensity factor at the leading-edge node is greater than the node-level defect propagation threshold, the defect at the leading-edge node will propagate; conversely, if the stress intensity factor is less than or equal to the node-level defect propagation threshold, the defect at the node will not propagate.

[0094] The safety assessment result can be a conclusion used to characterize whether a defective region is safe, determined based on the relationship between the stress characteristic value of each leading-edge node and the safety assessment index. For example, the safety factor of each leading-edge node can be determined based on the stress characteristic value of each leading-edge node and the safety assessment index. Based on the relationship between the minimum safety factor among all leading-edge node safety factors and a predetermined value (e.g., 1), if the minimum safety factor is greater than 1, the assessment result is that the defect will not have a risk of propagation, and the defect is safe. If the minimum safety factor is less than or equal to 1, the assessment result is that the defect will not have a risk of propagation, and the defect is dangerous.

[0095] This application processes the contour detection data of the defect region on the component to be evaluated to reconstruct a target defect contour node sequence that reflects the true geometry of the defect. Based on the baseline structural model, the target defect contour node sequence is used to generate leading-edge curves and cutting lines to determine the precise location and boundary of the defect in the model. Mesh elements are configured in the area between the cutting lines, and the mesh elements traversed by the leading-edge curve are replaced with defect elements, thereby establishing a defect structure model that can simulate the geometry of the defect. Furthermore, by solving this defect structure model, the stress intensity factor of each leading-edge node at each analysis step can be obtained, and the stress characteristic value and defect propagation threshold of each leading-edge node can be calculated accordingly. Finally, based on the defect propagation threshold and stress intensity factor range of each leading-edge node, the safety factor of each node can be obtained, and the minimum value is taken as the overall judgment criterion, thereby achieving a fine-grained safety assessment of each node at the defect leading edge.

[0096] According to an embodiment of this application, a target defect contour node sequence is obtained by processing the contour detection data of the defect area on the component to be evaluated; in the reference structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve are generated based on the target defect contour node sequence; multiple mesh elements are configured in the area between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structural model; the defect structural model is analyzed to obtain the stress intensity factor of each leading edge node on the leading edge curve of the defect structural model under each analysis step; based on the stress intensity factor of each leading edge node under each analysis step, the stress characteristic value and safety assessment index of each leading edge node are determined; based on the stress characteristic value and safety assessment index, the safety assessment result is determined. During the evaluation process, the contour detection data of the defect area on the component to be evaluated is processed to obtain the target defect contour node sequence, which preserves the true geometric features of the defect. Based on the target defect contour node sequence, a leading edge curve is generated on the benchmark structural model in a defect-free state. Using the leading edge nodes on the leading edge curve as units, the stress characteristic value and safety assessment index of each leading edge node on the defective structural model are determined, thus realizing node-level evaluation of the defect area and improving the accuracy of safety assessment.

[0097] In some embodiments, the aforementioned reference structural model may be constructed in the following manner: based on the identification information of the component to be evaluated, an initial reference structural model of the component to be evaluated in a defect-free state is obtained; the actual usage conditions of the component to be evaluated are applied to the initial reference structural model and analyzed to obtain the first stress field data of the initial reference structural model; if the first stress field data passes the verification, the initial reference structural model is used as the reference structural model.

[0098] The identification information of the component to be evaluated may include its name, model, etc. Based on this identification information, an initial reference structural model of the component to be evaluated can be obtained from the database. This initial reference structural model can be created by finite element software and then stored in the database.

[0099] For the initial baseline structural model established by finite element software, actual usage conditions can be applied to the components to be evaluated. These actual usage conditions can include assembly relationships, constraints, and load cases. Assembly relationships can include bolted connections, interference or clearance fits, component contact, etc. Constraints can include conventional boundary conditions (such as fixed constraints, symmetric constraints, displacement or rotation constraints, etc.) used to restrict the degrees of freedom of nodes, as well as constraints used to establish motion relationships between nodes (such as tie constraints, coupling constraints, rigid body constraints, etc.) to ensure the correctness of assembly, load transfer, and overall motion of local areas. Among the constraints are temporary constraints used to establish the initial equilibrium state (used only in the temporary analysis step and not involved in the force calculation of the actual working condition analysis step). Load cases can include self-weight, fatigue load, vibration acceleration, assembly preload, etc.

[0100] The initial reference structural model under actual usage conditions can be solved to derive the first stress field data. For example, the solution can be performed for each load case, and the principal stress directions, principal stress magnitudes, stress tensor distributions, and the direction of the maximum principal stress determined based on the principal stress magnitudes can be derived to obtain the first stress field data. Within this first stress field data, the principal stress directions corresponding to the defect regions can be of particular interest to determine the embedding of subsequent defects.

[0101] For the first stress field data, the rationality of the results can be verified. For example, verify whether stress concentration occurs in a reasonable geometric location and whether the peak value is normal; whether the displacement field is continuous near connections, contacts, and constraints without significant jumps; and whether the solution process is stable under various working conditions and whether the results change consistently. The calculated maximum stress should be located in the transition zone of the geometric section, without stress singularities, and should not exceed the fatigue limit. The displacement field at the contact and constraint interfaces should remain continuous without abrupt changes. If the stress concentration occurs in a reasonable geometric location and the peak value is normal; the displacement field is continuous near connections, contacts, and constraints without significant jumps; the solution process is stable under various working conditions, the results change consistently, the calculated maximum stress is located in the transition zone of the geometric section, without stress singularities, and should not exceed the fatigue limit; and the displacement field at the contact and constraint interfaces remains continuous without abrupt changes, then the verification is considered successful. This confirms that the stress and displacement responses of the initial benchmark model are reasonable and can meet the requirements of subsequent defect driving force calculations and safety assessments. The initial benchmark structural model can then be used as the benchmark structural model. If any of the above verifications fails to meet the passing conditions, the initial baseline result model can be reconstructed, the initial baseline structure model can be solved, or the applied actual usage conditions can be adjusted until the verification passes and the baseline structure model is obtained.

[0102] In some embodiments, the process of processing the contour detection data of the defect region on the component to be evaluated in operation S220 based on the direction corresponding to the maximum principal stress in the first stress field data to obtain the target defect contour node sequence may include the following operations: processing the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence; interpolating the initial discrete node sequence to obtain an interpolated contour node sequence, and generating an initial contour based on the interpolated contour node sequence; smoothing the initial contour to obtain a smooth contour; reconstructing the peak and valley regions of the smooth contour to obtain a reconstructed contour; and outputting the target defect contour node sequence based on the reconstructed contour.

[0103] In some embodiments, the process of processing contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence may include the following operations: based on the contour detection data of the defect region, locating the direction of the maximum principal stress at the location of the defect region in the reference structural model; establishing a reference coordinate system with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; placing the contour detection data in the reference coordinate system; projecting the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress to obtain multiple initial discrete nodes; and cleaning and sorting the initial discrete nodes to obtain an initial discrete node sequence.

[0104] Figure 3 A schematic diagram illustrating the projection of contour detection data is shown.

[0105] like Figure 3 As shown, based on the contour detection data, the direction of the maximum principal stress at the location of the defect area can be located in the baseline structural model, and a reference coordinate system can be established with the direction of the maximum principal stress as the first coordinate axis. The first coordinate axis of the reference coordinate system can be z, representing the direction of the maximum principal stress; the second coordinate axis can be x, representing the direction of the defect length; and the third coordinate axis can be y, representing the direction of the defect depth.

[0106] The contour detection data is placed in a reference coordinate system; and the contour detection data placed in the reference coordinate system is projected onto a plane perpendicular to the direction of the maximum principal stress, thereby transforming the three-dimensional defect geometry into a two-dimensional projection shape of the cross section. Multiple initial discrete nodes of the defect in this two-dimensional projection shape of the cross section can then be obtained. , where x is the defect length direction and y is the defect depth direction.

[0107] By numerically cleaning multiple initial discrete nodes to remove non-numerical, null, or outlier values, and sorting them according to the x-direction, the monotonic order of the defect contour in space is ensured, resulting in an initial discrete node sequence. This initial discrete node sequence can serve as the geometric input benchmark for subsequent defect contour smoothing fitting and leading edge node refinement reconstruction.

[0108] In some embodiments, the process of interpolating the initial discrete node sequence obtained by the above operations to obtain an interpolated contour node sequence may include the following operations: determining the defect length range of the initial discrete node sequence based on the second coordinate value of each initial discrete node in the defect length direction; constructing interpolated coordinate values ​​evenly distributed on the second coordinate axis in the defect length direction within the defect length range; and interpolating the initial discrete node sequence using the interpolated coordinate values ​​to obtain the interpolated contour node sequence.

[0109] In some embodiments, the defect length range, i.e., the x-range, of the initial discrete node sequence can be determined based on the x-coordinate value of each initial discrete node in the initial discrete node sequence. Within this x-range, a set of evenly distributed x-direction interpolated coordinate values ​​can be constructed. Then, by using a one-dimensional linear interpolation function, the initial discrete node sequence can be mapped to the interpolation coordinates to obtain the interpolated contour node sequence. Based on this interpolated contour node sequence, a one-dimensional smooth spline function can be constructed. This yields the initial contour.

[0110] For example, the initial discrete node sequence includes (1.0, 2.1), (2.5, 3.8), and (4.0, 5.2). The x-coordinates (1.0, 2.5, 4.0) of these three points are not uniformly distributed in the x-direction. If the constructed interpolated coordinate values ​​are 1.0, 2.0, 3.0, and 4.0, a total of 4 points, linear interpolation can be performed by finding the two adjacent x-coordinates related to each interpolated coordinate value in the initial discrete node sequence, and then calculating the y-value in the defect depth direction corresponding to that interpolated coordinate value through a linear relationship. For example, for the interpolated coordinate x=1, which coincides with 1.0 in (1.0, 2.1), the corresponding y-value is 2.1. For the interpolated coordinate x=2, which lies between (1.0, 2.1) and (2.5, 3.8), linear interpolation using these two points yields y=2.1+(3.8-2.1)×(2.0-1.0) / (2.5-1.0)=2.1+1.7×1.0 / 1.5≈3.23, so the corresponding y-value is 3.23. Similarly, the resulting interpolated contour node sequence is uniformly distributed along the x-direction: (1.0, 2.1), (2.0, 3.23), (3.0, 4.27), (4.0, 5.2). This example is for illustrative purposes only; the specific coordinates and calculation process can be adjusted according to actual needs.

[0111] In some embodiments, the initial contour described above can be smoothed to obtain a smooth contour. Specifically, this is achieved by setting smoothing parameters. The number of sampling points is 0.5 to 3 times the normal number, striking a balance between preserving the overall shape and suppressing local noise. This is achieved in higher resolution horizontal coordinates. The initial contour is evaluated to obtain the smoothed contour. Higher resolution horizontal coordinates can refer to smaller spacing between horizontal coordinates. Based on the linear interpolation example above, the spacing between uniformly distributed interpolated coordinate values ​​is 1, while higher resolution can refer to a spacing of 0.5, such as 1.0, 1.5, 2.0, 2.5, 3.0, 3.5, 4.0, etc. The spacing can also be 0.2 or 0.1, etc., and can be adjusted adaptively according to actual needs.

[0112] A smooth contour can have peak regions and valley regions, where peak regions include peak points and valley regions include valley points. Reconstructing the peak and valley regions of the smooth contour yields a reconstructed contour, including: constructing peak windows and valley windows of predetermined lengths centered on the peak and valley points respectively; extracting data within the peak and valley windows to obtain peak window data and valley window data; inputting the peak and valley window data into a contour reconstruction function to obtain initial reconstructed contours for the peak and valley windows respectively, where the contour reconstruction function is constructed with the peak or valley point as the center of symmetry; fusing the initial reconstructed contours of the peak and valley windows with the original smooth contours within the peak and valley windows respectively to obtain local reconstructed contours for the peak and valley windows; and replacing the original smooth contours within the peak and valley windows based on the local reconstructed contours of the peak and valley windows respectively to obtain the reconstructed contours.

[0113] In some embodiments, the initial discrete node sequence can be... In the process, the peak and trough points of defects are identified. .

[0114] Using the peak point and valley point as the center, select a window node on each side of the peak point or valley point. and This is to form peak and valley windows of predetermined lengths. The distance between the window node and the peak or valley point is Within the respective peak and valley windows, from the smooth contour Extracting partial data This yields peak window data and valley window data.

[0115] Using the peak point or valley point as the center of symmetry, construct a dome or bottom curve in the form of a quadratic function as the contour reconstruction function, as shown in formula (1).

[0116] (1)

[0117] Among them, coefficient The curve is obtained by least squares fitting, making it as close as possible to the original smooth curve within this local interval. x is the coordinate along the defect length direction. The x-coordinate of the peak or valley point. The y-coordinate of the peak or valley point. This represents the initial reconstructed profile of the peak window or the initial reconstructed profile of the valley window.

[0118] By inputting the peak window data and valley window data into the contour reconstruction function respectively, the initial reconstructed contours of the peak window and the valley window can be obtained.

[0119] The initial reconstructed contours of the peak window and the valley window are used to fuse with the original smooth contours within the peak window and the valley window, respectively, to obtain the local reconstructed contours of the peak window and the valley window.

[0120] For example, the original smooth contour within the peak and valley windows. The initial reconstructed profile of the peak window or the initial reconstructed profile of the valley window. By fusing according to the following formula (2), the local reconstructed contour of the peak window or the local reconstructed contour of the valley window can be obtained. .

[0121] (2)

[0122] in To make the interval Linear mapping to dimensionless parameters, It is a proportionality coefficient that varies with the process and is used to control... and In the final result The weights in the equation are: t is the progress parameter, such as the number of iterations or the transition from 0 to 1; S(t) is the weight calculated based on this progress, and its value is usually limited to between 0 and 1. The change in S(t) can be linear or non-linear, but it always remains within the range of 0 to 1, used to determine the final result. More biased towards local results Or is it more about the overall result? The purpose of this setting is to ensure that the calculation results transition smoothly as the process progresses, avoiding abrupt changes or instability in the contour curve.

[0123] Reconstructed contours using peak windows or localized contours using valley windows Replace the original smooth contours within the peak and valley windows. This yields a final defect reconstruction profile that is continuous overall and dome-shaped locally. .

[0124] In some embodiments, the reconstructed contour further includes a smooth region, which together with the peak and valley regions constitutes the reconstructed contour. The process of outputting the target defect contour node sequence based on the reconstructed contour may include the following operations: determining the total number of nodes to be output based on the contour length of the reconstructed contour and a preset node spacing; for each of the smooth, peak, and valley regions: determining the number of nodes in the region based on the total number of nodes to be output and the preset weight of the region; within the region, determining encrypted nodes based on the number of nodes in the region and the nodes at the region's endpoints; constructing a node set for the region based on the encrypted nodes in the region and the nodes at the region's endpoints; and processing the node sets of the smooth, peak, and valley regions to obtain the target defect contour node sequence.

[0125] In some embodiments, the resulting final defect reconstructed contour can be obtained. Output the discrete nodes as a table file. The discrete nodes output here are only to reflect the shape of the defect contour and are not the target defect contour node sequence used to generate the leading edge curve. The target defect contour node sequence used to generate the leading edge region can be obtained based on the following formulas (3) to (6).

[0126] For example, the total number of nodes to be output can be determined based on the contour length of the reconstructed contour and the preset node spacing. If the arc length of the defect fitting curve is L (in mm), and the target node spacing is... (Take 0.5–2.5 mm), then the total number of nodes It can be determined according to formula (3):

[0127] (3)

[0128] For each region in the flat, peak, and trough regions:

[0129] First, determine the node allocation. For example, determine the weight w for the smooth region (0.8~1.2), the weight w for the peak and valley regions (1.7~2.3), and the theoretical number of nodes for each of the smooth, peak, and valley regions. As shown in formula (4):

[0130] (4)

[0131] Where i is the index, used to represent the i-th region.

[0132] Within each of the flat, peak, and valley regions, encrypted nodes within the region can be determined based on the number of nodes in the region and the nodes at the region's endpoints.

[0133] Within each region, encrypted nodes are selected at equal intervals according to their horizontal coordinates:

[0134] (5)

[0135] in, and These are contour nodes representing the endpoints of a region, such as the contour nodes at the region's start and end positions. The index represents the k-th contour node selected at equal intervals. The coordinates of the encrypted node in the x-direction.

[0136] The coordinates of the encrypted node in the y-direction are determined by the fitted curve. The calculation is shown in formula (6):

[0137] (6)

[0138] For any of the flat, peak, and valley regions, a set of contour nodes for that region can be constructed based on the existing nodes (including nodes at the region's endpoints) and the encrypted nodes within that region.

[0139] By merging, deduplicating, and sorting the contour node sets within each of the flat, peak, and valley regions according to their coordinate values ​​along the x-axis, the target defect contour node sequence can be obtained.

[0140] Figure 4 A schematic diagram illustrating a target defect contour node sequence according to an embodiment of this application is shown. Figure 5 A schematic diagram of a target defect contour node sequence is shown according to another embodiment of this application.

[0141] like Figure 4 and Figure 5 As shown, the horizontal axis represents the defect length (x-axis), and the vertical axis represents the defect depth (y-axis). Figure 4 and Figure 5 All of these show contour detection data, contour nodes in the target defect contour node sequence, and contour curves fitted based on the target defect contour node sequence. Figure 4 It is the target defect contour node sequence of a single-peak defect. Figure 5 It is the target defect contour node sequence of a bimodal defect.

[0142] In some embodiments, in a reference structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve can be generated based on the target defect contour node sequence obtained by the above operations. Specifically, the process may include the following operations: in the reference structural model, in a plane perpendicular to the direction of the maximum principal stress, a leading edge curve is generated according to the target defect contour node sequence; cutting lines are generated on both sides of the leading edge curve at predetermined distances, with the leading edge curve as the center.

[0143] In some embodiments, discrete point coordinates can be obtained from the target defect contour node sequence. .

[0144] Based on the coordinates of the discrete point A continuous, smooth leading edge curve is generated in a plane perpendicular to the direction of the maximum principal stress at the defect. This curve serves as the geometric boundary of the actual defect and is used as a reference for subsequent geometric cutting.

[0145] Using the leading edge curve as the center, parallel cutting lines are generated on both sides of the leading edge center by a predetermined distance (e.g., 0.5~2 mm), and geometric cutting is completed on the plane where the defect is located accordingly, forming a pair of double boundary cutting lines corresponding to the leading edge curve.

[0146] Multiple mesh elements can be configured between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structure model. Specifically, this process may include the following operations: configuring multiple mesh elements on a reference structure model, wherein, in the region between the cutting lines, the number of mesh elements in the defect length direction is odd, and the number of nodes in the mesh elements in the defect depth direction is greater than or equal to the total number of contour nodes; verifying the reference structure model configured with mesh elements; if the verification passes, replacing the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structure model.

[0147] Structured quadrilateral elements are arranged in a plane between the two formed parallel cutting lines. The number of elements along the width direction between the two parallel cutting lines is set to an odd number. An odd number ensures that the center position between the cutting lines is within the mesh rather than at the mesh boundary. This allows the leading edge node of the leading edge curve to precisely correspond to the center position of a row of quadrilateral elements between the two parallel cutting lines. That is, the leading edge curve can pass through the mesh elements, but does not coincide with the mesh element boundary. This facilitates subsequent replacement of the mesh elements passed through by the leading edge curve, ensuring that the leading edge node of the leading edge curve coincides with the defect contour constructed in the aforementioned operation (e.g., ...). Figure 4 and Figure 5 (The contour curve based on the target defect contour node sequence fitting).

[0148] The number of nodes along the longitudinal direction of the defect within the area between two parallel cutting lines. Need to meet .

[0149] In the baseline structural model, quadrilateral elements can also be arranged in the remaining area between the two parallel cutting lines. For the quadrilateral elements between the two parallel cutting lines, the quadrilateral elements can be used as a base and extended to both sides to form corresponding hexahedral elements by stretching, sweeping or volume mapping along the thickness direction, so as to form hexahedral elements with a consistent topology in the area between the two parallel cutting lines.

[0150] For a reference structural model configured with mesh elements, verification can be performed. For example, the actual usage conditions of the component to be evaluated are applied to the reference structural model configured with mesh elements and analyzed to obtain the second stress field data of the reference structural model under the condition of mesh element configuration; based on the error between the second stress field data and the first stress field data, the reference structural model configured with mesh elements is verified.

[0151] After forming a structured hexahedral mesh element, the actual usage conditions of the component to be evaluated can be applied to the reference structural model configured with the mesh element. For example, the same assembly relationships, constraints, and load conditions as when constructing the reference result model can be applied, and a defect-free solution can be submitted to obtain the second stress field data. If the error between the second stress field data and the first stress field data is ≤3%, the verification can be considered passed, and the quality of the mesh element, the constraint relationship, and the load transfer are reasonable.

[0152] If the baseline structural model configured with mesh elements passes verification, mesh elements whose leading-edge curves pass through can be replaced with defective elements to obtain a defective structural model. For example, using 3D crack propagation behavior analysis software, an element replacement operation can be performed on the mesh elements whose leading-edge curves pass through, replacing the element with a crack-specific element. After replacement, loop hexahedral elements are automatically generated, resulting in a defective structural model.

[0153] Figure 6 The diagram illustrates a construction defect structure model according to an embodiment of this application. Figure 7 A schematic diagram illustrating the construction of a defect structure model according to another embodiment of this application is shown.

[0154] like Figure 6 and Figure 7 As shown, Figure 6 and Figure 7 The difference is Figure 6 It is a single-peak defect. Figure 7 It is a bimodal defect. Figure 6 For example, Figure 6(a) shows the contour nodes in the target defect contour node sequence, the leading edge curve formed by fitting the target defect contour node sequence, and the geometric cutting lines constructed on both sides of the leading edge curve. Figure 6 (b) shows that based on Figure 6 (a) shows the structured quadrilateral elements arranged with cutting lines, and the hexahedral elements formed by their extension in the thickness direction. Figure 6 (c) will Figure 6 In (b), the element crossed by the leading edge curve is replaced with a crack-specific element. The crack-specific element can be composed of wedge elements and hexahedral elements. Figure 6 Except for the two wedge-shaped elements marked in (c), all other elements are hexahedral. Figure 6 (c) also shows the leading edge node on the leading edge curve for subsequent safety assessment.

[0155] The difference between profile nodes and leading edge nodes is that profile nodes are geometrically generated points, while leading edge nodes are nodes of finite element units. Profile points are used to determine the shape of the leading edge, cutting planes to form hexahedral elements (e.g., 8 nodes per mesh element). In some areas, the spacing between profile points is large, resulting in poor element quality, which leads to the addition of leading edge nodes. Leading edge nodes are always present at the location of a profile node. Leading edge nodes are added in the middle of certain profile points based on their arrangement, but the number of leading edge nodes exceeds the number of profile points.

[0156] For this defective structural model, analysis can be performed to obtain the stress intensity factor of each leading node on the leading curve of the defective structural model at each analysis step during the analysis process. This process may include the following operations: applying the actual usage conditions of the component to be evaluated to the defective structural model, and analyzing the defective structural model to obtain the stress field, strain energy density, and displacement field distribution of each leading node on the leading curve of the defective structural model at each analysis step during the analysis process; based on the stress field, strain energy density, and displacement field distribution of each leading node at each analysis step, obtaining the stress intensity factor of each leading node at each analysis step. The calculation process of the stress intensity factor can be shown in formulas (7) to (8).

[0157] The stress intensity factor K can be obtained by solving the J-integral based on the plane strain condition at each leading edge node. In the three-dimensional structure, due to the local high constraint, the stress field at the leading edge node approximately satisfies the plane strain assumption. At this time, the J-integral and the stress intensity factor satisfy formula (7):

[0158] (7)

[0159] Where E is Young's modulus. The ratio is Poisson's ratio, typically 0.3 for metals. The J-integral is calculated using a domain integral form, that is, within the integration domain surrounding the defect front, it utilizes the energy density tensor composed of the stress field σ, displacement gradient ▽u, and strain energy density W obtained from the stress-strain relationship, along with the gradient of the virtual crack propagation weighting function. The energy release rate during virtual crack propagation (equal to J integral) is obtained by performing a volume integral, as shown in formula (8):

[0160] (8)

[0161] Where A is the integral domain surrounding the defect leading edge (a three-dimensional domain composed of several unit rings). The weight function for the virtual crack propagation direction (1 near the defect tip and 0 at the outer boundary). It is a unit tensor used to express the strain energy density W in tensor form WI.

[0162] In some embodiments, by submitting a defect structure model for solution, the stress, strain, and displacement field distributions, including the crack region, are obtained. The singular elements at the crack tip (i.e., crack-specific elements) can accurately capture stress singularities, providing high-precision input for fracture mechanics analysis. By extracting the solution result file, the coordinates of each node at the defect tip and the output values ​​of the stress intensity factor K corresponding to each analysis step can be obtained. The result file can be as follows: Figure 8 As shown.

[0163] Figure 8 A schematic diagram of the resulting document according to an embodiment of this application is shown.

[0164] like Figure 8As shown, the results file can include the model node number of the defect leading edge node (i.e., the number of the leading edge node among all nodes in the defect structure model), the defect number, the self-number of the defect leading edge node, the analysis step, the x-coordinate value, y-coordinate value, z-coordinate value, Young's modulus, Poisson's ratio, J-integral value, and strength factor K of the leading edge node. The normalized distance can be obtained by dividing the arc length coordinate of each leading edge node of the defect, using the leading edge starting point as a reference, by the total arc length of the defect leading edge, resulting in dimensionless data between 0 and 1. Each analysis step can correspond to each working condition. Taking the axle box as an example, these 9 working conditions can correspond to: Working Condition 1: Vertical-Roll-Sinking-Twist. Working Condition 2: Vertical-Roll-Sinking-Twist + Lateral + Longitudinal - Damper Vertical. Working Condition 3: Vertical-Roll-Sinking-Twist + Lateral - Longitudinal - Damper Vertical. Working Condition 4: Vertical-Roll-Sinking-Twist - Lateral + Longitudinal - Damper Vertical. Operating Condition 5: Vertical - Roll - Float - Track Twist - Lateral - Longitudinal - Damper Vertical. Operating Condition 6: Vertical + Roll + Float + Track Twist + Lateral + Longitudinal + Damper Vertical. Operating Condition 7: Vertical + Roll + Float + Track Twist + Lateral - Longitudinal + Damper Vertical. Operating Condition 8: Vertical + Roll + Float + Track Twist - Lateral + Longitudinal + Damper Vertical. Operating Condition 9: Vertical + Roll + Float + Track Twist - Lateral - Longitudinal + Damper Vertical. Where "-" indicates subtraction and "+" indicates addition.

[0165] In some embodiments, based on the stress intensity factor of each leading edge node obtained from the above operations at each analysis step, the stress characteristic value and safety assessment index of each leading edge node can be determined. This process may include the following operations: For each leading edge node: extracting the maximum and minimum stress intensity factors of the leading edge node from the stress intensity factors of the leading edge node at each analysis step; determining the stress intensity factor range and stress ratio of the leading edge node based on the maximum and minimum stress intensity factors; obtaining the stress characteristic value based on the maximum stress intensity factor, minimum stress intensity factor, stress intensity factor range, and stress ratio; and obtaining the safety assessment index based on the stress ratio and multiple assessment parameters.

[0166] Before analyzing the stress intensity factor of each leading node in each analysis step, the data from the temporary analysis step used for stability calculation can be filtered out, retaining only the data from the actual load case analysis step. The temporary analysis step establishes stable assembly relationships and initial constraint systems in the finite element model, applying auxiliary constraints to bring the model to a computable initial equilibrium state. The constraints in this step are only used for model initialization and do not participate in structural stress calculations after entering the actual load case analysis step. The actual load case analysis step retains only the actual assembly relationships and boundary conditions of the structure and applies actual loads to obtain the stress field and defect leading-edge fracture parameters of the structure under actual operating conditions.

[0167] For the filtered stress intensity factor, the number of defect leading edge nodes and the number of analysis steps can be counted, and a leading edge node number matrix and an analysis step matrix can be generated to prepare for subsequent group calculations; the stress intensity factor values ​​of all working conditions of the leading edge node i can be summarized according to the node by using the leading edge node number i as the grouping basis.

[0168] For each leading edge node i, the maximum stress intensity factor of the leading edge node under all working conditions is extracted according to formula (9). and minimum stress intensity factor :

[0169] (9)

[0170] The range of stress intensity factor for the leading edge node is determined according to formula (10). And the stress ratio is determined according to formula (11). :

[0171] (10)

[0172] (11)

[0173] Figure 9 A schematic diagram illustrating stress characteristic values ​​according to an embodiment of this application is shown.

[0174] K of each leading edge node max,i K min,i ΔK i R i By combining these values, a statistical table of stress characteristic values ​​can be formed, such as... Figure 9 As shown, these stress eigenvalues ​​can constitute the crack driving force. Figure 9 The automatic extraction and data aggregation results of the mechanical driving force characteristic parameters of each node at the defect leading edge are presented.

[0175] Based on the stress ratio in the stress characteristic value and multiple evaluation parameters, a safety assessment index can be constructed. Specifically, the process may include the following operations: For each leading-edge node: Based on the material properties corresponding to the leading-edge node, query the benchmark fatigue crack propagation threshold value from the standard file; Based on the stress ratio of the leading-edge node and the benchmark fatigue crack propagation threshold value, determine the target fatigue crack propagation threshold value of the leading-edge node; Based on the target fatigue crack propagation threshold value, tensile strength, and stress ratio, determine the material characteristic crack length corresponding to the leading-edge node; Based on the defect characteristic size of the leading-edge node, the target fatigue crack propagation threshold value, and the material characteristic crack length, obtain the node-level defect propagation threshold of the leading-edge node, which serves as the safety assessment index. The defect characteristic size of the leading-edge node is determined according to the defect type of the defect region.

[0176] In some embodiments, a baseline fatigue crack propagation threshold value can be queried from a standard file based on the material properties corresponding to the leading edge node. For example, the baseline fatigue crack propagation threshold value when the stress ratio is 0. According to BS 7910 standard, the steel base material is 170. 63 steel welded joint According to EN 1999-1-3 standard, aluminum alloys are 32... .

[0177] Based on the stress ratio at the leading-edge node and the baseline fatigue crack propagation threshold, the target fatigue crack propagation threshold value for the leading-edge node is determined. The process is shown in formula (12).

[0178] (12)

[0179] Where R is the stress ratio, which can be obtained by substituting it into formula (11), and γ is 0.5~1.0.

[0180] The determination of the material characteristic crack length a0 is a key parameter for assessing the defect propagation trend. This parameter describes the characteristic scale of the transition from short crack behavior to long crack propagation behavior in fatigue cracks. The process of determining the material characteristic crack length corresponding to the leading edge node based on the target fatigue crack propagation threshold, tensile strength, and stress ratio can be shown in formula (13).

[0181] (13)

[0182] in, Tensile strength can be determined based on the material's tensile test data or relevant standards. To ensure conservatism, the tensile test results... The statistical lower limit (such as the mean minus two standard deviations) or the minimum tensile strength value specified in the standard can be used; For the coefficient, according to BS17149 standard, 0.75 is used for rolled or forged steel, 0.57 for cast steel and cast iron, and 0.6 for aluminum alloys. R is the stress ratio, which can be obtained by substituting into formula (11). The advantage of this calculation process is that... It can be calculated directly using a small number of readily available material parameters, without the need for complex experiments.

[0183] The defect propagation threshold is a critical condition for the propagation of defects in the short crack stage, which is common in engineering structures. The fatigue propagation threshold value of the short crack is defined as the defect propagation threshold. The process of obtaining the node-level defect propagation threshold of the leading-edge node based on the defect characteristic size of the leading-edge node, the target fatigue crack propagation threshold value, and the characteristic crack length of the material can be determined by formula (14).

[0184] (14)

[0185] Among them, the defect feature size The definition is determined according to the defect type (internal defect or surface defect) and is used to characterize the geometric dimensions of the defect leading edge node relative to the defect feature center point.

[0186] Figure 10A This schematic diagram illustrates the determination of defect feature size according to an embodiment of this application. Figure 10B A schematic diagram illustrating the determination of defect feature size according to another embodiment of this application is shown.

[0187] like Figure 10A As shown, for internal defects, the defect feature size Defined as the distance from the leading edge node of the defect to the geometric center of the planar region containing the defect, it accurately reflects the relative position of the internal defect nodes in the defect depth direction and characterizes the size of the defect in that local region. The geometric center (or centroid) is calculated from the coordinates of the discrete nodes constituting the planar region.

[0188] like Figure 10B As shown, for surface defects, the defect feature size Defined as the distance from the leading edge node of the defect to the midpoint of the line connecting the two surface nodes of the defect boundary, this distance reflects the size and extent of the defect's inward expansion within a local region.

[0189] Based on each leading edge node i, we can query... Combined with stress ratio Substituting into formula (12), we get Substituting this into formula (13) again, we obtain the characteristic crack length at the node level. Then, the defect feature size of the node is... With the leading edge node and Substituting all the values ​​into formula (14), we obtain the node-level defect propagation threshold. . This is a general form given for the overall defect morphology. This refers to the specific calculation form for the i-th leading edge node. It represents expressions for different scenarios; although the forms differ, the calculated values ​​are all obtained through... get.

[0190] in, The nodal stress ratio of defect-leading node i; The nodal-level fatigue crack propagation threshold value determined by the stress ratio of the leading-edge node i; Material characteristic crack length at node i; The node-level defect feature size of leading edge node i; The node-level defect propagation threshold of leading edge node i is the critical resistance used to determine whether a defect at that node will propagate.

[0191] Figure 11 A schematic diagram illustrates a three-dimensional example of how the defect propagation threshold varies with the defect feature size and stress ratio according to an embodiment of this application.

[0192] Figure 11 This is a three-dimensional example diagram illustrating the variation of the defect propagation threshold with the defect feature size and stress ratio at each leading edge node of the defect in an embodiment of the present invention. It demonstrates the three-dimensional response surface and evolution law between the defect propagation threshold and the defect feature size and stress ratio. Figure 11 As shown, through the above-described mapping process for each leading edge node, the stress ratio and defect propagation threshold can be determined. The unit is The unified representation of the defect feature size (a, in mm) at the nodal scale enables the expansion criteria of each node at the defect leading edge to be evaluated within the same fracture mechanics framework.

[0193] In some embodiments, a safety assessment result can be determined based on the stress characteristic values ​​and safety assessment indices obtained from the above operations. This process may include the following operations: obtaining a safety factor for each leading-edge node based on the ratio of the node-level defect propagation threshold to the stress intensity factor range; extracting the minimum safety factor from the safety factors of each leading-edge node to obtain a target safety factor; obtaining an assessment result indicating the safety of the defect region if the target safety factor is greater than a predetermined value; and obtaining an assessment result indicating the danger of the defect region if the target safety factor is less than or equal to a predetermined value.

[0194] Based on the node-level defect propagation threshold of each leading edge node With stress intensity factor range The process of obtaining the safety factor of each leading edge node by the ratio of the two values ​​is shown in formula (15).

[0195] (15)

[0196] Output the model node numbers of all leading edge nodes and their corresponding K values. max,i K min,i ΔK i , ΔK th,R,i and S f,i .

[0197] The minimum safety factor is extracted from the safety factors of each leading edge node to obtain the target safety factor. The process is shown in formula (16).

[0198] (16)

[0199] If the target safety factor is greater than a predetermined value (e.g., 1), the defect is determined to have no risk of expansion and is considered safe, thus obtaining an assessment result indicating that the defect area is safe.

[0200] If the target safety factor is less than or equal to a predetermined value (e.g., 1), it indicates that the defect has a risk of expansion, and the defect is judged as dangerous, resulting in an assessment result representing the danger of the defect area. Simultaneously, all conditions that meet the following criteria are identified. The nodes are identified, their node numbers are output, and the defect is located in the hazardous area under multiple operating conditions, such as... Figure 12 As shown.

[0201] Figure 12 A schematic diagram illustrating the security assessment results according to an embodiment of this application is shown.

[0202] like Figure 12 As shown, Figure 12 This is a three-dimensional scatter plot of the safety assessment results of defect-leading nodes in an embodiment of the present invention. The scatter plot uses defect feature size, stress ratio, and safety factor as coordinate axes to visually display the safety margin distribution of each node at the defect-leading edge. A horizontal reference plane (blue semi-transparent plane) representing a critical safety state (safety factor of 1) is introduced in the figure: blue circles represent nodes with a safety factor greater than 1, indicating a safe state; red triangles represent dangerous nodes with a safety factor less than or equal to 1. Furthermore, the label box in the upper right corner of the figure clearly lists the model node numbers of dangerous leading-edge nodes that do not meet the safety criteria (e.g., 57661, 58217, 58773, 59329, 59885), enabling precise location and quantitative safety determination of weak areas and critical dangerous nodes at the defect-leading edge of structural metal components.

[0203] Figure 13 A flowchart illustrating a method for assessing the safety of component defects according to another embodiment of this application is shown schematically.

[0204] like Figure 13 As shown, the method for assessing the safety of component defects in this embodiment may include operations S1310 to S1360.

[0205] In operation S1301, a benchmark structural model is constructed and solved to obtain the first stress field data.

[0206] In operation S1320, a sequence of target defect contour nodes is generated based on the contour detection data.

[0207] In operation S1330, based on the target defect contour node sequence, mesh reconstruction and crack element embedding are performed on the baseline structural model to obtain the defect structural model.

[0208] In operation S1340, the stress characteristic value is calculated.

[0209] Calculation of safety assessment indicators during operation of S1350.

[0210] In operation S1360, determine the results of the security assessment.

[0211] The core of this application lies in establishing an evaluation method based on the crack driving force at the defect contour leading edge node level and the defect propagation threshold at the node level, enabling a unified evaluation of the fatigue propagation risk of defects under complex and diverse loading conditions. Without altering this core technical concept, the same evaluation objective can be achieved through different numerical implementation methods or data processing workflows. For example, different leading edge discretization methods, different stress intensity factor extraction strategies, different material threshold parameter determination methods, or different automated scripts can be used to calculate the node-level threshold and output the safety factor. However, these alternative solutions are merely differences in implementation paths or engineering details and do not affect the node-level judgment framework proposed in this application itself. Regardless of the implementation method, it is essential to rely on the node-level crack driving force and node-level defect propagation threshold constructed in this application to achieve a comprehensive evaluation of defect leading edge non-uniformity, stress ratio effect, and defect size effect. Therefore, while maintaining the technical concept of this application, there are multiple alternative implementation methods, but their technical effects all depend on the node-level threshold judgment mechanism proposed in this application. The method provided in this application can quantitatively determine whether a defect has the potential for fatigue crack propagation under complex and diverse working conditions and provide a remaining safety margin.

[0212] This application establishes an evaluation method based on discrete nodes at the defect leading edge, comparing the crack driving force at the node level with the defect propagation threshold at the node level. This method enables unified determination of defect propagation under different service conditions and has the following technical advantages:

[0213] This application reconstructs the defect profile based on actual measurement data, and achieves a refined expression of complex defect morphology by extracting peaks, valleys, and key geometric features. This method avoids the loss of detailed information caused by the excessive simplification of defect regularization in existing technologies, enabling the reconstructed defect profile to accurately reflect local geometric changes. The finite element model established using this profile can more accurately capture the local stress field characteristics at the leading edge and the corresponding extended driving force distribution, improving the accuracy of fracture mechanics assessment.

[0214] This application takes each node of the defect leading edge discretized as the object, and extracts the extreme values ​​of stress intensity factors and local stress ratios at the node level through finite element analysis to obtain the driving force for fatigue crack propagation at the node level. This node-by-node approach can truly reflect the non-uniformity of the defect leading edge, identify the danger point where propagation first occurs, and achieve a refined assessment of the defect leading edge, significantly improving the accuracy and engineering applicability of the assessment.

[0215] This application constructs an engineering-compliant and easily applicable process for determining the defect propagation threshold. This process takes discrete leading-edge nodes as the object, considering the stress ratio, material characteristic crack length, and defect characteristic size of each leading-edge node. Based on the fatigue crack propagation threshold, it forms a node-level defect propagation threshold. All parameters required for this process can be easily obtained through conventional material testing or existing standards, without relying on highly specialized and complex short-crack tests. Furthermore, it can obtain the node-level driving force extreme value set within the service condition space, and complete the node-level threshold calculation, node-level safety factor output, and statistical determination through automated data processing scripts, forming an engineering-implementable evaluation process.

[0216] This application proposes a unified defect assessment method covering complex and diverse service conditions. By mapping the extreme values ​​of stress intensity factors at each node under various service conditions to the driving force of defect propagation (stress intensity factor range), and mapping parameters such as stress ratio and defect feature size to node-level defect propagation thresholds, the propagation trends of each defect leading edge node under different service conditions can be compared and judged within the same physical system. This method can provide a consistent and systematic assessment of defect propagation risk throughout the entire service life.

[0217] Based on the above-described method for assessing the safety of component defects, this application also provides a system for assessing the safety of component defects. The following will be combined with... Figure 14 The system is described in detail.

[0218] Figure 14 A schematic diagram illustrates a structural block diagram of a system for assessing the safety of component defects according to an embodiment of this application.

[0219] like Figure 14 As shown, the system 1400 for evaluating the safety of component defects in this embodiment includes a processing module 1410, a generation module 1420, a configuration module 1430, an analysis module 1440, a first determination module 1450, and a second determination module 1460.

[0220] The processing module 1410 is used to process the contour detection data of the defect area on the component to be evaluated to obtain the target defect contour node sequence.

[0221] The generation module 1420 is used to generate a leading edge curve and cutting lines on both sides of the leading edge curve in the reference structural model based on the defect contour node sequence. The leading edge curve is used to represent the boundary of the defect region on the reference structural model, which is constructed by the component to be evaluated in a defect-free state.

[0222] Configuration module 1430 is used to configure multiple mesh elements in the area between cutting lines, and replace the mesh elements through which the leading edge curve passes with defect elements to obtain a defect structure model.

[0223] Analysis module 1440 is used to analyze the defective structure model and obtain the stress intensity factor of each leading node on the leading edge curve of the defective structure model at each analysis step during the analysis process.

[0224] The first determination module 1450 is used to determine the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node in each analysis step.

[0225] The second determining module 1460 is used to determine the safety assessment result based on the stress characteristic value and the safety assessment index.

[0226] In some embodiments, the system 1400 for assessing the safety of component defects may further include an acquisition module, an application module, and a verification module.

[0227] The acquisition module is used to acquire the initial baseline structural model of the component to be evaluated in a defect-free state based on the identification information of the component to be evaluated.

[0228] The application module is used to apply the actual usage conditions of the component to be evaluated to the initial reference structural model and perform analysis to obtain the first stress field data of the initial reference structural model.

[0229] The verification module is used to use the initial reference structural model as the reference structural model if the first stress field data passes the verification.

[0230] In some embodiments, the first stress field data includes the direction of the maximum principal stress, and the processing module 1410 may include a first processing submodule, an interpolation submodule, a second processing submodule, a reconstruction submodule, and an output submodule.

[0231] The first processing submodule is used to process the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence.

[0232] The interpolation submodule is used to interpolate the initial discrete node sequence to obtain the interpolated contour node sequence, and to generate the initial contour based on the interpolated contour node sequence.

[0233] The second processing submodule is used to smooth the initial contour to obtain a smooth contour.

[0234] The reconstruction submodule is used to reconstruct the peak and valley regions of the smooth contour to obtain the reconstructed contour.

[0235] The output submodule is used to output the target defect contour node sequence based on the reconstructed contour.

[0236] In some embodiments, the first processing submodule may include a positioning unit, an establishment unit, a first processing unit, a projection unit, and a second processing unit.

[0237] The positioning unit is used to locate the direction of the maximum principal stress in the defect area in the reference structural model based on the contour detection data of the defect area.

[0238] A unit is established to create a reference coordinate system with the direction of the maximum principal stress at the location of the defect area as the first coordinate axis.

[0239] The first processing unit is used to place the contour detection data in the reference coordinate system.

[0240] The projection element is used to project the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress, thus obtaining multiple initial discrete nodes.

[0241] The second processing unit is used to clean and sort the initial discrete nodes to obtain the initial discrete node sequence.

[0242] In some embodiments, the reference coordinate system further includes a second coordinate axis representing the defect length direction and a third coordinate axis representing the defect depth direction, and each initial discrete node in the initial discrete node sequence has a second coordinate value in the defect length direction and a third coordinate value in the defect depth direction. The interpolation submodule may include a first determining unit, a constructing unit, and an interpolation unit.

[0243] The first determining unit is used to determine the defect length range of the initial discrete node sequence based on the second coordinate value of each initial discrete node in the defect length direction.

[0244] The construction unit is used to construct interpolated coordinate values ​​that are evenly distributed on the second coordinate axis in the direction of the defect length within the defect length range.

[0245] The interpolation unit is used to interpolate the initial discrete node sequence using interpolated coordinate values ​​to obtain the interpolated contour node sequence.

[0246] In some embodiments, the peak region includes peak points, the valley region includes valley points, and the reconstruction submodule may include a construction unit, a truncation unit, an input unit, a fusion unit, and a replacement unit.

[0247] The building unit is used to construct peak windows and valley windows of predetermined lengths, centered on peak points and valley points respectively.

[0248] The interception unit is used to intercept the data within the peak window and the valley window to obtain the peak window data and the valley window data.

[0249] The input unit is used to input the peak window data and valley window data into the contour reconstruction function respectively to obtain the initial reconstructed contour of the peak window and the initial reconstructed contour of the valley window. The contour reconstruction function is constructed with the peak point or valley point as the center of symmetry.

[0250] The fusion unit is used to fuse the initial reconstructed contours of the peak window and the initial reconstructed contours of the valley window with the original smooth contours within the peak window and the valley window, respectively, to obtain the local reconstructed contours of the peak window and the local reconstructed contours of the valley window.

[0251] The replacement unit is used to replace the original smooth contours within the peak window and the valley window respectively, based on the local reconstructed contours of the peak window and the valley window, to obtain the reconstructed contours.

[0252] In some embodiments, the reconstructed contour further includes a smooth region, which, together with the peak and valley regions, constitutes the reconstructed contour. The output submodule may include a second determining unit, a third determining unit, a fourth determining unit, and a third processing unit.

[0253] The second determining unit is used to determine the total number of contour nodes to be output based on the contour length of the reconstructed contour and the preset node spacing.

[0254] For each region in the flat, peak, and trough regions:

[0255] The third determining unit is used to determine the number of nodes in a region based on the total number of contour nodes to be output and the preset weight of the region.

[0256] The fourth determining unit is used to determine the encrypted nodes within the region based on the number of nodes in the region and the nodes at the endpoints of the region, and to construct a node set.

[0257] The third processing unit is used to process the node sets of flat areas, peak areas, and valley areas to obtain the target defect contour node sequence.

[0258] In some embodiments, the generation module 1420 may include a first generation submodule and a second generation submodule.

[0259] The first generation submodule is used to generate a leading edge curve in the reference structural model, in a plane perpendicular to the direction of the maximum principal stress, based on the target defect profile node sequence.

[0260] The second generation submodule is used to generate cutting lines by offsetting a predetermined distance on both sides of the leading edge curve, with the leading edge curve as the center.

[0261] In some embodiments, the configuration module 1430 may include a configuration submodule, a verification submodule, and a first determination submodule.

[0262] The configuration submodule is used to configure multiple mesh cells between cutting lines, wherein the number of mesh cells in the region between cutting lines is odd in the defect length direction, and the number of nodes of the mesh cells in the defect depth direction is greater than or equal to the total number of contour nodes.

[0263] The verification submodule is used to verify the baseline structural model configured with mesh cells.

[0264] The first determination submodule is used to replace the grid cells through which the leading edge curve passes in multiple grid cells with defect cells, and obtain the defect structure model, if the verification passes.

[0265] In some embodiments, the verification submodule may include an analysis unit and a verification unit.

[0266] The analysis unit is used to apply the actual usage conditions of the component to be evaluated to the reference structural model configured with mesh elements and perform analysis to obtain the second stress field data of the reference structural model under the condition of configuring mesh elements.

[0267] The verification unit is used to verify the reference structural model configured with mesh elements based on the error between the second stress field data and the first stress field data.

[0268] In some embodiments, the analysis module 1440 may include an application submodule and a second determination submodule.

[0269] The application submodule is used to apply the actual usage conditions of the component to be evaluated to the defective structural model and analyze the defective structural model to obtain the stress field, strain energy density and displacement field distribution of each leading node on the leading edge curve of the defective structural model in each analysis step during the analysis process.

[0270] The second determination submodule is used to obtain the stress intensity factor of each leading edge node in each analysis step based on the stress field, strain energy density and displacement field distribution of each leading edge node in each analysis step.

[0271] In some embodiments, the first determining module 1450 may include an extraction submodule, a third determining submodule, a fourth determining submodule, and a fifth determining submodule.

[0272] For each leading edge node:

[0273] The extraction submodule is used to extract the maximum and minimum stress intensity factors of the leading edge node from the stress intensity factors of the leading edge node in each analysis step.

[0274] The third determination submodule is used to determine the stress intensity factor range and stress ratio of the leading edge node based on the maximum and minimum stress intensity factors.

[0275] The fourth determination submodule is used to obtain stress characteristic values ​​based on the maximum stress intensity factor, minimum stress intensity factor, stress intensity factor range, and stress ratio.

[0276] The fifth determination submodule is used to obtain safety assessment indicators based on the stress ratio and multiple assessment parameters.

[0277] In some embodiments, the fifth determining submodule may include a query unit, a fifth determining unit, a sixth determining unit, and a seventh determining unit.

[0278] For each leading edge node:

[0279] The query unit is used to query the baseline fatigue crack propagation threshold value from the standard file based on the material properties corresponding to the leading edge node.

[0280] The fifth determining unit is used to determine the target fatigue crack propagation threshold value of the leading edge node based on the stress ratio of the leading edge node and the reference fatigue crack propagation threshold value.

[0281] The sixth determining unit is used to determine the length of the material characteristic crack corresponding to the leading edge node based on the target fatigue crack propagation threshold value, tensile strength, and stress ratio.

[0282] The seventh determining unit is used to obtain the node-level defect propagation threshold of the leading-edge node based on the defect feature size of the leading-edge node, the target fatigue crack propagation threshold value, and the material feature crack length, which serves as a safety assessment index. The defect feature size of the leading-edge node is determined according to the defect type of the defect region.

[0283] In some embodiments, the second determining module 1460 may include a sixth determining submodule, a seventh determining submodule, a first result submodule, and a second result submodule.

[0284] The sixth determination submodule is used to obtain the safety factor of each leading edge node based on the ratio of the node-level defect propagation threshold to the stress intensity factor range of each leading edge node.

[0285] The seventh determination submodule is used to extract the minimum value of the safety factor from the safety factors of each leading edge node to obtain the target safety factor.

[0286] The first result submodule is used to obtain an assessment result indicating the safety of the defective area when the target safety factor is greater than a predetermined value.

[0287] The second result submodule is used to obtain an assessment result representing the danger of the defect area when the target safety factor is less than or equal to a predetermined value.

[0288] According to embodiments of this application, any multiple modules among processing module 1410, generation module 1420, configuration module 1430, analysis module 1440, first determination module 1450, and second determination module 1460 can be combined into one module, or any one of these modules can be split into multiple modules. Alternatively, at least some of the functions of one or more of these modules can be combined with at least some of the functions of other modules and implemented in one module. According to embodiments of this application, at least one of processing module 1410, generation module 1420, configuration module 1430, analysis module 1440, first determination module 1450, and second determination module 1460 can be at least partially implemented as hardware circuitry, such as field-programmable gate arrays (FPGAs), programmable logic arrays (PLAs), systems-on-a-chip, systems-on-a-substrate, systems-on-package, application-specific integrated circuits (ASICs), or implemented in hardware or firmware by any other reasonable means of integrating or packaging circuitry, or implemented in software, hardware, or firmware, or in any suitable combination of any of these three implementation methods. Alternatively, at least one of the processing module 1410, generation module 1420, configuration module 1430, analysis module 1440, first determination module 1450 and second determination module 1460 may be implemented at least partially as a computer program module, which can perform corresponding functions when the computer program module is run.

[0289] Based on the above-described method for assessing the safety of component defects, this application also provides a train, which will be described below in conjunction with... Figure 15 Describe the train.

[0290] Figure 15 A schematic diagram of a train according to an embodiment of this application is shown.

[0291] like Figure 15 As shown, the train includes a memory 1510 and a processor 1520.

[0292] The memory 1510 stores a computer program, which, when executed by the processor 1520, implements the steps of the method described above for evaluating the safety of component defects.

[0293] This application also provides a computer-readable storage medium, which may be included in the device / apparatus / system described in the above embodiments; or it may exist independently and not assembled into the device / apparatus / system. The computer-readable storage medium carries one or more programs, which, when executed, implement the method according to the embodiments of this application.

[0294] According to embodiments of this application, the computer-readable storage medium can be a non-volatile computer-readable storage medium, such as including but not limited to: portable computer disks, hard disks, random access memory (RAM), read-only memory (ROM), erasable programmable read-only memory (EPROM or flash memory), portable compact disk read-only memory (CD-ROM), optical storage devices, magnetic storage devices, or any suitable combination thereof. In this application, the computer-readable storage medium can be any tangible medium containing or storing a program that can be used by or in conjunction with an instruction execution system, apparatus, or device. For example, according to embodiments of this application, the computer-readable storage medium may include the ROM and / or RAM described above and / or one or more memories other than ROM and RAM.

[0295] Embodiments of this application also include a computer program product comprising a computer program containing program code for performing the methods shown in the flowchart. When the computer program product is run on a computer system, the program code is used to cause the computer system to implement the methods provided in the embodiments of this application.

[0296] When the computer program is executed by a processor, it performs the functions defined in the system / apparatus of this application embodiments. According to embodiments of this application, the systems, apparatuses, modules, units, etc., described above can be implemented by computer program modules.

[0297] In one embodiment, the computer program may rely on tangible storage media such as optical storage devices or magnetic storage devices. In another embodiment, the computer program may also be transmitted and distributed as signals over a network medium, and downloaded and installed via a communication component, and / or installed from a removable medium. The program code contained in the computer program can be transmitted using any suitable network medium, including but not limited to: wireless, wired, etc., or any suitable combination thereof.

[0298] In such an embodiment, the computer program can be downloaded and installed from a network via a communication component, and / or installed from a removable medium. When the computer program is executed by a processor, it performs the functions defined in the system of the embodiments of this application. According to embodiments of this application, the systems, devices, apparatuses, modules, units, etc., described above can be implemented by computer program modules.

[0299] According to embodiments of this application, program code for executing the computer programs provided in the embodiments of this application can be written in any combination of one or more programming languages. Specifically, these computational programs can be implemented using high-level procedural and / or object-oriented programming languages, and / or assembly / machine languages. Programming languages ​​include, but are not limited to, languages ​​such as Java, C++, Python, "C", or similar programming languages. The program code can be executed entirely on the user's computing device, partially on the user's device, partially on a remote computing device, or entirely on a remote computing device or server. In cases involving remote computing devices, the remote computing device can be connected to the user's computing device via any type of network, including a local area network (LAN) or a wide area network (WAN), or it can be connected to an external computing device (e.g., via the Internet using an Internet service provider).

[0300] The flowcharts and block diagrams in the accompanying drawings illustrate the architecture, functionality, and operation of possible implementations of systems, methods, and computer program products according to various embodiments of this application. In this regard, each block in a flowchart or block diagram may represent a module, segment, or portion of code containing one or more executable instructions for implementing a specified logical function. It should also be noted that in some alternative implementations, the functions indicated in the blocks may occur in a different order than those indicated in the drawings. For example, two consecutively indicated blocks may actually be executed substantially in parallel, and they may sometimes be executed in reverse order, depending on the functions involved. It should also be noted that each block in a block diagram or flowchart, and combinations of blocks in a block diagram or flowchart, may be implemented using a dedicated hardware-based system that performs the specified function or operation, or using a combination of dedicated hardware and computer instructions.

[0301] Those skilled in the art will understand that the features described in the various embodiments of this application can be combined and / or combined in various ways, even if such combinations or combinations are not explicitly described in this application. In particular, the features described in the various embodiments of this application can be combined and / or combined in various ways without departing from the spirit and teachings of this application. All such combinations and / or combinations fall within the scope of this application.

[0302] The embodiments of this application have been described above. However, these embodiments are merely illustrative and not intended to limit the scope of this application. Although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination. Without departing from the scope of this application, those skilled in the art can make various substitutions and modifications, all of which should fall within the scope of this application.

Claims

1. A method for assessing the safety of defects in a component, characterized in that, The method includes: The contour detection data of the defect area on the component to be evaluated is processed to obtain the target defect contour node sequence; In the benchmark structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve are generated based on the target defect contour node sequence. The leading edge curve is used to represent the boundary of the defect region on the benchmark structural model. The benchmark structural model is constructed by the component to be evaluated in a defect-free state. Multiple mesh elements are configured in the area between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structure model; The defective structure model is analyzed to obtain the stress intensity factor of each leading node on the leading edge curve of the defective structure model at each analysis step during the analysis process. Based on the stress intensity factor of each leading edge node in each analysis step, determine the stress characteristic value and safety assessment index of each leading edge node; The safety assessment result is determined based on the stress characteristic value and the safety assessment index.

2. The method according to claim 1, characterized in that, The baseline structural model is constructed in the following manner: Based on the identification information of the component to be evaluated, obtain the initial baseline structural model of the component to be evaluated in a defect-free state; The actual usage conditions of the component to be evaluated are applied to the initial reference structural model and analyzed to obtain the first stress field data of the initial reference structural model. If the first stress field data passes verification, the initial reference structure model is used as the reference structure model.

3. The method according to claim 2, characterized in that, The first stress field data includes the direction of the maximum principal stress; The process of processing the contour detection data of the defect region on the component to be evaluated to obtain the target defect contour node sequence includes: The contour detection data is processed based on the direction of the maximum principal stress to obtain an initial discrete node sequence; The initial discrete node sequence is interpolated to obtain an interpolated contour node sequence, and an initial contour is generated based on the interpolated contour node sequence. The initial contour is smoothed to obtain a smooth contour; The peak and valley regions of the smooth contour are reconstructed to obtain the reconstructed contour; Based on the reconstructed contour, the target defect contour node sequence is output.

4. The method according to claim 3, characterized in that, The process of processing the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence includes: Based on the contour detection data of the defect region, the direction of the maximum principal stress at the location of the defect region is located in the reference structural model. A reference coordinate system is established with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; Place the contour detection data in the reference coordinate system; The contour detection data placed in the reference coordinate system is projected onto a plane perpendicular to the direction of the maximum principal stress to obtain multiple initial discrete nodes; The initial discrete nodes are cleaned and sorted to obtain the initial discrete node sequence.

5. The method according to claim 4, characterized in that, The reference coordinate system further includes a second coordinate axis for representing the defect length direction and a third coordinate axis for representing the defect depth direction; each initial discrete node in the initial discrete node sequence has a second coordinate value in the defect length direction and a third coordinate value in the defect depth direction; The step of interpolating the initial discrete node sequence to obtain the interpolated contour node sequence includes: The defect length range of the initial discrete node sequence is determined based on the second coordinate value of each initial discrete node in the defect length direction. Within the range of the defect length, interpolated coordinate values ​​are constructed that are equally spaced along a second coordinate axis in the direction of the defect length; The interpolated coordinate values ​​are used to interpolate the initial discrete node sequence to obtain the interpolated contour node sequence.

6. The method according to claim 3, characterized in that, The peak region includes peak points, and the valley region includes valley points; The reconstruction of the peak and valley regions of the smooth contour to obtain the reconstructed contour includes: A peak window and a valley window of predetermined length are constructed, centered on the peak point and the valley point, respectively. Data within the peak window and the valley window are extracted to obtain peak window data and valley window data; The peak window data and the valley window data are respectively input into the contour reconstruction function to obtain the initial reconstructed contour of the peak window and the initial reconstructed contour of the valley window. The contour reconstruction function is constructed with the peak point or valley point as the center of symmetry. The initial reconstructed contours of the peak window and the initial reconstructed contours of the valley window are fused with the original smooth contours within the peak window and the valley window, respectively, to obtain the local reconstructed contours of the peak window and the valley window. Based on the local reconstructed contours of the peak window and the valley window, the original smooth contours within the peak window and the valley window are replaced respectively to obtain the reconstructed contours.

7. The method according to claim 3, characterized in that, The reconstructed contour also includes a smooth region, which together with the peak region and the valley region constitutes the reconstructed contour. The step of outputting the target defect contour node sequence based on the reconstructed contour includes: The total number of contour nodes to be output is determined based on the contour length of the reconstructed contour and the preset node spacing. For each of the flat region, the peak region, and the valley region: The number of nodes in a region is determined based on the total number of contour nodes to be output and the preset weight of the region. Within the region, based on the number of nodes in the region and the outline nodes at the region's endpoints, the encrypted nodes within the region are determined, and a node set is constructed. The node sets of the flat region, the peak region, and the valley region are processed to obtain the target defect contour node sequence.

8. The method according to claim 4, characterized in that, In the baseline structural model, generating a leading edge curve and cutting lines on both sides of the leading edge curve based on the target defect contour node sequence includes: In the reference structural model, the leading edge curve is generated based on the target defect profile node sequence in a plane perpendicular to the direction of the maximum principal stress. With the leading edge curve as the center, a cutting line is generated by offsetting a predetermined distance on both sides of the leading edge curve.

9. The method according to claim 1, characterized in that, The process involves configuring multiple mesh elements within the region between the cutting lines, and replacing the mesh elements traversed by the leading edge curve with defect elements to obtain a defect structure model, including: Multiple mesh cells are configured between the cutting lines, wherein the number of mesh cells in the region between the cutting lines is odd in the defect length direction, and the number of nodes of the mesh cells in the defect depth direction is greater than or equal to the total number of contour nodes. Verify the baseline structural model configured with grid cells; If the verification passes, the grid cells through which the leading edge curve passes are replaced with defect cells to obtain a defect structure model.

10. The method according to claim 9, characterized in that, The verification of the baseline structural model configured with mesh cells includes: The actual usage conditions of the component to be evaluated are applied to the reference structural model configured with mesh elements, and the analysis is performed to obtain the second stress field data of the reference structural model under the condition of configuring mesh elements; The reference structural model configured with grid cells is verified based on the error between the second stress field data and the first stress field data.

11. The method according to claim 1, characterized in that, The analysis of the defective structure model to obtain the stress intensity factor of each leading node on the leading edge curve of the defective structure model at each analysis step during the analysis process includes: The actual usage conditions of the component to be evaluated are applied to the defective structural model, and the defective structural model is analyzed to obtain the stress field, strain energy density and displacement field distribution of each leading node on the leading edge curve of the defective structural model in each analysis step during the analysis process; Based on the stress field, strain energy density, and displacement field distribution of each leading edge node in each analysis step, the stress intensity factor of each leading edge node in each analysis step is obtained.

12. The method according to claim 1, characterized in that, The determination of the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node in each analysis step includes: For each leading edge node: Extract the maximum and minimum stress intensity factors of the leading edge node from the stress intensity factors of the leading edge node in each analysis step; Based on the maximum and minimum stress intensity factors, determine the stress intensity factor range and stress ratio of the leading edge node; The stress characteristic value is obtained based on the maximum stress intensity factor, the minimum stress intensity factor, the stress intensity factor range, and the stress ratio; The safety assessment index is obtained based on the stress ratio and multiple assessment parameters.

13. The method according to claim 12, characterized in that, The safety assessment index is obtained based on the stress ratio and multiple assessment parameters, including: For each leading edge node: Based on the material properties corresponding to the leading edge node, the baseline fatigue crack propagation threshold value is queried from the standard file. Based on the stress ratio of the leading edge node and the reference fatigue crack propagation threshold value, the target fatigue crack propagation threshold value of the leading edge node is determined. Based on the target fatigue crack propagation threshold, tensile strength, and stress ratio, the length of the material characteristic crack corresponding to the leading edge node is determined. Based on the defect feature size of the leading edge node, the target fatigue crack propagation threshold value, and the material characteristic crack length, the node-level defect propagation threshold of the leading edge node is obtained and used as the safety assessment index. The defect feature size of the leading edge node is determined according to the defect type of the defect region.

14. The method according to claim 13, characterized in that, The determination of the safety assessment result based on the stress characteristic value and the safety assessment index includes: The safety factor of each leading edge node is obtained by the ratio of the node-level defect propagation threshold of each leading edge node to the range of the stress intensity factor. The minimum value of the safety factor is extracted from the safety factor of each leading edge node to obtain the target safety factor; When the target safety factor is greater than a predetermined value, an assessment result representing the safety of the defective area is obtained; When the target safety factor is less than or equal to the predetermined value, an assessment result representing the danger of the defective area is obtained.

15. A system for assessing the safety of defects in components, characterized in that, The system includes: The processing module is used to process the contour detection data of the defect area on the component to be evaluated to obtain the target defect contour node sequence; The generation module is used to generate a leading edge curve and cutting lines on both sides of the leading edge curve in the reference structural model based on the target defect contour node sequence. The leading edge curve is used to represent the boundary of the defect region on the reference structural model, which is constructed by the component to be evaluated in a defect-free state. A configuration module is used to configure multiple mesh cells in the area between cutting lines, and replace the mesh cells through which the leading edge curve passes with defect cells to obtain a defect structure model; The analysis module is used to analyze the defect structure model to obtain the stress intensity factor of each leading node on the leading curve of the defect structure model at each analysis step during the analysis process. The first determination module is used to determine the stress characteristic value and safety assessment index of each leading edge node based on the stress intensity factor of each leading edge node in each analysis step. The second determining module is used to determine the safety assessment result based on the stress characteristic value and the safety assessment index.

16. The system according to claim 15, characterized in that, The system for assessing the safety of component defects further includes: The acquisition module is used to acquire the initial baseline structural model of the component to be evaluated in a defect-free state based on the identification information of the component to be evaluated. An application module is used to apply the actual usage conditions of the component to be evaluated to the initial reference structural model and perform analysis to obtain the first stress field data of the initial reference structural model. The verification module is used to use the initial reference structure model as the reference structure model if the first stress field data passes the verification.

17. The system according to claim 16, characterized in that, The first stress field data includes the direction of the maximum principal stress; The processing module includes: The first processing submodule is used to process the contour detection data based on the direction of the maximum principal stress to obtain an initial discrete node sequence; An interpolation submodule is used to perform interpolation processing on the initial discrete node sequence to obtain an interpolated contour node sequence, and to generate an initial contour based on the interpolated contour node sequence. The second processing submodule is used to smooth the initial contour to obtain a smooth contour. The reconstruction submodule is used to reconstruct the peak and valley regions of the smooth contour to obtain the reconstructed contour. The output submodule is used to output the target defect contour node sequence based on the reconstructed contour.

18. The system according to claim 17, characterized in that, The first processing submodule includes: A positioning unit is used to locate the direction of the maximum principal stress at the location of the defect area in the reference structural model based on the contour detection data of the defect area. A unit is established to create a reference coordinate system with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis. The first processing unit is used to place the contour detection data in the reference coordinate system; A projection unit is used to project the contour detection data placed in the reference coordinate system onto a plane perpendicular to the direction of the maximum principal stress, thereby obtaining multiple initial discrete nodes; The second processing unit is used to clean and sort the initial discrete nodes to obtain the initial discrete node sequence.

19. A train, characterized in that, Including memory and processor; The memory stores a computer program, and when the computer program is executed by the processor, the processor is configured to: The contour detection data of the defect area on the component to be evaluated is processed to obtain the target defect contour node sequence; In the benchmark structural model, a leading edge curve and cutting lines located on both sides of the leading edge curve are generated based on the target defect contour node sequence. The leading edge curve is used to represent the boundary of the defect region on the benchmark structural model. The benchmark structural model is constructed by the component to be evaluated in a defect-free state. Multiple mesh elements are configured in the area between the cutting lines, and the mesh elements through which the leading edge curve passes are replaced with defect elements to obtain a defect structure model; The defect structure model is analyzed to obtain the stress intensity factor of each leading node on the leading edge curve of the defect structure model at each analysis step during the analysis process; Based on the stress intensity factor of each leading edge node in each analysis step, determine the stress characteristic value and safety assessment index of each leading edge node; The safety assessment result is determined based on the stress characteristic value and the safety assessment index.

20. The train according to claim 19, characterized in that, The processor is also configured to: Based on the identification information of the component to be evaluated, obtain the initial baseline structural model of the component to be evaluated in a defect-free state; The actual usage conditions of the component to be evaluated are applied to the initial reference structural model and analyzed to obtain the first stress field data of the initial reference structural model. If the first stress field data passes verification, the initial reference structure model is used as the reference structure model.

21. The train according to claim 20, characterized in that, The first stress field data includes the direction of the maximum principal stress, and the processor is further configured to: The contour detection data is processed based on the direction of the maximum principal stress to obtain an initial discrete node sequence; The initial discrete node sequence is interpolated to obtain an interpolated contour node sequence, and an initial contour is generated based on the interpolated contour node sequence. The initial contour is smoothed to obtain a smooth contour; The peak and valley regions of the smooth contour are reconstructed to obtain the reconstructed contour; Based on the reconstructed contour, the target defect contour node sequence is output.

22. The train according to claim 21, characterized in that, The processor is also configured to: Based on the contour detection data of the defect region, the direction of the maximum principal stress at the location of the defect region is located in the reference structural model. A reference coordinate system is established with the direction of the maximum principal stress at the location of the defect region as the first coordinate axis; Place the contour detection data in the reference coordinate system; The contour detection data placed in the reference coordinate system is projected onto a plane perpendicular to the direction of the maximum principal stress to obtain multiple initial discrete nodes; The initial discrete nodes are cleaned and sorted to obtain the initial discrete node sequence.