Electrodes and secondary batteries

By setting peaks and valleys of a waveform shape on the electrode film and controlling the interval between them to be less than the thickness of the electrode film, the problem of reduced strength caused by unevenness of the electrode film is solved, and the strength of the electrode is improved.

CN123073013APending Publication Date: 2026-11-10TOYOTA JIDOSHA KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202610593775.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-08
Filing Date
2026-04-30
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In existing electrode manufacturing methods, unevenness is easily formed on one side of the electrode film in the thickness direction, which leads to the lengthening of cracks and consequently reduces the strength of the electrode film and the electrode.

Method used

By setting a waveform shape on the first and second surfaces of the electrode film, the average interval between adjacent peaks is less than or equal to the average thickness of the electrode film, thus suppressing the length of cracks. A self-supporting film is used as the electrode film material, and the shape of the peaks and valleys remains unchanged during the pressing process.

Benefits of technology

It effectively suppressed the reduction in electrode film strength, improved the overall strength of the electrode, and ensured the stability and durability of the electrode.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123073013A_ABST
    Figure CN123073013A_ABST
Patent Text Reader

Abstract

The electrode comprises: a current collector extending along a length direction; and an electrode film disposed on the current collector. The electrode film includes active material powder and fibrillated binder. The electrode film has a first surface attached to the current collector and a second surface located on the opposite side of the first surface. The first surface has a waveform shape formed by repeated peaks and valleys along the length direction. When the average interval between adjacent peaks in the length direction is set as P, and the average thickness of the electrode film in the thickness direction orthogonal to the length direction is set as T, the relationship P≦T is satisfied.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to electrodes and secondary batteries. Background Technology

[0002] As a conventional electrode manufacturing method, Japanese Patent Application Publication No. 2024-140137 discloses a manufacturing method including: a step of stacking a positive electrode layer containing a positive electrode active material layer and an electrolyte layer containing a solid electrolyte to obtain a laminate; a step of forming a concave portion and a convex portion extending from one side of the surface direction of the laminate to the other; and a step of flattening the concave portion and the convex portion while applying pressure to the laminate in the thickness direction. Summary of the Invention

[0003] One method for manufacturing electrodes used in secondary batteries involves attaching a pre-formed electrode film to the surface of a current collector. During the film-forming process of the composite material layer, irregularities can sometimes form on the main surface of the electrode film, at least on one side in the thickness direction, due to processes such as roll forming, roller conveying, and roller transfer. Furthermore, along with these irregularities, cracks extending in the in-plane direction can sometimes form within the electrode film. If these cracks lengthen, the strength of the electrode film decreases, which in turn reduces the strength of the electrode itself.

[0004] This disclosure was made in view of the above-mentioned problems, and the purpose of this disclosure is to provide an electrode and a secondary battery capable of suppressing the reduction in the strength of the electrode film caused by cracks.

[0005] The electrode based on this disclosure comprises: a current collector extending along a length direction; and an electrode film disposed on the current collector. The electrode film comprises an active material powder and a fibrillated binder. The electrode film has a first surface attached to the current collector and a second surface located on the side opposite to the first surface. The first surface has a wave-like shape formed by repeatedly forming peaks and valleys along the length direction. When the average interval between adjacent peaks along the length direction is defined as P, and the average thickness of the electrode film in the thickness direction orthogonal to the length direction is defined as T, the relationship P ≤ T is satisfied.

[0006] According to the above configuration, by setting the average interval between adjacent peaks on the first surface of the electrode film with a waveform shape to below the average thickness of the electrode film, the length of cracks formed in the electrode film along the length direction due to the peaks and valleys becomes shorter, thereby suppressing the reduction in the strength of the electrode film.

[0007] The secondary battery disclosed herein includes an electrode body containing the aforementioned electrodes and a housing housing that contains the aforementioned electrode body.

[0008] Based on the above configuration, a secondary battery can be provided that includes an electrode body containing an electrode whose strength reduction is suppressed by using an electrode film.

[0009] The above and other objects, features, aspects and advantages of the present invention will become apparent from the following detailed description of the invention in conjunction with the accompanying drawings. Attached Figure Description

[0010] Figure 1 This is a simplified cross-sectional view of the secondary battery involved in the implementation method.

[0011] Figure 2 This is a simplified top view of the positive electrode involved in the implementation method after it has been unfolded.

[0012] Figure 3 This is a cross-sectional view of the positive electrode involved in the implementation method.

[0013] Figure 4 This is a schematic diagram illustrating the manufacturing process of the positive electrode involved in the embodiment.

[0014] Figure 5 This is a schematic diagram illustrating the process of forming a positive electrode film used in the positive electrode according to the embodiment. Detailed Implementation

[0015] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that in the embodiments shown below, the same or common parts are labeled with the same reference numerals in the drawings, and their descriptions are omitted.

[0016] (Secondary battery)

[0017] Figure 1 This is a simplified cross-sectional view of the secondary battery involved in the embodiment. (Refer to...) Figure 1 The secondary battery 100 involved in Embodiment 1 is described.

[0018] The secondary battery 100 is, for example, a lithium-ion battery installed in a vehicle. It should be noted that the uses and types of the secondary battery 100 are not limited to the examples above.

[0019] The secondary battery 100 according to Embodiment 1 includes a wound electrode body 1, a housing 2, a positive terminal 3, a positive current collector 4, an external gasket 5, an internal gasket 6, and a negative current collector 7.

[0020] The electrode body 1 is wound into a spiral shape. The wound electrode body 1 is housed in the housing 2. The housing 2 has a cylindrical shape. That is, the secondary battery 100 is a cylindrical battery.

[0021] The wound electrode body 1 includes a positive electrode 10, a negative electrode 20, and a separator 30. The separator 30 is disposed between the positive electrode 10 and the negative electrode 20 in a radial direction R of the wound electrode body 1. The separator 30 separates the positive electrode 10 and the negative electrode 20. On the other hand, the separator 30 is configured to allow ions (e.g., lithium ions) to move back and forth between the positive electrode 10 (more precisely, the positive electrode active material) and the negative electrode 20 (more precisely, the negative electrode active material).

[0022] The wound electrode body 1 is composed of an electrode plate assembly formed by winding a positive electrode 10 and a negative electrode 20 through a diaphragm 30. It should be noted that in this embodiment, the positive electrode 10 and the negative electrode 20 are electrodes used in the wound electrode body 1, and their polarities are different. One of the positive electrode 10 and the negative electrode 20 corresponds to the first electrode, and the other of the positive electrode 10 and the negative electrode 20 corresponds to the second electrode.

[0023] The housing 2 has an upper surface 2a, a lower surface 2b, and a side surface 2c. The upper surface 2a is the side of the housing 2 located axially in the cylindrical shape. Viewed from the perspective of the wound electrode body 1, the upper surface 2a is located on one side Z1 along the axial direction Z of the wound electrode body 1. The lower surface 2b is the other side Z2 of the housing 2 located axially in the cylindrical shape. Viewed from the perspective of the wound electrode body 1, the lower surface 2b is located on the other side along the axial direction Z of the wound electrode body 1. The side surface 2c has a cylindrical shape. The side surface 2c connects the upper surface 2a and the lower surface 2b. The housing 2 is formed of copper or aluminum, etc.

[0024] It should be noted that the casing 2 also contains electrolyte (not shown). On the other hand, in the case where the wound electrode body 1 is an all-solid-state battery, the electrolyte can be omitted.

[0025] The height dimension (dimension along the Z-axis) of the housing 2 is, for example, 50 mm or more, 60 mm or more, 70 mm or more, or 80 mm or more. The larger the height dimension (dimension along the Z-axis) of the housing 2, the larger the battery capacity of the secondary battery 100. Conversely, the height dimension (dimension along the Z-axis) of the housing 2 is, for example, 150 mm or less, 100 mm or less, or 80 mm or less. The smaller the height dimension (height dimension) along the Z-axis of the housing 2, the lower the height of the module housing the secondary battery 100 can be.

[0026] The diameter (radial dimension R) of the housing 2 is, for example, 15mm or more, 20mm or more, 25mm or more, 30mm or more, 40mm or more, 45mm or more, or 46mm or more. The larger the diameter (maximum radial dimension R) of the housing 2, the larger the battery capacity of the secondary battery 100. The diameter (radial dimension R) of the housing 2 is, for example, less than 100mm, less than 75mm, less than 50mm, or less than 46mm. The smaller the diameter (radial dimension R) of the housing 2, the more compactly the secondary battery 100 can be arranged within the module.

[0027] The positive terminal 3 is located on one side Z1 in the axial direction Z relative to the wound electrode body 1. The positive terminal 3 includes a disc portion 3a and a riveting portion 3b. The riveting portion 3b is connected to the disc portion 3a. The riveting portion 3b is configured to extend from the center of the disc portion 3a toward the other side Z2 in the axial direction Z. It should be noted that the positive terminal 3 is made of aluminum. The disc portion 3a is disposed on the upper surface portion 2a of the housing 2. A through hole 2d is provided on the upper surface portion 2a of the housing 2. The riveting portion 3b extends from the disc portion 3a disposed on the outside of the housing 2 through the through hole 2d into the interior of the housing 2.

[0028] The positive current collector 4 is housed within the housing 2. The positive current collector 4 is positioned on one side Z1 in the Z-axis direction relative to the wound electrode body 1. The positive current collector 4 is welded to the composite material unformed portion 12a of the positive electrode plate 10. Thus, the positive current collector 4 is positively charged. The positive current collector 4 is welded to the end of the riveting portion 3b on the other side Z2 in the Z-axis direction. Thus, the positive terminal 3 is positively charged.

[0029] An external gasket 5 is disposed between the disk portion 3a of the positive terminal 3 and the upper surface portion 2a of the housing 2. Thus, the positive terminal 3 and the housing 2 are insulated from each other.

[0030] An internal gasket 6 is disposed inside the housing 2 between the housing 2 and the positive current collector 4. Thus, the housing 2 and the positive current collector 4 are mutually insulated. It should be noted that the riveting part 3b contacts the positive current collector 4 by passing through the internal gasket 6.

[0031] The negative electrode current collector 7 is housed within the housing 2. The negative electrode current collector 7 is located on the opposite side Z2 in the axial direction Z relative to the wound electrode body 1. The negative electrode current collector 7 is welded to the unformed portion 22a of the composite material of the negative electrode 20. Thus, the negative electrode current collector 7 carries a negative charge. The negative electrode current collector 7 is in contact with the housing 2. Specifically, the negative electrode current collector 7 is in contact with the lower surface portion 2b and the side surface portion 2c. Thus, the housing 2 carries a negative charge. Furthermore, the upper surface portion 2a carries a negative charge.

[0032] Figure 2 This is a simplified top view of the positive electrode of the wound electrode body according to the embodiment after it has been unfolded. Figure 3This is a simplified cross-sectional view of the positive electrode of the wound electrode body according to the embodiment. It should be noted that... Figure 3 It is along Figure 2 The sectional view shown is taken along line III-III. (Refer to...) Figure 2 as well as Figure 3 This describes the positive electrode 10 involved in the implementation method.

[0033] The positive electrode 10, in its unfolded state, has a strip-like shape extending along its length direction D1 (long side direction). The length direction D1 is orthogonal to the thickness direction D3 of the positive electrode 10. The positive electrode 10 has a first end 10a and a second end 10b along the length direction D1. The first end 10a is the end located on the inner circumferential side of the wound electrode body 1 (the inner circumferential end). The second end 10b is the end located on the outer circumferential side of the wound electrode body 1 (the outer circumferential end).

[0034] The positive electrode 10 includes a positive current collector 11, a first positive electrode film 13, and a second positive electrode film 14. The positive current collector 11 is made of a metal foil such as aluminum. The positive current collector 11 has a wave-like shape with continuous concave and convex shapes along the length direction D1.

[0035] The positive current collector 11 has a first main surface 11a and a second main surface 11b arranged along the thickness direction D3. The first main surface 11a is located on one side of the positive current collector 11 in the thickness direction D3. The second main surface 11b is located on the other side of the positive current collector 11 in the thickness direction D3. In the state of winding the electrode body 1, that is, in the winding state after the positive electrode 10 is wound, the first main surface 11a faces the inner peripheral side, and the second main surface 11b faces the outer peripheral side. The first main surface 11a has a wave-like shape along the first surface 13a of the first positive electrode film 13 (described later). The second main surface 11b has a wave-like shape along the second surface 13b of the second positive electrode film 14 (described later).

[0036] The positive electrode 10 has a composite material unformed portion 12a and a composite material formed portion 12b. The composite material unformed portion 12a is the portion of the positive electrode current collector 11 exposed from both the first positive electrode film 13 and the second positive electrode film 14. The composite material formed portion 12b is the portion of the positive electrode 10 in which both the first positive electrode film 13 and the second positive electrode film 14 are formed. The composite material unformed portion 12a extends from the composite material formed portion 12b toward one side in the width direction D2. In the wound state, the composite material unformed portion 12a is exposed from the composite material formed portion 12b toward one side Z1 in the axial direction Z of the wound electrode body 1.

[0037] The first positive electrode film 13 is disposed on the first main surface 11a. The first positive electrode film 13 is disposed on the first main surface 11a with the first main surface 11a exposed on one side of the width direction D2, which is orthogonal to the aforementioned length direction D1. It should be noted that the width direction D2 is the direction parallel to the axial direction Z in the winding electrode body 1.

[0038] The first positive electrode film 13 has a first surface 13a attached to the positive current collector 11 and a second surface 13b located on the opposite side of the first surface 13a. The second surface 13b is formed to be flat.

[0039] The first surface 13a has a wave-like shape formed by repeated peaks R1 and valleys V1 along the length direction D1. The peaks R1 are concave portions toward the second surface 13b. The valleys V1 are convex portions toward the direction away from the second surface 13b.

[0040] In the first positive electrode film 13, when the average interval between adjacent peaks R1 in the length direction D1 is set to P1, and the average thickness of the first positive electrode film 13 in the thickness direction D3, which is orthogonal to the length direction D1, is set to T1, the relationship P1≦T1 is satisfied. As a result, the length of the cracks formed in the first positive electrode film 13 along the length direction D1 due to the peaks R1 and valleys V1 is shortened, and the reduction in the strength of the first positive electrode film 13 can be suppressed.

[0041] Furthermore, the relationship 0.1T1≦P1 can be further satisfied. This can suppress the average interval P1 between peaks R1 from being too small.

[0042] The aforementioned P1 and T1 can be calculated by SEM observation of a cross-section of the positive electrode 10 parallel to the thickness direction D3 and the length direction D1. Specifically, in the observed cross-section, five sets of adjacent peaks R1 along the length direction D1 are selected, and the average value of the interval between the five sets of peaks R1 along the length direction D1 is set as P1. Furthermore, the average value of the thickness of the first positive electrode film 13 at the five peaks R1 and the thickness of the first positive electrode film 13 at the five valleys V1 is set as T1. It should be noted that the above description illustrates a case where five positions are selected when calculating P1 and T1, but this is not a limitation, and the number can be appropriately set.

[0043] In the first positive electrode film 13 described above, when the maximum distance between the peak R1 and the valley V1 on the thickness direction D3, which is orthogonal to the length direction D1, is set to RT1, the relationship 0.1T1≦RT1≦0.5T1 is further satisfied. As a result, the length of the crack formed in the first positive electrode film 13 along the length direction D1 due to the peak R1 and the valley V1 can be shortened more effectively, and the strength reduction of the first positive electrode film 13 can be further suppressed.

[0044] RT1 can be defined, for example, as the maximum distance between the peak R1 and the valley V1 in the thickness direction D3 within the same field of view in the observed cross-section, but it is not limited to this. When there are multiple observation positions, RT1 can also be the average of the maximum distances between the peak R1 and the valley V1 in the thickness direction D3 observed at multiple positions. Alternatively, RT1 can also be the maximum value among the maximum distances observed at multiple positions.

[0045] The second positive electrode film 14 is disposed on the second main surface 11b. The second positive electrode film 14 is disposed on the second main surface 11b with the second main surface 11b exposed on one side of the width direction D2, which is orthogonal to the aforementioned length direction D1. It should be noted that the width direction D2 is the direction parallel to the axial direction Z in the winding electrode body 1.

[0046] The second positive electrode film 14 has a first surface 14a attached to the positive current collector 11 and a second surface 14b located on the opposite side of the first surface 14a. The second surface 14b is formed to be flat.

[0047] The first surface 14a has a wave-like shape formed by repeated peaks R2 and valleys V2 along the length direction D1. The peaks R2 are convex portions that become convex in the direction away from the second surface 14b. The valleys V2 are concave portions that become concave in the direction towards the second surface 14b.

[0048] In the second positive electrode film 14, when the average interval between adjacent peaks R2 along the length direction D1 is set to P2, and the average thickness of the second positive electrode film 14 along the thickness direction D3, which is orthogonal to the length direction D1, is set to T2, the relationship P2 ≤ T2 is also satisfied. As a result, the length of the cracks formed in the second positive electrode film 14 along the length direction D1 due to the peaks R1 and valleys V1 is shortened, and the reduction in the strength of the second positive electrode film 14 can be suppressed.

[0049] Furthermore, the relationship 0.1T2≦P2 can be further satisfied. This can suppress the average interval P2 between peaks R2 from being too small.

[0050] The aforementioned P2 and T2 can be calculated on the second positive electrode film 14 using the same method as the calculation method for P1 and T1. Furthermore, in the second positive electrode film 14, when the maximum distance between the peak R2 and the valley V2 in the thickness direction D3 is set to RT2, the relationship 0.1T2≦RT2≦0.5T2 is further satisfied. This effectively shortens the length of the crack formed along the length direction D1 in the second positive electrode film 14 due to the peak R2 and the valley V2, further suppressing the reduction in strength of the second positive electrode film 14.

[0051] RT2 can be calculated on the second positive electrode film 14 using the same method as the calculation method for RT1 described above.

[0052] Both the first positive electrode film 13 and the second positive electrode film 14 are composed of positive electrode films 131 and 132 (described later) containing positive electrode active materials (see reference). Figure 4 It should be noted that, in the first positive electrode film 13 and the second positive electrode film 14, by making the second surfaces 13b and 14b flat, it is easy to wind the positive electrode 10.

[0053] Since the structure of the negative electrode 20 is basically the same as that of the positive electrode 10, its unfolded view and cross-sectional view are not shown. The negative electrode 20 also has a strip-like shape extending along its length in its unfolded state. The negative electrode 20 has a first end and a second end in its length direction. The first end is the end located on the inner circumference side of the wound electrode body 1 (the inner circumference end). The second end is the end located on the outer circumference side of the wound electrode body 1 (the outer circumference end).

[0054] For example Figure 1 As shown, the negative electrode 20 includes a negative electrode current collector 21, a first negative electrode film 23, and a second negative electrode film 24. The negative electrode current collector 21 is made of a metal foil such as copper. The negative electrode current collector 21 has a first main surface 21a and a second main surface 21b arranged along the thickness direction. In the state of winding the electrode body 1, that is, in the wound state after the negative electrode 20 is wound, the first main surface 21a faces the inner peripheral side, and the second main surface 21b faces the outer peripheral side.

[0055] The negative electrode 20 has a composite material unformed portion 22a and a composite material formed portion. The composite material unformed portion 22a is the portion of the negative electrode current collector 21 exposed from both the first negative electrode film 23 and the second negative electrode film 24. The composite material formed portion is the portion of the negative electrode 20 where both the first negative electrode film 23 and the second negative electrode film 24 are formed. The composite material unformed portion 22a extends from the composite material formed portion to the other side in the width direction. In the wound state, the composite material unformed portion 22a is exposed from the composite material formed portion to the other side Z2 in the axial direction Z of the wound electrode body 1.

[0056] The first negative electrode film 23 is disposed on the first main surface 21a. The first negative electrode film 23 is disposed on the first main surface 21a on the other side of the width direction orthogonal to the aforementioned length direction, with the first main surface 21a exposed.

[0057] The second negative electrode film 24 is disposed on the second main surface 21b. The second negative electrode film 24 is disposed on the second main surface 21b on the other side of the width direction, which is orthogonal to the aforementioned length direction, with the second main surface 21b exposed. The second negative electrode film 24 is arranged to overlap with the first negative electrode film 23 in the thickness direction of the negative electrode 20. The dimensions of the second negative electrode film 24 are substantially the same as those of the first negative electrode film 23.

[0058] The first negative electrode film 23 has a first surface 23a attached to the negative electrode current collector 21 and a second surface 23b located on the opposite side of the first surface 23a. In the first negative electrode film 23, the first surface 23a also has a wave-like shape formed by repeated peaks and valleys along the length direction. On the other hand, the second surface 23b is formed to be flat.

[0059] The second negative electrode film 24 has a first surface 24a attached to the negative electrode current collector 21 and a second surface 24b located on the opposite side of the first surface 24a. In the second negative electrode film 24, the first surface 24a also has a wave-like shape formed by repeated peaks and valleys along the length direction. On the other hand, the second surface 24b is formed to be flat. By forming the second surfaces 23b and 24b to be flat, the negative electrode 20 is easier to wind.

[0060] In the first negative electrode film 23 and the second negative electrode film 24, the relationship between the average spacing between adjacent peaks in the length direction and the average thickness of the negative electrode film in the thickness direction orthogonal to the length direction also satisfies the same relationship as that between the first positive electrode film 13 and the second positive electrode film 14. Therefore, in the first negative electrode film 23 and the second negative electrode film 24, the length of cracks formed along the length direction due to peaks and valleys is shortened, which can suppress the reduction in strength of the first negative electrode film 23 and the second negative electrode film 24.

[0061] Furthermore, in the first negative electrode film 23 and the second negative electrode film 24, the relationship between the maximum distance between the peak and valley in the thickness direction and the average thickness of the negative electrode film in the thickness direction orthogonal to the length direction also satisfies the same relationship as that between the first positive electrode film 13 and the second positive electrode film 14. Therefore, it is possible to further suppress the reduction in strength of the first negative electrode film 23 and the second negative electrode film 24.

[0062] (Electrode manufacturing process)

[0063] Figure 4 This is a schematic diagram illustrating the manufacturing process of the positive electrode involved in Embodiment 1. (As shown...) Figure 4 As shown, the positive electrode 10 can be manufactured by attaching the electrode films 131 and 132 of the positive electrode to the positive current collector 11.

[0064] The positive electrode film 131 has a first surface 131a and a second surface 131b arranged along the thickness direction D3. The first surface 131a has a wave-like shape formed by alternating peaks and valleys in the length direction. The second surface 131b is formed to be flat.

[0065] The positive electrode film 132 has a first surface 132a and a second surface 132b arranged along the thickness direction D3. The first surface 132a has a wave-like shape formed by alternating peaks and valleys in the length direction. The second surface 132b is formed to be flat.

[0066] A positive electrode film 131 is disposed on the first main surface 11a with the first main surface 11a having a wave-shaped first surface 131a facing the first main surface 11a of the positive current collector 11, and a positive electrode film 132 is disposed on the second main surface 11b with the first main surface 132a having a wave-shaped first surface facing the second main surface 11b of the positive current collector 11. In this state, the positive electrode films 131 and 132 and the positive current collector 11 are conveyed while being pressed by the pressing device 90.

[0067] The pressing device 90 includes a pair of rollers 91 and 92. A positive current collector 11, with a positive electrode film 131 disposed on the first main surface 11a side and a positive electrode film 132 disposed on the second main surface 11b side, is pressed by the pair of rollers 91 and 92 as it passes between them. At this time, the positive electrode film 131 adheres to the first main surface 11a, and the positive electrode film 132 adheres to the second main surface 11b.

[0068] The positive electrode film 131 includes peaks K1 and valleys K2 that are alternately and continuously formed along the length direction D1. In the positive electrode film 131, peaks K1 and valleys K2 are formed on a first surface 131a. Similarly, the positive electrode film 132 also has peaks K1 and valleys K2 that are alternately and continuously formed along the length direction D1. In the positive electrode film 132, peaks K1 and valleys K2 are formed on a first surface 132a.

[0069] The positive electrode film 131 and the positive electrode film 132 are arranged such that the peaks K1 are staggered in the length direction D1. The peaks K1 of the positive electrode film 131 and the valleys K2 of the positive electrode film 132 face each other in the thickness direction D3, and the valleys K2 of the positive electrode film 131 and the peaks K1 of the positive electrode film 132 face each other in the thickness direction D3. In this state, the positive electrode film 131 and the positive electrode film 132 are disposed on the positive current collector 11.

[0070] Therefore, when pressing the positive electrode film 131, the positive current collector 11, and the positive electrode film 132, in the positive current collector 11, the portion between the peak K1 of the positive electrode film 131 and the valley K2 of the positive electrode film 132 becomes convex towards the second surface 13b. Similarly, in the positive current collector 11, the portion between the valley K2 of the positive electrode film 131 and the peak K1 of the positive electrode film 132 becomes concave towards the second surface 14b. That is, the positive current collector 11 forms a wave-like shape with continuous concavity and convexity along the length direction D1.

[0071] The first surface 131a of the positive electrode film 131 follows the waveform shape of the positive electrode current collector 11, and is formed with a waveform shape having a valley V1 and a peak R1 as described above. Furthermore, the first surface 132a of the positive electrode film 132 follows the waveform shape of the positive electrode current collector 11, and is formed with a waveform shape having a valley V2 and a peak R2 as described above.

[0072] On the other hand, the second surface 131b of the positive electrode film 131 is formed to maintain a flat state. The second surface 132b of the positive electrode film 132 is formed to maintain a flat state.

[0073] It should be noted that if the second surfaces 131b and 132b cannot maintain a flat state, other flattening processes may be included to make the second main surfaces 131b and 132b flat.

[0074] Figure 5 This is a schematic diagram illustrating the process of forming the electrode film of the positive electrode used in Embodiment 1. Figure 5 As shown, when preparing the aforementioned positive electrode films 131 and 132 with a wave-shaped positive electrode, for example, the positive electrode films 131 and 132, whose front and back sides are flat plates, are passed between a first roller 91A with an uneven surface and a second roller 92A with a smooth surface. This produces a wave-shaped positive electrode film 131 and 132, where the first surface 131a and 132a on the first roller 91A side is wave-shaped and the second surface 131b and 132b on the second roller 92A side is flat. The unevenness of the surface of the first roller 91A can also be periodically arranged.

[0075] The above examples illustrate cases where the surface of the first roller 91A has an uneven shape, but are not limited to this. Both the first roller 91A and the second roller 92A may also have smooth surfaces. In this case, ultrasonic vibration may be applied to one of the first roller 91A and the second roller 92A in a direction facing each other using an ultrasonic vibration device, while the electrode films 131 and 132, which are flat plates on both sides, pass between the first roller 91A and the second roller 92A.

[0076] It should be noted that since the negative electrode 20 is formed in essentially the same way as the positive electrode 10, detailed descriptions of the manufacturing process are omitted.

[0077] (Electrode film)

[0078] The electrode films 131 and 132 of the positive electrode can be made of self-supporting films. Similarly, the electrode film of the negative electrode can also be made of self-supporting films.

[0079] Self-supporting membranes are characterized by their ability to maintain their shape even without a support structure. For example, self-supporting membranes possess sufficient strength to withstand processes such as roller conveying, even without a support structure like a current collector (described later). The tensile strength range of a self-supporting membrane can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.1 MPa, 0.2 MPa, 0.3 MPa, 0.5 MPa, 0.6 MPa, 0.7 MPa, 0.8 MPa, 0.9 MPa, and 1.0 MPa, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The tensile strength range of a self-supporting membrane can be, for example, 0.1 MPa to 1.0 MPa. The tensile strength range of a self-supporting membrane can also be, for example, 0.5 MPa or higher. Having a tensile strength of 0.5 MPa or higher in a self-supporting membrane is expected to facilitate processes such as roll material handling.

[0080] The tensile strength of each of the above electrode films can be determined, for example, by the following method: A specimen is cut from the electrode film. The planar dimensions of the specimen are, for example, approximately 30 mm × 30 mm. A tensile test is performed on the specimen using a texture analyzer (e.g., manufactured by Eihong Seiki Co., Ltd.) at a speed of 2 mm / s. The maximum load during tension is measured. The tensile strength is calculated using the following formula. The tensile strength value is the arithmetic mean of three specimens.

[0081] Rm=(F×0.0098) / (t・W)

[0082] Rm: Tensile strength [MPa]

[0083] F: Maximum load [g]

[0084] t: Sample thickness [mm]

[0085] W: Sample width [mm]

[0086] The electrode film can have any planar shape. For example, the planar shape of the electrode film can be strip-shaped, rectangular, circular, etc. The dimensions of the electrode film (thickness, length, width, etc.) can be arbitrarily changed according to the electrode design. The thickness range of the electrode film can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 5μm, 10μm, 25μm, 50μm, 75μm, 100μm, 150μm, 200μm, 250μm, 300μm, 400μm, 500μm, 600μm, 700μm, 800μm, 900μm, and 1000μm, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The thickness range of the electrode film can be, for example, 5μm to 1000μm. The density range of the electrode film can be, for example, from 0.5g / cm³. 3 1.0g / cm 3 1.5g / cm 3 2.0g / cm 3 2.5g / cm 3 3.0g / cm 3 3.5g / cm 3 4.0g / cm 3 4.5g / cm 3 5.0g / cm 3 The range formed by selecting any one value can be a range with only an upper or lower limit, or a range with both an upper and lower limit can be obtained by selecting any two values. The range may or may not include endpoints. For example, the density range of the electrode film could be 0.5 g / cm³. 3 ~5.0g / cm 3 .

[0087] (composition)

[0088] The electrode membrane contains an electrode active material and a first binder. The first binder contains a fibrous binder. That is, the electrode membrane contains an electrode active material and a fibrous binder. The electrode membrane may further contain, for example, a second binder, a conductive material, a solid electrolyte, etc. For example, the electrode membrane contains, by mass fraction, 0.1% to 10% of the first binder, 0% to 10% of the second binder, 0% to 10% of the conductive material, 0% to 30% of the solid electrolyte, and the balance being the electrode active material.

[0089] (Electrode active material)

[0090] The electrode active material is a powder. The particle size distribution of the electrode active material can be, for example, a unimodal distribution. The particle size distribution can be a volume distribution or a number distribution. Volume distribution can be determined by laser diffraction. Number distribution can be determined by microscopy. "D50" represents the particle size at which the cumulative frequency reaches 50% in the cumulative distribution. The range of D50 for the electrode active material can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 0.1 μm, 0.5 μm, 1 μm, 3 μm, 5 μm, 10 μm, 15 μm, 20 μm, 25 μm, and 30 μm, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, the D50 range of the electrode active material can be 0.1 μm to 30 μm.

[0091] The particle size distribution of electrode active materials can be bimodal or multimodal. For example, in the case of a bimodal particle size distribution (frequency distribution), particles belonging to the peak with the larger particle size are called "large particles," and particles belonging to the peak with the smaller particle size are called "small particles." The mode particle size of each peak can be considered as the particle size of each particle. The "mode particle size" represents the particle size at the peak of the frequency distribution. The particle size of large particles is "D". L "Relative to the particle size of small particles" D S The ratio of "D" to " L / D S The range can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 1.2, 1.5, 2.0, 3.0, 4.0, and 5.0, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, a range can satisfy "1.2 ≦ D". L / D S Relationships such as ≦5.0”.

[0092] Electrode active materials can be primary or secondary particles. They can have any particle shape, such as spherical, ellipsoidal, scaly, plate-like, columnar, blocky, or irregular shapes.

[0093] The electrode active material can be a granulated body. Granulated bodies can be formed by any method. For example, they can be formed by spray drying, stirring granulation, etc. By granulation, the sphericity of the granulated body (secondary particles) can be adjusted. "Sphericity" refers to the roundness in an SEM image (two-dimensional image). Sphericity (roundness) is calculated using the following formula. Sphericity can be taken as the arithmetic mean of 10 particles.

[0094] ψ=4πS / L 2

[0095] ψ: Sphericity (roundness)

[0096] π: Pi

[0097] S: Cross-sectional area of ​​the particle (the area enclosed by the particle's outline)

[0098] L: The perimeter of the particle (the length of the particle's outline).

[0099] The range of sphericity "ψ" of the electrode active material can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, and 1.0, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy relationships such as "0.1 ≤ ψ ≤ 1.0".

[0100] In the negative electrode film, a negative electrode active material is used as the electrode active material. The negative electrode active material may contain at least one material selected from the group consisting of natural graphite (flake graphite, spherical graphite), artificial graphite, soft carbon, hard carbon, silicon, silicon oxide, silicon-based alloys, silicon-carbon composites "Si-C", lithium silicate, tin, tin oxide, tin-based alloys, and lithium titanate. Spherical graphite may be coated with amorphous carbon, for example. For example, natural graphite, artificial graphite, soft carbon, and hard carbon can be collectively referred to as "carbon-based active materials". Silicon may contain any crystalline phase. Silicon may contain at least one material selected from the group consisting of cage-like type I phase, cage-like type II phase, and diamond phase. Si-C represents composite particles containing at least one of silicon and silicon oxide with carbon. For example, silicon may be loaded into the internal voids of carbon particles. Carbon particles may be graphite particles or amorphous carbon particles. For example, silicon, silicon oxide, silicon-based alloys, and silicon-carbon composites can be collectively referred to as "silicon-based active materials".

[0101] The negative electrode active material can be, for example, a mixture of natural graphite and artificial graphite. The range of the mass ratio "natural graphite:artificial graphite" can be, for example, a range with any two pairs of values ​​selected from the groups consisting of "1:9", "2:8", "3:7", "4:6", "5:5", "6:4", "7:3", "8:2", and "9:1" as endpoints. For example, a mass ratio such as "natural graphite:artificial graphite = 1:9 to 9:1" can be satisfied.

[0102] The negative electrode active material can be, for example, a mixture of carbon-based and silicon-based active materials. The mass ratio of "carbon-based active material: silicon-based active material" can be, for example, a range of any two groups selected from the groups consisting of "1:99", "5:95", "10:90", "20:80", "30:70", "40:60", "50:50", "60:40", "70:30", "80:20", "90:10", "95:5", and "99:1" as endpoints. For example, a mass ratio of "carbon-based active material: silicon-based active material = 1:99 to 99:1" can be satisfied.

[0103] In the positive electrode film, a positive electrode active material is used as the electrode active material. The positive electrode active material may contain at least one compound selected from the group consisting of layered compounds, rock salt compounds, spinel compounds, and olivine compounds. For example, the positive electrode active material may be a mixture of layered compounds and olivine compounds. The range of the mass ratio "layered compound: olivine compound" may, for example, be a range with any two groups selected as endpoints from the group consisting of "1:9", "2:8", "3:7", "4:6", "5:5", "6:4", "7:3", "8:2", and "9:1". For example, a mass ratio relationship such as "layered compound: olivine compound = 1:9 to 9:1" may be satisfied.

[0104] The positive electrode active material may contain at least one material selected from the group consisting of Li(NiCoMn)O2 (layered compound), Li(NiCoAl)O2 (layered compound), LiMnO2 (rock salt compound), Li(NiMn)2O4 (spinel compound), and Li(MnFe)PO4 (olivine compound). It should be noted that the use of terms like (NiCoMn) indicates that the total composition ratio within parentheses is 1. As long as the total is 1, the composition ratio of each component within parentheses can be arbitrary. For example, it is also permissible for some components to have a composition ratio of 0.

[0105] Layered compounds, for example, can have the general formula "Li x Ni a Co b M c O yThe formula represents the composition. The range of "x" in the formula can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, 1.5, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy relationships such as "0.1≦x≦1.5". The formula satisfies the relationship "a+b+c=1". As long as this relationship is satisfied, the ranges of "a", "b", and "c" can be independently obtained by selecting any one value from the group consisting of 0, 0.05, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, each with only an upper or lower limit. This can be a range with upper and lower limits obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy relationships such as "0≦a≦1", "0≦b≦1", "0≦c≦1", etc. Similarly, it can satisfy relationships such as "0.5≦a≦0.9", "0.05≦b≦0.5", "0.05≦c≦0.5", etc. In the formula, "M" can be, for example, a range selected from the group consisting of Mn and A1. One less. The range of "y" in the formula can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, and 2.4, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy relationships such as "1.6 ≦ y ≦ 2.4".

[0106] Layered compounds, for example, can be derived from Li x NiO y Li x CoO y Li x MnO y Li x Ni 1 / 3 Co 1 / 3 Mn 1 / 3 O y Li x Ni 0.4 Co 0.3 Mn 0.3 O y Li x Ni 0.5 Co 0.2 Mn 0.3 O y Li x Ni0.5 Co 0.3 Mn 0.2 O y Li x Ni 0.5 Co 0.4 Mn 0.1 O y Li x Ni 0.5 Co 0.1 Mn 0.4 O y Li x Ni 0.6 Co 0.3 Mn 0.1 O y Li x Ni 0.6 Co 0.2 Mn 0.2 O y Li x Ni 0.6 Co 0.1 Mn 0.3 O y Li x Ni 0.7 Co 0.2 Mn 0.1 O y Li x Ni 0.7 Co 0.1 Mn 0.2 O y Li x Ni 0.8 Co 0.1 Mn 0.1 O y Li x Ni 0.8 Co 0.15 Al 0.05 O y and Li x Ni 0.9 Co 0.05 Mn 0.05 O y The selected group must be at least one of the following. For example, the formula can satisfy relationships such as "0.1≦x≦1.5" and "1.6≦y≦2.4".

[0107] Peridotite-type compounds may, for example, have a composition represented by the general formula "LiMPO4". In the formula, "M" may be at least one selected from the group consisting of Fe, Ni, Co, and Mn.

[0108] Peridotite-type compounds, for example, can have the general formula "Lix Mn 1-a Fe a PO y The formula represents the composition. The range of "x" can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, and 1.5, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not have endpoints. For example, it can satisfy relationships such as "0.1 ≦ x ≦ 1.5". The range of "a" can be, for example, a range obtained by selecting any one value from the group consisting of 0, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, and 1.0. The range of values ​​can be obtained by selecting any two values, which may or may not contain endpoints. For example, it can satisfy relationships such as "0 ≦ a ≦ 1.0" and "0.1 ≦ a ≦ 0.5". Similarly, the range of "y" can be obtained by selecting any value from the group consisting of 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, 4.3, and 4.4, which may or may not contain endpoints. For example, it can satisfy relationships such as "3.6 ≦ y ≦ 4.4".

[0109] Peridotite-type compounds may, for example, contain compounds derived from Li x MnPO y Li x Mn 0.9 Fe 0.1 PO y Li x Mn 0.8 Fe 0.2 PO y Li x Mn 0.7 Fe 0.3 PO y Li x Mn 0.6 Fe 0.4 PO y Li x Mn 0.5 Fe 0.5 PO y Li x Mn 0.4 Fe 0.6 PO y Lix Mn 0.3 Fe 0.7 PO y Li x Mn 0.2 Fe 0.8 PO y Li x Mn 0.1 Fe 0.9 PO y and Li x FePO y The selected group must be at least one of the following. For example, the expression can satisfy relationships such as "0.1≦x≦1.5" and "3.6≦y≦4.4".

[0110] Any dopant can be introduced into the positive electrode active material. The dopant can be interstitial or substitutional. For example, the dopant can include at least one element selected from the group consisting of B, C, N, halogens, Si, Na, Mg, Al, Mn, Co, Cr, Sc, Ti, V, Cu, Zn, Ga, Ge, Se, Sr, Y, Zr, Nb, Mo, In, Pb, Bi, Sb, Sn, W, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, and actinides. The molar fraction (doping amount) of the dopant can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.01%, 0.1%, 1%, 3%, and 5%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The doping amount can range from, for example, 0.01% to 5%.

[0111] (Conductive materials)

[0112] Conductive materials can form electron conduction pathways within the electrode film. Conductive materials may include, for example, at least one material selected from the group consisting of acetylene black, Ketjen black (registered trademark), thermal cracking carbon black, furnace black, carbon fibers, carbon nanotubes, graphene sheets, metal fibers, and metal powders. When the electrode active material is a positive electrode active material, the group of materials constituting the conductive material may further include, for example, natural graphite and artificial graphite.

[0113] The conductive material can be, for example, a powder. The conductive material can have a smaller D50 compared to the electrode active material. The range of the D50 of the conductive material can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.01 μm, 0.05 μm, 0.1 μm, 0.5 μm, 1 μm, 3 μm, and 5 μm, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The D50 range of the conductive material can be, for example, 0.01 μm to 5 μm.

[0114] The range of the mass fraction of conductive material in the electrode film can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9%, and 10%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, the range of the mass fraction of conductive material can be 0% to 10%.

[0115] (Solid electrolyte)

[0116] Solid electrolytes can form ion conduction pathways within the electrode film. Solid electrolytes may include at least one selected from the group consisting of sulfide solid electrolytes, halide solid electrolytes, oxide solid electrolytes, hydride solid electrolytes, and nitride solid electrolytes. Sulfide solid electrolytes may include at least one selected from the group consisting of amorphous phases, crystalline phases, and glass-ceramic phases (crystalline glass). Crystalline phases may include, for example, argentite-germanium sulfide type, LGPS type, etc. Sulfide solid electrolytes may contain, for example, LiI-LiBr-Li3PS4, Li2S-SiS2, LiI-Li2S-SiS2, LiI-Li2S-P2S5, LiI-Li2O-Li2S-P2S5, LiI-Li2S-P2O5, LiI-Li3PO4-P2S5, Li2S-GeS2-P2S5, Li2S-P2S5, Li 10 GeP2S 12 Li4P2S6, Li7P3S 11At least one of the following groups must be selected: LiI, LiBr, and Li7PS6. For example, "LiI-LiBr-Li3PS4" indicates a sulfide solid electrolyte formed by mixing LiI, LiBr, and Li3PS4 in any molar ratio. For example, the sulfide solid electrolyte can be generated by a mechanochemical method. The mixing ratio can be determined by marking numbers before each raw material. For example, "10LiI-15LiBr-75Li3PS4" indicates a mixing ratio (molar ratio) of "LiI:LiBr:Li3PS4=10:15:75".

[0117] Sulfide solid electrolytes can, for example, have a composition represented by the general formula "yLiI-zLiBr-(100-yz)[xLi2S-(1-x)P2S5]". The range of "x" in the formula can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.1, 0.2, 0.25, 0.3, 0.4, 0.5, 0.6, 0.7, 0.75, 0.8, and 0.9, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy relationships such as "0.1≦x≦0.9". The formula also satisfies the relationship "0<100-yz≦100". As long as this relationship is satisfied, the ranges of "y" and "z" can be independently obtained by selecting any one value from the group consisting of 0, 5, 10, 15, 20, 25, and 30, resulting in a range with only an upper or lower limit. Alternatively, they can be obtained by selecting any two values, resulting in a range with both an upper and lower limit. The range may or may not include endpoints. For example, relationships such as "0≦y≦30" and "0≦z≦30" can be satisfied.

[0118] Sulfide solid electrolytes, for example, can have the general formula "Li4-xM 1-x P x S4 represents the composition. The range of "x" in the formula can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 0, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, and 1, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy the relationship "0 < x < 1". "M" in the formula can, for example, contain at least one value selected from the group consisting of Al, Zn, In, Ge, Si, Sn, Sb, Ga, and Bi.

[0119] Sulfide solid electrolytes, for example, can have the general formula "Li 10+x Ge 1+x P 2-xS 12 The formula represents the composition. The range of "x" in the formula can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, and 0.7, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, it can satisfy a relationship such as "0 < x ≤ 0.7". A sulfide solid electrolyte represented by this formula may, for example, contain an LGPS-type crystalline phase.

[0120] Halogenated solid electrolytes, for example, can have the general formula "Li 6-na M a The composition is represented by "X6". In the formula, "n" represents the oxidation number of "M". "M" may, for example, contain atoms with an oxidation number of +3. "M" may, for example, contain atoms with an oxidation number of +4. "M" may, for example, contain at least one element selected from the group consisting of Y, Al, Ti, Zr, Ca, and Mg. For example, it may satisfy the relationship "0 < a < 2". "X" may, for example, contain at least one element selected from the group consisting of F, Cl, Br, and I.

[0121] Solid electrolytes can be, for example, powders. Solid electrolytes can have a smaller D50 compared to electrode active materials. The range of D50 for solid electrolytes can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.01 μm, 0.05 μm, 0.1 μm, 0.5 μm, 1 μm, 3 μm, and 5 μm, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The D50 range of solid electrolytes can be, for example, 0.01 μm to 5 μm.

[0122] The volume fraction of the solid electrolyte in the electrode membrane can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0%, 1%, 5%, 10%, 20%, 30%, 40%, 50%, 60%, and 70%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, the volume fraction of the solid electrolyte can range from 0% to 70%.

[0123] (First adhesive)

[0124] The first binder includes a fibrous binder. The first binder may also be substantially composed of a fibrous binder. The fibrous binder can be fibrillated, for example, by applying shear force to the granular binder (aggregates). For example, by feeding a composite material containing a granular binder to be converted into a fibrous binder and an electrode active material into the roll gap, shear force can be applied to the granular binder. By forming the granular binder into a fibrous binder, an electrode film can be formed. The rolling process can be performed once or repeatedly. Before the rolling process, shear force can be applied to the composite material, for example, by using a jet mill or a mixing granulator. For example, heating to 30°C to 150°C on top of the shear force can promote fibrillation. The granular binder can be completely or partially fibrillated. That is, the first binder may also contain granular components.

[0125] "Fibrous" indicates an aspect ratio (the ratio of the major diameter to the minor diameter) of 10 or higher. Materials with an aspect ratio less than 10 are considered "granular." The aspect ratio (the ratio of fiber length to fiber diameter) of fibrous materials can, for example, be 100 or higher. The minor diameter, major diameter, fiber diameter, and fiber length are determined by microscopy. The aspect ratio is the arithmetic mean of 10 measured samples. The length of the short side of the smallest bounding rectangle "MBR" of the measured sample is considered the minor diameter, and the length of the long side is considered the major diameter. The fiber diameter represents the dimension in the direction orthogonal to the axis of the measured sample. The fiber length represents the total length along the axial direction.

[0126] The fibrous adhesive may, for example, comprise a polymer composition. The polymer composition may be a homopolymer, copolymer, polymer blend, or polymer alloy. The fibrous adhesive may, for example, comprise polytetrafluoroethylene (PTFE). The fibrous adhesive may also contain any additives in addition to PTFE. Additives may include, for example, at least one selected from the group consisting of polyolefins, cellulose, polyethers, and polysiloxanes. The additives and PTFE may form at least one selected from the group consisting of polymer blends, polymer alloys, and copolymers. The range of the mass fraction of PTFE in the fibrous adhesive, or the range of the mass fraction of the tetrafluoroethylene (TFE) derivative, may be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 0%, 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, 95%, 99%, and 100%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The mass fraction of PTFE in fibrous binders can range from, for example, 0% to 100%.

[0127] The number-average molecular weight "Mn" of the polymer constituting the fibrous binder can, for example, be in the range of 10 × 10⁻⁶. 4 50×10 4 100×10 4 150×10 4 200×10 4 300×10 4 400×10 4 500×10 4 1000×10 4 2000×10 4 3000×10 4 The range formed by selecting any one value can be a range with only an upper or lower limit, or a range with both an upper and lower limit can be obtained by selecting any two values. The range may or may not include endpoints. For example, the range for number-average molecular weight could be 10 × 10⁻⁶. 4 ~3000×10 4 Number-average molecular weight can be obtained, for example, from standard specific gravity. Test samples are prepared according to ASTM D-4895 98. Standard specific gravity is determined using the water displacement method according to ASTM D-792.

[0128] The range of fiber diameter (fiber diameter) of the fibrous adhesive can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 1nm, 5nm, 10nm, 15nm, 20nm, 50nm, 100nm, 200nm, 500nm, and 1000nm, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. For example, the fiber diameter range can be 1nm to 1000nm.

[0129] Fibrous binders can form a fibrous matrix. For example, the fibrous matrix can be used to hold the electrode active material (powder) in place, thus maintaining the shape of the electrode membrane. The fibrous matrix can be evaluated, for example, by fiber density. Fiber density can be determined, for example, by the following method: Prepare a cross-sectional SEM image of the electrode membrane. In the cross-sectional SEM image, mark a 20 μm straight line at any location. Calculate the fiber density (unit: strands / 20 μm) by counting the fibrous portions intersecting this line. Measure the fiber density at at least three locations within the cross-sectional SEM image. Use the arithmetic mean of the three or more locations as the fiber density. The range of fiber density can be, for example, a range with only an upper or lower limit obtained by selecting any one value from the group consisting of 1, 2, 5, 10, 20, 40, 60, 80, and 100, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The range of fiber density can be, for example, 1 to 100.

[0130] The range of the mass fraction of the first binder in the electrode film can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9%, and 10%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The range of the mass fraction of the first binder in the electrode film can be, for example, 0.1% to 10%.

[0131] (Second adhesive)

[0132] The form of the second adhesive is arbitrary. For example, the second adhesive can be granular, film-like, fibrous, etc. For example, the second adhesive can have a greater adhesive force than the first adhesive. For example, the electrode film can be fixed to the current collector by the second adhesive. The second adhesive may contain at least one component selected from the group consisting of polyvinylidene fluoride (PVdF), polyvinylidene fluoride-hexafluoropropylene copolymer (PVdF-HFP), carboxymethyl cellulose (CMC), polyacrylic acid (PAA), polyvinyl alcohol (PVA), polyvinylpyrrolidone (PVP), polyethylene oxide (PEO), styrene-butadiene rubber (SBR), nitrile rubber (NBR), polyethylene (PE), polypropylene (PP), polyacrylonitrile (PAN), polyoxyethylene alkyl ether, polyimide (PI), polyamide-imide (PAI), and derivatives thereof.

[0133] The range of the mass fraction of the second binder in the electrode film can be, for example, a range with only an upper or lower limit obtained by selecting any value from the group consisting of 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9%, and 10%, or a range with both an upper and lower limit obtained by selecting any two values. The range may or may not include endpoints. The range of the mass fraction of the second binder in the electrode film can be, for example, 0% to 10%.

[0134] The range of the mass ratio "first adhesive: second adhesive" can be, for example, a range with any two pairs of pairs selected from the groups consisting of "1:9", "2:8", "3:7", "4:6", "5:5", "6:4", "7:3", "8:2", "9:1", and "10:0" as endpoints. For example, a mass ratio of "first adhesive: second adhesive = 1:9 to 10:0" can be satisfied.

[0135] (Added ingredients)

[0136] The electrode film can contain any additives. These additives may include, for example, inorganic fillers, organic fillers, surface modifiers, dispersants, lubricants, flame retardants, protective agents, fluxes, coupling agents, and adsorbents. Other additives may include, for example, polyoxyethylene allyl phenyl ether phosphate, zeolite, silane coupling agents, molybdenum sulfide, and tungsten oxide.

[0137] (Other variations)

[0138] The above description illustrates the case where both the first positive electrode film 13 and the second positive electrode film 14 are composed of self-supporting films, but it is not limited to this. It is also possible that one of the first positive electrode film 13 and the second positive electrode film 14 is composed of a self-supporting film.

[0139] Furthermore, the above description illustrates a case where a positive electrode film is provided on both sides of the positive current collector 11, but it is not limited to this. Alternatively, a positive electrode film may be provided on one side of the positive current collector 11, and a positive electrode composite material layer may be provided on the other side. In this case, the positive electrode composite material layer is formed by coating a slurry, as is conventional.

[0140] Similarly, although the example given is that both the first negative electrode film 23 and the second negative electrode film 24 are composed of self-supporting films, it is not limited to this. It is also possible that one of the first negative electrode film 23 and the second negative electrode film 24 is composed of a self-supporting film.

[0141] Furthermore, the above description illustrates a case where negative electrode films are provided on both sides of the negative electrode current collector 21, but it is not limited to this. Alternatively, a negative electrode film may be provided on one side of the negative electrode current collector 21, and a negative electrode composite material layer may be provided on the other side. In this case, the negative electrode composite material layer can be formed by coating a slurry as in the conventional manner.

[0142] Alternatively, either the positive electrode 10 or the negative electrode 20 can be formed by coating the current collector with a slurry.

[0143] (Postscript)

[0144] As described above, this embodiment includes the following disclosures.

[0145] [Component 1]

[0146] An electrode having:

[0147] Current collector, which extends along its length; and

[0148] An electrode film is disposed on the current collector.

[0149] The electrode membrane comprises active material powder and fibrillated binder.

[0150] The electrode film has a first side attached to the current collector and a second side located on the opposite side of the first side.

[0151] The first surface has a waveform shape formed by repeated peaks and valleys along the length direction.

[0152] When the average interval between the peaks that are adjacent to each other in the length direction is set as P, and the average thickness of the electrode film in the thickness direction orthogonal to the length direction is set as T, the relationship P≦T is satisfied.

[0153] [Component 2]

[0154] According to the electrode described in configuration 1, wherein...

[0155] The second surface is formed to be flat.

[0156] [Component 3]

[0157] According to the electrode configuration described in 1 or 2, wherein,

[0158] Further satisfy the relationship 0.1T≦P.

[0159] [Composition 4]

[0160] According to the electrode constituted in any one of 1 to 3, wherein,

[0161] When the maximum distance between the peak and the valley in the thickness direction is set to RT, the relationship 0.1T≦RT≦0.5T is further satisfied.

[0162] [Component 5]

[0163] According to the electrode constituted in any one of 1 to 4, wherein,

[0164] The current collector has a waveform shape along the first surface.

[0165] [Composition 6]

[0166] According to the electrode constituted in any one of 1 to 5, wherein,

[0167] The electrode membrane is a self-supporting membrane in which the active material powder is held in place by the fibrillated binder.

[0168] [Component 7]

[0169] A secondary battery, comprising:

[0170] An electrode body comprising the electrode as described in any one of 1 to 6; and

[0171] A housing housing that contains the electrode.

[0172] The embodiments of the present invention have been described above, but it should be considered that the embodiments disclosed herein are merely illustrative in all respects and are not restrictive. The scope of the present invention is set forth in the claims and is intended to include all modifications of the same meaning and scope as the claims.

Claims

1. An electrode comprising: Current collector, which extends along its length; and An electrode film is disposed on the current collector. The electrode membrane comprises active material powder and fibrillated binder. The electrode film has a first side attached to the current collector and a second side located on the opposite side of the first side. The first surface has a waveform shape formed by repeated peaks and valleys along the length direction. When the average interval between the peaks that are adjacent to each other in the length direction is set as P, and the average thickness of the electrode film in the thickness direction orthogonal to the length direction is set as T, the relationship P≦T is satisfied.

2. The electrode according to claim 1, wherein, The second surface is flat.

3. The electrode according to claim 1 or 2, wherein, Further satisfy the relationship 0.1T≦P.

4. The electrode according to any one of claims 1 to 3, wherein, When the maximum distance between the peak and the valley in the thickness direction is set to RT, the relationship 0.1T≦RT≦0.5T is further satisfied.

5. The electrode according to any one of claims 1 to 4, wherein, The current collector has a waveform shape along the first surface.

6. The electrode according to any one of claims 1 to 5, wherein, The electrode membrane is a self-supporting membrane in which the active material powder is held in place by the fibrillated binder.

7. A secondary battery, comprising: An electrode body comprising the electrodes of any one of claims 1 to 6; and A housing housing that contains the electrode.

Citation Information

Patent Citations

  • Manufacturing method of non-aqueous secondary battery and manufacturing apparatus of non-aqueous secondary battery

    JP2024140137A