Stabilization adaptive charge-discharge control method for lithium ion battery cathode material under high voltage working condition

By employing segmented current-voltage coordinated regulation and BMS software algorithms, the complex issues of material modification and preparation under high-voltage lithium battery charging and discharging modes are solved, achieving stability and extended lifespan of high-voltage lithium batteries, reducing production costs, and making it suitable for high-voltage lithium battery management systems of 4.4V and above.

CN123073232APending Publication Date: 2026-11-10HARBIN INST OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610933169.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-06-26
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

The existing 4.4V and above high-voltage lithium battery charging and discharging modes result in high production costs, complex cell manufacturing processes, and sacrifice of rate performance and discharge capacity. Furthermore, high-voltage charging leads to high risks of lithium-ion kinetic mismatch, interface polarization accumulation, and lattice mechanical failure, resulting in short battery cycle life and rapid capacity decay.

Method used

A segmented current and voltage coordinated regulation is adopted, including conventional constant current fast charging, gradient slow charging, micro-pulse voltage stabilization passivation, pre-discharge stress buffering, and adaptive correction of cycle health status. The adaptive charge and discharge control of the cathode material is realized through BMS software algorithm, which matches the lithium ion insertion and extraction dynamics, eliminates lattice stress and interface polarization, and avoids instantaneous stress impact during high-power discharge.

Benefits of technology

It significantly improves the stability of the cathode crystal and interface, extends battery cycle life, reduces production costs, is compatible with existing production lines, achieves intelligent adaptive regulation throughout the entire life cycle, and enhances the stability and safety of high-voltage lithium batteries.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123073232A_ABST
    Figure CN123073232A_ABST
Patent Text Reader

Abstract

The application discloses a high-voltage working condition lithium ion battery positive electrode material stabilization self-adaptive charging and discharging control method, relates to a lithium ion battery positive electrode material charging and discharging control method, and aims at solving the technical problems of high production cost, complex cell preparation process, and sacrifice of rate performance and discharging capacity caused by the existing 4.4V and above high-voltage lithium battery charging and discharging mode. The application adopts a segmented current-voltage cooperative regulation to match the positive electrode lithium deintercalation kinetics, and cooperates with pulse depolarization, stress pre-release and full-cycle self-adaptive correction strategies to perform charging and discharging control. The application does not need to change the cell positive electrode material doping coating, electrolyte formula and battery production manufacturing process, and only needs to realize regulation and control through a BMS software algorithm, so that the high-voltage working condition positive electrode crystal structure integrity and electrode interface stability are greatly improved, and the technical problems of high-voltage lithium battery capacity rapid diving, short cycle life and cell bulging expansion are effectively solved. The application can be used for high-voltage positive electrode systems of ternary, lithium cobaltate and lithium-rich manganese-based.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of lithium-ion battery charge and discharge control technology, specifically relating to a method for controlling the charge and discharge of lithium-ion battery cathode materials, adapted to the BMS algorithm control of high-voltage lithium battery management systems with a working voltage of 4.4V and above. Background Technology

[0002] The increasing demand for lithium battery energy density from new energy vehicles, large-scale energy storage, and portable high-end electronic devices has made high-voltage cathode systems the mainstream research and development direction. However, the high-voltage stability of cathode materials is a core technological bottleneck restricting the realization of battery energy density. Currently, the conventional operating cutoff voltage of commercially available ternary NCM and lithium cobalt oxide LCO cells is only 4.2V. To improve single-cell energy density, the industry generally raises the cell charging cutoff voltage to above 4.4V. However, using the existing constant current-constant voltage charging architecture for high-voltage charging has the following drawbacks, leading to a significant reduction in battery cycle life.

[0003] 1. Lithium-ion kinetic mismatch leads to irreversible degradation of the cathode crystal structure.

[0004] After constant current charging reaches the high voltage threshold, it directly enters the continuous constant voltage stage. The positive electrode is in a deep delithiation state, the lithium ion chemical potential increases and the bulk diffusion rate decreases significantly. The constant voltage continuous electric field drives the lithium ions on the positive electrode surface to be rapidly depleted, forming a huge ion concentration difference inside the cell, lattice stress concentration, inducing irreversible phase transition, lattice distortion, and microcracks inside the particles, resulting in permanent capacity loss.

[0005] 2. Continuous accumulation of interfacial polarization exacerbates electrolyte side reactions.

[0006] The existing constant voltage charging method continuously enhances the concentration polarization at the electrode-electrolyte interface. The high voltage polarization potential continuously induces the oxidative decomposition of the electrolyte, generating HF corrosive substances. At the same time, it promotes the dissolution of cobalt, nickel, and manganese transition metal ions, destroys the passivation protective film on the positive electrode surface, and causes the interface impedance to rise continuously, resulting in continuous degradation of battery performance.

[0007] 3. Direct high-power discharge from a fully charged state carries a high risk of lattice mechanical failure.

[0008] When the battery cell is fully charged and under high voltage, the positive electrode lattice is in a stretched metastable state. When high-power discharge is directly turned on, lithium ions are rapidly inserted, and the lattice contracts sharply in an instant. The instantaneous stress impact will cause the positive electrode particles to pulverize and the conductive network to break, resulting in a cliff-like capacity decay. In severe cases, it can induce thermal runaway and bulging of the battery cell.

[0009] Current technical approaches to address high-voltage cathode degradation focus on modifying the cell material, including metal doping, cathode surface coating, and the development of additives for high-voltage electrolytes. However, these solutions are costly to produce, involve complex cell fabrication processes, and generally sacrifice rate performance and discharge capacity. Therefore, there is an urgent need for a charge and discharge control strategy that does not require modification of the cell material, is compatible with existing production lines, and relies on control algorithms to achieve stable operation of the high-voltage cathode. Summary of the Invention

[0010] This invention aims to address the technical problems of high production costs, complex cell fabrication processes, and sacrificed rate performance and discharge capacity associated with existing 4.4V and above high-voltage lithium batteries. It provides an adaptive charge-discharge control method for stabilizing the cathode material of lithium-ion batteries under high-voltage conditions. This method is a purely algorithmic adaptive charge-discharge control approach adaptable to all types of high-voltage cathodes, achieving self-stabilization of the cathode crystal structure through electrochemical dynamic regulation.

[0011] The adaptive charge-discharge control method for stabilizing lithium-ion battery cathode materials under high-voltage conditions of the present invention adopts segmented current-voltage coordinated regulation to match the cathode lithium insertion / extraction dynamics, combined with pulse depolarization, stress pre-release, and full-cycle adaptive correction coordinated strategies, specifically including the following steps:

[0012] S1, Standard Constant Current Fast Charging Stage:

[0013] The battery is charged at a standard rate of 0.5C to 1C using constant current until the voltage of a single cell reaches the first threshold of 4.2V. During this stage, conventional fast charging logic is used to ensure basic charging efficiency.

[0014] S2, High-pressure gradient slow-charging transition stage:

[0015] Within the voltage range of 4.2V to the preset high voltage cutoff voltage, voltage-current coupled gradient slow charging control is adopted; that is, the charging current decreases linearly and stepwise as the cell voltage increases, and the current decreases by 10%~20% for every 0.1V increase in voltage. In this stage, by gradually reducing the charging current density, the lithium-ion diffusion coefficient decreases in the high voltage range, the lithium-ion extraction rate is smoothly controlled, the local ion concentration gradient is eliminated, and the lattice stress concentration and microcrack generation are suppressed from the source.

[0016] S3, High-voltage micro-pulse voltage regulation and passivation stage:

[0017] After the cell voltage reaches the preset high-voltage cutoff voltage, high-frequency micro-charge and micro-discharge alternating pulse voltage regulation control is adopted; that is, the pulse forward micro-charge rate is 0.02C~0.05C, the pulse reverse micro-discharge rate is 0.01C~0.03C, the forward and reverse pulse duty cycle is 1:1; the pulse period is 50ms~200ms, and the total pulse voltage regulation duration is 30s~300s. During this stage, the forward micro-pulse provides the delithiation potential to maintain the cell voltage, and the reverse micro-pulse disturbs the double layer of the electrode interface, breaks the static concentration polarization, realizes the dynamic homogenization of the lithium ion concentration at the interface, reduces the interface overpotential, blocks the continuous oxidation reaction of the electrolyte, and realizes long-term passivation protection of the positive electrode interface; at the same time, the pulse interval is used to promote the homogenization of lithium ion diffusion at the interface.

[0018] S4, Pre-discharge stress buffering stage:

[0019] After the high-voltage micro-pulse voltage regulation and passivation stage is completed, a short-term low-rate pre-discharge is first performed, and then normal continuous discharge is entered at the preset working rate to reach the discharge termination condition. In this stage, high-power discharge is not directly output. Low-rate lithium ions are slowly inserted into the stretched lattice, driving the lattice to relax slowly, releasing the internal tensile stress accumulated during the charging process, and transitioning the lattice from the metastable state to the stable state, avoiding particle pulverization caused by the instantaneous stress impact of high-power discharge.

[0020] S5. Determine whether the number of cycles has reached the preset number of detection cycles;

[0021] If not, increment the cycle count by 1, and control the cell to enter the static stabilization stage, then return to step S1 to repeat the cycle; in this step, static stabilization is used to eliminate concentration polarization and ohmic polarization generated during the discharge process, ensuring the accuracy of battery health parameter acquisition in subsequent stages.

[0022] If so, execute S6;

[0023] S6, Cyclic Adaptive Correction Phase:

[0024] Build a closed-loop feedback control logic based on the state of health (SOH) of the battery; monitor the cell internal resistance, available capacity, open circuit voltage (OCV) and polarization voltage in real time, and perform a health status assessment.

[0025] Determine if the battery has reached a health threshold; the health threshold is an increase in internal resistance exceeding 5% or a capacity decay exceeding 3% in a single cycle.

[0026] If not, return to step S1;

[0027] If so, reduce the current decay gradient in S2 and increase the reverse pulse duration in S3 to adapt to the polarization increment caused by cell aging and ensure the high-voltage operation stability of the battery throughout its entire life cycle.

[0028] S7. Determine if the battery has reached its full lifespan. If not, return to S1; if yes, end.

[0029] Furthermore, the short-time low-rate pre-discharge described in S4 has a rate of 0.05C to 0.1C and a pre-discharge duration of 3s to 10s.

[0030] Furthermore, the preset operating rate described in S4 is 0.2C to 2C.

[0031] Furthermore, the discharge termination condition described in S4 is either a voltage cutoff criterion, using the cell's rated discharge cutoff voltage as a benchmark, or a threshold value that is reached to terminate the discharge, thus avoiding deep over-discharge damage to the positive electrode lattice and negative electrode current collector; or a capacity cutoff criterion, using the difference between the charged capacity and the discharged capacity to verify the discharge depth, eliminating cutoff misjudgments caused by voltage polarization; or a protection cutoff criterion, using the lowest single-cell voltage as a trigger condition to address the risk of localized over-discharge caused by cell consistency deviations; the discharge termination condition precisely defines the boundary of a single complete charge-discharge cycle.

[0032] Furthermore, the preset number of detection cycles mentioned in step S5 is 5 to 20 times.

[0033] Furthermore, the stabilization process described in step S5 involves: after a single charge-discharge cycle, the cell is placed in an open-circuit, no-load state and left to stand for 30 to 120 seconds. During this stabilization period, concentration polarization and ohmic polarization within the cell gradually subside, the lithium-ion concentration distribution becomes uniform, and the terminal voltage drops back to a stable open-circuit voltage (OCV). This ensures the accuracy of subsequent testing of health parameters such as internal resistance and capacity, and avoids interference from polarization voltage in the test results.

[0034] Furthermore, the reduction of the current decay gradient in S2 described in step S6 is to increase the current decay amount corresponding to every 0.1V increase in voltage by 10% to 20%.

[0035] Furthermore, the step S6, which involves increasing the reverse pulse duration and duty cycle in S3, involves keeping the forward pulse duration constant while increasing the reverse pulse duration by 20% to 50%. This enhances the interface depolarization effect and counteracts the polarization increment caused by aging.

[0036] This invention discloses an adaptive charge-discharge control method for stabilizing cathode materials under high-voltage conditions, belonging to the field of lithium-ion battery charge-discharge management and control technology. Addressing the shortcomings of existing 4.4V and above high-voltage lithium batteries that utilize the traditional constant-current-constant-voltage charging architecture, such as lithium-ion diffusion kinetic mismatch during deep delithiation leading to cathode lattice distortion, particle collapse, concentration polarization accumulation at the electrode interface, continuous electrolyte oxidation side reactions, lattice stress overload and pulverization during discharge, and excessively rapid battery cycle degradation, this invention constructs a four-in-one collaborative control strategy: segmented gradient slow charging, high-voltage high-frequency micro-pulse voltage stabilization and passivation, pre-discharge lattice stress buffering, and adaptive closed-loop correction of cycle health status.

[0037] This invention employs voltage-coupled linear stepped decay current charging within the 4.2V to high-voltage cutoff voltage range to match the positive electrode delithiation kinetics and mitigate lattice stress. It abandons the traditional continuous constant-voltage stabilization method, instead using alternating positive and negative high-frequency micro-pulse dynamic clamping voltage to continuously disturb the ion concentration gradient at the electrode interface, eliminating polarization accumulation and suppressing electrolyte decomposition and transition metal dissolution. After full-charge stabilization, a low-rate short-time pre-discharge process is added to controllably release residual lattice tensile stress and avoid instantaneous stress impacts during high-power discharge. Based on battery internal resistance and capacity decay data, a full-lifecycle adaptive parameter correction mechanism is established to dynamically optimize control parameters at each stage as the battery ages. This invention requires no modification to the cell's positive electrode material doping and coating, electrolyte formulation, or battery manufacturing process; it achieves control solely through BMS software algorithms, significantly improving the integrity of the positive electrode crystal structure and the stability of the electrode interface under high-voltage conditions. It effectively solves industry pain points such as rapid capacity drop, short cycle life, and cell bulging in high-voltage lithium batteries, and is compatible with various high-voltage positive electrode systems, including ternary, lithium cobalt oxide, and lithium-rich manganese-based systems.

[0038] Compared with existing traditional constant current and constant voltage charging solutions and material modification solutions, this invention has four core advantages:

[0039] 1. Significantly improves the stability of the cathode crystal and interface.

[0040] Gradient slow charging matches the delithiation kinetics, and micro-pulses continuously eliminate interface polarization, simultaneously solving the two core problems of high-voltage charging body response force and interface side reactions; actual tests show that after 1000 cycles at 4.5V high voltage in NCM622 cells, the positive electrode particles remain intact without large-area microcracks, and the amount of transition metal dissolution is reduced by more than 60%.

[0041] 2. Significantly extends the cycle life of high-voltage battery cells

[0042] Pre-discharge stress buffering eliminates mechanical damage from high-power discharge, and the capacity retention rate can reach 82% after 1000 cycles under 4.5V high voltage; the traditional constant current and constant voltage solution only achieves 58%, and the cell thickness expansion rate is controlled within 5%, solving the pain point of high-voltage cell bulging failure.

[0043] 3. Low cost of industrialization and strong compatibility

[0044] This invention relies solely on the built-in software algorithm of the BMS, requiring no changes to the cathode material, electrolyte formulation, or cell manufacturing process. It is compatible with all existing high-voltage lithium battery production lines, has extremely low marginal modification costs, and can be rapidly applied in large quantities.

[0045] 4. Intelligent adaptive regulation throughout the entire life cycle

[0046] It features a built-in closed-loop correction mechanism for cyclic health, which dynamically optimizes control parameters at each stage as the battery cell ages. This avoids the accelerated degradation caused by fixed control parameters in the later stages of battery life, maintaining optimal charge and discharge control throughout the entire lifecycle. It can be used for BMS algorithm control in high-voltage lithium battery management systems with operating voltages of 4.4V and above. Attached Figure Description

[0047] Figure 1 This is a schematic diagram of the complete process of the overall charging and discharging control method of the present invention;

[0048] Figure 2 This is a schematic diagram of the current-voltage change curve during the S2 high-voltage gradient slow charging stage in Example 1.

[0049] Figure 3 This is a schematic diagram of the voltage and current waveforms of the S3 high-frequency micro-pulse regulated voltage in Example 1;

[0050] Figure 4 A photograph of the battery in Example 1 after 1000 charge-discharge cycles;

[0051] Figure 5 A photo of the battery in Comparative Example 1 after 500 charge-discharge cycles showing battery bulging.

[0052] Figure 6 This is a graph comparing the 4.5V high-voltage cycling performance of Example 1 and Comparative Example 1.

[0053] Figure 7 This is a schematic diagram of the adaptive charge-discharge data curves of the lithium cobalt oxide system in Example 2;

[0054] Figure 8 This is a schematic diagram of the adaptive charge-discharge data curves of the ternary lithium system in Example 3. Detailed Implementation

[0055] To clearly illustrate the technical solution of the present invention, the present invention will be described in detail below with reference to preferred embodiments. The embodiments are only used to explain the present invention and do not limit the scope of protection of the present invention.

[0056] Example 1: This example uses a commercial NCM622 / graphite system 5Ah soft-pack lithium battery as an example to illustrate the stabilization adaptive charge and discharge control method under high voltage conditions, which is carried out according to the following steps.

[0057] S1, Standard Constant Current Fast Charging Stage:

[0058] The standard 1C constant current charging rate is used until the soft-pack lithium battery voltage reaches the first threshold of 4.2V.

[0059] S2, High-pressure gradient slow-charging transition stage:

[0060] Within the 4.2V to 4.5V range, voltage-current coupled gradient slow-charge control is adopted; that is, the charging current decreases linearly in a stepwise manner as the cell voltage increases, with a corresponding current decrease of 15% for every 0.1V increase in voltage. A schematic diagram of the current-voltage change curve during the high-voltage gradient slow-charge stage is shown below. Figure 2 As shown;

[0061] S3, High-voltage micro-pulse voltage regulation and passivation stage:

[0062] After the cell voltage reaches 4.5V, high-frequency micro-charge and micro-discharge alternating pulse voltage regulation control is adopted; that is, the pulse forward micro-charge rate is 0.03C, the pulse reverse micro-discharge rate is 0.02C, the forward and reverse pulse duty cycle is P:N=1:1; the pulse period is 100ms, and the total pulse regulation duration is 120s; the high-frequency micro-pulse regulated voltage and current waveform diagram is shown below. Figure 3 As shown;

[0063] S4, Pre-discharge stress buffering stage:

[0064] After the high-voltage micro-pulse voltage regulation and passivation stage is completed, a 5-second pre-discharge buffer is first applied at a low rate of 0.05C, and then normal continuous discharge is initiated at a rate of 1C to reach a voltage of 2.8V.

[0065] S5. Determine whether the number of cycles has reached the preset detection cycle number of 10 times;

[0066] If not, increment the cycle count by 1, and control the battery cell to enter a resting state for 60 seconds, then return to step S1 to repeat the cycle;

[0067] If so, execute S6;

[0068] S6, Cyclic Adaptive Correction Phase:

[0069] Build a closed-loop feedback control logic based on the battery's state of health (SOH); monitor the core parameters of cell internal resistance and available capacity in real time and perform health status assessment.

[0070] Determine if the battery has reached a health threshold; the health threshold is an increase in internal resistance exceeding 5%.

[0071] If not, return to step S1;

[0072] If so, reduce the current decay gradient in S2, that is, increase the current decay by 20% for every 0.1V increase in voltage; keep the positive pulse duration unchanged in S3, and increase the reverse pulse duration by 20%.

[0073] S7. Determine if the battery has reached its full lifespan. If not, return to step S1; if yes, end.

[0074] The charge-discharge test in Example 1 was conducted at an ambient temperature of 25±2℃. After 1000 cycles, the cell capacity retention rate was 82%. SEM analysis of the cell revealed no obvious microcracks on the positive electrode, the electrolyte decomposition products were significantly less than in traditional methods, and the cell thickness expansion rate was only 4.2%. Figure 4 As shown, it has excellent safety performance.

[0075] Comparative Example 1: This comparative example uses a commercially available NCM622 / graphite system 5Ah soft-pack lithium battery as the test object and adopts a traditional charging scheme, specifically: 1C constant current charging to 4.5V, continuous constant voltage charging until the charging current is 0.05C, after charging is completed, 1C constant current discharging is used until the cell voltage reaches 2.8V, completing a single charge-discharge cycle; 1000 charge-discharge cycles are performed according to this charge-discharge cycle.

[0076] Test results: After 500 cycles at 4.5V high voltage, the capacity retention rate was only 58%, and the cells showed obvious bulging and expansion. Figure 5 As shown, SEM electron microscopy revealed large-area cracking and pulverization of the positive electrode particles, and severe decomposition of the electrolyte.

[0077] The high-pressure cycling performance comparison curves of Example 1 and Comparative Example 1 are shown in the figure below. Figure 6 As shown, from Figure 6 As can be seen, the battery cell using the control scheme of Example 1 exhibits a significantly slower capacity decay rate during 4.5V high-voltage cycling, maintaining a capacity retention rate of 82% after 1000 cycles, with a stable decay trend throughout. In contrast, the battery cell using the traditional constant current and constant voltage scheme experiences rapid capacity decay, with the capacity retention rate dropping to 58% after only 500 cycles, and subsequent decay accelerating further, resulting in bulging failure around 500 cycles. This comparison fully demonstrates that the method of Example 1 can significantly improve the cycle life and capacity stability of high-voltage lithium batteries, effectively suppressing the capacity drop problem under high-voltage conditions.

[0078] Example 2: The test object in this example is a lithium cobalt oxide LCO / graphite system lithium battery. The stabilization adaptive charge and discharge control method under high voltage conditions is carried out according to the following steps:

[0079] S1, Standard Constant Current Fast Charging Stage:

[0080] The standard constant current charging rate of 0.7C is used until the soft-pack lithium battery voltage reaches the first threshold of 4.2V;

[0081] S2, High-pressure gradient slow-charging transition stage:

[0082] Within the range of 4.2V to 4.45V, voltage-current coupled gradient slow charging control is adopted; that is, the charging current decreases linearly in a stepwise manner as the cell voltage increases, with a corresponding current decrease of 12% for every 0.1V increase in voltage.

[0083] S3, High-voltage micro-pulse voltage regulation and passivation stage:

[0084] After the cell voltage reaches 4.45V, high-frequency micro-charging and micro-discharging alternating pulse voltage regulation control is adopted; that is, the pulse forward micro-charging rate is 0.02C, the pulse reverse micro-discharging rate is 0.01C, the forward and reverse pulse duty cycle is P:N=1:1; the pulse period is 80ms, and the total pulse voltage regulation duration is 150s.

[0085] S4, Pre-discharge stress buffering stage:

[0086] After the high-voltage micro-pulse voltage regulation and passivation stage is completed, it is first pre-discharged at a small rate of 0.08C for 3 seconds, and then enters normal continuous discharge at a rate of 0.5C to reach a voltage of 2.75V.

[0087] S5. Determine whether the number of cycles has reached the preset detection cycle number of 10 times;

[0088] If not, increment the cycle count by 1, and control the battery cell to enter a resting state for 90 seconds, then return to step S1 to repeat the cycle;

[0089] If so, execute S6;

[0090] S6, Cyclic Adaptive Correction Phase:

[0091] Build a closed-loop feedback control logic based on the battery's state of health (SOH); monitor the core parameters of cell internal resistance and available capacity in real time and perform health status assessment.

[0092] Determine if the battery has reached its health threshold; the health threshold is 2% of the rated capacity.

[0093] If not, return to step S1;

[0094] If so, reduce the current decay gradient in S2, that is, increase the current decay by 25% for every 0.1V increase in voltage; keep the positive pulse duration unchanged in S3, and increase the reverse pulse duration by 20%.

[0095] S7. Determine if the battery has reached its full lifespan. If not, return to step S1; if yes, end.

[0096] Figure 7 The graph shows the adaptive charge-discharge data curves of the lithium cobalt oxide system in Example 2. After 800 cycles at a high voltage of 4.45V, the cell capacity retention rate was 78%, the internal resistance increased slowly throughout the cycle, and there was no cell swelling or lithium plating.

[0097] Example 3: This example uses a commercially available NCM811 / graphite ternary soft-pack lithium battery as the test object. The stabilization and adaptive charge / discharge control method under high voltage conditions is carried out according to the following steps:

[0098] S1, Standard Constant Current Fast Charging Stage:

[0099] The standard constant current charging rate of 0.8C is used until the soft-pack lithium battery voltage reaches the first threshold of 4.2V;

[0100] S2, High-pressure gradient slow-charging transition stage:

[0101] Within the range of 4.2V to 4.48V, voltage-current coupled gradient slow charging control is adopted; that is, the charging current decreases linearly in a stepwise manner as the cell voltage increases, and the current decreases by A=18% for every 0.1V increase in voltage.

[0102] S3, High-voltage micro-pulse voltage regulation and passivation stage:

[0103] After the cell voltage reaches 4.48V, high-frequency micro-charging and micro-discharging alternating pulse voltage regulation control is adopted; that is, the pulse forward micro-charging rate is 0.04C, the pulse reverse micro-discharging rate is 0.025C, the forward and reverse pulse duty cycle is P:N=1:1; the pulse period is 120ms, and the total duration of pulse voltage regulation is 180s.

[0104] S4, Pre-discharge stress buffering stage:

[0105] After the high-voltage micro-pulse voltage regulation and passivation stage is completed, it is first pre-discharged at a small rate of 0.06C for 8 seconds, and then enters normal continuous discharge at a rate of 1C to reach a voltage of 2.75V.

[0106] S5. Determine whether the number of cycles has reached the preset detection cycle number of 10 times;

[0107] If not, increment the cycle count by 1, and control the battery cell to enter a resting state for 90 seconds, then return to step S1 to repeat the cycle;

[0108] If so, execute S6;

[0109] S6, Cyclic Adaptive Correction Phase:

[0110] Build a closed-loop feedback control logic based on the battery's state of health (SOH); monitor the core parameters of cell internal resistance and available capacity in real time and perform health status assessment.

[0111] Determine if the battery has reached a health threshold; the health threshold is an internal resistance increase of ≥5%.

[0112] If not, return to step S1;

[0113] If so, reduce the current decay gradient in S2, that is, for every 0.1V increase in voltage, the corresponding current decay increases by 11%; keep the positive pulse duration in S3 unchanged, and increase the reverse pulse duration by 30%;

[0114] S7. Determine if the battery has reached its full lifespan. If not, return to step S1; if yes, end.

[0115] Figure 8 This is a graph showing the adaptive charge-discharge data of the ternary lithium system in Example 3. This ternary lithium battery, after 900 cycles at 4.48V, maintains 80% of its cell capacity. During cycling, the internal resistance increases steadily, with no significant swelling or lithium plating. Its high-voltage cycling stability is significantly better than traditional constant-current, constant-voltage solutions.

Claims

1. A method for adaptive charge-discharge control of lithium-ion battery cathode material stabilization under high-voltage conditions, characterized in that, The method includes the following steps: S1, Standard Constant Current Fast Charging Stage: The battery is charged using a standard constant current rate of 0.5C to 1C until the voltage of a single cell reaches the first threshold of 4.2V. S2, High-pressure gradient slow-charging transition stage: Within the voltage range of 4.2V to the preset high-voltage cutoff voltage, voltage-current coupled gradient slow charging control is adopted; that is, the charging current decreases linearly and stepwise as the cell voltage increases, with the current decreasing by 10% to 20% for every 0.1V increase in voltage. S3, High-voltage micro-pulse voltage regulation and passivation stage: After the cell voltage reaches the preset high voltage cutoff voltage, high-frequency micro-charging and micro-discharging alternating pulse voltage regulation control is adopted; that is, the pulse forward micro-charging rate is 0.02C~0.05C, the pulse reverse micro-discharging rate is 0.01C~0.03C, the forward and reverse pulse duty cycle is 1:1; the pulse period is 50ms~200ms, and the total pulse voltage regulation duration is 30s~300s. S4, Pre-discharge stress buffering stage: After the high-voltage micro-pulse voltage regulation and passivation stage is completed, a short-term low-rate pre-discharge is first performed, and then normal continuous discharge is performed at the preset working rate to reach the discharge termination condition. S5. Determine whether the number of cycles has reached the preset number of detection cycles; If not, increment the cycle count by 1, and control the cell to enter the static stabilization stage, then return to step S1 to repeat the cycle; if yes, execute S6. S6, Cyclic Adaptive Correction Phase: Build a closed-loop feedback control logic based on the battery state of health (SOH); monitor the core parameters of cell internal resistance and available capacity in real time and perform health status assessment. Determine if the battery has reached a health threshold; The health threshold is an increase in internal resistance ≥ 5% or a single cycle capacity decay ≥ 3%; if not, return to step S1; If so, reduce the current decay gradient in S2 and increase the reverse pulse duration in S3; S7. Determine if the battery has reached its full lifespan. If not, return to S1; if yes, end.

2. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high voltage conditions according to claim 1, characterized in that, The short-time low-rate pre-discharge described in S4 has a rate of 0.05C to 0.1C and a pre-discharge duration of 3s to 10s.

3. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high voltage conditions according to claim 1 or 2, characterized in that, The preset operating rate described in S4 is 0.2C to 2C.

4. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high-voltage conditions according to claim 1 or 2, characterized in that, The discharge termination condition described in S4 is either a voltage cutoff criterion, which uses the rated discharge cutoff voltage of the cell as a benchmark and terminates the discharge when the threshold is reached; or a capacity cutoff criterion, which verifies the depth of discharge by the difference between the charged capacity and the discharged capacity; or a protection cutoff criterion, which uses the lowest single-cell voltage as the trigger condition.

5. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high voltage conditions according to claim 1 or 2, characterized in that, The preset number of detection cycles mentioned in step S5 is 5 to 20 times.

6. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high voltage conditions according to claim 1 or 2, characterized in that, The static stabilization mentioned in step S5 is: after a single charge-discharge cycle, the battery cell is placed in an open-circuit, no-load state and left to stand for 30s to 120s.

7. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high-voltage conditions according to claim 1 or 2, characterized in that, The reduction of the current decay gradient in S2 mentioned in step S6 is to increase the current decay amount by 10% to 25% for every 0.1V increase in voltage.

8. The adaptive charge-discharge control method for stabilizing the cathode material of a lithium-ion battery under high voltage conditions according to claim 1 or 2, characterized in that, The step S6 described in increasing the reverse pulse duration and pulse duty cycle in S3 is to keep the forward pulse duration unchanged and increase the reverse pulse duration by 20% to 50%.