Semiconductor structure and its manufacturing method, electronic equipment

By covering the MTJ structure with a spin transition layer and a torque functional layer, the high manufacturing difficulty of bottom pinning and top SOT track MRAM structures is solved, improving spin current transfer or conversion efficiency and enhancing device performance.

CN123076173APending Publication Date: 2026-11-10BEIJING SUPERSTRING ACAD OF MEMORY TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510600588.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-09
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

The MRAM structure with bottom pins and top SOT tracks is difficult to manufacture and makes it hard to guarantee device performance.

Method used

A spin transition layer is covered on the MTJ structure, and a torque functional layer is covered on top of the spin transition layer. Spin current or orbital current is generated through the action of electric current to enhance the spin transfer torque. The spin transition layer is used to transfer the spin current or convert the orbital current into spin current.

Benefits of technology

It improves the efficiency of spin current transfer or conversion, thereby enhancing device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076173A_ABST
    Figure CN123076173A_ABST
Patent Text Reader

Abstract

This disclosure provides a semiconductor structure, a method for manufacturing the same, and an electronic device. The semiconductor structure includes: a substrate structure; an MTJ structure stacked on the substrate structure; a spin transition layer covering the top of the MTJ structure; a torque functional layer at least partially covering the surface of the spin transition layer; a first electrode and a second electrode located on opposite sides of the stack of the MTJ structure and the spin transition layer; the torque functional layer is electrically connected to the first electrode and the second electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to, but is not limited to, the field of semiconductor manufacturing, specifically to a semiconductor structure and its manufacturing method, and an electronic device. Background Technology

[0002] With the development of integrated circuit technology, applications such as autonomous driving, precision medical diagnosis, and satellite image recognition require a new generation of memory that is faster, more stable, and consumes less power. Memory based on SOT-MRAM (Spin Orbit Torque-Magnetoresistive Random Access Memory) is a strong contender for this new type of memory. Compared to traditional top-pinned SOT-MRAM structures, bottom-pinned, top-SOT-tracked MRAM structures offer advantages such as less metal sputtering during etching and higher thermal stability of the pinned layers. However, the bottom-pinned, top-SOT-tracked MRAM structure is more difficult to manufacture, making it challenging to guarantee device performance. Summary of the Invention

[0003] In view of the above, embodiments of the present disclosure provide a semiconductor structure, a method for manufacturing the same, and an electronic device.

[0004] On one hand, embodiments of this disclosure provide a semiconductor structure, including:

[0005] Substrate structure;

[0006] An MTJ (Magnetic Tunnel Junction) structure stacked on the substrate structure;

[0007] A spin transition layer covering the top of the MTJ structure;

[0008] A torque functional layer that at least partially covers the surface of the spin transition layer;

[0009] The first electrode and the second electrode are located on both sides of the stack of the MTJ structure and the spin transition layer; the torque functional layer is electrically connected to the first electrode and the second electrode.

[0010] In some embodiments, the torque functional layer includes a first type of material for providing spin flow;

[0011] The spin transition layer includes a second type of material for transmitting the spin flow.

[0012] In some embodiments, the first type of material includes: a heavy metal material having a spin-orbit coupling effect;

[0013] The second type of material includes materials whose spin diffusion length is greater than a preset first threshold.

[0014] In some embodiments, the torque functional layer includes a third type of material for providing orbital flow;

[0015] The spin transition layer includes a fourth type of material for converting the orbital flow into a spin flow.

[0016] In some embodiments, the third type of material includes: a material exhibiting the orbital Hall effect;

[0017] The fourth category of materials includes heavy metal materials with spin-orbit coupling effects.

[0018] In some embodiments, the MTJ structure includes: a buffer layer, a fixing layer, an isolation layer, and a free layer stacked sequentially;

[0019] The free layer is in contact with the spin transition layer; the buffer layer is in contact with the substrate structure.

[0020] In some embodiments, the semiconductor structure further includes:

[0021] A protective layer covering at least the stacked sidewalls of the MTJ structure and the spin transition layer;

[0022] The torque functional layer covers the surface of the top of the spin transition layer and the protective layer.

[0023] In some embodiments, the substrate structure includes:

[0024] Substrate;

[0025] A first bottom electrode that penetrates the substrate and is electrically connected to the first electrode;

[0026] A second bottom electrode that penetrates the substrate and is electrically connected to the bottom of the MTJ structure.

[0027] In some embodiments, the semiconductor structure further includes:

[0028] A filling layer located in at least a portion of the region outside the stack of the MTJ structure and the spin transition layer;

[0029] The first electrode and the second electrode are disposed within the filling layer;

[0030] The filling layer has an interconnection structure connecting the first electrode and the first bottom electrode.

[0031] In some embodiments, the semiconductor structure further includes a source line electrically connected to the second electrode.

[0032] On the other hand, embodiments of this disclosure also provide a method for manufacturing a semiconductor structure, including:

[0033] Provide the base structure;

[0034] A stack of an MTJ structure and a spin transition layer is formed on the substrate structure; wherein the spin transition layer covers the top of the MTJ structure;

[0035] A first electrode and a second electrode are formed on both sides of the stack of the MTJ structure and the spin transition layer;

[0036] A torque functional layer is formed covering the surfaces of the first electrode, the second electrode, and the spin transition layer; wherein the torque functional layer is electrically connected to the first electrode and the second electrode.

[0037] In some embodiments, the stack of the MTJ structure and the spin transition layer formed on the substrate structure includes:

[0038] A buffer material layer, a fixing layer, an isolation material layer, a free material layer, and a spin transition material layer are sequentially stacked on the substrate structure.

[0039] An etch stop material layer is placed on top of the spin transition material layer; wherein the etch stop layer is an oxide material.

[0040] A mask layer is applied to the surface of the etching stop layer;

[0041] The patterned mask layer is etched to form a stack of the MTJ structure and the spin transition layer located within a predetermined region.

[0042] In some embodiments, the method further includes:

[0043] A protective layer is formed that at least covers the sidewalls of the stack and the remaining mask layer on top;

[0044] A filler layer is formed in the area outside the protective layer;

[0045] A source line is formed within the filling layer.

[0046] In some embodiments, the first and second electrodes formed on both sides of the stack of the MTJ structure and the spin transition layer include:

[0047] A first recessed structure and a second recessed structure are formed within the filler layer on both sides of the stack; wherein at least a portion of the surface of the source line is exposed to the first recessed structure; and at least a portion of the surface of the first bottom electrode located in the substrate structure is exposed to the second recessed structure.

[0048] Conductive material is filled into the first recessed structure and the second recessed structure to form the first electrode and the second electrode.

[0049] In some embodiments, prior to forming a torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer, the method further includes:

[0050] The remaining mask layer on top of the stack and the protective layer on the surface of the mask layer are removed by a first etching process;

[0051] The etching stop layer is removed by a second etching process to expose the surface of the spin transition layer.

[0052] In some embodiments, removing the remaining mask layer on top of the stack and the protective layer on the surface of the mask layer by a first etching process includes:

[0053] Based on a preset polishing rate ratio between the conductive material and the filling layer material, the protective layer, the conductive material, and the mask layer on the top of the stack are subjected to CMP (Chemical Mechanical Polishing) treatment until the etching stop layer is exposed; wherein, after the CMP treatment, the etching stop layer protrudes from the surface of the conductive material.

[0054] In some embodiments, removing the etch stop layer by a second etching process to expose the surface of the spin transition layer includes:

[0055] The etching stop layer is removed by wet etching, making the conductive material flush with the surface of the spin transition layer.

[0056] In some embodiments, forming a torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer includes:

[0057] The torque functional layer is formed on the plane containing the first electrode, the second electrode, and the spin transition layer using a PVD (Physical Vapor Deposition) process.

[0058] In some embodiments, removing the remaining mask layer on top of the stack and the protective layer on the surface of the mask layer by a first etching process includes:

[0059] The remaining mask layer on top of the stack and the protective layer on the surface of the mask layer are removed using a dry etching process until the etching stop layer is exposed; wherein, after the dry etching process, the surface of the etching stop layer is recessed into the surface of the conductive material.

[0060] In some embodiments, removing the etch stop layer by a second etching process to expose the surface of the spin transition layer includes:

[0061] The etching stop layer is removed by wet etching, exposing the spin transition layer, and the surface of the spin transition layer is recessed into the surface of the conductive material.

[0062] In some embodiments, forming a torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer includes:

[0063] The torque functional layer is formed on the surfaces of the first electrode, the second electrode, and the spin transition layer using either CVD (Chemical Vapor Deposition) or ALD (Atomic Layer Deposition) processes.

[0064] In some embodiments, the method further includes:

[0065] The torque functional layer is graphically represented, and at least the torque functional layer that is in contact with the first electrode, the second electrode, and the spin transition layer is retained.

[0066] At least a portion of the region outside the graphical torque functional layer is filled with a dielectric layer.

[0067] In some embodiments, the provision of the substrate structure includes:

[0068] Provide substrate;

[0069] A first bottom electrode and a second bottom electrode are formed through the substrate; wherein the first bottom electrode is used for electrical connection with the first electrode; and the second bottom electrode is used for electrical connection with the bottom of the MTJ structure.

[0070] On the other hand, an electronic device according to an embodiment of the present disclosure includes at least one of the above-described semiconductor structures, or includes at least one semiconductor structure formed by any of the above-described manufacturing methods.

[0071] This disclosure provides a bottom-pinned MRAM structure, which covers an MTJ structure with a spin transition layer and a torque functional layer on top of the spin transition layer for connecting electrodes. The torque functional layer can generate orbital current or spin current under the influence of current between the first and second electrodes, used to generate spin-transfer torque (STT) or spin-orbit torque (SOT); while the spin transition layer can be used to transfer spin current or convert orbital current into spin current to promote the generation of torque from the spin current. Therefore, by combining the spin transition layer and the torque functional layer, better spin current transfer or conversion efficiency is achieved, thereby enhancing device performance. Attached Figure Description

[0072] Figure 1 A schematic diagram of a semiconductor structure provided in an embodiment of this disclosure;

[0073] Figure 2 A schematic diagram of a semiconductor structure provided in an embodiment of this disclosure;

[0074] Figure 3 A flowchart illustrating a method for manufacturing a semiconductor structure according to an embodiment of this disclosure;

[0075] Figures 4 to 17 A schematic diagram of the structure corresponding to each step in the manufacturing method provided in the embodiments of this disclosure;

[0076] Figure 18 This is a structural block diagram of an electronic device provided in an embodiment of the present disclosure.

[0077] Figure label:

[0078] Semiconductor structure-100; Substrate structure-110; Substrate-111; First bottom electrode-112; Second bottom electrode-113; MTJ structure-120; Buffer layer-121; Buffer material layer-121a; Fixing layer-122; Fixing material layer-122a; Isolation layer-123; Isolation material layer-123a; Free layer-124; Free material layer-124a; Spin transition layer-130; Spin transition material layer-130a; Torque functional layer-140; First electrode-150; Second electrode-160; Protective layer-210; Filling layer-220; First recessed structure-221; Second recessed structure-222; Source line-230; Etch stop layer-410; Etch stop material layer-410a; Mask layer-420; Electronic device-300; Memory-310; Processor-320. Detailed Implementation

[0079] The technical solutions of this disclosure will be further described in detail below with reference to the accompanying drawings and embodiments. Although exemplary embodiments of this disclosure are shown in the drawings, it should be understood that this disclosure can be implemented in various forms and should not be limited to the embodiments described herein. Rather, these embodiments are provided to enable a more thorough understanding of this disclosure and to fully convey the scope of this disclosure to those skilled in the art.

[0080] The present disclosure is described in more detail below by way of example with reference to the accompanying drawings. The advantages and features of the present disclosure will become clearer from the following description and claims. It should be noted that the drawings are in a very simplified form and use non-precise proportions, and are only used to facilitate and clarify the illustration of the embodiments of the present disclosure.

[0081] In this disclosure, the terms "first," "second," etc., are used to distinguish similar objects, and not to describe a specific order, sequence, quantity, or importance.

[0082] In the embodiments of this disclosure, terms such as "middle," "upper," "lower," "front," "rear," "vertical," "horizontal," "top," "bottom," "inner," and "outer" may be used to describe the positional relationships of the constituent elements with reference to the accompanying drawings. These terms are used solely for ease of description and simplification and are not intended to indicate or imply that the device or element referred to must have a specific orientation, be constructed or operated in a specific orientation, and therefore should not be construed as a limitation on the embodiments of this disclosure. The positional relationships and orientations of the constituent elements may change depending on the placement direction of each constituent element.

[0083] In this embodiment of the disclosure, "parallel" means approximately parallel or nearly parallel, and the included angle between the two elements defined therein may be within the allowable range of process tolerance. Similarly, "perpendicular" means approximately perpendicular or nearly perpendicular, and the included angle between the two elements defined therein may be an error angle relative to a 90° right angle that is within the allowable range of process tolerance.

[0084] It should be noted that the technical solutions described in the embodiments of this disclosure can be combined arbitrarily without conflict. In the methods involved in the embodiments of this disclosure, unless otherwise specified or described, the execution order of each step can be adjusted according to actual circumstances or needs. That is, different combinations of the sequences of steps involved in the embodiments of this disclosure all fall within the protection scope of this disclosure.

[0085] The deposition processes involved in the embodiments of this disclosure include, but are not limited to: chemical vapor deposition (CVD), physical vapor deposition (PVD), plasma enhanced chemical vapor deposition (PECVD), sputtering, metal-organic chemical vapor deposition (MOCVD), atomic layer deposition (ALD), and combinations thereof.

[0086] The growth processes described in this disclosure include, but are not limited to: vapor phase epitaxy (VPE), liquid phase epitaxy (LPE), molecular beam epitaxy (MBE), ion beam epitaxy, solid phase epitaxy, and combinations thereof.

[0087] The etching processes disclosed herein include, but are not limited to, dry etching, wet etching, and combinations thereof.

[0088] The semiconductor structure disclosed herein is at least a portion of the structure that will be used in subsequent processes to form the final device structure. Here, the final device may be a memory, such as MRAM (Magnetoresistive Random Access Memory), or other memory chips or processing chips containing MRAM memory cells.

[0089] This disclosure provides a semiconductor structure 100, such as... Figure 1 As shown, the semiconductor structure 100 includes: a substrate structure 110; an MTJ structure 120 stacked on the substrate structure 110; a spin transition layer 130 covering the top of the MTJ structure 120; a torque functional layer 140 at least partially covering the surface of the spin transition layer 130; a first electrode 150 and a second electrode 160 located on both sides of the stack of the MTJ structure 120 and the spin transition layer 130; the torque functional layer 140 is electrically connected to the first electrode 150 and the second electrode 160.

[0090] The MTJ structure 120 refers to the magnetic tunnel junction, a core component of MRAM memory cells, consisting of two layers of ferromagnetic material and one insulating layer. The two ferromagnetic layers are called the free layer (FL) and the pinned layer (PL or Reference Layer, RL). The magnetization direction of the free layer can be changed, while the magnetization direction of the pinned layer is fixed. When the magnetization directions of the free and pinned layers are parallel, the probability of electron tunneling is higher, and the resistance is lower; when the magnetization directions are antiparallel, the probability of electron tunneling is lower, and the resistance is higher. By detecting changes in resistance, data stored in the MTJ can be read; this is the read / write principle of MRAM memory cells.

[0091] In some embodiments, the torque functional layer 140 includes a first type of material for providing spin flow.

[0092] Spin current refers to the directional flow of spin angular momentum, characterized by the movement of spin-up and spin-down electrons in opposite directions. Spin current can be generated through the spin Hall effect or the non-equilibrium state of magnetic materials. The generation of spin current depends on the specific physical properties of the material (such as spin-orbit coupling, magnetic or topological properties). The following are the main types of materials capable of generating spin current and their physical mechanisms:

[0093] First, heavy metals, such as platinum (Pt), tantalum (Ta), and tungsten (W).

[0094] Mechanism: Spin Hall Effect (SHE).

[0095] Principle: When an electric current passes through a heavy metal, spin-orbit coupling (SOC) causes electron spin to accumulate in the lateral direction, forming a spin current. Electrons with spin up and spin down are deflected in opposite directions due to SOC, resulting in spin polarization. The direction of the spin current is perpendicular to the charge current (right-hand rule).

[0096] Second, ferromagnetic materials, such as cobalt (Co), iron (Fe), and nickel (Ni).

[0097] Mechanism: Spin polarization current.

[0098] Principle: In ferromagnetic materials, the electron state density at the Fermi level is asymmetrical between spin-up and spin-down, and the current naturally carries spin polarization when it passes through.

[0099] Third, semiconductor heterojunctions, such as gallium arsenide (GaAs), aluminum gallium arsenide (AlGaAs), and indium arsenide (InAs).

[0100] Mechanisms: The "Rashba" effect and the "Dresselhaus" effect.

[0101] Principles: "Rashba" effect: Asymmetric interfaces (such as heterojunctions or surface electric fields) cause momentum-spin locking, where the spin direction changes with the momentum direction as electrons move. "Dresselhaus" effect: Spin splitting caused by the asymmetry of the crystal structure in bulk materials. Spin current generation: When an electric field or light excitation is applied, the momentum distribution of electrons is biased, leading to spin current (e.g., through the inverse spin Hall effect).

[0102] Fourth, topological materials, such as bismuth selenide (Bi2Se3) and bismuth telluride (Bi2Te3).

[0103] Mechanism: Spin momentum locking of topological surface states.

[0104] Principle: The surface states of topological insulators exhibit a strictly locked spin-momentum property, meaning that the spin direction is perpendicular to the momentum direction when current flows. For example, the surface current of Bi₂Se₃ is accompanied by a 100% polarized spin current.

[0105] Fifth, two-dimensional materials, such as graphene and molybdenum disulfide (MoS2).

[0106] Mechanism: Interface effect and electric field modulation.

[0107] Principle: Graphene: Spin-orbit coupling is introduced through proximity effects (such as contact with tungsten disulfide (WS2) or ferromagnets), generating spin current. Transition metal sulfides (TMDs): Strong SOC and valley degrees of freedom can be used to modulate spin polarization using an electric field.

[0108] Sixth, antiferromagnetic materials, such as gold-manganese alloy (Mn2Au) and iridium manganese (IrMn).

[0109] Mechanism: Spin structure symmetry breaking.

[0110] Principle: In antiferromagnets, adjacent spins are arranged antiparallel, but a net spin current can be generated by driving an electric current (such as the Nair spin-orbit torque). Current-induced spin polarization occurs in strongly SOC materials (such as the inverse spin Hall effect of Mn₂Au).

[0111] Seventh, multiferroic materials, such as bismuth ferrite (BiFeO3).

[0112] Mechanism: Magnetoelectric coupling effect.

[0113] Principle: The electric field modulates the magnetic order, indirectly inducing spin current (e.g., through strain or interface charge transfer). This spin current couples with ferromagnetic polarization, achieving low-power control. For example, in an MTJ (Metal-Touch Jet), the spin-polarized current emitted by the ferromagnetic electrode is injected into another magnetic layer, generating a spin-to-touch (STT).

[0114] The first type of material of the torque functional layer 140 is used to provide spin flow, and therefore can be composed of one or more of the above-mentioned materials.

[0115] In some embodiments, the first type of material includes heavy metal materials with spin-orbit coupling effects. For example, it includes iridium (Ir) and its oxides, platinum (Pt), ruthenium (Ru) and its oxides, tantalum (Ta), tantalum nitride (TaN), chromium-platinum alloy CrPt, palladium (Pd), gold (Au), lead (Pb), etc.

[0116] The aforementioned heavy metal materials exhibit a strong spin-orbit coupling effect, enabling them to efficiently provide spin flow.

[0117] In some embodiments, the spin transition layer 130 includes a second type of material for transmitting the spin flow.

[0118] When the torque functional layer 140 is a first-class material with spin-orbit coupling effect used to provide spin flow, the spin transition layer 130 can be used to transmit the spin flow provided by the torque functional layer 140. Therefore, the spin transition layer 130 can be made of a material with a long spin diffusion length. Materials with a long spin diffusion length can efficiently transmit spin flow.

[0119] Spin Diffusion Length (L) s Spin diffusion length is a core parameter in spintronics, used to describe the average propagation distance of spin-polarized electrons in a material while maintaining their spin direction. It is defined as the distance a spin-polarized electron travels in a material until its spin polarization (spin direction consistency) decays to 1 / e (approximately 37%) of its initial value. During propagation, electrons undergo spin direction randomization due to scattering (such as interactions with impurities, phonons, or other electrons); this phenomenon is called spin relaxation. A longer spin diffusion length results in weaker spin relaxation, a stronger ability of the material to maintain spin information, and is more advantageous for spintronic devices, enabling more efficient transmission of spin current.

[0120] In some embodiments, the second type of material includes materials with a spin diffusion length greater than a preset first threshold. That is, materials with a long spin diffusion length can be used as the second type of material. For example, a first threshold is set as the standard for determining whether a material has a long spin diffusion length; if the spin diffusion length of a material is greater than the first threshold, it is considered to be a material with a long spin diffusion length. Alternatively, the characteristics of the material's spin flow transmission can be directly used to determine whether it belongs to a material with a long spin diffusion length, and thus whether it can be used as a second type of material in the spin transition layer 130.

[0121] For example, the second type of material may include copper (Cu), nickel oxide (NiO), etc.

[0122] In some embodiments, the torque functional layer 140 may further include a third type of material for providing orbital flow.

[0123] Orbital Current (J) L Orbital current density (J) is the directional flow of orbital angular momentum in an electronic system, commonly used to describe the orbital motion patterns of electrons in atoms, molecules, or solids. It is closely related to the spin-orbit coupling effect of electrons. L It can be used to quantitatively describe orbital flow and to define the flow rate of orbital angular momentum L. Orbital flow refers to the motion pattern of electrons in orbits, while spin flow refers to the directional motion of electron spins. The two can interact: orbital flow can be converted into spin flow through the spin-orbit coupling effect, i.e., the SOC effect.

[0124] In some embodiments, the third type of material includes materials exhibiting the orbital Hall effect.

[0125] The Orbital Hall Effect (OHE) refers to the phenomenon in conductors or semiconductors where the orbital angular momentum of electrons separates and accumulates laterally under the influence of an electric current. Similar to the lateral deflection of spin in the Spin Hall Effect (SHE), the Orbital Hall Effect focuses on the non-equilibrium distribution of orbital degrees of freedom.

[0126] Materials exhibiting the orbital Hall effect can provide orbital flow and thus can be used as the third type of material to form the torque functional layer 140.

[0127] For example, materials exhibiting the orbital Hall effect may include: light metals such as titanium (Ti) and chromium (Cr); two-dimensional materials such as molybdenum disulfide (MoS2) and tungsten ditelluride (WTe2); and topological materials such as bismuth selenide (Bi2Se3).

[0128] The orbital current generated by the third type of material mentioned above can be converted into a spin current. The spin transition layer 130 improves the conversion efficiency, ensuring efficient conversion of the orbital current into a spin current. In some materials, the orbital current can generate a spin current through spin-orbit coupling. For example, in heavy metals such as platinum (Pt) or tantalum (Ta), the orbital current converts orbital angular momentum into spin angular momentum through spin-orbit coupling, thus generating a spin current. This phenomenon is called spin-orbit moment, and its physical process is as follows: when an electric current passes through a heavy metal material, the orbital motion of electrons (orbital current) generates a transverse spin-polarized current (spin current) through spin-orbit coupling.

[0129] The conversion efficiency from orbital flow to spin flow depends on the spin-orbit coupling strength and the symmetry of the crystal structure of the material. The spin transition layer 130 can enhance the spin-orbit coupling strength, thereby improving the conversion efficiency.

[0130] In some embodiments, the spin transition layer 130 includes a fourth type of material for converting the orbital flow into a spin flow.

[0131] Since the conversion between orbital flow and spin flow occurs through a spin-orbit coupling effect, in some embodiments, the fourth type of material may include materials with a spin-orbit coupling effect, such as heavy metal materials. Exemplarily, the fourth type of material may be of the same type as the first type of material described above; for specific selection, please refer to the description of the first type of material.

[0132] In some embodiments, such as Figure 1 As shown, the MTJ structure 120 includes: a buffer layer 121, a fixing layer 122, an isolation layer 123, and a free layer 124 stacked sequentially; wherein, the free layer 124 is in contact with the spin transition layer 130; and the buffer layer 121 is in contact with the substrate structure 110.

[0133] The buffer layer 121 can be made of a metallic material, such as heavy metals like tantalum (Ta) or platinum (Pt). The buffer layer 121 can reduce surface roughness, improve the crystal quality of the film, and regulate the magnetic anisotropy of the ferromagnetic material.

[0134] In some embodiments, such as Figure 1 As shown, the semiconductor structure 100 further includes:

[0135] A protective layer 210 covering at least the stacked sidewalls of the MTJ structure 120 and the spin transition layer 130;

[0136] The torque functional layer 140 covers the surface of the top of the spin transition layer 130 and the protective layer 210.

[0137] Understandably, each MTJ structure requires graphical processing to form a memory cell, and this memory cell needs to be isolated from external electrodes, such as the first electrode 150 and the second electrode 160. Therefore, a protective layer 210 is used to cover the stack consisting of the MTJ structure 120 and the spin transition layer 130.

[0138] The top of the spin transition layer 130 may be flush or substantially flush with the top of the protective layer 210, and the torque functional layer 140 covers it, such that the top surface of the spin transition layer 130 is covered by the torque functional layer 140, and the top of the protective layer 210 is also covered by the torque functional layer 140.

[0139] In some embodiments, such as Figure 2 As shown, the substrate structure 110 includes: a substrate 111; a first bottom electrode 112 that penetrates the substrate 111 and is electrically connected to the first electrode 150; and a second bottom electrode 113 that penetrates the substrate 111 and is electrically connected to the bottom of the MTJ structure 120.

[0140] In other words, the electrodes used for signal transmission in the MTJ structure can be disposed within the substrate structure 110. The second bottom electrode 113 can be located below the MTJ structure 120, contacting the buffer layer 121 at the bottom of the MTJ structure 120. That is, the buffer layer 121 in the MTJ structure 120 is connected to the second bottom electrode 113. Additionally, the first bottom electrode 112 is used to connect to the first electrode 150, which is located on one side of the MTJ structure 120 and may not be in direct contact with the substrate structure 110. Therefore, the first bottom electrode 112 and the first electrode 150 can also be connected through other conductive structures (e.g., conductive pillars). Furthermore, the first bottom electrode 112 is not connected to the MTJ structure 120 or the second bottom electrode 113; they are isolated from each other.

[0141] Furthermore, the first bottom electrode 112 and the second bottom electrode 113 may each include a bottom metal structure (BM) as a bottom electrode and a bottom via (BV), wherein the cross-sectional dimension of the BV parallel to the substrate surface is smaller than the cross-sectional dimension of the BM. The BM may connect to multiple BVs, and each BV may be connected to either an MTJ structure 120 or a first electrode 150.

[0142] In some embodiments, continue to refer to Figure 2 The semiconductor structure 100 further includes:

[0143] A filling layer 220 located in at least a portion of the region outside the stack of the MTJ structure 120 and the spin transition layer 130;

[0144] The first electrode 150 and the second electrode 160 are disposed within the filling layer 220;

[0145] The filling layer 220 has an interconnection structure connecting the first electrode 150 and the first bottom electrode 112, such as the conductive pillar mentioned in the above embodiments, or a metal contact structure, etc., and the interconnection structure can be integrally formed with the first electrode 150.

[0146] In some embodiments, the semiconductor structure further includes a source line 230 electrically connected to the second electrode 160.

[0147] The first electrode 150 is connected to the first bottom electrode 112 located in the substrate structure 110, and the second electrode 160 is electrically connected to the source line 230. A current path is formed between the first bottom electrode 112 and the source line 230 through the first electrode 150, the torque functional layer 140, and the second electrode 160. When a voltage is applied between the first bottom electrode 112 and the source line 230, a current is generated in this current path, which in turn causes the torque functional layer 140 to generate a spin current or orbital current, and with the assistance of the spin transition layer 130, the spin current is transmitted to the free layer 124.

[0148] The above Figure 2 This illustration only shows one possible specific structure of the semiconductor structure provided in the embodiments of this disclosure, and is not intended to limit the actual structural form, size, or proportion of the semiconductor structure. All structures that conform to the above description of the embodiments of this disclosure fall within the scope of the semiconductor structures referred to in the embodiments of this disclosure, and will not be listed individually here.

[0149] Based on the same inventive concept, this disclosure also provides a method for manufacturing a semiconductor structure 100, the main steps of which are as follows: Figure 3 As shown, the specific process can be found by referring to [the diagram]. Figures 4 to 10 The method includes:

[0150] Step S101: Provide a base structure 110.

[0151] In some embodiments, step S101 may specifically include:

[0152] Step S11: Provide substrate 111;

[0153] Step S12: Form a first bottom electrode 112 and a second bottom electrode 113 through the substrate 111; wherein the first bottom electrode 112 is used to be electrically connected to the first electrode 150; and the second bottom electrode 113 is used to be electrically connected to the bottom of the MTJ structure 120.

[0154] This disclosure does not specifically limit the constituent materials of the substrate 111. As an example, the substrate 111 can be constructed from semiconductor materials, insulating materials, conductive materials, or any combination thereof. The substrate 111 can be a single-layer structure or a multi-layer structure. For example, the substrate 111 can be a silicon (Si) substrate, a silicon-germanium (SiGe) substrate, a silicon-germanium-carbon (SiGeC) substrate, a silicon carbide (SiC) substrate, a gallium arsenide (GaAs) substrate, an indium arsenide (InAs) substrate, an indium phosphide (InP) substrate, or other III / V or II / VI semiconductor substrates. Alternatively, for example, the substrate 111 can be a layered substrate comprising, for example, a stack of Si and SiGe, a stack of Si and SiC, silicon-on-insulator (SOI), or silicon-germanium-on-insulator.

[0155] The process of forming the first bottom electrode 112 and the second bottom electrode 113 may include: forming a structure such as a recess or through hole that meets the shape requirements of the bottom electrode on the substrate 111, and then filling it with a metallic material or a non-metallic conductive material.

[0156] Step S102: Form a stack of MTJ structure 120 and spin transition layer 130 on the substrate structure; wherein the spin transition layer covers the top of the MTJ structure.

[0157] Specifically, in some embodiments, step S102 can be implemented by the following steps:

[0158] Step S21: Buffer material layer 121a, fixing material layer 122a, isolation material layer 123a, free material layer 124a and spin transition material layer 130a are sequentially stacked on the substrate structure.

[0159] Step S22: Cover the top of the spin transition material layer 130a with an etch stop material layer 410a. The etch stop material layer 410a is an oxide material, such as aluminum oxide (Al2O3) or silicon oxide (SiO2).

[0160] Step S23: Cover the surface of the etching stop material layer 410a with a mask layer 420. At this time, a mask layer 420 is formed as shown in the figure. Figure 4 The stacked structure shown consists of a buffer material layer 121a, a fixed material layer 122a, an isolation material layer 123a, a free material layer 124a, a spin transition material layer 130a, an etch stop material layer 410a, and a mask layer 420.

[0161] Step S24: The patterned mask layer 420 is etched to form a stack of the MTJ structure 120 and the spin transition layer 130 located in a predetermined area.

[0162] Here, patterning processing may include processes such as photolithography and etching, by confining the aforementioned stacked structure within a predetermined area for forming memory cells using a mask layer 420. In the patterned buffer layer 121, fixing layer 122, isolation layer 123, free layer 124, spin transition layer 130, etch stop layer 410, and mask layer 420, the buffer layer 121, fixing layer 122, isolation layer 123, and free layer 124 constitute the MTJ structure 120, as shown below. Figure 5 As shown.

[0163] For example, the buffer material layer 121a can be a metallic material, such as heavy metals like tantalum (Ta) or platinum (Pt). The fixing material layer 122a can be a synthetic antiferromagnetic (SAF) film. SAF is a structure composed of two layers of ferromagnetic material separated by a non-magnetic spacer layer. In the MTJ structure, the patterned SAF structure is used as the fixing layer 122 to provide a stable magnetization direction, preventing it from being accidentally changed during writing, thereby improving the stability of stored data. The isolation material layer 123a can be a non-magnetic isolation layer, such as an oxide material or a non-magnetic metallic material. Its structure can be an ultrathin film of a few nanometers. The isolation layer 123 formed by it can allow the tunneling of spin-polarized electrons while maintaining the independence of the two magnetic moments. The free material layer 124a can be composed of a thin ferromagnetic material, not limited to cobalt-iron-boron (CoFeB) material, but can also include magnetic materials such as cobalt-platinum alloy (CoPt), cobalt-nickel alloy (CoNi), cobalt-nickel (Co / Ni) multilayer film, iron-platinum alloy (FePt), iron (Fe), nickel-iron alloy (NiFe), and cobalt-iron alloy (CoFe); it can also be one or a combination of non-collinear antiferromagnetic materials such as platinum-manganese ternary alloy (PtMn3) and collinear antiferromagnetic oxides such as ruthenium oxide (RuO2). The magnetic moment direction of the above materials can be changed by spin polarization current, and the formed free layer 124 is used to store information.

[0164] The spin transition material layer 130a is used to obtain the spin transition layer 130 after patterning. Its material has been described in detail in the previous embodiments and will not be repeated here.

[0165] The etching stop material layer 410a can be an oxide material, such as aluminum oxide (Al2O3) or silicon oxide (SiO2), to serve as a stop layer for the subsequent etching process of removing the mask layer 420.

[0166] The mask layer 420a can be a metal or compound material containing tantalum (Ta) or titanium (Ti), such as titanium nitride (TiN), tantalum nitride (TaN), or a tantalum metal film.

[0167] In some embodiments, before performing step S103, the method may further include the following steps S201-203:

[0168] Step S201: Form a protective layer 210 that at least covers the sidewalls of the stack and the remaining top mask layer 420, such as... Figure 6As shown; here, the stack refers to the buffer layer 121, fixing layer 122, isolation layer 123, free layer 124, spin transition layer 130, etch stop layer 410, and mask layer 420 retained after the above patterning process. The sidewalls of the stack are the exposed side surfaces of the stack. The protective layer 210 can cover the entire surface of the current structure. Exemplarily, the protective layer 210 can be formed by processes such as ALD or CVD. The material of the protective layer 210 can be an insulating material different from the materials in any of the above stacks, such as silicon nitride or silicon oxide.

[0169] Step S202: Form a filling layer 220 in the area outside the protective layer 210, such as... Figure 7 As shown, the material of the filling layer 220 can be an insulating dielectric material such as oxide or nitride, like silicon oxide or silicon nitride. It should be noted that the filling layer 220 can be made of a different material than the protective layer 210, which facilitates the subsequent formation of structures such as electrodes in the filling layer 220 without affecting the protective layer 210.

[0170] Step S203: Form source line 230 within the filling layer 220, such as... Figure 8 As shown. The source line can extend in a direction perpendicular to the plane of the paper, and connect to one or more electrodes, such as the subsequently formed second electrode 160. Figure 7 The stacked structure shown is used to form a storage array consisting of multiple magnetic storage cells.

[0171] Step S103: Form a first electrode 150 and a second electrode 160 on both sides of the stack of the MTJ structure 120 and the spin transition layer 130.

[0172] Here, the first electrode 150 and the second electrode 160 may be spaced apart from the aforementioned stack, or they may be located on opposite sides of the stack, i.e., the stack and the first electrode 150 or the second electrode 160 are isolated by the protective layer 210. The first electrode 150 and the second electrode 160 may also be spaced apart from the stack and the protective layer 210 covering its sidewalls, and are isolated by the aforementioned filler layer 220.

[0173] Furthermore, the upper surfaces of the first electrode 150 and the second electrode 160 are used to contact and connect with the torque functional layer 140 to form a current path. The torque functional layer 140 covers the first electrode 150, the second electrode 160, and the top surface of the stack. Its morphology depends on the positional relationship between the first electrode 150, the second electrode 160, and the top surface of the stack. The first electrode 150, the second electrode 160, and the top surface of the stack can be flush or uneven. If flush, the formed torque functional layer 140 can be a thin film with a planar surface; if uneven, the formed torque functional layer 140 can be a thin film with depressions or protrusions on its surface.

[0174] In some embodiments, step S103, forming a first electrode 150 and a second electrode 160 on both sides of the stack of the MTJ structure 120 and the spin transition layer 130, includes:

[0175] Step S31: Form a first recessed structure 221 and a second recessed structure 222 located on both sides of the stack within the filling layer 220; wherein at least a portion of the surface of the source line 230 is exposed to the first recessed structure 221; at least a portion of the surface of the first bottom electrode 112 located in the substrate structure 110 is exposed to the second recessed structure 222, as shown. Figure 9 As shown.

[0176] Specifically, trenches or holes are formed by etching the filling layer until the source line 230 and the first bottom electrode 112 are exposed. It should be noted that since the depths of the first recessed structure 221 and the second recessed structure 222 may differ, the first recessed structure 221 and the second recessed structure 222 can be etched in two steps. For example, first, the surface of the area where the second recessed structure 222 needs to be formed is shielded, and the first recessed structure 221 is etched to form. Then, the first recessed structure 221 is shielded, and the second recessed structure 222 is etched to form. Alternatively, the areas containing the first recessed structure 221 and the second recessed structure 222 can be etched simultaneously. After the first recessed structure 221 is etched, it is shielded, and then the second recessed structure 222 is etched to continue.

[0177] Step S32: Fill the first recessed structure 221 and the second recessed structure 222 with conductive material to form the second electrode 160 and the first electrode 150, such as... Figure 10 As shown.

[0178] Here, a dual damask process can be used to grow the electrodes and interconnects. This is achieved by simultaneously filling the first recessed structure 221 and the second recessed structure 222 with metallic materials, such as copper (Cu), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), ruthenium (Ru), aluminum (Al), gold (Au), platinum (Pt), etc., or with conductive compounds containing non-metallic elements such as silicon (Si), carbon (C), nitrogen (N), and oxygen (O), such as titanium nitride (TiN). The filling continues until the conductive material covers the device surface, and then CMP polishing is performed until the top of the protective layer 210 and the top of the filling layer 220 are exposed.

[0179] In some embodiments, prior to step S104 below, the method may further include steps S301-S302 below:

[0180] Step S301: Remove the remaining mask layer 420 on the top of the stack and the protective layer 210 on the surface of the mask layer 420 by the first etching process;

[0181] Step S302: Remove the etch stop layer 410 by a second etching process to expose the surface of the spin transition layer 130.

[0182] In forming the above Figure 9 After the structure is completed, the protective layer 210 on top of the stack needs to be removed, and the mask layer 420 needs to be further removed. It is understood that the etch stop layer 410 plays a role in this process, that is, the etching process of the first etching process mentioned above stops at the etch stop layer 410.

[0183] In this embodiment of the disclosure, oxide is used as the material of the etching stop layer 410, which provides a larger process window. The structure does not involve the accumulation of materials with opposite spin Hall angles. Furthermore, the high selectivity etching of oxide and metal can reduce the loss of spin transition layer 130, improve the controllability of the thickness of spin transition layer 130, and is conducive to improving yield and performance.

[0184] In some other embodiments, tantalum (Ta) metal is used as a hard mask. The hard mask is removed using a wet etching selectivity ratio of Ta and ruthenium (Ru) metal in the free layer. Etching stops on the ruthenium (Ru) layer, and then a SOT layer, such as an SOT layer containing tantalum (Ta) or tungsten (W) metal, is fabricated. However, since ruthenium (Ru) has opposite spin Hall angles to tantalum (Ta) or tungsten (W), the ruthenium (Ru) layer will reduce the overall spin current intensity of the SOT layer to some extent.

[0185] Compared to the methods in the other embodiments described above, this embodiment utilizes an etch stop layer 410 made of oxide to remove the hard mask. This does not affect the spin transition layer 130 during the first etching process, facilitates precise control of the thickness of the spin transition layer 130, and avoids the influence of the opposite spin Hall angle. Therefore, it can effectively improve device performance. The etch stop layer 410 is then removed separately using a second etching process to expose the surface of the spin transition layer 130.

[0186] Step S104: Form a torque functional layer 140 covering the surfaces of the first electrode 150, the second electrode 160, and the spin transition layer 130; wherein the torque functional layer 140 is electrically connected to the first electrode 150 and the second electrode 160.

[0187] Here, since the surfaces of the spin transition layer 130, the first electrode 150, and the second electrode 160 are exposed on the top of the device, a thin film of the torque functional layer 140 can be deposited on the top of the device by a deposition process to form a uniform torque functional layer 140, so that the torque functional layer 140 covers and connects the first electrode 150, the second electrode 160, and the spin transition layer 130.

[0188] Steps S103 to S104 and each intermediate step described above can be implemented in various ways. Two specific implementation examples are provided below:

[0189] Example 1:

[0190] In some embodiments, step S301 above may include:

[0191] Step S301-a: Based on the preset grinding rate ratio of the conductive material to the material of the filling layer 220, perform CMP (chemical mechanical polishing) on ​​the protective layer, the conductive material, and the mask layer on the top of the stack until the etching stop layer is exposed; wherein, after the CMP treatment, the etching stop layer protrudes from the surface of the conductive material.

[0192] The conductive material here refers to the material of the first electrode 150 and the second electrode 160.

[0193] Based on the above Figure 10 The structure shown is further subjected to CMP processing, which simultaneously thins the tops of the first electrode 150, the second electrode 160, the peripheral filler layer 220, and the protective layer 210 until the mask layer 420 is exposed, and then the mask layer is further removed. Exemplarily, grinding can be performed at a grinding rate with an etching selectivity ratio of 1:1 between the electrode material (e.g., metallic Cu) and the filler layer 220 material, such as silicon oxide (SiO2). Grinding can then continue at the aforementioned rate, making it difficult to remove the etching stop layer 410, thus forming a structure as shown. Figure 11 The MTJ shows a raised structure on top.

[0194] It should be noted that, since some of the conductive material of the electrodes needs to be removed by grinding during this process, the thickness of the first electrode 150 and the second electrode 160 is reduced. Therefore, when the first recessed structure 221 and the second recessed structure 222 are formed in the above step S31, the etching can be deeper, so that the depth of the first recessed structure 221 and the second recessed structure 222 is greater than the required thickness of the first electrode 150 and the second electrode 160.

[0195] Then, after filling with conductive material in step S32, a thicker first electrode 150 and second electrode 160 are formed. In this way, through the grinding in step S301-a, the first electrode 150 and the second electrode 160 can be thinned to a suitable thickness.

[0196] In some embodiments, step S302 above may include:

[0197] Step S302-a: Remove the etch stop layer 410 by wet etching, making the conductive material flush with the surface of the spin transition layer 130, such as... Figure 12 As shown.

[0198] Since the etching stop layer 410 protrudes from the conductive material after the above step S301-a, removing the etching stop layer 410 in this step can make the remaining top of the stack, i.e. the surface of the spin transition layer 130, substantially in the same plane as the conductive material of the electrodes on both sides.

[0199] In some embodiments, step S104 above may include:

[0200] Step S104-a: The torque functional layer 140 is formed on the plane containing the first electrode 150, the second electrode 160 and the spin transition layer 130 by PVD process.

[0201] Since the surface of the spin transition layer 130 and the conductive material of the electrodes on both sides are essentially on the same plane after the above-mentioned step S302-a, a uniform material film of the torque functional layer 140 can be formed using the PVD process, such as... Figure 13 As shown.

[0202] In other words, the embodiments of this disclosure grind the first electrode 150 and the second electrode 160 to an appropriate height using the above method, reducing the height difference between the electrode and the spin transition layer 130, making the growth surface of the torque functional layer 140 smoother, improving the uniformity of PVD growth, and helping to improve the quality of the film.

[0203] Example 2:

[0204] In some embodiments, step S301 may further include:

[0205] Step S301-b: Remove the remaining mask layer 420 on the top of the stack and the protective layer 210 on the surface of the mask layer 420 using a dry etching process until the etching stop layer 410 is exposed; wherein, after the dry etching process, the surface of the etching stop layer 410 is recessed into the surface of the conductive material.

[0206] like Figure 14As shown, the protective layer 210 at the top of the stack can be removed first using a dry etching process, followed by the removal of the mask layer 420. This process stops at the etching stop layer 410. Furthermore, due to the high etching selectivity of dry etching, the electrodes on both sides and the fill layer 220 are not thinned.

[0207] In some embodiments, step S302 may further include:

[0208] Step S302-b: Remove the etching stop layer 410 by wet etching to expose the spin transition layer 130, and the surface of the spin transition layer 130 is recessed into the surface of the conductive material.

[0209] Next, the etch stop layer 410 is removed by high-selectivity wet etching. During this process, the protective layers on both sides are somewhat damaged. The high etch selectivity between the etch stop layer 410 and the electrode ensures that the electrode is almost not thinned, thus obtaining... Figure 15 The structure shown.

[0210] It should be noted that, since no thinning of the conductive material is performed in this example, the depth of the first recessed structure 221 and the second recessed structure 222 formed in step S31 does not need to be too deep. The first electrode 150 and the second electrode 160 formed after filling the conductive material in step S32 meet the required thickness of the electrode and maintain this thickness in subsequent processes.

[0211] In some embodiments, step S104 may further include:

[0212] Step S104-b: The torque functional layer 140 is formed on the surface of the first electrode 150, the second electrode 160 and the spin transition layer 130 by CVD or ALD process.

[0213] Because the structure formed by steps S301-b and S302-b causes the spin transition layer 130 to be recessed between the electrodes on both sides, it may be difficult to control the film thickness when using the PVD process to deposit the torque functional layer 140, resulting in uneven film thickness. For example, accumulation may occur at the top of the protective layer 210, i.e., at the corner between the spin transition layer 130 and the electrode, which in turn affects the film quality.

[0214] Therefore, CVD or ALD processes can be used to deposit the material of the torque functional layer 140, which facilitates control of the film thickness and forms a surface torque functional layer 140 that uniformly covers the first electrode 150, the second electrode 160, and the spin transition layer 130, such as... Figure 16 As shown.

[0215] In some embodiments, the method further includes:

[0216] Step S401: Graphicalize the torque functional layer 140, at least retaining the torque functional layer 140 that is in contact with the first electrode 150, the second electrode 160 and the spin transition layer 130;

[0217] Step S402: Fill at least a portion of the region outside the graphical torque function layer 140 with a dielectric layer.

[0218] like Figure 17 or Figure 2 As shown, the torque functional layer 140 can be patterned using processes such as photolithography or etching to remove the unnecessary torque functional layer 140 in areas other than the first electrode 150 and the second electrode 160, while retaining the portion connecting the first electrode 150, the spin transition layer 130 and the second electrode 160, so as to form a current path for generating spin current or orbital current during read and write operations.

[0219] The dielectric material is then filled, which, for example, can be the same dielectric material as the filling layer 220, such as silicon oxide (SiO2). This forms an integral isolation structure between the dielectric layer and the original filling layer, isolating adjacent memory cells and facilitating the formation of memory arrays or other structures.

[0220] Based on the same inventive concept, this disclosure also provides an electronic device, such as... Figure 18 As shown, the electronic device 300 may include a memory 310 and / or a processor 320. The memory 310 and / or the processor 320 may include the semiconductor structure 100 formed by the manufacturing method of the semiconductor structure 100 provided in any of the above embodiments, or may include the semiconductor structure 100 provided in any of the above embodiments. The electronic device may be various types of electronic devices such as storage devices, smartphones, computers, tablets, artificial intelligence devices, wearable devices, power banks, and electric vehicles. Storage devices may include memory in computers, etc., and are not limited thereto.

[0221] It should be understood that the phrases "some embodiments," "one embodiment," or "an embodiment" throughout the specification mean that a specific feature, structure, or characteristic related to an embodiment is included in at least one embodiment of this disclosure. Therefore, "in one embodiment" or "in an embodiment" appearing throughout the specification do not necessarily refer to the same embodiment. Furthermore, these specific features, structures, or characteristics can be combined in any suitable manner in one or more embodiments. It should be understood that in the various embodiments of this disclosure, the sequence numbers of the above-described processes do not imply a sequential order of execution; the execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of this disclosure. The sequence numbers of the above-described embodiments are for descriptive purposes only and do not represent the superiority or inferiority of the embodiments.

[0222] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element.

[0223] The above description is merely an embodiment of this disclosure, but the scope of protection of this disclosure is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this disclosure should be included within the scope of protection of this disclosure. Therefore, the scope of protection of this disclosure should be determined by the scope of the claims.

Claims

1. A semiconductor structure, characterized in that, include: Substrate structure; A magnetic tunnel junction (MTJ) structure stacked on the substrate structure; A spin transition layer covering the top of the MTJ structure; A torque functional layer that at least partially covers the surface of the spin transition layer; The first electrode and the second electrode are located on both sides of the stack of the MTJ structure and the spin transition layer; the torque functional layer is electrically connected to the first electrode and the second electrode.

2. The semiconductor structure according to claim 1, characterized in that, The torque functional layer includes a first type of material for providing spin flow; The spin transition layer includes a second type of material for transmitting the spin flow.

3. The semiconductor structure according to claim 2, characterized in that, The first category of materials includes: heavy metal materials with spin-orbit coupling effect; The second type of material includes materials whose spin diffusion length is greater than a preset first threshold.

4. The semiconductor structure according to claim 1, characterized in that, The torque functional layer includes: a third type of material for providing orbital flow; The spin transition layer includes a fourth type of material for converting the orbital flow into a spin flow.

5. The semiconductor structure according to claim 4, characterized in that, The third category of materials includes: materials exhibiting the orbital Hall effect; The fourth category of materials includes heavy metal materials with spin-orbit coupling effects.

6. The semiconductor structure according to any one of claims 1 to 5, characterized in that, The MTJ structure includes: a buffer layer, a fixing layer, an isolation layer, and a free layer stacked in sequence; The free layer is in contact with the spin transition layer; the buffer layer is in contact with the substrate structure.

7. The semiconductor structure according to any one of claims 1 to 5, characterized in that, The semiconductor structure also includes: A protective layer covering at least the stacked sidewalls of the MTJ structure and the spin transition layer; The torque functional layer covers the surface of the top of the spin transition layer and the protective layer.

8. The semiconductor structure according to any one of claims 1 to 5, characterized in that, The substrate structure includes: Substrate; A first bottom electrode that penetrates the substrate and is electrically connected to the first electrode; A second bottom electrode that penetrates the substrate and is electrically connected to the bottom of the MTJ structure.

9. The semiconductor structure according to claim 8, characterized in that, The semiconductor structure also includes: A filling layer located in at least a portion of the region outside the stack of the MTJ structure and the spin transition layer; The first electrode and the second electrode are disposed within the filling layer; The filling layer has an interconnection structure connecting the first electrode and the first bottom electrode.

10. The semiconductor structure according to claim 8, characterized in that, The semiconductor structure further includes a source line electrically connected to the second electrode.

11. A method for manufacturing a semiconductor structure, characterized in that, The method includes: Provide the base structure; A stack of an MTJ structure and a spin transition layer is formed on the substrate structure; wherein the spin transition layer covers the top of the MTJ structure; A first electrode and a second electrode are formed on both sides of the stack of the MTJ structure and the spin transition layer; A torque functional layer is formed covering the surfaces of the first electrode, the second electrode, and the spin transition layer; wherein the torque functional layer is electrically connected to the first electrode and the second electrode.

12. The manufacturing method according to claim 11, characterized in that, The stack of the MTJ structure and spin transition layer formed on the substrate structure includes: A buffer material layer, a fixing material layer, an isolation material layer, a free material layer, and a spin transition material layer are sequentially stacked on the substrate structure. An etch stop material layer is placed on top of the spin transition material layer; wherein the etch stop layer is an oxide material. A mask layer is applied to the surface of the etching stop layer; The patterned mask layer is etched to form a stack of the MTJ structure and the spin transition layer located within a predetermined region.

13. The manufacturing method according to claim 12, characterized in that, The method further includes: A protective layer is formed that at least covers the sidewalls of the stack and the remaining mask layer on top; A filler layer is formed in the area outside the protective layer; A source line is formed within the filling layer.

14. The manufacturing method according to claim 13, characterized in that, The first and second electrodes formed on both sides of the stack of the MTJ structure and the spin transition layer include: A first recessed structure and a second recessed structure are formed within the filler layer on both sides of the stack; wherein at least a portion of the surface of the source line is exposed to the first recessed structure; and at least a portion of the surface of the first bottom electrode located in the substrate structure is exposed to the second recessed structure. Conductive material is filled into the first recessed structure and the second recessed structure to form the first electrode and the second electrode.

15. The manufacturing method according to claim 14, characterized in that, Prior to forming the torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer, the method further includes: The remaining mask layer on top of the stack and the protective layer on the surface of the mask layer are removed by a first etching process; The etching stop layer is removed by a second etching process to expose the surface of the spin transition layer.

16. The manufacturing method according to claim 15, characterized in that, The removal of the remaining mask layer at the top of the stack and the protective layer on the surface of the mask layer by the first etching process includes: Based on a preset grinding rate ratio between the conductive material and the filling layer material, the protective layer, the conductive material, and the mask layer on top of the stack are subjected to chemical mechanical polishing (CMP) until the etching stop layer is exposed; wherein, after the CMP treatment, the etching stop layer protrudes from the surface of the conductive material.

17. The manufacturing method according to claim 16, characterized in that, The step of removing the etch stop layer through a second etching process to expose the surface of the spin transition layer includes: The etching stop layer is removed by wet etching, making the conductive material flush with the surface of the spin transition layer.

18. The manufacturing method according to claim 17, characterized in that, The formation of the torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer includes: The torque functional layer is formed on the plane containing the first electrode, the second electrode, and the spin transition layer using a physical vapor deposition (PVD) process.

19. The manufacturing method according to claim 15, characterized in that, The removal of the remaining mask layer at the top of the stack and the protective layer on the surface of the mask layer by the first etching process includes: The remaining mask layer on top of the stack and the protective layer on the surface of the mask layer are removed using a dry etching process until the etching stop layer is exposed; wherein, after the dry etching process, the surface of the etching stop layer is recessed into the surface of the conductive material.

20. The manufacturing method according to claim 19, characterized in that, The step of removing the etch stop layer through a second etching process to expose the surface of the spin transition layer includes: The etching stop layer is removed by wet etching, exposing the spin transition layer, and the surface of the spin transition layer is recessed into the surface of the conductive material.

21. The manufacturing method according to claim 17, characterized in that, The formation of the torque functional layer covering the surface of the first electrode, the second electrode, and the spin transition layer includes: The torque functional layer is formed on the surfaces of the first electrode, the second electrode, and the spin transition layer using chemical vapor deposition (CVD) or atomic layer deposition (ALD) processes.

22. The manufacturing method according to any one of claims 11 to 21, characterized in that, The method further includes: The torque functional layer is graphically represented, and at least the torque functional layer that is in contact with the first electrode, the second electrode, and the spin transition layer is retained. A dielectric layer is filled in at least a portion of the area outside the graphical torque functional layer.

23. The manufacturing method according to any one of claims 11 to 21, characterized in that, The provided substrate structure includes: Provide substrate; A first bottom electrode and a second bottom electrode are formed through the substrate; wherein the first bottom electrode is used for electrical connection with the first electrode; and the second bottom electrode is used for electrical connection with the bottom of the MTJ structure.

24. An electronic device, characterized in that, It includes at least one semiconductor structure as described in any one of claims 1 to 10, or includes at least one semiconductor structure formed by the manufacturing method as described in any one of claims 11 to 23.