Low-Temperature Packaging Structure and Manufacturing Method of Chips Based on Nanowires
By growing nano-metal wire arrays in situ on chips and glass substrates and using a low-temperature interlocking electrical connection structure, the signal loss and contamination problems in traditional connection processes are solved, achieving high-strength and clean connections in high-frequency applications.
Patent Information
- Application Number
- CN202611307837.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-10
AI Technical Summary
Traditional wire bonding and flip-chip bonding technologies suffer from signal loss, delay, and crosstalk issues in high-frequency transmission. Furthermore, high-temperature bonding processes may damage the chip and introduce flux residues, leading to insufficient reliability.
In-situ growth of nanoscale metal wire arrays on chips and glass substrates is employed, and interconnection between the chip and the substrate is achieved through an interlocking electrical connection structure under low-temperature conditions. Metallic bonds are formed by solid-state diffusion and sintering of the nanoscale metal wire arrays.
It achieves high-strength, clean electrical and mechanical connections at low temperatures, reduces signal loss and flux contamination risks, and provides high reliability and excellent electrical pathways, making it suitable for high-frequency applications.
Smart Images

Figure CN123076291A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of semiconductor packaging technology, and in particular relates to a low-temperature chip packaging structure based on nanowires and its manufacturing method. Background Technology
[0002] In traditional optical modules, the electrical connection between chips such as lasers, detectors, and driver chips and the substrate is mostly achieved through wire bonding (WB). However, with the increasing demand for transmission rates of 100Gbps, 400Gbps, and even higher, the limitations of wire bonding are becoming increasingly apparent. Gold wires are typically on the order of millimeters, and their inherent parasitic inductance and capacitance introduce significant signal loss, delay, and crosstalk, becoming a key bottleneck limiting system performance improvements.
[0003] To overcome the drawbacks of wire bonding, the industry is increasingly turning to flip-chip (FC) technology. However, in flip-chip structures, an interposer is typically required to match the significant difference in the coefficient of thermal expansion (CTE) between the chip and the organic substrate. While traditional silicon interposers offer superior performance, they are expensive, and their semiconductor properties introduce additional signal coupling issues.
[0004] Glass substrates, as an emerging interposer material, have shown great application potential. However, reliably attaching chips to glass substrates remains a challenge: traditional thermo-compression bonding (TCB), while achieving high-precision connections, typically requires temperatures above 300°C and high pressures. This not only increases manufacturing costs and energy consumption but can also cause thermal damage to the chips (especially temperature-sensitive optoelectronic devices such as VCSELs and EMLs). Another common process, reflow soldering, while allowing for slightly lower temperatures (around 200-260°C), introduces flux residues. These residues are corrosive and can contaminate sensitive areas of optical devices (such as light-emitting surfaces), leading to performance degradation or long-term reliability issues. Summary of the Invention
[0005] This application addresses the problems of high temperature, easy contamination, high cost and insufficient reliability in the existing chip-to-glass substrate connection process. It provides a low-temperature, clean and highly reliable interconnection structure for chips and substrates in optical modules and other high-frequency applications, and realizes flip-chip connection by using nanoscale metal wire arrays grown in situ on the chip and glass substrate.
[0006] To solve the above-mentioned technical problems, the technical solution adopted in this application is: a low-temperature chip packaging structure based on nano-metal wires, which includes: a first nano-metal wire array formed on the chip pad; a second nano-metal wire array formed on the connection area on the substrate side; and an interlocking electrical connection structure, which is formed by interleaving and bonding the first nano-metal wire array and the second nano-metal wire array under preset conditions.
[0007] Optionally, in any of the above-described chip low-temperature packaging structures based on nanowires, the material of the nanowire array includes: gold, silver, copper, nickel, platinum, palladium, or an alloy of any of the aforementioned metal materials.
[0008] Optionally, in any of the above-described low-temperature chip packaging structures based on nanowires, the preset conditions are: a connection temperature of 170°C to 240°C and a connection pressure of at least 10 MPa applied to the pads.
[0009] Optionally, in any of the above-described low-temperature chip packaging structures based on nanowires, the interlocking electrical connection structure includes metallic bonds formed by solid-state diffusion and sintering between metal atoms activated by preset environmental conditions.
[0010] Optionally, in any of the above-described chip low-temperature packaging structures based on nanowires, the first nanowire array and the second nanowire array are formed along the porous film covering the connection area surface of the chip pad and the substrate side by chemical vapor deposition, physical vapor deposition, electrochemical deposition, template-assisted growth, or any one or a combination of the above deposition processes.
[0011] Optionally, in any of the above-described low-temperature chip packaging structures based on nanowires, the average diameter of each nanowire in the first and second nanowire arrays is in the range of 10 nanometers to 300 nanometers.
[0012] Meanwhile, this application also provides a method for manufacturing a low-temperature chip packaging structure based on nanowires, used to manufacture the low-temperature chip packaging structure based on nanowires as described above. The method involves generating the nanowire arrays on pads according to the following steps: removing the metal oxide layer from the pad surface; attaching photoresist to the working area outside the pad; depositing a metal substrate on the pad area exposed to the photoresist; attaching a porous film to the photoresist; growing nanowire structures along the pores of the porous film on the metal substrate; removing the porous film; and removing the photoresist to obtain nanowire arrays grown on each pad.
[0013] Optionally, in any of the above-described methods for manufacturing a low-temperature chip packaging structure based on nanowires, after generating the first nanowire array and the second nanowire array on the connection area of the chip pad and the substrate side respectively, an interlocking electrical connection structure is formed according to the following steps: the first nanowire array and the second nanowire array are positioned opposite each other, so that the nanowires in the array interpenetrate each other, and the interlocking electrical connection structure is formed by metal bonds formed by cold soldering, low-temperature sintering or hot-pressing solid-phase diffusion.
[0014] Optionally, the chip low-temperature packaging structure manufacturing method based on nanowires as described above involves growing a nanowire structure on a metal substrate along the pores of a porous film using chemical vapor deposition, physical vapor deposition, electrochemical deposition, template-assisted growth, or any one or a combination of the above deposition processes.
[0015] Optionally, in any of the above-described methods for manufacturing a low-temperature chip packaging structure based on nanowires, a protective adhesive is applied to the working area outside the pads after removing the metal oxide layer on the surface of the pads and before applying photoresist, so that the metal substrate can be attached to the pad area exposed to the protective adhesive; the photoresist is applied to the area where the protective adhesive is attached; the thickness of the photoresist is between 3 and 8 μm; and the length of the nanowires on the surface of the pads is between 20 μm and 30 μm. Beneficial effects
[0016] This application provides a low-temperature chip packaging structure and manufacturing method based on nanowires. Two nanowire arrays are formed on the connection areas of the chip pads and the substrate side, respectively. These two arrays are interlocked and metal bonds are formed under a predetermined environment through cold soldering, low-temperature sintering, or hot-pressing solid-state diffusion to achieve interlocking. This application enables high-strength, high-conductivity, and high-reliability electrical and mechanical connections between the chip and the glass substrate in a clean environment, even at low temperatures or room temperature. The low-temperature process significantly reduces residual stress generated during cooling due to thermal expansion coefficient mismatch, lowering the risk of chip cracking or solder joint fatigue. Furthermore, the connection technology provided in this application requires neither solder nor flux, thus eliminating expensive and complex cleaning steps, reducing contamination, and providing extremely high mechanical strength and stable electrical pathways. Attached Figure Description
[0017] The embodiments of this application will be described in further detail below with reference to the accompanying drawings: Figure 1 This is a schematic diagram illustrating the process of forming the first nanometer metal line array on the chip pads of this application. Figure 2 This is a schematic diagram of the process of forming a second nano-metal wire array on the connection region on the substrate side of this application. Figure 3 This is a schematic diagram of an interlocking electrical connection structure.
[0018] In the diagram, 100 - chip; 101 - chip pad; 102 - first photoresist layer; 103 - chip-side metal substrate; 104 - chip-side porous film; 105 - first nano-metal line array; 106 - second photoresist layer; 200 - substrate; 201 - protective adhesive; 202 - substrate-side metal substrate; 203 - third photoresist layer; 204 - substrate-side porous film; 205 - second nano-metal line array; 206 - fourth photoresist layer; 300 represents an interlocking electrical connection structure. Detailed Implementation
[0019] To make the objectives and technical solutions of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this application. All other embodiments obtained by those skilled in the art based on the described embodiments of this application without creative effort are within the scope of protection of this application.
[0020] Those skilled in the art will understand that, unless otherwise defined, all terms used herein (including technical and scientific terms) have the same meaning as commonly understood by one of ordinary skill in the art to which this application pertains. It should also be understood that terms such as those defined in general dictionaries should be understood to have the same meaning as in the context of the prior art, and should not be interpreted in an idealized or overly formal sense unless defined as herein.
[0021] The term "connection" as used in this application can mean a direct connection between components or an indirect connection between components through other components.
[0022] The meaning of "and / or" as used in this application includes situations where each exists alone or both exist simultaneously.
[0023] The terms "inner" and "outer" as used in this application refer to the direction from the boundary of the pad area to the center of the pad, which is considered "inner" and vice versa, relative to the pad area itself; rather than a specific limitation on the device mechanism of this application.
[0024] The low-temperature chip packaging structure based on nanowires provided in this application includes: Figure 3As shown: a first nano-metal wire array 105 is formed on the pads of chip 100; and a second nano-metal wire array 205 is formed on the pads of substrate 200. Under preset conditions, the first and second nano-metal wire arrays are positioned so that they interpenetrate. By compressing the two nano-metal wire arrays, solid-state diffusion occurs between them under high pressure, dominated by van der Waals forces and metallic bonding forces. Through surface diffusion and / or grain boundary diffusion, an interlocking electrical connection structure is formed without the need for the overall melting of the metal structure in the traditional way. That is, this application can achieve atomic interpenetration through the interpenetrating bonding between nano-metal wire arrays to form an interlocking electrical connection structure.
[0025] The aforementioned nano-metal wire arrays located on the chip pads and substrate pads can be formed on the pads by chemical vapor deposition, physical vapor deposition, electrochemical deposition, template-assisted growth, or any one or a combination of the above deposition processes. The material of the nano-metal wire array can be optionally set as gold (Au), silver (Ag), copper (Cu), nickel (Ni), platinum (Pt), palladium (Pd), or an alloy of any of the aforementioned metal materials.
[0026] This application achieves an interlocking electrical connection structure on the pads by interlocking and bonding the aforementioned nano-metal arrays at a relatively low connection temperature of 170°C to 240°C and applying a pressure of at least 10 MPa. Therefore, the pad connection structure provided by this application avoids signal loss and interference introduced by parasitic inductance and capacitance in existing wire bonding processes through metal bonds formed by cold soldering, low-temperature sintering, or hot-pressing solid-state diffusion. It also avoids connection defects caused by differences in material expansion coefficients in existing heating processes above 300°C through a completely different bonding process path. Furthermore, the bonding process provided by this application does not require reflow, thus effectively avoiding flux residue and contaminants generated during processing.
[0027] In a more specific implementation, this application may configure the first nanometer metal array 105 on the chip pads to be generated on the chip pads in accordance with the following arrangements A1 to A4: Step A1: Remove the metal oxide layer on the surface of the chip pad 101, attach the first photoresist layer to the working area outside the chip pad, and deposit a metal substrate on the chip pad area exposed to the first photoresist layer. Step A2: After attaching the porous film to the first photoresist layer, a nano-metal structure is grown on the metal substrate along the pores of the porous film. Step A3: Remove the porous film; Step A4: Remove the first photoresist layer with a stripper solution to obtain the first nano-metal line array 105 grown on the chip pad 101.
[0028] However, for the substrate connected to the opposite side of the chip, considering that the substrate is usually made of glass, it is difficult for the second metal array on the substrate pads to be directly and stably attached to the glass material. Therefore, it is preferable to use the methods provided in B1 to B5 below to generate the second nano-metal line array 205 in order to achieve stable bonding with the first nano-metal line array 105: Step B1: Remove the metal oxide layer on the surface of the connection area on the substrate side, use the TGV hole metal surface obtained after removing the oxide layer as the substrate pad, apply protective adhesive 201 to the area outside the substrate pad, and apply a metal substrate plating layer to the pad area exposed to the protective adhesive. Step B2: After applying the third photoresist layer to the area where the protective adhesive is applied, a porous film is attached to the third photoresist layer. Step B3: Growing nano-metal structures along the pores of a porous thin film on a metal substrate coating; Step B4: Remove the porous film; Step B5: Remove the photoresist layer on the substrate using a photoresist remover to obtain the second nano-metal line array 205 grown on the connection areas of each substrate.
[0029] The second nanoscale metal wire array 205 was thus obtained.
[0030] After obtaining the aforementioned nano-metal wire arrays on both sides, this application can align the chip with the glass substrate in a flip-chip manner, so that the first nano-metal wire array 105 and the second nano-metal wire array 205 are opposite each other, maintaining the relative insertion of the metal wire structures on the chip side and the substrate side pads. Then, at a bonding temperature below 200°C and a bonding pressure of 25 MPa, the chip is pressed against the glass substrate, and a preset bonding time is maintained. Through the metal bonds between metal atoms activated by cold soldering, low-temperature sintering, or hot-pressing solid-state diffusion, an interlocking metal bond electrical connection structure is formed. The "activation" mentioned here mainly refers to the ability of the interconnected nanowire arrays formed in this application to achieve atomic-level metallurgical bonding through surface diffusion and grain boundary diffusion of the nanowire structure, driven by nanoscale effects. This is achieved at temperatures far below the melting point of bulk metals (e.g., for copper wires, the conventional bonding process uses a melting point of 170°C, and for silver wires, it uses a melting point of 250°C). Simultaneously, the mechanical interlocking between the wires caused by mutual pressing after interlocking provides structural strength, and electrical connection is achieved through metallic bonding. Therefore, this application can achieve [the following conditions] without the use of a dielectric or flux: Figure 3 The connection structure between the chip and the substrate shown enables a signal interaction path between the substrate and the chip.
[0031] To ensure the stable formation of the aforementioned bonding structure, this application generally prefers to grow nanoscale metal structures that meet the van der Waals force intermolecular spacing requirements on the metal substrate or pads using any one or a combination of chemical vapor deposition (CVD), physical vapor deposition (PVD), electrochemical deposition, template-assisted growth, or other deposition processes. Specifically, by selecting the pore size of the porous film, the average diameter of the nanoscale metal wires in the nanoscale metal structure is controlled within the range of 10 nm to 300 nm by utilizing the constraint of the film's own pore structure on the deposited metal material. Thus, within the porous film with pore sizes of 10 nm to 300 nm covering the chip pads 105 and the photoresist layer surface of the substrate connection area, nanoscale metal wires with lengths between 20 μm and 30 μm and diameters that meet the van der Waals force requirements in an interlocking state can be grown by controlling the current and time during the electrochemical reaction. After growing the required nanowire structures, the pads on both sides can achieve solid-state diffusion (surface diffusion, grain boundary diffusion) between the intersecting metal wires under pressure at a lower temperature, dominated by van der Waals forces and metal bonding forces. This allows atomic interpenetration to occur without overall melting, thus achieving a stable and robust metal connection structure.
[0032] Reference Figure 1 , Figure 2 In addition to the steps shown, this application further optimizes the manufacturing method of the nanowires corresponding to the metal substrate covering the entire wafer surface based on the aforementioned low-temperature packaging structure of nanowires, so as to improve the processing accuracy and connection strength of the electrical connection structure.
[0033] In this embodiment, the first nanometer metal array 105 on the chip pad 101 can be arranged in the following manner from C1 to C6. Figure 1 The process shown generates the data on the pads on the surface of chip 100: Step C1: Remove the metal oxide layer on the surface of the chip pad 101, attach the first photoresist layer 102 to the working area outside the chip pad 101, and deposit the chip-side metal substrate 103 on the pad area exposed to the first photoresist layer. Step C2: After attaching the porous film 104 on the chip side to the first photoresist layer 102, a nano-metal structure is grown on the chip side metal substrate 103 along the pores of the porous film. Step C3: Remove the porous film 104 on the chip side; Step C4: Remove the first photoresist layer using a resist remover; Step C5: Apply a second photoresist layer 106 on the nano-metal structure, exposing the metal substrate outside the pads. Then, use an etching solution to completely etch the metal substrate outside the pads. Step C6: The second photoresist layer 106 on the nano-metal structure is removed by a photoresist remover to obtain the first nano-metal line array 105 grown on the chip pad 101.
[0034] In this embodiment, considering that the metal substrate will still adhere to the entire wafer surface after the photoresist is removed, in order to remove the metal substrate outside the pads and retain the metal substrate on the pads, this application can further cover the surface of the generated nano-metal structure with a layer of photoresist, and then etch the remaining metal positions.
[0035] Corresponding to the chip pad side of this embodiment, the second metal array on its inorganic substrate connection area can preferably be arranged in the manner provided by D1 to D7 as follows. Figure 2 The process shown generates a second nanoscale metal wire array 205 to stably attach the metal array to the inorganic substrate 200, achieving a stable bond with the first nanoscale metal wire array 105: Step D1: Remove the metal oxide layer on the surface of the substrate side pads, apply protective adhesive 201 to the working area outside the pads, and apply a plating structure to form the substrate side metal substrate 202 on the pad area exposed to the protective adhesive 201. Step D2: After applying the third photoresist layer 203 to the protective adhesive adhesion area, a porous film 204 on the substrate side is attached to the third photoresist layer 203. Step D3: Growing a nano-metal structure along the pores of the porous film 204 on the substrate side of the metal substrate. Step D4: Remove the porous film 204 on the substrate side; Step D5: Remove the third photoresist layer 203 using a photoresist remover. Step D6: Apply a fourth photoresist layer 206 on the nano-metal structure and expose the metal substrate outside the pads. Then, use an etching solution to completely etch the metal substrate outside the pads. Step D7: The fourth photoresist layer 206 on the nano-metal structure is removed by a photoresist remover to obtain the second nano-metal line array 205 grown on each pad.
[0036] In practical applications, this application can achieve chip-to-glass substrate connection by using copper nanowires and low-temperature hot pressing in the following manner: like Figure 1 , Figure 2As shown at the top, this embodiment provides a silicon-based chip (PIC) wafer with an optical structure and a silicon-based chip (EIC) wafer with an electrical structure. In this embodiment, the metal stacking structure of the first pad 101 on the surface of the chip 100 is Al / Cu or Cu, serving as a catalyst and adhesion layer for nanowire growth. Before growth, the wafer and substrate are subjected to plasma cleaning to remove surface organic contaminants and activate the surface. Using porous thin film and electrochemical deposition processes, the first nanowire array 105 on the chip is obtained.
[0037] The chip wafer with grown nanowires is diced to obtain individual chips. A high-precision flip-chip bonder is used to pick up and invert the chips.
[0038] Then, refer to Figure 2 As shown, pads are formed in several TGV holes on the borosilicate glass substrate 200 where the chip needs to be connected by via electroplating. CMP process is used to make the glass substrate surface flat and expose the fresh surface of the Cu metal. A layer of PI adhesive is applied to the glass substrate surface as a protective adhesive to remain on the wafer surface to protect the wafer, and the Cu metal structure of the pads is kept exposed during the application of this protective adhesive, forming a full-surface substrate-side metal substrate 202 on the pads.
[0039] Subsequently, a layer of photoresist is coated onto the surface of the glass substrate. The exposed areas of the photoresist define the locations of the pads where the nanowires need to be grown. After photoresist coating, exposure, and development, the pads on the glass substrate and chip are exposed. A porous film with a thickness between 3 and 8 μm is then laminated onto the photoresist surface. This porous film defines the locations where the nanowires need to be grown, and its voids ensure that the nanowires are oriented according to the pore size in the film. This allows the metal wires to grow from bottom to top along the multiple pores of the porous film using an electrochemical deposition process. Therefore, after trimming the grown nano-metal wire structure, the metal substrate outside the pads can be removed by etching process to obtain the second nano-metal wire array 205.
[0040] Thus, in this embodiment, after using electrochemical deposition to grow multiple metal nanowires with an average diameter of 10 nanometers to 300 nanometers and an average length of 1 micrometer to 20 micrometers on the surface of the pads, the pads on both sides can be joined together to prepare for nanowire bonding.
[0041] When fabricating nanowires on both sides, the length of the nanowires is generally controlled to be between 80% and 90% of the thickness of the porous film structure itself, which is composed of AAO templates or similar structures. During the formation of the nanowires, the length of the metal can be controlled through real-time electrochemical monitoring (It curve) and pulse electrodeposition to ensure uniformity and the thickness relative to the porous film. In the process, we can keep the nanowires upright through supercritical drying, which facilitates the successful interpenetration of the metal fibers between the nanowire arrays on both sides of the chip and the substrate. Finally, a stable interconnect electrical pathway structure is achieved through metal deformation and solid-phase diffusion caused by pressure.
[0042] During bonding, the chip is flip-chip mounted on the glass substrate, allowing the first and second nanowire arrays to interlock and intertwine within a temperature range of room temperature to 180°C. A pressure of 15 MPa is applied to the opposing nanowire arrays. During this pressure application, the interlaced nanowires bend and entangle due to their flexibility, forming an interlocking structure of mechanical solid-state bonding at multiple contact points. At this point, due to the extremely high specific surface area and surface energy of the nanowires, metal atoms can be activated at their contact points and undergo rapid solid-state diffusion and sintering, forming strong metallic bonds. Ultimately, a structure is formed as shown... Figure 3 The diagram shows a three-dimensional, porous, conductive interconnect structure 300 composed of countless interwoven nanowires.
[0043] Therefore, this embodiment can obtain nanowires with a large specific surface area on the pad surface by introducing porous alumina into the surface of the metal pad, guiding the electrodeposition or chemical deposition of metal nanowires within the channels of the porous film, and then etching away the unwanted metal structure. By selecting the diameter and length of the nanowires, this embodiment utilizes the high flexibility and ductility of copper nanowires to ensure that the interlocking metal wires on the substrate side and chip side can stably withstand a certain degree of bending and stretching, while maintaining their electrical connection structure without breakage.
[0044] In summary, this application places the chip on a glass substrate using a flip-chip method, allowing the tops of the first nanometer metal wire array on the chip and the second nanometer metal wire array on the glass substrate to contact, align, and physically mechanically weave and interlock. By applying specific temperature and pressure conditions, the nanometer metal wires on both sides of the chip and the substrate can undergo plastic deformation and tightly wrap around each other. Utilizing the huge specific surface area and highly active surface atoms of the metal wires on both sides, a large number of solid-state bonds are formed at the contact points, thereby constituting a unified three-dimensional interconnect network with excellent conductivity and mechanical strength, providing reliable mechanical strength and stable electrical pathways. The low-temperature chip packaging structure and manufacturing method provided in this application have the following advantages compared to traditional connection methods: 1. Extremely low bonding temperature, protecting sensitive devices: The core advantage of this invention lies in its extremely low bonding temperature. Depending on the selected metal material and process parameters, the bonding process can be completed in the range of room temperature to 240°C. The low-temperature process significantly reduces the residual stress generated during cooling due to coefficient of thermal expansion mismatch (CTE mismatch), reducing the risk of chip cracking or solder joint fatigue.
[0045] 2. A completely clean bonding process ensures optimal optical performance: The bonding process of this invention is completed in a solid state, without involving the melting of any solder, thus eliminating the need for flux. This fundamentally eliminates the problem of flux residue contaminating optical components (such as lenses, gratings, and laser output ports), saving expensive and complex cleaning steps. The entire bonding environment can maintain a high degree of cleanliness, preventing particulate contamination such as solder ball spatter that may occur during reflow soldering. This is crucial for fields requiring extremely high cleanliness, such as optical module packaging, CMOS image sensor packaging, and MEMS device packaging.
[0046] 3. Superior Mechanical Connection Strength and Reliability: The interconnect structure of this invention does not rely on a single interface connection, but is formed through three-dimensional interlocking and entanglement between two sets of nanoscale metal wire arrays. This mechanical interlocking structure, similar to a "micro-Velcro," combines metallic bonds formed at countless contact points, providing extremely high mechanical strength.
[0047] 4. Excellent High-Frequency Electrical Performance: The nanowires themselves are excellent conductors. Through the interconnect structure formed by this invention, current can be transmitted from the chip to the substrate via tens of thousands of parallel paths of nanowires. This large-scale parallel effect results in extremely low total contact resistance. In contrast, the contact resistance of traditional solder ball connections is typically in the tens of milliohms. The extremely low contact resistance provided by this application means lower power loss and less signal attenuation. Simultaneously, the interconnect height (i.e., nanowire length) can be precisely controlled at the micrometer level, much shorter than wire bonding, thereby further reducing the parasitic inductance generated by the electrical connection structure. The extremely low impedance provides an ideal electrical path for ultra-high-speed signal transmission exceeding 200 Gbps / lane.
[0048] 5. Process Flexibility and Cost Potential: The growth processes of nanowires (such as CVD, PVD, and electroplating) are highly compatible with standard semiconductor wafer-level manufacturing processes, allowing for easy integration into existing production lines to achieve wafer-level nanostructure fabrication, thereby significantly reducing unit costs. Compared to expensive silicon interposers and complex heterogeneous integration technologies, the use of low-cost glass substrates combined with the low-temperature bonding technology of this invention provides a highly cost-effective solution for high-performance optical modules and other advanced packaging.
[0049] The foregoing has shown and described the basic principles, main features, and advantages of this application. Those skilled in the art should understand that this application is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of this application. Various changes and modifications can be made to this application without departing from the spirit and scope thereof, and all such changes and modifications fall within the scope of this application as claimed. The scope of protection of this application is defined by the appended claims and their equivalents.
Claims
1. A low-temperature chip packaging structure based on nanowires, characterized in that, include: A first nanoscale metal wire array (105) is formed on the chip pad (101). A second nano-metal wire array (205) is formed on the connection region on the substrate side. An interlocking electrical connection structure is formed by interleaving and bonding two nano-metal wire arrays (105 and 205) under preset conditions.
2. The low-temperature chip packaging structure based on nanowires as described in claim 1, characterized in that, The materials of the nano-metal wire array include: gold, silver, copper, nickel, platinum, palladium, or alloys of any of the aforementioned metal materials.
3. The low-temperature chip packaging structure based on nanowires as described in claim 1, characterized in that, The preset conditions are: a connection temperature of 170°C to 240°C and a connection pressure of at least 10 MPa applied to the pads.
4. The low-temperature chip packaging structure based on nanowires as described in claim 3, characterized in that, The interlocking electrical connection structure includes metallic bonds formed by solid-state diffusion and sintering between metal atoms activated by preset environmental conditions.
5. The low-temperature chip packaging structure based on nanowires as described in claim 3, characterized in that, The first nano-metal wire array (105) and the second nano-metal wire array (205) are respectively formed along the porous film covering the connection area surface of the chip pad (101) and the substrate side by chemical vapor deposition, physical vapor deposition, electrochemical deposition, template-assisted growth or any one or a combination of the above deposition processes.
6. The low-temperature chip packaging structure based on nanowires as described in claim 5, characterized in that, The average diameter of each nanowire in the first nanowire array (105) and the second nanowire array (205) is in the range of 10 nanometers to 300 nanometers.
7. A method for manufacturing a chip cryogenic packaging structure based on nanowires, used to manufacture the chip cryogenic packaging structure based on nanowires as described in claims 1-5, characterized in that, The nano-metal wire arrays are generated on the pads according to the following steps: Remove the metal oxide layer on the surface of the pads, apply photoresist to the working area outside the pads, and plate a metal substrate on the pad area exposed to the photoresist. After a porous film is attached to a photoresist, a nanostructure is grown on a metal substrate along the pores of the porous film. Remove porous films; Remove the photoresist to obtain nano-metal line arrays grown on each pad.
8. The method for manufacturing a low-temperature chip packaging structure based on nanowires as described in claim 7, characterized in that, After generating a first nano-metal wire array (105) and a second nano-metal wire array (205) on the chip pad (101) and the connection area on the substrate side, respectively, an interlocked electrical connection structure is formed according to the following steps: the first nano-metal wire array (105) and the second nano-metal wire array (205) are placed opposite each other so that the nano-metal wires in the array interpenetrate each other, and an interlocked electrical connection structure is formed by metal bonds formed by cold soldering, low temperature sintering or hot pressing solid phase diffusion.
9. The method for manufacturing a low-temperature chip packaging structure based on nanowires as described in claim 7, characterized in that, On a metal substrate, nanostructures are grown along the pores of a porous thin film using any one or a combination of autochemical vapor deposition, physical vapor deposition, electrochemical deposition, template-assisted growth, or other deposition processes.
10. The method for manufacturing a low-temperature chip packaging structure based on nanowires as described in claim 7, characterized in that, After removing the metal oxide layer on the surface of the pads and before applying photoresist, a protective adhesive is applied to the working area outside the pads so that the metal substrate can adhere to the pad area exposed to the protective adhesive. The photoresist is applied to the area where the protective adhesive is attached; The thickness of the photoresist is between 3 and 8 μm; the length of the nano-metal lines on the surface of the pads is between 20 μm and 30 μm.