Methods and systems for determining parameters of high-temperature liquids

By using an acceleration device above the surface of a high-temperature liquid to accelerate the sensor unit for measurement, the problems of high invasiveness and inaccurate measurement in metallurgical processes are solved. This enables rapid and reliable measurement of high-temperature liquid parameters, reduces equipment complexity and operational hazards, and improves measurement frequency and accuracy.

CN123076785APending Publication Date: 2026-11-10贺利氏电测骑士有限公司
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202580026828.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-06-21
Filing Date
2025-03-10
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing technologies for measuring high-temperature liquid parameters in metallurgical processes suffer from problems such as high invasiveness, operational hazards, inaccurate measurements, low frequency, high cost, and complex equipment. In particular, it is difficult to achieve non-invasive, rapid, and reliable parameter measurements in electric arc furnaces.

Method used

An acceleration device is used to provide a sensor unit above the surface of a high-temperature liquid. The acceleration device accelerates the sensor unit and causes it to enter the surface of the high-temperature liquid at a high speed, reducing the immersion depth and time. The sensor unit is then used to measure parameters.

Benefits of technology

It enables non-invasive, rapid, and reliable measurement of high-temperature liquid parameters, reduces equipment complexity and operational hazards, improves measurement frequency and accuracy, and reduces interference with metallurgical facilities and energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076785A_ABST
    Figure CN123076785A_ABST
Patent Text Reader

Abstract

This invention relates to a method for determining at least one parameter of a high-temperature liquid using a sensor unit, and a system for implementing the method. A measuring probe releasably carrying the sensor unit is provided to an acceleration device that accelerates the sensor unit after it is separated from the measuring probe. The acceleration device is provided at a distance D from the surface of the high-temperature liquid. A The distance D between the surfaces of the high-temperature liquid. A Less than the distance D from the surface of the high-temperature liquid to the container opening M 50%. The sensor unit emits in the direction of the high-temperature liquid, is immersed below the surface, and measures the parameter of interest. The invention also relates to a system suitable for implementing the method of the invention and a metallurgical container including the system of the invention.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This invention relates to a method for determining at least one parameter of a high-temperature liquid using a sensor unit, and a system for implementing the method. The invention also relates to a metallurgical container incorporating the system of the present invention.

[0002] Particularly during metal manufacturing processes in the steel industry, several parameters of the molten metal are critical for controlling the metallurgical process, such as the molten pool chemistry or temperature. For both economic and quality reasons, the ability to continuously and / or periodically monitor these variables is highly desirable. Accurate monitoring can significantly reduce energy consumption caused by overheating. Other benefits of continuous monitoring include the ability to measure high-temperature phase transitions, chemical reactions, and other related phenomena.

[0003] Methods and apparatus for determining these process-related parameters are known in the art, and typically involve the use of disposable probes that carry sensors. Typically, the probes are brought below the surface of the melt either in the form of drop-in units or by means of a spray gun assembly. The spray gun assembly can be operated manually, fully automatically, or semi-automatically. Sensors are typically connected via wires or cables to processing equipment for processing the recorded data, but wireless data transmission is also described. The data is acquired and processed in real-time or near real-time, providing operators of the metallurgical facility with critical information about the progress or status of the metal manufacturing process occurring within the vessel.

[0004] The spray gun assembly used to introduce the probe into molten metal requires many parts, with at least one measuring head carrying the disposable sensor and the spray gun itself. The spray gun is immersed into the melt from an opening in the container (i.e., close to the molten metal), causing metal splatter and posing a hazardous operation, especially when operated manually. To introduce such a spray gun into the molten metal, the operation of the metallurgical container must be interrupted to open it, reducing process yield. Measurement quality varies depending on the operator used. Measurement accuracy depends on several parameters, such as the immersion depth and immersion rate of the probe in the liquid metal melt. Immersion that is too slow causes premature probe burn-out and erroneous measurements. Insufficient probe immersion depth can lead to temperature instability or unreliable electromotive force of the oxygen sensor. From a safety perspective, manual operation of such spray guns is also undesirable—the general trend in industry is towards "unmanned" operation as much as possible.

[0005] Automated equipment solves this problem, but requires significantly more operating equipment and maintenance. Operation of such equipment also relies on probes being inserted through relatively large openings. Furthermore, all facilities near the container are susceptible to heat or mechanical damage, and the required openings must be kept unobstructed.

[0006] Furthermore, as described, for example, in WO 2015070316 A1, a new probe must be installed on the spray gun after each measurement, which may require additional components, process steps, and extend the time interval between subsequent measurements. Therefore, a higher measurement frequency is desired.

[0007] Especially in the field of electric arc furnaces (EAFs), currently only a limited number of methods are available for determining the parameters of molten metal, which can be done during vessel operation. EAFs produce steel by melting one or more charges—scrap metal, hot metal, iron-based materials, or other fusible materials—placed within the furnace using an electric arc. In a common procedure in EAFs, the operator manually inserts a lance carrying a suitable sensor into the furnace through a slag door, a relatively wide opening in the furnace shell. When the slag door is open, any slag and metal trapped at the door opening must be removed to allow for the insertion of the measuring probe. Such an invasive step is highly undesirable because it disrupts the environment within the vessel during the metallurgical process. Furthermore, energy is wasted due to the intake of cold ambient air through the slag door when it is open.

[0008] For measurements using drop-in sensors, the measuring probe is dropped into a container containing the molten metal. Suitable probes are disclosed, for example, in EP 0758445 A1. In current practice, the sensor is introduced from a relatively large height above the container containing the molten metal, typically within a range of 10 to 20 meters above the surface of the molten metal. Such sensors cannot be used in these facilities due to the design of the EAF (Electrical Adjustable Surface) in which the electrodes are positioned above the container.

[0009] Several probes can be stored in a cartridge, and one probe is released from the cartridge for each measurement. The probe falls in free fall, accelerated by gravity, and plunges into the molten metal. Therefore, the final velocity of the probe upon reaching the surface of the molten metal is determined by the distance between the drop station and the molten metal. The probe needs to have a certain mass to plunge sufficiently deep below the surface of the melt to obtain reliable measurement data. Additional components (such as a counterweight) are needed, independent of the recording of the measurement itself, to provide the required orientation of the sensor in order to provide reliable data. Therefore, drop-in sensors introduce a relatively large amount of additional contaminant material into the molten material being measured. Furthermore, the immersion point cannot be reliably controlled.

[0010] Molten metal is typically covered with a slag layer during its production, subjecting any probes or sensors passing through it to increased corrosive conditions, regardless of the specific method used. Therefore, it is desirable to minimize the duration of sensor exposure to slag as much as possible.

[0011] Known injection devices used in the metallurgical field are used to introduce liquid and / or granular materials for pyrometallurgical treatment of molten metal. Particularly in EAFs (Extractable Aerated Furnaces), such injectors are used to blow oxygen-enriched gas, lime, and / or carbonaceous particles into the metallurgical vessel. Typically, these devices are positioned near the surface of the molten metal to be treated through appropriate openings in the vessel. Typically, such injectors are provided as combined units located in a so-called cold box, which is a protective compartment provided adjacent to the interior of the vessel. During operation, all openings are typically kept unobstructed by a flow of nitrogen or compressed air. Therefore, further openings are not desirable, as increased gas requirements would increase operating costs. Thus, it would be advantageous to provide methods for further utilizing the available openings.

[0012] Given the existing technology, there is a need for an improved measurement method and system to allow non-invasive measurements with little or no human intervention, insertion of a spray gun, or equivalent invasive actions. Furthermore, a rapid and reliable method is needed that can be performed frequently and provides reproducible results. Additionally, the mass of material introduced through the measurement should be minimized.

[0013] Therefore, the object of the present invention is to provide an improved method for determining at least one parameter of a high-temperature liquid (such as molten metal) using a sensor unit, which solves at least one of the problems discussed above.

[0014] Specifically, one objective is to provide an improved method that allows the use of a simplified sensor unit with reduced weight and number of parts. Furthermore, an objective of the invention is to provide a method for obtaining parameters when the sensor unit is submerged at a certain depth below the surface of a hot liquid.

[0015] An additional aspect of the object of the present invention is to provide a method that allows for simplification of the hardware required to implement the method. Furthermore, the sensor unit should be introduced into the container containing the high-temperature liquid using an available inlet point within the container.

[0016] A further objective is to minimize the time the sensor unit is exposed to the environment in the container before being immersed in the hot liquid.

[0017] Another object of the present invention is to provide a system configured to implement the method of the present invention.

[0018] Another object of the present invention is to provide a system for implementing the method of the present invention, which allows for the determination of parameters in terms of equipment, control technology and organization with reduced workload and cost, while achieving increased reliability and quality of the obtained measurements.

[0019] Another object of the present invention is to provide a metallurgical container comprising a system configured to implement the method of the present invention.

[0020] Another object of the present invention is to provide an apparatus comprising an acceleration device configured to carry out the method of the present invention.

[0021] These objectives are achieved through the subject matter defined in the independent claims.

[0022] This invention provides a method for determining at least one parameter of a high-temperature liquid using a sensor unit.

[0023] The high-temperature liquid includes a surface and is provided in a metallurgical vessel, the metallurgical vessel including a top opening opposite the surface of the high-temperature liquid, and the surface of the high-temperature liquid level has a position L. M This location is at a distance D from the top opening of the metallurgical vessel. M The method includes:

[0024] (a) The distance D between the surface of the high-temperature liquid and the top opening of the metallurgical vessel A An acceleration device is provided above the surface of the high-temperature liquid, wherein the acceleration device is adapted to increase the speed of the sensor unit;

[0025] (b) Providing the acceleration device with a measurement probe, wherein the measurement probe carries the sensor unit, and wherein the sensor unit is detachable from the measurement probe;

[0026] (c) The sensor unit is separated from the measuring probe;

[0027] (d) Accelerate the sensor unit using the acceleration device;

[0028] (e) The sensor unit is emitted in the direction of the high-temperature liquid;

[0029] (f) Immerse the sensor unit under the surface of the high-temperature liquid;

[0030] (g) Measure at least one parameter of the high-temperature liquid;

[0031] Its characteristic is D A < 50% D M .

[0032] The steps of this method are performed in a given sequential order.

[0033] Surprisingly, it has been found that the acceleration of the sensor unit offers several advantages beyond just gravity. The probe housing the sensor unit can be reduced in weight, size, and number of components. Reduced material requirements lead to lower costs and less contaminant material introduced into the high-temperature liquid. This miniaturization of the sensor and its associated carrier probe, in turn, allows the sensor unit to be introduced through a smaller opening that was previously unusable for introducing probes using existing techniques.

[0034] Furthermore, placing the acceleration device at a short distance from the high-temperature liquid further minimizes the time the sensor unit is exposed to the container environment. In metallurgical facilities, inlet points for handling molten metal are typically placed at a short distance from the metal surface and are considered unsuitable as inlet points for measuring equipment due to their harsh environment. These inlet points can be used in a dual-function manner by the method of the present invention, namely for introducing the processed material and for the sensor unit. Particularly in containers where there is no top-side inlet available for introducing measuring equipment, the method of the present invention expands the possibility of obtaining reliable data.

[0035] Another advantage of the method of the present invention is that it does not use a spray gun at all, which further reduces the need for components such as drive or control devices for operation. Therefore, the method can be applied to almost all metallurgical vessels. Additionally, it minimizes the need for human interaction, enhancing operational safety. Particularly in EAFs, this provides the additional advantage of eliminating the need for an opening in the slag door to obtain measurements. Furthermore, interruptions to the metallurgical facility can be minimized to obtain the desired parameters; in particular, the method is suitable for continuous operation. This minimizes total operating costs, especially the required energy input, and increases the productivity of the metallurgical facility and the quality of the products produced.

[0036] Another factor that reduces the system's installation and maintenance requirements is a simplified operating system that can be located at a short distance from containers containing hot liquids.

[0037] Furthermore, due to the controlled angle and velocity of immersion, this method allows the sensor unit to be placed in reproducible impact zones on and within the surface of high-temperature liquids.

[0038] This invention relates to the determination of parameters for high-temperature liquids. High-temperature liquids should be understood as liquids with temperatures above 600°C, preferably above 800°C, and more preferably above 1000°C. The temperature of a high-temperature liquid can, for example, be in the range of 1000°C to 1900°C, more preferably in the range of 1200°C to 1800°C, and even more preferably in the range of 1400°C to 1700°C.

[0039] The properties of the high-temperature liquid are not further limited, but preferably the high-temperature liquid is a melt of a material with a melting point above 500°C, particularly a melt of metal, cryolite, or glass. Preferably, the high-temperature liquid is a molten metal, most preferably molten steel. The terms "molten" or "molten metal" do not exclude the presence of any solid or gaseous portion, including, for example, the non-molten portion of the corresponding metal. The temperature of a metal melt varies and generally depends on the composition of the metal and the stage of the melting process.

[0040] In the case of molten metal, the melt may be covered with a layer of slag. The term "slag" refers to a non-steel byproduct that is typically produced in steelmaking furnaces and usually exists as molten material floating on top of the molten metal. Slag may include metal oxides, metal sulfides, calcium oxide, magnesium oxide, magnesite, dolomite, iron oxide, aluminum oxide, manganese oxide, silicon dioxide, sulfur, phosphorus, or combinations thereof. To obtain reliable measurements, the sensor introduced into the melt should pass through the slag layer as quickly as possible to minimize corrosion before reaching the final point of measurement and before the slag material freezes on the cold sensor. Such a frozen layer needs to melt when the sensor finally reaches the molten metal before a reliable measurement can be made, thus extending the time the sensor needs to withstand the decomposition environment of the molten metal.

[0041] The high-temperature liquid is supplied in a metallurgical vessel; in other words, the high-temperature liquid is supplied in the form of a molten pool in a suitable vessel. The high-temperature liquid includes a surface, and therefore also a bottom side. The bottom side should be understood as the side of the molten pool of the high-temperature liquid that is in contact with the interior of the metallurgical vessel opposite the surface.

[0042] The metallurgical container can be any container suitable for containing high-temperature liquids, and can be, for example, a metal processing container or a furnace, particularly an electric arc furnace. In a preferred embodiment, the metallurgical container is an electric arc furnace.

[0043] The metallurgical vessel includes a bottom and a top opening opposite the bottom. The bottom should be understood as part of the metallurgical vessel, which is at least partially in contact with the high-temperature liquid, particularly with the bottom side of the high-temperature liquid molten pool. The surface of the high-temperature liquid level has a position L. M Its distance from the top opening of the metallurgical container is D. M .

[0044] Preferably, the metallurgical vessel includes facilities fixedly mounted thereon or thereon. Such facilities may be, for example, devices for heating, electrodes, measuring devices, or devices for handling high-temperature liquids. In the case of molten metal, such devices for handling molten metal may be, for example, carbon injectors, lime injectors, oxygen lances, oxy-fuel lances, or air-fuel burners.

[0045] Metallurgical vessels typically include an inner surface defining an internal volume suitable for containing a hot liquid, such as a pool of molten metal or molten glass. As used herein, the term "molten metal pool" is used in particular to describe molten metal in a metallurgical vessel. The inner surface of a metallurgical vessel may include a bottom and at least one or more sidewalls.

[0046] Typically, such metallurgical vessels also include at least one inlet point through which a high-temperature liquid, preferably a molten metal pool, can be accessed and / or processed. This inlet point may be located in the sidewall. In the case of an EAF (Extremely Aerated Container), multiple openings may be used: a larger opening, often referred to as a slag gate, and the inlet point located in the sidewall.

[0047] This invention provides a method for determining parameters of a high-temperature liquid. The parameters can be physical, chemical, or metallurgical parameters, such as temperature, the presence and / or concentration of chemical compounds, particularly oxygen content, carbon content, hydrogen content, nitrogen content, aluminum content, or chemical composition.

[0048] The term "determine parameter" may be used herein as a synonym for measurement parameter. According to a preferred embodiment, the parameter may be determined by single-point measurement or multi-point measurement. This determination may include determining a single parameter or a combination of more than one parameter. For example, the determination may include measuring the oxygen content of a high-temperature liquid. The determination may also include measuring both oxygen content and temperature.

[0049] The parameters of the high-temperature liquid are determined using a sensor unit. In other words, the sensor unit is adapted to measure at least one parameter of the high-temperature liquid. It should be understood that the sensor unit includes at least one sensing element; it may include additional components. The sensor unit is, in principle, configured as a disposable component that dissolves or burns in the high-temperature liquid after the parameter is determined. Parts of the sensor unit may have dissolved before or during parameter determination.

[0050] The sensor unit includes a sensing element, which may be selected from at least one of the following: an electrochemical sensor, an electromagnetic sensor, an optical sensor, a thermoelectric sensor, a sensor for detecting voltage, a sensor for detecting current, a sensor for detecting resistance, or any combination of said sensors, such that combined measurements of several parameters can be performed.

[0051] Specifically, the sensor unit may include a thermocouple and / or an electrochemical cell for measuring the temperature of a high-temperature liquid, preferably an electrochemical cell for determining the oxygen activity of the high-temperature liquid.

[0052] Electrochemical cells (particularly those used to determine oxygen activity) may include a solid electrolyte tube closed at one end and containing a reference material and an electrode at the closed end. Such sensors are disclosed, for example, in EP0059222 A1. Electrochemical cells may also be provided as needle sensors, comprising conductive wires serving as electrodes having at least a solid electrolyte coating and a reference material coating. Such sensors are disclosed, for example, in US 5332449 A.

[0053] The sensor unit may include a molten pool contact. A molten pool contact should be understood as a conductive device that provides electrical contact between the sensor unit and the high-temperature liquid. The molten pool contact may be made of a metal, such as molybdenum (Mo) or steel. The molten pool contact may be annular or rod-shaped; preferably, it is annular. When the sensor unit includes a thermocouple, such annular molten pool contact preferably surrounds the thermocouple.

[0054] Preferred sensor units include a needle sensor for determining oxygen activity, a thermocouple (preferably encapsulated in a quartz sheath), and an annular molten pool contact surrounding the thermocouple. Such sensor units have a compact and robust design, which allows for miniaturization of the measuring probe that carries them.

[0055] Preferably, the sensing element of the sensor unit is embedded in an immersion body. Such an immersion body is provided with a sheath in such a way that the sensing element remains operable throughout the measurement duration. Furthermore, once the sensor unit is immersed, the immersion body aligns the sensor unit, giving the sensing element a suitable orientation and measurement position for determining the parameter of interest. Additionally, the immersion body preferably surrounds the connection between the sensing element and the signal lines, providing further protection for these sensitive and critical components of the sensor unit. Preferably, the immersion body is made of an insulating material (typically metal). In a preferred embodiment, the immersion body is made of steel, stainless steel, or copper.

[0056] Preferably, the sensor unit has a weight of less than 1500g, more preferably less than 1000g, even more preferably less than 800g, and most preferably less than 500g. Currently used drop-in sensors weigh between 4kg and 6kg. The method of the present invention allows for a significant reduction in this weight, reducing the amount of material introduced into the high-temperature liquid and additionally reducing production costs due to material savings. Furthermore, the measurement is only minimally affected by the cold mass introduced by the lightweight sensor unit, allowing for reliable and accurate data.

[0057] Preferably, the sensor unit has a density higher than that of the high-temperature liquid. It has proven particularly advantageous when the density of the sensor unit is at least 5% higher than that of the high-temperature liquid, more preferably at least 8%, and even more preferably more than 10%. The density of the sensor unit can be higher than 7.2 g / cm³. 3 More preferably higher than 7.5 g / cm³ 3 .

[0058] Preferably, the sensor unit does not include any additional weight or floating components. Due to the high speed provided by the acceleration device, further balancing of the sensor unit is unnecessary. Therefore, the sensor unit design can be simplified and miniaturized. This miniaturization further allows, in particular, the sensor unit to be introduced into the metallurgical vessel through available inlet points for which conventional drop-in sensor or spray gun systems would be too large.

[0059] Preferably, the sensor unit is configured to be connected to a processing unit. Such a processing unit is configured to process the measurement data from the sensor unit and determine the parameters of the high-temperature liquid.

[0060] The sensor unit may be covered with a protective element that covers the sensing element during processing and protects it from damage caused by impacts to the surface of the high-temperature liquid. Preferably, the sensor unit is covered with a protective cap that at least encloses the sensing element and is formed of a material that dissolves or melts in the high-temperature liquid. It should be understood that such a protective element is not part of the sensor unit when considering its density.

[0061] Preferably, the sensor unit includes a contact element adapted to connect the sensor unit to a suitable device for transmitting measurement data, preferably to a signal line. The sensor unit typically includes an immersion end and a contact end. Advantageously, the contact element is arranged on or within the contact end of the sensor unit. Such a contact element allows for easy mounting of the sensor unit in or at a measurement probe, provides stable contact with the signal line, and reduces forces on the sensor unit during acceleration.

[0062] The method according to the invention includes providing an acceleration device suitable for increasing the velocity of a sensor unit. In other words, the acceleration device is adapted to launch the sensor unit in a predetermined direction. Therefore, the acceleration device is sized, configured, and arranged as a channel for accommodating the sensor unit.

[0063] The accelerator is positioned above the surface of the hot liquid. In other words, the accelerator is positioned above the highest permissible level of the hot liquid surface. The highest permissible level is the level of the hot liquid reached when the container is filled with its maximum fill capacity. "Above" in relation to the hot liquid in the container refers to a position above zero level, which exists at the bottom of the container. In configurations where the hot liquid is covered by another layer of material (e.g., a slag layer), the accelerator is (if preferably) positioned above this other material layer.

[0064] Preferably, the acceleration device is adapted to separate the sensor unit from at least one additional component of the measuring probe and accelerate the sensor unit. It should be understood that at least one additional component of the measuring probe is not accelerated.

[0065] When the sensor unit is connected to the processing unit via a signal line (e.g., via a cable or wire), the signal line is not specifically accelerated by the acceleration device, but rather pulled behind the accelerated sensor unit. However, a portion of the signal line, particularly the portion directly connected to the sensor unit, will naturally also be accelerated by the acceleration device.

[0066] The acceleration device is provided at a distance D from the surface of the high-temperature liquid. A The distance D between the surfaces of the high-temperature liquids. A Less than the distance D from the surface of the high-temperature liquid to the opening of the container. M 50% (D) A <50% D M In other words, the accelerating device is preferably positioned below half the distance from the hot liquid to the top opening of the container including it.

[0067] Previously, it was assumed that it was not feasible to provide the sensor unit near the hot liquid, i.e., in an apparatus that provides it before it is introduced into the metallurgical container, because the gravitational velocity gained over the significantly shortened travel distance would be insufficient for a proper impact across the surface of the hot liquid. Surprisingly, it has been found that such positioning of the acceleration device is not only suitable for but even advantageous for the method of the present invention, even though the distance to the hot liquid surface is significantly shorter than in classical installations. Furthermore, it allows for several advantages. The proximity to the hot liquid surface shortens the distance the sensor unit must travel through the interior of the metallurgical container, which allows for a reduction in the amount of protective devices and / or materials required for the sensor unit, as well as the required signal line length, resulting in reduced material requirements and thus lower manufacturing costs for disposable components. Additionally, the reduced residence time of the sensor unit inside the container before immersion in the hot liquid mitigates the corrosive effects of the high-temperature environment.

[0068] Preferably, the distance D A Less than the distance D from the surface of the high-temperature liquid to the opening of the container.M 40% (D) A <40% D M (and even more preferably, distance D) A Less than the distance D from the surface of the high-temperature liquid to the opening of the container. M 30% (D) A <30% D M ).

[0069] Preferably, the acceleration device is positioned in and / or on the sidewall of the metallurgical vessel supplying the high-temperature liquid. Therefore, the acceleration device is preferably positioned laterally to the surface of the high-temperature liquid; in other words, the acceleration device is laterally positioned to the high-temperature liquid. It was previously assumed that it was not possible to provide the sensor unit laterally, i.e., in equipment that provides it before its introduction into the metallurgical vessel, because the harsh environments at these locations were unsuitable as entry points. Surprisingly, it has been found that lateral positioning of the acceleration device is not only suitable but even advantageous for carrying out the method of the present invention, even though the distance to the surface of the high-temperature liquid is significantly shorter than that in classical installations.

[0070] The accelerator can extend into or be adjacent to the volume of the metallurgical vessel containing the high-temperature liquid through an opening in the sidewall of the vessel. In other words, the accelerator preferably extends through the sidewall of the vessel. It is advantageous to position the accelerator on the side of the molten pool, particularly where access from a vertical position above the vessel or from the slag door is not possible. This is particularly advantageous in EAF facilities, which are covered by a removable cap and include electrodes introduced through the cap.

[0071] Preferably, the acceleration device is installed in a removable manner. In the case of a metallurgical vessel, when sidewalls are provided, the acceleration device can be anchored in the insulation layer of the sidewall.

[0072] The accelerating device can pass through the sidewall of the metallurgical vessel and be oriented downwards toward the high-temperature liquid. In a preferred embodiment, the angle between the accelerating device and the inner surface of the sidewall toward the high-temperature liquid is at least 25°, more preferably at least 30°, and even more preferably at least 35°. Preferably, this angle is in the range of 25° to 75°, and more preferably between 35° and 65°.

[0073] In a preferred embodiment, the metallurgical vessel is an EAF including a slag door, and the accelerating device is not installed in, at, or on the slag door.

[0074] The acceleration device typically includes a loading end with a loading opening and a front end with an outlet opening. The loading opening is adapted to insert a measuring probe carrying a sensor unit. It should be understood that the acceleration device is therefore configured to accommodate the measuring probe carrying the sensor unit. The outlet opening is adapted to allow the sensor unit to exit the acceleration device after acceleration. Preferably, the distance between the loading opening and the outlet opening is less than 2 m, more preferably less than 1.5 m, and even more preferably less than 1.3 m. The distance between the loading opening and the outlet opening can, for example, be in the range of 0.3 m to 1.5 m, preferably in the range of 0.5 m to 1.3 m.

[0075] The acceleration device is configured to accelerate the sensor unit along an acceleration path extending between the loading end and the outlet opening. In other words, the acceleration path is the path along which the sensor unit accelerates within the acceleration device during acceleration. The acceleration path typically does not begin at the loading end because the measuring probe carrying the sensor unit and the sensor unit itself may have a certain length, positioning the sensor unit at a distance from the loading end in the direction of the outlet opening before acceleration. In other words, the acceleration path begins at the location of the sensor unit when it is supplied to the acceleration device and after separation from the measuring probe. In a preferred embodiment, the acceleration path is a straight line. Preferably, the acceleration path is positioned parallel to the central longitudinal axis of the acceleration device along its length; more preferably, the acceleration path is coaxial with the central longitudinal axis. In other words, the sensor unit is preferably accelerated centrally within the acceleration device. Preferably, the length of the acceleration path is at least 0.2 m, more preferably at least 0.4 m. The length of the acceleration path can, for example, range from 0.2 m to 1.4 m, preferably from 0.4 m to 1.2 m.

[0076] Preferably, the acceleration device comprises a hollow, elongated member, such as a tube. Preferably, the acceleration device comprises a tube. In such cases, the acceleration path is preferably positioned parallel to the central longitudinal axis of the hollow, elongated member.

[0077] After acceleration, the sensor unit can be ejected from the hollow, slender member through the outlet opening.

[0078] The front end of the accelerator can be flush with the inside of the side wall of the container, or it can extend out of the side wall and thus be positioned within the volume of the container.

[0079] The front end may include a nozzle. In one embodiment, the end of the acceleration device, which is guided or can be guided toward a high-temperature liquid, is implemented as a Laval nozzle. This allows the purge gas flow to be introduced into the metallurgical vessel at high speed and / or supersonic velocity.

[0080] The acceleration device can be operated by any mechanism known to those skilled in the art, such as a pneumatic mechanism, a hydraulic mechanism, a mechanical mechanism (such as a push mechanism or spring, especially a preloaded spring), or an electromagnetic mechanism. In a preferred embodiment, the acceleration device includes a pneumatic device configured as an acceleration sensor unit, such device may include a compressed gas supply.

[0081] In the case of a pneumatic mechanism, a gas flow is used to accelerate the sensor unit. In the context of this invention, the term "gas" refers to any gaseous material, such as a gas, a gas mixture, and / or a dispersion having a gas as a continuous medium. Therefore, the gas flow can be a flow of a mixture of gases such as air. Specifically, the acceleration device can be operated by pressurized air or nitrogen. Typically, gas lines are heat-resistant, making them particularly suitable for use in high-temperature environments. Pneumatically driven acceleration devices are further advantageous because only minimal equipment needs to be installed near the operating point, and this installation requires only mechanical parts that can be robustly designed. Therefore, facilities with low maintenance requirements can be utilized. Furthermore, and particularly in metallurgical containers, such gas flows can additionally prevent the ingress of molten slag that could cause blockage of the acceleration device.

[0082] In embodiments with a pneumatic mechanism, the accelerating device preferably has an inlet or coupling for introducing a gas flow, preferably a pressurized gas flow, into the interior of the accelerating device. The gas flow is then discharged through an outlet opening during operation. The accelerating device is preferably connected to at least one gas line for connecting a high-pressure gas source to generate a gas flow in the accelerating device along the accelerating path. Preferably, the inlet or coupling for introducing the gas flow is laterally positioned on the accelerating device.

[0083] The acceleration device may include a second inlet or coupling for introducing a second gas flow. This second gas flow may be provided as a purge gas flow, which may be permanently applied during processing operations in the metallurgical vessel. The purge gas flow can be used to keep the hollow space within the acceleration device free of debris from the hot liquid and to ensure reliable operation.

[0084] In a preferred embodiment, the acceleration device is permanently purged with a purge gas flow, and an additional gas flow is applied during acceleration of the sensor unit. Therefore, the use of pressurized gas can be minimized.

[0085] Preferably, the accelerating device is made of a suitable heat-resistant material, such as ceramic, metal, or alloy. Preferably, the accelerating device is made of steel or stainless steel.

[0086] Acceleration devices may include means for releasing the sensor unit from the rest of the probe when the sensor unit is provided within such a probe, such as an ejector for releasing the sensor unit or a mechanical device configured to separate the sensor unit from the carrier element of the measuring probe.

[0087] During metallurgical processing, chemicals, typically in specific forms such as lime, calcium, carbon, oxygen, aluminum, and silicon, can be introduced into molten metal to alter its chemical composition. Devices for such insertions can be, for example, purging lances or injection systems used for the active treatment of hot liquids with additives in particulate or gaseous form. A purging lance is a nozzle capable of blowing a gas stream into the metallurgical vessel. The gas stream may include additional elements for processing the molten metal. Additionally, devices that introduce chemical energy in fluid (particularly gaseous) form to heat and / or process the molten metal are typically provided, such as burners or oxygen injectors. Such devices are usually permanently or removably installed at the metallurgical vessel and introduced through an opening, often positioned directly above the level of the molten metal. To ensure the opening toward the molten metal remains open, such facilities are purged with a permanent flow of gas, primarily compressed air or nitrogen.

[0088] In a preferred embodiment, the accelerating device is provided in or on an insertion device adapted to insert fluid and / or particles into a high-temperature liquid. In other words, the accelerating device can be provided as a device with dual functions. This helps prevent metal, slag, and / or debris from penetrating into the supply channels of the injection device and / or the accelerating device. Therefore, the installation of the accelerating system can be facilitated in a space-saving manner and further reduce installation costs.

[0089] In particular, the installation of pneumatically driven acceleration devices in or on insertion devices allows for advantageous installation, requiring only a minimal number of additional components and a small footprint within the limited space available in metallurgical facilities. No moving parts are needed near the container, thus reducing the risk of time-consuming accidents.

[0090] The method according to the invention includes providing a measuring probe carrying a sensor unit to an acceleration device. It should be understood that "providing a measuring probe to an acceleration device" includes loading the measuring probe onto or into the acceleration device. In other words, after this step, the acceleration device is loaded and / or brought into contact with the measuring probe.

[0091] A measuring probe should be understood as a device configured to provide a sensor unit and / or sensing element prior to its use. In other words, a measuring probe includes a sensor unit and at least one additional element. For example, such a probe may include protective elements for carrying and / or protecting the sensor unit during transport and storage, connecting elements for electrical and / or mechanical connections, and / or means for transmitting signals generated by the sensor unit as signal lines.

[0092] The sensor unit can be detached from the measuring probe. In other words, the sensor unit can be detached from at least one additional element of the measuring probe. For example, at least one additional element of the measuring probe may include a first coupling member configured to releasably engage a second coupling member disposed on or at the sensor unit. At least one additional element of the measuring probe may also include a trapping element that releases the sensor unit upon application of a force.

[0093] Preferably, the measuring probe includes a carrier element, preferably a carrier tube, such as a cardboard tube, which can at least partially house the sensor unit and optionally other elements of the measuring probe. Preferably, the measuring probe does not include elements extending laterally from the carrier element.

[0094] Preferably, the measuring probe includes at least one signal line configured to connect the sensor unit to the processing unit. The signal line may include one or more wires or cables. In such cases, the measuring probe advantageously includes a probe contact element configured to connect to at least one signal line.

[0095] At least one signal wire may be wound inside the measuring probe carrying the sensor unit, particularly inside the tube of the measuring probe. For example, one or more signal wires may extend through the interior of the carrier tube and be wound around its longitudinal axis inside the carrier tube.

[0096] Alternatively, the sensor unit may include means for wirelessly transmitting measurement data to a processing unit. In such cases, the sensor unit is adapted to transmit measurement data to a wireless data signal receiver via radio frequency signals or the like.

[0097] Before being provided to the acceleration device, the measurement probes can be stored individually; alternatively, they can be stored in a storage unit containing multiple measurement probes. Such storage units make it particularly possible to automatically trigger measurement cycles without any manual intervention in the system performing the method of the present invention. Thus, the storage unit further enhances the autonomy of such systems, as the system can simultaneously carry several probes and necessary further interactions are minimized.

[0098] The method according to the invention includes separating the sensor unit from the measuring probe. In other words, the sensor unit is released from another component of the measuring probe before acceleration.

[0099] This separation can be achieved, for example, by a release mechanism equipped with a measuring probe and / or a corresponding release device provided by an acceleration device. Separation can also be performed by an external separation device.

[0100] The method according to the invention includes accelerating a sensor unit using an acceleration device. During acceleration, the sensor unit is accelerated along the acceleration path of the acceleration device.

[0101] The sensor unit is accelerated. As known to those skilled in the art, acceleration is the rate of change of an object's velocity relative to time. Acceleration should be understood as the average acceleration along the acceleration path. Preferably, the acceleration is at least 15 m / s². 2 More preferably at least 20 m / s 2 Even more preferred is at least 25 m / s 2 In the preferred embodiment, the acceleration is 15 m / s². 2 Up to 80m / s 2 Within the range, preferably within 25 m / s 2 Up to 70m / s 2 Within this range. This type of acceleration allows even lightweight sensor units weighing less than 1500g or even less than 1000g to be sufficiently accelerated.

[0102] When the acceleration path has a length between 0.2m and 1.4m and the acceleration is 15m / s² 2 Up to 80m / s 2 This has proven advantageous when operating within a certain range. Such a configuration allows even lightweight sensor units to be accelerated sufficiently and efficiently.

[0103] The acceleration along the acceleration path may be constant or not. For example, the acceleration may include an upward phase with increasing acceleration and a constant phase with constant acceleration. The acceleration may include more than one acceleration; for example, the acceleration may include a first acceleration and a second acceleration, preferably the first acceleration is less than the second acceleration.

[0104] Preferably, the exit velocity of the sensor unit is at least 3 m / s, more preferably at least 5 m / s, and even more preferably greater than 8 m / s. In an advantageous embodiment, the exit velocity of the sensor unit is in the range of 3 m / s to 18 m / s, more preferably in the range of 5 m / s to 15 m / s. The exit velocity should be understood as the velocity possessed by the sensor unit when it is launched from the acceleration device. For lightweight sensor units, such as those weighing less than 1500 g or even less than 1000 g, a minimum exit velocity has proven particularly advantageous. A minimum exit velocity allows such sensor units to achieve a sufficiently high impact to enter the surface of a hot liquid.

[0105] In a preferred embodiment, the acceleration device includes an acceleration path shorter than 1.5 m, and the sensor unit is accelerated to a speed of at least 5 m / s. This configuration allows even lightweight sensor units to have a sufficiently high impact when reaching the surface of a hot liquid.

[0106] In a preferred embodiment, the sensor unit has a weight of less than 1000g, more preferably less than 500g, and is accelerated to a speed of at least 5m / s. This combination allows even these lightweight sensor units to have a sufficiently high impact when reaching the surface of a hot liquid.

[0107] After acceleration, the sensor unit will acquire a certain momentum. As known to those skilled in the art, momentum is the product of the mass and velocity of an object. Preferably, the sensor unit is accelerated to obtain a momentum of at least 1000 g*m / s, more preferably at least 1500 g*m / s, and even more preferably at least 2000 g*m / s. ​​In a preferred embodiment, the momentum is in the range of 1000 g*m / s to 10000 g*m / s, preferably in the range of 1500 g*m / s to 8000 g*m / s. ​​Minimal momentum allows even lightweight sensor units to achieve sufficiently high impacts to penetrate the surface of a hot liquid.

[0108] In a preferred embodiment, the sensor unit has a weight of less than 1000g and is accelerated to obtain a momentum of at least 1000g*m / s. ​​This combination allows even these lightweight sensor units to have sufficiently high impact when reaching the surface of a hot liquid.

[0109] The method according to the invention includes launching a sensor unit in the direction of a high-temperature liquid. "Launch sensor unit" means that the sensor unit is released from an acceleration device. Subsequently, the sensor unit moves toward the high-temperature liquid. During this movement, the sensor unit travels along a launch trajectory.

[0110] Preferably, the sensor unit emits at an angle of at least 25°, more preferably at least 30°, or even more preferably at least 35° relative to the surface normal of the high-temperature liquid. The surface normal of the high-temperature liquid should be understood as an axis perpendicular to the surface. It should be understood that the emission angle is primarily determined by the position and orientation of the accelerating device relative to the sidewall of the metallurgical vessel. In configurations of metallurgical vessels having sidewalls arranged perpendicular to the surface of the high-temperature liquid, the surface normal is aligned parallel to the sidewall. Preferably, the emission angle is in the range of 25° to 75°, more preferably in the range of 35° to 65°. Emission at an angle relative to the surface normal or sidewall allows the sensor unit to reach a certain distance from the sidewall before entering the high-temperature liquid, and in this way, more reliable and representative measurement results can be obtained over a generally more uniform area.

[0111] Preferably, the launch trajectory is a straight line; in other words, the launch trajectory is not curved. A straight launch trajectory allows for the shortest trajectory length and thus minimizes the travel time of the sensor unit. It is perhaps preferable that the launch trajectory has a curvature of less than 5°, more preferably less than 3°.

[0112] When the sensor unit is connected to the signal line, for example via a wire, cable, or wire, the signal line is pulled by the sensor unit and moves with it. If the signal line is wrapped around the measuring probe, it unwinds during this phase.

[0113] The method according to the invention involves immersing a sensor unit beneath the surface of a high-temperature liquid. In other words, the sensor unit enters the high-temperature liquid after a phase in which it moves toward the liquid at a speed provided by an acceleration device. In the case of molten metal having the slag layer of the invention, the sensor unit will move through the slag layer before entering the molten metal.

[0114] The distance D of the sensor unit from the inlet point in the container I The point of impact enters the surface of the high-temperature liquid. Preferably, the point of impact is located at a point smaller than the container diameter (D). V At half the distance of ), in other words, D I < 50% D V Even better, D I < 30% D V Impacts near the container sidewall are advantageous because the distance the sensor unit must travel inside the container is minimized.

[0115] Preferably, the sensor unit is immersed at an angle of less than 65° relative to the surface of the hot liquid, more preferably less than 60°, and even more preferably less than 55°. Dropping the sensor typically involves immersion at an angle of approximately 90° across the molten metal surface. A smaller immersion angle reduces the resistance of the hot liquid surface during the immersion phase, thus making the sensor unit less susceptible to impact damage. This is particularly advantageous in metallurgical applications where a slag layer needs to be passed before immersion under the molten metal surface; a lower immersion angle is beneficial for the operability of the sensor unit. The sensor unit can enter the hot liquid, for example, at an immersion angle between 15° and 65°, preferably between 25° and 55°, and more preferably between 30° and 50°. Immersion angles within the preferred range allow for a sufficient distance between the impact point and the sidewall while minimizing the impact point distance, which minimizes the required signal line length and achieves a sufficient descent depth for the sensor unit. Furthermore, when the immersion angle becomes too small, the distance the sensor unit needs to travel through the additional material layer increases, which may reduce its speed too much before impacting the surface of the high-temperature material.

[0116] The method according to the invention includes measuring at least one parameter of a high-temperature liquid. It should be understood that the measurement is performed while the sensor unit is immersed below the surface of the high-temperature liquid. The word "measurement" is used herein to describe the steps leading to the determination of at least one parameter of the high-temperature liquid. This step may include measuring a single data point or measuring more than one data point; that is, measuring a series of data points.

[0117] Measurements may include additional steps, such as transmitting data to a processing unit and / or processing the data.

[0118] After passing through the surface of the hot liquid, the sensor unit descends to a certain depth. During this descent phase, its speed gradually decreases as the sensor unit is slowed down by the surrounding hot liquid. During this phase, the sensor unit is heated by the hot liquid. Eventually, its speed in the forward direction will reach zero; in other words, the movement of the sensor unit will stop. When the weight and density of the sensor unit are thus selected, an ascent phase will follow, during which the sensor unit will again move in the upward direction. Preferably, measurements are taken during this ascent phase. Therefore, the recorded data will originate from a portion of the hot liquid that was not previously affected by the sensor unit, thus providing more accurate data.

[0119] After measuring the parameters of a high-temperature liquid, additional steps may follow, such as releasing or ejecting the measuring probe components retained in or at the acceleration device after the sensor unit has been accelerated, or cutting the retained cable.

[0120] This invention also relates to a system for carrying out the method of the invention. All embodiments described with respect to the method of the invention can also be applied to the system of the invention in any combination.

[0121] Preferably, the system includes an acceleration device.

[0122] In a preferred embodiment, the acceleration device is configured to accelerate a sensor unit weighing less than 1000g to obtain a momentum of at least 1000g*m / s.

[0123] In a preferred embodiment, the acceleration device is configured to accelerate a sensor unit weighing less than 1000g, more preferably less than 500g, to a speed of at least 5m / s on an acceleration path shorter than 1.5m.

[0124] Preferably, the system according to the invention includes a processing unit. The processing unit should be understood as a unit configured to acquire and process signals obtained by a suitable sensor unit to determine parameters of interest for the high-temperature liquid. In a preferred embodiment, the processing unit is configured to be disposed outside the metallurgical vessel containing the high-temperature liquid.

[0125] Preferably, the system includes means for transmitting signals obtained by suitable sensor units. These means may include, for example, extension wires configured to connect to the sensor units and the processing unit, and means for wireless transmission may also be suitable.

[0126] The system may also include a loading unit for loading the measuring probe into the acceleration device.

[0127] The system may also include a storage unit in which the measuring probe can be stored before use.

[0128] The present invention also relates to a metallurgical container comprising a system for carrying out the method of the present invention. All embodiments described with respect to the method or system of the present invention can also be applied to the metallurgical container of the present invention in any combination.

[0129] Preferably, the metallurgical container is an electric arc furnace.

[0130] The following schematic diagrams illustrate aspects of the invention to aid in understanding the invention in conjunction with some exemplary illustrations. However, it should be understood that the invention is not limited to the precise arrangements and tools shown. Elements in the drawings are not necessarily to scale relative to each other. Similar reference numerals denote corresponding similar parts. In this document…

[0131] Figure 1 A schematic cross-sectional view of an exemplary measuring probe is shown;

[0132] Figure 2 A schematic metallurgical vessel with an acceleration device mounted in the sidewall is shown;

[0133] Figure 3 Acceleration and velocity curves for an exemplary measurement sequence used in a high-temperature liquid without an additional layer of material are shown.

[0134] Figure 4 Acceleration and velocity curves for an exemplary measurement sequence covered with an additional material layer are shown;

[0135] Figure 5 A schematic cross-sectional view of a container containing a high-temperature liquid with an accelerator arranged on the side is shown.

[0136] Figure 1 A schematic cross-sectional view of an exemplary measuring probe 1 is shown. Probe 1 includes a carrier tube 2, which may be formed of cardboard. A sensor unit 3 is at least partially mounted at one end within the carrier tube 2 and held by a release mechanism 4. The sensor unit 3 includes a sensing element 5 and an immersion body 6. The sensing element 5 is selected according to the parameter to be measured; for example, it may include an oxygen detection element and / or a temperature measuring element (such as a thermocouple). The immersion body 6 is preferably a solid metal body with high density and high thermal conductivity, such as a solid steel body with holes for engaging the sensing element 5. To protect the sensing element 5 during handling of the measuring probe 1, a protective cap 7 formed of a material dissolved or melted in a corresponding high-temperature liquid encapsulates the sensing element.

[0137] Along the interior of the carrier tube 2, a signal line 8, connected at one end to the sensor unit 3, is wound in a coiled manner 9. This connection can be achieved via a contact (not shown) arranged in the immersion body 6. The other end of the signal line is connected to a connecting element 10 at the other end of the carrier tube. The connecting element 10 provides a suitable connection point to an extension cable or device to wirelessly transmit the signal acquired by the sensor unit to the analysis unit.

[0138] Figure 2 A schematic metallurgical vessel 20 (such as an electric arc furnace (EAF)) is shown, having an acceleration device (accelerator, 21) integrated into the sidewall. An EAF for steelmaking typically comprises a vessel 22 containing a pool of molten metal 23 and a removable cover 25 through which one or more electrodes 26 enter the furnace. A slag layer 24 covers the molten metal 23. Electrodes 26 for heating the metal are arranged above the vessel 22. Typically, the interior of the metallurgical vessel 20 is heated to approximately 600°C to 2000°C or even higher during processing.

[0139] The inlet point 27 of a facility typically used for processing molten metal pools (such as a carbon injector) is located in the side wall 28 of the container 22. This inlet point 27 can also accommodate an accelerator 21, preferably in combination with a device for processing the molten metal pool 23. The accelerator 21 can be, for example, an elongated tube, such as a pneumatically driven blower. Advantageously, such a pneumatic device can be permanently purged with an airflow that keeps the inlet point and the accelerator opening open. In a preferred embodiment, the accelerator includes a vacuum conveyor mounted on a steel tube (e.g., commercially available from, for example, Sommer Technik GmbH, Straubenhardt, Germany). In one exemplary embodiment, the inner tube of the accelerator has a length of 1.5 m. When a probe is provided, the sensor unit is positioned at a distance of 1.3 m from the opening of the accelerator oriented towards the molten metal pool 23. To accelerate the sensor unit, a gas flow of 3200 l / min is applied, resulting in an exit velocity of 10 m / s for a 200 g sensor unit.

[0140] Accelerator 21 traverses the side wall 28 of the container, with its tip arranged flush with the interior of the side wall 28. Accelerator 21 is arranged such that sensor units emitted from accelerator 21 after the acceleration phase enter the surface of the melt 29. Accelerator 21 may also be surrounded by a so-called cold box, a solid structure disposed inside the container to protect the packaged equipment. Typically, components inside the container that are not in contact with the molten metal pool are supplied with cooling mechanisms, such as water cooling.

[0141] exist Figure 2 In the configuration shown, accelerator 21 is equipped with a measurement probe 1, which carries a suitable sensor unit (not shown). Extension cable 30 connects the sensor unit to processing device 31, which can be placed at a distance from the container.

[0142] In a typical measurement sequence, the accelerator is loaded with a measurement probe in the first step. Inside the accelerator, the sensor unit is separated from the probe's carrier components. This separation can be achieved, for example, through suitable facilities within the accelerator, such as a shoulder or barrel cone, against which the probe's holding device is pushed to release the sensor unit. It should be emphasized that any connection between the sensor unit and signal lines or suitable connectors is not released and is configured to remain in place at least until the measurement sequence is complete.

[0143] Subsequently, the sensor unit is accelerated, for example, by compressed air, and ejected from the accelerator 21 into the interior of the container 22 with high initial velocity and momentum, and towards the molten metal pool 23. The sensor unit flies in a straight path toward the molten metal and enters the surface 29. The signal line connected to the sensor unit is pulled behind the sensor unit and out of the probe's carrier element, and is selected to survive long enough in the environment inside the container to ensure that measurements can be taken.

[0144] When the sensor unit is immersed below the surface of the molten metal pool, desired parameters can be measured, and the corresponding signals are transmitted to appropriate analytical equipment. After the required data is recorded, the accelerator can be removed from the probe's components that have not yet been ejected into the molten metal, for example, by spraying them into the molten metal pool.

[0145] Figure 3 Acceleration (A) and velocity curves (B) of an exemplary measurement sequence for measurements in a hot liquid without an additional layer of material are shown. The curves begin after the sensor unit has been separated from the immersion probe and cover the phases during which the sensor unit accelerates and / or moves. In the first phase (I), the sensor unit is actively accelerated by the accelerator at an acceleration significantly higher than that of gravity. It should be understood that the constant acceleration shown refers to the average acceleration during this phase, which may include several acceleration phases or phases with increasing or decreasing acceleration. Therefore, the constant increasing velocity of phase I shown should also be understood as an average value and may include more than one phase. It has been shown that sensor units smaller than 1000g require a high exit velocity of at least 5 m / s to allow sufficient impact through the surface of the hot liquid. The sensor unit is then ejected from the accelerator at this exit velocity. In the subsequent “free flight” phase (II), gravity further accelerates the sensor unit and the travel velocity increases. After impacting through the surface of the hot liquid, the sensor unit decelerates due to the opposing force of the liquid. In this “descent phase” (III), the velocity decreases until it reaches zero. At this point in time, the sensor unit has reached its final measurement position, and its depth below the surface is sufficient to obtain reliable results in a uniform region of the high-temperature liquid.

[0146] Figure 4 Acceleration (A) and velocity curves (B) of an exemplary measurement sequence covered with an additional material layer (such as a slag layer) are shown. Before impacting in the high-temperature liquid, the sensor unit passes through an additional layer that has a deceleration and velocity reduction effect (stage III-a).

[0147] Because the sensor unit is provided with high momentum by active acceleration, it descends deep into the molten metal despite its low mass, short distance between the entry point and the surface, and the slag layer which slows the unit down before it is finally immersed in the molten metal. Furthermore, the measurement is minimally affected by the cold mass introduced by the lightweight sensor unit, allowing for reliable and accurate results.

[0148] Figure 5 A schematic cross-sectional view of a metallurgical vessel 22 is shown, which includes a molten metal pool 23 with an accelerator 21 arranged on its side, wherein relevant geometric parameters are indicated. The accelerator 21 is positioned at a horizontal distance L from the surface of the molten metal. M Distance D A At this location, the distance D between the surface of the molten metal and the opening of container 33 is... M The container has a diameter D. V After the free-flight phase, the sensor unit enters the molten metal at impact point 34 on its surface, which is a distance D from the inlet point 27 in the sidewall 28. I The incident angle, denoted by α, is the angle between the normal to the surface of the high-temperature liquid and the trajectory of the sensor unit ejected from the accelerator. The incident angle is also the emission angle, which is the angle between the emission trajectory of the sensor unit and the surface normal of the high-temperature liquid (indicated by the dashed line). The immersion angle β is the angle between the surface of the high-temperature liquid and the trajectory of the sensor unit.

[0149] Figure Labels

[0150] 1 Measurement probe

[0151] 2 carrier tubes

[0152] 3 sensor units

[0153] 4 release mechanism

[0154] 5 sensing elements

[0155] 6 Immersed Main Body

[0156] 7 Protective Caps

[0157] 8 signal lines

[0158] 9-signal line winding

[0159] 10 connecting elements

[0160] 20 Metallurgical Containers

[0161] 21 Accelerator

[0162] 22 containers

[0163] 23 Molten Metal Pool

[0164] 24 slag layer

[0165] 25 removable caps

[0166] 26 electrodes

[0167] 27 entry points

[0168] 28. Side walls of the container

[0169] 29 Surface of molten metal pool

[0170] 30 extension cable

[0171] 31 processing equipment

[0172] 32 high temperature liquid

[0173] 33. Container opening

[0174] 34 impact points

[0175] L M Horizontal position of the surface of a high-temperature liquid

[0176] D A Distance between the accelerator and the surface of the high-temperature liquid

[0177] D M Distance between container opening and the surface of high-temperature liquid

[0178] D V Container diameter

[0179] D I Distance from impact point to entry point

[0180] α Incident angle / Emission angle

[0181] β immersion angle

Claims

1. A method for determining at least one parameter of a high-temperature liquid using a sensor unit, The high-temperature liquid includes a surface and is provided in a metallurgical vessel, the metallurgical vessel including a top opening opposite the surface of the high-temperature liquid, and The surface of the high-temperature liquid level has a position L. M The location is at a distance D from the top opening of the metallurgical vessel. M place, The method includes: (a) The distance D between the surface of the high-temperature liquid and the top opening of the metallurgical vessel A An acceleration device is provided above the surface of the high-temperature liquid, wherein the acceleration device is adapted to increase the speed of the sensor unit; (b) Providing a measurement probe to the acceleration device, wherein the measurement probe carries the sensor unit, and wherein the sensor unit is detachable from the measurement probe; (c) Separate the sensor unit from the measuring probe; (d) Accelerate the sensor unit using the acceleration device; (e) The sensor unit is emitted in the direction of the high-temperature liquid; (f) Immerse the sensor unit under the surface of the high-temperature liquid; (g) Measure at least one parameter of the high-temperature liquid; Its characteristic is that D A < 50% D M .

2. The method of claim 1, wherein the accelerating device is provided in and / or attached to the sidewall of the metallurgical vessel.

3. The method according to claim 1 or 2, wherein the accelerating device extends through an opening in the side wall of the metallurgical vessel into or adjacent to the volume of the metallurgical vessel containing the high-temperature liquid.

4. The method according to any one of the preceding claims, wherein the accelerating device is oriented downward toward the high-temperature liquid through the sidewall of the metallurgical vessel.

5. The method according to any one of the preceding claims, wherein the sensor unit is immersed in the surface of the high-temperature liquid at an immersion angle of less than 65°.

6. The method according to any one of the preceding claims, wherein the sensor unit emits at an angle greater than 25° relative to the sidewall of the container.

7. The method according to any one of the preceding claims, wherein the sensor unit is accelerated to obtain a momentum of at least 1000 g*m / s.

8. The method according to any one of the preceding claims, wherein the sensor unit has a weight of less than 1500g.

9. The method according to any one of the preceding claims, wherein the sensor unit is accelerated to a speed of at least 5 m / s.

10. The method according to any one of the preceding claims, wherein the acceleration is at 15 m / s². 2 Up to 80m / s 2 Within the range.

11. The method according to any one of the preceding claims, wherein the launch trajectory of the sensor unit is linear after launch and before immersion.

12. A system for implementing the method according to claims 1 to 11.

13. A metallurgical container, the metallurgical container comprising a system for implementing the method according to claims 1 to 11 or an apparatus according to claim 12.

Citation Information

Patent Citations

  • Oxygen level sensor for molten metal

    EP0059222A1

  • Drop-in immersion probe

    EP0758445A1

  • Immersion sensor for molten metals

    US5332449A

  • Metallurgical furnace probe with ejecting cartridge sensor

    WO2015070316A1