Application of an iron-nitrogen co-pyrolysis biochar composite chitosan granular material for adsorbing phosphates in water
By preparing iron-nitrogen co-pyrolysis biochar composite chitosan granular material, the problems of low efficiency and poor selectivity of existing adsorbents in treating phosphates in wastewater are solved, achieving efficient removal of phosphates and making it suitable for practical wastewater treatment over a wide pH range.
Patent Information
- Application Number
- CN202510629207.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-16
- Publication Date
- 2026-11-17
AI Technical Summary
Existing adsorbents are inefficient, have poor selectivity, and are costly when treating phosphates in wastewater, making them difficult to effectively treat livestock wastewater with high concentrations and complex compositions.
By preparing iron-nitrogen co-pyrolysis biochar composite chitosan particles, the iron-based active sites form insoluble iron phosphate precipitates with phosphates, and the amino groups in chitosan molecules enhance the selective adsorption capacity for phosphates, thus achieving efficient adsorption of the composite material.
It significantly improves the removal efficiency of low-concentration phosphate in actual wastewater, has a wide applicable pH range, and is suitable for simulating actual livestock wastewater, with a removal rate of 71.8%.
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] This invention relates to the field of environmental functional materials technology, specifically to the removal of phosphates from wastewater using composite adsorbents. This invention also relates to the reuse of waste biomass and the application of adsorbents in simulated real wastewater, specifically to the resource utilization of agricultural waste corn stalks and the application of materials in adsorbing phosphates from livestock wastewater. Background Technology
[0002] As a major livestock producer, China generates 3-4 billion tons of livestock wastewater annually, with a considerable amount of phosphate. This wastewater is diverse, containing ammonia nitrogen, high concentrations of organic matter, and phosphate, with slaughterhouse and pig farm wastewater exhibiting particularly high phosphorus content. With economic development and increasing demand for livestock products, small-scale, individual farming has expanded to large-scale, systematic operations, leading to a year-on-year increase in livestock wastewater discharge, making it a major source of pollution. Phosphate is a primary cause of eutrophication, and the discharge of large amounts of phosphorus-containing wastewater can cause soil compaction, affecting crop growth. Phosphate can also seep into groundwater through the soil, polluting water bodies and endangering human health. Furthermore, eutrophication causes economic losses to fisheries and agriculture, significantly increasing the cost of water treatment. Therefore, phosphorus control is urgent, and more efficient and economical methods for phosphorus removal must be explored.
[0003] Biochar is an economical, environmentally friendly, and widely available adsorbent material. The raw materials for biochar are diverse, including crop straw, crab shells, livestock manure, and plant peels. The adsorption capacity of biochar can generally be enhanced through carbonization and pyrolysis, as well as by selecting appropriate raw materials. Chemical modification, impregnation, and pyrolysis are common methods for modifying biochar, which can endow it with richer functional groups and pores, increasing its specific surface area and making it more conducive to adsorbing pollutants. Modification can be tailored to the characteristics of the pollutants; phosphates can form surface complexes with many metal cations, forming insoluble precipitates that are then removed. They can also be adsorbed by hydroxyl and amino groups through electrostatic attraction and other mechanisms. However, many adsorbents suffer from narrow pH ranges, poor resistance to interference, and poor selectivity for phosphates.
[0004] Although research on phosphate adsorption materials is extensive both domestically and internationally, existing materials still suffer from limitations in practical wastewater treatment applications, such as low adsorption efficiency, poor selectivity, or high cost. Therefore, this study proposes a novel method for preparing a composite adsorption material: firstly, phosphorus-affinity metal iron is uniformly loaded onto the surface of biochar via urea-assisted pyrolysis to form an iron-nitrogen co-doped biochar substrate; subsequently, the substrate is modified into a composite particulate material using the cross-linking effect of chitosan. This material forms a poorly soluble iron phosphate precipitate with phosphate through iron-based active sites, while simultaneously enhancing the selective adsorption capacity of phosphate through the abundant amino groups in chitosan molecules, thereby significantly improving the removal efficiency of low-concentration phosphate in practical wastewater. This synergistic mechanism effectively solves key problems such as low phosphorus removal efficiency and poor selectivity in practical wastewater treatment, and has significant application value. Summary of the Invention
[0005] The purpose of this invention is to provide a method for adsorbing phosphates in water using iron-nitrogen co-pyrolysis biochar composite chitosan granular material, so as to solve the problem of poor phosphate removal performance in wastewater.
[0006] The technical solution of the present invention is as follows: This invention provides a method for preparing iron-nitrogen co-pyrolysis biochar composite chitosan particulate material, comprising the following steps: (1) Preparation of modified biochar: Iron chloride and urea are mixed and dissolved in 50 ml of deionized water at a certain molar ratio. Straw powder is added to the above mixed solution, stirred and impregnated, precipitated, dried and then calcined in a muffle furnace to obtain iron-nitrogen co-pyrolysis biochar material.
[0007] (2) Preparation of chitosan gel: Add chitosan to 50 ml of acetic acid solution and stir at a certain temperature to form a gel.
[0008] (3) Preparation of composite particle material: The modified biochar prepared in step (1) is added to the gel in step (2), and after being stirred thoroughly, it is dropped into the precipitation tank by a dropper to precipitate into spheres. The obtained microspheres are repeatedly washed in the crosslinking agent for crosslinking. After the fully crosslinked microspheres are repeatedly washed to neutral pH, they are dried in an oven to obtain iron-nitrogen co-pyrolysis biochar composite chitosan particle material.
[0009] In one specific embodiment, in step (1), the molar ratio of ferric chloride to urea is (1:0.5), the amount of straw powder added is 5g, the rotation speed is controlled at 250rpm / min, the stirring time is 6h, the sedimentation time is 18h, the drying temperature is 60℃, the calcination temperature is 600°C, the heating rate is controlled at 5℃ / min, the holding time is 15min, and the calcination time is 1h.
[0010] In one specific embodiment, in step (2), the chitosan is 1g, the acetic acid solution concentration is 2%, the rotation speed is controlled at 250rpm / min, and the temperature is 40℃.
[0011] In one specific embodiment, in step (3), the modified biochar is 2g, the precipitation tank is 1mol NaOH solution, the precipitation is 1h, the crosslinking agent is 2% glutaraldehyde, the crosslinking is 6h, and the drying temperature is 60℃.
[0012] In this invention, iron and nitrogen co-pyrolysis biochar composite chitosan particles are added at a concentration of 0.6 g / L to a phosphate standard solution (pH=6-10; PO4). 3- =50mg / L) and simulated livestock wastewater (PO4) 3- =100mg / l; NH4 + =100mg / l; COD=3500mg / l; CO3 2- In a system with a concentration of 31.21 mg / L and a pH of 6.47, the removal efficiency and application potential of this adsorbent material for phosphate in wastewater were systematically investigated. By comparing the adsorption performance of the material in single phosphate solutions and simulated wastewater with complex compositions, its feasibility for application in actual livestock wastewater treatment was comprehensively evaluated.
[0013] Technical effects and advantages of the present invention: The present invention prepares an iron-nitrogen co-pyrolysis biochar composite chitosan particle material by means of impregnation pyrolysis and chemical cross-linking. The material has strong adsorption performance for phosphate and has a wide applicability in a pH range (6-10). It has shown good application performance in simulated actual livestock wastewater. Attached Figure Description
[0014] Figure 1 Flowchart of the preparation process of this invention Figure 2 Effect of adsorption time on phosphate adsorption of composite materials Figure 3 Experiment on the effect of solution pH Figure 4 Simulated livestock wastewater treatment results diagram Detailed Implementation Example
[0015] This invention provides, for example Figure 1 The preparation method and physical image of the iron-nitrogen co-pyrolysis biochar composite chitosan particle material shown include the following steps: S1: Modified biochar was obtained by impregnating and pyrolyzing ferric chloride, urea and corn stalks with ferric chloride as the iron source and urea as the nitrogen source. The molar ratio of ferric chloride to urea was (1:0.5), the volume was 50 ml, the corn stalk powder was 5 g, the speed was controlled at 250 rpm / min, the stirring time was 6 h, the sedimentation time was 18 h, the drying temperature was 60 ℃, the calcination temperature was 600 ℃, and the calcination time was 1 h.
[0016] S2: Add 1g of chitosan to 50ml of 2% acetic acid solution, control the rotation speed at 250rpm / min, and prepare a gel at 40℃. Add the above material to the gel and stir evenly. Drop the mixture into a 1mol NaOH precipitator and precipitate for 1h. Use 2% glutaraldehyde as the crosslinking agent and crosslink for 6h. Dry at 60℃.
[0017] The iron-nitrogen co-pyrolysis biochar composite chitosan granular material prepared by the above process achieved a phosphate removal rate of 71.8% when the adsorption time was 90 min, the adsorbent dosage was 0.6 g / L, and the simulated phosphate concentration in livestock wastewater was 100 mg / L. Example
[0018] like Figure 2-4 This invention demonstrates the application of an iron-nitrogen co-pyrolysis biochar composite chitosan granular material in the selective removal of phosphates from phosphate-containing wastewater. like Figure 2 The adsorption capacity can reach 89.99% at adsorption equilibrium, and adsorption equilibrium is reached at 60 min.
[0019] like Figure 3 The iron-nitrogen co-pyrolysis biochar composite chitosan particle material still exhibits good adsorption performance within the initial pH range (6-10).
[0020] like Figure 4 To simulate livestock wastewater (PO4) 3- =100mg / l; NH4 + =100mg / l; COD=3500mg / l; CO3 2- The sample (31.21 mg / L; pH 6.47) reached adsorption equilibrium in 90 min, with a removal rate of 71.8%.
Claims
1. An application of an iron-nitrogen co-pyrolysis biochar composite chitosan particle material for adsorbing phosphate in water, the specific steps of which are: adding 0.6 g / L iron-nitrogen co-pyrolysis biochar composite chitosan particles to a 50 mg / L phosphate system, and removing phosphate under shaking conditions.
2. The application of the iron-nitrogen co-pyrolysis biochar composite chitosan particle material as described in claim 1 for adsorbing phosphate in water, characterized in that, Under the condition of shaking reaction for 60 min to 70 min, the removal rate reached 89.99% to 90.04%.
3. The application of the iron-nitrogen co-pyrolysis biochar composite chitosan particle material as described in claim 1 for adsorbing phosphate in water, characterized in that, Phosphate removal rates ranged from 82.6% to 91.1% across a wide pH range of water samples (6–10).
4. The application according to claim 1, characterized in that, The material is suitable for the removal of phosphates from livestock wastewater.