3D printing equipment and 3D printing methods

By combining a molding module and jetting modules of different viscosities, the problem of binder jetting 3D printing being incompatible with materials with a wide viscosity range has been solved, and stable multi-material printing results have been achieved.

CN123104061APending Publication Date: 2026-11-17SHENZHEN SOONGON TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611475166.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing binder jetting 3D printing methods are difficult to be compatible with liquid materials with a wide viscosity range, and suffer from problems such as unstable jetting, nozzle clogging, ink interruption, and jetting deviation.

Method used

This 3D printing equipment combines a molding module, a regular viscosity jetting module, a high viscosity jetting module, and an ultra-high viscosity jetting module to process media of different viscosities. Through the coordinated operation of the control module, it can achieve zoned jetting of binders of various viscosities.

Benefits of technology

It achieves compatibility with materials across a wide viscosity range, avoids jet instability and nozzle clogging issues, and improves the forming stability and accuracy of multi-material printing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123104061A_ABST
    Figure CN123104061A_ABST
Patent Text Reader

Abstract

This invention discloses a 3D printing device and a 3D printing method, relating to the field of 3D printing technology. The 3D printing device includes a frame, a forming module, a normal viscosity jetting module, a high viscosity jetting module, an ultra-high viscosity jetting module, and a control module. The above-mentioned configuration allows the normal viscosity jetting module and the high viscosity jetting module to respectively jet low-viscosity liquid materials and high-viscosity liquid materials. The ultra-high viscosity jetting module supplements the jetting of high-viscosity materials and the extrusion of high-viscosity plastic substrates. The multi-module split-flow operation architecture enables wide viscosity range material compatibility and overcomes the shortcomings of ordinary inkjet heads being unable to jet high-viscosity materials and the difficulty of single hardware simultaneously achieving binder jetting and high-viscosity plastic substrate extrusion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of 3D printing technology, and in particular to a 3D printing device and a 3D printing method. Background Technology

[0002] Binder jetting 3D printing is a typical powder bed additive manufacturing process. Its basic process is as follows: first, a layer of powder material is laid on the forming platform, and then a binder is jetted into a predetermined area of ​​the powder layer through the inkjet head to make the powder particles in the target area bond together. Then, the powder laying and jetting process is repeated to finally form a three-dimensional part.

[0003] In related technologies, traditional inkjet structures are only suitable for low-viscosity liquids and cannot stably output high-viscosity slurries, gels, viscous functional resins and other materials; and are prone to problems such as unstable jetting, nozzle clogging, ink interruption, satellite droplets, and off-center spraying. Summary of the Invention

[0004] The main objective of this invention is to propose a 3D printing device and a 3D printing method, which aims to solve the problem that traditional binder jet 3D printing is difficult to be compatible with liquid materials with a wide viscosity range in related technologies.

[0005] To achieve the above objectives, the present invention provides a 3D printing device comprising: frame; A forming module, comprising a printing platform and a powder spreading component, wherein the powder spreading component is disposed on the frame and located above the printing platform; A standard viscosity jetting module is elliptically mounted on one side of the frame and located on one side of the printing platform; the standard viscosity jetting module includes at least one inkjet head, each inkjet head having at least two jetting channels formed therein, each jetting channel being configured to connect to a feeding system respectively; A high-viscosity spraying module is movably mounted on the frame, the high-viscosity spraying module including a first high-viscosity spraying element configured to communicate with the feeding system; An ultra-high viscosity spraying module is movably mounted on the frame, and the ultra-high viscosity spraying module includes a second high viscosity spraying element configured to connect to a feeding system; The control module is communicatively connected to the molding module, the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module.

[0006] In one embodiment, each of the inkjet heads is one of a piezoelectric inkjet head, a thermal inkjet head, or a continuous inkjet head.

[0007] In one embodiment, the first high-viscosity spraying element is either a piezoelectric spray valve or a needle-type spray valve; And / or, the second high-viscosity spraying component is one of a pneumatic dispensing valve, a screw valve, a plunger valve, a micro-dispensing valve, or a DIW direct-write extruder.

[0008] In one embodiment, the powder spreading assembly includes a powder spreading section, a powder supply cylinder, a forming cylinder, and a recovery cylinder. The powder spreading section is slidably disposed on the frame, and the powder supply cylinder and the forming cylinder are arranged side by side in the printing platform. The recovery cylinder is disposed on the side of the printing platform away from the powder supply cylinder.

[0009] The present invention also proposes a 3D printing method for use in the 3D printing equipment described above, the method comprising the following steps: Construct a 3D model to obtain contour data, material partition data, and injection path data; Based on the contour data, the material partition data, and the jetting path data, the powder spreading component is controlled to spread a powder layer on the printing platform to obtain an initial powder bed. Based on the form of the molding material and the viscosity of the binder, select the corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module, and spray the binder onto the initial powder bed through the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module. The printing platform is controlled to descend to a preset layer thickness, and the steps of controlling the powder spreading component to spread a powder layer on the printing platform according to the contour data, the material partition data, and the jetting path data to obtain an initial powder bed are repeated until printing is completed.

[0010] In one embodiment, the step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module based on the morphology of the molding material and the viscosity type of the binder, and spraying the binder onto the initial powder bed using the ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module includes: Confirm the shape type of the molding material and the viscosity type of all the adhesives to be sprayed, determine whether the set of adhesives to be sprayed contains one or more different viscosity types, and obtain the determination result; When the determination result is yes, for each type of adhesive viscosity, a corresponding spraying module is matched, and at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module are used in combination to spray the adhesive of the corresponding viscosity type into the initial powder bed in sections; If the determination result is negative, select one of the following modules—ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module—based on the viscosity type of the adhesive to spray the adhesive onto the initial powder bed.

[0011] In one embodiment, when the determination result is yes, the step of matching a corresponding spraying module for each viscosity type of binder, and using at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module in combination to spray the binder of the corresponding viscosity type into the initial powder bed in sections includes: The adhesive is divided into a first adhesive, a second adhesive, and an Nth adhesive (N is greater than or equal to 2) according to its viscosity coefficient. One or more combinations of the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module are selected according to the viscosity range of each adhesive. Different spraying modules are selected according to the shape type of the molding material to spray the initial powder bed with the adhesive of the corresponding viscosity type.

[0012] In one embodiment, the step of selecting one of a normal viscosity spraying module, a high viscosity spraying module, or an ultra-high viscosity spraying module to spray the binder onto the initial powder bed when the determination result is negative includes: The adhesive to be sprayed is taken as a single adhesive, and one of the following modules is selected according to the viscosity range of the single adhesive: ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module; and according to the morphology of the molding material, the selected spraying module is controlled to spray the adhesive of the single viscosity type onto the initial powder bed.

[0013] In one embodiment, the step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module based on the morphology of the molding material and the viscosity type of the binder, and then spraying the binder onto the initial powder bed using the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module, includes the following: The initial powder bed after spraying is then stabilized.

[0014] In one embodiment, the step of controlling the printing platform to descend a preset layer thickness and repeatedly controlling the powder spreading component to spread a powder layer on the printing platform according to the contour data, the material partitioning data, and the jetting path data to obtain an initial powder bed, until the printing is completed, includes: The printed parts are retrieved and then processed.

[0015] The 3D printing equipment provided by this invention, by employing a molding module, ordinary viscosity jetting modules, high viscosity jetting modules, ultra-high viscosity jetting modules corresponding to different viscosity media, and a control module working together, can solve the problems of existing binder jetting 3D printing being unable to be compatible with printing binders with a wide viscosity range and multiple molding materials, single nozzles being unable to adapt to media with a full viscosity range, multiple flow channels being prone to mutual interference, and poor coordination of multi-material printing control. Specifically, the molding module is equipped with a printing platform and a powder spreading component. The powder spreading component completes the powder spreading to build an initial powder bed on the printing platform. The ordinary viscosity jetting module can be raised and lowered and arranged on one side of the frame. Its inkjet head is equipped with at least two independent jetting channels that are connected to the feeding system respectively, and is specifically responsible for the jetting of ordinary viscosity media. The high viscosity jetting module and the ultra-high viscosity jetting module can be moved and arranged on the frame. They are connected to the feeding system by the first high viscosity jetting component and the second high viscosity jetting component respectively, and are respectively responsible for processing high viscosity media and ultra-high viscosity media. The control module is communicatively connected to the molding module and the above three jetting modules. It can schedule a single jetting module to work independently, or it can combine two or even three jetting modules to work together. The combination of jetting modules participating in the work can be selected according to the form of the molding material and the viscosity type of the binder to achieve single or multiple different viscosity binders for zoned jetting, which can adapt to different molding material combination conditions. Each jetting module has a degree of freedom of raising or lowering or moving, which can match the requirements of printing layer height changes and planar zoned jetting. Compared to existing technologies that rely on a single jetting device to handle various viscosity media, this invention distributes media of different viscosities to three independent jetting modules for processing. This avoids nozzle clogging and jetting instability issues caused by a single printhead adapting to a wide viscosity range. The above setup uses a standard viscosity jetting module and a high viscosity jetting module to jet low-viscosity and high-viscosity liquid materials respectively, while an ultra-high viscosity jetting module supplements the jetting of high-viscosity materials and the extrusion of high-viscosity plastic substrates. This multi-module flow-dividing architecture achieves wide viscosity range material compatibility, overcoming the limitations of ordinary inkjet heads in jetting high-viscosity materials and the difficulty of a single hardware device simultaneously performing binder jetting and high-viscosity plastic substrate extrusion. The three jetting modules of different viscosities can be flexibly combined and work collaboratively to achieve the combined jetting of standard, high, and ultra-high viscosity media, significantly expanding the viscosity range of binders and molding materials that the equipment can adapt to, and improving the molding stability and molding accuracy of powder bed printing under multi-material, wide viscosity range conditions. Attached Figure Description

[0016] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.

[0017] Figure 1 This is a schematic diagram of the structure of the 3D printing equipment provided by the present invention; Figure 2 A flowchart illustrating the steps of the 3D printing method provided by this invention; Figure 3 This is a flowchart of some steps of the 3D printing method provided by the present invention.

[0018] Explanation of icon numbers: 100. 3D printing equipment; 1. Frame; 2. Molding module; 21. Printing platform; 22. Powder spreading assembly; 221. Powder spreading section; 222. Powder supply cylinder; 223. Molding cylinder; 224. Recovery cylinder; 3. Ordinary viscosity jetting module; 31. Inkjet head; 4. High viscosity jetting module; 41. First high viscosity jetting component.

[0019] The realization of the objective, functional features and advantages of the present invention will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation

[0020] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0021] It should be noted that if the embodiments of the present invention involve directional indicators (such as up, down, left, right, front, back, etc.), the directional indicators are only used to explain the relative positional relationship and movement of the components in a specific posture. If the specific posture changes, the directional indicators will also change accordingly.

[0022] Furthermore, if the embodiments of this invention involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the use of "and / or" or "and / or" throughout the text includes three parallel solutions. For example, "A and / or B" includes solution A, solution B, or a solution where both A and B are satisfied simultaneously. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.

[0023] This invention proposes a 3D printing device 100.

[0024] Please see Figure 1 In one embodiment of the present invention, the 3D printing equipment 100 includes a frame 1, a forming module 2, a normal viscosity jetting module 3, a high viscosity jetting module 4, an ultra-high viscosity jetting module, and a control module. The forming module 2 includes a printing platform 21 and a powder spreading assembly 22, the powder spreading assembly 22 being disposed on the frame 1 and located above the printing platform 21. The normal viscosity jetting module 3 is vertically and vertically disposed on one side of the frame 1 and located on one side of the printing platform 21. The normal viscosity jetting module 3 includes at least one inkjet head 31, and each inkjet head 31 has at least two... Each spray channel is configured to be connected to the feeding system; a high-viscosity spray module 4 is movably mounted on the frame 1, and the high-viscosity spray module 4 includes a first high-viscosity spray element 41, which is configured to be connected to the feeding system; an ultra-high viscosity spray module is movably mounted on the frame, and the ultra-high viscosity spray module includes a second high-viscosity spray element, which is configured to be connected to the feeding system; the control module is communicatively connected to the molding module 2, the ordinary viscosity spray module 3, the high-viscosity spray module 4, and the ultra-high viscosity spray module.

[0025] In this embodiment, the 3D printing equipment 100 can be applied to powder bed material systems such as metal powder, ceramic powder, sand mold materials, pharmaceutical powder, biomaterial powder, polymer powder, and composite powder. It is also suitable for applications requiring the local introduction of high-viscosity resin, silicone, ceramic slurry, metal slurry, conductive slurry, thermally conductive slurry, magnetic slurry, biogel, two-component reaction liquid, or functional liquid materials into the powder bed; no limitation is made here. The frame 1 provides the mounting base for the entire equipment. The frame 1 can be in the form of aluminum profiles and a plate box, or it can be an integrated sheet metal welded box, etc.; no limitation is made here. The molding module 2 includes a printing platform 21 and a powder spreading component 22. The printing platform 21 is the supporting base for the entire equipment and is vertically mounted on the frame 1. It is understood that the printing platform 21 can be mounted on the frame 1 by means of lead screw lifting, synchronous belt lifting, etc. The printing platform 21 has a cylinder; this can be set according to existing technology and is not limited. The powder spreading assembly 22 is used to evenly spread powder on the printing platform 21, forming a powder layer of uniform thickness and a smooth surface. The thickness of the powder layer can be from 20μm to 500μm, preferably from 50μm to 200μm. The powder spreading assembly 22 can accommodate powder types such as metal powder, ceramic powder, polymer powder, pharmaceutical powder, sand-like materials, biomaterial powder, composite powder, or powder containing functional components. The powder spreading assembly 22 can be a scraper-type powder spreading assembly, a roller-type powder spreading assembly, etc., which can be set according to specific requirements. The powder spreading assembly 22 is connected to the frame 1 through linear guide rails or bolts, so that the powder spreading assembly 22 can move laterally back and forth along the printing platform 21. The ordinary viscosity jetting module 3 is used to transport and jet low-viscosity printing materials. The low-viscosity printing materials can be binders, functional solutions and low-viscosity slurries, color liquids, catalysts, penetration conditioners, etc., which are not limited here. The inkjet head 31 receives the fluid from the feeding system and is conveyed through the jet flow channel, enabling precise, targeted material ejection according to instructions from the control module. The jet flow channel guides the low-viscosity printing material from the feeding system to the ejection outlet of the inkjet head 31. It is understood that the inkjet head 31 can be a piezoelectric inkjet head 31, a thermal inkjet head 31, or other ejection devices. Each inkjet head 31 has two physically isolated independent jet channels, each connected to the feeding system. It should be noted that the number of inkjet heads 31 can be two, three, or more, and each inkjet head 31 can have one, two, or more jet channels, depending on specific requirements. The ordinary viscosity jet module 3 and the frame 1 can be connected via a vertical screw slide or a synchronous belt lifting module; this is not limited here.The high-viscosity jetting module 4 is used to transport and jet high-viscosity printing material. The high-viscosity jetting module 4 includes a first high-viscosity jetting element 41, which can be a piezoelectric jet valve, a striker-type jet valve, etc. The high-viscosity jetting module 4 can use a single type of first high-viscosity jetting element 41, or it can be used in combination with multiple different types of first high-viscosity jetting elements 41; this is not limited here. The high-viscosity printing material is a high-viscosity liquid material, which can be epoxy resin, silicone rubber, photocurable resin, high-solids ceramic slurry, metal slurry, conductive silver paste, thermally conductive slurry, magnetic slurry, biogel, hydrogel, pharmaceutical slurry, viscous binder, or other functional liquid materials. The high-viscosity jetting module 4 can be connected to the frame 1 via a gantry linear module or a cross slide, etc.; this is not limited here. It is understood that the ordinary viscosity jetting module 3 can jet low-viscosity liquids from 1 cp to 30 cp, while the high-viscosity jetting module 4 can jet liquid materials greater than 30 cp; this is not limited here. The ultra-high viscosity spraying module can supply molding materials and also spray ultra-high viscosity liquid materials. The type of ultra-high viscosity spraying module can be a pneumatic dispensing valve, screw valve, plunger valve, micro-dispensing valve, etc., capable of spraying low-precision, ultra-high viscosity materials. The connection relationship between the ultra-high viscosity spraying module and frame 1 can be referenced to the connection relationship between the high viscosity spraying module 4 and frame 1, and is not limited here. The control module is used to establish communication connections with molding module 2, ordinary viscosity spraying module 3, and high viscosity spraying module 4. The control module can use wired or wireless communication connections with molding module 2, ordinary viscosity spraying module 3, and high viscosity spraying module 4.

[0026] The 3D printing equipment 100 provided by the present invention, by employing a molding module 2, a common viscosity jetting module 3, a high viscosity jetting module 4, an ultra-high viscosity jetting module corresponding to different viscosity media, and a control module working together, can solve the problems of existing binder jetting 3D printing being unable to be compatible with printing binders with a wide viscosity range and multiple molding materials, a single nozzle being unable to adapt to media with a full viscosity range, multiple flow channels being prone to mutual interference, and poor coordination of multi-material printing control. Specifically, the molding module 2 is equipped with a printing platform 21 and a powder spreading component 22. The powder spreading component 22 completes the powder spreading to build an initial powder bed on the printing platform 21. The ordinary viscosity jetting module 3 can be raised and lowered and arranged on one side of the frame 1. Its inkjet head 31 is equipped with at least two independent jetting channels that are connected to the feeding system respectively, and is specifically responsible for the jetting operation of ordinary viscosity media. The high viscosity jetting module 4 and the ultra-high viscosity jetting module can be moved and arranged on the frame 1. They are respectively connected to the feeding system by the first high viscosity jetting component 41 and the second high viscosity jetting component, and are respectively responsible for processing high viscosity media and ultra-high viscosity media. The control module is communicatively connected to the molding module 2 and the above three jetting modules. It can schedule a single jetting module to work independently, or it can combine two or even three jetting modules to work together. The combination of jetting modules participating in the work can be selected according to the molding material form and the adhesive viscosity type to realize the partitioned jetting of single or multiple adhesives with different viscosities, and adapt to different molding material combination conditions. Each jetting module has a degree of freedom of raising or lowering or moving, which can match the requirements of printing layer height changes and planar partitioned jetting. Compared to existing technologies that rely on a single jetting device to handle various viscosity media, this invention distributes media of different viscosities to three independent jetting modules for processing. This avoids nozzle clogging and jetting instability issues caused by a single printhead adapting to a wide viscosity range. The above setup uses a standard viscosity jetting module 3 and a high viscosity jetting module 4 to jet low-viscosity and high-viscosity liquid materials respectively, while an ultra-high viscosity jetting module supplements the jetting of high-viscosity materials and the extrusion of high-viscosity plastic substrates. This multi-module flow-dividing architecture achieves wide viscosity range material compatibility, overcoming the limitations of ordinary inkjet heads in jetting high-viscosity materials and the difficulty of a single hardware device simultaneously achieving binder jetting and high-viscosity plastic substrate extrusion. The three jetting modules of different viscosities can be flexibly combined and work collaboratively to achieve combined jetting of standard, high, and ultra-high viscosity media, significantly expanding the viscosity range of binders and molding materials that the equipment can adapt to, and improving the molding stability and molding accuracy of powder bed printing under multi-material, wide viscosity range conditions.

[0027] In one embodiment of the present invention, each inkjet head 31 is one of a piezoelectric inkjet head 31, a thermal inkjet head 31, or a continuous inkjet head 31.

[0028] In this embodiment, to match different materials and molding precision requirements, the type of inkjet head 31 can be selected according to specific needs, and the number of inkjet heads 31 is not limited. It can be understood that the piezoelectric inkjet head 31 generates microdroplets by compressing the fluid through the deformation of the piezoelectric crystal; the thermally foaming inkjet head 31 generates bubbles by heating and pushes the liquid out; the continuous inkjet head 31 continuously ejects liquid flow and achieves selective deposition through electric field sorting.

[0029] It should be noted that the ordinary viscosity jetting module 3 provided by the present invention also has the following technical effects: In the first embodiment, each inkjet head 31 can jet materials of different components through different jetting channels, enabling the two to react in situ on the powder bed of the printing platform 21. It is understood that the spatial position, jetting volume, and reaction sequence of different components can be adjusted according to specific needs. In the second embodiment, each inkjet head 31 can perform spatial dosage control within the powder bed of the printing platform 21 through multiple different jetting channels. The control module can adjust the jetting point density, droplet volume, jetting times, jetting sequence, and coverage of different liquid materials in the XY plane, Z direction, or three-dimensional space, thereby achieving spatial gradient changes in material content, porosity, strength, conductivity, thermal conductivity, magnetism, drug loading, or bioactive components.

[0030] In one embodiment of the present invention, the first high-viscosity spraying element 41 is one of a piezoelectric spraying valve or a needle-type spraying valve; And / or, the type of the second high-viscosity spraying component is one of the following: pneumatic dispensing valve, screw valve, plunger valve, micro-dispensing valve, or DIW direct-write extrusion component.

[0031] In this embodiment, to adapt to different molding methods, both the high-viscosity jetting module 4 and the ultra-high viscosity jetting module can be of different types. It is understood that, to facilitate the printing of high-viscosity powder and paste materials, the high-viscosity jetting module 4 and the ultra-high viscosity jetting module can be used in combination. The high-viscosity jetting module 4 can employ a piezoelectric jet valve, while the ultra-high viscosity jetting module can employ a DIW direct-write extruder. The piezoelectric jet valve can jet high-viscosity materials, while the DIW direct-write extruder can jet fluid materials with a viscosity higher than that of liquids.

[0032] In one embodiment of the present invention, the powder spreading component 22 includes a powder spreading part 221, a powder supply cylinder 222, a forming cylinder 223 and a recovery cylinder 224. The powder spreading part 221 is slidably disposed on the frame 1, and the powder supply cylinder 222 and the forming cylinder 223 are arranged side by side in the printing platform 21. The recovery cylinder 224 is disposed on the side of the printing platform 21 away from the powder supply cylinder 222.

[0033] In this embodiment, the powder spreading section 221 is used to receive powder conveyed from the powder supply cylinder 222. The powder spreading section 221 can be of the type of scraper-type powder spreading, roller-type powder spreading, etc., and can be set according to specific needs. The powder supply cylinder 222 serves as a dedicated storage cavity for powder, centrally storing the powder raw materials required for printing. The powder supply cylinder 222 can be directly embedded in the printing platform 21, or it can be set on the inner wall of the inner cavity of the printing platform 21 by means of bolt connection, etc. The powder spreading section 221 and the powder supply cylinder 222 can be connected by pipeline connection. It is understood that the powder spreading section 221 can be slidably mounted on the frame 1 by means of guide rails and sliders. The guide rails can be fixed on the frame 1 by means of bolt connection, snap-fit, etc. The form of the guide rails can be linear ball guide rails, linear roller guide rails, dovetail groove guide rails, etc., and is not limited here. In one embodiment, a slider is fixed to the bottom of the powder spreading component 22. The slider is directly engaged with the guide rail. The powder spreading component 22 drives the slider to reciprocate along the guide rail, and the slider has a built-in rolling element to achieve movement. In another embodiment, the powder spreading component 22 is equipped with a support roller. The roller is limited and fits against the upper and lower or side guide surfaces of the guide rail. The roller is used to achieve rolling movement along the guide rail. The roller can be configured with a bearing structure. The recovery cylinder 224 is used to collect excess powder that exceeds the printing platform 21 during the powder spreading operation, realizing centralized powder recovery. The recovery cylinder 224 can be installed on the frame 1 by means of snap-fit ​​connection or bolt connection. The upper part of the recovery cylinder 224 has a powder receiving port aligned with the powder spreading endpoint. The bottom of the recovery cylinder 224 can be provided with a discharge port. Optional screening device and negative pressure conveying pipeline can be used to return the powder to the powder supply cylinder 222. The forming cylinder 223 serves as a cavity for layer-by-layer stacking and forming of parts. An adjustable forming base plate is provided inside. The powder spreading part 221 spreads the powder on the forming base plate inside the forming cylinder 223. The powder supply cylinder 222 and the forming cylinder 223 are mounted side by side and fixed inside the printing platform 21. They can be connected to the printing platform 21 by means of flange bolt locking, slot limiting, etc. No limitation is made here.

[0034] It should be noted that the ordinary viscosity spraying module 3 and high viscosity spraying module 4 provided by the present invention also have the following technical effects: In the first embodiment, taking the ceramic powder bed scenario of the printing platform 21 as an example, the ordinary viscosity spraying module 3 sprays low viscosity liquid material, and the high viscosity spraying module 4 sprays high viscosity liquid material. Here, the first low viscosity liquid material can be a low viscosity pre-constraint liquid and a binder, and the high viscosity liquid material can be a high solids content ceramic slurry, a sintering aid, or a functional reinforcing phase, thereby achieving local reinforcement, local densification, or local functionalization of the ceramic preform. In the second embodiment, a penetration inhibitor, boundary conditioner, surface energy conditioner, or local curing agent can be sprayed first through the ordinary viscosity spraying module 3, and then a high viscosity liquid material can be sprayed through the high viscosity spraying module 4; this controls the diffusion range and boundary accuracy of the high viscosity liquid material in the powder bed of the printing platform 21. In the third embodiment, the present invention can also spray two different components of materials through different spraying modules respectively, so that the two can undergo in-situ contact reaction in the initial powder bed. For example, the ordinary viscosity spraying module 3 sprays the low viscosity first component or the first catalyst, and the high viscosity spraying module 4 sprays the high viscosity second component or the main resin; or the ordinary viscosity spraying module 3 can first spray the pre-constraint liquid, and then spray the first component and the second component respectively, so that they can be locally cross-linked, cured, gelled or bonded on the initial powder bed.

[0035] The present invention also proposes a 3D printing method for use in the 3D printing equipment described above, the method comprising the following steps: Construct a 3D model to obtain contour data, material partition data, and injection path data; Based on the contour data, the material partition data, and the jetting path data, the powder spreading component is controlled to spread a powder layer on the printing platform to obtain an initial powder bed. Based on the form of the molding material and the viscosity of the binder, select the corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module, and spray the binder onto the initial powder bed through the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module. The printing platform is controlled to descend to a preset layer thickness, and the steps of controlling the powder spreading component to spread a powder layer on the printing platform according to the contour data, the material partition data, and the jetting path data to obtain an initial powder bed are repeated until printing is completed.

[0036] In this embodiment, combined with Figure 2 The method includes steps S10-S40: Step S10: Construct a 3D model to obtain contour data, material partitioning data, and spraying path data. It should be noted that constructing a 3D model refers to creating a complete digital solid model using 3D modeling software based on the design requirements of the part to be manufactured, such as its shape, internal cavities, functional partitions, gradient material distribution, and local high-viscosity functional enhancement areas. The model simultaneously distinguishes between ordinary powder matrix areas, areas requiring low-viscosity binder spraying, and special functional areas requiring high-viscosity printing material spraying. It carries all the design information regarding the part's shape and material differences. Contour data refers to the boundary geometry information of each layer of the 3D model's two-dimensional plane after layering. It includes the coordinates, line segments, and closed shape parameters of the single-layer part's outer contour, internal hollow boundaries, and functional partitioning boundaries. This accurately defines the area on the powder bed that needs to be formed and cured, distinguishing between the forming area and the blank powder area, thus defining the basic operational boundaries for the spraying module. Material zoning data refers to the supporting data generated based on different material regions pre-divided in the 3D model. It separately marks conventional areas within a single layer where only low-viscosity binders are sprayed, target areas requiring pre-constraint liquid spraying followed by high-viscosity materials, two-component in-situ reaction areas, conductive or thermally conductive gradient functional areas, and drug zones, recording the material type, viscosity, spray dosage, and spray density parameters corresponding to each zone, enabling precise control of various liquid material zones. Spray path data refers to the spray motion trajectory data generated for each type of zone, including the inkjet scanning trajectory of the ordinary viscosity spray module, the pre-constraint liquid spray trajectory, the high-viscosity slurry extrusion or spraying path of the high-viscosity spray module, the moving speed of each spray module, droplet spray frequency, coordinate compensation parameters, and spray timing interval. Understandably, the process involves several steps. First, 3D modeling software is used to construct a 3D model based on the part's shape, internal structure, and differentiated functional requirements. During the modeling phase, different material blocks are simultaneously defined to provide a complete design basis for subsequent layered data extraction. Second, the constructed 3D model undergoes layered slicing operations, disassembling the 3D entity layer by layer into multiple 2D planes. The closed boundary lines and internal / external boundary coordinates of each layer are extracted to form contour data, preventing the sprayed material from exceeding the part's contour and causing dimensional deviations. Then, based on the functional blocks defined during the modeling phase, the data for each zone is matched to distinguish multiple printing zones and prevent the mixing of different functional materials from interfering with the molding process. Finally, combining the single-layer contour range with the material process parameters of each block, the scanning trajectory of the ordinary viscosity spraying module and the walking trajectory of the high viscosity spraying module are generated, and parameters such as spraying speed, landing point compensation, spraying density, and timing interval are simultaneously entered to obtain spraying path data.Furthermore, to improve the initial powder bed's impact resistance and reduce powder contamination in the printing area, the target area for printing the high-viscosity liquid material can be obtained using the aforementioned data. Various pre-constraint patterns can be employed for spraying, including complete coverage, outward expansion coverage, dot matrix, grid, annular boundary, center reinforcement, and gradient dosage. Complete coverage refers to completely covering the target area of ​​the high-viscosity liquid material. Outward expansion coverage means the target area extends a certain distance outward from the landing point of the high-viscosity liquid material to resist droplet edge impact and spread. Dot matrix spraying creates multiple local anchoring points in the powder bed. Grid spraying creates a continuous or semi-continuous impact-resistant network. Annular boundary spraying forms an annular pre-constraint zone outside the boundary of the high-viscosity liquid material target area, limiting subsequent spillage of the high-viscosity material. Center reinforcement spraying increases the pre-constraint liquid spray density in the central region of the high-viscosity liquid material landing point, enhancing the impact center's resistance to disturbance. Gradual dosage type refers to the pre-constraint liquid with different injection volumes set according to the impact energy of high viscosity liquid materials, the boundary accuracy of the target area, or the material spreading requirements.

[0037] Step S20: Based on the contour data, material partitioning data, and jetting path data, control the powder spreading component to spread a powder layer on the printing platform to obtain an initial powder bed. It should be noted that the powder spreading component can uniformly spread various printing powders such as metals, ceramics, polymers, pharmaceuticals, and sand molds on the surface of the printing platform. It can adopt structures such as scraper type, roller type, and hopper powder dropping type, and is responsible for constructing the powder substrate required for each printing layer. The powder spreading component can reciprocate along the frame via guide rails. The printing platform refers to a powder supply cylinder internally integrated for storing printing powder. It can controllably decrease the thickness of each single layer, receiving all the powder spread by the powder spreading component and the formed blank deposited and solidified by the ordinary viscosity jetting module and the high viscosity jetting module, providing a flat and stable forming working surface for powder spreading, low viscosity liquid material jetting, and high viscosity liquid material extrusion jetting. The powder layer refers to the thin layer of powder that the powder spreading component spreads onto the surface of the printing platform in a single pass. Its thickness can be adjusted between 20μm and 500μm, preferably between 50μm and 200μm. It consists of single or mixed powders such as metal powder, ceramic powder, composite powder, and pharmaceutical powder, and serves as a carrier for the deposition and molding of low-viscosity and high-viscosity liquid materials. The initial powder bed refers to the complete and flat powder layer on the printing platform after the powder spreading component has completed the uniform spreading of a single layer of powder, but before any liquid material is sprayed. This is the basic molding substrate, free from localized liquid wetting and powder disturbance. Understandably, the process begins by retrieving pre-analyzed single-layer contour data, material partitioning data, and spraying path data. Pre-process parameters such as the required powder thickness and powder type for the current layer are then read to ensure precise matching between the powder spreading parameters and the single-layer forming requirements, preventing inconsistent powder layer thickness and insufficient powder spreading area. Next, the control module drives the powder spreading component to reciprocate linearly along the frame guide rail, synchronously linking with the powder supply system to continuously deliver powder to the powder spreading start point. The powder spreading component pushes the powder at a uniform speed and scrapes or rolls it to form a uniform powder layer. This operation relies on uniform mechanical movement to achieve even powder spreading, ensuring the accuracy of subsequent liquid spraying molding. Finally, the powder spreading component completes its full stroke and pushes excess powder to the recycling tank for collection. An undisturbed, unwetted initial powder bed forms on the printing platform surface, completing the pre-processing steps for this layer's powder spreading. This avoids uneven spraying droplet penetration and powder collapse caused by uneven powder distribution or powder shortages, providing a suitable operating medium for the localized impact-resistant pre-constraint process.

[0038] Step S30: Based on the morphology of the molding material and the viscosity type of the binder required for the molding material, select the corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module, and spray the binder onto the initial powder bed using the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module. It should be noted that the morphology of the molding material refers to the physical form of the substrate constituting the physical body of the printed part during the printing process. This molding material can be a single material or a combination of multiple different materials; a single material includes powder molding materials, liquid molding materials, and high-viscosity plastic molding materials, wherein high-viscosity plastic molding materials are paste-like or slurry-like molding substrates. The viscosity type of the binder refers to the viscosity property of the binder used to achieve interfacial bonding between materials during the printing process, which can be divided into low viscosity and high viscosity according to viscosity property. It can be understood that the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module are all used for spraying the binder, and the ultra-high viscosity spraying module can also be used to supply the molding material. Among them, the low-viscosity liquid materials involved in the ordinary viscosity jetting module, high viscosity jetting module, and ultra-high viscosity jetting module all correspond to the viscosity type of the binder. The ordinary viscosity jetting module can jet low-viscosity liquid materials. The ordinary viscosity jetting module can be a piezoelectric inkjet head or a thermally foamed inkjet head, which can jet high-precision and low-viscosity liquid materials. Low-viscosity liquid materials refer to liquid materials with a viscosity range of 1cp to 30cp, including ordinary molding binders, local anti-impact pre-constraint liquids, surface energy conditioning liquids, penetration conditioners, crosslinking catalysts, diluents, aqueous coloring liquids, low-concentration colloidal solutions, etc. They have strong fluidity, can be stably discharged through the micro-inkjet flow channel, will not clog the inkjet head, and can uniformly penetrate the gaps between powder particles in the form of micro-droplets. High-viscosity jetting modules can jet high-viscosity liquid materials. Types of high-viscosity jetting modules include piezoelectric jet valves and needle-type jet valves. They can jet medium-precision, high-viscosity liquid materials. High-viscosity liquid materials refer to viscous materials with a viscosity range greater than 30 cp, preferably 30 cp to 200,000 cp, that cannot be stably jetted by ordinary viscosity jetting module inkjet heads. These include high-solids ceramic slurries, conductive metal slurries, silicone rubber, biogels, and other functional slurries. The ejection impact energy is high, and direct jetting into a loose powder bed will damage the powder layer. Ultra-high viscosity jetting modules can supply molding materials and can also jet high-viscosity liquid materials. Types of ultra-high viscosity jetting modules include pneumatic dispensing valves, screw valves, plunger valves, and micro-dispensing valves. They can jet low-precision, ultra-high viscosity materials. Spraying refers to the process of using a regular viscosity spraying module (or a high viscosity spraying module or an ultra-high viscosity spraying module) to directionally output liquid material to the surface of the initial powder bed along the printing path; the binder is an adhesive agent used to bond loose powder forming material particles together, so that the powder layer forms a printing layer with a certain strength.Understandably, the process begins by reading the material partition data obtained from model analysis, identifying the actual shape of the molding material corresponding to the current printing layer, and matching the viscosity of the binder suitable for that molding material. This allows for the selection of different jetting modules. The simultaneous consideration of both the molding material shape and the binder viscosity is crucial because the molding material shape determines whether an extrusion-type jetting module is needed, while the binder viscosity determines the compatibility of the fluid jetting unit, preventing printing failures caused by module-material mismatch. Next, the selected jetting module is invoked, and the binder is applied directionally to the target printing area of ​​the initial powder bed along a preset jetting path. This operation is performed by a standard viscosity jetting module, a high viscosity jetting module, or an ultra-high viscosity jetting module, ensuring that the binder is applied only to the powder bed area corresponding to the part entity, avoiding waste of binder material in non-molding areas. Finally, the binder jetting operation for this layer is completed. This step allows the material particles at the target location within the powder bed to adhere and solidify, forming a single-layer printed entity outline, laying the foundation for subsequent layer-by-layer stacking printing. Furthermore, it should be noted that when the molding material is a single material, the ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module can be selected according to the viscosity type of the adhesive; when the molding material is a combination of multiple different materials, multiple adhesives of different viscosity types can be selected simultaneously for the combined operation according to the viscosity type of the adhesive.

[0039] Step S40: Control the printing platform to descend to a preset layer thickness, and cyclically repeat the steps of controlling the powder spreading component to spread powder layers on the printing platform according to the contour data, material partitioning data, and jetting path data to obtain an initial powder bed, until printing is complete. It should be noted that the printing platform is used to receive the powder layers spread by the powder spreading component, the liquid material deposited by each jetting unit, and the part blanks formed layer by layer throughout the process. It can be vertically raised and lowered in a controlled manner to divide the forming operation space, and is equipped with a powder supply cylinder for powder storage and supply. The preset layer thickness refers to the thickness of a single layer of powder spread in advance based on the printing powder material, forming accuracy, and part performance requirements. It corresponds to the powder spreading height of each layer and determines the single-layer forming resolution and overall printing efficiency. Printing completion means that all two-dimensional single-layer processes obtained by slicing the 3D model have been cyclically executed. Multiple layers of powder and liquid material are bonded and stacked layer by layer to form a complete 3D solid blank. The cyclical processes of powder spreading, jetting, and platform descent are no longer required, and the process enters the part post-processing stage. Understandably, the process begins by moving the printing platform vertically downwards a pre-set distance for a single-layer powder thickness. This action creates a new, flat, and even powder-spreading space above the existing powder layer, preventing issues like part delamination, cracking, and dimensional errors caused by uneven layer thickness. Then, based on the single-layer contour data, material zoning data, and jetting path data, the powder-spreading component moves smoothly back and forth along the frame guide rails. A new, uniform layer of powder is spread on the lowered printing platform, forming a new initial powder bed. The entire single-layer forming process is repeated, including identifying the target area for high-viscosity material, spraying pre-constraint liquid, waiting for the pre-constraint liquid to complete the temporary anti-constraint construction of the powder bed, spraying high-viscosity liquid functional materials, spraying low-viscosity binders and reactive components as needed, and in-layer drying, curing, and shaping. This entire single-layer process is repeated because three-dimensional parts are composed of multiple layers of two-dimensional powder structures, and a single powder layer cannot form a three-dimensional entity. Finally, the entire process of platform descent, powder spreading, and layered spraying continues until all single-layer processes for the 3D model slices are completed. Printing is then considered complete, and all powder spreading, spraying, and platform lifting / lowering movements cease.

[0040] In one embodiment of the present invention, the step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module according to the morphology of the molding material and the viscosity of the binder, and spraying the binder onto the initial powder bed through the ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module includes: Confirm the shape type of the molding material and the viscosity type of all the adhesives to be sprayed, determine whether the set of adhesives to be sprayed contains one or more different viscosity types, and obtain the determination result; When the determination result is yes, for each type of adhesive, a corresponding spraying module is matched, and at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module are used together to spray the adhesive of the corresponding viscosity type into the initial powder bed in sections; If the determination result is negative, select one of the following modules—ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module—based on the viscosity type of the adhesive to spray the adhesive onto the initial powder bed.

[0041] In this embodiment, combined with Figure 3 Step S30 includes steps S31-S33: Step S31: Confirm the morphology of the molding material and the viscosity of all the adhesives to be sprayed, and determine whether the set of adhesives to be sprayed contains one or more different viscosity types, obtaining a judgment result. It should be noted that the morphology of the molding material refers to the material form of the substrate constituting the printed entity in the printing layer, which can be divided into single material forms and combinations of multiple materials, specifically including powder molding materials, liquid molding materials, and high-viscosity plastic molding substrates. The viscosity type of the adhesive refers to the viscosity property of the bonding agent used to achieve material interface bonding, which can be divided into low viscosity types and high viscosity types. The judgment refers to the 3D printing equipment's logical determination of whether the sprayed adhesive is one or more different viscosity types based on the read process data. The judgment result refers to the output result after the logical determination, which is either "yes" or "no." A "yes" result indicates that the adhesive is a combination of one or more different viscosity types, while a "no" result indicates that the adhesive is of only one viscosity type. The three spraying modules can spray not only adhesives but also molding materials. Different binders are sprayed using spraying modules corresponding to their viscosity types. Low-viscosity binders are sprayed using ordinary viscosity spraying modules, high-viscosity binders using high viscosity spraying modules, and ultra-high viscosity binders using ultra-high viscosity spraying modules. Powder molding materials are supplied via a powder supply cylinder, while liquid molding materials are also categorized into low-viscosity and high-viscosity liquid molding materials. High-viscosity plastic molding substrates are ultra-high viscosity fluid molding materials. Low-viscosity liquid molding materials are sprayed using ordinary viscosity spraying modules, high-viscosity liquid molding materials using high viscosity spraying modules, and high-viscosity plastic molding substrates using ultra-high viscosity spraying modules. Understandably, the process involves several steps. First, obtaining the molding material morphology information for the current printing layer and then reading the viscosity parameters of all adhesives to be sprayed in this layer based on the molding material morphology information. This prevents mismatches between subsequent spraying actions and the molding material system. Second, comparing and identifying the viscosity parameters of all adhesives to be sprayed to determine if there are different viscosity types within the set of adhesives to be sprayed, preventing module mismatches and omissions. Finally, the corresponding judgment result is output, which serves as the basis for switching subsequent spraying control branches. This allows the control module to automatically redirect to the corresponding spraying control logic, enabling the selection of a single adapter module for a single viscosity adhesive and the use of multiple modules for partitioned operations for multiple adhesives of different viscosities, thus ensuring spraying stability under different adhesive-molding material combinations.

[0042] Step S32: When the judgment result is yes, for each viscosity type of binder, a corresponding spraying module is matched. At least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module are used in combination to spray the corresponding viscosity type of binder into the initial powder bed in sections. It should be noted that viscosity type refers to the category obtained according to the viscosity of the binder, which is divided into three categories: ordinary viscosity, high viscosity, and ultra-high viscosity. The classification of viscosity here refers to the above embodiment and is not limited here. Binder refers to the liquid medium that plays a role in binding loose powder particles. All three spraying modules can output binder. A spraying module refers to a functional unit that performs binder spraying operations, including ordinary viscosity spraying modules, high viscosity spraying modules, and ultra-high viscosity spraying modules. Ordinary viscosity spraying modules, such as piezoelectric inkjet heads, are designed for spraying low-viscosity binders and offer high-precision spraying capabilities. High viscosity spraying modules, such as piezoelectric spray valves and needle-type spray valves, are designed for spraying high-viscosity binders. Ultra-high viscosity spraying modules, such as DIW extruders, pneumatic dispensing valves, screw valves, plunger valves, and micro-dispensing valves, can extrude high-viscosity plastic molding substrates and also output ultra-high viscosity binders. Zoning refers to dividing the same initial powder bed into multiple different spatial regions, each of which can be allocated for spraying binders of different viscosities. Initial powder bed spraying refers to the operation of applying binder to the surface of an already laid powder layer. Understandably, firstly, after determining that multiple binders of different viscosities exist, each type of binder to be used is iterated through, and a suitable spraying module is assigned to each type of binder. Secondly, in order to simultaneously apply multiple binders within the same powder layer while avoiding mixing and cross-contamination of binders of different viscosities within the flow channel, at least two spraying modules are scheduled to participate in the printing operation of this layer. According to the powder bed space division, binders of different viscosities are allocated to different spatial areas corresponding to the powder bed. Finally, each spraying module is driven to spray the corresponding binder to its respective powder bed spatial position. This enables the application of binders of different viscosities to different areas on the same powder layer, and can adapt to the simultaneous printing of multiple binders under various molding material combinations such as powder materials, powder materials and liquid materials, and powder materials and high-viscosity plastic molding substrates. It eliminates the need for multiple powder layer printing, improving the printing efficiency of multiple binders within a layer and enabling spatial differential control of binder performance within the powder bed layer. Furthermore, in order to mitigate the impact of high-viscosity material spraying, reduce powder splashing and powder layer collapse defects, ensure that the binder fully wets the powder particles, and achieve reliable powder layer bonding and molding, a low-viscosity pre-constraint liquid can be sprayed onto the initial powder bed first through a normal viscosity spraying module, and then a high-viscosity liquid material can be sprayed onto the initial powder bed through a high-viscosity spraying module.The low-viscosity pre-constraint liquid here is a low-viscosity liquid material adapted to ordinary viscosity spraying modules, with a viscosity range of 1cp~30cp. It includes water, solvent, diluted low-viscosity binder, surfactant solution, low-concentration colloid, and photocurable monomer. It is used to construct a temporary impact-resistant structure in the spraying area of ​​high-viscosity materials. By forming powder capillary bridges, weak particle bonding, and adjusting powder surface energy, it improves the impact resistance of the local powder bed. According to the pre-constraint pattern of preset dot matrix, grid, outward expansion coverage, and annular boundary, the low-viscosity pre-constraint liquid is quantitatively sprayed along the planned spraying path to cover the target powder bed area. This allows the pre-constraint liquid to penetrate into the gaps between powder particles, forming capillary bridges and temporary weak bonding structures between particles, thus constructing a local powder bed state with impact resistance.

[0043] Step S33: If the judgment result is negative, select one of the following modules—a normal viscosity spraying module, a high viscosity spraying module, or an ultra-high viscosity spraying module—based on the viscosity type of the adhesive to spray the initial powder bed. It should be noted that a negative judgment result means that the adhesive set to be sprayed contains only an adhesive of a single viscosity type. This means that, firstly, after obtaining the judgment result that only an adhesive of a single viscosity exists, the viscosity type of the adhesive to be applied is read; then, based on the viscosity type, a uniquely suitable spraying module is selected from multiple selectable spraying modules; finally, the selected spraying module is driven to perform the adhesive spraying operation on the powder layer after it has been laid, thereby completing the application of the adhesive to this layer. This allows for adaptation to various printing conditions and ensures the stability and forming accuracy of the adhesive spraying.

[0044] In one embodiment of the present invention, when the determination result is yes, the step of matching a corresponding spraying module for each viscosity type of binder, and using at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module in combination to spray the binder of the corresponding viscosity type into the initial powder bed in sections includes: The adhesive is divided into a first adhesive, a second adhesive, and an Nth adhesive (N is greater than or equal to 2) according to its viscosity coefficient. One or more combinations of the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module are selected according to the viscosity range of each adhesive. Different spraying modules are selected according to the shape type of the molding material to spray the initial powder bed with the adhesive of the corresponding viscosity type.

[0045] In this embodiment, step S32 includes step S321: In step S321, it should be noted that the viscosity coefficient is a physical property parameter that characterizes the viscosity of the binder fluid and is used to distinguish the viscosity range of different binders; the first binder, the second binder, and the Nth binder (N is greater than or equal to 2) refer to the serial numbers assigned to one or more different viscosity binders that need to be sprayed in this printing layer; among them, the first binder and the second binder are the binders output by the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module. The numerical number here is only used to distinguish the type and quantity of binder used and does not represent the order of binder spraying. Viscosity range refers to the viscosity range corresponding to the spraying of ordinary viscosity spraying modules, high viscosity spraying modules, and ultra-high viscosity spraying modules, respectively. These ranges correspond to the suitable working ranges of different spraying modules, as described in the above embodiments, and will not be elaborated further. The form type of the molding material refers to various categories, including powder molding material only, liquid molding material only, high-viscosity plastic molding substrate only, a combination of powder molding material and liquid molding material, a combination of powder molding material and high-viscosity plastic molding substrate, and a combination of liquid molding material and high-viscosity plastic molding substrate. Spraying the corresponding viscosity type of binder means selecting the spraying module based on the binder's viscosity type, and having the spraying module output a binder medium to the initial powder bed that matches the viscosity properties of the binder itself. It can be understood that, firstly, for one or more binders required for this printing layer, the type and quantity of binders are determined by the viscosity coefficients corresponding to different spraying modules, and then different binders are selected. Then, the viscosity range corresponding to each numbered binder is read sequentially, and a spraying module with the appropriate output capability is matched for each binder. The spraying module matching scheme is further verified and confirmed in combination with the current molding material morphology, and the pre-processing actions required for the corresponding molding material are completed. Finally, the confirmed spraying module combination is called to spray the corresponding binder onto the initial powder bed that has been prepared. This processing method can be adapted to the working conditions of any two or more binders working together. On the one hand, it can ensure that each type of binder is output under the appropriate spraying module, avoiding problems such as nozzle clogging and spraying instability. On the other hand, it can be adapted to the pre-processing corresponding to various molding materials, fully covering all multi-binder printing application scenarios in the briefing document, and stably achieving the application of multiple viscosity binders in the same powder bed layer, so as to achieve the purpose of differentiated control of the bonding effect in different areas of the powder bed.

[0046] This step involves several different printing conditions. The following examples illustrate some of these conditions: In the first case, when the adhesive to be sprayed is a combination of two adhesives (i.e., the first adhesive is a low-viscosity adhesive and the second is a high-viscosity adhesive), and the molding material is only in powder form, the ordinary viscosity spraying module and the high viscosity spraying module work together to spray the low-viscosity adhesive and the high-viscosity adhesive into the initial powder bed in sections. In the second case, when the adhesive to be sprayed is a combination of two adhesives (i.e., the first adhesive is a low-viscosity adhesive and the second is a high-viscosity adhesive), and the molding material is a combination of powder and liquid molding material, the ordinary viscosity spraying module and the high viscosity spraying module are used in combination, each selecting a different adhesive for printing; the liquid molding material is sprayed through the ordinary viscosity spraying module (or through the high viscosity spraying module), where the only difference between the two liquid molding materials is their viscosity type. In the third scenario, when the adhesive to be sprayed consists of two combinations—a low-viscosity adhesive and a high-viscosity adhesive—and the molding material is a combination of powder molding material and a high-viscosity plastic molding substrate, a combination of ordinary spraying modules and high-viscosity spraying modules is used, each selecting a different adhesive for printing. The high-viscosity plastic molding substrate is then extruded using an ultra-high viscosity spraying module. In the fourth scenario, when the adhesive to be sprayed contains multiple adhesives (in which case the two adhesives can be a combination of multiple low-viscosity adhesives or multiple high-viscosity adhesives), and the molding material is only a powder molding material, if the multiple adhesives are multiple low-viscosity adhesives, only multiple ordinary viscosity spraying modules are used for spraying the adhesives; if the multiple adhesives are multiple high-viscosity adhesives, only multiple high-viscosity spraying modules are used for spraying the adhesives. In the fifth case, when the adhesive to be sprayed contains multiple adhesives (in this case, the two adhesives can be a combination of multiple low-viscosity adhesives or a combination of multiple high-viscosity adhesives), and the molding material is a combination of powder molding material and high-viscosity plastic molding substrate, when the multiple adhesives are multiple low-viscosity adhesives, only multiple ordinary viscosity spraying modules are used to spray the adhesives, and the high-viscosity plastic molding substrate is sprayed through an ultra-high viscosity spraying module; when the multiple adhesives are multiple high-viscosity adhesives, only multiple high-viscosity spraying modules are used to spray the adhesives, and the high-viscosity plastic molding substrate is sprayed through an ultra-high viscosity spraying module.In the sixth case, when the adhesive to be sprayed contains multiple adhesives (in which case the two adhesives can be a combination of multiple low-viscosity adhesives or a combination of multiple high-viscosity adhesives), and the form of the molding material is a combination of powder molding material and liquid molding material, when the multiple adhesives are multiple low-viscosity adhesives, only multiple ordinary viscosity spraying modules are used to spray the adhesives, and the low-viscosity liquid molding material is sprayed through the ordinary viscosity spraying module or the high-viscosity liquid molding material is sprayed through the high viscosity spraying module; when the multiple adhesives are multiple high-viscosity adhesives, multiple high-viscosity spraying modules are used to spray the adhesives, and the low-viscosity liquid molding material is sprayed through the ordinary viscosity spraying module or the high-viscosity liquid molding material is sprayed through the high viscosity spraying module.

[0047] It should be noted that the specific implementation method of this step is not limited to the above six printing conditions, and can be set according to specific needs.

[0048] In one embodiment of the present invention, the step of selecting one of a normal viscosity spraying module, a high viscosity spraying module, or an ultra-high viscosity spraying module to spray the binder onto the initial powder bed when the determination result is negative includes: The adhesive to be sprayed is taken as a single adhesive, and one of the following modules is selected according to the viscosity range of the single adhesive: ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module; and according to the morphology of the molding material, the selected spraying module is controlled to spray the adhesive of the single viscosity type onto the initial powder bed.

[0049] In this embodiment, step S33 further includes step S331: Step S331 requires clarification. The adhesive to be sprayed refers to the adhesive medium that needs to be applied to the initial powder bed for this printing layer. A single adhesive means that only one adhesive of a specific viscosity type exists within the set of adhesives to be sprayed in this layer. Viscosity range refers to the viscosity value range that distinguishes between ordinary, high, and ultra-high viscosity adhesives, corresponding one-to-one with the adaptive working range of each spraying module. A single viscosity type adhesive means that all adhesives in this layer are within the same viscosity range. In essence, firstly, for the adhesive required for this printing layer, the selection of the corresponding spraying module is determined based on the adhesive's viscosity type. Then, process verification is performed in conjunction with the current molding material's morphology, driving the selected spraying module to spray the single viscosity type adhesive onto the initial powder bed after powder spreading.

[0050] This step involves several different printing conditions. Examples of some of these conditions are given below: In the first case, when the adhesive to be sprayed is a low-viscosity adhesive and the molding material is only a powder molding material, the low-viscosity adhesive is sprayed onto the initial powder bed using the ordinary viscosity spraying module. In the second case, when the adhesive to be sprayed is a high-viscosity adhesive and the molding material is only a powder molding material, the high-viscosity adhesive is sprayed onto the initial powder bed using the high-viscosity spraying module. In the third case, when the adhesive to be sprayed is a low-viscosity adhesive and the molding material is a combination of powder molding material and liquid molding material, the low-viscosity adhesive is sprayed using the ordinary viscosity spraying module, and the low-viscosity liquid molding material is printed using the ordinary spraying module, or the high-viscosity liquid molding material is sprayed using the high-viscosity spraying module. In the fourth case, when the adhesive to be sprayed is a high-viscosity adhesive and the molding material is a combination of powder molding material and liquid molding material, the high-viscosity adhesive is sprayed using the high-viscosity spraying module, and the low-viscosity liquid molding material is printed using the ordinary spraying module, or the high-viscosity liquid molding material is sprayed using the high-viscosity spraying module. In the fifth case, when the adhesive to be sprayed is a low-viscosity adhesive, and the molding material is a combination of powder molding material and high-viscosity plastic molding substrate, the low-viscosity adhesive is sprayed onto the initial powder bed through the ordinary viscosity spraying module, and the high-viscosity plastic molding substrate is extruded through the ultra-high viscosity spraying module. In the sixth case, when the adhesive to be sprayed is a high-viscosity adhesive, and the molding material is only a powder molding material, the high-viscosity adhesive is sprayed onto the initial powder bed through the high-viscosity spraying module, and the high-viscosity plastic molding substrate is extruded through the ultra-high viscosity spraying module.

[0051] It should be noted that the specific implementation method of this step is not limited to the above six printing conditions, and can be set according to specific needs.

[0052] In one embodiment of the present invention, after the step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module according to the morphology type of the molding material and the viscosity type of the binder, and spraying the binder onto the initial powder bed through the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module, the following steps are included: stabilizing the sprayed initial powder bed.

[0053] In this embodiment, it should be noted that the stabilization process refers to, after the liquid material is sprayed, performing one or more combined processes on the initial powder bed formed by the powder layer, including in-layer curing, heating, light exposure, drying, cross-linking, and preliminary shaping, as needed. This process is used to adjust the liquid wetting state and curing degree within the powder bed, strengthen the temporary bonding structure of the powder, and suppress defects such as liquid flow and powder layer disturbance. It can be understood that curing is to quickly form a solid bonding structure to lock in the powder particles, which has the beneficial effect of immediately increasing the hardness of the powder bed in the target area, preventing contour deformation caused by subsequent processes. Heating, drying, and cross-linking processes are used to reduce the fluidity of the liquid on the powder bed surface, preventing the diffusion of high-viscosity slurry from blurring the part boundaries, reducing molding contour errors, and shortening the interlayer waiting time, thus improving the overall printing efficiency. Preliminary shaping is to ensure that the molded structure of this layer has basic structural strength.

[0054] In one embodiment of the present invention, the step of controlling the printing platform to descend a preset layer thickness and repeatedly controlling the powder spreading component to spread a powder layer on the printing platform according to the contour data, the material partition data and the jetting path data to obtain an initial powder bed, until the printing is completed, includes: removing the printed part and performing subsequent processing.

[0055] In this embodiment, it should be noted that "part removal" refers to the removal of the entire powder containing the molded blank from the forming station of the equipment after all the above steps are completed. Subsequent processing refers to operations such as powder removal, curing, degreasing, sintering, heat treatment, and cleaning after part removal. Specifically, powder removal refers to removing loose, unbonded raw powder that is attached to the outside of the part blank and fills the internal pores. Curing refers to fully chemically reacting various binders, pre-constraint liquids, and high-viscosity functional resins inside the part, allowing the organic bonding system to form a stable and continuous skeleton, improving the overall strength of the green blank. Degreasing refers to decomposing, volatilizing, and burning off all organic bonding components, gel carriers, and solvent residues within the blank at high temperatures, leaving only the inorganic powder particle skeleton. Sintering refers to further increasing the furnace temperature after degreasing, causing diffusion and fusion on the surface of the powder particles, achieving densification of the part. Heat treatment refers to temperature control adjustments such as heat preservation, temperature control during heating and cooling, tempering, and solution treatment after sintering, according to the material properties. Cleaning refers to the process of removing sintering residues, oxide scale, precipitated additives, and loose surface dust from the surface of parts using solvents, water, ultrasound, airflow, or other methods to obtain a clean finished product surface.

[0056] The above description is merely an exemplary embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformations made using the contents of the present invention specification and drawings under the technical concept of the present invention, or direct / indirect applications in other related technical fields, are included within the patent protection scope of the present invention.

Claims

1. A 3D printing device, characterized in that, include: frame; A forming module, comprising a printing platform and a powder spreading component, wherein the powder spreading component is disposed on the frame and located above the printing platform; A standard viscosity jetting module is elliptically mounted on one side of the frame and located on one side of the printing platform; the standard viscosity jetting module includes at least one inkjet head, each inkjet head having at least two jetting channels formed therein, each jetting channel being configured to connect to a feeding system respectively; A high-viscosity spraying module is movably mounted on the frame, the high-viscosity spraying module including a first high-viscosity spraying element configured to communicate with the feeding system; An ultra-high viscosity spraying module is movably mounted on the frame, and the ultra-high viscosity spraying module includes a second high viscosity spraying element configured to connect to a feeding system; The control module is communicatively connected to the molding module, the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module.

2. The 3D printing equipment as described in claim 1, characterized in that, Each of the aforementioned inkjet heads is one of the following: piezoelectric inkjet head, thermal inkjet head, or continuous inkjet head.

3. The 3D printing equipment as described in claim 1, characterized in that, The first high-viscosity spraying component is either a piezoelectric spray valve or a needle-type spray valve; And / or, the second high-viscosity spraying component is one of a pneumatic dispensing valve, a screw valve, a plunger valve, a micro-dispensing valve, or a DIW direct-write extruder.

4. The 3D printing equipment as described in claim 1, characterized in that, The powder spreading assembly includes a powder spreading section, a powder supply cylinder, a forming cylinder, and a recycling cylinder. The powder spreading section is slidably disposed on the frame. The powder supply cylinder and the forming cylinder are arranged side by side in the printing platform. The recycling cylinder is disposed on the side of the printing platform away from the powder supply cylinder.

5. A 3D printing method, applied to printing using a 3D printing device as described in any one of claims 1 to 4, characterized in that, The method includes the following steps: Construct a 3D model to obtain contour data, material partition data, and injection path data; Based on the contour data, the material partition data, and the jetting path data, the powder spreading component is controlled to spread a powder layer on the printing platform to obtain an initial powder bed. Based on the form of the molding material and the viscosity of the binder, select the corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module, and spray the binder onto the initial powder bed through the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module. The printing platform is controlled to descend to a preset layer thickness, and the steps of controlling the powder spreading component to spread a powder layer on the printing platform according to the contour data, the material partition data, and the jetting path data to obtain an initial powder bed are repeated until printing is completed.

6. The 3D printing method as described in claim 5, characterized in that, The step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module based on the morphology of the molding material and the viscosity type of the binder, and then spraying the binder onto the initial powder bed using the ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module includes: Confirm the shape type of the molding material and the viscosity type of all the adhesives to be sprayed, determine whether the set of adhesives to be sprayed contains one or more different viscosity types, and obtain the determination result; When the determination result is yes, for each type of adhesive, a corresponding spraying module is matched, and at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module are used together to spray the adhesive of the corresponding viscosity type into the initial powder bed in sections; If the determination result is negative, select one of the following modules—ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module—based on the viscosity type of the adhesive to spray the adhesive onto the initial powder bed.

7. The 3D printing method as described in claim 6, characterized in that, When the determination result is yes, the step of matching the corresponding spraying module for each viscosity type of binder, and using at least two modules from the ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module in combination to spray the binder of the corresponding viscosity type into the initial powder bed in sections includes: The adhesive is divided into a first adhesive, a second adhesive, and an Nth adhesive (N is greater than or equal to 2) according to its viscosity coefficient. One or more combinations of the ordinary viscosity spraying module, the high viscosity spraying module, and the ultra-high viscosity spraying module are selected according to the viscosity range of each adhesive. Different spraying modules are selected according to the shape type of the molding material to spray the initial powder bed with the adhesive of the corresponding viscosity type.

8. The 3D printing method as described in claim 6, characterized in that, When the determination result is negative, the step of selecting one of the following modules—a normal viscosity spraying module, a high viscosity spraying module, or an ultra-high viscosity spraying module—to spray the binder onto the initial powder bed, based on the viscosity type of the binder, includes: The adhesive to be sprayed is taken as a single adhesive, and one of the following modules is selected according to the viscosity range of the single adhesive: ordinary viscosity spraying module, high viscosity spraying module, and ultra-high viscosity spraying module; and according to the morphology of the molding material, the selected spraying module is controlled to spray the adhesive of the single viscosity type onto the initial powder bed.

9. The 3D printing method as described in claim 5, characterized in that, The step of selecting a corresponding ordinary viscosity spraying module, high viscosity spraying module, or ultra-high viscosity spraying module based on the form type of the molding material and the viscosity type of the binder, and then spraying the binder onto the initial powder bed using the ordinary viscosity spraying module, the high viscosity spraying module, or the ultra-high viscosity spraying module includes the following: The initial powder bed after spraying is then stabilized.

10. The 3D printing method as described in claim 5, characterized in that, The process of controlling the printing platform to descend to a preset layer thickness and repeatedly controlling the powder spreading component to spread a powder layer on the printing platform based on the contour data, the material partitioning data, and the jetting path data to obtain an initial powder bed, until printing is completed, includes the following steps: The printed parts are retrieved and then processed.