A method for pre-fracture modification of hard rock strata near the aquifer

By preparing a double-expansion active suspension of calcium silicate-coated nano-calcium oxide powder and slow-release magnesium oxide powder, and combining it with microwave selective heating, the problems of insufficient crack support, weak interfacial bonding and inaccurate heating in the pre-fracture modification of hard rock strata were solved, achieving effective crack support and long-term modification effect.

CN123106345APending Publication Date: 2026-11-17SHENHUA SHENDONG COAL GRP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611452028.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-18
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the process of deep mining of coal, it is difficult to achieve effective support and long-term reinforcement of cracks in the hard rock layer close to the aquifer, the bonding force between the modified material and the rock mass interface is insufficient, and the range of microwave selective heating is difficult to control precisely, which makes it difficult to maintain the pre-splitting modification effect in a long-term stable manner.

Method used

Calcium silicate-coated nano-calcium oxide powder was prepared by reacting nano-calcium oxide with sodium silicate solution. Slow-release magnesium oxide powder was prepared by coating the surface of lightly calcined magnesium oxide powder with citric acid. The magnesium oxide powder, silicon carbide micro powder, calcium silicate-coated nano-calcium oxide powder, slow-release magnesium oxide powder and 3-aminopropyltriethoxysilane were dispersed in an aqueous solution containing hydroxypropyl methylcellulose and sodium polynaphthalene sulfonate to form a double-expansion active suspension. Initial cracks were induced by fiber-reinforced fracturing explosives. The double-expansion active suspension was injected and filled with carbon dioxide gas. The chemical reaction was carried out by selective heating with microwave radiation.

Benefits of technology

It achieves the maintenance of residual crack aperture under high geostress environment, overcomes the crack propagation threshold of hard rock layers with high elastic modulus, improves the bonding force between modified material and rock mass interface, and accelerates chemical reaction by selective heating to avoid heat diffusion to the overlying aquifer, thus ensuring the long-term effectiveness of pre-crack modification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106345A_ABST
    Figure CN123106345A_ABST
Patent Text Reader

Abstract

This invention relates to the field of chemical synthesis technology and discloses a method for pre-fracture modification of hard rock strata located near an aquifer. The method includes preparing calcium silicate-coated nano-calcium oxide powder, slow-release magnesium oxide powder, a double-expansion active suspension, and surface silicate-modified silicon carbide fibers; pressing fiber-reinforced fracturing explosive charges; drilling directional boreholes to induce fracturing; injecting the double-expansion active suspension and sealing it with carbon dioxide; initiating microwave radiation to activate the carbonization and hydration gradient double-expansion reaction; and finally curing to complete the modification.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of chemical synthesis technology, and more specifically, to a method for pre-fracture modification of hard rock strata located close to aquifers. Background Technology

[0002] During deep coal mining, the interlayer spacing of the nearby hard rock layers below the aquifer is 5 to 20 meters, with a compressive strength greater than 120 MPa and a quartz content greater than 70%. These hard rock layers are difficult to collapse during mining, easily forming large-area overhangs and triggering strong mine pressure manifestations.

[0003] In existing technologies, chemical fracturing and expansion material injection techniques are commonly used to deal with such geological conditions. The principle is to inject expansion materials into rock fissures and use the stress generated by the expansion of the material volume to promote the extension of the fissures.

[0004] However, existing technologies suffer from several drawbacks in the unique geomechanical environment of nearby hard rock strata beneath aquifers: initial fractures rapidly rebound and close under high geostress, preventing subsequent expansion materials from penetrating the fractures; the expansion stress generated by a single expansion system is insufficient to overcome the fracture propagation threshold of high-elastic-modulus hard rock strata; carbonization and hydration reaction rates are extremely slow under low-temperature underground conditions, resulting in excessively long engineering modification cycles; the expansion products adhere only physically to the smooth quartzite surface, making them prone to detachment and failure under mining-induced stress disturbances; and existing overall heating methods cannot precisely confine heat within the fracture-filling area, posing a risk of damaging the water-impermeable integrity when heat is conducted upwards to the overlying aquifer. These drawbacks collectively make it difficult to maintain the long-term stable effect of pre-fracture modification of nearby hard rock strata beneath aquifers. Summary of the Invention

[0005] This invention provides a method for pre-fracture modification of hard rock strata located close to aquifers, which solves the technical problems in related technologies, such as the difficulty in achieving effective support and long-term strengthening of fractures in hard rock strata located close to aquifers, insufficient bonding force between modified materials and rock mass interfaces, and difficulty in accurately controlling the range of microwave selective heating.

[0006] This invention discloses a method for pre-fracture modification of nearby hard rock strata below aquifers, comprising the following steps: In situ reaction of nano-calcium oxide in sodium silicate solution was carried out to obtain calcium silicate-coated nano-calcium oxide powder. Slow-release magnesium oxide powder was prepared by coating the surface of lightly calcined magnesium oxide powder with citric acid in anhydrous ethanol. A double-expansion active suspension was prepared by dispersing silicon carbide micro powder, calcium silicate-coated nano-calcium oxide powder, slow-release magnesium oxide powder, and 3-aminopropyltriethoxysilane in an aqueous solution containing hydroxypropyl methylcellulose and sodium polynaphthalene sulfonate. Short silicon carbide fibers were modified by impregnation with sodium silicate solution, and then kneaded and pressed with ammonium nitrate, ferrosilicon powder and sodium carboxymethyl cellulose to form fiber-reinforced catalytic charge. Fiber-reinforced fracturing charge is loaded into the borehole of the target hard rock layer to induce fracturing and form an initial fracture. Surface silicate-modified silicon carbide fibers enter the fracture to form a supporting skeleton. A double-expansion active suspension was injected into the crack and filled with carbon dioxide gas. The crack filling area was selectively heated by a microwave radiation antenna inside the hole, which sequentially triggered carbonization expansion and hydration expansion reactions, and promoted the hydrolysis and condensation of silane coupling agent to form a chemical bonding interface. Allow to cure until the reaction is complete.

[0007] Furthermore, in the preparation of the calcium silicate-coated nano-calcium oxide powder, the mass ratio of nano-calcium oxide to sodium silicate solution with a modulus of 2.0 to 3.0 is 1:1.5 to 1:3. The mixed suspension is heated to 55 to 70°C at a heating rate of 2 to 5°C / min and kept at this temperature for 2 to 3 hours. The reaction product is filtered, washed, dried at 110 to 120°C, and ground to obtain powder with a particle size of 37.5 to 75 μm.

[0008] Furthermore, in the preparation of the slow-release magnesium oxide powder, the activity of the light-burned magnesium oxide powder is not less than 65%, the particle size is 10 to 50 μm, the mass ratio of light-burned magnesium oxide powder to anhydrous ethanol is 1:2.5 to 1:5, the mass ratio of light-burned magnesium oxide powder to citric acid is 1:0.12 to 1:0.28, the mixture is stirred at 28 to 35 °C for 0.5 to 1 h and then filtered. The filter cake is dried at 65 to 80 °C for 3 to 5 h.

[0009] Furthermore, the double-expansion active suspension is prepared by stirring at 180 to 260 parts by weight of water as the base liquid, and includes 8 to 14 parts by weight of hydroxypropyl methylcellulose, 3 to 5 parts by weight of sodium polynaphthalene sulfonate, 20 to 30 parts by weight of silicon carbide micro powder with a particle size of 1 to 10 μm, 30 to 45 parts by weight of calcium silicate-coated nano-calcium oxide powder, 18 to 28 parts by weight of slow-release magnesium oxide powder, and 3 to 6 parts by weight of 3-aminopropyltriethoxysilane at 30 to 40°C at 400 to 500 r / min for 1.5 to 2.5 h, with a viscosity of 800 to 1500 mPa·s.

[0010] Furthermore, in the dual-expansion active suspension, the mass ratio of calcium silicate-coated nano-calcium oxide powder to slow-release magnesium oxide powder is 1:0.4 to 1:0.93, and the particle size of silicon carbide micro powder is 3 to 5 μm.

[0011] Furthermore, the fiber-reinforced catalytic charge is made by kneading 20 to 30 parts by weight of ammonium nitrate, 7 to 12 parts by weight of ferrosilicon powder with a silicon content of not less than 72% and a particle size of 150 to 250 μm, 8 to 15 parts by weight of surface silicate-modified silicon carbide fiber, and 3 to 5 parts by weight of sodium carboxymethyl cellulose with 10 to 15 parts by weight of water, and then pressing it into a cylinder with a diameter of 35 to 42 mm and a length of 50 to 70 mm under a pressure of 5 to 8 MPa. The surface silicate-modified silicon carbide fiber is made by impregnating short silicon carbide fibers with a length of 3 to 8 mm and a diameter of 10 to 20 μm in a sodium silicate solution with a modulus of 2.5 to 3.2 for 1 to 2 hours and then drying it.

[0012] Furthermore, within 20 to 60 minutes after fracturing, a double-expansion active suspension is injected into the borehole at an injection pressure of 10 to 18 MPa, with an injection volume of 0.8 to 2.0 m³ per borehole; after injection, carbon dioxide gas with a pressure of 1 to 3 MPa and a purity of not less than 99% is introduced into the borehole.

[0013] Furthermore, the microwave radiating antenna operates at a frequency of 2.45 GHz and has an output power of 4 to 10 kW. It continuously radiates the fracture filling area for 4 to 12 hours, keeping the temperature of the fracture filling area stable at 80 to 120°C, with the temperature rise of the entire rock strata and the overlying aquifer not exceeding 15°C.

[0014] Furthermore, the microwave radiation adopts an intermittent heating mode, with a cycle of continuous radiation for 30 to 45 minutes followed by a pause of 10 to 15 minutes, and a total effective radiation time of 4 to 12 hours.

[0015] Furthermore, the curing time is 48 to 96 hours, during which the carbon dioxide gas pressure in the pore is maintained at 0.5 to 1.0 MPa by supplementing gas, and the gas supplementation rate is 0.05 to 0.15 MPa / min.

[0016] The beneficial effects of this invention are as follows: This invention addresses the technical problem of rapid rebound and closure of initial cracks under high geostress conditions, which prevents the penetration of expansion materials, by introducing surface silicate-modified silicon carbide fibers into fiber-reinforced fracturing propellant columns. This achieves the technical effect of maintaining the residual crack aperture and ensuring the effective penetration of the dual-expansion active suspension. Furthermore, this invention utilizes a gradient dual-expansion system, with calcium silicate-coated nano-calcium oxide carbonization expansion and citric acid-coated slow-release magnesium oxide powder hydration expansion sequentially in time. This solves the technical problem that the expansion stress of a single expansion system is insufficient to overcome the crack propagation threshold in high-elastic-modulus hard rock formations, achieving the technical effect of cumulative expansion stress meeting the crack propagation requirements of high-strength hard rock formations.

[0017] This invention solves the technical problems of slow reaction rate under low underground conditions and the threat to the integrity of the overlying aquifer by introducing silicon carbide micropowder as a microwave selective absorption medium into a double-expansion active suspension. It achieves the technical effects of selective heating of the fracture filling zone, accelerating the chemical reaction and preventing heat from diffusing into the overlying aquifer.

[0018] This invention solves the technical problem that the weak interfacial bonding between the expansion products and the smooth quartzite surface makes it difficult to maintain the modification effect in the long term by introducing 3-aminopropyltriethoxysilane into the double-expansion active suspension. It achieves the technical effect that the double-expansion products are anchored to the fracture surface through covalent bonding interface and are not easy to fall off under mining stress disturbance. Attached Figure Description

[0019] Figure 1 This is a flowchart of the preparation process of the pre-fracture modification method for the near-distant hard rock layer below the aquifer provided in the embodiments of the present invention; Figure 2 This is a schematic diagram showing a comprehensive comparison of the modification effects of the various embodiments and comparative examples provided in this invention; Figure 3 This is a schematic diagram comparing the temperature distribution of microwave heating and overall heating provided in an embodiment of the present invention; Figure 4 This is a schematic diagram comparing the gradient timing interval and the interface shear strength provided in an embodiment of the present invention; Figure 5 This is a schematic diagram of the volume expansion rate curve of the dual-expansion active suspension curing process provided in the embodiments of the present invention; Figure 6 This is a schematic diagram of the SEM morphology of calcium silicate-coated nano-calcium oxide powder provided in an embodiment of the present invention; Figure 7 This is a schematic diagram of the SEM morphology of the cross-section of the fiber-reinforced detonating explosive column provided in an embodiment of the present invention; Figure 8 This is a schematic diagram of the FTIR spectrum of the double-expanded active suspension filler provided in the embodiment of the present invention. Detailed Implementation

[0020] The subject matter described herein will now be discussed with reference to exemplary embodiments. It should be understood that these embodiments are discussed only to enable those skilled in the art to better understand and implement the subject matter described herein, and changes may be made to the function and arrangement of the elements discussed without departing from the scope of this specification. Various processes or components may be omitted, substituted, or added as needed in the examples. Furthermore, some features described in the examples may be combined in other examples.

[0021] At least one embodiment of the present invention discloses a method for pre-fracture modification of nearby hard rock strata below aquifers, see [link to relevant documentation]. Figure 1 ,include: Step 1, Preparation of calcium silicate-coated nano-calcium oxide powder 45 to 60 parts by weight of nano-calcium oxide are placed in a reaction vessel, and 90 to 130 parts by weight of a sodium silicate solution with a modulus of 2.0 to 3.0 are added. The mixture is stirred and dispersed at a speed of 300 to 400 r / min, so that the nano-calcium oxide particles are uniformly suspended in the sodium silicate solution. The mass ratio of nano-calcium oxide to sodium silicate solution is 1:1.5 to 1:3, preferably 1:2 to 1:2.5. The above mixed suspension is heated to 55 to 70°C at a heating rate of 2 to 5°C / min, and the reaction is maintained at this temperature for 2 to 3 hours. The silicate ions in the sodium silicate react in situ with the calcium ions on the surface of the nano-calcium oxide particles, forming a dense calcium silicate coating layer on the surface of the nano-calcium oxide particles. After the reaction is complete, filter the cake and wash it with deionized water 3 to 4 times to remove residual sodium silicate. Place the cake in an oven and dry it at 110 to 120°C for 5 to 8 hours until it is completely dehydrated. The dried material is then ball-milled and sieved to obtain powder with a particle size of 37.5 to 75 μm (200 to 400 mesh), which is called calcium silicate coated nano-calcium oxide powder.

[0022] Furthermore, the heating process of the mixed suspension in step 1 is carried out at a heating rate of 2 to 5 °C / min to ensure that the in-situ deposition rate of silicate ions on the surface of the nano-calcium oxide particles is uniform, and to avoid local discontinuity of the calcium silicate coating layer due to excessive heating.

[0023] Furthermore, the entire reaction in step 1 is carried out under normal pressure and air atmosphere; the stirring, dispersion and heat preservation reaction stages are all carried out in an open stirred tank, without the need for inert gas protection.

[0024] Furthermore, there is a risk of localized carbonization side reactions during the heat preservation reaction stage in step 1: carbon dioxide in the air can come into contact with the active sites on the surface of the nano-calcium oxide particles that are not yet covered by the calcium silicate coating layer, generating a small amount of calcium carbonate byproduct, resulting in a decrease in the effective calcium oxide content. To suppress this side reaction, continuous stirring is used during the heat preservation reaction stage to keep the nano-calcium oxide particles in suspension, and the liquid film formed by the sodium silicate solution shields the surface of the nano-calcium oxide particles from direct contact with gaseous carbon dioxide; the filtration and deionized water washing operations after the reaction are completed should be completed within 30 minutes to shorten the time that the nano-calcium oxide particles are exposed to air.

[0025] Furthermore, in step 1, the nano-calcium oxide is an alkaline powder and is corrosive. Operators must wear protective gloves and dust masks during weighing and feeding. The sodium silicate solution is strongly alkaline. During preparation and transfer, alkali-resistant gloves and goggles must be worn to avoid direct skin and eye contact.

[0026] Furthermore, the alkaline waste liquid containing residual sodium silicate obtained from filtration in step 1 must be collected centrally and neutralized to neutral before it can be discharged or handed over to a professional waste liquid treatment agency for treatment. It must not be directly discharged into environmental water bodies.

[0027] It should be noted that the calcium silicate coating layer is chemically stable during the preparation and injection of the suspension at room temperature and pressure. It effectively prevents external moisture and carbon dioxide from contacting the internal nano-calcium oxide, inhibiting pre-carbonization of the nano-calcium oxide before construction. During the subsequent microwave heating stage, the temperature of the crack filling zone rises to 80-120℃, and combined with the injection pressure, the calcium silicate coating layer ruptures, allowing the internal nano-calcium oxide to be released in a controlled time and rapidly carbonize in a carbon dioxide atmosphere. The thickness of the calcium silicate coating layer is controlled by coordinating the amount of sodium silicate solution used and the reaction time. A sodium silicate solution with a modulus of 2.0 to 3.0 ensures that the silicate ion concentration is within the appropriate range for the coating reaction rate. If the modulus is too low, the silicate ion concentration will be insufficient, resulting in a discontinuous calcium silicate coating layer; if the modulus is too high, the solution viscosity will be too high, which is not conducive to uniform coating.

[0028] Step 2, Preparation of slow-release magnesium oxide powder 25 to 35 parts by weight of lightly calcined magnesium oxide powder with an activity of not less than 65% and a particle size of 10 to 50 μm are placed in a stirring container. 80 to 120 parts by weight of anhydrous ethanol are added, and the mixture is stirred and dispersed evenly at a speed of 200 to 300 r / min. Then, 4 to 7 parts by weight of citric acid are added, and the mixture is stirred continuously at 200 to 300 r / min at 28 to 35°C for 0.5 to 1 h to ensure that the citric acid is fully dissolved in the ethanol system and uniformly adsorbed and coated on the surface of the lightly calcined magnesium oxide powder particles. The mass ratio of lightly calcined magnesium oxide powder to anhydrous ethanol is 1:2.5 to 1:5, preferably 1:3 to 1:4; the mass ratio of lightly calcined magnesium oxide powder to citric acid is 1:0.12 to 1:0.28, preferably 1:0.15 to 1:0.22. The filter cake was then filtered and placed in an oven at 65 to 80°C for 3 to 5 hours to allow the anhydrous ethanol to evaporate completely, resulting in a slow-release magnesium oxide powder with a citric acid protective layer on the surface. The powder was then sealed for later use.

[0029] Furthermore, in step 2, the citric acid is added by directly adding it to the evenly dispersed lightly calcined magnesium oxide powder anhydrous ethanol suspension without the need to prepare a citric acid solution in advance; the stirring temperature is controlled at 28 to 35°C, which is lower than the boiling point of anhydrous ethanol (78.4°C); the entire operation is carried out in a well-ventilated environment without the need for inert gas protection.

[0030] Furthermore, in step 2, anhydrous ethanol is a flammable liquid (flash point 13°C), and the operation must be carried out in a fume hood or a well-ventilated place, away from open flames and heat sources; operators must wear anti-static work clothes and protective gloves; the stirring container and drying equipment must be reliably grounded to prevent static electricity from igniting ethanol vapors.

[0031] Furthermore, the filtrate obtained in step 2 is mainly composed of anhydrous ethanol, which should be collected in a sealed container for centralized recycling and treatment, and should not be discharged directly; the drying operation should be carried out at 65 to 80°C, and the drying chamber must be kept ventilated to prevent the accumulation of ethanol vapor; the ethanol vapor discharged during the drying process must be led to a safe discharge port through a ventilation duct, away from ignition sources.

[0032] It should be noted that the citric acid protective layer completely coats the surface of the lightly calcined magnesium oxide powder particles under dry conditions at room temperature, inhibiting premature hydration due to contact with moisture in the air. When external water seeps into the cracks, it gradually dissolves the citric acid protective layer. Once the citric acid protective layer is fully dissolved, the lightly calcined magnesium oxide powder particles come into contact with water and undergo a hydration reaction to generate magnesium hydroxide under microwave-maintained conditions of 80-120°C, resulting in a volume expansion effect. Both the dissolution of the citric acid protective layer and the water seepage process within the cracks have time delays. The hydration expansion of the lightly calcined magnesium oxide powder is necessarily later than the carbonization expansion of the nano-calcium oxide, thus creating a gradient superposition effect. The aforementioned activity of the lightly calcined magnesium oxide powder of not less than 65% refers to its activity index measured by the iodine adsorption value method or the citric acid activity determination method. This activity level ensures that the lightly calcined magnesium oxide powder can generate magnesium hydroxide at a sufficient hydration rate after the citric acid protective layer dissolves.

[0033] Step 3, Preparation of the double-expansion active suspension Add 180 to 260 parts by weight of water to a mixing vessel, heat to 30 to 40°C, and then add 8 to 14 parts by weight of hydroxypropyl methylcellulose and 3 to 5 parts by weight of sodium polynaphthalene sulfonate. Stir at 200 to 250 r / min until completely dissolved to form a homogeneous base liquid. Then, add 20 to 30 parts by weight of silicon carbide micro powder with a particle size of 1 to 10 μm, 30 to 45 parts by weight of calcium silicate-coated nano-calcium oxide powder obtained in step 1, 18 to 28 parts by weight of slow-release magnesium oxide powder obtained in step 2, and 3 to 6 parts by weight of 3-aminopropyltriethoxysilane (Chemical Abstracts Service Registry No. 919-30-2, purity not less than 97%) to the above homogeneous base liquid in sequence. Stir continuously at high speed at 400 to 500 r / min at 30 to 40°C for 1.5 to 2.5 h until there are no obvious agglomerated particles and the whole is in a uniform and stable suspension state to obtain a double-expansion active suspension.

[0034] Furthermore, in step 3, the order of adding each solid powder component is as follows: silicon carbide micro powder, calcium silicate-coated nano-calcium oxide powder, and slow-release magnesium oxide powder are added sequentially. After each powder is added, it is stirred evenly at a speed of 400 to 500 r / min before adding the next one. 3-Aminopropyltriethoxysilane is added last after all three powders have been added and dispersed evenly, to avoid premature hydrolysis of 3-aminopropyltriethoxysilane affecting its subsequent functions. The entire preparation process is carried out at 30 to 40°C, under normal pressure, and in an air atmosphere.

[0035] Furthermore, in step 3, 3-aminopropyltriethoxysilane is an organic amine compound that is irritating to the skin and eyes. Operators must wear chemical-resistant gloves and goggles during handling and addition, and operate in a well-ventilated environment.

[0036] Furthermore, in step 3, during the preparation of the dual-expansion active suspension, there is a partial pre-hydrolysis side reaction of 3-aminopropyltriethoxysilane in a homogeneous aqueous base solution. The silanol groups generated by pre-hydrolysis have a low polycondensation rate at 30 to 40°C and will not cause significant gelation of the dual-expansion active suspension within the 12-hour effective usage period. To further suppress the pre-hydrolysis side reaction, 3-aminopropyltriethoxysilane should be slowly added dropwise to the dual-expansion active suspension under stirring to avoid excessively high local concentrations that could accelerate hydrolysis. After preparation, the dual-expansion active suspension should be stored in a sealed container at room temperature, with an effective usage period of no more than 12 hours after preparation.

[0037] Furthermore, the containers and stirring utensils used in the preparation process in step 3 must be thoroughly cleaned with water after use. The cleaning waste liquid contains a small amount of silicon carbide micro powder, nano calcium oxide and silane coupling agent residues, which must be collected and handed over to a professional waste liquid treatment agency for treatment, and must not be directly discharged into the sewer network.

[0038] The mass ratios of each component relative to water are as follows: hydroxypropyl methylcellulose to water is 1:13 to 1:33, preferably 1:18 to 1:25; sodium polynaphthalene sulfonate to water is 1:36 to 1:87, preferably 1:45 to 1:65; silicon carbide micro powder to water is 1:6 to 1:13, preferably 1:7 to 1:10; calcium silicate-coated nano-calcium oxide powder to slow-release magnesium oxide powder is 1:0.4 to 1:0.93, preferably 1:0.5 to 1:0.7; 3-aminopropyltriethoxysilane to water is 1:30 to 1:87, preferably 1:40 to 1:65.

[0039] The viscosity of the prepared double-expansion active suspension was controlled within the range of 800 to 1500 mPa·s. The viscosity was measured at 30 to 40°C using a rotational viscometer (rotor model and speed selected according to the actual viscosity range). The double-expansion active suspension was stored at room temperature in a sealed container and its effective usage period was within 12 hours after preparation.

[0040] Furthermore, the quality control method for the double-expansion active suspension obtained in step 3 is as follows: take a sample of the double-expansion active suspension and use a rotational viscometer to measure its viscosity to confirm that the viscosity is within the range of 800 to 1500 mPa·s; at the same time, take a sample and place it on a clean glass plate for visual inspection to confirm that the double-expansion active suspension is a uniform slurry with no obvious solid particle sedimentation or color unevenness before it can be used for subsequent injection operations.

[0041] The functions of each component are as follows: Silicon carbide micropowder, as a microwave selective absorption medium, has a significantly higher dielectric loss factor for 2.45 GHz microwave frequencies than hard rock minerals such as quartzite, enabling the directional conversion of microwave energy into localized thermal energy and achieving selective heating of the crack filling zone; Hydroxypropyl methylcellulose (viscosity grade 4000 to 6000 mPa·s, 2% aqueous solution measured at 20℃), as a thickening and water-retaining agent, ensures the retention stability of the double-expansion active suspension after injection into the crack by increasing the viscosity; Sodium polynaphthalene sulfonate, as an anionic dispersant, has sulfonic acid groups adsorbed on the surface of powder particles, inhibiting particle agglomeration through electrostatic repulsion; 3-aminopropyltriethoxysilane, as a functional silane coupling agent, contains both ethoxy groups that can react with the surface of inorganic minerals and amino groups that can interact with the expansion products in its molecular structure. Under microwave heating conditions, the ethoxy groups hydrolyze to generate active silanol groups, which undergo a condensation reaction with the surface hydroxyl groups of the quartzite crack surface to form a stable... Chemical bonding interface.

[0042] It should be noted that the particle size of the silicon carbide micropowder is selected to be 1 to 10 μm, preferably 3 to 5 μm. Silicon carbide micropowder with a particle size within this range can maintain dispersion stability in the double-expanded active suspension while providing sufficient specific surface area for efficient microwave absorption. When the particle size is less than 1 μm, the van der Waals forces between particles are too large, leading to agglomeration; when the particle size is greater than 10 μm, sedimentation and stratification are prone to occur.

[0043] Step 4, Surface silicate modification of silicon carbide fibers Eight to 15 parts by weight of silicon carbide chopped fibers with a length of 3 to 8 mm and a diameter of 10 to 20 μm were placed in an impregnation tank, and 20 to 35 parts by weight of a sodium silicate solution with a modulus of 2.5 to 3.2 were added. The mass ratio of silicon carbide chopped fibers to sodium silicate solution was 1:1.3 to 1:4.4, preferably 1:2 to 1:3. After thorough stirring, the fibers were impregnated at room temperature for 1 to 2 hours to allow silicate ions to adsorb onto the surface of the silicon carbide chopped fibers and form a silicate-modified layer. After impregnation, the fibers were filtered, and the silicon carbide chopped fibers were placed in an oven and dried at 60 to 80 °C for 2 to 4 hours. After cooling, the surface silicate-modified silicon carbide fibers were obtained for later use.

[0044] Furthermore, in step 4, the silicon carbide chopped fibers are added in small, multiple batches to the sodium silicate solution. After each addition, the solution is thoroughly stirred until the silicon carbide chopped fibers are evenly dispersed before adding the next batch. This prevents the concentrated addition of silicon carbide chopped fiber bundles from causing local entanglement and agglomeration, which would affect the uniformity of the silicate modified layer. The impregnation process is carried out at room temperature, normal pressure, and in an air atmosphere.

[0045] Furthermore, the sodium silicate solution in step 4 is highly alkaline. Operators must wear alkali-resistant gloves and goggles during preparation and stirring to prevent the solution from splashing onto their skin and eyes.

[0046] Furthermore, the filtrate obtained in step 4 is an alkaline aqueous solution containing residual sodium silicate. It should be collected centrally and neutralized before being discharged or handed over to a professional waste liquid treatment agency. It must not be directly discharged into the environment. The silicate-modified silicon carbide fibers obtained after drying and cooling should be stored in a sealed bag to prevent moisture absorption that could cause the silicate-modified layer to dissolve and fall off.

[0047] The role of the silicate-modified layer is twofold: firstly, by introducing a hydrophilic silicate layer, the original hydrophobic surface properties of the silicon carbide chopped fibers are improved, enabling the silicon carbide chopped fibers to be uniformly dispersed in the aqueous matrix during the preparation of fiber-reinforced cracking propellant columns, and to have good interfacial compatibility with the active components in the double-expansion active suspension after entering the crack space; secondly, the silicate-modified layer can serve as a chemically active interface, further undergoing a condensation reaction with the hydrolysis products of 3-aminopropyltriethoxysilane in the double-expansion active suspension under microwave heating conditions, thereby strengthening the interfacial bonding between the surface silicate-modified silicon carbide fiber support skeleton and the crack filler.

[0048] Step 5, Compression molding of fiber-reinforced fracturing explosive charges Place 20 to 30 parts by weight of ammonium nitrate, 7 to 12 parts by weight of ferrosilicon powder with a particle size of 150 to 250 μm (silicon content not less than 72%), 8 to 15 parts by weight of surface silicate modified silicon carbide fiber obtained in step 4, and 3 to 5 parts by weight of sodium carboxymethyl cellulose in a kneader, add 10 to 15 parts by weight of water, and knead at a speed of 60 to 80 r / min for 15 to 25 min until the material is uniform and there is no dry powder agglomeration. The moisture content of the kneaded material should be controlled between 8% and 12%.

[0049] Furthermore, in step 5, the order of adding each component is as follows: first, dry-mix ammonium nitrate and sodium carboxymethyl cellulose in a kneader until homogeneous; then, add ferrosilicon powder and mix until homogeneous; finally, add surface silicate-modified silicon carbide fiber; and add water slowly in batches while kneading at a speed of 60 to 80 r / min until the moisture content of the kneaded material reaches 8% to 12%. The entire kneading process is carried out in a well-ventilated environment at room temperature.

[0050] Furthermore, the safety compatibility of ammonium nitrate and ferrosilicon powder during the kneading stage in step 5 must be strictly controlled: the kneading temperature must be strictly maintained at room temperature, and kneading operations are prohibited under heating conditions; ammonium nitrate is a strong oxidizing substance, and any sensitive impurities such as organic oils, sulfur, and chlorides must not be mixed in during the kneading process; the kneading equipment and kneading site must be reliably grounded to prevent static electricity accumulation; the kneading operation must be carried out in a well-ventilated dedicated area, and operators must be equipped with personal protective equipment in accordance with relevant safety regulations.

[0051] The mass ratios of each component relative to ammonium nitrate are as follows: the mass ratio of ammonium nitrate to ferrosilicon powder is 1:0.23 to 1:0.6, preferably 1:0.33 to 1:0.5; the mass ratio of ammonium nitrate to surface silicate-modified silicon carbide fiber is 1:0.27 to 1:0.75, preferably 1:0.33 to 1:0.6; the mass ratio of ammonium nitrate to sodium carboxymethyl cellulose is 1:0.1 to 1:0.25, preferably 1:0.13 to 1:0.2; and the mass ratio of ammonium nitrate to water is 1:0.33 to 1:0.75, preferably 1:0.4 to 1:0.6.

[0052] The kneaded material is pressed into cylindrical fiber-reinforced fracturing explosive charges with a diameter of 35 to 42 mm and a length of 50 to 70 mm using a hydraulic press. The molding pressure is controlled at 5 to 8 MPa, and the holding time is 60 to 90 seconds. The pressed fiber-reinforced fracturing explosive charges are then air-dried under natural ventilation for 12 to 24 hours until there are no cracks on the surface and the hardness is uniform, and then ready for use.

[0053] Furthermore, after the fiber-reinforced catalytic cracking cartridges in step 5 are pressed and formed, they must be stored in a cool, dry, and well-ventilated special warehouse, away from heat sources and open flames, and the temperature of the storage area shall not exceed 35°C; the finished cartridges must be packaged individually to prevent them from colliding and being squeezed together.

[0054] Furthermore, the quality inspection method for the fiber-reinforced fracturing propellant columns obtained in step 5 is as follows: for each batch of pressed fiber-reinforced fracturing propellant columns, at least 3 samples are randomly selected for visual inspection to confirm that there are no visible cracks on the surface of the fiber-reinforced fracturing propellant columns and that the end faces are flat; the diameter and length of the fiber-reinforced fracturing propellant columns are measured using vernier calipers to confirm that the dimensions are within the set range; the mass of the fiber-reinforced fracturing propellant columns is weighed using an electronic balance to verify the density uniformity; only after the above inspections are qualified can they be used for the loading operation in step 6.

[0055] It should be noted that ammonium nitrate and ferrosilicon powder constitute an exothermic fracturing reaction system. Under electric ignition, ammonium nitrate decomposes, releasing heat and providing an oxidizing atmosphere. Silicon and iron in the ferrosilicon powder participate in an exothermic oxidation reaction at high temperatures. Together, they rapidly raise the temperature inside the pore to 400-580℃ and the pressure to 50-120MPa, forming an initial radial fracture network in the surrounding rock. Surface silicate-modified silicon carbide fibers are uniformly distributed within the fiber-reinforced fracturing propellant matrix. After the fracturing reaction is complete, they are carried by a high-pressure gas flow and distributed throughout the fracture space. Utilizing their compressive strength (the axial compressive strength of surface silicate-modified silicon carbide fibers is not less than 2000MPa, far exceeding the elastic rebound stress of 15-40MPa in deep surrounding rock), they form a three-dimensional rigid support skeleton, maintaining the residual fracture aperture within the range of 0.1-0.5mm and preventing the fracture from rebounding and closing under high ground stress. The mass ratio of ammonium nitrate to ferrosilicon powder is 1.5:1 to 4.3:1, preferably 2:1 to 3:1. Within this ratio range, the fracturing reaction can generate sufficient temperature and pressure to form an effective fracture network in hard rock layers with a compressive strength greater than 120 MPa.

[0056] Step 6, Directional drilling and initial crack formation At the construction location of the hard rock layer close to the target aquifer, directional drilling technology was used to drill boreholes. The borehole diameter was 5 to 10 mm larger than the diameter of the fiber-reinforced fracturing charge prepared in step 5. A microwave radiating antenna guide with an operating frequency of 2.45 GHz was arranged along the entire borehole wall. The guide was made of high-temperature polytetrafluoroethylene (PTFE), with a 2 to 3 mm gap between the outer diameter of the guide and the borehole wall. After installation, it was fixed to the borehole opening section with a high-temperature pressure-resistant sealing ring. The fiber-reinforced fracturing charges obtained in step 5 were sequentially loaded into the borehole at a density of 3 to 5 charges per meter of borehole depth, with a spacing of approximately 200 to 330 mm between adjacent charges. The borehole opening section, from 2.0 to 3.5 m, was sealed with a fast-setting cement-based sealing material with a compressive strength of not less than 50 MPa.

[0057] After the borehole is sealed and the sealing quality is confirmed to be acceptable, the fiber-reinforced fracturing propellant is ignited using electric ignition. The ignition current is not less than 1.5A, and the ignition duration is not less than 200ms. The fracturing reaction causes a series of radial initial fractures to form in the hard rock layer along the borehole axis. The fractures extend along the brittle fracture surface of the hard rock layer, forming a fracture network radiating outward from the borehole. The surface silicate-modified silicon carbide fibers, uniformly dispersed in the fiber-reinforced fracturing propellant, are carried into the fracture space by the high-pressure gas flow. During the fracture closure process, they are compressed by the surrounding rock to form a three-dimensional rigid support skeleton, maintaining the residual fracture aperture within the range of 0.1 to 0.5 mm.

[0058] Furthermore, in step 6, the electric ignition operation must strictly follow the blasting operation safety procedures: after the explosives are loaded, all personnel must evacuate to a shelter at a safe distance, and the ignition operation can only be carried out after confirming that no one is in the warning area; the ignition circuit must be tested for insulation, and the detonation power supply can only be connected after confirming that there is no short circuit or leakage; after fracturing is completed, no less than 15 minutes must be waited before entering the borehole area for subsequent operations.

[0059] Furthermore, the high-temperature and high-pressure gas (mainly composed of nitrogen, water vapor and a small amount of nitrogen oxides) generated by the cracking reaction in step 6 is discharged through the pressure relief valve of the sealing section. The discharged exhaust gas may contain a small amount of nitrogen oxides. A water spray absorption device must be installed in the orifice exhaust section or the gas must be guided to a well-ventilated place for natural dilution. Construction personnel must not approach the orifice area within 15 minutes after cracking.

[0060] Step 7: Injection and filling of the dual-expansion active suspension and carbon dioxide sealing. Within 20 to 60 minutes after the initial crack formation, the double-expansion active suspension obtained in step 3 is pumped into the borehole through a pre-embedded grouting pipeline at the borehole opening using a grouting pump at an injection pressure of 10 to 18 MPa. The injection volume is controlled at 0.8 to 2.0 m³ per borehole. The injection pressure and cumulative injection volume are monitored throughout the process. Injection is stopped when the injection pressure rises to 120% of the set value and the cumulative injection volume reaches the design volume. After injection, the grouting pipeline is sealed, and then industrial-grade carbon dioxide gas (purity not less than 99%) at a pressure of 1 to 3 MPa is introduced into the borehole as a continuous gaseous carbon source for the subsequent carbonization reaction. The carbon dioxide gas pressure in the borehole is maintained stable through a one-way valve at the borehole opening.

[0061] Furthermore, in step 7, the working pressure of the grouting pump is 10 to 18 MPa, which is a high-pressure operation. The grouting pipeline and its joints must undergo a pressure resistance test before use, and the test pressure shall not be less than 1.5 times the working pressure. During the grouting operation, the operator shall not stand directly in front of the high-pressure pipeline, but shall operate from the side of the pipeline.

[0062] Furthermore, the carbon dioxide gas filling operation in step 7 must be carried out in a well-ventilated construction environment. The carbon dioxide concentration in the filling area must be monitored in real time. When the volume fraction of carbon dioxide in the ambient air exceeds 0.5%, forced ventilation measures should be activated immediately. Operators must be equipped with portable gas detectors. The pipelines and valves of the carbon dioxide filling equipment must be tested for airtightness before use, and the equipment can only be filled to the working pressure after confirming that there are no leaks.

[0063] It should be noted that the injection time window is limited to 20 to 60 minutes after fracturing because the surface silicate-modified silicon carbide fiber support skeleton immediately provides support after fracturing. Within this time window, the fracture maintains a residual opening of 0.1 to 0.5 mm, allowing the double-expanding active suspension to fully penetrate along the open fracture. After 60 minutes, the creep effect of the surrounding rock may cause some displacement of the surface silicate-modified silicon carbide fiber support skeleton, reducing the effective seepage area of ​​the fracture. The injection pressure is selected to be 10 to 18 MPa, preferably 12 to 15 MPa. This pressure range can overcome the fluid flow resistance within the fracture to achieve sufficient filling without extending the fracture and penetrating into the overlying aquifer.

[0064] Step 8, Microwave radiation activation and chemothermal coupling reaction After carbon dioxide gas filling and sealing, the microwave radiating antenna inside the borehole is activated, continuously radiating the fracture zone filled with double-expansion active suspension for 4 to 12 hours at a working frequency of 2.45 GHz and an output power of 4 to 10 kW. The uniformly distributed silicon carbide micropowder in the fracture filling zone preferentially absorbs microwave energy and transfers it to the surrounding filling medium via heat conduction, causing the local temperature of the fracture filling zone to rise at a rate of approximately 8 to 15 °C / min and remain stable at 80 to 120 °C. The microwave absorption capacity of hard rock mineral components such as quartzite is much lower than that of silicon carbide micropowder; the temperature rise of the entire rock layer and the overlying aquifer does not exceed 15 °C, achieving directional heat concentration.

[0065] Furthermore, before starting the microwave radiation activation stage in step 8, it is necessary to confirm that the carbon dioxide gas pressure inside the hole has been stably maintained at 1 to 3 MPa before the microwave radiation antenna can be turned on, so as to ensure that the gaseous carbon source required for the carbonization reaction is continuously supplied throughout the heating stage.

[0066] Furthermore, during the operation of the microwave radiating antenna in step 8, a microwave leakage protection shield must be set up in the aperture area, and operators must not enter within 2m of the aperture during the operation of the microwave radiating antenna; the waveguide connection between the microwave generator and the radiating antenna must be checked for sealing to prevent microwave leakage from causing non-ionizing radiation damage to personnel.

[0067] Furthermore, during the microwave radiation process in step 8, an intermittent heating mode can be adopted: a cycle of continuous radiation for 30 to 45 minutes followed by a 10 to 15 minute pause is performed. During the pause, the heat energy absorbed by the silicon carbide micropowder in the crack filling area is evenly diffused to the surrounding filling medium through heat conduction, making the temperature distribution more uniform and avoiding local overheating that could damage the filling structure. The total effective radiation time for intermittent heating remains 4 to 12 hours.

[0068] Under the combined influence of the above temperature and carbon dioxide atmosphere, the chemical reaction proceeds in the following order: Step 8.1, First Stage Carbonization Expansion: After the temperature in the crack-filled zone rises to 80 to 120°C, the calcium silicate coating layer ruptures under the combined action of thermal stress and injection pressure. The internal nano-calcium oxide is released into the carbon dioxide-rich crack environment, where it rapidly undergoes a carbonization reaction with carbon dioxide to form calcium carbonate crystals. ,in It is nano-calcium oxide. Carbon dioxide gas was used to fill the borehole. (Calcium carbonate, a carbonation expansion product), the expansion stress generated by the growth of calcium carbonate crystals continues to act on the crack tip in a wedge-shaped crack propagation manner, driving the crack to further extend.

[0069] Step 8.2, Second Stage Hydration Expansion: As water continues to seep into the crack, it gradually dissolves the citric acid protective layer on the surface of the slow-release magnesium oxide powder particles. After the citric acid protective layer is fully dissolved, the slow-release magnesium oxide powder particles react with water under high-temperature conditions maintained by microwaves to generate magnesium hydroxide. ,in It is a slow-release magnesium oxide powder. Water seeping from the cracks The hydration expansion product (magnesium hydroxide) produces a volume expansion effect. The peak of hydration expansion occurs after the peak of carbonization expansion, and the two form a gradient superposition in time sequence, with a total expansion rate of 18% to 27%. The accumulated expansion stress is sufficient to overcome the crack propagation threshold of hard rock layers with high elastic modulus.

[0070] Furthermore, the total expansion rate in step 8.2 is characterized as follows: Under laboratory simulation conditions, a double-expanding active suspension is prepared according to the proportions in step 3, injected into a standard mold, placed in a constant temperature chamber at 80 to 120°C, and purged with carbon dioxide gas at 1 to 3 MPa. After curing, it is processed according to the formula... Calculate the total expansion rate, where The total inflation rate, The volume of the filling material after curing is completed. The initial volume of the double-expanding active suspension injected.

[0071] Step 8.3, Interfacial Chemical Bonding: Simultaneously with the aforementioned expansion reaction, the 3-aminopropyltriethoxysilane in the dual-expansion active suspension undergoes accelerated hydrolysis under microwave heating, with the ethoxy group reacting with water to generate an active silanol group (…). ,in The ethoxy group in 3-aminopropyltriethoxysilane, The active silanol group generated by hydrolysis, (Ethanol, a hydrolysis byproduct), active silanol groups undergo a dehydration condensation reaction with the surface hydroxyl groups of the quartzite crack surface to form a stable... The chemically bonded interface anchors the calcium carbonate and magnesium hydroxide dual expansion products to the crack surface, preventing them from falling off under mining stress disturbances.

[0072] Furthermore, the ethanol byproduct generated from the hydrolysis of 3-aminopropyltriethoxysilane in step 8.3 ( Within the crack-filled zone at 80 to 120°C, the carbon dioxide exists in gaseous form. Its accumulation concentration within the sealed pore space is constrained by both the total gas pressure and the partial pressure of ethanol vapor within the pore. The carbon dioxide pressure within the pore is maintained at 1 to 3 MPa, and the partial pressure of ethanol vapor at this total pressure is extremely low, thus there are no conditions for the formation of a flammable gas mixture. Ethanol byproducts are discharged during the pressure relief process at the pore opening after curing. The pressure relief operation must be carried out in a well-ventilated area, and the vented gas should be directed to an area away from open flames.

[0073] Step 9, Maintenance After the microwave radiation activation stage is completed, the wellhead is kept sealed, and the modified area is cured under natural geothermal conditions for 48 to 96 hours. During the curing period, the carbon dioxide gas pressure inside the well is maintained at 0.5 to 1.0 MPa by supplementing gas to ensure that the carbonation reaction continues until the nano-calcium oxide components are fully converted, while ensuring that the double expansion products of calcium carbonate and magnesium hydroxide are fully crystallized and solidified, and that the 3-aminopropyltriethoxysilane interfacial bonding reaction is fully completed. After the curing is completed, the pre-fracture modification process of the nearby hard rock layer below the aquifer is finished.

[0074] Furthermore, during the curing process in step 9, the carbon dioxide gas pressure inside the borehole is monitored in real time by a pressure gauge at the borehole opening. When the pressure is lower than 0.5 MPa, the gas replenishment program is started, and the gas replenishment rate is controlled at 0.05 to 0.15 MPa / min. After the pressure inside the borehole is restored to 0.8 to 1.0 MPa, the gas replenishment is stopped to maintain a continuous supply of gaseous carbon source required for the carbonization reaction.

[0075] Furthermore, after the maintenance in step 9 is completed, the pressure relief operation at the orifice must be carried out slowly, with a pressure relief rate not exceeding 0.1 MPa / min, in order to avoid the sudden drop in air pressure inside the orifice causing impact damage to the filling structure; the carbon dioxide gas discharged during the pressure relief process must be guided to a ventilated area, and the operator must be equipped with a portable gas detector for environmental monitoring.

[0076] Furthermore, after the curing in step 9 is completed, the pre-crack modification effect of the modified area is verified on-site. The verification method is as follows: single-hole acoustic wave testing is used between adjacent boreholes to characterize the degree of crack development by the change rate of acoustic wave velocity of the borehole wall rock before and after curing; at the same time, the residual solid filling material sample in the borehole is taken out, and the formation of calcium carbonate and magnesium hydroxide crystal phases is identified by X-ray diffraction to confirm that the chemical reaction of the double-expansion active suspension has been fully completed.

[0077] This invention involves uniformly distributing surface silicate-modified silicon carbide fibers within a fiber-reinforced fracturing propellant column. After fracturing, these fibers are carried into the fracture space by a high-pressure gas flow, forming a three-dimensional rigid support framework under the pressure of the surrounding rock. The axial compressive strength of the surface silicate-modified silicon carbide fibers is not less than 2000 MPa, exceeding the elastic rebound stress of deep rock strata by 15 to 40 MPa. The support framework does not experience crush failure under high geostress conditions, maintaining the residual fracture aperture within the range of 0.1 to 0.5 mm. This allows the dual-expansion active suspension to penetrate and fill each branch of the fracture before it closes, thus solving the problem of rapid initial fracture rebound closure under high geostress conditions preventing the expansion material from penetrating.

[0078] This invention employs a gradient dual-expansion system, where calcium silicate-coated nano-calcium oxide undergoes carbonization to generate the first stage of expansion, while citric acid-coated slow-release magnesium oxide powder undergoes hydration to generate the second stage of expansion. The time required for the citric acid protective layer to dissolve and the time delay in water seepage within the cracks ensure that the peak of hydration expansion is necessarily later than the peak of carbonization expansion. The two stages of expansion are sequential rather than simultaneous, avoiding stress concentration that could lead to self-damage to the infill. Under simulated laboratory conditions, the dual-expansion active suspension prepared according to the ratio in step 3, after curing at 80 to 120°C and introducing carbon dioxide gas at 1 to 3 MPa, achieves a total expansion rate of 18% to 27%. The accumulated expansion stress is sufficient to overcome the crack propagation threshold of high-strength hard rock layers with an elastic modulus greater than 40 GPa, thus solving the problem of insufficient expansion stress in a single expansion system.

[0079] This invention introduces silicon carbide micropowder as a microwave selective absorption medium into a double-expansion active suspension. The dielectric loss factor of silicon carbide micropowder at the 2.45 GHz microwave frequency is significantly higher than that of rock mineral components such as quartzite. Microwave energy is selectively concentrated in the fracture-filled area, raising the temperature in this area to 80-120°C, while the temperature rise of the entire rock strata and the overlying aquifer does not exceed 15°C. The localized high temperature in the fracture-filled area accelerates the carbonization and hydration reaction rates, compressing the engineering modification cycle to 48-96 hours. Simultaneously, it avoids the risk of thermal damage to the impermeable rock strata and phase change of aquifer water caused by heat diffusion to the nearby overlying aquifer, thus solving the problems of slow reaction rates under low underground conditions and the threat to aquifer integrity posed by the overall heating method.

[0080] This invention introduces 3-aminopropyltriethoxysilane into a double-expansion active suspension. Under microwave heating conditions, its ethoxy groups hydrolyze to generate active silanol groups. These active silanol groups undergo a dehydration condensation reaction with the surface hydroxyl groups on the quartzite crack surface to form... Covalently bonded interface. The calcium carbonate and magnesium hydroxide dual expansion products are anchored to the fracture surface through this covalently bonded interface. The interface bonding mode changes from pure physical adhesion to chemical bonding, making it less prone to detachment under repeated disturbances of mining stress. This solves the problem that the weak interface bonding between the expansion products and the smooth quartzite surface makes it difficult to maintain the modification effect in the long term.

[0081] Furthermore, the main waste generated in the entire process of this invention includes: alkaline waste liquid containing sodium silicate obtained from filtration in steps 1 and 4, anhydrous ethanol filtrate recovered in step 2, equipment cleaning waste liquid in step 3, and nitrogen oxide-containing waste gas emitted during cracking in step 6. The aforementioned alkaline waste liquid is neutralized and then centrally disposed of by a professional waste liquid treatment facility; the anhydrous ethanol filtrate is sealed and recovered, then distilled, purified, and recycled to reduce organic solvent consumption; the equipment cleaning waste liquid contains trace amounts of inorganic powder and silane coupling agent residues, which must be collected and disposed of by a professional waste liquid treatment facility; the nitrogen oxide content in the cracking waste gas is low, and it is discharged after being absorbed by water spray or diluted by natural ventilation. This invention uses water as the main carrier of the double-expansion active suspension, does not use large amounts of toxic organic solvents, and the overall process has the environmental advantage of generating less waste.

[0082] Examples and comparative examples: Example 1

[0083] Step 1: Place 45 parts by mass of nano-calcium oxide in a reaction vessel, add 90 parts by mass of sodium silicate solution with a modulus of 2.0 (mass ratio of nano-calcium oxide to sodium silicate solution 1:2.0), and disperse by stirring at 300 r / min. Increase the temperature to 55℃ at a rate of 2℃ / min and maintain the temperature for 2 h. After the reaction is complete, filter, wash the filter cake three times with deionized water, dry at 110℃ for 5 h, ball mill, and sieve to obtain powder with a particle size of 75 μm (200 mesh) to obtain calcium silicate-coated nano-calcium oxide powder.

[0084] Step 2: Place 25 parts by weight of lightly calcined magnesium oxide powder with an activity of not less than 65% and a particle size of 10 μm in a stirring container, add 80 parts by weight of anhydrous ethanol (the mass ratio of lightly calcined magnesium oxide powder to anhydrous ethanol is 1:3.2), and stir at 200 r / min to disperse evenly. Then add 4 parts by weight of citric acid (the mass ratio of lightly calcined magnesium oxide powder to citric acid is 1:0.16), and continue stirring at 200 r / min at 28℃ for 0.5 h. After filtration, dry at 65℃ for 3 h to obtain slow-release magnesium oxide powder.

[0085] Step 3: Add 180 parts by weight of water to the mixing vessel, heat to 30°C, and then add 8 parts by weight of hydroxypropyl methylcellulose (water ratio 1:22.5) and 3 parts by weight of sodium polynaphthalene sulfonate (water ratio 1:60) in sequence. Stir at 200 r / min until completely dissolved. Then add 20 parts by weight of silicon carbide micro powder with a particle size of 1 μm, 30 parts by weight of calcium silicate-coated nano-calcium oxide powder obtained in Step 1, 18 parts by weight of slow-release magnesium oxide powder obtained in Step 2 (both in a ratio of 1:0.6), and 3 parts by weight of 3-aminopropyltriethoxysilane. Stir continuously at 400 r / min and 30°C for 1.5 h to obtain a double-expansion active suspension with a viscosity of 800 mPa·s.

[0086] Step 4: Place 8 parts by weight of silicon carbide short chopped fibers with a length of 3 mm and a diameter of 10 μm in an impregnation tank, add 16 parts by weight of sodium silicate solution with a modulus of 2.5 (fiber to sodium silicate solution mass ratio 1:2.0), stir thoroughly, and impregnate at room temperature for 1 hour. After filtration, dry at 60°C for 2 hours to obtain surface silicate modified silicon carbide fibers.

[0087] Step 5: Place 20 parts by weight of ammonium nitrate, 7 parts by weight of ferrosilicon powder with a particle size of 150 μm (ammonium nitrate to ferrosilicon powder mass ratio 1:0.35), 8 parts by weight of surface silicate modified silicon carbide fiber obtained in Step 4 (ammonium nitrate to silicon carbide fiber mass ratio 1:0.4), and 3 parts by weight of sodium carboxymethyl cellulose (ammonium nitrate to sodium carboxymethyl cellulose mass ratio 1:0.15) in a kneader, add 10 parts by weight of water (ammonium nitrate to water mass ratio 1:0.5), knead at 60 r / min for 15 min, and control the moisture content of the kneaded material to 8%. Use a hydraulic press to press the kneaded material into cylindrical fiber-reinforced fracturing explosive charges with a diameter of 35 mm and a length of 50 mm, with a molding pressure of 5 MPa, a holding time of 60 s, and natural ventilation drying for 12 h.

[0088] Step 6: The borehole diameter is 5mm larger than the diameter of the fiber-reinforced fracturing charge. The gap between the outer diameter of the microwave radiating antenna conduit and the borehole wall is 2mm. The packing density is 3 charges / m. The spacing between adjacent fiber-reinforced fracturing charges is 200mm. The borehole sealing length is 2.0m. Fracturing is initiated with an ignition current of 1.5A, and the residual crack aperture is maintained at 0.1mm.

[0089] Step 7: Within 20 minutes after fracturing, inject the double-expansion active suspension obtained in step 3 into the injection pressure pump at 10 MPa, with an injection volume of 0.8 m³ / well, and then pressurize with 1 MPa carbon dioxide gas.

[0090] Step 8: Activate the 2.45GHz microwave radiating antenna with an output power of 4kW and a radiating time of 4 hours. The temperature of the crack-filling zone is increased to and maintained at 80℃ at a rate of 8℃ / min, using an intermittent heating mode of continuous radiating for 30 minutes followed by a 10-minute pause. After curing the double-expanding active suspension at 80℃ and introducing 1MPa carbon dioxide gas, the total expansion rate is 18%.

[0091] Step 9: Curing time 48h, maintain carbon dioxide pressure in the borehole at 0.5MPa, gas supply rate at 0.05MPa / min, target gas supply pressure at 0.8MPa, and depressurization rate not exceeding 0.1MPa / min. Example 2

[0092] Step 1: Place 60 parts by mass of nano-calcium oxide in a reaction vessel, add 180 parts by mass of sodium silicate solution with a modulus of 3.0 (mass ratio of nano-calcium oxide to sodium silicate solution 1:3.0), and disperse by stirring at 400 r / min. Increase the temperature to 70℃ at a rate of 5℃ / min and maintain the temperature for 3 h. After the reaction is complete, filter, wash the filter cake four times with deionized water, dry at 120℃ for 8 h, ball mill, and sieve to obtain powder with a particle size of 37.5 μm (400 mesh) to obtain calcium silicate-coated nano-calcium oxide powder.

[0093] Step 2: Place 35 parts by weight of lightly calcined magnesium oxide powder with an activity of not less than 65% and a particle size of 50 μm in a stirring container, add 175 parts by weight of anhydrous ethanol (the mass ratio of lightly calcined magnesium oxide powder to anhydrous ethanol is 1:5.0), and stir at 300 r / min to disperse evenly. Then add 10.5 parts by weight of citric acid (the mass ratio of lightly calcined magnesium oxide powder to citric acid is 1:0.30), and continue stirring at 300 r / min for 1 h at 35 °C. After filtration, dry at 80 °C for 5 h to obtain slow-release magnesium oxide powder.

[0094] Step 3: Add 260 parts by weight of water to the mixing vessel, heat to 40°C, and then add 14 parts by weight of hydroxypropyl methylcellulose (water ratio 1:18.6) and 5 parts by weight of sodium polynaphthalene sulfonate (water ratio 1:52) in sequence. Stir at 250 r / min until completely dissolved. Then add 30 parts by weight of silicon carbide micro powder with a particle size of 10 μm, 45 parts by weight of calcium silicate-coated nano-calcium oxide powder obtained in Step 1, 28 parts by weight of slow-release magnesium oxide powder obtained in Step 2 (both in a ratio of 1:0.62), and 6 parts by weight of 3-aminopropyltriethoxysilane. Stir continuously at 500 r / min at 40°C for 2.5 h to obtain a double-expansion active suspension with a viscosity of 1500 mPa·s.

[0095] Step 4: Place 15 parts by weight of silicon carbide short chopped fibers with a length of 8 mm and a diameter of 20 μm in an impregnation tank, add 45 parts by weight of sodium silicate solution with a modulus of 3.2 (fiber to sodium silicate solution mass ratio 1:3.0), stir thoroughly, and impregnate at room temperature for 2 hours. After filtration, dry at 80℃ for 4 hours to obtain surface silicate modified silicon carbide fibers.

[0096] Step 5: Place 30 parts by weight of ammonium nitrate, 15 parts by weight of ferrosilicon powder with a particle size of 250 μm (ammonium nitrate to ferrosilicon powder mass ratio 1:0.5), 15 parts by weight of surface silicate-modified silicon carbide fiber obtained in Step 4 (ammonium nitrate to silicon carbide fiber mass ratio 1:0.5), and 6 parts by weight of sodium carboxymethyl cellulose (ammonium nitrate to sodium carboxymethyl cellulose mass ratio 1:0.2) in a kneader, add 18 parts by weight of water (ammonium nitrate to water mass ratio 1:0.6), knead at 80 r / min for 25 min, and control the moisture content of the kneaded material to 12%. Use a hydraulic press to press the kneaded material into cylindrical fiber-reinforced fracturing explosive charges with a diameter of 42 mm and a length of 70 mm, with a molding pressure of 8 MPa, a holding time of 90 s, and natural ventilation drying for 24 h.

[0097] Step 6: The borehole diameter is 10mm larger than the diameter of the fiber-reinforced fracturing charge. The gap between the outer diameter of the microwave radiating antenna conduit and the borehole wall is 3mm. The packing density is 5 charges / m. The spacing between adjacent fiber-reinforced fracturing charges is 330mm. The borehole sealing length is 3.5m. Fracturing is initiated with a 2.0A ignition current, and the residual crack aperture is maintained at 0.5mm.

[0098] Step 7: Within 60 minutes after fracturing, inject the double-expansion active suspension obtained in step 3 at a pressure of 18 MPa, with an injection volume of 2.0 m³ / well, and then pressurize with 3 MPa carbon dioxide gas.

[0099] Step 8: Activate the 2.45GHz microwave radiating antenna with an output power of 10kW and a radiating time of 12 hours. The temperature of the crack-filling zone is increased to and maintained at 120℃ at a rate of 15℃ / min, using an intermittent heating mode of continuous radiating for 45 minutes followed by a 15-minute pause. After curing at 120℃ and introducing 3MPa carbon dioxide gas, the total expansion rate of the double-expansion active suspension is 27%.

[0100] Step 9: Curing time 96h, carbon dioxide maintenance pressure in the borehole 1.0MPa, gas supply rate 0.15MPa / min, target gas supply pressure 1.0MPa, pressure relief rate not exceeding 0.1MPa / min. Example 3

[0101] Step 1: Place 52 parts by mass of nano-calcium oxide in a reaction vessel, add 130 parts by mass of sodium silicate solution with a modulus of 2.5 (mass ratio of nano-calcium oxide to sodium silicate solution 1:2.5), and disperse by stirring at 350 r / min. Increase the temperature to 60℃ at a rate of 3℃ / min and maintain the temperature for 2.5 h. After the reaction is complete, filter, wash the filter cake three times with deionized water, dry at 115℃ for 6 h, ball mill, and sieve to obtain powder with a particle size of 56 μm (approximately 270 mesh), thus obtaining calcium silicate-coated nano-calcium oxide powder.

[0102] Step 2: Place 30 parts by weight of lightly calcined magnesium oxide powder with an activity of not less than 65% and a particle size of 30 μm in a stirring container, add 105 parts by weight of anhydrous ethanol (mass ratio of lightly calcined magnesium oxide powder to anhydrous ethanol 1:3.5), stir and disperse evenly at 250 r / min, then add 6.0 parts by weight of citric acid (mass ratio of lightly calcined magnesium oxide powder to citric acid 1:0.20), and continue stirring at 250 r / min for 0.75 h at 30 °C. After filtration, dry at 72 °C for 4 h to obtain slow-release magnesium oxide powder.

[0103] Step 3: Add 220 parts by weight of water to the mixing vessel, heat to 35°C, and then add 11 parts by weight of hydroxypropyl methylcellulose (water ratio 1:20) and 4 parts by weight of sodium polynaphthalene sulfonate (water ratio 1:55) in sequence. Stir at 225 r / min until completely dissolved. Then add 25 parts by weight of silicon carbide micro powder with a particle size of 4 μm, 37 parts by weight of calcium silicate-coated nano-calcium oxide powder obtained in Step 1, 23 parts by weight of slow-release magnesium oxide powder obtained in Step 2 (mass ratio of the two is 1:0.62), and 4.5 parts by weight of 3-aminopropyltriethoxysilane. Stir continuously at 35°C and 450 r / min for 2 h to obtain a double-expansion active suspension with a viscosity of 1150 mPa·s.

[0104] Step 4: Place 11 parts by weight of silicon carbide short chopped fibers with a length of 5 mm and a diameter of 15 μm in an impregnation tank, add 27.5 parts by weight of sodium silicate solution with a modulus of 2.8 (fiber to sodium silicate solution mass ratio 1:2.5), stir thoroughly, and impregnate at room temperature for 1.5 h. After filtration, dry at 70 °C for 3 h to obtain surface silicate modified silicon carbide fibers.

[0105] Step 5: Place 25 parts by weight of ammonium nitrate, 10 parts by weight of ferrosilicon powder with a particle size of 200 μm (ammonium nitrate to ferrosilicon powder mass ratio 1:0.4), 11 parts by weight of surface silicate-modified silicon carbide fiber obtained in Step 4 (ammonium nitrate to silicon carbide fiber mass ratio 1:0.44), and 4 parts by weight of sodium carboxymethyl cellulose (ammonium nitrate to sodium carboxymethyl cellulose mass ratio 1:0.16) in a kneader, add 12.5 parts by weight of water (ammonium nitrate to water mass ratio 1:0.5), and knead at 70 r / min for 20 min, controlling the moisture content of the kneaded material to 10%. Use a hydraulic press to press the kneaded material into cylindrical fiber-reinforced fracturing explosive charges with a diameter of 38 mm and a length of 60 mm, with a molding pressure of 6 MPa, a holding time of 75 s, and natural ventilation drying for 18 h.

[0106] Step 6: The borehole diameter is 7mm larger than the diameter of the fiber-reinforced fracturing charge. The gap between the outer diameter of the microwave radiating antenna conduit and the borehole wall is 2.5mm. The packing density is 4 charges / m. The spacing between adjacent fiber-reinforced fracturing charges is 265mm. The borehole sealing length is 2.75m. Fracturing is initiated with an ignition current of 1.8A, and the residual crack aperture is maintained at 0.3mm.

[0107] Step 7: Within 40 minutes after fracturing, inject the double-expansion active suspension obtained in step 3 at a pressure of 13 MPa, with an injection volume of 1.4 m³ / well, and then pressurize with 2 MPa carbon dioxide gas.

[0108] Step 8: Activate the 2.45GHz microwave radiating antenna with an output power of 7kW and a radiating time of 8 hours. The temperature of the crack-filling zone is increased to and maintained at 100℃ at a rate of 11℃ / min, using an intermittent heating mode of continuous radiating for 37 minutes followed by a 12-minute pause. After curing the double-expanding active suspension at 100℃ and introducing 2MPa carbon dioxide gas, the total expansion rate is 22%.

[0109] Step 9: Curing time 72h, maintain carbon dioxide pressure in the borehole at 0.8MPa, gas supply rate at 0.1MPa / min, target gas supply pressure at 0.9MPa, and depressurization rate not exceeding 0.1MPa / min.

[0110] Comparative Example 1

[0111] Step 1 omits the calcium silicate coating process and directly uses 52 parts by weight of uncoated nano-calcium oxide powder with a particle size of 56 μm (approximately 270 mesh) obtained by ball milling and sieving. All parameters in steps 2 through 9 are the same as in Example 3.

[0112] Comparative Example 2

[0113] Step 2 omits the citric acid coating process and directly uses 30 parts by weight of uncoated light-burned magnesium oxide powder with a particle size of 30 μm and an activity of not less than 65%. All parameters in steps 1 and 3 through 9 are the same as in Example 3.

[0114] Comparative Example 3

[0115] In step 3, silicon carbide micropowder is not added; instead, an equal amount of water (25 parts by mass) is used to replace the silicon carbide micropowder. The amounts of each component in the remaining steps of step 3 are the same as in Example 3. The viscosity of the resulting suspension is adjusted to maintain the same order of magnitude (approximately 1000 mPa·s). In step 8, the microwave radiation antenna inside the borehole is removed, and a conventional integral heating furnace arranged around the borehole area is used to heat the fracture zone and surrounding rock strata as a whole with the same total heat input (equivalent power 7 kW, continuous for 8 hours). The parameters of the remaining steps 6 to 9 are the same as in Example 3.

[0116] experiment:

[0117] Examples 1 to 3 were used to verify that the process of the present invention can achieve stable crack modification effect at different parameter endpoints and preferred ranges. Comparative Examples 1 to 3 were used to verify the necessity of the three key technical features of calcium silicate coating layer, citric acid protective layer and selective microwave absorption of silicon carbide micropowder for the modification effect.

[0118] Specific verifications included: the protective effect and time-controlled release function of the calcium silicate coating layer on the pre-carbonization of nano-calcium oxide; the control effect of the citric acid protective layer on the superposition effect of the time gradient in the dual expansion system; the function of silicon carbide micropowder as a microwave selective absorption medium to achieve local heating of the crack region rather than overall heating; and the comprehensive performance of total expansion rate and interfacial chemical bonding strength under overall process conditions.

[0119] Experimental sample preparation:

[0120] Following the formulations and process parameters specified in Examples 1 to 3 and Comparative Examples 1 to 3, double-expansion active suspensions and fiber-reinforced fracturing explosive charges were prepared on a laboratory scale. To simulate the in-situ geomechanical environment, high-strength quartz sandstone samples (uniaxial compressive strength 125 MPa, quartz content approximately 73%, elastic modulus approximately 42 GPa) were used as the modified rock mass, and a confining pressure of 15 MPa was applied on a hydraulic servo testing machine to simulate a deep high-stress environment. The quartz sandstone samples were standard cylinders with a diameter of 100 mm and a height of 200 mm, with a simulated borehole of 40 mm diameter pre-fabricated in the center. Six quartz sandstone samples were prepared for each set of examples and comparative examples, of which three were used for evaluating the fracture modification effect and three for repeatability verification.

[0121] Experimental conditions:

[0122] Confining pressure of rock sample: 15 MPa (applied by a hydraulic servo testing machine). Simulated borehole temperature conditions: 80°C for Example 1, 120°C for Example 2, and 100°C for Examples 3 and Comparative Examples 1 to 3 (controlled by a constant temperature chamber). Carbon dioxide filling pressure: applied according to the specified values ​​for each example and comparative example. Comparative Example 3: The entire rock sample was heated using an external electric furnace. The surface temperature of the rock sample and the borehole wall were recorded, along with the temperature change at the simulated overlying aquifer location (20 mm from the top of the borehole). Ambient temperature: 25 to 30°C (indoors).

[0123] Experimental steps: Step A: Prepare double-expansion active suspensions according to the formulations of each embodiment and comparative example. Immediately after preparation, measure the viscosity with a rotational viscometer, record the measured viscosity value, and use it within 12 hours after confirming that the viscosity is within the specified range.

[0124] Step B: Insert the fiber-reinforced fracturing charge into the center of the quartz sandstone sample and drill a hole. Seal the hole opening with a fast-setting cement-based plugging material. After curing until the compressive strength of the plugging material is not less than 50 MPa, conduct a fracturing test and record the residual crack opening after fracturing (indirectly characterized on the outside of the hole wall using an ultrasonic detector).

[0125] Step C: Inject the double-expansion active suspension into the borehole of the cracked sample within the specified time window, record the injection pressure and injection volume, and seal the pressure with carbon dioxide gas at the specified pressure after injection is completed.

[0126] Step D: Apply heat in the manner specified in each embodiment and comparative example (microwave radiation was used in Examples 1 to 3 and Comparative Examples 1 to 2, and an integral heating furnace was used in Comparative Example 3), and record the changes in temperature of the crack filling zone and the simulated aquifer location over time.

[0127] Step E: After microwave radiation or overall heating is completed, curing is carried out according to the curing conditions specified in each embodiment and comparative example. After curing is completed, the pressure is released and the sample is removed.

[0128] Step F: The modified quartz sandstone samples were characterized as follows:

[0129] (1) Total expansion rate: according to the formula calculate, The total inflation rate, The volume of the filling material after curing is completed. The initial volume of the double-expanding active suspension injected.

[0130] (2) Shear strength of the infill interface: The infill-rock composite specimens were subjected to a direct shear test on a universal testing machine at a shear rate of 0.5 mm / min. The peak shear force was recorded and converted into the interface shear strength in MPa.

[0131] (3) Retention rate of filling material under mining stress disturbance: Cyclic load (0 to 10 MPa, frequency 1 Hz, 500 cycles, simulating mining stress disturbance) is applied to the modified sample. After the cycle, the residual mass of the filling material is weighed. The retention rate is calculated by the ratio of the mass of the filling material after disturbance to the mass of the initial filling material.

[0132] (4) The highest temperature rise at the simulated aquifer location: The highest temperature rise at 20 mm from the top of the hole during the overall heating process recorded in Comparative Example 3 was compared with the temperature rise at the same location under microwave radiation conditions in Example 3, in °C.

[0133] (5) Carbonation reaction conversion rate: X-ray diffraction analysis was performed on the filling sample, and the conversion rate of nano-calcium oxide to calcium carbonate was estimated by the diffraction peak intensity ratio, in units.

[0134] (6) Difference between the peak time of carbonization expansion and the peak time of hydration expansion (gradient time interval): By analyzing the real-time volume expansion curve during the curing process of the filling body, the peak time of carbonization expansion rate and the peak time of hydration expansion rate are read respectively. The difference is the gradient time interval, in h.

[0135] The experimental or test results are shown in the table below and Figures 2-8 As shown:

[0136] Table 1 Summary of preparation parameters for the double-expansion active suspension in each example and comparative example

[0137] As shown in Table 1, the measured viscosities of the suspensions in Examples 1 to 3 all fell within the specified range of 800 to 1500 mPa·s. Visually, they appeared as uniform slurries with no obvious sedimentation or stratification. Comparative Examples 1 to 3 were also prepared within similar viscosity ranges, ensuring that the interference of rheological differences on the modification effect was minimized in subsequent control experiments.

[0138] Table 2 Summary of preparation parameters for fiber-reinforced destructive propellant columns in each example and comparative example

[0139] As shown in Table 2, the fiber-reinforced destructive charges prepared in Examples 1 to 3 and Comparative Examples 1 to 3 all have qualified appearances, dimensions within the specified range, and the moisture content of the kneading material meets the control requirements of 8% to 12%, and can be used for subsequent charge loading operations.

[0140] Table 3 Comparison of temperature distribution between microwave heating and overall heating (location of crack filling zone and simulated aquifer)

[0141] As shown in Table 3, Examples 1 to 3, employing the synergistic effect of silicon carbide micropowder and microwave radiation, selectively raised the temperature of the fracture-filled zone to 80-120°C, while the maximum temperature rise at the simulated aquifer location was only 9-14°C, far below the threshold that could cause thermal damage to the aquitard. Comparative Example 3, using a monolithic heating furnace without silicon carbide micropowder in the suspension, achieved a maximum temperature rise of 47°C at the simulated aquifer location, approximately 327% higher than in Example 3, indicating that the monolithic heating method carries the risk of significant heat diffusion to the overlying aquifer. Furthermore, the temperature rise rate of the fracture-filled zone in Comparative Example 3 was only 3.2°C / min, significantly lower than that of the microwave radiation mode, reflecting a significant reduction in heat transfer efficiency under conditions without a selective absorbing medium.

[0142] Table 4. Comprehensive comparison of the modification effects of each embodiment and comparative example

[0143] As can be seen from the results in Table 4, Examples 1 to 3, which meet all the necessary conditions of the present invention, show excellent performance in various indicators such as total expansion rate, carbonization reaction conversion rate, gradient time interval, interface shear strength and retention rate of backfill after mining disturbance. The specific analysis is as follows.

[0144] Comparative Example 1 omitted the calcium silicate coating process. The uncoated nano-calcium oxide was exposed to a carbon dioxide atmosphere prematurely during suspension preparation and injection, resulting in pre-carbonization. This significantly reduced the effective calcium oxide content available for expansion reaction upon reaching the crack filling zone. The total expansion rate of Comparative Example 1 was only 8.3%, approximately 62% lower than Example 3 (22.1%); the carbonization reaction conversion rate was only 52%, approximately 44% lower than Example 3 (93%). These data indicate that the calcium silicate coating layer is indispensable for pre-carbonization protection of nano-calcium oxide during construction and for subsequent time-controlled release. Due to the significant attenuation of carbonization expansion in Comparative Example 1, the expansion peaks of the two stages were difficult to distinguish effectively, and the gradient time interval was not comparable; therefore, it was marked with "—".

[0145] Comparative Example 2 omitted the citric acid coating process. The uncoated lightly calcined magnesium oxide powder came into contact with water during the preparation of the dual-expansion active suspension and began hydration. The peak time of hydration expansion was almost synchronous with the peak time of carbonization expansion, with a gradient time interval of only 0.4 h, which was about 91% shorter than that of Example 3 (4.5 h). The two stages of expansion were almost simultaneously superimposed, resulting in local stress concentration and microcracks in the infill. Although the total expansion rate (14.6%) was higher than that of Comparative Example 1, it was about 34% lower than that of Example 3. Moreover, the interfacial shear strength (2.71 MPa) was close to that of Example 3 (2.73 MPa), indicating that the interface between the infill and the rock surface was not the main point of damage, but rather the integrity of the internal structure of the infill was affected, ultimately resulting in a loss of total expansion efficiency.

[0146] Comparative Example 3, which did not add silicon carbide micropowder and used a monolithic heating furnace, maintained the temperature of the fracture filling zone at 100°C, but the heating rate (3.2°C / min) was significantly lower than that of Example 3 (11°C / min). The carbonization and hydration reaction rates were limited by inefficient heat transfer, and the carbonization reaction conversion rate (61%) was about 34% lower than that of Example 3 (93%), and the total expansion rate (13.4%) was about 39% lower than that of Example 3. More importantly, the monolithic heating caused the highest temperature at the simulated aquifer location to rise to 47°C, which is about 4.3 times that of Example 3 (11°C), exceeding the thermal stability threshold of the aquifer group and posing a risk of damaging the integrity of the aquifer. Meanwhile, the interfacial shear strength of Comparative Example 3 (1.82 MPa) was about 33% lower than that of Example 3 (2.73 MPa). Under the overall heating mode, the hydrolysis active silanol group generation rate of 3-aminopropyltriethoxysilane was low, and the degree of Si-O-Si chemical bonding interface formation was insufficient, which led to a decrease in the interfacial bonding strength between the filling body and the quartzite fracture surface. Consequently, the retention rate of the filling body after mining disturbance (75.4%) was about 16% lower than that of Example 3 (89.6%).

[0147] Based on the above experimental results, Examples 1 to 3 achieved stable performance across the entire parameter range, with a total expansion rate of 18% to 27%, a gradient time interval of 3.2 to 5.8 h, an interfacial shear strength of 2.41 to 2.89 MPa, and a backfill retention rate of 87.3% to 91.2% after mining disturbance. Furthermore, the temperature rise at the simulated aquifer location consistently did not exceed 15°C. The three key technical features (calcium silicate coating, citric acid protective layer, and selective microwave absorption by silicon carbide micropowder) are indispensable. Each feature addresses the core technical challenges of nano-calcium oxide pre-carbonization protection and time-controlled release, gradient dual expansion time control, and selective heating of the fracture zone and aquifer thermal protection. Their synergistic effect ensures the engineering effectiveness and safety of pre-fracture modification of the nearby hard rock strata below the aquifer.

[0148] The embodiments of the present invention have been described above. However, the embodiments are not limited to the specific implementation methods described above. The specific implementation methods described above are merely illustrative and not restrictive. Those skilled in the art can make more equivalent embodiments under the guidance of the present embodiments, and all of them are within the protection scope of the present embodiments.

Claims

1. A method for pre-fracture modification of a nearby hard rock stratum below an aquifer, characterized in that, Includes the following steps: In situ reaction of nano-calcium oxide in sodium silicate solution was carried out to obtain calcium silicate-coated nano-calcium oxide powder. Slow-release magnesium oxide powder was prepared by coating the surface of lightly calcined magnesium oxide powder with citric acid in anhydrous ethanol. A double-expansion active suspension was prepared by dispersing silicon carbide micro powder, calcium silicate-coated nano-calcium oxide powder, slow-release magnesium oxide powder, and 3-aminopropyltriethoxysilane in an aqueous solution containing hydroxypropyl methylcellulose and sodium polynaphthalene sulfonate. Short silicon carbide fibers were modified by impregnation with sodium silicate solution, and then kneaded and pressed with ammonium nitrate, ferrosilicon powder and sodium carboxymethyl cellulose to form fiber-reinforced catalytic charge. Fiber-reinforced fracturing charge is loaded into the borehole of the target hard rock layer to induce fracturing and form an initial fracture. Surface silicate-modified silicon carbide fibers enter the fracture to form a supporting skeleton. A double-expansion active suspension was injected into the crack and filled with carbon dioxide gas. The crack filling area was selectively heated by a microwave radiation antenna inside the hole, which sequentially triggered carbonization expansion and hydration expansion reactions, and promoted the hydrolysis and condensation of silane coupling agent to form a chemical bonding interface. Allow to cure until the reaction is complete.

2. The pre-crack modification method according to claim 1, characterized in that, In the preparation of the calcium silicate-coated nano-calcium oxide powder, the mass ratio of nano-calcium oxide to sodium silicate solution with a modulus of 2.0 to 3.0 is 1:1.5 to 1:

3. The mixed suspension is heated to 55 to 70°C at a heating rate of 2 to 5°C / min and kept at this temperature for 2 to 3 hours. The reaction product is filtered, washed, dried at 110 to 120°C, and ground to obtain powder with a particle size of 37.5 to 75 μm.

3. The pre-crack modification method according to claim 1, characterized in that, In the preparation of the slow-release magnesium oxide powder, the activity of the light-burned magnesium oxide powder is not less than 65%, the particle size is 10 to 50 μm, the mass ratio of light-burned magnesium oxide powder to anhydrous ethanol is 1:2.5 to 1:5, the mass ratio of light-burned magnesium oxide powder to citric acid is 1:0.12 to 1:0.28, the mixture is stirred at 28 to 35 °C for 0.5 to 1 h and then filtered. The filter cake is dried at 65 to 80 °C for 3 to 5 h.

4. The pre-crack modification method according to claim 1, characterized in that, The double-expansion active suspension is prepared by stirring at 400 to 500 r / min for 1.5 to 2.5 h at 30 to 40 °C for 1.5 to 2.5 h with 180 to 260 parts by weight of water as the base liquid, and comprising 8 to 14 parts by weight of hydroxypropyl methylcellulose, 3 to 5 parts by weight of sodium polynaphthalene sulfonate, 20 to 30 parts by weight of silicon carbide micro powder with a particle size of 1 to 10 μm, 30 to 45 parts by weight of calcium silicate-coated nano-calcium oxide powder, 18 to 28 parts by weight of slow-release magnesium oxide powder and 3 to 6 parts by weight of 3-aminopropyltriethoxysilane. The viscosity is 800 to 1500 mPa·s.

5. The pre-crack modification method according to claim 4, characterized in that, The mass ratio of calcium silicate-coated nano-calcium oxide powder to slow-release magnesium oxide powder in the double-expansion active suspension is 1:0.4 to 1:0.93, and the particle size of silicon carbide micro powder is 3 to 5 μm.

6. The pre-crack modification method according to claim 1, characterized in that, The fiber-reinforced catalytic charge is made by kneading 20 to 30 parts by weight of ammonium nitrate, 7 to 12 parts by weight of ferrosilicon powder with a silicon content of not less than 72% and a particle size of 150 to 250 μm, 8 to 15 parts by weight of surface silicate-modified silicon carbide fiber, and 3 to 5 parts by weight of sodium carboxymethyl cellulose with 10 to 15 parts by weight of water, and then pressing it into a cylinder with a diameter of 35 to 42 mm and a length of 50 to 70 mm under a pressure of 5 to 8 MPa. The surface silicate-modified silicon carbide fiber is made by impregnating short silicon carbide fibers with a length of 3 to 8 mm and a diameter of 10 to 20 μm in a sodium silicate solution with a modulus of 2.5 to 3.2 for 1 to 2 hours and then drying.

7. The pre-crack modification method according to claim 1, characterized in that, Within 20 to 60 minutes after fracturing, a double-expansion active suspension is injected into the borehole at an injection pressure of 10 to 18 MPa, with an injection volume of 0.8 to 2.0 m³ per borehole; after injection, carbon dioxide gas with a pressure of 1 to 3 MPa and a purity of not less than 99% is introduced into the borehole.

8. The pre-crack modification method according to claim 1, characterized in that, The microwave radiating antenna operates at a frequency of 2.45 GHz and has an output power of 4 to 10 kW. It continuously radiates the fracture-filled area for 4 to 12 hours, keeping the temperature of the fracture-filled area stable at 80 to 120°C, with the temperature rise of the entire rock strata and the overlying aquifer not exceeding 15°C.

9. The pre-crack modification method according to claim 8, characterized in that, The microwave radiation adopts an intermittent heating mode, with a cycle of continuous radiation for 30 to 45 minutes followed by a pause of 10 to 15 minutes, and a total effective radiation time of 4 to 12 hours.

10. The pre-crack modification method according to claim 1, characterized in that, The curing time is 48 to 96 hours. During the curing period, the carbon dioxide gas pressure in the pore is maintained at 0.5 to 1.0 MPa by supplementing gas, and the gas supplementation rate is 0.05 to 0.15 MPa / min.