Method for preparing pimelic acid using polycaprolactone
By using the catalytic reaction of PCL with pimelic acid metal salt and rhodium carbonyl complex under the action of carbon monoxide and hydrogen, the problem of converting PCL into high-value-added dicarboxylic acids in the existing technology has been solved, and pimelic acid has been prepared with high selectivity, thereby improving the resource utilization efficiency of waste polymers.
Patent Information
- Application Number
- CN202611363180.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-03
- Publication Date
- 2026-11-17
AI Technical Summary
Existing PCL recycling technologies suffer from problems such as insufficient reaction directionality, complex byproducts, limited added value of target products, and cumbersome separation and purification processes, making it difficult to directly convert waste PCL into high-value-added dicarboxylic acids.
A catalytic reaction was carried out in a closed reactor using PCL, pimelic acid metal salt, a rhodium carbonyl complex, and a mixed solvent (formic acid and water). Carbon monoxide and hydrogen were introduced to directionally convert PCL into pimelic acid through the catalytic process. The pimelic acid metal salt was used to stabilize the low-valent rhodium active center and improve selectivity.
This method achieves highly selective conversion of PCL to pimelic acid, enhances the high-value utilization of waste polymers, simplifies the separation and purification process, and improves the yield and selectivity of the target product.
Smart Images

Figure CN123106400A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of chemical recycling technology, and in particular to a method for preparing pimelic acid using polycaprolactone. Background Technology
[0002] Polycaprolactone (PCL) is an aliphatic polyester material with good biocompatibility and biodegradability, widely used in packaging materials, medical materials, 3D printing materials, and daily consumer products. With the continuous expansion of PCL production and application, the amount of oligomer waste and post-consumer waste generated during its production process is constantly increasing. How to achieve high-value conversion of waste PCL has become an important research direction in the field of polymer waste resource utilization and green recycling.
[0003] Existing PCL recycling technologies mainly fall into two categories: physical recycling and chemical recycling. Chemical recycling methods primarily include hydrolysis, alcoholysis, and pyrolysis, converting PCL into products primarily composed of ε-caprolactone (ε-CL) or 6-hydroxyhexanoic acid. However, these technologies typically suffer from problems such as insufficient reaction directionality, complex byproducts, limited added value of the target product, and cumbersome subsequent separation and purification processes. Furthermore, waste PCL is usually difficult to directly convert into high-value-added dicarboxylic acids. Summary of the Invention
[0004] Therefore, it is necessary to provide a method and application for preparing pimelic acid using PCL to address the above problems. The preparation method can catalytically convert PCL into pimelic acid in a directional and highly selective manner, thereby realizing the high-value transformation of waste polymers into fine chemical intermediates.
[0005] A method for preparing pimelic acid using PCL includes the following steps:
[0006] PCL, heptanedioic acid metal salt, rhodium carbonyl complex, and mixed solvent are mixed and placed in a closed reactor, wherein the mixed solvent includes formic acid and water;
[0007] A mixture of carbon monoxide and hydrogen gas is introduced into the closed reactor, and a catalytic reaction is carried out by heating. After the reaction is completed, the mixture is separated and purified to obtain pimelic acid.
[0008] In one embodiment, the molar amount of the pimelic acid metal salt is 5% to 20% of the molar amount of the PCL repeating unit;
[0009] And / or, the molar amount of the rhodium carbonyl complex is 1% to 10% of the molar amount of the PCL repeating unit;
[0010] And / or, the amount of the mixed solvent added to each gram of PCL is 2 mL to 20 mL;
[0011] And / or, the mixed gas is introduced into the closed reactor until the pressure in the closed reactor reaches 4.5 MPa to 5.5 MPa.
[0012] In one embodiment, the volume ratio of formic acid to water in the mixed solvent is 1:3 to 1:8;
[0013] And / or, in the mixed gas, the volume ratio of carbon monoxide to hydrogen is 1:0.5 to 1:2.
[0014] In one embodiment, the metal element in the pimelic acid metal salt is selected from at least one of alkali metals, alkaline earth metals, or transition metals.
[0015] And / or, the carbonyl rhodium complex is selected from carbonyl rhodium complexes in which rhodium is monovalent and contains two carbonyl groups.
[0016] In one embodiment, the pimelic acid metal salt is selected from at least one of calcium pimelic acid, sodium pimelic acid, potassium pimelic acid, or zinc pimelic acid.
[0017] In one embodiment, the carbonyl rhodium complex is selected from at least one of dicarbonylacetylacetone rhodium or tetracarbonyl dichloride.
[0018] In one embodiment, the catalytic reaction is carried out at a temperature of 120 °C to 160 °C for a time of 9 h to 11 h.
[0019] In one embodiment, the separation and purification steps include: mixing the reaction solution obtained from the catalytic reaction with an alkaline aqueous solution, then extracting it with an organic solvent and collecting the aqueous phase; then adjusting the pH to 2-4 to precipitate pimelic acid crystals; collecting the obtained solid through solid-liquid separation, washing and drying it to obtain pimelic acid.
[0020] In one embodiment, the PCL is selected from waste containing PCL.
[0021] In one embodiment, the number-average molecular weight of the PCL is selected from 400 Da to 100,000 Da.
[0022] In this invention, PCL is first degraded into hydroxyl-terminated PCL oligomers under high temperature and formic acid, then further degraded into alkenyl-terminated PCL oligomers, and finally gradually depolymerized into 5-hexenoic acid. Then, the carbonyl rhodium complex is used to generate a hydrogen rhodium carbonyl active species in situ under the action of a carbon monoxide and hydrogen mixture. The terminal carbon-carbon double bond of 5-hexenoic acid coordinates with the active rhodium center and undergoes hydrogen metallization, preferentially generating a straight-chain alkyl-rhodium intermediate. Then, through the migration and insertion of carbon monoxide, an acyl-rhodium intermediate is formed, which undergoes nucleophilic attack and hydrolysis by water to obtain dicarboxylated pimelic acid, while simultaneously regenerating the hydrogen rhodium carbonyl active species, completing the catalytic cycle. During the catalytic reaction, the carboxylate group in the pimelic acid metal salt promoter can stabilize the low-valence rhodium active center, improve the proton transfer efficiency of the system, reduce by-product formation, and improve the selectivity of pimelic acid. Therefore, the preparation method of this application can directionally catalytically convert PCL into pimelic acid, achieving highly selective preparation of pimelic acid, which is beneficial for the high-value recycling of PCL waste. Attached Figure Description
[0023] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0024] Figure 1 This is a gas chromatogram obtained after the reaction solution obtained in Example 1 of the present invention has undergone methyl esterification derivatization. Detailed Implementation
[0025] To facilitate understanding of the present invention, it will be described in more detail below. However, it should be understood that the present invention can be implemented in many different forms and is not limited to the embodiments or examples described herein. Rather, these embodiments or examples are provided to make the disclosure of the present invention more thorough and complete.
[0026] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein in the specification of this invention is for the purpose of describing particular embodiments or examples only and is not intended to limit the invention. The optional scope of the term "and / or" as used herein includes any one of two or more of the related listed items, as well as any and all combinations of the related listed items, including any two related listed items, any more related listed items, or a combination of all the related listed items.
[0027] In this invention, numerical ranges are involved. Unless otherwise specified, the numerical ranges are considered continuous and include the minimum and maximum values of the range, as well as every value between the minimum and maximum values. Furthermore, when the range refers to integers, it includes every integer between the minimum and maximum values of the range. Additionally, when multiple ranges are provided to describe features or characteristics, the ranges may be merged. In other words, unless otherwise specified, all ranges disclosed herein should be understood to include any and all subranges to which they are included.
[0028] This invention provides a method for preparing pimelic acid using PCL, comprising the following steps:
[0029] PCL, heptanedioic acid metal salt, rhodium carbonyl complex, and mixed solvent are placed in a closed reactor. The mixed solvent includes formic acid (HCOOH) and water (H2O).
[0030] A mixture of carbon monoxide (CO) and (H2) gas is introduced into the closed reactor, and a catalytic reaction is carried out by heating. After the reaction is completed, the mixture is separated and purified to obtain pimelic acid.
[0031] The catalytic reaction process of this invention is as follows, where n≥3, and n, x, y, z, and m are all positive integers, and R, R 1 and R 2 Each of the following groups is independently selected from hydroxyl, hydrogen, and C1-C20 straight-chain or branched alkane groups, preferably R, R 1 and R 2 Each of the following is independently selected from at least one of hydroxyl, hydrogen, methyl, ethyl, n-octyl, and n-hexadecyl. It is understandable that when R... 1 and / or R 2 When the hydroxyl group is used, the PCL used is hydroxyl-terminated PCL (PCL-OH):
[0032]
[0033] In this invention, formic acid has strong acidity. Under high temperature conditions, PCL is degraded into PCL oligomers with different degrees of polymerization. At the same time, under the hydrolysis of formic acid, these PCL oligomers are catalytically dehydrated to obtain alkenyl-terminated PCL oligomers. The olefin-terminated PCL oligomers continue to depolymerize to generate 5-hexenoic acid and PCL oligomers with a chain length reduced by one repeating unit. This cycle can be repeated to gradually depolymerize into 5-hexenoic acid.
[0034] Then, the carbonyl rhodium complex catalyst generates a hydrogen rhodium carbonyl active species in situ under the action of a mixture of carbon monoxide and hydrogen. After the terminal carbon-carbon double bond of 5-hexenoic acid coordinates with the active rhodium center, it undergoes hydrogen metallization, preferentially generating a straight-chain alkyl-rhodium intermediate. Subsequently, carbon monoxide migrates and inserts between the rhodium-carbon bonds to obtain an acyl-rhodium intermediate. Water in the mixed solvent acts as a nucleophile to attack the carbonyl carbon of the acyl group, resulting in nucleophilic addition-proton dissociation. The acyl group hydrolyzes to generate a carboxylic acid, yielding pimelic acid with carboxyl groups at both ends. At the same time, the rhodium active center removes the organic fragment and regenerates the rhodium active species, returning to the catalytic cycle to achieve highly selective catalytic conversion to pimelic acid.
[0035] In the catalytic reaction, pimelic acid metal salt is the core promoter for the rhodium-catalyzed preparation of pimelic acid from 5-hexenoic acid. It stabilizes the active center by forming monodentate or intermolecular / bridging chelates with low-valent rhodium via the carboxylate group. This allows the carboxylate group to stabilize the low-valent rhodium active center while retaining rhodium coordination vacancies, thus enabling 5-hexenoic acid and the carbonyl group to participate normally in the catalytic cycle. Furthermore, the pimelic acid group can coordinate with rhodium through only one carboxylate group, while the other relatively free carboxylate group can be protonated, promoting the nucleophilic attack and hydrolysis of the acyl rhodium intermediate by water, assisting in the regeneration of the hydrogen rhodium active species. In addition, the addition of pimelic acid metal salt as a promoter does not introduce exogenous acid radicals, which is beneficial for improving product selectivity. By controlling product solubility through the salt effect and avoiding solid product encapsulation of catalyst sites, the reaction efficiency and target product yield are synergistically improved from multiple dimensions.
[0036] In summary, the preparation method of this application can convert PCL into pimelic acid in a one-step directional catalytic process, achieving highly selective preparation of pimelic acid, which is beneficial for the high-value recycling of PCL waste.
[0037] Optionally, the molar amount of the carbonyl rhodium complex is preferably 1% to 10% of the molar amount of the PCL repeating unit, and can be selected as any one of 1%, 3%, 5%, 7%, 9% or 10% or any range between two. Within this range, the carbonyl rhodium complex can provide sufficient rhodium active sites to drive the catalytic reaction to generate pimelic acid.
[0038] Optionally, the molar amount of pimelic acid metal salt is preferably 5% to 20% of the molar amount of the PCL repeating unit, and can be selected as any value or a range between 5%, 8%, 11%, 14%, 17% or 20%. Within this range, the pimelic acid metal salt can provide sufficient pimelic acid ligands to stabilize the low-valence rhodium active center in the system, maintain a suitable ionic strength to ensure the smooth progress of proton transfer and hydrolysis, and effectively control the dissolution state of the generated pimelic acid salt to avoid catalyst encapsulation.
[0039] It is understandable that the PCL repeating unit refers to the smallest structural segment that repeats continuously in its molecular chain, and the chemical structure of the repeating unit is -(CH2)5-COO-.
[0040] To promote the hydrolysis of PCL and provide dispersibility of intermediate and target products, the amount of mixed solvent added per gram of PCL is preferably 2 mL to 20 mL, and can be any value or a range between 5 mL, 10 mL, 15 mL or 20 mL; the volume ratio of formic acid to water in the mixed solvent is preferably 1:3 to 1:8, and can be any ratio of 1:3, 1:4, 1:5, 1:6, 1:7 or 1:8.
[0041] To remove air from the sealed reactor, the air inside the sealed reactor can be replaced three times with a mixed gas before the mixed gas is introduced into the sealed reactor. Preferably, the introduced mixed gas can make the pressure in the sealed reactor reach 4.5 MPa to 5.5 MPa, which can be any value among 4.5 MPa, 4.7 MPa, 4.9 MPa, 5.1 MPa, 5.3 MPa or 5.5 MPa or any range between two of them.
[0042] Optionally, the metal element in the pimelic acid metal salt may be selected from at least one of alkali metal elements, alkaline earth metal elements, or transition metal elements. For example, the pimelic acid metal salt may be selected from at least one of calcium pimelic acid, sodium pimelic acid, potassium pimelic acid, or zinc pimelic acid.
[0043] To improve catalytic reaction efficiency and product selectivity, the rhodium active center in the carbonyl rhodium complex is preferably in a low valence state and has a coordination unsaturated structure. Preferably, the carbonyl rhodium complex is selected from carbonyl rhodium complexes in which rhodium is monovalent and contains two carbonyl groups; for example, the carbonyl rhodium complex can be selected from at least one of dicarbonyl acetylacetone rhodium (Rh(acac)(CO)2) or tetracarbonyl dirhodium chloride.
[0044] To improve the efficiency of the catalytic reaction, the temperature of the catalytic reaction is preferably 120 ℃ to 160 ℃, and can be any value among 120 ℃, 130 ℃, 140 ℃, 150 ℃ or 160 ℃ or any range between two; the time of the catalytic reaction is preferably 9 h to 11 h, and can be any value among 9 h, 10 h or 11 h or any range between two.
[0045] Optionally, the separation and purification steps include: mixing the reaction solution obtained from the catalytic reaction with an alkaline aqueous solution, then extracting with an organic solvent and collecting the aqueous phase; then adjusting the pH to 2-4 to precipitate pimecrolic acid crystals; collecting the obtained solid through solid-liquid separation, washing and drying to obtain pimecrolic acid. The alkaline aqueous solution is preferably a 3%-10% sodium hydroxide aqueous solution, the organic solvent is preferably ethyl acetate, and the washing step uses ethanol.
[0046] To improve resource recycling, the PCL raw materials used in this invention are preferably PCL-containing waste products. These waste products have a wide range of sources, including PCL-containing packaging materials or medical materials, as well as PCL waste generated during PCL production. For waste products with low PCL content, pretreatment can be performed before use to increase the PCL content.
[0047] This invention does not impose any special limitation on the molecular weight of PCL. The number average molecular weight of PCL can be selected from 400 Da to 100,000 Da, for example, any value or a range between 500 Da, 5,000 Da, 10,000 Da, 50,000 Da or 80,000 Da.
[0048] The technical solution of the present invention will be further described below through specific embodiments. However, those skilled in the art will understand that the following embodiments are only for illustrating the present invention and should not be regarded as limiting the scope of the present invention. Unless otherwise specified, specific conditions in the embodiments are performed under conventional conditions or conditions recommended by the manufacturer. Reagents or instruments used without specified manufacturers are all commercially available conventional products.
[0049] In the following examples and comparative examples, PCL conversion rate refers to the mass percentage of the initial PCL input that has completely broken down its molecular chains and dissolved from the PCL bulk into the liquid phase after the reaction. This value only includes PCL degradation components that have completely separated from the solid phase, excluding undissolved PCL. Product selectivity refers to the mass fraction of each small molecule degradation product, such as pimelic acid, adipic acid, 6-hydroxyhexanoic acid, and ε-CL, among the soluble degradation products, relative to the total mass of all soluble degradation products.
[0050] The conversion rate detection method is as follows: After the reaction solution is cooled to room temperature, a non-soluble solvent of PCL (cold anhydrous ethanol / n-hexane) is added, and the system is repeatedly ultrasonically soaked and washed to ensure that all small molecule degradation products are completely eluted. The undegraded solid phase PCL is collected by filtration, dried under vacuum at 40°C to constant weight, and then weighed. The conversion rate is then calculated using the formula: Conversion rate = (total mass of initial PCL input - mass of residual PCL after drying) / total mass of initial PCL input × 100%.
[0051] The selective detection method is as follows: Take the reaction solution, wash the reaction solution and collect the washing liquid, take the washing liquid to make up the volume, add n-dodecane internal standard, and then add excess methanol and concentrated sulfuric acid to carry out methyl esterification derivatization reaction to ensure that pimelic acid, adipic acid, and 6-hydroxyhexanoic acid are completely converted into the corresponding methyl ester products (dimethyl pimelic acid, dimethyl adipic acid, and methyl 6-hydroxyhexanoate in sequence). ε-CL is stable under these conditions and does not undergo ring opening. Gas chromatography detection is performed, and the actual mass of each small molecule degradation product is obtained by converting it through the pre-established internal standard calibration curve. Combined with the total mass of soluble degradation products obtained by rotary evaporation and weighing, the mass fraction of each small molecule degradation product is calculated.
[0052] Example 1
[0053] Waste PCL film was mechanically crushed and then vacuum dried at 60 °C for 4 h to obtain PCL.
[0054] 2.0 g of PCL, calcium pimecronate auxiliary agent, and Rh(acac)(CO)2 catalyst were added to a 50 mL high-pressure reactor. The molar amount of calcium pimecronate was 10% of the molar amount of the PCL repeating unit, and the molar amount of Rh(acac)(CO)2 catalyst was 5% of the molar amount of the PCL repeating unit. Then, 20 mL of a 1:5 volume ratio mixture of formic acid and water was added. After sealing the reactor, a 1:1 volume ratio mixture of CO and H2 gas was introduced to replace the air in the reactor three times. The pressure was then adjusted to 5 MPa, and the temperature was raised to 150 °C and maintained at this temperature for 10 h.
[0055] After the reaction was completed, the mixture was cooled to room temperature and depressurized. The resulting reaction solution was pretreated and derivatized by methyl esterification. The selectivity of the PCL-catalyzed reaction to prepare pimelic acid was then detected by gas chromatography. Figure 1 As shown, the main product is pimelic acid, which corresponds to dimethyl pimelic acid derived by methyl esterification. Byproducts include adipic acid (corresponding to dimethyl adipic acid), 6-hydroxyhexanoic acid (corresponding to methyl 6-hydroxyhexanoate), and other unknown oligomers. The calculated mass fraction of pimelic acid in the reaction solution is 86%. The resulting reaction solution was poured into 100 mL of a 5% sodium hydroxide aqueous solution and stirred for 30 min. Extraction was performed three times with 30 mL of ethyl acetate each time, and the aqueous phase was collected. 1 mol / L dilute hydrochloric acid was added dropwise to the aqueous phase to adjust the pH to 3, and the solid precipitated. The solid was filtered, washed twice with anhydrous ethanol, and dried under vacuum at 50 ℃ for 6 h to obtain pimelic acid with a purity of 98.2%. The calculated yield of pimelic acid was 78% (pimelic acid yield = mass of pimelic acid produced after separation and purification / mass of PCL added × 100%).
[0056] Example 2
[0057] The only difference between Example 2 and Example 1 is that the calcium pimecronate adjuvant is replaced with sodium pimecronate adjuvant.
[0058] Example 3
[0059] The only difference between Example 3 and Example 1 is that the calcium pimeite adjuvant is replaced with potassium pimeite adjuvant.
[0060] Example 4
[0061] The only difference between Example 4 and Example 1 is that the calcium pimerate adjuvant is replaced with the zinc pimerate adjuvant.
[0062] Example 5
[0063] The only difference between Example 5 and Example 1 is that the temperature of the catalytic reaction is 120 °C.
[0064] Example 6
[0065] The only difference between Example 6 and Example 1 is that the temperature of the catalytic reaction is 160 °C.
[0066] Example 7
[0067] The only difference between Example 7 and Example 1 is that a mixed gas is introduced and the pressure is adjusted to 4.5 MPa.
[0068] Example 8
[0069] The only difference between Example 8 and Example 1 is that a mixed gas is introduced and the pressure is adjusted to 5.5 MPa.
[0070] Example 9
[0071] The only difference between Example 9 and Example 1 is that the isothermal reaction time is 9 hours.
[0072] Example 10
[0073] The only difference between Example 10 and Example 1 is that the isothermal reaction time is 11 h.
[0074] Example 11
[0075] The only difference between Example 11 and Example 1 is that PCL waste with a molecular weight of 5000 Da to 6000 Da obtained from the production of PCL is used.
[0076] 2.0 g of PCL waste, calcium pimecroate, and rhodium tetracarbonyl chloride catalyst were added to a 50 mL high-pressure reactor. The molar amount of calcium pimecroate was 15% of the molar amount of the PCL repeating unit, and the molar amount of rhodium tetracarbonyl chloride catalyst was 2% of the molar amount of the PCL repeating unit. Then, 20 mL of a formic acid and water mixture (volume ratio 1:7) was added. After sealing the reactor, a CO and H2 mixture (volume ratio 1:0.8) was introduced to purge the air from the reactor three times. The pressure was then adjusted to 5 MPa, and the temperature was raised to 150 °C. The reaction was maintained at this temperature for 10 h.
[0077] Comparative Example 1
[0078] The only difference between Comparative Example 1 and Example 1 is that Rh(acac)(CO)2 catalyst was not added.
[0079] Comparative Example 2
[0080] The only difference between Comparative Example 2 and Example 1 is that calcium pimeite was not added.
[0081] Comparative Example 3
[0082] The only difference between Comparative Example 3 and Example 1 is that calcium pimerate is replaced with calcium adipic acid.
[0083] Comparative Example 4
[0084] The only difference between Comparative Example 4 and Example 1 is that calcium pimedate is used instead of calcium stearate.
[0085] Comparative Example 5
[0086] The only difference between Comparative Example 5 and Example 1 is that the 20 mL formic acid and water mixture with a volume ratio of 1:5 was replaced with 20 mL of water.
[0087] Comparative Example 6
[0088] The only difference between Comparative Example 6 and Example 1 is that the 20 mL formic acid and water mixture with a volume ratio of 1:5 was replaced with 20 mL formic acid.
[0089] Comparative Example 7
[0090] The only difference between Comparative Example 7 and Example 1 is that no mixed gas of CO and H2 was introduced before the reaction.
[0091] Comparative Example 8
[0092] The only difference between Comparative Example 8 and Example 1 is that the Rh(acac)(CO)2 catalyst is replaced with RhI3.
[0093] The results of the PCL conversion rate and the selectivity of small molecule degradation products (pimelic acid, ε-CL, 6-hydroxyhexanoic acid, adipic acid) in the above examples and comparative examples are shown in Table 1.
[0094] Table 1
[0095]
[0096] Table 1 shows the following analysis: Examples 1-4 demonstrate that replacing calcium pimecronate with sodium pimecronate, potassium pimecronate, or zinc pimecronate, which can provide pimecronate ions, still yields a high PCL conversion rate and a high proportion of pimecronate, indicating that this selective regulation is not limited to specific metal cations. Examples 5-10 show that introducing a mixed gas to a pressure of 4.5 MPa-5.5 MPa, followed by a reaction at a temperature range of 120 ℃-160 ℃ and a time range of 9 h-11 h, all resulted in PCL conversion and the formation of pimecronate. The conditions of a pressure of 5 MPa, a reaction temperature of 150 ℃, and a reaction time of 10 h exhibited higher depolymerization of PCL and higher selectivity for pimecronate.
[0097] Comparative Example 1 shows that without the addition of Rh(acac)(CO)₂ catalyst, the PCL conversion rate is significantly reduced, and pimelic acid is not detected, indicating that the rhodium carbonyl complex plays an important role in promoting PCL conversion and the formation of the target product, pimelic acid. Comparative Example 2 shows that without the addition of a pimelic acid-containing promoter, PCL can still undergo a high degree of conversion, but pimelic acid is not detected, indicating that the pimelic acid-containing promoter has a significant selective regulatory effect on the formation of the target product, pimelic acid. Comparative Example 3 shows that replacing pimelic acid with adipic acid results in a worse PCL conversion rate, indicating that adipic acid has two fewer carbons in its molecular chain than pimelic acid, making it easier to form a stable chelate, poisoning the rhodium active center. Simultaneously, because both carboxyl groups are easily involved in coordination or fixed, the proton transport capacity decreases, and the selectivity and proton transport also deteriorate. Comparative Example 4 shows that although PCL still undergoes a high degree of conversion after replacing calcium pimecrolate with calcium stearate, pimecrolate was not detected. This indicates that the selective control effect of the present invention does not originate from the action of general calcium salts or general organic acid salts, but is closely related to the presence of pimecrolate ions. Comparative Examples 5 and 6 show that the overall PCL conversion rate is low when water or formic acid is used alone as the reaction medium. When water is used alone as the solvent, although the selectivity for pimecrolate is high, the overall yield of pimecrolate is limited due to the low PCL conversion rate. When formic acid is used alone as the solvent, both the PCL conversion rate and the selectivity for pimecrolate are low. Therefore, a combined solvent of water and formic acid is beneficial for balancing PCL conversion rate and pimecrolate formation. Comparative Example 7 shows that when a mixture of CO and H2 gas is not introduced, the PCL conversion rate is significantly reduced and pimecrolate is not detected, indicating that the mixture of CO and H2 gas plays an important role in the formation of the target product, pimecrolate. Comparative Example 8 shows that replacing the carbonyl rhodium complex catalyst with other rhodium-based catalysts reduces the selectivity for pimelic acid.
[0098] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0099] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A method for preparing pimelic acid using polycaprolactone, characterized in that, Includes the following steps: Polycaprolactone, heptahydrate metal salt, rhodium carbonyl complex, and mixed solvent are mixed and placed in a closed reactor, wherein the mixed solvent includes formic acid and water; A mixture of carbon monoxide and hydrogen gas is introduced into the closed reactor, and a catalytic reaction is carried out by heating. After the reaction is completed, the mixture is separated and purified to obtain pimelic acid.
2. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The molar amount of the pimelic acid metal salt is 5% to 20% of the molar amount of the polycaprolactone repeating unit; And / or, the molar amount of the rhodium carbonyl complex is 1% to 10% of the molar amount of the polycaprolactone repeating unit; And / or, in each gram of the polycaprolactone, the amount of the mixed solvent added is 2 mL to 20 mL; And / or, the mixed gas is introduced into the closed reactor until the pressure in the closed reactor reaches 4.5 MPa to 5.5 MPa.
3. The method for preparing pimelic acid using polycaprolactone according to claim 1 or claim 2, characterized in that, In the mixed solvent, the volume ratio of formic acid to water is 1:3 to 1:8; And / or, in the mixed gas, the volume ratio of carbon monoxide to hydrogen is 1:0.5 to 1:
2.
4. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The metal element in the pimelic acid metal salt is selected from at least one of alkali metal elements, alkaline earth metal elements, or transition metal elements. And / or, the carbonyl rhodium complex is selected from carbonyl rhodium complexes in which rhodium is monovalent and contains two carbonyl groups.
5. The method for preparing pimelic acid using polycaprolactone according to claim 4, characterized in that, The pimelic acid metal salt is selected from at least one of calcium pimelic acid, sodium pimelic acid, potassium pimelic acid, or zinc pimelic acid.
6. The method for preparing pimelic acid using polycaprolactone according to claim 4, characterized in that, The carbonyl rhodium complex is selected from at least one of dicarbonyl acetylacetone rhodium or tetracarbonyl dichloride.
7. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The catalytic reaction was carried out at a temperature of 120 ℃ to 160 ℃ for a time of 9 h to 11 h.
8. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The separation and purification steps include: mixing the reaction solution obtained from the catalytic reaction with an alkaline aqueous solution, then extracting it with an organic solvent and collecting the aqueous phase; then adjusting the pH to 2-4 to precipitate pimelic acid crystals; collecting the obtained solid through solid-liquid separation, washing and drying it to obtain pimelic acid.
9. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The polycaprolactone is selected from waste products containing polycaprolactone.
10. The method for preparing pimelic acid using polycaprolactone according to claim 1, characterized in that, The number-average molecular weight of the polycaprolactone is selected from 400 Da to 100,000 Da.