A low-temperature deposition apparatus and method for flip-chip soldering indium pillar arrays

By using low-temperature deposition equipment and methods, and utilizing localized electron beam heating and cryogenic module cooling, the thermal impact and oxidation problems in the deposition process of indium pillar arrays were solved, achieving the formation of indium pillar arrays with high precision and low contact resistance.

CN123108486APending Publication Date: 2026-11-17厦门韫茂原子级制造科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611578886.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-13
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies for indium pillar array deposition suffer from problems such as large heat-affected zones, complex processes, poor indium pillar positioning accuracy and coplanarity, and severe oxidation and impurity contamination.

Method used

The low-temperature deposition equipment includes a front-end transfer module, a buffer module, a central vacuum transfer module, a pretreatment module, and an evaporation module. It reduces thermal radiation and oxidation and improves positional accuracy and coplanarity by using electron beam local heating of the indium source, cryogenic module cooling of the wafer, ion beam cleaning, and collimated evaporation of particles.

Benefits of technology

A single continuous deposition of indium pillar arrays at low temperatures was achieved, reducing thermal impact and oxidation, improving the sidewall morphology and array coplanarity of the indium pillars, and lowering the contact resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108486A_ABST
    Figure CN123108486A_ABST
Patent Text Reader

Abstract

This invention provides a low-temperature deposition apparatus and method for flip-chip indium pillar arrays, relating to the field of packaging technology. The apparatus includes a front-end transfer module, a buffer module, a central vacuum transfer module, a pretreatment module, an evaporation module, and multiple vacuum isolation devices. The pretreatment module is equipped with an active temperature control module and an ion beam source device for pre-cooling, heating, and surface cleaning of the wafer. The evaporation module includes a cryogenic module, an electron beam evaporation device, and a collimated evaporation accessory, which locally heats the indium source using an electron beam and filters the movement direction of the evaporating indium particles. This invention can reduce wafer temperature rise during deposition, reduce indium pillar oxidation, contamination, and slippage, improve the sidewall morphology and array coplanarity of the indium pillars, and is suitable for high-density inter-chip interconnects in superconducting quantum chips.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of packaging technology, and more specifically, to a low-temperature deposition apparatus and method for flip-chip soldering indium pillar arrays. Background Technology

[0002] With the development of quantum computing technology, the number of qubits and the density of input / output electrodes in superconducting quantum chips are constantly increasing, placing higher demands on chip wiring density, interconnection distance, and packaging integration. Flip-chip packaging can vertically stack qubit chips and control chips through bump arrays, shortening the interconnection distance between chips to the micrometer level, which helps reduce parasitic parameters and signal transmission losses. Indium has the characteristics of low melting point, good ductility, high low-temperature plasticity, and good superconducting compatibility, so indium pillars or indium bumps can be used as the inter-chip interconnection structure in the flip-chip packaging of superconducting quantum chips.

[0003] To reduce the thermal impact during deposition, existing technologies typically employ a method of first fabricating an indium bump array on a sacrificial substrate and then transferring and bonding the indium bump array to the target chip. While this approach reduces the thermal impact of directly evaporating indium material on the target chip, it requires additional steps such as sacrificial substrate fabrication, bump transfer, alignment, and bonding, resulting in a more complex process flow and placing high demands on bump transfer yield and alignment accuracy.

[0004] Some methods involve repeatedly performing processes such as resist coating, exposure, indium layer deposition, resist removal, and mechanical compression to form or modify the height and morphology of indium pillars layer by layer. This type of method requires multiple transfers of the wafer between different equipment or processes, which can easily expose the indium pillar surface to the atmospheric environment, leading to oxidation or the introduction of impurities, increasing the contact resistance of the flip-chip interconnect structure. Simultaneously, repeated mechanical compression may cause lateral slippage of the indium pillars, reducing the positional accuracy and coplanarity of the indium pillar array, and increasing the consumption of photolithography materials, masks, and equipment time. Summary of the Invention

[0005] In view of this, the purpose of the present invention is to provide a low-temperature deposition apparatus and method for flip-chip soldering indium pillar arrays to solve the above problems.

[0006] The present invention adopts the following solution: This application provides a flip-chip indium pillar array low-temperature deposition apparatus, including a front-end transfer module, a buffer module, a central vacuum transfer module, a pretreatment module, an evaporation module, and at least two vacuum isolation devices; wherein, the low-temperature deposition range is between -90°C and 0°C; The buffer module is disposed between the front-end transmission module and the central vacuum transmission module; the pretreatment module and the evaporation module are distributed around the central vacuum transmission module and are connected to the central vacuum transmission module via a vacuum isolation device, respectively; the central vacuum transmission module includes a central vacuum transmission cavity and a vacuum manipulator disposed within the central vacuum transmission cavity. The preprocessing module includes a preprocessing cavity, a third wafer carrier mechanism disposed within the preprocessing cavity, an active temperature control module, and an ion beam source device. The active temperature control module is used to pre-cool or heat the wafer carried by the third wafer carrier mechanism, and the ion beam source device is used to pre-process the wafer surface. The active temperature control module is a bidirectional temperature control module based on the thermoelectric effect and is configured to cool or heat the wafer within a range of -20°C to 120°C. The ion beam source device is configured to form an angle of 0° to 30° between the ion beam and the wafer surface to remove the natural oxide layer, impurities, and photoresist edge residues on the wafer surface. The active temperature control module is also used to cool the wafer when the ion beam source device is operating, so that the wafer temperature is lower than the glass transition temperature of the photoresist on the wafer surface. The evaporation module includes an evaporation vacuum chamber, a fourth wafer support mechanism disposed within the evaporation vacuum chamber, a cryogenic module, an electron beam evaporation device, and a collimating evaporation accessory. The cryogenic module is configured to cool the wafer supported by the fourth wafer support mechanism within a temperature range of -120°C to 20°C. The electron beam evaporation device is used to generate indium evaporation particles by locally heating an indium source with an electron beam. The collimating evaporation accessory is disposed between the indium source and the wafer to filter the movement direction of the indium evaporation particles.

[0007] Furthermore, the front-end transfer module includes a rack, a microenvironment control system, a loading / unloading robot, a wafer calibration and positioning module, and at least one wafer rack; the rack is used to isolate the internal environment of the front-end transfer module from the external atmospheric environment; the microenvironment control system is disposed on the rack and includes a gas circulation system and a filtration system for controlling the gas composition, pressure, and cleanliness within the rack; the wafer calibration and positioning module is disposed above the opening of the wafer rack for identifying wafer information and calibrating the wafer position; the loading / unloading robot is movably disposed within the rack for transferring wafers between the wafer rack and the buffer module.

[0008] Furthermore, the buffer module includes an injection buffer chamber, an unloading buffer chamber, a first wafer carrier mechanism, a second wafer carrier mechanism, a buffer vacuum system, and a gas delivery system; the first wafer carrier mechanism and the second wafer carrier mechanism are respectively disposed in the injection buffer chamber and the unloading buffer chamber; the buffer vacuum system is used to evacuate the injection buffer chamber and the unloading buffer chamber respectively; the gas delivery system is used to deliver inert gas into the injection buffer chamber and the unloading buffer chamber to restore the injection buffer chamber and the unloading buffer chamber to atmospheric pressure.

[0009] Furthermore, both the first wafer carrier mechanism and the second wafer carrier mechanism include a base unit, at least three wafer support units, a synchronization guide unit, a drive unit, and a buffer limiting unit; the wafer support units are spaced circumferentially along the base unit and are movable between a support position extending beyond the upper surface of the base unit and a transfer position retracted below the upper surface of the base unit; the synchronization guide unit is connected to the wafer support units; the drive unit is used to drive the wafer support units to move synchronously up and down through the synchronization guide unit; the buffer limiting unit is used to buffer and limit the movement of the wafer support units and detect the position of the wafer support units.

[0010] Furthermore, the evaporation module also includes a second clamping assembly, a movable shutter baffle, a film thickness monitoring system, and a fourth vacuum system; the second clamping assembly is used to press the wafer against the cooling surface of the cryogenic module and can adjust the contact pressure between the wafer and the cooling surface; the movable shutter baffle is disposed between the electron beam evaporation device and the collimating evaporation accessory; the film thickness monitoring system is used to detect the evaporation rate of indium evaporation particles and the deposition thickness on the wafer surface, and controls the output power of the electron beam evaporation device according to the detection results; the fourth vacuum system is used to maintain the evaporation vacuum chamber at a certain temperature. Torr and lower ultra-high vacuum states.

[0011] Furthermore, the collimation evaporation accessory is provided with multiple through-channels, and the axial direction of each collimation channel is parallel to the normal direction of the wafer surface.

[0012] A method for low-temperature deposition of indium-indium-pole arrays using flip-chip soldering indium-indium-pole arrays, comprising the following steps: The wafer with the indium pillar array photoresist mask pattern is placed on the wafer rack, and the wafer is positioned and calibrated. The wafer after positioning and calibration is transferred to the buffer module, the buffer module is evacuated, and the wafer is transferred to the preprocessing module in a vacuum environment. The wafer is pre-cooled in the pre-processing module, and while the temperature of the wafer is controlled, the metal pads and photoresist patterns on the wafer surface are cleaned with an ion beam. The pre-cooled and cleaned wafers are transferred to the evaporation module in a vacuum environment, where the deep cryogenic module cools and keeps the wafers warm. The distance between the indium source and the wafer is adjusted, and the shutter baffle between the indium source and the wafer is kept closed. The indium source is pre-melted and degassed by local heating with an electron beam. The shutter baffle is opened so that the indium evaporation particles are filtered by the collimation evaporation accessory and deposited in the photoresist mask opening on the wafer surface, forming an indium pillar array through a single continuous deposition; After the indium pillar array reaches a predetermined height, heating of the indium source is stopped and the shutter baffle is closed. The wafer with the indium pillar array formed is transferred to the preprocessing module in a vacuum environment, where the wafer is heated in a controlled manner, then transferred to the buffer module that breaks the vacuum, and finally the wafer is output. The output wafer is stripped of its adhesive and the wafer with the indium pillar array is flip-chip bonded to the chip to be interconnected.

[0013] Furthermore, the vacuum degree of the buffer module is 5× Torr below; the vacuum degree of the preprocessing module is 5× Below Torr, the pre-cooling temperature of the wafer is -20°C to 0°C, and the ion energy of the ion beam is 100eV to 300eV; the vacuum degree of the evaporation module is 5× Below Torr, the wafer deposition temperature is -90°C to -70°C, and the wafer holding time at the deposition temperature is 30 min to 120 min; the distance between the indium source and the wafer is 200 mm to 600 mm, the output power of the electron beam evaporation device is 1 kW to 7 kW, the evaporation rate of the indium evaporation particles is 5 Å / s to 200 Å / s, and the height of the formed indium pillar is 5 μm to 20 μm.

[0014] Furthermore, the pre-melting and degassing includes at least two power stages: in the first power stage, the indium source is heated to the temperature at which indium evaporates and held for 3 to 5 minutes; in the second power stage, the output power of the electron beam evaporation device is increased to form a stable indium evaporation particle stream from the indium source; the thickness of the photoresist mask pattern is greater than the height of the indium pillar to be formed, and the opening of the photoresist mask pattern has a structure that is narrow at the top and wide at the bottom.

[0015] By adopting the above technical solution, the present invention can achieve the following technical effects: Using electron beam localized heating of the indium source reduces the heated area of ​​the evaporation source and the amount of heat radiation transferred from the evaporation source to the wafer compared to thermal evaporation methods that require heating the entire crucible. Continuous cooling of the wafer during indium pillar deposition via a cryogenic module effectively removes the heat generated by the condensation of evaporation particles, reducing wafer temperature rise and the impact of high temperatures on the Josephson junction and related dielectric interfaces.

[0016] By using an active temperature control module to cool the wafer during ion beam cleaning, the thermal load generated by ion beam bombardment can be offset, keeping the photoresist on the wafer surface below its glass transition temperature and reducing the risks of photoresist softening, flowing, carbonizing, and pattern deformation. After deposition, the active temperature control module can also controllably raise the temperature of the wafer, reducing the possibility of condensation caused by direct contact between the low-temperature wafer and the external environment, and reducing the stress caused by the difference in thermal expansion between the wafer, photoresist, and indium pillars.

[0017] By using a collimated evaporation attachment to filter the movement direction of indium evaporation particles, particles moving parallel or nearly parallel to the wafer surface normal can pass through. This reduces the deposition of tilted indium evaporation particles on the photoresist sidewalls and indium pillar sides, thereby improving the sidewall morphology of the indium pillars and reducing the possibility of mushroom-shaped structures forming at the top of the indium pillars and adhesion between adjacent indium pillars.

[0018] The buffer module, central vacuum transmission module, and vacuum isolation device enable the wafer to be transported in a vacuum environment between the pretreatment module and the evaporation module, reducing the number of times the wafer comes into contact with the external atmosphere during processing and reducing the risk of oxidation and impurity contamination on the indium pillar surface. Attached Figure Description

[0019] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained from these drawings without creative effort.

[0020] Figure 1 This is a schematic diagram of the structure of a flip-chip indium pillar array cryogenic deposition apparatus according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the front-end transmission module structure of a flip-chip soldering indium pillar array cryogenic deposition apparatus according to an embodiment of the present invention; Figure 3 This is a schematic diagram of the buffer module structure of a flip-chip soldering indium pillar array low-temperature deposition equipment according to an embodiment of the present invention; Figure 4 This is a schematic diagram of the central vacuum transmission module structure of a flip-chip indium pillar array cryogenic deposition apparatus according to an embodiment of the present invention; Figure 5 This is a schematic diagram of the pretreatment module structure of a flip-chip soldering indium pillar array low-temperature deposition equipment according to an embodiment of the present invention; Figure 6 This is a schematic diagram of the evaporation module structure of a flip-chip soldering indium pillar array low-temperature deposition equipment according to an embodiment of the present invention; Icons: Front-end transmission module 100; Buffer module 200; Pre-processing module 300; Evaporation module 400; Central vacuum transmission module 500; Vacuum isolation device 600; Microenvironment control system 101; Loading and unloading robot 102; Wafer calibration and positioning module 103; Rack 104; Slide rail system 105; Wafer rack 106; Reserved expansion interface 107; Wafer 108; Buffer cavity 201; Wafer carrying mechanism 202; First vacuum system 203; First gas delivery system 204; Wafer support unit 2021; Base unit 2022; Synchronous guiding unit 2023; Drive unit 2024; Buffer limiting unit 2025; Central vacuum transmission chamber 501; vacuum manipulator 502; second vacuum system 503; second gas delivery system 504; pretreatment chamber 301; third wafer carrier mechanism 302; active temperature control module 303; first clamping assembly 304; ion beam source device 305; third vacuum system 306; third gas delivery system 307; evaporation vacuum chamber 401; fourth wafer carrier mechanism 402; cryogenic module 403; second clamping assembly 404; electron beam evaporation device 405; film thickness monitoring system 406; movable shutter baffle 407; fourth vacuum system 408; collimating evaporation accessory 409; fourth gas delivery system 410. Detailed Implementation

[0021] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention. Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to represent selected embodiments of the invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0022] Example Combination Figures 1 to 6As shown, this embodiment of the invention provides a flip-chip soldering indium pillar array low-temperature deposition apparatus, including a front-end transmission module 100, a buffer module 200, a pretreatment module 300, an evaporation module 400, a central vacuum transmission module 500, and multiple vacuum isolation devices 600.

[0023] In this embodiment, the central vacuum transmission module 500 constitutes the vacuum transmission hub of the equipment. The buffer module 200, pretreatment module 300, and evaporation module 400 are distributed around the central vacuum transmission module 500 and are connected to the central vacuum transmission module 500 via vacuum isolation devices 600. The buffer module 200 is also connected to the front-end transmission module 100 to facilitate the transition of the wafer 108 between the external atmospheric pressure environment and the internal vacuum environment of the equipment.

[0024] Please refer to the following: Figure 2 and Figure 4 In this embodiment, the vacuum isolation device 600 can be an all-metal sealed gate valve or a rectangular slit transfer valve. When the wafer 108 does not need to be transferred between the two modules, the corresponding vacuum isolation device 600 remains closed, allowing each module to maintain its own vacuum level and process environment; when the wafer 108 needs to be transferred, the corresponding vacuum isolation device 600 opens to allow the vacuum robot 502 to pass through.

[0025] Combination Figure 2 As shown, the front-end transmission module 100 includes a micro-environment control system 101, a loading and unloading robot 102, a wafer calibration and positioning module 103, a rack 104, a slide rail system 105, at least one wafer rack 106, and a reserved expansion interface 107.

[0026] The rack 104 forms the main structure of the front-end transfer module 100, isolating its internal environment from the external environment. A microenvironment control system 101, mounted on the rack 104, includes a gas circulation system and a filtration system to control the gas composition, pressure, and cleanliness within the rack 104, reducing particulate contamination during wafer 108 loading and unloading. A wafer rack 106 accommodates multiple wafers 108. A wafer calibration and positioning module 103, located above the opening of the wafer rack 106, includes a positioning module and an optical module. The optical module can employ a charge-coupled device image sensor or other optical detection devices to acquire information such as the center, flat edge, notch, and wafer number of the wafer 108. Based on the positional deviation detected by the optical module, the positioning module controls the loading / unloading robot 102 or a corresponding positioning mechanism to adjust the position and angle of the wafer 108.

[0027] The loading / unloading robot 102 is movably mounted within the frame 104 and can move along the slide rail system 105. The loading / unloading robot 102 may be a multi-jointed robotic arm with a vacuum adsorption structure or electrostatic adsorption structure at its end for loading, unloading, and transferring wafers 108 between the wafer rack 106 and the buffer module 200. The reserved expansion interface 107 may include at least one of a mechanical interface, an electrical interface, a gas interface, and a communication interface for connecting to lithography equipment, etching equipment, cleaning equipment, flip-chip bonding equipment, or other wafer processing equipment.

[0028] Combination Figure 3 As shown, the buffer module 200 includes an injection buffer chamber, an unloading buffer chamber, a first wafer carrier mechanism, a second wafer carrier mechanism, a first vacuum system 203, and a first gas delivery system 204. The injection buffer chamber and the unloading buffer chamber can be mirrored and operate independently.

[0029] The first wafer carrier mechanism and the second wafer carrier mechanism are respectively disposed in the sample loading buffer cavity and the sample unloading buffer cavity, and both can adopt the structure shown in wafer carrier mechanism 202. Wafer carrier mechanism 202 includes at least three wafer support units 2021, a base unit 2022, a synchronization guide unit 2023, a drive unit 2024, and a buffer limiting unit 2025. The base unit 2022 is disposed at the bottom of the corresponding buffer cavity. The at least three wafer support units 2021 are spaced apart circumferentially along the base unit 2022. The wafer support unit 2021 can be a support pin capable of rising and falling relative to the base unit 2022. When the wafer support unit 2021 is in the support position, its upper end extends beyond the upper surface of the base unit 2022 to support the wafer 108; when the wafer support unit 2021 is in the transfer position, its upper end retracts below the upper surface of the base unit 2022 to avoid obstruction of the loading / unloading robot 102 or the vacuum robot 502.

[0030] The synchronization guide unit 2023 is connected to each wafer support unit 2021, and is used to limit the movement of each wafer support unit 2021 along the normal direction of the base unit 2022, and to synchronize the lifting and lowering of each wafer support unit 2021. The drive unit 2024 is connected to the synchronization guide unit 2023, and can be a servo motor and a lead screw drive mechanism. When the drive unit 2024 is located outside the buffer cavity, it can transmit driving force into the buffer cavity through a metal bellows or other vacuum-sealed structure.

[0031] The buffer limiting unit 2025 includes an elastic damping buffer and a position detection sensor. The elastic damping buffer is used to absorb impact when the wafer support unit 2021 reaches the support position or transfer position, and the position detection sensor is used to detect the position of the wafer support unit 2021 and send the detection result to the equipment control system.

[0032] The first vacuum system 203 is used to evacuate the buffer chamber 201, which includes a sample inlet buffer chamber and a sample outlet buffer chamber, so that the vacuum level of the buffer chamber 201 matches the vacuum level of the central vacuum transmission chamber 501. The first gas delivery system 204 is used to deliver high-purity nitrogen, argon or other inert gases to the sample inlet buffer chamber and the sample outlet buffer chamber, so that the corresponding buffer chambers are restored to normal pressure.

[0033] Combination Figure 4 As shown, the central vacuum transmission module 500 includes a central vacuum transmission cavity 501, a vacuum manipulator 502, a second vacuum system 503, and a second gas delivery system 504.

[0034] The central vacuum transmission chamber 501 is a vacuum-sealed chamber. The second vacuum system 503 is connected to the central vacuum transmission chamber 501 and is used to extract and maintain the vacuum inside the central vacuum transmission chamber 501. The second gas delivery system 504 is used to deliver inert gas into the central vacuum transmission chamber 501 during equipment maintenance or when the central vacuum transmission chamber 501 is opened.

[0035] A vacuum manipulator 502 is disposed within a central vacuum transfer chamber 501 and is used to transfer wafers 108 between the buffer module 200, the preprocessing module 300, and the evaporation module 400. The vacuum manipulator 502 includes a base assembly, a multi-jointed robotic arm, and an end effector. The base assembly can be fixed to the bottom of the central vacuum transfer chamber 501, and the drive device can be disposed outside the chamber, driving the robotic arm movement through a magnetohydrodynamic sealing structure or other vacuum dynamic sealing structure. The end effector can employ a vacuum adsorption structure, an edge clamping structure, or a ceramic support structure.

[0036] Combination Figure 5 As shown, the preprocessing module 300 includes a preprocessing cavity 301, a third wafer carrier 302, an ion beam source device 305, a third vacuum system 306, and a third gas delivery system 307.

[0037] The third wafer carrier mechanism 302 is disposed within the preprocessing cavity 301 and is used to carry the wafer 108. It includes an active temperature control module 303 and a first clamping assembly 304. The active temperature control module 303 is capable of cooling or heating the wafer 108 within a temperature range of -20°C to 120°C. The active temperature control module 303 may employ a bidirectional temperature control component based on the thermoelectric effect and be connected to a water-cooling circulation system.

[0038] The first clamping assembly 304 is used to press the wafer 108 onto the temperature control surface of the active temperature control module 303. The first clamping assembly 304 includes at least a drive source and a transmission clamping mechanism, and is disposed opposite to the active temperature control module 303. The drive source can be a servo motor or a cylinder, and the transmission clamping mechanism is connected between the power output end of the drive source and the wafer 108. This mechanism also includes a pressure ring or pressure plate, the upper surface contour of which is adapted to the edge contour of the wafer 108 to ensure uniform pressure distribution. To prevent the wafer 108 from shifting or experiencing uneven force during clamping, a guide assembly is also provided in the transmission clamping mechanism to ensure that the pressure ring only moves in a direction perpendicular to the temperature control surface of the active temperature control module 303. When this mechanism is in the released state, it avoids the vacuum manipulator 502 from grasping and placing the wafer 108.

[0039] An ion beam source device 305 is used to clean the surface of wafer 108 before indium pillar deposition. The ion beam source device 305 can be located at the bottom or side of the pretreatment chamber 301, and the ion beam forms an angle of 0° to 30° with the surface of wafer 108, preferably 20°. Ion beam bombardment removes the natural oxide layer, organic impurities, inorganic impurities, and photoresist edge residues from the surface of the metal pads. During operation, the ion beam source device 305 inputs heat to wafer 108, and the active temperature control module 303 simultaneously cools wafer 108, keeping its temperature below the glass transition temperature of the photoresist to reduce photoresist softening, flow, carbonization, or pattern collapse.

[0040] After the indium pillar deposition is completed, the wafer 108 can return to the preprocessing module 300. At this time, the active temperature control module 303 controls the temperature of the wafer 108 to gradually rise from the deposition temperature to room temperature or close to room temperature, reducing the occurrence of condensation when the low-temperature wafer 108 comes into contact with the external environment, and gradually releasing the thermal stress between the indium pillar, photoresist and wafer 108.

[0041] The third vacuum system 306 is used to control the vacuum level of the pretreatment chamber 301. The third gas delivery system 307 can deliver working gases such as argon, oxygen, hydrogen or nitrogen to the ion beam source device 305, and can also deliver inert gases into the pretreatment chamber 301 during equipment maintenance.

[0042] Combination Figure 6 As shown, the evaporation module 400 includes an evaporation vacuum chamber 401, a fourth wafer support mechanism 402, a cryogenic module 403, a second clamping assembly 404, an electron beam evaporation device 405, a film thickness monitoring system 406, a movable shutter baffle 407, a fourth vacuum system 408, a collimation evaporation accessory 409, and a fourth gas delivery system 410.

[0043] A fourth wafer support mechanism 402 is disposed within the evaporation vacuum chamber 401 and is used to support the wafer 108. A cryogenic module 403 is integrated with the fourth wafer support mechanism 402 and is used to cool the wafer 108 during indium pillar deposition. The cryogenic module 403 may include a metal cold plate with cooling channels connected to an external circulating refrigeration system. The circulating refrigeration medium may be a fluorinated liquid, liquid nitrogen, or other media capable of providing a low-temperature environment. A second clamping assembly 404 is used to press the wafer 108 against the cooling surface of the cryogenic module 403 and can adjust the contact pressure between the wafer 108 and the cooling surface. By adjusting the contact pressure, the contact thermal resistance can be reduced, the cooling efficiency of the cryogenic module 403 on the wafer 108 can be improved, and displacement of the wafer 108 during the low-temperature deposition process can be prevented. The structure of the second clamping assembly 404 is the same as that of the first clamping assembly 304, and will not be described in detail here.

[0044] The electron beam evaporation apparatus 405 includes an electron gun, an indium source support crucible, and a cooling system. The electron beam emitted by the electron gun is focused on a localized area of ​​the indium source, causing localized heating of the indium source and generating indium evaporation particles. Compared to heating the entire crucible, localized heating reduces the area of ​​the high-temperature region and decreases the thermal radiation from the indium source to the wafer 108. A collimating evaporation attachment 409 is disposed between the indium source and the wafer 108. The collimating evaporation attachment 409 has multiple through-hole collimating channels, the axis of each collimating channel being parallel to the normal direction of the wafer 108 surface. Each collimating channel can have a predetermined length and aperture ratio, allowing indium evaporation particles moving parallel or nearly parallel to the collimating channel axis to pass through, and blocking indium evaporation particles moving deviating from the collimating channel axis. After being screened by the collimating evaporation attachment 409, the indium evaporation particles reaching the wafer 108 surface are incident primarily along the normal direction of the wafer 108 surface, which reduces the deposition of indium evaporation particles on the sidewalls of the photoresist openings and the sides of the indium pillars, thereby forming indium pillars with larger sidewall angles.

[0045] A movable shutter baffle 407 is positioned between the electron beam evaporation apparatus 405 and the collimating evaporation accessory 409. During the pre-melting and degassing of the indium source, the movable shutter baffle 407 is closed to prevent impurities, oxides, and unstable evaporation particles on the surface of the indium source from reaching the wafer 108. After the indium source forms a stable indium evaporation particle flow, the movable shutter baffle 407 opens, and formal deposition begins.

[0046] The film thickness monitoring system 406 includes a quartz crystal oscillation sensor and a film thickness monitor, used to detect the evaporation rate of indium evaporation particles and the deposition thickness on the surface of wafer 108 in real time. The film thickness monitoring system 406 is communicatively connected to the electron beam evaporation apparatus 405 and adjusts the output power of the electron beam evaporation apparatus 405 according to the detection results to keep the indium evaporation rate within a predetermined range. When the deposition thickness reaches the predetermined indium pillar height, the film thickness monitoring system 406 controls the electron beam evaporation apparatus 405 to stop outputting power and controls the movable shutter baffle 407 to close.

[0047] The fourth vacuum system 408 is used to maintain the evaporation vacuum chamber 401 in an ultra-high vacuum state. The fourth gas delivery system 410 is used to deliver high-purity nitrogen or argon gas into the evaporation vacuum chamber 401 during equipment maintenance or when the chamber is opened.

[0048] The pretreatment module 300 and the evaporation module 400 can operate independently. The evaporation module 400 can also be configured in two or more configurations, allowing different wafers 108 to be deposited simultaneously in different evaporation modules 400, thereby improving equipment utilization and wafer processing efficiency.

[0049] Example 2 This embodiment provides a method for low-temperature deposition of flip-chip solder indium pillar arrays using the equipment described in Embodiment 1, specifically including the following steps.

[0050] Step S1: Place the wafer 108 with the indium pillar array photoresist mask pattern into the wafer rack 106.

[0051] Wafer 108 can be a superconducting quantum bit chip wafer that has completed Josephson junction patterning and metal pad fabrication and is ready for flip-chip packaging. Wafer 108 can have a diameter of 300 mm. An adhesion layer and a wetting layer can be pre-formed on the surface of the metal pads. The thickness of the photoresist mask pattern is greater than the height of the indium pillars to be formed, and the opening of the photoresist mask pattern can have a structure that is narrower at the top and wider at the bottom to facilitate subsequent resist removal.

[0052] In step S2, the wafer calibration and positioning module 103 acquires the center, notch, flat edge, or wafer number of the wafer 108, and calibrates the position and angle of the wafer 108. The loading and unloading robot 102 transfers the calibrated wafer 108 to the sample loading buffer cavity according to the wafer number sequence or a specified number.

[0053] The cavity door between the sample injection buffer chamber and the front-end transfer module 100 is closed, and the sample injection buffer chamber is evacuated through the first vacuum system 203 to achieve a vacuum level of 5×10⁻⁶. -8 Torr below. Open the vacuum isolation device 600 between the sample injection buffer chamber and the central vacuum transmission chamber 501, and the vacuum robot 502 takes out the wafer 108.

[0054] In step S3, the vacuum robot 502 transfers the wafer 108 to the preprocessing module 300. The vacuum isolation device 600 between the preprocessing module 300 and the central vacuum transfer chamber 501 is shut off, and the vacuum level of the preprocessing chamber 301 is controlled at 5 × 10⁻⁶ via the third vacuum system 306. -9 Torr below.

[0055] The first clamping assembly 304 presses the wafer 108 against the temperature control surface of the active temperature control module 303. The active temperature control module 303 pre-cools the wafer 108 to -20°C to 0°C. While maintaining the temperature of the wafer 108, the ion beam source device 305 emits an ion beam onto the surface of the wafer 108. The ion energy of the ion beam is 100 eV to 300 eV, and the angle between the ion beam and the surface of the wafer 108 is 0° to 30°.

[0056] An ion beam cleans the metal pads, photoresist patterns, and photoresist opening sidewalls on the surface of wafer 108 to remove the native oxide layer, impurities, and photoresist edge residue. An active temperature control module 303 continuously cools wafer 108 during the cleaning process, keeping its temperature below the glass transition temperature of the photoresist.

[0057] In step S4, after cleaning, the vacuum robot 502 transfers the wafer 108 from the pretreatment module 300 to the evaporation module 400. The second clamping assembly 404 presses the wafer 108 against the cooling surface of the cryogenic module 403.

[0058] The fourth vacuum system 408 controls the vacuum level of the evaporation vacuum chamber 401 to 5× Below Torr. The cryogenic module 403 cools the wafer 108 to -90°C to -70°C and holds it within this temperature range for 30 min to 120 min to make the overall temperature of the wafer 108 tend to be uniform.

[0059] Step S5: Adjust the distance between the indium source and the wafer 108 to 200mm to 600mm.

[0060] In step S6, keeping the movable shutter baffle 407 closed, the indium source is locally heated by the electron beam evaporation device 405 to pre-melt and degas the indium source. The output power of the electron beam evaporation device 405 can be adjusted within the range of 1kW to 7kW.

[0061] The pre-melting degassing process includes at least two power stages. In the first power stage, the output power is gradually increased to heat the indium source to the starting temperature range of indium evaporation and hold for 3 to 5 minutes to remove adsorbed gases, oxides, and impurities from the surface of the indium source. In the second power stage, the output power of the electron beam evaporation device 405 is further increased to form a stable indium evaporation particle stream from the indium source.

[0062] In step S7, after the indium evaporation particle stream stabilizes, the movable shutter baffle 407 is opened. After being screened by the collimation channel of the collimation evaporation accessory 409, the indium evaporation particles are incident on the wafer 108 along a direction parallel or nearly parallel to the surface normal of the wafer 108 and deposited in the opening of the photoresist mask pattern.

[0063] The film thickness monitoring system 406 monitors the evaporation rate and deposition thickness of the indium evaporation particles in real time. The evaporation rate of the indium evaporation particles is controlled between 5 Å / s and 200 Å / s. An array of indium pillars is formed on the surface of wafer 108 through a single continuous deposition.

[0064] The cryogenic module 403 continuously cools the wafer 108 during the deposition process to remove the heat released by the condensation of indium evaporated particles and reduce the diffusion of indium atoms on the surface of the wafer 108 and the photoresist surface, so that the formed indium pillars have a refined grain structure.

[0065] In step S8, when the film thickness monitoring system 406 detects that the indium pillar height reaches 5μm to 20μm, it stops the power output of the electron beam evaporation device 405 and closes the movable shutter baffle 407.

[0066] Under the above deposition conditions, the temperature rise of wafer 108 during the deposition of indium pillar array can be less than 3°C, the sidewall angle of the formed indium pillars can be greater than 85°, and the average grain size of the indium pillars can be less than 300nm.

[0067] In step S9, the vacuum robot 502 transfers the wafer 108 with the indium pillar array formed from the evaporation module 400 to the preprocessing module 300. The active temperature control module 303 controls the temperature of the wafer 108 to gradually increase it to 15°C to 35°C, preferably to 25°C.

[0068] After the wafer 108 has been heated, the vacuum robot 502 transfers it to the unloading buffer chamber. The vacuum isolation device 600 between the unloading buffer chamber and the central vacuum transfer chamber 501 is closed, and inert gas is supplied to the unloading buffer chamber via the first gas delivery system 204, restoring the unloading buffer chamber to atmospheric pressure. The loading / unloading robot 102 removes the wafer 108 from the unloading buffer chamber and transfers it to the wafer rack 106.

[0069] In step S10, the output wafer 108 is stripped of the photoresist mask to remove the photoresist mask pattern and the indium material deposited on the photoresist surface, retaining the indium pillar array formed within the photoresist openings. Subsequently, the wafer 108 with the indium pillar array is flip-chip bonded to the chip to be interconnected using a low-temperature ultrasonic bonding process.

[0070] Because the indium pillars form a fine-grained structure and maintain good plasticity during the low-temperature deposition process, they can undergo controlled plastic deformation during the subsequent low-temperature ultrasonic bonding process, so that a stable connection can be formed between the oppositely arranged indium pillars or metal pads, thereby reducing the contact resistance of the inter-chip interconnect.

[0071] This embodiment combines electron beam local heating of the indium source, wafer deep cooling, evaporation particle collimation, ultra-high vacuum transport, and controlled heating after deposition to enable the wafer 108 to complete a single continuous deposition of the indium pillar array at a lower temperature. This reduces indium pillar slippage, oxidation, and impurity contamination caused by multiple depositions and mechanical compression, and improves the sidewall morphology and array coplanarity of the indium pillars.

[0072] The above are merely preferred embodiments of the present invention. The scope of protection of the present invention is not limited to the above embodiments. All technical solutions that fall within the scope of the present invention are within the scope of protection of the present invention.

Claims

1. A low-temperature deposition apparatus for flip-chip soldering indium pillar arrays, characterized in that, It includes a front-end transmission module, a buffer module, a central vacuum transmission module, a pretreatment module, an evaporation module, and at least two vacuum isolation devices; wherein, the low temperature range of the low-temperature deposition is between -90°C and 0°C; The buffer module is disposed between the front-end transmission module and the central vacuum transmission module; the pretreatment module and the evaporation module are distributed around the central vacuum transmission module, and the pretreatment module, the evaporation module and the buffer module are respectively connected to the central vacuum transmission module through the vacuum isolation device; the central vacuum transmission module includes a central vacuum transmission cavity and a vacuum manipulator disposed in the central vacuum transmission cavity; The preprocessing module includes a preprocessing cavity, a third wafer carrier mechanism disposed within the preprocessing cavity, an active temperature control module, and an ion beam source device. The active temperature control module is used to pre-cool or heat the wafer carried by the third wafer carrier mechanism, and the ion beam source device is used to pre-process the wafer surface. The active temperature control module is a bidirectional temperature control module based on the thermoelectric effect and is configured to cool or heat the wafer within a range of -20°C to 120°C. The ion beam source device is configured to form an angle of 0° to 30° between the ion beam and the wafer surface to remove the natural oxide layer, impurities, and photoresist edge residues on the wafer surface. The active temperature control module is also used to cool the wafer when the ion beam source device is operating, so that the wafer temperature is lower than the glass transition temperature of the photoresist on the wafer surface. The evaporation module includes an evaporation vacuum chamber, a fourth wafer support mechanism disposed within the evaporation vacuum chamber, a cryogenic module, an electron beam evaporation device, and a collimating evaporation accessory. The cryogenic module is configured to cool the wafer supported by the fourth wafer support mechanism within a temperature range of -120°C to 20°C. The electron beam evaporation device is used to generate indium evaporation particles by locally heating an indium source with an electron beam. The collimating evaporation accessory is disposed between the indium source and the wafer to filter the movement direction of the indium evaporation particles.

2. The flip-chip indium pillar array cryogenic deposition apparatus according to claim 1, characterized in that, The front-end transfer module includes a rack, a microenvironment control system, a loading / unloading robot, a wafer calibration and positioning module, and at least one wafer rack. The rack isolates the internal environment of the front-end transfer module from the external atmospheric environment. The microenvironment control system is mounted on the rack and includes a gas circulation system and a filtration system to control the gas composition, pressure, and cleanliness within the rack. The wafer calibration and positioning module is located above the opening of the wafer rack and is used to identify wafer information and calibrate the wafer position. The loading / unloading robot is movably mounted within the rack and is used to transfer wafers between the wafer rack and the buffer module.

3. The flip-chip indium pillar array cryogenic deposition apparatus according to claim 1, characterized in that, The buffer module includes an injection buffer chamber, an unloading buffer chamber, a first wafer carrier mechanism, a second wafer carrier mechanism, a buffer vacuum system, and a gas delivery system. The first wafer carrier mechanism and the second wafer carrier mechanism are respectively disposed in the injection buffer chamber and the unloading buffer chamber. The buffer vacuum system is used to evacuate the injection buffer chamber and the unloading buffer chamber respectively. The gas delivery system is used to deliver inert gas into the injection buffer chamber and the unloading buffer chamber to restore the injection buffer chamber and the unloading buffer chamber to atmospheric pressure.

4. The flip-chip indium pillar array cryogenic deposition apparatus according to claim 3, characterized in that, Both the first wafer carrier mechanism and the second wafer carrier mechanism include a base unit, at least three wafer support units, a synchronization guide unit, a drive unit, and a buffer limiting unit. The wafer support units are spaced circumferentially along the base unit and can move between a support position extending beyond the upper surface of the base unit and a transfer position retracted below the upper surface of the base unit. The synchronization guide unit is connected to the wafer support units. The drive unit is used to drive the wafer support units to move synchronously up and down through the synchronization guide unit. The buffer limiting unit is used to buffer and limit the movement of the wafer support units and detect the position of the wafer support units.

5. The flip-chip indium pillar array cryogenic deposition apparatus according to claim 1, characterized in that, The evaporation module further includes a second clamping assembly, a movable shutter baffle, a film thickness monitoring system, and a fourth vacuum system. The second clamping assembly is used to press the wafer against the cooling surface of the cryogenic module and can adjust the contact pressure between the wafer and the cooling surface. The movable shutter baffle is disposed between the electron beam evaporation device and the collimating evaporation accessory. The film thickness monitoring system is used to detect the evaporation rate of indium evaporation particles and the deposition thickness on the wafer surface, and controls the output power of the electron beam evaporation device based on the detection results. The fourth vacuum system is used to maintain the evaporation vacuum chamber at a certain vacuum level. Ultra-high vacuum states of Torr and below.

6. The flip-chip indium pillar array cryogenic deposition apparatus according to claim 5, characterized in that, The collimation evaporation accessory is provided with multiple through-channels, and the axial direction of each collimation channel is parallel to the normal direction of the wafer surface.

7. A low-temperature deposition method for flip-chip soldering indium pillar arrays, characterized in that, The method employing the flip-chip indium pillar array cryogenic deposition apparatus as described in any one of claims 1 to 6 includes the following steps: The wafer with the indium pillar array photoresist mask pattern is placed on the wafer rack, and the wafer is positioned and calibrated. The wafer after positioning and calibration is transferred to the buffer module, the buffer module is evacuated, and the wafer is transferred to the preprocessing module in a vacuum environment. The wafer is pre-cooled in the pre-processing module, and while the temperature of the wafer is controlled, the metal pads and photoresist patterns on the wafer surface are cleaned with an ion beam. The pre-cooled and cleaned wafers are transferred to the evaporation module in a vacuum environment, where the deep cryogenic module cools and keeps the wafers warm. The distance between the indium source and the wafer is adjusted, and the shutter baffle between the indium source and the wafer is kept closed. The indium source is pre-melted and degassed by local heating with an electron beam. The shutter baffle is opened, allowing indium evaporation particles to be deposited in the photoresist mask opening on the wafer surface after being screened by the collimating evaporation accessory. An indium pillar array is formed through a single continuous deposition. After the indium pillar array reaches a predetermined height, heating of the indium source is stopped and the shutter baffle is closed. The wafer with the indium pillar array formed is transferred to the preprocessing module in a vacuum environment, where the wafer is heated in a controlled manner, then transferred to the buffer module that breaks the vacuum, and finally the wafer is output. The output wafer is stripped of its adhesive and the wafer with the indium pillar array is flip-chip bonded to the chip to be interconnected.

8. The low-temperature deposition method for flip-chip soldering indium pillar arrays according to claim 7, characterized in that, The vacuum level of the buffer module is 5× Torr below; the vacuum degree of the preprocessing module is 5× Below Torr, the pre-cooling temperature of the wafer is -20°C to 0°C, and the ion energy of the ion beam is 100eV to 300eV; the vacuum degree of the evaporation module is 5× Below Torr, the wafer deposition temperature is -90°C to -70°C, and the wafer holding time at the deposition temperature is 30 min to 120 min; the distance between the indium source and the wafer is 200 mm to 600 mm, the output power of the electron beam evaporation device is 1 kW to 7 kW, the evaporation rate of the indium evaporation particles is 5 Å / s to 200 Å / s, and the height of the formed indium pillar array is 5 μm to 20 μm.

9. The low-temperature deposition method for flip-chip soldering indium pillar arrays according to claim 7, characterized in that, The pre-melting and degassing process includes at least two power stages: in the first power stage, the indium source is heated to the temperature at which indium evaporates and held for 3 to 5 minutes; in the second power stage, the output power of the electron beam evaporation device is increased to form a stable indium evaporation particle stream from the indium source; the thickness of the photoresist mask pattern is greater than the height of the indium pillar array to be formed, and the opening of the photoresist mask pattern has a structure that is narrow at the top and wide at the bottom.