A high-bonding-strength, fatigue-resistant hard coating structure for the flexible wheel of a harmonic reducer
By adopting a multi-layer gradient coating structure on the flexible wheel of the harmonic reducer, the problems of weak coating adhesion and poor fatigue resistance are solved, achieving high adhesion, wear resistance and deformation adaptability, extending the service life of the flexible wheel and improving transmission accuracy.
Patent Information
- Application Number
- CN202611298869.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
The coating structure of the flexible wheel in existing harmonic reducers has weak adhesion, is easy to peel off, is brittle, and has poor fatigue resistance. It cannot adapt to high-frequency alternating deformation working conditions, resulting in short service life and hindering the localization process.
A multi-layer gradient composite coating structure is adopted, consisting of a substrate roughening modification layer, a nano-transition buffer layer, a dense hard support layer, and a wear-resistant and fatigue-resistant top layer. Through micro-anchoring interface, mechanical gradient transition, and local coating design, the bonding strength is improved, stress is relieved, and fatigue resistance is enhanced.
It significantly improves the bonding strength between the coating and the substrate, extends the fatigue life of the flexible wheel by 50%, ensures transmission accuracy and stability, adapts to high-frequency deformation conditions of the flexible wheel, and meets the long-term use requirements of high-end equipment.
Abstract
Description
Technical Field
[0001] This invention relates to the field of surface strengthening coating technology for core components of harmonic reducers, specifically a high-bonding-strength, fatigue-resistant hard coating structure for the flexible wheel of a harmonic reducer. Background Technology
[0002] Harmonic reducers, with their advantages of small size, large transmission ratio, high precision, and small backlash, are widely used in high-end equipment fields such as industrial robots, humanoid joints, aerospace precision equipment, and precision machine tools. The flexible gear, as a core vulnerable component of the harmonic reducer, continuously endures high-frequency periodic radial bending deformation, tooth meshing extrusion stress, and micro-slip friction during operation. Under complex alternating load conditions for extended periods, it is highly susceptible to surface wear, micro-crack initiation, fatigue spalling, and even overall fracture failure, directly determining the transmission accuracy and overall service life of the harmonic reducer.
[0003] Currently, the industry commonly uses single hard coatings or simple double-layer coatings to strengthen the surface of flexible gears. Commonly used coatings include TiN, AlTiN, and DLC hard coatings. Although these can improve surface wear resistance to a certain extent, they have significant technical defects: First, single hard coatings are brittle and have large differences in mechanical properties with the flexible gear alloy substrate, resulting in weak interfacial bonding. During the high-frequency elastic deformation of the flexible gear, stress concentration easily occurs at the interface between the coating and the substrate, causing the coating to peel, crack, and flake off. This not only fails to provide protection but also exacerbates gear wear by detaching particles, leading to a decrease in reducer accuracy. Second, without a gradient buffer structure, the overall stress adaptability of the coating is poor, failing to adapt to the periodic deformation characteristics of the flexible gear. Under alternating loads, microcracks propagate rapidly, resulting in poor fatigue resistance and limited improvement in the fatigue life of the flexible gear. Third, the coating structure design is not targeted enough. Overall coating can easily lead to a decrease in the toughness of the flexible gear and stress concentration, while local coating lacks a layered protective structure, making it impossible to simultaneously achieve wear resistance and fatigue resistance.
[0004] Current technologies lack specialized coating structures for the high-frequency alternating deformation conditions of flexure wheels, failing to simultaneously meet the multiple requirements of high adhesion, high wear resistance, high fatigue resistance, and deformation adaptability. This results in the service life of flexure wheels in domestically produced harmonic reducers being significantly shorter than that of imported products, hindering the domestic substitution process for high-end harmonic reducers. Therefore, developing a gradient composite hard coating structure that adapts to the special operating conditions of flexure wheels, exhibits high adhesion, fatigue resistance, and excellent deformation adaptability is a key technological breakthrough for addressing the current shortcomings in the service life of harmonic reducers. Summary of the Invention
[0005] This invention provides a high-bonding, fatigue-resistant hard coating structure for the flexible wheel of a harmonic reducer, which solves the technical problems of traditional coatings such as weak bonding, easy peeling, high brittleness, poor fatigue resistance, and insufficient deformation adaptability. It achieves the dual effects of high hardness and wear-resistant protection on the surface of the flexible wheel and stress relief by alternating deformation, thereby significantly improving the fatigue life of the flexible wheel and the long-term transmission accuracy and stability of the harmonic reducer.
[0006] This invention constructs a microscopic anchoring interface through a substrate roughening modification layer, fundamentally improving the bonding strength between the coating and the substrate; a nano-transition buffer layer achieves a mechanical gradient transition from the substrate's toughness to the hard coating's hardness, mitigating interfacial stress and solving deformation cracking problems; a dense, hard support layer provides high-strength, wear-resistant support to resist meshing and extrusion wear on the tooth surface; and a wear-resistant, fatigue-resistant top layer reduces the coefficient of friction, inhibits microcrack propagation, and improves fatigue resistance under alternating loads. The precise matching and synergistic effect of the structural parameters and material properties of each layer achieves a balance of high bonding strength, high hardness, high wear resistance, high fatigue resistance, and excellent deformation adaptability.
[0007] Meanwhile, this invention defines a localized coating strategy, coating only the critical areas of the flexible wheel's meshing deformation, preserving the original toughness of the substrate in non-working areas, avoiding stress concentration caused by the overall coating constraint, and further optimizing the overall mechanical properties and fatigue life of the flexible wheel. This invention also includes a dedicated fabrication process, employing stepwise deposition and low-temperature stress tempering to eliminate residual stress in the coating, ensuring the integrity and stability of the multi-layer coating structure.
[0008] The present invention provides the following technical solution: a high-bonding-strength fatigue-resistant hard coating structure for a harmonic reducer flexure, comprising a harmonic reducer flexure, disposed on the outer tooth working surface and outer wall deformation area of the harmonic reducer flexure, and sequentially stacked from the inside to the outside including: a matrix roughening modification layer, a nano-transition buffer layer, a dense hard support layer, and a wear-resistant and fatigue-resistant top layer; The substrate roughening and modification layer is formed on the surface of the flexible wheel substrate to construct a micro-anchoring interface and improve the overall adhesion between the coating and the substrate. The nano-transition buffer layer covers the surface of the substrate roughening modification layer and is a soft-hard composite gradient nanostructure. It is used to mitigate the interfacial stress generated by the high-frequency deformation of the flexible wheel and prevent the coating from cracking and peeling off at the interface with the substrate. The dense, rigid support layer covers the surface of the nano-transition buffer layer and has high hardness and high density. It is used to provide structural support and improve the overall coating rigidity and compressive and wear-resistant properties. The wear-resistant and fatigue-resistant top layer covers the surface of the dense and hard support layer, and has a low coefficient of friction and high resistance to microcrack propagation. It is used to reduce the meshing friction loss of the tooth surface, suppress the initiation of microcracks under alternating loads, and improve fatigue life.
[0009] The selected flexible wheel substrate is made of high-strength alloy structural steel, and the substrate roughening modification layer is a plasma etching and low-temperature carburizing and nitriding modification layer with a thickness of 3μm to 8μm. The surface of the substrate roughening modification layer forms a micron-level concave-convex anchoring micropore structure with a pore diameter of 0.5μm to 2μm, a porosity of 15% to 25%, and a surface roughness Ra controlled at 0.8μm to 1.2μm.
[0010] The selected nano-transition buffer layer is a TiN-TiCN gradient composite nanolayer with a thickness of 500nm to 1200nm and a nanocrystal size of 20nm to 80nm. The nano-transition buffer layer transitions from a high-toughness TiN material close to the substrate to a high-hardness TiCN material on the outer side, with the hardness increasing from 800HV to 1200HV, thus achieving a smooth transition in the mechanical properties between the substrate and the hard coating.
[0011] The selected dense hard support layer is an ultrafine-grained AlTiN hard coating with a thickness of 4μm to 10μm, a density of ≥98%, and a microhardness of 1800HV to 2200HV. The dense hard support layer contains uniformly distributed nano-dispersed reinforcing phases to improve the coating's compressive strength and structural stability, and to resist the meshing extrusion load on the tooth surface.
[0012] The preferred wear-resistant and fatigue-resistant top layer is a DLC (diamond-like carbon) coating with a thickness of 1μm to 3μm, a friction coefficient ≤0.15, and a microhardness of 2500HV to 3000HV. The wear-resistant and fatigue-resistant top layer is an amorphous carbon nanostructure with excellent deformation adaptability. It can undergo micro-deformation synchronously with the elastic deformation of the flexible wheel, suppressing the generation and propagation of microcracks in the coating under alternating bending loads.
[0013] The selected coating has a total thickness of 10μm to 22μm, with no obvious delamination interfaces or pores and cracks between layers. The coating has a bonding strength of ≥80N with the flexible wheel substrate and can accommodate ±5% high-frequency elastic radial deformation of the flexible wheel. The coating does not peel off or crack under cyclic alternating loads.
[0014] Specifically, the coating structure only covers the meshing working surface of the outer teeth of the flexible wheel and the deformation area of the outer wall. The bottom connection area of the flexible wheel cup and the non-deformation area of the inner ring are not coated, so as to retain the original toughness of the substrate and avoid stress concentration caused by the overall coating constraint.
[0015] A selected method for preparing a high-adhesion, fatigue-resistant hard coating for the flexure of a harmonic reducer includes the following steps: S1. Pretreatment of flexible wheel substrate: Polishing, degreasing, and dust removal are performed on the processed flexible wheel to remove surface burrs, oxide scale and impurities, and ensure the cleanliness of the substrate surface. S2. Preparation of substrate roughening modification layer: The surface of the area to be coated on the flexible wheel is modified by low-pressure plasma etching process, combined with low-temperature vacuum carburizing and nitriding treatment, to form a roughening modification layer with micron-level anchoring micropore structure on the substrate surface. S3. Preparation of nano-transition buffer layer: Using magnetron sputtering, Ti, N, and C reaction gases are introduced in a gradient to deposit a TiN-TiCN gradient nanocomposite layer on the surface of the roughened modified layer. By controlling the deposition power and gas ratio, a gradient transition of hardness and toughness is achieved. S4. Preparation of a dense hard support layer: Using an arc ion plating process, Ti, Al and N are introduced in a gradient to deposit an ultrafine-grained AlTiN hard coating. By controlling the temperature and bias voltage, the coating grains are refined to improve the coating density and structural strength. S5. Preparation of wear-resistant and fatigue-resistant top layer: A DLC diamond-like carbon coating is deposited on the surface of the hard support layer using plasma-enhanced chemical vapor deposition process to complete the preparation of multi-layer composite coating; S6. Post-processing inspection: The coated flexible wheel is subjected to low-temperature stress tempering to eliminate residual stress from the coating deposition. The coating thickness, hardness, bonding strength and surface integrity are inspected, and defective products are rejected.
[0016] In step S2, the plasma etching power is 300W to 500W, the etching time is 15min to 30min, the low-temperature carburizing and nitriding temperature is 180℃ to 220℃, and the holding time is 40min to 60min.
[0017] In step S6, the low-temperature stress tempering temperature is 120℃~150℃, the holding time is 30min, and the coating is naturally cooled to room temperature to eliminate internal stress and improve the coating's deformation adaptability and fatigue resistance.
[0018] The present invention has the following beneficial effects: 1. Significantly improved bonding strength, completely solving the coating peeling problem. This invention replaces the traditional single-plane bonding structure with a double-layer bonding reinforcement design through micro-anchoring modification of the substrate and gradient transition buffer. The bonding strength between the coating and the substrate is ≥80N, which is more than 40% higher than the bonding strength of traditional coatings. It can adapt to the high-frequency elastic deformation of flexible wheels and does not peel, crack, or flake off under long-term alternating loads. The coating has extremely strong protective stability.
[0019] 2. Gradient stress relief and excellent fatigue resistance. This invention adopts a multi-layer gradient structure with gradually changing toughness. The mechanical properties transition smoothly from the substrate to the coating surface, effectively relieving the alternating stress generated by the bending deformation of the flexible wheel and the meshing of the tooth surface, inhibiting the initiation and propagation of microcracks in the coating, increasing the fatigue service life of the flexible wheel by more than 50%, and significantly extending the service life of the entire harmonic reducer.
[0020] 3. High hardness and low friction, providing significant wear resistance and protection. The surface DLC coating, combined with the middle high-hardness AlTiN support structure, achieves a surface hardness of over 2500 HV and a friction coefficient of ≤0.15. This effectively reduces meshing friction loss of the flexible gear teeth, resists extrusion wear, avoids transmission accuracy attenuation caused by tooth surface wear, and ensures long-term high-precision operation of the reducer.
[0021] 4. Strong deformation adaptability and high adaptability to working conditions. The multi-layer composite coating has good flexible adaptability and can synchronously deform slightly with the periodic elastic deformation of the flexible wheel without stress stagnation and accumulation. At the same time, the local coating design retains the inherent toughness of the flexible wheel substrate and avoids the risk of brittle fracture caused by overall coating hardening, perfectly adapting to the special working conditions of the flexible wheel.
[0022] 5. Simple structure, controllable process, and strong practicality. The coating structure has clear layers and precise parameters. The supporting preparation process is mature and stable, enabling large-scale mass production. It is suitable for surface strengthening modification of flexible wheels of various specifications of harmonic reducers and can be widely used in high-end scenarios such as industrial robots, humanoid joints, and aerospace precision transmission equipment. It has extremely high domestic substitution value. Detailed Implementation
[0023] The technical solutions in the embodiments of the present invention have been clearly and completely described. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0024] A high-bonding-strength fatigue-resistant hard coating structure for a harmonic reducer flexure includes a harmonic reducer flexure, and is disposed on the outer tooth working surface and outer wall deformation area of the harmonic reducer flexure, and comprises, from the inside to the outside, the following layers stacked sequentially: a matrix roughening modification layer, a nano-transition buffer layer, a dense hard support layer, and a wear-resistant and fatigue-resistant top layer. A substrate roughening and modification layer is formed on the surface of the flexible wheel substrate to construct a micro-anchoring interface and improve the overall adhesion between the coating and the substrate. A nano-transition buffer layer covers the surface of the substrate roughening modification layer. It is a soft-hard composite gradient nanostructure used to mitigate the interfacial stress generated by the high-frequency deformation of the flexible wheel and prevent the coating from cracking and peeling off at the interface with the substrate. A dense, rigid support layer covers the surface of the nano-transition buffer layer. It has high hardness and high density, and is used to provide structural support and improve the overall coating rigidity and compressive and wear resistance. The wear-resistant and fatigue-resistant top layer covers the surface of the dense and hard support layer. It has a low coefficient of friction and high resistance to microcrack propagation. It is used to reduce the meshing friction loss of the tooth surface, suppress the initiation of microcracks under alternating loads, and improve fatigue life.
[0025] The flexible wheel substrate is made of high-strength alloy structural steel. The substrate roughening and modification layer is a plasma etching and low-temperature carburizing and nitriding modification layer with a thickness of 3μm to 8μm. The surface of the substrate roughening and modification layer forms a micron-level uneven anchoring micropore structure with a pore size of 0.5μm to 2μm, a porosity of 15% to 25%, and a surface roughness Ra controlled at 0.8μm to 1.2μm. The nano-transition buffer layer is a TiN-TiCN gradient composite nanolayer with a thickness of 500nm to 1200nm and a nanocrystal size of 20nm to 80nm. The nano-transition buffer layer transitions from the high-toughness TiN material close to the substrate to the high-hardness TiCN material on the outside, with the hardness increasing from 800HV to 1200HV, achieving a smooth transition in the mechanical properties between the substrate and the hard coating. The dense hard support layer is an ultra-fine crystalline AlTiN hard coating with a thickness of 4μm to 10μm, a density of ≥98%, and a microhardness of 1800HV to 2200HV. The dense hard support layer contains uniformly distributed nano-dispersed reinforcing phases to improve the coating's compressive strength and structural stability, and resist the meshing extrusion load on the tooth surface. The wear-resistant and fatigue-resistant top layer is a diamond-like carbon (DLC) coating with a thickness of 1μm to 3μm, a friction coefficient of ≤0.15, and a microhardness of 2500HV to 3000HV. The wear-resistant and fatigue-resistant top layer is an amorphous carbon nanostructure with excellent deformation adaptability. It can deform slightly in sync with the elastic deformation of the flexible wheel, suppressing the generation and propagation of microcracks in the coating under alternating bending loads. The overall coating structure has a total thickness of 10μm to 22μm. There are no obvious delamination interfaces or pores and cracks between the layers. The coating has a bonding strength of ≥80N with the flexible wheel substrate. It can accommodate ±5% high-frequency elastic radial deformation of the flexible wheel. The coating does not peel off or crack under cyclic alternating load. The coating structure only covers the meshing working surface of the outer teeth of the flexible wheel and the deformation area of the outer wall. The bottom connection area of the flexible wheel cup and the non-deformation area of the inner ring are not coated, so as to retain the original toughness of the substrate and avoid the stress concentration of the flexible wheel deformation caused by the overall coating constraint. A method for preparing a high-adhesion, fatigue-resistant hard coating for the flexible wheel of a harmonic reducer includes the following steps: S1. Pretreatment of flexible wheel substrate: Polishing, degreasing, and dust removal are performed on the processed flexible wheel to remove surface burrs, oxide scale and impurities, and ensure the cleanliness of the substrate surface. S2. Preparation of substrate roughening modification layer: The surface of the area to be coated on the flexible wheel is modified by low-pressure plasma etching process, combined with low-temperature vacuum carburizing and nitriding treatment, to form a roughening modification layer with micron-level anchoring micropore structure on the substrate surface. S3. Preparation of nano-transition buffer layer: Using magnetron sputtering, Ti, N, and C reaction gases are introduced in a gradient to deposit a TiN-TiCN gradient nanocomposite layer on the surface of the roughened modified layer. By controlling the deposition power and gas ratio, a gradient transition of hardness and toughness is achieved. S4. Preparation of a dense hard support layer: Using an arc ion plating process, Ti, Al and N are introduced in a gradient to deposit an ultrafine-grained AlTiN hard coating. By controlling the temperature and bias voltage, the coating grains are refined to improve the coating density and structural strength. S5. Preparation of wear-resistant and fatigue-resistant top layer: A DLC diamond-like carbon coating is deposited on the surface of the hard support layer using plasma-enhanced chemical vapor deposition process to complete the preparation of multi-layer composite coating; S6. Post-processing inspection: The coated flexible wheel is subjected to low-temperature stress tempering to eliminate residual stress from the coating deposition. The coating thickness, hardness, bonding strength and surface integrity are inspected, and defective products are rejected. In step S2, the plasma etching power is 300W to 500W, the etching time is 15min to 30min, the low temperature carburizing and nitriding temperature is 180℃ to 220℃, and the holding time is 40min to 60min. In step S6, the low-temperature stress tempering temperature is 120℃~150℃, the holding time is 30min, and it is naturally cooled to room temperature to eliminate internal stress in the coating and improve the coating's deformation adaptability and fatigue resistance.
[0026] This embodiment applies to the flexible wheel of a conventional industrial robot harmonic reducer. The flexible wheel substrate is 40CrNiMoA high-strength alloy structural steel, and the coating adopts a four-layer gradient composite structure. The specific parameters are as follows: Substrate roughening modification layer: 5 μm thick, surface micropore diameter 1 μm, porosity 20%, surface roughness Ra 1.0 μm, formed by plasma etching and low-temperature carburizing and nitriding at 200℃ to construct a uniform micro-anchoring interface; Nano-transition buffer layer: 800 nm thick, TiN-TiCN gradient nanostructure, grain size 50 nm, hardness gradient from 900 HV to 1100 HV; Dense hard support layer: 6 μm thick, ultrafine-grained AlTiN coating, density 98.5%, hardness 2000 HV; Wear-resistant and fatigue-resistant top layer: 2 μm thick, DLC diamond-like carbon coating, friction coefficient 0.12, hardness 2800 HV.
[0027] Fabrication process: After cleaning and removing impurities from the substrate, plasma etching at 400W power for 20 min is performed, followed by low-temperature carburizing and nitriding at 200℃ for 50 min; a gradient transition layer is deposited by magnetron sputtering, a hard support layer is deposited by arc ion plating, and a top coating is deposited by PECVD; finally, a low-temperature tempering at 130℃ for 30 min is performed to eliminate residual stress.
[0028] Testing revealed that the total coating thickness in this embodiment is 13.8 μm, with a bonding strength of 85 N. After the flexible wheel underwent 10 million cycles of alternating deformation, the coating showed no cracking, peeling, or wear. The fatigue life was increased by 55% compared to traditional single coatings, and the transmission accuracy and stability were significantly improved.
[0029] This embodiment is applicable to the flexible gear of a harmonic reducer in a heavy-duty precision machine tool, and optimizes the coating parameters for high-load, high-frequency alternating operating conditions. Matrix roughening modification layer: 7μm thick, 1.5μm micropore diameter, 23% porosity, enhancing anchoring bonding effect; Nano-transition buffer layer: 1000nm thick, 60nm grain size, hardness gradient range 850HV~1200HV, improving stress relief capability; Dense hard support layer: 9μm thick, 99% density, 2100HV hardness, enhancing compressive strength and wear resistance; Wear-resistant and fatigue-resistant top layer: 2.5μm thick, 2900HV hardness, coefficient of friction 0.13.
[0030] This embodiment is applicable to the flexible wheel of a micro harmonic reducer for humanoid robots, and adopts a thin and lightweight coating design: The substrate roughening modification layer has a thickness of 3 μm, a micropore diameter of 0.5 μm, and a porosity of 16%; the nano-transition buffer layer has a thickness of 500 nm; the dense hard support layer has a thickness of 4 μm; the wear-resistant and fatigue-resistant top layer has a thickness of 1 μm, and the total coating thickness is only 8.5 μm.
[0031] The coating in this embodiment is thin and lightweight with no added weight, and does not affect the deformation accuracy of the miniature flexible wheel. At the same time, it retains high adhesion and high fatigue resistance, making it suitable for the lightweight, high precision, and long service life requirements of miniature high-precision harmonic reducers.
[0032] The coating in this embodiment has stronger overall rigidity and impact resistance, making it suitable for heavy-duty meshing and extrusion conditions. After heavy-duty fatigue testing, the wear resistance of the flexible wheel is improved by 60%, and the resistance to crack propagation under alternating loads is significantly enhanced, fully meeting the long-term service requirements of high-end heavy-duty precision transmission equipment.
[0033] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A high bond fatigue resistant hard coating structure for a harmonic reducer flexspline, comprising a harmonic reducer flexspline, characterized in that: The outer tooth working surface and outer wall deformation area of the flex wheel of the harmonic reducer are arranged in the following order from the inside to the outside: a matrix roughening modification layer, a nano transition buffer layer, a dense hard support layer, and a wear-resistant and fatigue-resistant top layer. The substrate roughening modification layer is formed on the surface of the flexible wheel substrate to construct a micro-anchoring interface and improve the overall adhesion between the coating and the substrate. The nano-transition buffer layer covers the surface of the substrate roughening modification layer and is a soft-hard composite gradient nanostructure. It is used to mitigate the interfacial stress generated by the high-frequency deformation of the flexible wheel and prevent the coating from cracking and peeling off at the interface with the substrate. The dense, rigid support layer covers the surface of the nano-transition buffer layer and has high hardness and high density. It is used to provide structural support and improve the overall coating rigidity and compressive and wear-resistant properties. The wear-resistant and fatigue-resistant top layer covers the surface of the dense and hard support layer, and has a low coefficient of friction and high resistance to microcrack propagation. It is used to reduce the meshing friction loss of the tooth surface, suppress the initiation of microcracks under alternating loads, and improve fatigue life.
2. A high bond fatigue resistant hard coating structure for a flexspline of a harmonic reducer according to claim 1, characterized in that: The flexible wheel substrate is made of high-strength alloy structural steel. The substrate roughening modification layer is a plasma etching and low-temperature carburizing and nitriding modification layer with a thickness of 3μm to 8μm. The surface of the substrate roughening modification layer forms a micron-level concave-convex anchoring micropore structure with a pore diameter of 0.5μm to 2μm, a porosity of 15% to 25%, and a surface roughness Ra controlled at 0.8μm to 1.2μm.
3. A high bond strength fatigue resistant hard coating structure for a flexspline of a harmonic reducer according to claim 1, characterized in that: The nano-transition buffer layer is a TiN-TiCN gradient composite nanolayer with a thickness of 500nm to 1200nm and a nanocrystal size of 20nm to 80nm. The nano-transition buffer layer transitions from a high-toughness TiN material close to the substrate to a high-hardness TiCN material on the outer side, with the hardness increasing from 800HV to 1200HV, thus achieving a smooth transition in the mechanical properties between the substrate and the hard coating.
4. A high bond fatigue resistant hard coating structure for a flexspline of a harmonic reducer according to claim 1, characterized in that: The dense hard support layer is an ultrafine-grained AlTiN hard coating with a thickness of 4μm to 10μm, a density of ≥98%, and a microhardness of 1800HV to 2200HV. The dense hard support layer contains uniformly distributed nano-dispersed reinforcing phases to improve the coating's compressive strength and structural stability, and resist the meshing extrusion load on the tooth surface.
5. A high bond fatigue resistant hard coating structure for a flexspline of a harmonic reducer according to claim 1, characterized in that: The wear-resistant and fatigue-resistant top layer is a diamond-like carbon (DLC) coating with a thickness of 1μm to 3μm, a friction coefficient ≤0.15, and a microhardness of 2500HV to 3000HV. The wear-resistant and fatigue-resistant top layer is an amorphous carbon nanostructure with excellent deformation adaptability. It can undergo slight deformation synchronously with the elastic deformation of the flexible wheel, suppressing the generation and propagation of microcracks in the coating under alternating bending loads.
6. A high bond fatigue resistant hard coating structure for a flexspline of a harmonic reducer according to claim 1, characterized in that: The overall coating structure has a total thickness of 10μm to 22μm, with no obvious delamination interfaces or pores and cracks between the layers. The coating has a bonding strength of ≥80N with the flexible wheel substrate and can accommodate ±5% high-frequency elastic radial deformation of the flexible wheel. The coating does not peel off or crack under cyclic alternating loads.
7. A high bond strength, fatigue resistant hard coating structure for a flexspline of a harmonic reducer as defined in claim 1, wherein: The coating structure only covers the meshing working surface of the outer teeth of the flexible wheel and the deformation area of the outer wall. The bottom connection area of the flexible wheel cup and the non-deformation area of the inner ring are not coated, so as to retain the original toughness of the substrate and avoid stress concentration caused by the overall coating constraint.
8. The high-bonding-strength, fatigue-resistant hard coating structure for the flexible wheel of a harmonic reducer according to claim 1, characterized in that: A method for preparing a high-adhesion, fatigue-resistant hard coating for the flexible wheel of a harmonic reducer includes the following steps: S1. Pretreatment of flexible wheel substrate: Polishing, degreasing, and dust removal are performed on the processed flexible wheel to remove surface burrs, oxide scale and impurities, and ensure the cleanliness of the substrate surface. S2. Preparation of substrate roughening modification layer: The surface of the area to be coated on the flexible wheel is modified by low-pressure plasma etching process, combined with low-temperature vacuum carburizing and nitriding treatment, to form a roughening modification layer with micron-level anchoring micropore structure on the substrate surface. S3. Preparation of nano-transition buffer layer: Using magnetron sputtering, Ti, N, and C reactive elements are introduced in a gradient to deposit a TiN-TiCN gradient nanocomposite layer on the surface of the roughened modified layer. By controlling the deposition power and gas ratio, a gradient transition of hardness and toughness is achieved. S4. Preparation of a dense hard support layer: Using an arc ion plating process, Ti, Al and N are introduced in a gradient to deposit an ultrafine-grained AlTiN hard coating. By controlling the temperature and bias voltage, the coating grains are refined to improve the coating density and structural strength. S5. Preparation of wear-resistant and fatigue-resistant top layer: A DLC diamond-like carbon coating is deposited on the surface of the hard support layer using plasma-enhanced chemical vapor deposition process to complete the preparation of multi-layer composite coating; S6. Post-processing inspection: The coated flexible wheel is subjected to low-temperature stress tempering to eliminate residual stress from the coating deposition. The coating thickness, hardness, bonding strength and surface integrity are inspected, and defective products are rejected.
9. A high-bonding-strength, fatigue-resistant hard coating structure for a harmonic reducer flexspline according to claim 8, characterized in that: In step S2, the plasma etching power is 300W to 500W, the etching time is 15min to 30min, the low-temperature carburizing and nitriding temperature is 180℃ to 220℃, and the holding time is 40min to 60min.
10. A high-bonding-strength, fatigue-resistant hard coating structure for a flexural wheel of a harmonic reducer according to claim 8, characterized in that: In step S6, the low-temperature stress tempering temperature is 120℃~150℃, the holding time is 30min, and it is naturally cooled to room temperature to eliminate internal stress in the coating and improve the coating's deformation adaptability and fatigue resistance.