A method for constructing concrete floors

By using the armored joint technology to rigidly connect with the floor steel mesh and the adaptive stress management of the pressure relief unit, combined with the prefabricated three-dimensional module to handle stress concentration nodes, the problems of low construction efficiency and cracking of traditional concrete floors are solved, achieving efficient and environmentally friendly floor construction.

CN123109359APending Publication Date: 2026-11-17GUANGZHOU XIEAN CONSTR ENG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611465277.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional concrete flooring construction methods consume a lot of building materials and manpower, have low construction efficiency, and the cutting process pollutes the environment, making it difficult to effectively prevent floor cracking.

Method used

The system employs an armored seam technology, which uses anchored steel plates and ground steel mesh to form an integrated load-bearing grid. It integrates pressure relief units to adaptively absorb stress from temperature changes, and combines prefabricated three-dimensional adjustable flexible modules to handle stress concentration nodes, using highly elastic sealing materials.

Benefits of technology

Improve construction efficiency, reduce material consumption and environmental pollution, lower maintenance costs, prevent floor cracks, and form an integrated load-bearing system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123109359A_ABST
    Figure CN123109359A_ABST
Patent Text Reader

Abstract

This invention discloses a method for constructing a concrete floor, comprising the following steps: S1, base treatment, removing debris, oil stains, laitance, and other attachments, and repairing defects such as cracks, honeycombing, and pitting in the base layer; S2, laying an isolation layer, laying a layer of fine sand between the base layer and the floor surface layer, and then laying a PE film on the fine sand layer, with the overlaps sealed with tape. The armored joint of this invention achieves a rigid connection with the floor reinforcement mesh through anchor steel plates, forming an integral load-bearing frame. The armored joint itself can effectively transmit vertical shear force and constrain the settlement difference between floor sections; furthermore, the armored joint integrates a pressure relief unit that can preset stress response thresholds according to the floor load level and ambient temperature and humidity, adaptively absorbing and releasing the hydration heat of concrete and the horizontal expansion and contraction stress caused by changes in ambient temperature, reducing floor cracks caused by temperature stress accumulation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of concrete floor construction technology, and specifically relates to a concrete floor construction method. Background Technology

[0002] The floor refers to the ground surface of a building that is in direct contact with the foundation soil. Concrete floors are widely used in industrial plants, logistics warehouses, hospitals, aquatic product markets, and other buildings. They need to withstand complex forces such as static loads from heavy equipment and dynamic loads from cargo transportation over long periods of time. Therefore, the floor should have good strength, rigidity, flatness, and durability.

[0003] Currently, traditional concrete floor construction techniques mainly employ a compartmentalized construction method. This involves dividing a large area of ​​the floor into several compartments using formwork, pouring concrete in each compartment, and then cutting expansion joints into the surface using a joint cutter after the concrete has reached a certain strength. This avoids cracking of the large area of ​​the floor due to concrete shrinkage, thus ensuring the quality of the concrete floor construction. However, this method requires a large amount of building materials such as wooden formwork and timber during compartmentalization, and the repeated setting up and dismantling of these materials consumes a significant amount of manpower, resulting in low construction efficiency. Furthermore, the cutting of expansion joints generates a large amount of mud and dust, polluting the environment and requiring thorough cleaning before proceeding to the next step, further contributing to low construction efficiency. Summary of the Invention

[0004] The purpose of this invention is to provide a concrete floor construction method to solve at least one of the aforementioned technical problems. The armored joint of this invention achieves a rigid connection with the floor reinforcement mesh through anchor steel plates, forming an integral load-bearing frame. The armored joint itself can effectively transmit vertical shear force and constrain the settlement difference between floor sections. Furthermore, the armored joint is integrated with a pressure relief unit that can preset stress response thresholds based on the floor load level and ambient temperature and humidity, adaptively absorbing and releasing the horizontal expansion and contraction stress caused by concrete hydration heat and changes in ambient temperature, reducing floor cracks caused by temperature stress accumulation. Simultaneously, for complex nodes with stress concentration such as column bases, wall roots, door openings, wells, and irregularly shaped components, a combination of prefabricated three-dimensional adjustable flexible modules and on-site injection of highly elastic sealing materials is used to solve the technical problem of easy cracking at irregularly shaped nodes, significantly reducing the cost of later floor maintenance and repair.

[0005] To achieve the above-mentioned objectives, the technical solution adopted by the present invention is as follows: A method for constructing a concrete floor, the method comprising the following steps in sequence: S1. Substrate treatment: Remove debris, oil stains, laitance, and repair defects such as cracks, honeycombing, and pitting in the substrate. S2. Laying the isolation layer: Lay a layer of fine sand between the base layer and the floor surface layer, and then lay a PE film on the fine sand layer, and use tape to stick the overlaps. S3. Armor seam positioning: Armor seams are installed at the intersections of longitudinal and transverse seams or starting from the base of the wall or column and installed in sequence; the elevation is measured from the benchmark point, the theodolite is used to lay out the lines, the installation position of the armor seams and the elevation control line are marked, and the level is used to verify; S4. Adjust the armored joint: The armored joint is equipped with a pressure relief unit. Adjust the pressure threshold of the pressure relief unit according to the on-site construction conditions. S5. Welding of Armored Joints: S5.1. Install the armored joints in sections, and tie the reinforcing mesh in sections based on the armored joints; S5.2. Place each section of the armored joint in the correct position according to the layout line, and use an adjuster to fine-tune the height and flatness of each section independently. Use a laser level to measure and verify at both ends of the connector; S5.3. Use short steel bars for temporary fixing of the armored joints, drive them into the foundation, and set at least four fixing points for each section of the armored joint. Weld the top of the short steel bars to the side wall of the armored joint and weld the upper layer of reinforcing mesh to the short steel bars; S6. Concrete pouring; S7. Concrete leveling, troweling, and polishing; S8. Concrete curing.

[0006] Preferably, the armor seam includes: two vertically parallel supporting steel plates connected by adjusting bolts; movable steel plates symmetrically arranged on both sides of the supporting steel plates, the movable steel plates being able to slide along the height direction of the supporting steel plates, and a movable sleeve fitted at one end of the movable steel plate; the top and bottom ends of the supporting steel plates extending obliquely outward to form anchoring steel plates; a reserved groove is provided between the movable sleeve and the anchoring steel plates, and a pressure relief unit is provided in the reserved groove.

[0007] Preferably, the pressure relief unit is an elastic rubber body. In step S4, the pre-compression of the high-performance elastic rubber body is changed by turning the adjusting bolt, taking into account the shrinkage and expansion of the concrete, the ambient temperature and humidity, and the heavy load level of the floor. The pre-compression of the rubber body is increased for heavy-load floors and decreased for ordinary floors.

[0008] Preferably, in step S5, the armor seam is installed in sections, with a standard length of 3m for each section. Adjacent armor seam sections are connected by spring pins and easily broken bolts, and a 1-2mm expansion gap is reserved at the top flat steel of the joint.

[0009] Preferably, in step S5, the short reinforcing bars are driven into the foundation alternately in a vertical manner and at a 30° angle to the vertical to form a triangular stress structure, and the weld between the top of the short reinforcing bar and the anchoring steel plate of the armor seam is ≥10cm.

[0010] Preferably, in step S5, the irregular junction between the floor and the column base / wall base is treated as follows: Column base joint treatment: At the junction of the floor and the steel column, prefabricated three-dimensional adjustable flexible armored joint modules are installed around the column base. The three-dimensional adjustable flexible armored joint modules are finely adjusted using three-dimensional adjusting bolts to ensure a tight fit between the module and the column base. A 10-15mm wide flexible gap is left between the three-dimensional adjustable flexible armored joint module and the column base. After the concrete surface layer is completed, polyurethane caulking is used to seal the gap to a depth of 30-50mm. For circular steel columns, the module is made of 2mm thick steel plate bent into an arc shape and installed around the column base. The arc shape of the steel plate avoids the formation of internal and external corners, effectively preventing cracking of the floor concrete at the corners. For rectangular steel columns, the module is made of 2mm thick steel plate bent into a rectangle and installed around the column base. Treatment of joints between wall base, ground rail beam and pressure beam: At the junction of the floor and the wall, ground rail beam and pressure beam, 20mm thick PE foam cotton is used for isolation, with a foam cotton height of 350mm. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Doorway joint treatment: At the junction of the hangar door and factory gate opening and the ground, prefabricated three-dimensional adjustable modules are arranged along the edge of the doorway. L50×5 galvanized angle steel is set as corner guards within a 200mm width range on both sides of the doorway. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Treatment of the top node of the manhole: A reinforcing steel mesh is added at the junction of the ground and the top of the manhole. The reinforcing steel mesh is supported by steel legs. The bottom of the legs is spot-welded to the bottom steel bars of the manhole top plate. The top of the steel mesh is 30-40mm away from the finished surface of the ground. Other irregular node treatments: including at least irregular column bases, multi-column side-by-side column bases, complex outlines of equipment foundations, and corners of trenches and pits. After cleaning the node area, set up simple templates, pour in two-component high-elasticity sealing material, and allow it to self-level and cure.

[0011] Preferably, in step S6, the garbage in the trough is cleaned a second time and rinsed with water before pouring concrete; after the concrete mixer truck arrives at the site, the concrete opening test and slump are checked, and unloading is carried out after the requirements are met; laser leveling machine is used for compartment pouring and leveling construction. For areas around columns, walls and compartments that cannot be operated by laser leveling machine, construction personnel need to perform manual vibration.

[0012] Preferably, in step S7, laser signal transmitters are deployed, the pouring area is demarcated and surrounding templates are erected, and the pouring sequence is determined; laser transmitters are installed at selected locations, the elevation of the concrete surface layer is determined according to the design elevation, and the elevation of the laser leveling machine's working unit is adjusted; when mechanically pouring concrete, the material is unloaded evenly to ensure sufficient working space for the laser leveling equipment; the laser leveling machine is used to level the concrete, and the elevation of the working surface is re-checked during the leveling operation; for areas around column bases, walls, and compartments where the laser leveling machine cannot operate, manual scraping is used for leveling, and the elevation is repeatedly checked.

[0013] Preferably, in step S7, when the concrete surface has lost most of its bleed water and leaves a slight fingerprint when lightly pressed with a finger but is not sticky, indicating it is in the initial setting state, the specified amount of wear-resistant material is evenly spread on the initially set concrete surface. A trowel is used to smooth the surface horizontally and vertically, and the finished surface elevation and flatness are checked. After the wear-resistant material absorbs some moisture, a single-wheel grinder is started for the first grinding and compaction operation. After the wear-resistant material hardens, a second application of wear-resistant material is performed, and the trowel is again used to smooth the surface horizontally and vertically, and the finished surface elevation and flatness are checked. If the trowel leveling and verification are correct, a double-wheel grinder is started for the final finishing and compaction operation. The grinder is used in a cycle of grinding 3-4 times, starting slowly and then speeding up, and starting horizontally and then vertically. Each grinding should be performed immediately after the trowel marks left by the previous grinding have disappeared.

[0014] Preferably, the concrete surface should be covered with plastic film and felt for moisture retention and curing. During the curing period, the concrete surface should be kept moist at all times, and the curing time should not be less than 7 days.

[0015] Compared with the prior art, the present invention has the following beneficial effects: 1. The armored joint of this invention achieves rigid connection with the ground reinforcement mesh through anchor steel plates, forming an integral load-bearing grid. The armored joint body can effectively transmit vertical shear force and constrain the settlement difference between the floor compartments. Furthermore, the armored joint is integrated with a pressure relief unit that can preset stress response thresholds according to the floor load level and ambient temperature and humidity. It can adaptively absorb and release the horizontal expansion and contraction stress caused by concrete hydration heat and ambient temperature changes, reducing floor cracks caused by temperature stress accumulation. At the same time, for complex nodes with stress concentration such as column bases, wall bases, door openings, wells, and irregular components, a combination of prefabricated three-dimensional adjustable flexible modules and on-site injection of high-elasticity sealing materials is used to solve the technical problem of easy cracking at irregular node locations, significantly reducing the cost of later maintenance and repair of the floor.

[0016] 2. This invention utilizes the armored joint as a modular formwork, allowing for parallel installation of the armored joint and reinforcement mesh binding. This eliminates the traditional steps of waiting for concrete to reach its strength, mechanically cutting the joint, and cleaning up mud and dust after cutting, significantly reducing waiting time. The armored joint uses prefabricated 3m standard segments in the factory, with spring pins used on-site. The use of easily breakable bolts for rapid splicing, alternating anchoring of short steel bars, and a high degree of modular assembly reduces on-site formwork dismantling work and effectively shortens the overall floor construction period. Attached Figure Description

[0017] Figure 1 This is a structural diagram of the installation of the armor seam and the floor of the present invention; Figure 2 This is a schematic diagram illustrating the casting of walls or foundation beams according to the present invention; Figure 3 This is a field diagram of the column base treatment according to the present invention; Figure 4 This is a diagram showing the concrete floor pouring process of the present invention.

[0018] Figure Labels 1. Flooring; 2. Supporting steel plate; 3. Adjusting bolts; 4. Movable steel plate; 5. Movable sleeve; 6. Anchoring steel plate; 7. Pressure relief unit; 8. Wall; 9. Foam; 10. Wide flexible gap; 11. Three-dimensional adjustable flexible armored joint module. Detailed Implementation

[0019] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the specific implementation methods of the present invention will be described below with reference to the accompanying drawings. Obviously, the drawings described below are merely some embodiments of the present invention. For those skilled in the art, other drawings and other implementation methods can be obtained based on these drawings without any creative effort.

[0020] The technical solution of the present invention will be described in detail below with specific embodiments.

[0021] refer to Figure 1-4 As shown, a concrete floor construction method of the present invention includes the following steps in sequence: S1. Substrate treatment: Remove debris, oil stains, laitance and other attachments, and repair defects such as cracks, honeycomb and pitting in the substrate. S2. Laying the isolation layer: Lay a layer of fine sand between the base layer and the floor surface layer, and then lay a 0.3-0.4mm thick PE film on the fine sand layer, and use tape to stick the overlaps. S3. Armor seam positioning: Armor seams are installed at the intersections of longitudinal and transverse seams or starting from the base of the wall or column and proceeding in sequence; the elevation is measured from the benchmark point, and a theodolite is used to lay out the lines, marking the installation position of the armor seams and the elevation control line. The axis deviation is ≤±5mm, and a level is used to verify. S4. Adjust the armored joint: The armored joint is equipped with a pressure relief unit. Adjust the pressure threshold of the pressure relief unit according to the on-site construction conditions. S5. Welding of Armored Joints: S5.1. Install the armored joints in sections and tie the reinforcing mesh in sections based on the armored joints; S5.2. Place each section of the armored joint in the correct position according to the layout line, and use an adjuster to fine-tune the height and flatness of each section independently, so that the top of the armored joint is 1-2mm lower than the ground surface. Use a laser level to measure and verify at both ends of the connector; S5.3. Temporarily fix the armored joints with short steel bars of 12-16mm in diameter, drive them into the foundation to a depth of at least 300mm, and set at least four fixing points for each section of the armored joint. Weld the top of the short steel bars to the side wall of the armored joint and weld the upper layer of reinforcing mesh to the short steel bars; S6. Concrete pouring; S7. Concrete leveling, troweling, and polishing; S8. Concrete curing.

[0022] Specifically, in step S2, the PE film needs to be passed through the bottom of the armor seam and extended to the wall surface, with an upward height of not less than 400mm. The function of the PE film is: (1) to reduce the friction coefficient between the bottom of the floor and the base layer, so that the shrinkage and expansion of the concrete floor are not restricted, and to reduce the possibility of cracks forming at the bottom of the slab; (2) to prevent concrete leakage and premature water loss, and to serve as a moisture-proof layer.

[0023] In this embodiment, as Figure 1 As shown, the armor seam includes: two vertically parallel supporting steel plates connected by adjusting bolts; movable steel plates symmetrically arranged on both sides of the supporting steel plates, the movable steel plates being able to slide along the height direction of the supporting steel plates, and a movable sleeve fitted at one end of the movable steel plate; the top and bottom ends of the supporting steel plates extending obliquely outward to form anchoring steel plates; a reserved groove is provided between the movable sleeve and the anchoring steel plates, and a pressure relief unit is provided in the reserved groove.

[0024] Specifically, the adjusting bolt is a breakable bolt used to temporarily connect the two supporting steel plates. The adjusting bolt will automatically break after the subsequent concrete pouring and hardening.

[0025] Traditional compartment joints serve only as "isolation and separation" components and do not have the capacity to transfer loads. When the floor is subjected to the static load of heavy equipment or the dynamic load of transport vehicles, the floor slabs on both sides of the compartment joint are independent of each other, and their stress deformation is not restrained by each other. Vertical settlement difference is likely to occur between the slabs, and significant stress concentration occurs at the edge of the joint, which further induces quality defects such as edge chipping, misalignment, and cracking. In this invention, the armored joint is rigidly connected to the ground reinforcement mesh by welding, forming a unified spatial load-bearing frame. When the ground is subjected to vertical forces, one side of the ground slab bears vertical loads such as equipment weight and vehicle loads, and tends to be compressed and settle. The load is transferred to the armored joint sidewall by the mechanical gripping force formed between the hardened concrete and the outer surface of the armored joint sidewall. The large-area contact surface between the sidewall and the concrete is the primary interface for vertical load transfer, ensuring that the load can be effectively transferred from the concrete to the armored joint. Subsequently, the armored joint sidewall further disperses the received load through anchoring steel plates extending outward from the bottom, transferring it to the deeper concrete area of ​​the concrete slab on that side. The anchoring steel plates adopt a bent structure and have a raised surface structure, which greatly enhances the mechanical interlocking force between the anchoring steel plates and the concrete, preventing the armored joint from separating or slipping from the concrete under stress, and ensuring reliable anchoring connection. The sidewalls of the supporting steel plate in the expansion joint are firmly bonded to the concrete of the corresponding side slab. During construction, the sidewalls are temporarily connected and positioned using easily breakable bolts. After the concrete hardens, these bolts break or loosen under temperature stress, and the load is no longer transferred between the sidewalls. The sidewalls of the supporting steel plate are then integrated with their respective concrete slabs, forming a unified load-bearing system for the floor. This system effectively transfers the vertical shear force between the slabs, constrains the relative vertical displacement of the slabs, and prevents excessive settlement differences between the slabs. In other words, when uneven settlement occurs in the floor sections on both sides of the expansion joint, the sidewalls of the supporting steel plate, through anchored steel plates, distribute the settlement force to the interior of the concrete slab on their respective sides. The unified load-bearing system composed of the expansion joint and the steel mesh works together to resist uneven settlement deformation, thereby avoiding the appearance of uneven steps on both sides of the expansion joint and protecting the integrity of the floor joint.

[0026] In this embodiment, the pressure relief unit is an elastic rubber body. In step S4, the pre-compression amount of the high-performance elastic rubber body is changed by turning the adjusting bolt, taking into account the shrinkage and expansion of the concrete, the ambient temperature and humidity, and the heavy load level of the floor. The pre-compression amount of the rubber body is increased for heavy-load floors and decreased for ordinary floors.

[0027] Specifically, all vertical loads are transferred and diffused to the concrete floor and the underlying foundation through the armored joint body (supporting steel plate sidewalls and anchoring steel plates); while the pressure relief unit (elastic rubber body) integrated on the top of the armored joint does not bear any vertical loads. Its only function is to absorb and release the horizontal expansion and contraction stresses of the concrete caused by the rise and fall of hydration heat and changes in ambient temperature.

[0028] When concrete expands due to the heat of hydration or increased ambient temperature, its internal compressive stress increases accordingly. When this compressive stress exceeds the preset activation threshold of the pressure relief unit, it pushes the movable steel plate upwards (or outwards), compressing the high-performance elastic rubber body and causing it to deform. The compression deformation of the rubber body provides a buffer space for the volume expansion of the concrete, thus absorbing and releasing the accumulated compressive stress in the form of elastic potential energy, preventing stress concentration that could lead to concrete cracking. When the ambient temperature decreases or the shrinkage stress decreases, the compressed elastic rubber body uses its own rebound energy to push the movable steel plate back to its original position, keeping the two sides of the joint tightly fitted and effectively preventing external debris, dust, or moisture from penetrating the joint. The above "compression-rebound" process can cycle repeatedly with the periodic changes in ambient temperature and concrete temperature, keeping the pressure relief unit in a dynamic and adaptive working state. This enables the quantitative, continuous, and automatic absorption and release of horizontal expansion / shrinkage stress in the concrete, ensuring that the floor structure maintains a stable stress balance throughout its entire life cycle.

[0029] In this embodiment, in step S5, the armor seam is installed in sections, with a standard length of 3m for each section. Adjacent armor seam sections are connected by spring pins and easily broken bolts, and a 1-2mm expansion gap is reserved at the top flat steel of the joint.

[0030] Specifically, the armored seams are prefabricated in 3m standard segments at the factory. On-site, spring pins are used to achieve radial positioning and coaxial connection between segments, ensuring the overall straightness after splicing multiple segments. The breakable bolts serve only as temporary connectors during the construction phase, restraining the relative displacement between segments and ensuring that the armored seam splicing position does not deform or misalign when the concrete is poured. After the concrete hardens, the breakable bolts break due to the temperature contraction and expansion, releasing the restraint between segments. The 1-2mm expansion gap provides deformation margin for the temperature deformation of the concrete, preventing the armored seams from arching due to the thermal expansion and compression of the concrete. After splicing, the misalignment at the joint needs to be checked, and the misalignment deviation should not exceed 1mm to ensure that the joint is straight and flat after the floor is completed.

[0031] In this embodiment, in step S5, the short steel bars are driven into the foundation alternately in a vertical manner and at a 30° angle to the vertical to form a triangular stress structure, and the weld between the top of the short steel bar and the armored seam anchoring steel plate is ≥10cm.

[0032] Specifically, diameter φ12 φ16 short steel bars are alternately arranged vertically and at a 30° angle, forming a triangular stable force system in pairs to enhance the anti-buoyancy and anti-lateral displacement capacity of the armored joint. The short steel bars are driven into the foundation to a depth of not less than 300mm to reliably anchor the armored joint anchoring steel plate to the foundation. The weld length is not less than 10cm, and double-sided intermittent welding is used. After welding, the weld slag is removed and anti-corrosion treatment is applied. There are no less than four anchoring points every 3m of armored joint. The vertical and inclined steel bars are arranged alternately to resist the lateral thrust and buoyancy generated during concrete pouring and vibration, preventing the armored joint from shifting, floating, or twisting, and ensuring that the elevation and verticality of the armored joint meet the construction requirements. At the same time, the short steel bars can also serve as auxiliary support points for the steel mesh, reducing the investment in additional supports.

[0033] In this embodiment, as Figure 2 and Figure 3 As shown, in step S5, the irregular junctions between the floor and column bases, wall bases, etc., are processed as follows: Column base joint treatment: At the junction of the floor and the steel column, prefabricated three-dimensional adjustable flexible armored joint modules are installed around the column base. The three-dimensional adjustable flexible armored joint modules are finely adjusted using three-dimensional adjusting bolts to ensure a tight fit between the module and the column base. A 10-15mm wide flexible gap is left between the three-dimensional adjustable flexible armored joint module and the column base. After the concrete surface layer is completed, polyurethane caulking is used to seal the gap to a depth of 30-50mm. For circular steel columns, the module is made of 2mm thick steel plate bent into an arc shape and installed around the column base. The arc shape of the steel plate avoids the formation of internal and external corners, effectively preventing cracking of the floor concrete at the corners. For rectangular steel columns, the module is made of 2mm thick steel plate bent into a rectangle and installed around the column base. Treatment of joints between wall base, ground rail beam and pressure beam: At the junction of the floor and the wall, ground rail beam and pressure beam, 20mm thick PE foam cotton is used for isolation, with a foam cotton height of 350mm. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Doorway joint treatment: At the junction of doorways such as hangar doors and factory gates and the ground, prefabricated three-dimensional adjustable modules are arranged along the edge of the doorway. L50×5 galvanized angle steel is installed as corner guards within a 200mm width range on both sides of the doorway. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Treatment of the top node of the manhole: A reinforcing steel mesh is added at the junction of the ground and the top of the manhole. The reinforcing steel mesh is supported by steel legs. The bottom of the legs is spot welded to the bottom steel bars of the manhole top plate. The embedding depth of the reinforcing steel mesh should not be too large. The top of the steel mesh is 30-40mm away from the finished surface of the ground. Other irregular node treatments include: at least irregular column bases (H-shaped, cross-shaped, L-shaped steel columns, etc.), multi-column side-by-side column bases, complex outlines of equipment foundations (pipeline outlets, maintenance ports, and other ancillary facilities), and the corners of trenches and pits. After cleaning the node area, set up simple templates, pour in two-component high-elasticity sealing material, and allow it to self-level and cure.

[0034] In this embodiment, in step S6, the garbage in the trough is cleaned a second time and rinsed with water before pouring concrete; after the concrete mixer truck arrives at the site, the concrete opening test and slump must be checked, and unloading is carried out after the requirements are met; a laser leveling machine is used for compartment pouring and leveling construction, and the laser leveling machine has uniform high-frequency vibration. However, for the column edges, wall edges and the area around the compartment where the laser leveling machine cannot be used, construction personnel need to perform manual vibration.

[0035] In this embodiment, in step S7, laser signal transmitters are deployed, the pouring area is demarcated and surrounding templates are erected, and the pouring sequence is determined; laser transmitters are installed at selected locations, the elevation of the concrete surface layer is determined according to the design elevation, and the elevation of the laser leveling machine's working unit is adjusted; when mechanically pouring concrete, the material is unloaded evenly to ensure sufficient working space for the laser leveling equipment; the laser leveling machine is used to level the concrete, and the elevation of the working surface is re-checked during the leveling operation; areas that the laser leveling machine cannot operate on, such as column bases, walls, and the perimeter of compartments, are manually leveled, and the elevation is repeatedly checked.

[0036] Specifically, after concrete slurry removal and compaction of the concrete floor, excess laitance should first be scraped off and the surface adjusted to the approximate elevation. Then, a high-precision leveling operation should be performed using an intelligent laser screed. Before operation, the laser transmitter should be set up and the receiver calibrated to ensure a leveling accuracy of 2mm / 1m (i.e., a height difference of no more than 2mm within a 2-meter range). The screed should travel at a uniform speed, parallel to the direction of the armor seams, ensuring no areas are missed during overlapping. For areas such as column bases, wall edges, and armor seams—areas where the laser screed may not be operational—professional leveling personnel should use a 3m scraper to level and smooth the surface using a cross-hatching method, repeatedly checking that the elevation meets requirements to ensure consistency with the main surface. Any noticeably low-lying areas should be promptly filled with material and re-leveled.

[0037] In this embodiment, in step S7, when the concrete surface has lost most of its bleed water and leaves a slight fingerprint when lightly pressed with a finger but is not sticky, i.e., it is in the initial setting state, the specified amount of wear-resistant material is evenly spread on the initial setting concrete surface to complete the first material spreading; after the wear-resistant material absorbs a certain amount of moisture, during the rough troweling, a 6m straightedge is used to scrape the surface horizontally and vertically to check the finished surface elevation and flatness; after the straightedge scraping and checking are correct, the single-wheel grinder (with a disc) is then started to perform the first grinding and compaction operation. After the wear-resistant material hardens, a second application of the material is performed. A 6m straightedge is then used to level the surface both horizontally and vertically, and the elevation and flatness of the finished surface are checked. Finally, a dual-wheel grinder (without a disc) is started for final finishing and compaction. The grinder should be equipped with metal blades, and grinding should be done in a slow-to-fast, horizontal-to-vertical cycle for 3-4 passes. Each pass should be performed immediately after the trowel marks from the previous pass have disappeared to fully seal surface pores and improve surface density and wear resistance. Before each pass, the blade angle and grinder speed should be adjusted appropriately. Wetting the surface with water is strictly prohibited to avoid reducing surface strength or causing defects such as sanding and peeling. Areas inaccessible to the grinder, such as wall bases, column feet, sides of mounting seams, and corners, should be trimmed and smoothed using a hand trowel, working in tandem with the mechanical grinding process, to ensure the entire floor surface is uniform in color, smooth, flat, and free of trowel marks and pinholes. After the edges and corners are polished, they should be covered and cured in time to prevent the surface from drying out and cracking due to excessive water loss.

[0038] In this embodiment, in step S8, the concrete surface is covered with plastic film and felt for moisture retention and curing. During the curing period, the concrete surface should be kept moist at all times, and the curing time should be no less than 7 days. During the curing period, the strength test should be based on the test blocks cured under the same conditions left on site. Only when the measured compressive strength of the test blocks cured under the same conditions reaches 5 MPa can construction personnel be allowed to walk on the surface or perform minor surface cleaning, measurement, and other auxiliary operations. However, it is strictly forbidden to pile materials, conduct impact construction, or disturb the armored joint structure. Before the concrete compressive strength reaches 90% of the design strength standard value, it is strictly forbidden to allow any form of motor vehicle traffic, equipment movement, or ground loading. The specific time for officially opening vehicle traffic must be based on the measured compressive strength of the test blocks cured under the same conditions reaching 90% or more of the design strength grade value, and the curing age being no less than 14 days. It is strictly forbidden to prematurely lift the closure or open traffic without passing the strength test to ensure the safety and long-term durability of the floor structure.

[0039] The embodiments of a concrete floor construction method provided by the present invention have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of the present invention, and the descriptions of the embodiments above are only for the purpose of helping to understand the core ideas of the present invention. It should be noted that those skilled in the art can make several improvements and modifications to the present invention without departing from the principles of the present invention, and these improvements and modifications also fall within the protection scope of the claims of the present invention.

Claims

1. A method of constructing a concrete floor, characterized by, The construction method includes the following steps in sequence: S1. Substrate treatment: Remove debris, oil stains, laitance, and repair defects such as cracks, honeycombing, and pitting in the substrate. S2. Laying the isolation layer: Lay a layer of fine sand between the base layer and the floor surface layer, and then lay a PE film on the fine sand layer, and use tape to stick the overlaps. S3. Armor seam positioning: Armor seams are installed at the intersections of longitudinal and transverse seams or starting from the base of the wall or column and installed in sequence; the elevation is measured from the benchmark point, the theodolite is used to lay out the lines, the installation position of the armor seams and the elevation control line are marked, and the level is used to verify; S4. Adjust the armored joint: The armored joint is equipped with a pressure relief unit. Adjust the pressure threshold of the pressure relief unit according to the on-site construction conditions. S5. Welding of Armored Joints: S5.

1. Install the armored joints in sections, and tie the reinforcing mesh in sections based on the armored joints; S5.

2. Place each section of the armored joint in the correct position according to the layout line, and use an adjuster to fine-tune the height and flatness of each section independently. Use a laser level to measure and verify at both ends of the connector; S5.

3. Use short steel bars for temporary fixing of the armored joints, drive them into the foundation, and set at least four fixing points for each section of the armored joint. Weld the top of the short steel bars to the side wall of the armored joint and weld the upper layer of reinforcing mesh to the short steel bars; S6. Concrete pouring; S7. Concrete leveling, troweling, and polishing; S8. Concrete curing.

2. A method of constructing a concrete floor slab as claimed in claim 1 wherein, The armor seam includes: two vertically parallel supporting steel plates connected by adjusting bolts; movable steel plates symmetrically arranged on both sides of the supporting steel plates, the movable steel plates being able to slide along the height direction of the supporting steel plates, and a movable sleeve fitted at one end of the movable steel plate; the top and bottom ends of the supporting steel plates extending obliquely outward to form anchoring steel plates; a reserved groove is provided between the movable sleeve and the anchoring steel plates, and a pressure relief unit is provided in the reserved groove.

3. A method of constructing a concrete floor slab as claimed in claim 2 wherein, The pressure relief unit is an elastic rubber body. In step S4, the pre-compression of the high-performance elastic rubber body is changed by turning the adjusting bolt, taking into account the shrinkage and expansion of the concrete, the ambient temperature and humidity, and the heavy load level of the floor. The pre-compression of the rubber body is increased for heavy-load floors and decreased for ordinary floors.

4. The method of claim 1, wherein In step S5, the armor seams are installed in sections, with a standard length of 3m for each section. Adjacent armor seam sections are connected by spring pins and easily broken bolts, and a 1-2mm expansion gap is reserved at the top flat steel of the joint.

5. The method of claim 2, wherein In step S5, the short steel bars are driven into the foundation alternately in a vertical manner and at a 30° angle to the vertical to form a triangular stress structure, and the weld between the top of the short steel bar and the anchoring steel plate of the armor seam is ≥10cm.

6. The method of claim 1, wherein In step S5, the irregular junctions between the floor and column bases / wall bases are treated as follows: Column base joint treatment: At the junction of the floor and the steel column, prefabricated three-dimensional adjustable flexible armored joint modules are installed around the column base. The three-dimensional adjustable flexible armored joint modules are finely adjusted using three-dimensional adjusting bolts to ensure a tight fit between the module and the column base. A 10-15mm wide flexible gap is left between the three-dimensional adjustable flexible armored joint module and the column base. After the concrete surface layer is completed, polyurethane caulking is used to seal the gap to a depth of 30-50mm. For circular steel columns, the module is made of 2mm thick steel plate bent into an arc shape and installed around the column base. The arc shape of the steel plate avoids the formation of internal and external corners, effectively preventing cracking of the floor concrete at the corners. For rectangular steel columns, the module is made of 2mm thick steel plate bent into a rectangle and installed around the column base. Treatment of joints between wall base, ground rail beam and pressure beam: At the junction of the floor and the wall, ground rail beam and pressure beam, 20mm thick PE foam cotton is used for isolation, with a foam cotton height of 350mm. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Doorway joint treatment: At the junction of the hangar door and factory gate opening and the ground, prefabricated three-dimensional adjustable modules are arranged along the edge of the doorway. L50×5 galvanized angle steel is set as corner guards within a 200mm width range on both sides of the doorway. After the concrete surface layer is completed, polyurethane caulking is used with a depth of 50mm. Treatment of the top node of the manhole: A reinforcing steel mesh is added at the junction of the ground and the top of the manhole. The reinforcing steel mesh is supported by steel legs. The bottom of the legs is spot-welded to the bottom steel bars of the manhole top plate. The top of the steel mesh is 30-40mm away from the finished surface of the ground. Other irregular node treatments: including at least irregular column bases, multi-column side-by-side column bases, complex outlines of equipment foundations, and corners of trenches and pits. After cleaning the node area, set up simple templates, pour in two-component high-elasticity sealing material, and allow it to self-level and cure.

7. The method of claim 1, wherein In step S6, the garbage in the trench is cleaned a second time and rinsed with water before pouring concrete; after the concrete mixer truck arrives at the site, the concrete pouring test and slump are checked, and unloading is carried out after the requirements are met; laser leveling machine is used for compartment pouring and leveling construction. For areas around columns, walls and compartments that cannot be operated by laser leveling machine, construction personnel will manually vibrate.

8. The method of claim 1, wherein In step S7, laser signal transmitters are deployed, the pouring area is demarcated and surrounding templates are erected, and the pouring sequence is determined; laser transmitters are installed at selected locations, the elevation of the concrete surface layer is determined according to the design elevation, and the elevation of the laser leveling machine's working unit is adjusted; when mechanically pouring concrete, the material is unloaded evenly to ensure sufficient working space for the laser leveling equipment; the laser leveling machine is used to level the concrete, and the elevation of the working surface is re-checked during the leveling operation; for areas around column bases, walls, and compartments where the laser leveling machine cannot operate, manual scraping is used for leveling, and the elevation is repeatedly checked.

9. The method of claim 1, wherein In step S7, when the concrete surface has lost most of its bleed water and leaves a slight fingerprint when lightly pressed with a finger but is not sticky, indicating it is in the initial setting state, evenly spread the specified amount of wear-resistant material on the initially set concrete surface. Use a trowel to scrape the surface horizontally and vertically to level it and check the finished surface elevation and flatness. After the wear-resistant material absorbs some moisture, start the single-wheel grinder for the first grinding and compaction operation. After the wear-resistant material hardens, perform the second application of wear-resistant material, and again use a trowel to scrape the surface horizontally and vertically to check the finished surface elevation and flatness. If the trowel leveling and verification are correct, start the double-wheel grinder for the final finishing and compaction operation. The grinder should be used in a slow-to-fast, horizontal-to-vertical cycle for 3-4 passes, with each pass performed immediately after the trowel marks left by the previous pass have disappeared.

10. The method of claim 1, wherein In step S8, cover the concrete surface with plastic film and felt for moisture retention and curing. The concrete surface should be kept moist at all times during the curing period, and the curing time should not be less than 7 days.