A method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes

By measuring polarization resistance through four-point bending loading and linear polarization curves, the stress corrosion performance of sulfur-resistant pipes under high temperature and high pressure environments was quantified, solving the problem of difficult evaluation in existing technologies and realizing accurate corrosion performance assessment and life prediction.

CN123111844APending Publication Date: 2026-11-17ANGANG STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611196856.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-07
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies struggle to accurately evaluate the stress corrosion performance of sulfur-resistant pipes under high temperature and pressure conditions, especially in acidic environments containing hydrogen sulfide. They cannot effectively quantify the impact of stress corrosion, making it difficult to assess the corrosion risk of oil and gas well pipelines. Furthermore, traditional methods require stringent testing conditions and yield limited results.

Method used

The influence of applied stress on the corrosion performance of sulfur-resistant pipes was calculated based on polarization resistance. A four-point bending loading test combined with linear polarization curves was used to measure the polarization resistance of the surface under tensile and compressive stress, respectively. The stress corrosion performance index and contribution rate were calculated to quantify the influence of stress on corrosion performance.

Benefits of technology

It enables accurate evaluation of the stress corrosion resistance of sulfur-containing pipes in sulfur-containing environments, provides a theoretical basis for early corrosion prevention and life assessment, simplifies the test procedure, and improves the accuracy and reliability of measurement results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123111844A_ABST
    Figure CN123111844A_ABST
Patent Text Reader

Abstract

This invention relates to the field of stress corrosion performance testing technology for sulfur-resistant pipes, and provides a method for calculating the influence of applied stress on the corrosion performance of sulfur-resistant pipes based on polarization resistance. The method includes the following steps: processing the sample to a predetermined size, and grinding and degreasing the sample surface; subjecting the sample to a four-point bending load at a predetermined loading ratio; placing the fixture and sample together in a sealed tank for stress corrosion testing, and simultaneously conducting a first electrochemical test on the upper and lower surfaces of the sample; after completing the predetermined test cycle, conducting a second electrochemical test on the upper and lower surfaces of the unfailed sample simultaneously; analyzing the first and second electrochemical data to obtain the stress corrosion performance index and the contribution rate of bending stress to the corrosion performance of sulfur-resistant pipes. This invention provides a theoretical basis for elucidating the control mechanism of stress corrosion fracture in sulfur-resistant pipes and improving their SCC resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of stress corrosion performance detection of sulfur-resistant pipes, and in particular, relates to a method for calculating the influence degree of applied stress on the corrosion performance of sulfur-resistant pipes based on polarization resistance. Background Art

[0002] Stress Corrosion Cracking (SCC) refers to a phenomenon of delayed fracture that occurs in a metal material under tensile stress in certain specific media due to the synergistic effect of the corrosive medium and the stress, and is one of the most common and most harmful corrosion failure modes. Even materials with excellent corrosion resistance, such as stainless steels or nickel-based alloys, cannot easily avoid stress corrosion cracking in specific service environments.

[0003] In recent years, with the exploration and development of oil and gas wells in harsh environments with ultra-depth, ultra-high temperature and ultra-high corrosion, the working conditions of oil and gas wells generally feature "high temperature, high pressure, high , high , high salinity". Due to the complex and harsh working conditions coupled with special operation processes, the steels used for downhole and surface transmission pipelines are facing severe challenges. Especially during long-distance, high-temperature and high-pressure transmission, and in acidic well conditions containing hydrogen sulfide, steels for different transmission pipes need to withstand the combined effects of factors such as tensile stress, compressive stress and corrosion. For example, when serving in an oilfield downhole, the pipe string is subjected to a certain stress due to its own weight, and the swing and flutter of the oil pipe cause the inclination and bending of the pipe body, which may lead to sudden stress corrosion cracking in severe cases and cause major accidents, thus affecting the normal production and operation of the oil and gas field.

[0004] At present, the four-point bending loading test in the ASTM G39 standard is generally referenced to evaluate the stress corrosion performance of sulfur-resistant pipes. The standard solution of Method A is adopted, products that do not fracture within 720 hours are regarded as qualified, and products that fracture within 720 hours are regarded as unqualified. A 10-times magnifying glass is used to observe whether there are cracks on the surface of the unfractured sample. The test results can only provide information on failure or non-failure, and the test conditions are relatively harsh. For non-failed samples, further analysis combined with other additional tests is required to quantitatively evaluate the stress corrosion resistance of the non-failed samples. For example, the weight loss method is used to calculate the corrosion rate or corrosion weight loss of the bending-loaded sample to assist in evaluating the stress corrosion resistance of the pipes.

[0005] Normally, when a corrosion sample is not loaded, the corrosion degree of the upper surface and the lower surface is the same, and it is approximately considered that the upper surface and the lower surface contribute equally to the corrosion rate. After the corrosion sample is subjected to bending loading, the upper surface bears tensile stress and the lower surface bears compressive stress, and the stress states of the upper surface and the lower surface have different influence degrees on the corrosion rate.

[0006] Electrochemistry is a commonly used method for testing the corrosion rate and corrosion resistance of materials, characterized by its simplicity, speed, and accuracy. Examples include potentiodynamic polarization curves, Tafel curves, linear polarization curves, and electrochemical impedance spectroscopy. Among these, the linear polarization curve, by applying a very small potential change (±10mV) and measuring the change in corrosion current caused by the potential change, allows for the calculation of the material's polarization resistance. It is an important parameter in electrochemical testing, mainly used to evaluate the corrosion performance of materials.

[0007] Based on the above, in order to accurately calculate the influence of bending loading stress on the corrosion resistance of sulfur-resistant pipes, and to quantify and quickly evaluate the stress corrosion resistance of sulfur-resistant pipes, this invention is proposed to evaluate the contribution ratio of stress to the corrosion resistance of sulfur-resistant pipes based on polarization resistance. Summary of the Invention

[0008] To address the aforementioned technical issues, a method is provided that uses polarization resistance to calculate the impact of applied stress on the corrosion performance of sulfur-resistant pipes. This method aims to accurately evaluate the stress corrosion performance of sulfur-resistant pipes, further quantify the contribution of bending stress in a hydrogen sulfide environment to corrosion performance, analyze the influence of stress on stress corrosion fracture of pipes, solve the corrosion risk rating problem of pipe sections at bends in oil and gas pipelines, and contribute to early corrosion prevention and pipeline life assessment.

[0009] A method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance includes the following steps: S1: Process the specimen to the set size, and grind and degrease the surface of the specimen; according to the nominal yield strength, use a fixture to apply a four-point bending load to the specimen at the set loading ratio; S2: Place the fixture and sample as a whole into a sealed storage tank for stress corrosion resistance test, and simultaneously conduct the first electrochemical test on the upper and lower surfaces of the sample, and record the first electrochemical data; after completing the set test cycle, conduct the second electrochemical test on the upper and lower surfaces of the unfailed sample, and record the second electrochemical data; both the first and second electrochemical tests use linear polarization curves. S3: Calculate the polarization resistance of the tensile stress-loaded surface in the first electrochemical test using the first electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the first electrochemical test. The polarization resistance of the tensile stress-loaded surface in the second electrochemical experiment was calculated using the second electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the second electrochemical test. The stress corrosion performance index, the contribution rate of bending loading tensile stress to the corrosion resistance of sulfur-containing pipes, and the contribution rate of bending loading compressive stress to the corrosion resistance of sulfur-containing pipes were calculated. The stress corrosion performance index The calculation formula is:

[0010] in, The value of is related to the polarization resistance of the sample surface, and the range is 0.5~1. The contribution rate of the bending loading tensile stress to the corrosion resistance of sulfur pipes The calculation formula is:

[0011] in, For loading ratio, The stress corrosion resistance index for sulfur-resistant pipes; The contribution rate of the bending loading compressive stress to the corrosion resistance of sulfur pipes The calculation formula is:

[0012] in, For loading ratio, The stress corrosion resistance index is used for sulfur-resistant pipe materials.

[0013] Furthermore, the dimensions set in S1 are 100~120mm in length, 10~20mm in width, and 3~6mm in thickness.

[0014] Furthermore, the polishing and degreasing process in S1 includes the following steps: First, remove the burrs from the edge of the sample and polish the sample evenly with sandpaper; then clean the sample twice in acetone using an ultrasonic cleaner; finally, clean the sample once with anhydrous ethanol.

[0015] Furthermore, the protruding part between the two inner supports on the specimen is defined as the upper surface of the specimen, and the concave part corresponding to the upper surface of the specimen is defined as the lower surface of the specimen; the four-point bending loading ensures that uniform longitudinal tensile stress and compressive stress are generated on the upper and lower surfaces of the specimen, respectively, and the stress linearly decreases to zero from the inner support to the outer support on the specimen.

[0016] Furthermore, the loading ratio set in S1 is 50% to 80% of the nominal yield strength; the test period set in S2 is 360 to 720 hours.

[0017] Furthermore, the test solutions for both the first and second electrochemical tests are 5% sodium chloride solutions containing sulfur, with a pH value of 2 ≤ pH ≤ 6; the sulfur is in a gaseous state. and Any one of them, or any one of solid sodium sulfide and thiourea, or and The mixture of any one of the following is a mixture of sodium sulfide and thiourea; the first and second electrochemical tests both use a three-electrode system, with applied potentials of ±10mV and scan rates of 30mV / min.

[0018] Compared with the prior art, the present invention has the following advantages: This invention conducts electrochemical tests on bending-loaded specimens. By measuring the polarization resistance of the tensile stress-loaded surface and the compressive stress-loaded surface, the stress corrosion performance index of sulfur-resistant pipes is calculated. Through the correlation between polarization resistance and corrosion rate, the influence and contribution rate of the loading stress in the hydrogen sulfide environment on the corrosion performance of the loaded specimens are quantitatively calculated. This provides a theoretical basis for elucidating the control mechanism of stress corrosion cracking in sulfur-resistant pipes and improving their SCC resistance. This invention is simple to operate and produces accurate measurement results. Attached Figure Description

[0019] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0020] Figure 1 This is an overall flowchart of the method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to the present invention. Figure 2 This is a structural diagram of the fixture and sample in this invention under four-point bending loading. Figure 3 The first linear polarization curve of the loaded sample in Example 1 of this invention; Figure 4 This is the second linear polarization curve of the loaded sample in Example 1 of the present invention; Reference numerals: 1-sample; 2-clamp; 101-inner fulcrum; 102-outer fulcrum. Detailed Implementation

[0021] It should be noted that, unless otherwise specified, the embodiments and features described in the present invention can be combined with each other. The present invention will now be described in detail with reference to the accompanying drawings and embodiments.

[0022] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The following description of at least one exemplary embodiment is merely illustrative and is in no way intended to limit the present invention or its application or use. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0023] Example 1: like Figures 1 to 4 As shown, the method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance includes the following steps: S1: Process the specimen 1 to the set size, and grind and degrease the surface of the specimen 1; according to the nominal yield strength, use the fixture 2 to apply a four-point bending load to the specimen 1 at the set loading ratio. S2: Place the fixture 2 and the sample 1 into a sealed storage tank for stress corrosion resistance test, and simultaneously conduct the first electrochemical test on the upper and lower surfaces of the sample 1, and record the first electrochemical data; after completing the set test cycle, conduct the second electrochemical test on the upper and lower surfaces of the unfailed sample 1, and record the second electrochemical data; both the first and second electrochemical tests use linear polarization curves; S3: Calculate the polarization resistance of the tensile stress-loaded surface in the first electrochemical test using the first electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the first electrochemical test. The polarization resistance of the tensile stress-loaded surface in the second electrochemical experiment was calculated using the second electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the second electrochemical test. ; Calculate the stress corrosion performance index and the contribution rate of bending loading tensile stress to the corrosion resistance of sulfur pipes; The stress corrosion performance index The calculation formula is:

[0024] in, The value of is related to the polarization resistance of the surface of sample 1, and the range is 0.5~1; the contribution rate of the bending loading tensile stress to the corrosion resistance of the anti-sulfur pipe is % The calculation formula is:

[0025] in, For loading ratio, The stress corrosion resistance index is used for sulfur-resistant pipe materials.

[0026] The contribution rate of the bending loading compressive stress to the corrosion resistance of sulfur pipes The calculation formula is:

[0027] in, For loading ratio, The stress corrosion resistance index is used for sulfur-resistant pipe materials.

[0028] Specifically, the test period set in S2 is 360~720h to ensure that sample 1 does not fail within the test period.

[0029] In this embodiment, the dimensions set in S1 are 100~120mm in length, 10~20mm in width, and 3~6mm in thickness.

[0030] In this embodiment, the polishing and degreasing process in S1 includes the following steps: First, remove the burrs from the edge of sample 1 and polish sample 1 evenly with sandpaper; then clean sample 1 twice in acetone using an ultrasonic cleaner; finally, clean sample 1 once with anhydrous ethanol.

[0031] In this embodiment, the protruding part between the two inner support points 101 on the sample 1 is defined as the upper surface of the sample 1, and the concave part corresponding to the upper surface of the sample 1 is defined as the lower surface of the sample 1. The four-point bending loading ensures that the upper and lower surfaces of the sample 1 generate uniform longitudinal tensile stress and compressive stress, respectively. From the inner support point 101 to the outer support point 102 on the sample 1, the stress linearly decreases to zero.

[0032] In this embodiment, the loading ratio set in S1 is 50% to 80% of the nominal yield strength.

[0033] In this embodiment, the test solutions for the first and second electrochemical tests are both 5% sodium chloride solutions containing sulfur, with a pH value of 2 ≤ 6.

[0034] Specifically, sulfur can be in a gaseous state. , It may be a solid form such as sodium sulfide or thiourea, or a mixture of a gaseous and a solid substance.

[0035] In this embodiment, both the first and second electrochemical experiments used a three-electrode system, with applied potentials of ±10mV and scan rates of 30mV / min.

[0036] Specifically, the polarization resistance is inversely proportional to the corrosion current (i.e., the corrosion rate) and directly proportional to the corrosion performance. > , > .

[0037] In this embodiment, the method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance consists of four steps: sample preparation (step a), surface treatment (step b), bending loading and electrochemical testing (step c), and calculation of test results (step d).

[0038] In step a, sample 1 is processed to a size of 115mm. 15mm 5mm; In step b, first remove the edge burrs, then polish with 2000# sandpaper to achieve a surface finish of 0.3μm, and then clean with acetone twice and anhydrous ethanol once in the ultrasonic process. In step c, the bending loading test employs a four-point bending loading method, applying a load of 50% of the nominal yield strength of the well tubing. After loading, sample 1 and fixture 2 are placed as a whole into a sealed storage tank for stress corrosion resistance testing. The test solution is solution A (NACE standard) containing 1000 ppm hydrogen sulfide, pH=3. The first electrochemical test is also conducted simultaneously on both the upper and lower surfaces, and the first electrochemical data is recorded. The linear polarization curve is shown in [reference needed]. Figure 3 The slope of the curve is calculated by fitting, and the polarization resistance of the tensile stress-loaded surface is obtained. =978Ω.cm 2 Polarization resistance of the compressive stress-loaded surface =1005Ω.cm 2 After 720 hours of testing, a second electrochemical test was conducted simultaneously on the upper and lower surfaces of the unfailed sample 1. The second electrochemical data was recorded, and the linear polarization curve is shown in [reference needed]. Figure 4 The slope of the curve is calculated by fitting, and the polarization resistance of the tensile stress-loaded surface is obtained. =824Ω.cm 2 Polarization resistance of the compressive stress-loaded surface =897Ω.cm 2 ; In the calculation of the test results in step d, The value is set to 0.89, based on the stress corrosion performance index. The calculation formula and the contribution rate of bending loading tensile stress to the corrosion resistance of sulfur-containing pipes. The calculation formula and the contribution rate of bending loading compressive stress to the corrosion resistance of sulfur pipes. The calculation formula yields a stress corrosion performance index r = 0.63, indicating the contribution rate of tensile stress under bending load to the corrosion resistance of sulfur-resistant pipes. =41.57%, the contribution rate of bending loading compressive stress to the corrosion resistance of sulfur-resistant pipes =38.19%.

[0039] Therefore, it can be seen that when the loading ratio is 50%, the stress corrosion performance index of the sulfur-resistant pipe is 0.63, the contribution rate of bending loading tensile stress to the corrosion performance of the sulfur-resistant pipe is 41.57%, and the contribution rate of bending loading compressive stress to the corrosion performance of the sulfur-resistant pipe is 38.19%.

[0040] Example 2: The data results under the test environment of 5% NaCl containing sodium sulfide and pH=3 are shown in the table below:

[0041] The above test results show that when the loading ratio is 80% and the test period is 720h, the stress corrosion performance index of the sulfur-resistant pipe is 0.59, the contribution rate of bending loading tensile stress to the corrosion performance of the sulfur-resistant pipe is 72.06%, and the contribution rate of bending loading compressive stress to the corrosion performance of the sulfur-resistant pipe is 62.84%.

[0042] Example 3: The data results under the test environment of thiourea-containing 5% NaCl pH=6 are shown in the table below:

[0043] The above test results show that when the loading ratio is 80% and the test period is 720h, the stress corrosion performance index of the sulfur-resistant pipe is 0.61, the contribution rate of bending loading tensile stress to the corrosion performance of the sulfur-resistant pipe is 70.64%, and the contribution rate of bending loading compressive stress to the corrosion performance of the sulfur-resistant pipe is 61.26%.

[0044] Further analysis of the above experimental results reveals that, under the same loading ratio, the r-value is smaller in the 5% NaCl solution containing sodium sulfide (pH=3), while the r-value is larger in the 5% NaCl solution containing thiourea (pH=6). The lower pH indicates a more demanding testing environment, resulting in a lower stress corrosion performance index and a greater influence and contribution of loading stress on corrosion performance. Under the same pH conditions, as the loading ratio and test period increase, the r-value decreases, the stress corrosion performance of the sulfur-resistant pipe decreases, and the proportion and contribution of loading stress to the corrosion performance of the sulfur-resistant pipe increase.

[0045] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance, characterized in that, Includes the following steps: S1: Process the specimen (1) to the set size, grind and degrease the surface of the specimen (1); according to the nominal yield strength, use the fixture (2) to perform a four-point bending load on the specimen (1) at the set loading ratio; S2: Place the fixture (2) and the sample (1) into a sealed storage tank for stress corrosion resistance test, and conduct the first electrochemical test on the upper and lower surfaces of the sample (1) at the same time, and record the first electrochemical data; after completing the set test cycle, conduct the second electrochemical test on the upper and lower surfaces of the unfailed sample (1) at the same time, and record the second electrochemical data; the first electrochemical test and the second electrochemical test both use linear polarization curves; S3: Calculate the polarization resistance of the tensile stress-loaded surface in the first electrochemical test using the first electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the first electrochemical test. ; The polarization resistance of the tensile stress-loaded surface in the second electrochemical experiment was calculated using the second electrochemical data. And the polarization resistance of the compressive stress-loaded surface in the second electrochemical test. ; The stress corrosion performance index, the contribution rate of bending loading tensile stress to the corrosion performance of sulfur-containing pipes, and the contribution rate of bending loading compressive stress to the corrosion performance of sulfur-containing pipes were calculated. The stress corrosion performance index The calculation formula is: in, The value of is related to the polarization resistance of the surface of the sample (1), and the value range is 0.5~1; The contribution rate of the bending loading tensile stress to the corrosion resistance of sulfur pipes The calculation formula is: in, For loading ratio, The stress corrosion resistance index for sulfur-resistant pipes; The contribution rate of the bending loading compressive stress to the corrosion resistance of sulfur pipes The calculation formula is: in, For loading ratio, The stress corrosion resistance index is used for sulfur-resistant pipe materials.

2. The method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to claim 1, characterized in that, The dimensions set in S1 are 100-120mm in length, 10-20mm in width, and 3-6mm in thickness.

3. The method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to claim 1, characterized in that, The polishing and degreasing process in S1 includes the following steps: First, remove the burrs from the edge of the sample (1) and polish the sample (1) evenly with sandpaper; then clean the sample (1) twice in acetone using an ultrasonic cleaner; finally, clean the sample (1) once with anhydrous ethanol.

4. The method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to claim 1, characterized in that, The raised portion between the two inner support points (101) on the sample (1) is defined as the upper surface of the sample (1), and the recessed portion corresponding to the upper surface of the sample (1) is defined as the lower surface of the sample (1). The four-point bending load ensures that uniform longitudinal tensile stress and compressive stress are generated on the upper and lower surfaces of the specimen (1), respectively, and the stress linearly decreases to zero from the inner support (101) to the outer support (102) on the specimen (1).

5. The method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to claim 1, characterized in that, The loading ratio set in S1 is 50% to 80% of the nominal yield strength; the test period set in S2 is 360 to 720 hours.

6. The method for calculating the influence of applied stress on the corrosion resistance of sulfur-resistant pipes based on polarization resistance according to claim 1, characterized in that, The test solutions for both the first and second electrochemical tests were 5% sodium chloride solutions containing sulfur, with a pH value of 2 ≤ 6; the sulfur was in a gaseous state. and Any one of them, or any one of solid sodium sulfide and thiourea, or and Any one of them can be mixed with any one of sodium sulfide and thiourea; Both the first and second electrochemical experiments used a three-electrode system, with applied potentials of ±10mV and scan rates of 30mV / min.