Silicon-based liquid crystal structure and its preparation method
By forming a passivation layer on the side of the metal reflective layer in the silicon-based liquid crystal structure, the reliability problem caused by the side etching of the metal reflective layer during the etching process is solved, and the reliability of the structure is improved.
Patent Information
- Application Number
- CN202510622986.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-14
- Publication Date
- 2026-11-17
AI Technical Summary
Existing silicon-based liquid crystal structures are prone to lateral etching of the metal reflective layer during the etching process, forming a necked structure, which leads to tip discharge and breakdown failure, resulting in low reliability.
A passivation layer is formed on the side of the metal reflective layer to cover its side surface, thereby improving its morphology and preventing tip discharge.
By using a passivation layer covering the metal reflective layer, the reliability of the silicon-based liquid crystal structure is improved, the possibility of tip discharge is avoided, and reliability is enhanced.
Smart Images

Figure CN123113187A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and in particular to a silicon-based liquid crystal structure and its preparation method. Background Technology
[0002] Liquid Crystal on Silicon (LCOS) is a novel reflective projection structure characterized by high light utilization efficiency, small size, high aperture ratio, and mature manufacturing technology, offering significant advantages in large-screen display applications. A typical LCOS structure comprises a substrate, an adhesive layer, and a metal reflective layer (i.e., pixel electrode layer) stacked sequentially. The metal reflective layer is usually made of metals such as aluminum (AL). After forming the metal reflective layer, both the metal reflective layer and the adhesive layer are etched. However, etching the adhesive layer is challenging and can easily lead to the metal reflective layer being side-cut during the etching process, resulting in a necked-down shape. The necked-down metal reflective layer has pointed areas at both ends, which can easily cause tip discharge during subsequent reliability testing, leading to breakdown failure and low reliability. Summary of the Invention
[0003] The purpose of this application is to provide a silicon-based liquid crystal structure and its preparation method to solve the problems of existing silicon-based liquid crystal structures being easily broken down and having low reliability.
[0004] To achieve the above objectives, this application provides a silicon-based liquid crystal structure, comprising:
[0005] substrate;
[0006] A stacked structure, located on the substrate, includes an adhesive layer and a metal reflective layer stacked sequentially, wherein the metal reflective layer is necked; and,
[0007] A passivation layer covers the sides of the metal reflective layer.
[0008] Optionally, the stacked structure further includes an anti-reflective layer located on the metal reflective layer.
[0009] Optionally, each of the stacked structures has the same size and shape, and the distance between any two adjacent stacked structures is the same.
[0010] Optionally, the passivation layer is an oxide formed after the metal reflective layer is oxidized.
[0011] Optionally, the material of the adhesion layer includes titanium nitride or titanium nitride; and / or, the material of the metal reflective layer includes at least one of magnesium, aluminum, copper, titanium, tantalum, silver, zinc and gold.
[0012] This application also provides a method for preparing a silicon-based liquid crystal structure, including:
[0013] Provide substrate;
[0014] A stacked structure is formed on the substrate, the stacked structure comprising an adhesion layer and a metal reflective layer stacked sequentially, the metal reflective layer being necked in shape; and,
[0015] A passivation layer is formed on the side of the metal reflective layer.
[0016] Optionally, the step of forming the stacked structure on the substrate includes:
[0017] An adhesive material layer and a metal reflective material layer are formed sequentially stacked on the substrate; and,
[0018] The metal reflective material layer and the adhesive material layer are etched to form a dividing groove that penetrates the metal reflective material layer and the adhesive material layer. The remaining metal reflective material layer and the adhesive material layer respectively constitute the metal reflective layer and the adhesive layer. When etching the adhesive material layer, the metal reflective material layer is side-cut to make the metal reflective layer appear necked.
[0019] Optionally, after forming the metal reflective material layer, an anti-reflective material layer is also formed on the metal reflective material layer;
[0020] Before etching the metal reflective material layer and the adhesive material layer, the reflective material layer is also etched, such that the dividing groove also penetrates the reflective material layer. After etching the adhesive material layer, the remaining reflective material layer constitutes the reflective layer.
[0021] Optionally, after forming the metallic reflective material layer, the method further includes:
[0022] The top surface of the metal reflective material layer is treated with a reducing gas.
[0023] Optionally, the reducing gas includes at least one of silane, hydrogen, and carbon monoxide.
[0024] Optionally, an oxidation process is performed to oxidize the sides of the metal reflective layer to form the passivation layer.
[0025] The silicon-based liquid crystal structure provided in this application includes a substrate, a stacked structure, and a passivation layer. The stacked structure is located on the substrate, and the passivation layer includes an adhesion layer and a metal reflective layer stacked sequentially. The metal reflective layer is necked, and the passivation layer covers the sides of the metal reflective layer. This application utilizes the passivation layer to cover the sides of the metal reflective layer, improving the morphology of the metal reflective layer, avoiding the possibility of tip discharge, and improving the reliability of the silicon-based liquid crystal structure. Correspondingly, this application also provides a method for fabricating a silicon-based liquid crystal structure. Attached Figure Description
[0026] Figure 1 A flowchart illustrating the method for fabricating a silicon-based liquid crystal structure provided in this application embodiment;
[0027] Figures 2-7 A schematic diagram of the corresponding steps in the method for preparing the silicon-based liquid crystal structure provided in the embodiments of this application;
[0028] The attached figures are labeled as follows:
[0029] 100 - Substrate; 200 - Adhesive material layer; 201 - Adhesive layer; 300 - Metal reflective material layer; 301 - Metal reflective layer; 400 - Metal oxide layer; 500 - Anti-reflective material layer; 501 - Anti-reflective layer; 600 - Dividing groove; 700 - Stacked structure; 800 - Passivation layer. Detailed Implementation
[0030] The specific embodiments of this application will now be described in more detail with reference to the accompanying drawings. The advantages and features of this application will become clearer from the following description. It should be noted that the drawings are all in a very simplified form and use non-precise proportions, and are only used to facilitate and clarify the illustration of the embodiments of this application.
[0031] Figure 7 This is a schematic diagram of the silicon-based liquid crystal structure in this embodiment. Figure 7 As shown, the silicon-based liquid crystal structure includes a substrate 100, a stacked structure 700, and a passivation layer 800.
[0032] Specifically, the substrate 100 can be made of any suitable semiconductor material known to those skilled in the art, such as silicon, germanium, silicon germanide, silicon carbide, silicon-on-insulator, germanium-on-insulator, and gallium arsenide, or the substrate 100 can be a silicon substrate.
[0033] The stacked structures 700 are spaced apart on the substrate 100. Each stacked structure 700 includes an adhesive layer 201, a metal reflective layer 301, and an anti-reflective layer 501. The adhesive layer 201, the metal reflective layer 301, and the anti-reflective layer 501 are stacked sequentially on the substrate 100 from bottom to top. The adhesive layer 201 can be used to improve the adhesion between the metal reflective layer 301 and the substrate 100, and at the same time prevent the metal reflective layer 301 from undergoing electron migration during subsequent reliability testing. The metal reflective layer 301 is used to perform the main reflection function, and the anti-reflective layer 501 can improve the reflectivity.
[0034] Optionally, the material of the adhesion layer 201 includes titanium nitride or tantalum nitride, etc.; the material of the metal reflective layer 301 includes at least one of magnesium, aluminum, copper, titanium, tantalum, silver, zinc and gold, and the material of the metal reflective layer 301 is preferably aluminum; the material of the anti-reflective layer 501 can be silicon oxide and / or silicon nitride, etc., and the material of the anti-reflective layer 501 is preferably silicon oxide.
[0035] Furthermore, the thickness of the adhesive layer 201 can be 200 angstroms to 800 k angstroms, and the thickness of the metal reflective layer 301 can be greater than the thickness of the adhesive material layer 200. For example, the thickness of the metal reflective material layer 300 can be 1500 angstroms to 1700 k angstroms, and the thickness of the anti-reflective layer 501 can be 200 angstroms to 800 k angstroms.
[0036] In some embodiments, the anti-reflective layer 501 may be omitted, that is, the anti-reflective layer 501 may only include the adhesion layer 201 and the metal reflective layer 301.
[0037] The stacked structures 700 are isolated from each other by dividing slots 600. In some embodiments, in order to improve reflection uniformity and image quality, each stacked structure 700 may have the same size and shape, and the distance between two adjacent stacked structures 700 may also be the same (i.e., the width of the dividing slots 600 may also be the same).
[0038] Furthermore, the metal reflective layer 301 is necked, or it can be understood that the central region of the metal reflective layer 301 is contracted. In short, the lateral width of the metal reflective layer 301 gradually decreases from both ends to the center, forming a necked shape that is wide at both ends and narrow in the middle. The two ends of the necked metal reflective layer 301 have pointed areas, which can easily generate tip discharge during subsequent reliability testing, leading to breakdown failure.
[0039] Furthermore, the passivation layer 800 covers the side surface of the metal reflective layer 301, and the passivation layer 800 also covers the tip region of the metal reflective layer 301, thereby improving the morphology of the metal reflective layer 301, avoiding the possibility of tip discharge, and improving the reliability of the silicon-based liquid crystal structure.
[0040] In some embodiments, the passivation layer 800 is an oxide formed after the metal reflective layer 301 is oxidized. For example, if the metal reflective layer 301 is made of aluminum, the passivation layer 800 can be aluminum oxide. In some embodiments, a medium such as silicon oxide can be directly deposited on the side of the metal reflective layer 301 to serve as the passivation layer 800.
[0041] Optionally, the passivation layer 800 may be made of materials such as metal oxide, silicon oxide, or silicon nitride.
[0042] In some embodiments, the silicon-based liquid crystal structure can be a silicon-based liquid crystal display, and the stacked structure 700 may also have a liquid crystal layer, a transparent cover plate, and other structures, which will not be explained in detail here.
[0043] Based on this, this embodiment also provides a method for preparing a silicon-based liquid crystal structure. Figure 1 This is a flowchart of the method for preparing the silicon-based liquid crystal structure provided in this embodiment, as shown below. Figure 1 As shown, the method for preparing the silicon-based liquid crystal structure includes:
[0044] Step S100: Provide substrate 100;
[0045] Step S200: A stacked structure 700 arranged at intervals is formed on the substrate 100. The stacked structure 700 includes an adhesion layer 201 and a metal reflective layer 301 stacked sequentially, wherein the metal reflective layer 301 is necked in shape; and,
[0046] Step S300: A passivation layer 800 is formed on the side of the metal reflective layer 301.
[0047] Figures 2-7 This is a schematic diagram of the corresponding steps in the fabrication method of the silicon-based liquid crystal structure provided in this embodiment. Next, we will combine... Figures 2-7 The corresponding steps of the method for preparing the silicon-based liquid crystal structure provided in this embodiment will be described in detail.
[0048] like Figure 2 As shown, in step S100, the substrate 100 is provided. The substrate 100 can be made of any suitable semiconductor material well known to those skilled in the art, such as silicon, germanium, silicon germanide, silicon carbide, silicon-on-insulator, germanium-on-insulator, and gallium arsenide, or the substrate 100 can be a silicon substrate. Interconnection structures for interconnection are formed within the substrate 100.
[0049] like Figures 2-5 A stacked structure 700 is formed on the substrate 100. The following is in conjunction with... Figure 2 , Figure 3 , Figure 4 and Figure 5 The fabrication steps of the stacked structure 700 are described in detail.
[0050] like Figure 2As shown, an adhesive material layer 200 and a metal reflective material layer 300 are sequentially stacked on the substrate 100. The adhesive material layer 200 covers the top surface of the substrate 100, and the metal reflective material layer 300 covers the top surface of the adhesive material layer 200. The adhesive material layer 200 can be used to improve the adhesion between the metal reflective material layer 300 and the substrate 100, while preventing electron migration of the metal reflective material layer 300 during subsequent reliability testing.
[0051] Optionally, the material of the adhesive material layer 200 includes titanium nitride or titanium nitride, and the material of the metal reflective material layer 300 includes at least one of magnesium, aluminum, copper, titanium, tantalum, silver, zinc and gold, but is not limited thereto.
[0052] Furthermore, the thickness of the adhesive material layer 200 can be 200 angstroms to 800 k angstroms, and the thickness of the metal reflective material layer 300 can be greater than the thickness of the adhesive material layer 200. For example, the thickness of the metal reflective material layer 300 can be 1500 angstroms to 1700 k angstroms.
[0053] Please continue reading. Figure 2 After the metal reflective material layer 300 is formed, its surface is easily oxidized, forming a metal oxide layer 400 that covers the top surface of the metal reflective material layer 300. It should be noted that the metal oxide layer 400 is not intentionally formed, but rather naturally formed during the manufacturing process when the metal reflective material layer 300 comes into contact with air and is oxidized by oxygen in the air.
[0054] like Figure 3 As shown, a reducing gas is used to treat the top surface of the metal reflective material layer 300. After the reducing gas contacts the metal oxide layer 400, it reduces the metal oxide layer 400 to metal, thereby removing the metal oxide layer 400. For example, if the material of the metal reflective material layer 300 is aluminum, the material of the metal oxide layer 400 is aluminum oxide, and the reducing gas can reduce aluminum oxide to aluminum.
[0055] Optionally, the reducing gas includes at least one of silane, hydrogen, and carbon monoxide, but should not be limited thereto; the reducing gas may also be other gases with reducing properties.
[0056] like Figure 4As shown, an anti-reflective material layer 500 is formed on the metal reflective material layer 300, and the anti-reflective material layer 500 covers the top surface of the metal reflective material layer 300. The anti-reflective material layer 500 can be used to increase the reflective performance of the metal reflective material layer 300. In some embodiments, the step of forming the anti-reflective material layer 500 can be omitted.
[0057] Optionally, the material of the reflective material layer 500 may be silicon oxide and / or silicon nitride, and the thickness of the reflective material layer 500 may be 200 angstroms to 800 k angstroms.
[0058] Furthermore, such as Figures 5-6 As shown, the reflective material layer 500, the metal reflective material layer 300 and the adhesive material layer 200 are etched sequentially to form a dividing groove 600. The dividing groove 600 penetrates the reflective material layer 500, the metal reflective material layer 300 and the adhesive material layer 200, exposing the substrate 100.
[0059] Specifically, such as Figure 5 As shown, in this embodiment, a plasma etching process is used to first etch the antireflective material layer 500 and the metal reflective material layer 300. At this time, the dividing groove 600 penetrates the antireflective material layer 500 and the metal reflective material layer 300, exposing the adhesive material layer 200. It should be noted that, since the top surface of the metal reflective material layer 300 is treated with a reducing gas to remove the metal oxide layer 400 on the top surface of the metal reflective material layer 300, after etching the antireflective material layer 500, it is not necessary to etch the metal oxide layer 400, and the metal reflective material layer 300 can be directly etched, thereby reducing the etching difficulty and improving the etching efficiency.
[0060] like Figure 6 As shown, the plasma etching process continues to etch downwards along the dividing groove 600 until it penetrates the adhesive material layer 200. At this point, the dividing groove 600 will penetrate the antireflective material layer 500, the metal reflective material layer 300, and the adhesive material layer 200, exposing the substrate 100. After etching, the remaining antireflective material layer 500, the metal reflective material layer 300, and the adhesive material layer 200 respectively constitute the antireflective layer 501, the metal reflective layer 301, and the adhesive layer 201. The antireflective layer 501, the metal reflective layer 301, and the adhesive layer 201 are stacked sequentially to form the stacked structure 700. Adjacent stacked structures 700 are separated by the dividing groove 600.
[0061] Optionally, the width of the dividing grooves 600 can be equal, so that the spacing between adjacent stacked structures 700 is also equal, which can improve reflection uniformity and thus improve imaging quality. In some embodiments, the size and shape of each stacked structure 700 can also be equal, thereby further improving reflection uniformity and imaging quality.
[0062] Please continue reading. Figure 6 The etching of the adhesive material layer 200 is quite difficult. During etching, the adhesive material layer 200 is unlikely to react with the plasma gas. As the plasma continuously bombards the adhesive material layer 200, it is reflected back onto the surface of the metal reflective material layer 300, causing the metal reflective material layer 300 to be side-hollowed out, resulting in a necked-down shape for the formed metal reflective layer 301. Figure 6 As can be seen, the two ends of the necked-down metal reflective layer 301 have pointed regions. Figure 6 (The area marked by the dotted circle in the diagram) is prone to tip discharge during subsequent reliability testing, which can lead to breakdown failure and low reliability.
[0063] like Figure 7 As shown, in step S300, a passivation layer 800 is formed on the side of the metal reflective layer 301. Since the passivation layer 800 covers the side of the metal reflective layer 301, the morphology of the metal reflective layer 301 can be improved, the possibility of tip discharge can be avoided, and the reliability of the silicon-based liquid crystal structure can be improved.
[0064] In some embodiments, an oxidation process can be performed to oxidize the side surface of the metal reflective layer 301 to form the passivation layer 800. In this case, the passivation layer 800 is an oxide formed after the metal reflective layer 301 is oxidized. For example, the material of the metal reflective layer 300 is aluminum, and the material of the passivation layer 800 can be aluminum oxide. The process time of the oxidation process can be set according to actual conditions, for example, it can be 50s to 70s, ensuring that the passivation layer 800 can completely cover the tip region of the metal reflective layer 301.
[0065] In some embodiments, a medium can be deposited directly on the side of the metal reflective layer 301 to serve as the passivation layer 800.
[0066] Optionally, the passivation layer 800 may be made of materials such as metal oxide, silicon oxide, or silicon nitride.
[0067] Subsequently, structures such as liquid crystal layers and transparent cover plates can be formed on the stacked structure 700 according to specific designs, which will not be described in detail here.
[0068] In summary, the silicon-based liquid crystal structure provided in this application includes a substrate 100, a stacked structure 700, and a passivation layer 800. The stacked structure 700 is located on the substrate 100. The passivation layer 800 includes an adhesion layer 201 and a metal reflective layer 301 stacked sequentially. The metal reflective layer 301 is necked, and the passivation layer 800 covers the sides of the metal reflective layer 301. This application utilizes the passivation layer 800 to cover the sides of the metal reflective layer 301, improving the morphology of the metal reflective layer 301, avoiding the possibility of tip discharge, and improving the reliability of the silicon-based liquid crystal structure. Correspondingly, this application also provides a method for fabricating a silicon-based liquid crystal structure.
[0069] It should be noted that the various embodiments in this specification are described in a progressive manner, with each embodiment focusing on the differences from other embodiments. Similar or identical parts between embodiments can be referred to interchangeably. For the systems disclosed in the embodiments, since they correspond to the methods disclosed in the embodiments, the descriptions are relatively simple, and relevant parts can be referred to the method section.
[0070] It should also be noted that although preferred embodiments have been disclosed above, these embodiments are not intended to limit this application. Any person skilled in the art can make many possible variations and modifications to the technical solutions of this application, or modify them into equivalent embodiments, without departing from the scope of the technical solutions of this application. Therefore, any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of this application, without departing from the content of the technical solutions of this application, shall still fall within the scope of protection of the technical solutions of this application.
[0071] It should also be understood that, unless otherwise specified or indicated, the terms “first,” “second,” “third,” etc., in the specification are used only to distinguish the various components, elements, and steps in the specification, and not to indicate the logical or sequential relationships between the various components, elements, and steps.
[0072] Furthermore, it should be recognized that the terminology described herein is used only to describe particular embodiments and is not intended to limit the scope of this application. It must be noted that the singular forms “a” and “an” used herein and in the appended claims include plural bases unless the context clearly indicates otherwise. For example, a reference to “a step” or “an apparatus” means a reference to one or more steps or apparatuses, and may include secondary steps and secondary apparatuses. All conjunctions used should be understood in the broadest sense. Also, the word “or” should be understood to have the definition of logical “or” rather than logical “exclusive OR”, unless the context clearly indicates otherwise. Furthermore, implementations of the methods and / or devices in the embodiments of this application may include performing selected tasks manually, automatically, or in combination.
Claims
1. A silicon-based liquid crystal structure, characterized in that, include: substrate; A stacked structure, spaced apart on the substrate, includes an adhesive layer and a metal reflective layer stacked sequentially, wherein the metal reflective layer is necked in shape; as well as, A passivation layer covers the sides of the metal reflective layer.
2. The silicon-based liquid crystal structure as described in claim 1, characterized in that, The stacked structure further includes an anti-reflective layer, which is located on the metal reflective layer.
3. The silicon-based liquid crystal structure as described in claim 1 or 2, characterized in that, Each of the stacked structures is identical in size and shape, and the distance between any two adjacent stacked structures is the same.
4. The silicon-based liquid crystal structure as described in claim 1, characterized in that, The passivation layer is an oxide formed after the metal reflective layer is oxidized.
5. The silicon-based liquid crystal structure as described in claim 1, characterized in that, The material of the adhesion layer includes titanium nitride or titanium nitride; and / or, the material of the metal reflective layer includes at least one of magnesium, aluminum, copper, titanium, tantalum, silver, zinc and gold.
6. A method for preparing a silicon-based liquid crystal structure, characterized in that, include: Provide substrate; A stacked structure arranged at intervals is formed on the substrate, the stacked structure including an adhesion layer and a metal reflective layer stacked sequentially, the metal reflective layer being necked in shape; and, A passivation layer is formed on the side of the metal reflective layer.
7. The method for preparing a silicon-based liquid crystal structure as described in claim 6, characterized in that, The step of forming the stacked structure on the substrate includes: An adhesive material layer and a metal reflective material layer are formed sequentially stacked on the substrate; and, The metal reflective material layer and the adhesive material layer are etched to form a dividing groove that penetrates the metal reflective material layer and the adhesive material layer. The remaining metal reflective material layer and the adhesive material layer respectively constitute the metal reflective layer and the adhesive layer. When etching the adhesive material layer, the metal reflective material layer is side-cut to make the metal reflective layer appear necked.
8. The method for preparing a silicon-based liquid crystal structure as described in claim 7, characterized in that, After forming the metal reflective material layer, an anti-reflective material layer is also formed on the metal reflective material layer; Before etching the metal reflective material layer and the adhesive material layer, the reflective material layer is also etched, such that the dividing groove also penetrates the reflective material layer. After etching the adhesive material layer, the remaining reflective material layer constitutes the reflective layer.
9. The method for preparing a silicon-based liquid crystal structure as described in claim 7, characterized in that, After forming the metal reflective material layer, the method further includes: The top surface of the metal reflective material layer is treated with a reducing gas.
10. The method for preparing a silicon-based liquid crystal structure as described in claim 9, characterized in that, The reducing gas includes at least one of silane, hydrogen, and carbon monoxide.