Methods, apparatus, equipment, media, and products for modeling, curing, and simulation of variable thickness adhesive films.

By acquiring the geometric morphology of the pre-cured stringer's deformation and adjusting its position on the uncured skin, a three-dimensional variable-thickness adhesive film solid finite element model was established. This solved the consistency problem of adhesive co-curing analysis in the existing technology and enabled more accurate prediction of stiffened panel forming deformation and residual stress.

CN123116730APending Publication Date: 2026-11-17NORTHWESTERN POLYTECHNICAL UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611601545.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-16
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing numerical analysis of adhesive co-curing does not reconstruct the three-dimensional variable thickness adhesive film solid finite element model based on the actual manufacturing deformation of the pre-cured stringer, resulting in poor consistency between numerical prediction and actual manufacturing state.

Method used

By acquiring the geometric morphology of the pre-cured stringer's deformation, determining its actual deformation bonding surface, and adjusting its position on the uncured skin, a three-dimensional variable thickness adhesive film solid finite element model is established. Combined with the pre-cured stringer and the uncured skin, a thermo-chemical-mechanical coupling analysis is performed to obtain the final forming deformation and residual stress of the stiffened panel.

Benefits of technology

It improves the prediction accuracy of stiffened panel forming deformation and residual stress, ensures that the adhesive film modeling boundary comes from the actual deformed adhesive surface, avoids the simplification caused by uniform design of adhesive film thickness, and improves the consistency between numerical prediction and actual manufacturing state.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123116730A_ABST
    Figure CN123116730A_ABST
Patent Text Reader

Abstract

This application discloses a method, apparatus, equipment, medium, and product for modeling, curing, and simulating variable thickness adhesive film, relating to the field of computer simulation technology. The method includes: acquiring the free-state forming deformation geometry of a pre-cured stringer; determining its actual deformed adhesive bonding surface; placing the pre-cured stringer above the uncured skin and adjusting its overall position along the assembly normal to ensure the minimum gap in the adhesive bonding area meets the preset adhesive film thickness requirement, with the gaps in other areas determined by the forming deformation geometry; establishing a three-dimensional variable thickness adhesive film solid finite element model using the actual deformed adhesive bonding surface and the uncured skin assembly surface as boundaries; combining the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model, and the uncured skin to establish a stiffened wall panel adhesive co-curing model and establish heat transfer and load transfer connections; and conducting a thermo-chemical-mechanical sequential coupling analysis to obtain the final forming deformation and residual stress. This application can improve the consistency between numerical prediction and actual manufacturing conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of computer simulation technology, and in particular to a method, apparatus, equipment, medium and product for modeling and curing simulation of variable thickness adhesive films. Background Technology

[0002] In the co-curing process of adhesive bonding of reinforced composite panels, the pre-cured stringers are usually cured independently first, and then the pre-cured stringers, adhesive film, and uncured skin are assembled and a second curing is completed. In existing numerical analyses of adhesive co-curing, the adhesive film is often ignored or simplified as a material layer of uniform thickness with a consistent design thickness.

[0003] However, during pre-curing and demolding, the pre-cured stringer is affected by factors such as thermal expansion, curing shrinkage, and release of tooling constraints, resulting in warping and springback. This causes the actual deformation of the pre-cured stringer's adhesive surface to deviate from the ideal design position. Therefore, the actual assembly gap between the pre-cured stringer and the uncured skin will change, and the adhesive film is not of uniform thickness in the actual structure. If a uniformly thick adhesive film is still used for modeling, it will be difficult to accurately reflect the actual bonding state.

[0004] Therefore, the main problem with the existing technology is that the existing adhesive co-curing numerical analysis does not reconstruct the three-dimensional variable thickness adhesive film entity finite element model based on the actual manufacturing deformation of the pre-cured stringer and participate in the subsequent adhesive co-curing analysis, resulting in poor consistency between numerical prediction and actual manufacturing state. Summary of the Invention

[0005] The purpose of this application is to provide a method, apparatus, equipment, medium and product for modeling, curing and simulating variable thickness adhesive film. It can establish a three-dimensional finite element model of the variable thickness adhesive film based on the actual manufacturing deformation of the pre-cured stringer, and enable the model to participate in the adhesive co-curing analysis, so as to improve the prediction accuracy of the forming deformation and residual stress of the stiffened wall panel.

[0006] To achieve the above objectives, this application provides the following solution: In a first aspect, this application provides a method for modeling and simulating the curing of variable thickness adhesive films, including: Obtain the geometric morphology of the pre-cured stringer under free state of molding deformation; Based on the described molding deformation geometry, the actual deformation bonding surface of the pre-cured stringer is determined; The pre-cured stringer is placed above the uncured skin, and the overall position of the pre-cured stringer is adjusted along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection. The actual deformed adhesive bonding surface of the pre-cured stringer after assembly and positioning is taken as the upper boundary of the adhesive film, and the uncured skin assembly surface is taken as the lower boundary of the adhesive film. The upper boundary and lower boundary of the adhesive film are used as the boundaries of the solid model to establish a three-dimensional variable thickness adhesive film solid finite element model. By combining the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin, a stiffened wall panel adhesive co-curing model is established. The connection relationship for heat transfer and mechanical load is established between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin. A thermo-chemical-mechanical sequential coupling analysis was conducted on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

[0007] Optionally, obtaining the molding deformation geometry of the pre-cured stringer in a free state specifically includes: A finite element model of the pre-cured stringer was established based on the actual geometric configuration and ply design of the pre-cured stringer. Based on the material properties of the pre-cured stringer and the first curing process, the curing process was analyzed. The temperature and curing state of the pre-cured stringer during the curing process were calculated in the thermochemical analysis, and the degree of curing at each time point was updated based on the material curing kinetics. The temperature history obtained from thermochemical analysis is transferred to the mechanical model in the form of a predefined field for mechanical analysis, and the material state is updated according to the temperature and degree of curing. In the mechanical analysis, the total strain is decomposed into elastic strain, thermal strain and chemical shrinkage strain. Within each time increment of the mechanical analysis, the current mechanical state of the material is determined based on the current temperature and degree of curing, and the material stiffness parameters are updated. The elastic strain is determined, and the element stress is calculated in combination with the current material stiffness. Under given boundary constraints, the structural equilibrium equations are solved to obtain the displacements of each node and the stress of each element, thus obtaining the stress and deformation evolution of the pre-cured stringer during the heating, curing and cooling processes. After the first curing and cooling is completed, a new stress release analysis step is created. The stress, strain and deformation state of the pre-cured stringer at the end of the previous analysis step are inherited. The full displacement constraint applied to the mold surface of the pre-cured stringer during the curing stage is released. The minimum displacement constraint used to limit the translation and rotation of the overall rigid body is retained on the pre-cured stringer. Static equilibrium solution is performed to obtain the molding deformation geometry of the pre-cured stringer after demolding.

[0008] Optionally, determining the actual deformation bonding surface of the pre-cured stringer based on the molded deformation geometry specifically includes: The deformed geometry is taken as the manufacturing state of the pre-cured stringer. The deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is extracted from the manufacturing state, and the deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is taken as the actual deformed adhesive surface of the pre-cured stringer.

[0009] Optionally, adjusting the overall position of the pre-cured stringer along the assembly normal to ensure that the minimum gap in the adhesive area meets the preset adhesive film thickness requirement specifically includes: Within the adhesive bonding area, select corresponding points on the actual deformed adhesive bonding surface of the pre-cured stringer and the uncured skin assembly surface that have the same in-plane projection position, and calculate the local gap along the assembly normal at each corresponding position. The minimum gap within the adhesive bonding area is determined based on the local gaps at each corresponding location; Based on the difference between the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness and the minimum gap, determine the signed overall translation amount of the pre-cured stringer along the assembly normal. The pre-cured stringer is rigidly translated as a whole based on the signed overall translation amount, so that the local gaps at each position after adjustment meet the requirement that the minimum gap is equal to the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness.

[0010] Optionally, the step of establishing a three-dimensional variable thickness finite element model of the adhesive film using the upper and lower boundaries of the film as the boundaries of the solid model specifically includes: Extract the actual deformation adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh after the assembly and positioning are completed; Import the actual deformed adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh into the finite element preprocessing software, keeping the node coordinates, geometric shape and relative spatial position unchanged; Using the solid mesh generation function in the finite element preprocessing software, three-dimensional solid elements are generated between the mesh of the actual deformable adhesive surface of the pre-cured stringer and the mesh of the uncured skin assembly surface according to the preset number of element layers in the thickness direction. This makes the local thickness of the three-dimensional variable thickness adhesive film solid finite element model change with the actual assembly gap between the two surfaces. The quality of the 3D solid elements is checked, and those that do not meet the quality requirements are corrected by locally adjusting the node positions or regenerating the local solid mesh.

[0011] Optionally, establishing the connection relationship for heat transfer and mechanical load transfer between the pre-cured stringer and the three-dimensional variable thickness adhesive film finite element model, and between the three-dimensional variable thickness adhesive film finite element model and the uncured skin, specifically includes: Establish binding constraints between the actual deformable adhesive bonding surface of the pre-cured stringer and the upper surface of the three-dimensional variable thickness adhesive film solid finite element model, and between the lower surface of the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin assembly surface. In each set of binding constraints, specify the interconnected master surface and slave surface respectively, so that the degrees of freedom involved in the binding remain continuous between the two surfaces; In thermochemical analysis, the binding constraints are applied to the temperature degrees of freedom on both sides of the interface, and the temperature of the subordinate surface node is kept consistent with the temperature of the corresponding position on the main surface, so as to achieve the continuity of the temperature field and the interfacial heat transfer between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin. In mechanical analysis, the binding constraint acts on the displacement degrees of freedom on both sides of the interface, so that the bound surfaces maintain displacement coordination during deformation, restrict the normal separation and tangential relative slip of the interface, and realize the continuous transfer of normal and tangential loads between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin.

[0012] Secondly, this application provides a variable thickness adhesive film modeling and curing simulation device, comprising: The forming deformation geometry acquisition unit is used to acquire the forming deformation geometry of the pre-cured stringer in a free state; The actual deformation adhesive surface determination unit is used to determine the actual deformation adhesive surface of the pre-cured stringer based on the molding deformation geometry. The assembly position determination unit is used to arrange the pre-cured stringer above the uncured skin and adjust the overall position of the pre-cured stringer along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection. The adhesive film boundary determination unit is used to take the actual deformed adhesive bonding surface of the pre-cured stringer after assembly and positioning as the upper boundary of the adhesive film and the uncured skin assembly surface as the lower boundary of the adhesive film. The adhesive film model building unit is used to establish a three-dimensional variable thickness adhesive film solid finite element model with the upper and lower boundaries of the adhesive film as the boundaries of the solid model. The co-curing model establishment unit is used to combine the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin to establish a stiffened wall panel adhesive co-curing model, and to establish the connection relationship for heat transfer and mechanical load between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin. The analysis unit is used to perform a thermo-chemical-mechanical sequential coupling analysis on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

[0013] Thirdly, this application provides a computer device, including: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the steps of the variable thickness adhesive film modeling and curing simulation method described in any one of the above.

[0014] Fourthly, this application provides a computer-readable storage medium having a computer program stored thereon, which, when executed by a processor, implements the steps of the variable thickness adhesive film modeling and curing simulation method described in any one of the above.

[0015] Fifthly, this application provides a computer program product, including a computer program that, when executed by a processor, implements the steps of the variable thickness adhesive film modeling and curing simulation method described above.

[0016] According to the specific embodiments provided in this application, the following technical effects are disclosed: This application provides a method, apparatus, equipment, medium, and product for modeling, curing, and simulating variable thickness adhesive film. By acquiring the geometric morphology of the pre-cured stringer in its free state, the geometric deviations generated during the first curing of the pre-cured stringer can be calculably incorporated into the second bonding and co-curing model, avoiding the problem of neglecting the manufacturing deformation of the pre-cured stringer in existing technologies. By determining the actual deformed bonding surface of the pre-cured stringer based on the geometric morphology of the molding deformation, the manufacturing deformation generated during the first curing can be inherited to the subsequent adhesive film modeling process, ensuring that the adhesive film modeling boundary originates from the actual deformed bonding surface, rather than the ideal design surface. By arranging the pre-cured stringer on the uncured... Above the skin, the overall position of the pre-cured stringer is adjusted along the assembly normal to ensure that the minimum gap between the actual deformed adhesive surface of the pre-cured stringer and the assembly surface of the uncured skin meets the preset adhesive film thickness requirement. Local gaps in other areas are determined by the molding deformation geometry. This approach, while meeting the minimum adhesive layer thickness requirement, preserves the influence of the actual manufacturing deformation of the pre-cured stringer on local gaps, avoiding the simplification of the adhesive bonding state caused by using a uniformly designed adhesive film thickness. By using the actual deformed adhesive surface of the pre-cured stringer after assembly positioning as the upper boundary of the adhesive film and the assembly surface of the uncured skin as the lower boundary, the adhesive film space is jointly defined by the two actual assembly surfaces, allowing the adhesive... The film thickness is no longer a uniformly specified constant, but is jointly determined by the actual deformation of the pre-cured stringer's adhesive bonding surface and the uncured skin's assembly surface after assembly and positioning. By using the upper and lower boundaries of the adhesive film as the boundaries of the solid model, a three-dimensional variable-thickness adhesive film solid finite element model can be established. This enables the establishment of a continuous analysis process between pre-cured manufacturing deformation, actual adhesive layer geometry, and secondary curing response, improving the consistency between numerical prediction and actual manufacturing conditions. By combining the pre-cured stringer, the three-dimensional variable-thickness adhesive film solid finite element model, and the uncured skin, a stiffened wall panel adhesive co-curing model is established. Establishing connections for heat transfer and mechanical load transfer between the models and between the 3D variable thickness adhesive film solid finite element model and the uncured skin enables the 3D variable thickness adhesive film solid finite element model to participate in the heat conduction, curing reaction, chemical shrinkage and stress transfer in the subsequent adhesive co-curing process, avoiding analysis distortion caused by ignoring the adhesive film or using an adhesive film of uniform thickness. By conducting thermo-chemical-mechanical sequential coupling analysis on the adhesive co-curing model of the stiffened wall panel, the final forming deformation and residual stress of the stiffened wall panel can be obtained, which can obtain the final forming deformation and residual stress of the stiffened wall panel that are more consistent with the actual manufacturing state, providing numerical basis for the adhesive co-curing manufacturing of composite material stiffened wall panels. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0018] Figure 1 A flowchart illustrating a variable thickness adhesive film modeling and curing simulation method provided in an embodiment of this application; Figure 2 A schematic diagram of the geometric morphology of the pre-cured stringer after curing deformation according to an embodiment of this application; Figure 3 A schematic diagram of the actual deformed adhesive surface of a pre-cured stringer provided in an embodiment of this application; Figure 4 This is a schematic diagram of the assembly and positioning of a pre-cured deformable stringer provided in an embodiment of this application; Figure 5 for Figure 4 Top view; Figure 6 This is a schematic diagram showing the determination of the upper and lower boundaries of the adhesive film according to an embodiment of this application. Figure 7 This is a schematic diagram of a three-dimensional solid model of a variable thickness adhesive film provided in an embodiment of this application; Figure 8 A schematic diagram of the thickness distribution of a three-dimensional solid model of a variable thickness adhesive film provided in an embodiment of this application; Figure 9 This is a schematic diagram of a finite element model of a stiffened wall panel provided in an embodiment of this application; Figure 10 A schematic diagram of the functional modules of a variable thickness adhesive film modeling and curing simulation device provided in an embodiment of this application; Figure 11 This is a schematic diagram of the structure of a computer device provided in an embodiment of this application. Detailed Implementation

[0019] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0020] To make the above-mentioned objectives, features and advantages of this application more apparent and understandable, the application will be further described in detail below with reference to the accompanying drawings and specific embodiments.

[0021] In one exemplary embodiment, such as Figure 1 As shown, a method for modeling and curing a variable thickness adhesive film is provided. This method is executed by a computer device, which can be executed by a computer device such as a terminal or a server alone, or by both a terminal and a server.

[0022] In this embodiment, a stiffened wall panel composed of a pre-cured T-shaped composite material stringer and an uncured composite material skin is used as the object. The structural forming process includes two stages: a first curing and a second curing. First, the pre-cured stringer is independently cured and formed. Then, the pre-cured stringer is assembled with the uncured skin through an adhesive film, and a second co-curing is performed.

[0023] In this embodiment, the first curing involves independently curing and shaping the pre-cured stringer. The purpose of the first curing is to allow the pre-cured stringer to complete the curing reaction and develop load-bearing capacity. However, due to factors such as thermal expansion, curing shrinkage, and release of tooling constraints, the pre-cured stringer will warp and spring back after the first curing and cooling, resulting in a deformed geometry that deviates from the ideal design position. Therefore, the first curing mainly addresses the acquisition and inheritance of the manufacturing deformation of the pre-cured stringer in subsequent modeling.

[0024] In this embodiment, the second curing involves co-curing the pre-cured stringer with the uncured skin after assembly using the adhesive film. The purpose of the second curing is to allow the adhesive film and the uncured skin to complete the curing reaction, connecting the pre-cured stringer, adhesive film, and uncured skin into a single stiffened panel. Simultaneously, the second curing process further generates thermal deformation, curing chemical shrinkage, and residual stress, ultimately forming the geometry of the stiffened panel. Therefore, the second curing primarily addresses the establishment of a three-dimensional variable-thickness adhesive film solid finite element model, the establishment of a stiffened panel adhesive co-curing model, and the sequential coupling analysis of thermo-chemical-mechanical forces in subsequent modeling.

[0025] In this embodiment, the difference between the two curing processes is as follows: the first curing is only for the pre-cured stringer, which has reached a cured state after the first curing and mainly participates in heat transfer during the second curing process; the second curing is for the overall structure composed of the pre-cured stringer, the adhesive film, and the uncured skin, wherein the adhesive film and the uncured skin undergo curing reactions and material property evolution during the second curing process, while the pre-cured stringer retains the manufacturing deformation geometry formed after the first curing.

[0026] In this embodiment, the relationship between the two curing processes is as follows: the geometric shape of the pre-cured stringer formed by the first curing is the input for the modeling of the second curing, that is, the thickness of the adhesive film in the second curing is determined by the actual assembly gap between the actual deformed adhesive surface of the pre-cured stringer and the uncured skin assembly surface; the final forming deformation and residual stress of the stiffened panel obtained after the second curing analysis are the result of the combined effect of the deformation of the first curing and the co-curing response of the adhesive bonding in the second curing.

[0027] In this embodiment of the application, the variable thickness adhesive film modeling and curing simulation method includes the following steps 101 to 106. Wherein: Step 101: Obtain the geometric shape of the pre-cured stringer in its free state.

[0028] In this embodiment, a pre-curing analysis model is established based on the pre-cured stringer structure, layup information, material properties, and the first curing process. Thermochemical and mechanical analyses are performed, and the tooling constraints are released after curing to obtain the geometric morphology of the pre-cured stringer in a free state. (See [link to relevant documentation]). Figure 2 , Figure 2 This is a schematic diagram of the geometric shape of the pre-cured stringer after curing deformation, provided in an embodiment of this application.

[0029] As an optional implementation, obtaining the molding deformation geometry of the pre-cured stringer in a free state includes: A finite element model of the pre-cured stringer was established based on the actual geometric configuration and ply design of the pre-cured stringer. Based on the material properties of the pre-cured stringer and the first curing process, the curing process was analyzed. The temperature and curing state of the pre-cured stringer during the curing process were calculated in the thermochemical analysis, and the degree of curing at each time point was updated based on the material curing kinetics. The temperature history obtained from thermochemical analysis is transferred to the mechanical model in the form of a predefined field for mechanical analysis, and the material state is updated according to the temperature and degree of curing. In the mechanical analysis, the total strain is decomposed into elastic strain, thermal strain and chemical shrinkage strain. Within each time increment of the mechanical analysis, the current mechanical state of the material is determined based on the current temperature and degree of curing, and the material stiffness parameters are updated. The elastic strain is determined, and the element stress is calculated in combination with the current material stiffness. Under given boundary constraints, the structural equilibrium equations are solved to obtain the displacements of each node and the stress of each element, thus obtaining the stress and deformation evolution of the pre-cured stringer during the heating, curing and cooling processes. After the first curing and cooling is completed, a new stress release analysis step is created. The stress, strain and deformation state of the pre-cured stringer at the end of the previous analysis step are inherited. The full displacement constraint applied to the mold surface of the pre-cured stringer during the curing stage is released. The minimum displacement constraint used to limit the translation and rotation of the overall rigid body is retained on the pre-cured stringer. Static equilibrium solution is performed to obtain the molding deformation geometry of the pre-cured stringer after demolding.

[0030] In this embodiment of the application, during thermochemical analysis, the internal temperature field of the pre-cured stringer is calculated based on the curing process, and the degree of curing at each moment is updated based on the material curing kinetics: ; In the formula, The degree of curing is dimensionless. Time, in seconds; The temperature of the material is expressed in °C. The curing reaction rate is a function determined by the material curing kinetic parameters, and the unit is seconds (s).

[0031] In the embodiments of this application, the total strain is decomposed into elastic strain, thermal strain, and chemical contraction strain in the mechanical analysis: ; In the formula, For total strain, For elastic strain, Thermal strain caused by temperature changes The strains are chemical shrinkage strains caused by changes in curing degree; all strains mentioned above are dimensionless.

[0032] This implementation method can accurately obtain the geometric shape of the pre-cured stringer in a free state based on the actual geometric configuration, layup design, material properties and first curing process of the pre-cured stringer, thus providing a basis for determining the actual deformed adhesive surface and establishing a three-dimensional variable thickness adhesive film solid finite element model that conforms to the actual manufacturing state.

[0033] Step 102: Determine the actual deformation bonding surface of the pre-cured stringer based on the formed deformation geometry.

[0034] In this embodiment, based on the deformation results of the pre-cured stringer molding, the deformed lower surface of the contact area between the pre-cured stringer edge and the adhesive film is extracted and used as the actual deformed bonding surface for subsequent adhesive film modeling. This ensures that the manufacturing deformation generated during the first curing is inherited by the subsequent adhesive co-curing model. See the actual deformed bonding surface for details. Figure 3 , Figure 3 This is a schematic diagram of the actual deformed adhesive surface of a pre-cured stringer provided in an embodiment of this application.

[0035] As an optional implementation, determining the actual deformed adhesive surface of the pre-cured stringer based on the molded deformation geometry includes: The deformed geometry is taken as the manufacturing state of the pre-cured stringer. The deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is extracted from the manufacturing state, and the deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is taken as the actual deformed adhesive surface of the pre-cured stringer.

[0036] This implementation method allows the manufacturing deformation generated during the first curing to be inherited by the subsequent adhesive co-curing model, so that the subsequent adhesive film modeling is no longer based on the ideal design surface, but on the actual deformed adhesive surface of the pre-cured stringer.

[0037] Step 103: Arrange the pre-cured stringer on top of the uncured skin, and adjust the overall position of the pre-cured stringer along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection.

[0038] In the embodiments of this application, see Figure 4 and Figure 5 , Figure 4 This is a schematic diagram of the assembly and positioning of a pre-cured deformable stringer according to an embodiment of this application. Figure 5 for Figure 4 A top view. The deformed pre-cured stringer, after its first curing, is positioned above the uncured skin according to the actual structural location. Because the pre-cured stringer has undergone manufacturing deformation, the bonded surfaces of its pre-cured stringer edges and the assembly surfaces of the uncured skin no longer maintain the equidistant relationship as designed. To establish a reasonable initial assembly state, while maintaining the curing deformation morphology of the pre-cured stringer, the overall position of the pre-cured stringer is adjusted along the structural assembly normal, ensuring that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area, except for the position corresponding to the minimum gap, are determined by the molding deformation geometry.

[0039] As an optional implementation, adjusting the overall position of the pre-cured stringer along the assembly normal includes: Within the adhesive bonding area, select corresponding points on the actual deformed adhesive bonding surface of the pre-cured stringer and the uncured skin assembly surface that have the same in-plane projection position, and calculate the local gap along the assembly normal at each corresponding position. The minimum gap within the adhesive bonding area is determined based on the local gaps at each corresponding location; Based on the difference between the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness and the minimum gap, determine the signed overall translation amount of the pre-cured stringer along the assembly normal. The pre-cured stringer is rigidly translated as a whole based on the signed overall translation amount, so that the local gaps at each position after adjustment meet the requirement that the minimum gap is equal to the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness.

[0040] In this embodiment, corresponding points with the same in-plane projection position on the actual deformed adhesive surface of the pre-cured stringer and the uncured skin assembly surface are selected within the adhesive bonding area, and the local gaps along the assembly normal at each corresponding position are calculated: ; In the formula, For the first Local gaps at corresponding locations, in mm; and These are the coordinates of the corresponding positions of the actual deformed adhesive bonding surface of the pre-cured stringer and the uncured skin assembly surface, respectively; The assembly normal unit vector pointing from the uncured skin to the precured stringer.

[0041] In this embodiment of the application, the minimum gap within the adhesive bonding area is: ; In the formula, This represents the minimum gap within the adhesive bonding area.

[0042] In this embodiment of the application, the preset nominal thickness of the adhesive film or the minimum allowable thickness of the adhesive layer is set as follows: The signed overall translation of the pre-cured stringer along the assembly normal is: ; In the formula, The signed overall translation of the pre-cured stringer along the assembly normal; This is the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness. When At that time, the pre-cured stringer moves away from the uncured skin; when At that time, the pre-cured stringer moves toward the direction of the uncured skin.

[0043] Local gaps at various locations after adjustment for: ; Thus, the adjusted minimum gap satisfy: ; In this embodiment, during the adjustment process described in step 103, only the pre-cured stringer undergoes a rigid overall translation, without altering its deformation morphology formed after the first curing. The local gaps at other locations are naturally determined by the actual manufacturing deformation of the pre-cured stringer. Since the deformation at different locations after pre-curing of the pre-cured stringer varies, while the overall translation remains consistent, the adjusted local gaps change with the bonding position, thereby forming a spatially non-uniform actual assembly gap within the bonding area of ​​the pre-cured stringer, determined by the manufacturing deformation of the pre-cured stringer.

[0044] This implementation method can retain the actual assembly gap caused by the spatial non-uniformity of the pre-cured stringer manufacturing deformation while meeting the minimum adhesive layer thickness constraint, thus providing a real geometric boundary for the subsequent three-dimensional variable thickness adhesive film solid finite element model.

[0045] Step 104: Take the actual deformed adhesive surface of the pre-cured stringer after assembly and positioning as the upper boundary of the adhesive film, and the uncured skin assembly surface as the lower boundary of the adhesive film. Use the upper boundary and lower boundary of the adhesive film as the boundaries of the solid model to establish a three-dimensional variable thickness adhesive film solid finite element model.

[0046] In this embodiment, after the pre-cured stringer is assembled and positioned, the adhesive gaps at other locations are no longer manually specified, but are naturally determined by the actual deformation morphology formed after the first curing of the pre-cured stringer. Therefore, a spatially non-uniform actual assembly gap is formed along the adhesive area of ​​the pre-cured stringer. The actual deformed lower surface of the pre-cured stringer edge after assembly and positioning is defined as the upper boundary of the adhesive film; based on the corresponding assembly position of the pre-cured stringer edge on the uncured skin, the corresponding area on the upper surface of the uncured skin is extracted and defined as the lower boundary of the adhesive film, as detailed in [reference needed]. Figure 6 Using the upper and lower boundaries of the adhesive film as the boundaries of the solid model, a three-dimensional variable thickness adhesive film solid finite element model is established between them, so that the local thickness of the adhesive film varies spatially with the actual assembly gap formed by the manufacturing deformation of the pre-cured stringer.

[0047] As an optional implementation, the step of establishing a three-dimensional variable thickness finite element model of the adhesive film, using the upper and lower boundaries of the film as the boundaries of the solid model, includes: Extract the actual deformation adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh after the assembly and positioning are completed; Import the actual deformed adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh into the finite element preprocessing software, keeping the node coordinates, geometric shape and relative spatial position unchanged; Using the solid mesh generation function in the finite element preprocessing software, three-dimensional solid elements are generated between the mesh of the actual deformable adhesive surface of the pre-cured stringer and the mesh of the uncured skin assembly surface according to the preset number of element layers in the thickness direction. This makes the local thickness of the three-dimensional variable thickness adhesive film solid finite element model change with the actual assembly gap between the two surfaces. The quality of the 3D solid elements is checked, and those that do not meet the quality requirements are corrected by locally adjusting the node positions or regenerating the local solid mesh.

[0048] In this embodiment, the actual deformed adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh are extracted after assembly and positioning. Both sets of surface meshes are imported into the Hyper Mesh finite element preprocessing software, maintaining their node coordinates, geometric shapes, and relative spatial positions. Then, using the Linear Solid mesh generation function in Hyper Mesh, three-dimensional solid elements are generated between the two sets of surface meshes according to a preset number of thickness direction element layers. This allows the local thickness of the adhesive film solid to vary with the actual assembly gap between the two surfaces, thereby obtaining a three-dimensional variable-thickness adhesive film solid finite element model. See details [link to relevant documentation]. Figure 7 and Figure 8 After the solid mesh is generated, the Check Elems function in Hyper Mesh is used to check indicators such as warpage, aspect ratio, skew, and Jacobian ratio. For elements that do not meet the quality requirements, the corresponding regions are located based on the check results, and corrections are made by locally adjusting node positions or regenerating the local solid mesh until the requirements for subsequent finite element analysis are met.

[0049] This implementation method enables the establishment of a three-dimensional variable-thickness adhesive film solid finite element model that is consistent with the actual assembly state, avoiding the simplification of the bonding state caused by ignoring the adhesive film or using a uniform thickness adhesive film.

[0050] Step 105: Combine the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model, and the uncured skin to establish a stiffened wall panel adhesive co-curing model, and establish the connection relationship for heat transfer and mechanical load transfer between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model, and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin.

[0051] In the embodiments of this application, see Figure 9The pre-cured stringer after the first curing, the aforementioned three-dimensional variable-thickness adhesive film finite element model, and the uncured skin are combined to form a reinforced wall panel adhesive co-curing model. The pre-cured stringer retains the actual deformation geometry and cured material state formed during the first curing; the adhesive film uses a three-dimensional variable-thickness adhesive film finite element model determined by the actual assembly gaps; and the uncured skin maintains the uncured material state before the second curing begins. Connections enabling the transfer of heat and mechanical loads are established between the pre-cured stringer and the adhesive film, as well as between the adhesive film and the uncured skin.

[0052] As an optional implementation, establishing the connection relationship for heat transfer and mechanical load transfer between the pre-cured stringer and the three-dimensional variable thickness adhesive film finite element model, and between the three-dimensional variable thickness adhesive film finite element model and the uncured skin, includes: Establish binding constraints between the actual deformable adhesive bonding surface of the pre-cured stringer and the upper surface of the three-dimensional variable thickness adhesive film solid finite element model, and between the lower surface of the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin assembly surface. In each set of binding constraints, specify the interconnected master surface and slave surface respectively, so that the degrees of freedom involved in the binding remain continuous between the two surfaces; In thermochemical analysis, the binding constraints are applied to the temperature degrees of freedom on both sides of the interface, and the temperature of the subordinate surface node is kept consistent with the temperature of the corresponding position on the main surface, so as to achieve the continuity of the temperature field and the interfacial heat transfer between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin. In mechanical analysis, the binding constraint acts on the displacement degrees of freedom on both sides of the interface, so that the bound surfaces maintain displacement coordination during deformation, restrict the normal separation and tangential relative slip of the interface, and realize the continuous transfer of normal and tangential loads between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin.

[0053] In this embodiment, within the Abaqus Interaction module, binding constraints are established between the actual deformable adhesive surface of the pre-cured stringer and the upper surface of the 3D variable thickness adhesive film finite element model, and between the lower surface of the 3D variable thickness adhesive film finite element model and the uncured skin assembly surface. Each binding constraint specifies the interconnected primary and secondary surfaces, ensuring continuity of the binding degrees of freedom between the two surfaces. In thermochemical analysis, the binding constraints act on the temperature degrees of freedom on both sides of the interface, ensuring that the temperature of the secondary surface nodes matches the temperature at the corresponding position on the primary surface. This guarantees the continuity of the temperature field between the pre-cured stringer, the 3D variable thickness adhesive film finite element model, and the uncured skin, and enables interface heat transfer. In mechanical analysis, the binding constraints act on the displacement degrees of freedom on both sides of the interface, ensuring that the bound surfaces maintain displacement coordination during deformation, restricting normal separation and tangential relative slippage, thereby achieving continuous transfer of normal and tangential loads between the pre-cured stringer, the 3D variable thickness adhesive film finite element model, and the uncured skin. This allows the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model, and the uncured skin to participate together in the subsequent adhesive bonding and co-curing process.

[0054] This implementation method enables the finite element model of the three-dimensional variable thickness adhesive film to participate in the heat conduction, curing reaction, chemical shrinkage and stress transfer in the subsequent adhesive co-curing process, thereby achieving a continuous correlation between the pre-cured stringer manufacturing deformation, the actual adhesive layer geometry and the adhesive co-curing response.

[0055] Step 106: Perform a thermo-chemical-mechanical sequential coupling analysis on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

[0056] In this embodiment, based on the second adhesive co-curing process, a time-varying curing temperature boundary condition is applied to the stiffened wall panel adhesive co-curing model, which consists of a pre-cured stringer, a three-dimensional variable-thickness adhesive film finite element model, and an uncured skin, for thermochemical analysis. The pre-cured stringer adopts the material state after the first curing and mainly participates in heat transfer within the structure during the second curing process. For the adhesive film and uncured skin, the curing state during the second curing process is calculated based on the curing kinetics of their respective materials. Within each time increment, the curing reaction rate is calculated based on the current temperature and the degree of curing in the previous increment, and the current degree of curing is updated in conjunction with the time increment. The updated degree of curing is passed as a state variable to the next time increment, thereby gradually obtaining the evolution of the degree of curing throughout the entire curing process. Simultaneously, the influence of the exothermic curing reaction on the temperature field is considered based on the curing reaction rate. This yields the temperature history of the stiffened wall panel adhesive co-curing model during the second curing process, as well as the curing states of the adhesive film and uncured skin.

[0057] In this embodiment, after completing the thermochemical analysis, the obtained temperature history is transferred to the mechanical model as a predefined temperature field, and the curing state of the adhesive film and uncured skin is updated according to the imported temperature history. For the adhesive film and uncured skin, the thermal expansion, curing chemical shrinkage, and material property evolution generated during the second curing process are considered; for the precured stringer, the manufacturing deformation geometry formed after the first curing is retained, and the thermodynamic response caused by the second thermal cycle is considered. Thus, the stress and deformation of the stiffened panel adhesive co-curing model during the heating, curing, and cooling processes are calculated. After the second curing and cooling are completed, the tooling constraints are released, obtaining the final forming geometry and residual stress distribution of the stiffened panel in its free state.

[0058] In this embodiment of the application, the manufacturing deformation formed by the first curing of the pre-cured stringer is continuously transferred to the second curing model of the adhesive film geometry and bonding through the above implementation process, so that the adhesive film thickness in the second curing analysis is determined by the actual manufacturing state, rather than using a uniform ideal design thickness.

[0059] By implementing steps 101 to 106 above, this application, through obtaining the molding deformation geometry of the pre-cured stringer in a free state, can calculably incorporate the geometric deviations generated during the first curing of the pre-cured stringer into the second adhesive co-curing model, avoiding the problem of prior art ignoring the manufacturing deformation of the pre-cured stringer; by determining the actual deformation adhesive surface of the pre-cured stringer based on the molding deformation geometry, the manufacturing deformation generated during the first curing can be inherited to the subsequent adhesive film modeling process, ensuring that the adhesive film modeling boundary originates from the actual deformation adhesive surface, rather than the ideal design surface; by retaining the influence of the actual manufacturing deformation of the pre-cured stringer on local gaps while meeting the minimum adhesive layer thickness requirement, it can avoid the simplification of the adhesive state caused by using an adhesive film with a uniform design thickness; by having the adhesive film space jointly defined by two actual assembly surfaces, it can... This allows the adhesive film thickness to no longer be a uniformly specified constant, but rather determined jointly by the actual deformed adhesive surface of the pre-cured stringer after assembly and positioning, and the uncured skin assembly surface. By establishing a three-dimensional variable-thickness adhesive film solid finite element model, a continuous analysis process can be established between pre-cured manufacturing deformation, actual adhesive layer geometry, and secondary curing response, improving the consistency between numerical prediction and actual manufacturing conditions. By involving the three-dimensional variable-thickness adhesive film solid finite element model in the subsequent adhesive co-curing process of heat conduction, curing reaction, chemical shrinkage, and stress transfer, analysis distortions caused by ignoring the adhesive film or using an adhesive film of uniform thickness can be avoided. By conducting thermo-chemical-mechanical sequential coupling analysis, the final forming deformation and residual stress of the stiffened panel that are more consistent with the actual manufacturing conditions can be obtained, providing numerical basis for the adhesive co-curing manufacturing of composite stiffened panel.

[0060] Based on the same inventive concept, this application also provides a variable thickness adhesive film modeling and curing simulation device for implementing the variable thickness adhesive film modeling and curing simulation method described above. The solution provided by this device is similar to the solution described in the above method. Therefore, the specific limitations in one or more embodiments of the variable thickness adhesive film modeling and curing simulation device provided below can be found in the limitations of the variable thickness adhesive film modeling and curing simulation method described above, and will not be repeated here.

[0061] In one exemplary embodiment, such as Figure 10 As shown, a variable thickness adhesive film modeling and curing simulation device is provided, comprising: The molding deformation geometry acquisition unit 201 is used to acquire the molding deformation geometry of the pre-cured stringer in a free state. Actual Deformation Bonding Surface Determination Unit 202 is used to determine the actual deformation bonding surface of the pre-cured stringer based on the molding deformation geometry. Assembly position determination unit 203 is used to arrange the pre-cured stringer above the uncured skin and adjust the overall position of the pre-cured stringer along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection. The adhesive film boundary determination unit 204 is used to take the actual deformed adhesive surface of the pre-cured stringer after assembly and positioning as the upper boundary of the adhesive film and the uncured skin assembly surface as the lower boundary of the adhesive film. The adhesive film model building unit 205 is used to build a three-dimensional variable thickness adhesive film solid finite element model with the upper boundary and lower boundary of the adhesive film as the solid model boundary. The co-curing model establishment unit 206 is used to combine the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin to establish a stiffened wall panel adhesive co-curing model, and to establish the connection relationship for heat transfer and mechanical load between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin. Analysis unit 207 is used to perform thermo-chemical-mechanical sequential coupling analysis on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

[0062] In one exemplary embodiment, a computer device is provided, which may be a server or a terminal, and its internal structure diagram may be as follows. Figure 11As shown, the computer device includes a processor, memory, input / output (I / O) interfaces, and a communication interface. The processor, memory, and I / O interfaces are connected via a system bus, and the communication interface is also connected to the system bus via the I / O interfaces. The processor provides computational and control capabilities. The memory includes non-volatile storage media and internal memory. The non-volatile storage media stores the operating system, computer programs, and a database. The internal memory provides the environment for the operation of the operating system and computer programs stored in the non-volatile storage media. The database stores simulation data for modeling and curing variable thickness adhesive films. The I / O interfaces are used for exchanging information between the processor and external devices. The communication interface is used for communication with external terminals via a network connection. When the computer program is executed by the processor, it implements a method for modeling and curing variable thickness adhesive films.

[0063] Those skilled in the art will understand that Figure 11 The structure shown is merely a block diagram of a portion of the structure related to the present application and does not constitute a limitation on the computer device to which the present application is applied. Specific computer devices may include more or fewer components than those shown in the figure, or combine certain components, or have different component arrangements.

[0064] In one exemplary embodiment, a computer device is also provided, including a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the steps in the above-described method embodiments.

[0065] In one exemplary embodiment, a computer-readable storage medium is provided storing a computer program that, when executed by a processor, implements the steps in the above-described method embodiments.

[0066] In one exemplary embodiment, a computer program product is provided, including a computer program that, when executed by a processor, implements the steps in the above-described method embodiments.

[0067] It should be noted that the user information (including but not limited to user device information, user personal information, etc.) and data (including but not limited to data used for analysis, data stored, data displayed, etc.) involved in this application are all information and data authorized by the user or fully authorized by all parties, and the collection, use and processing of the relevant data must comply with relevant regulations.

[0068] Those skilled in the art will understand that all or part of the processes in the above embodiments can be implemented by a computer program instructing related hardware. The computer program can be stored in a non-volatile computer-readable storage medium. When executed, the computer program can include the processes of the embodiments described above. Any references to memory, databases, or other media used in the embodiments provided in this application can include at least one of non-volatile and volatile memory. Non-volatile memory can include read-only memory (ROM), magnetic tape, floppy disk, flash memory, optical memory, high-density embedded non-volatile memory, resistive random access memory (ReRAM), magnetic random access memory (MRAM), ferroelectric random access memory (FRAM), phase change memory (PCM), graphene memory, etc. Volatile memory can include random access memory (RAM) or external cache memory, etc. By way of illustration and not limitation, RAM can take many forms, such as Static Random Access Memory (SRAM) or Dynamic Random Access Memory (DRAM).

[0069] The databases involved in the embodiments provided in this application may include at least one type of relational database and non-relational database. Non-relational databases may include, but are not limited to, blockchain-based distributed databases. The processors involved in the embodiments provided in this application may be general-purpose processors, central processing units, graphics processing units, digital signal processors, programmable logic devices, quantum computing-based data processing logic devices, etc., and are not limited to these.

[0070] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0071] This document uses specific examples to illustrate the principles and implementation methods of this application. The descriptions of the above embodiments are only for the purpose of helping to understand the methods and core ideas of this application. Furthermore, those skilled in the art will recognize that, based on the ideas of this application, there will be changes in the specific implementation methods and application scope. Therefore, the content of this specification should not be construed as a limitation of this application.

Claims

1. A method of modeling and curing simulation of variable thickness adhesive film, characterized in that, The variable thickness adhesive film modeling and curing simulation method includes: Obtain the geometric morphology of the pre-cured stringer under free state of molding deformation; Based on the described molding deformation geometry, the actual deformation bonding surface of the pre-cured stringer is determined; The pre-cured stringer is placed above the uncured skin, and the overall position of the pre-cured stringer is adjusted along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection. The actual deformed adhesive bonding surface of the pre-cured stringer after assembly and positioning is taken as the upper boundary of the adhesive film, and the uncured skin assembly surface is taken as the lower boundary of the adhesive film. The upper boundary and lower boundary of the adhesive film are used as the boundaries of the solid model to establish a three-dimensional variable thickness adhesive film solid finite element model. By combining the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin, a stiffened wall panel adhesive co-curing model is established. The connection relationship for heat transfer and mechanical load is established between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin. A thermo-chemical-mechanical sequential coupling analysis was conducted on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

2. The variable thickness adhesive film modeling and curing simulation method of claim 1, wherein, The acquisition of the pre-cured stringer's geometric morphology under free state of molding deformation specifically includes: A finite element model of the pre-cured stringer was established based on the actual geometric configuration and ply design of the pre-cured stringer. Based on the material properties of the pre-cured stringer and the first curing process, the curing process was analyzed. The temperature and curing state of the pre-cured stringer during the curing process were calculated in the thermochemical analysis, and the degree of curing at each time point was updated based on the material curing kinetics. The temperature history obtained from thermochemical analysis is transferred to the mechanical model in the form of a predefined field for mechanical analysis, and the material state is updated according to the temperature and degree of curing. In the mechanical analysis, the total strain is decomposed into elastic strain, thermal strain and chemical shrinkage strain. Within each time increment of the mechanical analysis, the current mechanical state of the material is determined based on the current temperature and degree of curing, and the material stiffness parameters are updated. The elastic strain is determined, and the element stress is calculated in combination with the current material stiffness. Under given boundary constraints, the structural equilibrium equations are solved to obtain the displacements of each node and the stresses of each element, thus obtaining the stress and deformation evolution of the pre-cured stringer during the heating, curing and cooling processes. After the first curing and cooling is completed, a new stress release analysis step is created. The stress, strain and deformation state of the pre-cured stringer at the end of the previous analysis step are inherited. The full displacement constraint applied to the mold surface of the pre-cured stringer during the curing stage is released. The minimum displacement constraint used to limit the translation and rotation of the overall rigid body is retained on the pre-cured stringer. Static equilibrium solution is performed to obtain the molding deformation geometry of the pre-cured stringer after demolding.

3. The variable thickness adhesive film modeling and curing simulation method of claim 1, wherein, The step of determining the actual deformation bonding surface of the pre-cured stringer based on the formed deformation geometry specifically includes: The deformed geometry is taken as the manufacturing state of the pre-cured stringer. The deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is extracted from the manufacturing state, and the deformed lower surface of the area where the bottom edge strip of the pre-cured stringer contacts the adhesive film is taken as the actual deformed adhesive surface of the pre-cured stringer.

4. The variable thickness adhesive film modeling and curing simulation method of claim 1, wherein, The adjustment of the overall position of the pre-cured stringer along the assembly normal to ensure that the minimum gap in the adhesive area meets the preset adhesive film thickness requirement specifically includes: Within the adhesive bonding area, select corresponding points on the actual deformed adhesive bonding surface of the pre-cured stringer and the uncured skin assembly surface that have the same in-plane projection position, and calculate the local gap along the assembly normal at each corresponding position. The minimum gap within the adhesive bonding area is determined based on the local gaps at each corresponding location; Based on the difference between the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness and the minimum gap, determine the signed overall translation amount of the pre-cured stringer along the assembly normal. The pre-cured stringer is rigidly translated as a whole based on the signed overall translation amount, so that the local gaps at each position after adjustment meet the requirement that the minimum gap is equal to the preset nominal thickness of the adhesive film or the minimum allowable adhesive layer thickness.

5. The variable thickness adhesive film modeling and curing simulation method of claim 1, wherein, The establishment of a three-dimensional variable-thickness finite element model of the adhesive film, using the upper and lower boundaries of the film as the boundaries of the solid model, specifically includes: Extract the actual deformation adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh after the assembly and positioning are completed; Import the actual deformed adhesive surface mesh of the pre-cured stringer and the uncured skin assembly surface mesh into the finite element preprocessing software, keeping the node coordinates, geometric shape and relative spatial position unchanged; Using the solid mesh generation function in the finite element preprocessing software, three-dimensional solid elements are generated between the mesh of the actual deformable adhesive surface of the pre-cured stringer and the mesh of the uncured skin assembly surface according to the preset number of element layers in the thickness direction. This makes the local thickness of the three-dimensional variable thickness adhesive film solid finite element model change with the actual assembly gap between the two surfaces. The quality of the 3D solid elements is checked, and those that do not meet the quality requirements are corrected by locally adjusting the node positions or regenerating the local solid mesh.

6. The variable thickness adhesive film modeling and curing simulation method of claim 1, wherein, The establishment of connections for heat transfer and mechanical load transfer between the pre-cured stringer and the 3D variable thickness adhesive film finite element model, and between the 3D variable thickness adhesive film finite element model and the uncured skin, specifically includes: Establish binding constraints between the actual deformable adhesive bonding surface of the pre-cured stringer and the upper surface of the three-dimensional variable thickness adhesive film solid finite element model, and between the lower surface of the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin assembly surface. In each set of binding constraints, specify the interconnected master surface and slave surface respectively, so that the degrees of freedom involved in the binding remain continuous between the two surfaces; In thermochemical analysis, the binding constraints are applied to the temperature degrees of freedom on both sides of the interface, and the temperature of the subordinate surface node is kept consistent with the temperature of the corresponding position on the main surface, so as to achieve the continuity of the temperature field and the interfacial heat transfer between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin. In mechanical analysis, the binding constraint acts on the displacement degrees of freedom on both sides of the interface, so that the bound surfaces maintain displacement coordination during deformation, restrict the normal separation and tangential relative slip of the interface, and realize the continuous transfer of normal and tangential loads between the pre-cured stringer, the three-dimensional variable thickness film solid finite element model and the uncured skin.

7. A variable thickness adhesive film modeling cure simulation apparatus, comprising: The variable thickness adhesive film modeling and curing simulation device includes: The forming deformation geometry acquisition unit is used to acquire the forming deformation geometry of the pre-cured stringer in a free state; The actual deformation adhesive surface determination unit is used to determine the actual deformation adhesive surface of the pre-cured stringer based on the molding deformation geometry. The assembly position determination unit is used to arrange the pre-cured stringer above the uncured skin and adjust the overall position of the pre-cured stringer along the assembly normal so that the minimum gap in the bonding area meets the preset adhesive film thickness requirement. The gaps in the bonding area other than the position corresponding to the minimum gap are determined by the molding deformation geometry. The bonding area is the area where the actual deformed bonding surface of the pre-cured stringer and the assembly surface of the uncured skin overlap in the in-plane projection. The adhesive film boundary determination unit is used to take the actual deformed adhesive bonding surface of the pre-cured stringer after assembly and positioning as the upper boundary of the adhesive film and the uncured skin assembly surface as the lower boundary of the adhesive film. The adhesive film model building unit is used to establish a three-dimensional variable thickness adhesive film solid finite element model with the upper and lower boundaries of the adhesive film as the boundaries of the solid model. The co-curing model establishment unit is used to combine the pre-cured stringer, the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin to establish a stiffened wall panel adhesive co-curing model, and to establish the connection relationship for heat transfer and mechanical load between the pre-cured stringer and the three-dimensional variable thickness adhesive film solid finite element model and between the three-dimensional variable thickness adhesive film solid finite element model and the uncured skin. The analysis unit is used to perform thermo-chemical-mechanical sequential coupling analysis on the adhesive co-curing model of the stiffened wall panel to obtain the final forming deformation and residual stress of the stiffened wall panel.

8. A computer device comprising: A memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that the processor executes the computer program to implement the steps of the variable thickness adhesive film modeling and curing simulation method according to any one of claims 1-6.

9. A computer readable storage medium having stored thereon a computer program, characterized in that, When the computer program is executed by a processor, it implements the steps of the variable thickness adhesive film modeling and curing simulation method as described in any one of claims 1-6.

10. A computer program product comprising a computer program, characterized in that, When the computer program is executed by a processor, it implements the steps of the variable thickness adhesive film modeling and curing simulation method as described in any one of claims 1-6.