A concrete production process management system and method based on recycled aggregates

By combining online detection, mix proportion adjustment, and early monitoring modules, the problem of aggregate composition fluctuation in recycled aggregate concrete production was solved, achieving continuity of batch mixture performance and accuracy of design requirements, and improving the precision and quality control of the production process.

CN123120088APending Publication Date: 2026-11-17YICHENG COUNTY YONGXIN CONSTR SERVICES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611190768.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-06
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In traditional recycled aggregate concrete production management systems, the batch correlation between aggregate composition fluctuations and early hydration data, acoustic characteristic data, and long-term performance measurement data is discontinuous, causing the performance of batch mixtures to deviate from design requirements.

Method used

An online detection module is used to detect the sulfur content of recycled aggregates. Combined with a mix proportion adjustment module and an early monitoring module, batch correlation is performed using hydration exothermic curves and acoustic characteristic data. A feedback correction module adjusts parameters to form a closed-loop correction relationship, ensuring the continuity of raw material testing, early performance characterization, and long-term validation.

Benefits of technology

This enables continuity in raw material testing and performance characterization during the production of recycled aggregate concrete, preventing batch mixtures from deviating from design requirements and improving the accuracy and quality control of the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120088A_ABST
    Figure CN123120088A_ABST
Patent Text Reader

Abstract

This invention relates to the field of concrete production management technology, specifically to a concrete production process management system and method based on recycled aggregates. The system includes: an online detection module for obtaining the sulfur content of recycled aggregates and associating it with batch aggregate information; a mix proportion adjustment module for determining a standard mix proportion based on strength grade and determining the addition parameters of mineral admixtures and additives based on sulfur content to form a compensated mix proportion; an early monitoring module for generating early performance characteristic data from hydration heat release curves and acoustic data; and a feedback correction module for adjusting the addition parameters based on long-term performance deviation data. In this invention, by associating batch aggregate information, compensated mix proportions, early performance characteristic data, and long-term performance data, the basis for mix proportion adjustment is extended from post-construction testing to raw material testing, early characterization, and long-term verification, reducing performance deviations caused by aggregate composition fluctuations.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of concrete production management technology, and in particular to a concrete production process management system and method based on recycled aggregates. Background Technology

[0002] The field of concrete production management technology mainly revolves around the management of the production process, including the recording of incoming materials such as cement, aggregates, mineral admixtures, additives, and mixing water; quality inspection; mix proportion retrieval; metering and addition; mixing and molding; curing registration; and archiving of test data. Typically, weighing devices, silos, mixers, testing instruments, production control terminals, and databases transmit raw material parameters, feeding records, mixing status, and test records batch by batch. Traditional concrete production process management systems based on recycled aggregates refer to systems that establish management records for batches of recycled coarse and fine aggregates used in concrete production. Typically, upon arrival of aggregates, the source, particle size, moisture content, gradation, and routine test results are registered. Based on the design strength grade, the water-cement ratio, cementitious material dosage, aggregate dosage, and additive dosage are selected from the mix proportion library. The production control terminal then issues the feeding sequence to the weighing hopper, powder silo, liquid admixture metering device, and mixer. After mixing, the state of the mixture, specimen number, curing age, and compressive strength test data are recorded and stored by production batch.

[0003] Traditional recycled aggregate concrete production management relies on aggregate source, particle size, moisture content, gradation, and compressive strength test records as batch basis. Mix proportion calls and metering additions depend heavily on fixed formulas and post-test block results, which do not adequately reflect changes in the sulfur content of aggregates entering the production line. The batch correlation between aggregate composition fluctuations and early hydration data, acoustic characteristic data, and long-term performance measurement data is discontinuous. The adjustment and correction of mineral admixture and additive addition parameters are lagging behind, resulting in batch mixture performance deviating from design requirements. Summary of the Invention

[0004] The purpose of this invention is to address the shortcomings of existing technologies by proposing a concrete production process management system and method based on recycled aggregates.

[0005] To achieve the above objectives, the present invention adopts the following technical solution: a concrete production process management system based on recycled aggregates includes: The online detection module is used to detect the sulfur content of recycled aggregates entering the production line, obtain the sulfur content detection value, and associate the sulfur content detection value with batch aggregate information to obtain raw material characteristic data. The mix proportion adjustment module is used to obtain the design strength grade of the target concrete, determine the standard mix proportion based on the design strength grade of the target concrete, call the sulfur content detection amount in the raw material characteristic data, determine the addition parameters of mineral admixtures and additives based on the sulfur content detection amount, adjust the standard mix proportion based on the addition parameters of mineral admixtures and additives to obtain the compensated mix proportion, and perform metering and addition according to the compensated mix proportion to obtain the compensated mixture. An early monitoring module is used to collect the hydration exothermic curve of the compensated mixture and extract its features to obtain early hydration data. At the same time, it collects acoustic data and extracts its features to obtain acoustic feature data. The early hydration data and acoustic feature data are batch-correlated with the raw material feature data and the compensated mix ratio to obtain early performance feature data. The feedback correction module is used to perform performance tests on concrete test blocks formed from the compensated mixture after curing to a set age, obtain the measured long-term performance data of the batch corresponding to the early performance characteristic data, calculate the long-term performance deviation data based on the measured long-term performance data and the long-term performance threshold, and adjust the addition parameters of mineral admixtures and additives based on the long-term performance deviation data.

[0006] As a further aspect of the present invention, the online detection module includes: The signal detection submodule is used to detect recycled aggregates entering the production line, read the characteristic X-ray signals output by the online X-ray fluorescence analyzer, extract sulfur element peak data from the characteristic X-ray signals; The content calculation submodule is used to read the preset sulfur element calibration data based on the sulfur element spectral peak data, calculate the content correspondence between the sulfur element spectral peak data and the sulfur element calibration data, and obtain the sulfur element content detection amount. The information association submodule is used to read batch aggregate information from the batch management record, associate batch identifiers based on the sulfur content detection amount and batch aggregate information, and obtain raw material characteristic data.

[0007] As a further aspect of the present invention, the process for obtaining the sulfur content detection amount is specifically as follows: Read the sulfur element peak intensity in the sulfur element peak data, and read the preset sulfur element calibration data, which includes the sulfur element peak intensity range and the sulfur element mass percentage calibration value. The intensity of the sulfur element spectral peak is compared with the intensity range of the sulfur element spectral peak, and the corresponding sulfur element mass percentage calibration value is read. The corresponding sulfur element mass percentage calibration value is used as the sulfur element content detection quantity.

[0008] As a further aspect of the present invention, the proportion adjustment module includes: The mix proportion determination submodule is used to obtain the design strength grade of the target concrete, read the preset strength grade mix proportion table, match it with the strength grade mix proportion table according to the design strength grade, and obtain the standard mix proportion. The strength grade mix proportion table contains the mapping relationship between the strength grade identifier and the corresponding benchmark dosage of each component of cement, mineral admixtures, aggregates, water and admixtures. The parameter filtering submodule is used to read the sulfur content detection amount in the raw material characteristic data, read the preset sulfur content detection amount range table and the addition parameter correspondence table. The addition parameter correspondence table contains the mapping relationship between the sulfur content detection amount range and the corresponding mineral admixture addition amount and additive adjustment amount. The sulfur content detection amount is compared with the sulfur content detection amount range table to determine the sulfur content detection amount range. The addition parameters of the mineral admixture and additive are obtained by filtering the sulfur content detection amount range in the addition parameter correspondence table. The proportioning adjustment submodule is used to adjust the amount of cement and admixture added in the standard mix proportion based on the addition parameters of the mineral admixture and admixture, and write the amount of mineral admixture added in the addition parameters of the mineral admixture and admixture into the standard mix proportion to obtain the compensated mix proportion, and perform metering and addition according to the compensated mix proportion to obtain the compensated mixture.

[0009] As a further aspect of the present invention, the process of obtaining the compensation mix ratio is specifically as follows: Read the cement dosage and admixture dosage in the standard mix proportion, and read the mineral admixture addition amount and admixture adjustment amount in the mineral admixture and admixture addition parameters. The mineral admixture addition amount is the amount of mineral admixture that replaces part of the cement, and the admixture adjustment amount is the increase in admixture dosage relative to the standard mix proportion. Calculate the difference between the cement dosage and the mineral admixture dosage to obtain the adjusted cement dosage; calculate the sum of the admixture dosage and the adjusted admixture dosage to obtain the adjusted admixture dosage. The adjusted cement dosage, mineral admixture dosage, and admixture dosage are written into the standard mix proportion to obtain the compensated mix proportion.

[0010] As a further aspect of the present invention, the early monitoring module includes: The hydration extraction submodule is used to sample the compensated mixture, collect the hydration exothermic curve, extract the exothermic peak value and peak time in the hydration exothermic curve, and obtain early hydration data. The acoustic extraction submodule is used to perform acoustic monitoring on concrete test blocks formed from the compensated mixture during a preset early curing stage, collect acoustic data, extract frequency components and energy distribution from the acoustic data, and obtain acoustic feature data. The feature association submodule is used to perform batch association based on the early hydration data, the acoustic feature data, the raw material feature data, and the compensation mix ratio to obtain early performance feature data.

[0011] As a further aspect of the present invention, the process of acquiring the acoustic feature data is specifically as follows: Acoustic data generated by concrete test blocks formed from the compensated mixture during a preset early curing stage are monitored using acoustic sensors, and preset acoustic frequency ranges and preset acoustic energy thresholds are read. Frequency components and energy distribution are extracted from the acoustic data. Acoustic signals whose frequency components are within the acoustic frequency range are selected. The signal energy of the selected acoustic signals is compared with the acoustic energy threshold. The occurrence time, duration and maximum energy of acoustic signals that exceed the acoustic energy threshold are extracted to obtain the acoustic feature data.

[0012] As a further aspect of the present invention, the feedback correction module includes: The test block testing submodule is used to perform performance tests on concrete test blocks formed from the compensated mixture after curing to a set age, read the batch identifier in the early performance characteristic data, and obtain the long-term performance test data associated with the batch identifier. The interval aggregation submodule is used to read the sulfur content detection amount in the raw material characteristic data, read the preset sulfur content detection amount interval table, compare the sulfur content detection amount with the sulfur content detection amount interval table, determine the sulfur content detection amount interval, and aggregate the long-term performance measured data according to the sulfur content detection amount interval to obtain performance interval aggregation data. The deviation calculation submodule is used to read a preset long-term performance threshold based on the performance interval aggregation data. The long-term performance threshold is the lower limit of the performance value of the corresponding intensity level. The module calculates the difference between the long-term performance value in the performance interval aggregation data and the long-term performance threshold to obtain long-term performance deviation data. The parameter adjustment submodule is used to read the preset allowable deviation range based on the long-term performance deviation data, compare the deviation in the long-term performance deviation data with the allowable deviation range, filter the sulfur content detection range where the deviation exceeds the allowable deviation range, and adjust the addition parameters of mineral admixtures and additives according to the sulfur content detection range.

[0013] As a further aspect of the present invention, the adjustment process of the addition parameters of the mineral admixture and additives is specifically as follows: Read the deviation value and sulfur content detection range in the long-term performance deviation data, and read the preset allowable deviation range and preset parameter adjustment step size. The allowable deviation range includes the lower limit of deviation, and the parameter adjustment step size includes the adjustment step size of mineral admixture dosage and the adjustment step size of additive dosage. The deviation value is compared with the lower limit of the deviation value, and the sulfur content detection range with the deviation value less than the lower limit of the deviation value is selected. The mineral admixture dosage is increased according to the adjustment step size of the mineral admixture dosage, and the additive addition parameters corresponding to the sulfur content detection range are increased according to the adjustment step size of the additive dosage, so as to obtain the adjusted mineral admixture and additive addition parameters.

[0014] A method for managing the concrete production process based on recycled aggregates, wherein the method is executed based on the aforementioned concrete production process management system based on recycled aggregates, and includes the following steps: S1: Detect the sulfur content of the recycled aggregate entering the production line, obtain the sulfur content detection amount, and correlate the sulfur content detection amount with the batch aggregate information to obtain raw material characteristic data; S2: Obtain the design strength grade of the target concrete, determine the standard mix proportion based on the design strength grade of the target concrete, call the sulfur content detection amount in the raw material characteristic data, determine the addition parameters of mineral admixtures and additives based on the sulfur content detection amount, adjust the standard mix proportion based on the addition parameters of mineral admixtures and additives to obtain the compensation mix proportion, and perform metering and addition according to the compensation mix proportion to obtain the compensated mixture; S3: Collect the hydration exothermic curve of the compensated mixture and extract its features to obtain early hydration data. At the same time, collect acoustic data and extract its features to obtain acoustic feature data. Batch-associate the early hydration data and acoustic feature data with the raw material feature data and the compensated mix ratio to obtain early performance feature data. S4: After the concrete test blocks formed from the compensated mixture are cured to a set age, performance tests are conducted to obtain the measured long-term performance data of the batch corresponding to the early performance characteristic data. The long-term performance deviation data is calculated based on the measured long-term performance data and the long-term performance threshold, and the addition parameters of mineral admixtures and additives are adjusted based on the long-term performance deviation data.

[0015] Compared with the prior art, the advantages and positive effects of the present invention are as follows: In this invention, the online detection module associates the sulfur content detection of recycled aggregate entering the production line with batch aggregate information. The mix proportion adjustment module determines the addition parameters of mineral admixtures and additives based on the design strength grade and sulfur content detection, so that the compensated mix proportion is formed based on the raw material characteristic data. The early monitoring module incorporates the hydration exothermic curve characteristics and acoustic characteristics into the batch record. The feedback correction module adjusts the addition parameters based on the deviation between the measured long-term performance data and the threshold, so that a closed-loop correction relationship is formed between raw material detection, early performance characterization and long-term verification, avoiding the batch mixture performance from deviating from the design requirements. Attached Figure Description

[0016] Figure 1 This is a schematic diagram of the structure of the concrete production process management system based on recycled aggregate of the present invention; Figure 2 This is a schematic diagram of the workflow of the concrete production process management system based on recycled aggregate of the present invention. Figure 3 This is a schematic diagram of the online detection module of the present invention; Figure 4 This is a schematic diagram of the feedback correction module of the present invention; Figure 5 This is a schematic diagram of the concrete production process management method based on recycled aggregates according to the present invention. Detailed Implementation

[0017] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.

[0018] This embodiment provides a concrete production process management system based on recycled aggregates. The system is applied to the following processes after recycled aggregates enter the production line: raw material testing, mix proportion determination, component metering and addition, mixture formation, specimen molding, early performance monitoring, long-term performance testing, and feedback correction of addition parameters.

[0019] Each batch of recycled aggregate entering the production line corresponds to a batch aggregate information entry. The batch aggregate information includes at least a batch identifier used to distinguish different batches of recycled aggregate. Sulfur content detection, standard mix proportion, compensated mix proportion, early hydration data, acoustic characteristic data, and long-term performance measurement data are all associated with the corresponding batch identifier, creating a continuous data flow relationship between the raw material status, production process, early performance status, and long-term performance status of the same batch.

[0020] Please see Figure 1 and Figure 2The concrete production process management system based on recycled aggregates includes an online detection module, a mix proportion adjustment module, an early monitoring module, and a feedback correction module. Raw material characteristic data generated by the online detection module is transmitted to the mix proportion adjustment module, the early monitoring module, and the feedback correction module; compensated mix proportions and corresponding information of the compensated mixture generated by the mix proportion adjustment module are transmitted to the early monitoring module and the feedback correction module; early performance characteristic data generated by the early monitoring module are transmitted to the feedback correction module; and adjusted mineral admixture and additive dosage parameters generated by the feedback correction module are returned to the mix proportion adjustment module for use in subsequent batches.

[0021] Please see Figure 1 , Figure 2 and Figure 3 The online detection module is used to detect the sulfur content of recycled aggregate entering the production line, obtain the sulfur content detection value, and correlate the sulfur content detection value with batch aggregate information to obtain raw material characteristic data. The online detection module includes a signal detection submodule, a content calculation submodule, and an information correlation submodule.

[0022] The signal detection submodule is used to read the characteristic X-ray signals output by the online X-ray fluorescence analyzer after detecting the recycled aggregate entering the production line. When the recycled aggregate passes through the detection area of ​​the online X-ray fluorescence analyzer, different elements produce characteristic X-rays corresponding to their element types. These characteristic X-ray signals form corresponding spectral lines according to different energy positions. Sulfur forms a sulfur peak at the corresponding spectral line position, and the intensity of the sulfur peak has a pre-established correspondence with the sulfur content in the recycled aggregate through calibration.

[0023] The signal detection submodule extracts sulfur peaks from the characteristic X-ray signal according to preset sulfur spectral line positions. The peak extraction process first determines the peak region corresponding to sulfur, then reads the sulfur peak intensity from this region, and excludes signal components located at other element spectral line positions to obtain sulfur peak data. This sulfur peak data, carrying the batch identifier of the current recycled aggregate batch, the sulfur peak position, and the sulfur peak intensity, serves as input to the content calculation submodule.

[0024] After reading the characteristic X-ray signal, the signal detection submodule checks the signal integrity and data format. When the characteristic X-ray signal is complete, can be parsed, and the peak region corresponding to sulfur can be identified, the sulfur peak data is output. If the characteristic X-ray signal is missing, the signal format cannot be parsed, the sulfur peak position cannot be identified, or the peak data does not correspond to the current batch identifier, the sulfur peak data is not output, and an anomaly is recorded for the current batch.

[0025] If an anomaly is detected, the characteristic X-ray signal output from the online X-ray fluorescence analyzer is reread, and the sulfur element peak extraction is repeated. If complete and resolvable sulfur element peak data still cannot be formed after re-detection, the current batch is stopped from entering the proportion adjustment process to prevent sulfur content measurements without a reliable source from being used in determining subsequent dosing parameters.

[0026] The content calculation submodule is used to read sulfur element peak data and preset sulfur element calibration data, and to obtain the sulfur element content detection amount based on the content correspondence between the sulfur element peak data and the sulfur element calibration data. The sulfur element calibration data includes the sulfur element peak intensity range and the corresponding sulfur element mass percentage calibration value for each sulfur element peak intensity range.

[0027] Sulfur calibration data is generated before online detection. During the generation of sulfur calibration data, characteristic X-ray detection is performed on calibration objects with known sulfur content. The peak intensities of sulfur spectral data for each calibration object are extracted, and a correspondence is established between these peak intensities and the corresponding sulfur mass percentage calibration values. Sulfur peak intensities with continuous correspondence are organized into sulfur peak intensity intervals, and each sulfur peak intensity interval, along with its corresponding sulfur mass percentage calibration value, is written into the sulfur calibration data.

[0028] The content calculation submodule reads the sulfur element peak intensity from the sulfur element spectral peak data and compares it sequentially with the sulfur element peak intensity ranges in the sulfur element calibration data. When the sulfur element peak intensity falls within a sulfur element peak intensity range, the corresponding sulfur element mass percentage calibration value is read, and the read sulfur element mass percentage calibration value is used as the sulfur element content detection amount for the current batch.

[0029] When the sulfur element peak intensity is located at the common boundary of adjacent sulfur element peak intensity intervals, a unique sulfur element peak intensity interval is determined according to the pre-defined boundary assignment rules in the sulfur element calibration data. When the sulfur element peak intensity does not fall into any sulfur element peak intensity interval, one sulfur element peak intensity corresponds to multiple conflicting calibration values, or the sulfur element calibration data cannot be resolved, no sulfur element content detection value is generated, and the process returns to the sulfur element peak extraction process for re-detection or waits for the sulfur element calibration data to be corrected.

[0030] The information association submodule is used to read batch aggregate information from the batch management record and compare the batch identifier carried by the sulfur content detection quantity with the batch identifier in the batch aggregate information. If the batch identifiers match, the sulfur content detection quantity is written into the corresponding batch aggregate information to obtain raw material characteristic data.

[0031] Raw material characteristic data uses batch identifiers as a correlation index, carrying batch aggregate information and sulfur content detection quantities. This raw material characteristic data is transmitted to the mix proportion adjustment module to determine the addition parameters of mineral admixtures and additives; it is also transmitted to the early monitoring module and feedback correction module to establish batch correspondences between early performance data, long-term performance data, and the sulfur content of recycled aggregates.

[0032] Raw material characteristic data will not be generated when batch management records are missing, batch identifier formats are inconsistent, one sulfur content detection quantity corresponds to multiple batches, or the sulfur content detection quantity cannot be located in the batch management record. After completing the supplementation of batch management records, standardizing batch identifier formats, or eliminating duplicate batch relationships, batch identifier comparison will be performed again. Raw material characteristic data will only be output when a unique correspondence is formed.

[0033] Please see Figure 1 and Figure 2 The mix proportion adjustment module is used to obtain the design strength grade of the target concrete, determine the standard mix proportion based on the design strength grade, retrieve the sulfur content detection value from the raw material characteristic data, determine the addition parameters of mineral admixtures and additives based on the sulfur content detection value, adjust the standard mix proportion based on the addition parameters of mineral admixtures and additives to obtain the compensated mix proportion, and perform metered addition according to the compensated mix proportion to obtain the compensated mixture. The mix proportion adjustment module includes a mix proportion determination submodule, a parameter screening submodule, and a mix proportion adjustment submodule.

[0034] The mix design submodule is used to obtain the design strength grade of the target concrete from the current production task record and read the preset strength grade mix design table. The strength grade mix design table includes strength grade identifiers and the corresponding baseline dosages of cement, mineral admixtures, aggregates, water, and additives for each strength grade identifier.

[0035] The strength grade mix proportion table is generated before the production task is executed. When generating the strength grade mix proportion table, the determined design strength grade is used as the retrieval identifier, and the benchmark dosage of each component of cement, mineral admixtures, aggregates, water and additives corresponding to the design strength grade is written into the same mix proportion record, so that each design strength grade corresponds to a benchmark mix proportion relationship that can be read by the production process.

[0036] The mix proportion determination submodule matches the design strength grade in the current production task with the strength grade identifier in the strength grade mix proportion table. When a mix proportion record with a matching strength grade identifier is found, the baseline dosage of each component in that mix proportion record is read to obtain the standard mix proportion. The standard mix proportion is associated with the batch identifier of the current production batch and serves as the basis for subsequent adjustments to the cement dosage, mineral admixture dosage, and additive dosage.

[0037] When the design strength grade is missing, the strength grade identifier format is inconsistent, the corresponding mix proportion record is not found, or there are multiple conflicting mix proportion records corresponding to the same design strength grade, the standard mix proportion will not be output. After the production task record is checked, the strength grade identifier is unified, or the mix proportion record is confirmed, the matching operation will be performed again.

[0038] The parameter filtering submodule is used to read the sulfur content detection value from the raw material characteristic data, and to read the preset sulfur content detection value interval table and the dosing parameter correspondence table. The sulfur content detection value interval table consists of multiple consecutive sulfur content status intervals, which are used to classify the sulfur content detection values ​​of different batches into the corresponding sulfur content detection value intervals.

[0039] The dosage parameter correspondence table includes the mapping relationship between the sulfur content detection range and the dosage of mineral admixtures and the adjustment amount of additives. The dosage of mineral admixtures represents the amount of mineral admixtures used to replace part of the cement in the standard mix proportion, and the adjustment amount of additives represents the amount added to the standard mix proportion's additive dosage. The dosage of mineral admixtures and the adjustment amount of additives together constitute the dosage parameters for mineral admixtures and additives.

[0040] The parameter filtering submodule compares the sulfur content detection value of the current batch with the interval boundaries in the sulfur content detection value interval table to determine the unique corresponding sulfur content detection value interval. Then, using the determined sulfur content detection value interval as the search term, it reads the corresponding mineral admixture dosage and additive adjustment amount from the addition parameter correspondence table to obtain the addition parameters for the mineral admixture and additives.

[0041] When the sulfur content detection value falls within the common boundary of adjacent intervals, a unique corresponding interval is determined according to the pre-set boundary assignment rules in the sulfur content detection value interval table. When the sulfur content detection value does not fall into any interval, there is no corresponding record in the addition parameter correspondence table, or multiple conflicting addition parameters are associated with the same interval, the addition parameters for mineral admixtures and additives are not output until the sulfur content detection value interval table or the addition parameter correspondence table is calibrated.

[0042] The mix proportion adjustment submodule is used to read the cement dosage and admixture dosage in the standard mix proportion, and to read the mineral admixture addition amount and admixture adjustment amount in the mineral admixture and admixture addition parameters.

[0043] The mineral admixture is used to replace a portion of the cement in the standard mix proportion. The mix proportion adjustment submodule deducts the portion corresponding to the mineral admixture from the cement dosage in the standard mix proportion to obtain the adjusted cement dosage. This process maintains the correspondence between the mineral admixture dosage and the replaced cement dosage, allowing the source of the cement dosage reduction to be traced in the compensation mix proportion.

[0044] The admixture adjustment amount represents the increase in admixture dosage relative to the standard mix proportion. The mix proportion adjustment submodule combines the admixture dosage in the standard mix proportion with the admixture adjustment amount according to the addition relationship to obtain the adjusted admixture dosage.

[0045] The mix proportion adjustment submodule writes the adjusted cement dosage, mineral admixture dosage, and admixture dosage into the corresponding component positions in the standard mix proportion. The baseline dosages of aggregates and water that were not adjusted in the standard mix proportion are kept as they were, thus obtaining the compensated mix proportion.

[0046] The compensated mix design is linked to the current batch identifier, including the design strength grade, sulfur content detection range, cement dosage, mineral admixture dosage, aggregate dosage, water dosage, and additive dosage. The batch identifier allows for tracing the standard mix design upon which the compensated mix design is based, the sulfur content detection range, and the dosage parameters of mineral admixtures and additives.

[0047] The mix proportioning adjustment submodule metered and added cement, mineral admixtures, aggregates, water, and additives according to the compensated mix proportion, and associated the actual metering records of each component with the current batch identifier. After the metering and mixing of each component are completed, the compensated mixture is obtained.

[0048] A portion of the compensated mix was used for collecting hydration exothermic curves, and another portion was used to form concrete specimens. The formed concrete specimens were used for early acoustic monitoring and long-term performance testing after a set age, ensuring that the compensated mix proportions, early monitoring results, and long-term performance test results originated from the same batch.

[0049] When metering command transmission fails, actual metering records are missing, component addition status cannot be confirmed, or the compensation mix proportion is inconsistent with the current batch identifier, the mixing and molding process of the current batch is stopped, and the completed metering records are retained. After the metering interface is restored, records are supplemented, and batch consistency is verified, the metering and addition of the affected components are executed again; if the actual addition status cannot be confirmed, the current batch does not enter the early monitoring process.

[0050] Please see Figure 1 and Figure 2 The early monitoring module is used to collect the hydration exothermic curve of the compensated mixture and extract its features to obtain early hydration data; simultaneously, it collects acoustic data generated by concrete test blocks formed from the compensated mixture and extracts its features to obtain acoustic characteristic data; then, it performs batch correlation on the early hydration data, acoustic characteristic data, raw material characteristic data, and compensated mix proportion to obtain early performance characteristic data. The early monitoring module includes a hydration extraction submodule, an acoustic extraction submodule, and a feature correlation submodule.

[0051] The hydration extraction submodule is used to obtain monitoring samples corresponding to the current batch identifier from the compensated mixture and continuously collect the hydration exothermic curves of the monitoring samples during the early hydration process. The hydration exothermic curves record the changes in the exothermic state of the compensated mixture according to the collection time, and are used to describe the exothermic changes in the process of cement and mineral admixtures participating in the hydration reaction.

[0052] The hydration extraction submodule performs a continuity check on the hydration exothermic curve and identifies the exothermic peak region based on the curve's transition from rising to falling. The exothermic peak value represents the exothermic state when the hydration exothermic curve reaches a relatively high level, and the peak time indicates the location of the exothermic peak value in the early hydration process.

[0053] The hydration extraction submodule extracts the exothermic peak value and peak time from the hydration exothermic curve to obtain early hydration data. This early hydration data is associated with the current batch identifier and passed to the feature association submodule.

[0054] Early hydration data is not generated when the hydration exothermic curve has missing data segments, incorrect data acquisition order, unparseable curve format, or inability to identify a unique exothermic peak region. Feature extraction is performed again after completing data acquisition connection restoration, sample batch verification, and re-acquiring the hydration exothermic curve.

[0055] The acoustic extraction submodule is used to monitor the acoustic data generated by concrete specimens formed from the compensated mixture during the preset early curing stage using acoustic sensors. The acoustic data records the acoustic signals generated by the concrete specimens according to the acquisition time, and includes different frequency components and the corresponding energy distribution of each frequency component.

[0056] The acoustic extraction submodule reads the preset acoustic frequency range and acoustic energy threshold. The acoustic frequency range is used to limit the frequency region of signals participating in acoustic feature extraction, and the acoustic energy threshold is used to distinguish acoustic signals that meet the acoustic event recording conditions from background signals that do not meet the recording conditions.

[0057] The acoustic frequency range is established before early acoustic monitoring. When establishing the acoustic frequency range, frequency components corresponding to the early curing state are extracted from the confirmed early curing acoustic monitoring records of concrete test blocks, and the acoustic frequency range is determined based on the distribution boundaries of these frequency components.

[0058] The acoustic energy threshold is established before early acoustic monitoring. When establishing the acoustic energy threshold, the energy state of confirmed valid acoustic events is compared with that of background acoustic signals, and the determination boundary of acoustic events is determined based on the energy difference between valid acoustic events and background acoustic signals.

[0059] The acoustic extraction submodule extracts frequency components from the acoustic data, decomposing the mixed acoustic signal into signal components at different frequency positions and reading the energy distribution of each frequency component during acquisition. Subsequently, acoustic signals whose frequency components fall within the acoustic frequency range are selected, and the signal energy of the selected acoustic signals is compared with an acoustic energy threshold.

[0060] For acoustic signals whose energy exceeds the acoustic energy threshold, the acoustic extraction submodule extracts the occurrence time, duration, and maximum energy of the acoustic signal, and forms acoustic feature data according to the order of occurrence. The occurrence time is used to locate the occurrence position of the effective acoustic event in the early maintenance process, the duration is used to describe the continuous existence range of the effective acoustic event, and the maximum energy is used to describe the energy state when the effective acoustic event reaches a relatively high level.

[0061] Acoustic feature data is not generated when the acoustic sensor fails to return acoustic data, the acoustic data acquisition time sequence is abnormal, frequency components cannot be resolved, signal energy information is missing, or the batch identifier of the concrete specimen is inconsistent with the batch identifier of the compensated mixture. After completing the acoustic sensor connection restoration, acoustic data format correction, and batch identifier verification, acoustic data acquisition and feature extraction are performed again.

[0062] When there is no acoustic signal with energy exceeding the acoustic energy threshold within the acoustic frequency range, an acoustic feature record without valid acoustic events is formed, and complete status information of acoustic data acquisition is saved, thereby distinguishing the state of no valid acoustic events detected from the state of acoustic data acquisition failure.

[0063] The feature association submodule is used to read the batch identifiers carried by early hydration data, acoustic feature data, raw material feature data, and compensation mix proportions, and to compare the consistency of the batch identifiers. When the batch identifiers of the four types of data are consistent and all types of data pass the integrity check, the four types of data are written into the same batch performance record to obtain the early performance feature data.

[0064] Early performance characteristic data uses batch identifier as the main index, carrying sulfur content detection amount, compensation ratio, exothermic peak value, peak time, acoustic signal occurrence time, duration and maximum energy, and serves as the basis for the feedback correction module to obtain the measured performance data of the same batch over a long period.

[0065] When any type of data is missing, batch identifiers do not match, one piece of data corresponds to multiple batches, or an anomaly occurs during the association write process, complete early performance characteristic data is not output, and the data already formed is retained in the original batch record. After completing the missing data acquisition, batch identifier correction, duplicate association resolution, or association write recovery, batch association is executed again.

[0066] Please see Figure 1 , Figure 2 and Figure 4 The feedback correction module is used to perform performance tests on concrete test blocks formed from the compensated mixture after curing to a set age. It obtains long-term performance test data corresponding to the early performance characteristic data of each batch, generates long-term performance deviation data based on the long-term performance test data and long-term performance thresholds, and adjusts the dosage parameters of mineral admixtures and additives based on the long-term performance deviation data. The feedback correction module includes a test block testing submodule, an interval aggregation submodule, a deviation calculation submodule, and a parameter adjustment submodule.

[0067] The test block testing submodule is used to read the batch identifier from the early performance characteristic data and locate the concrete test blocks formed from the same batch of compensated mixture in the test block curing record based on the batch identifier. The set curing age is a pre-determined performance test curing node in the production quality record, used to determine whether the concrete test blocks have entered the long-term performance testing stage.

[0068] When the concrete test blocks reach the set age and the curing records are complete, the test block testing submodule performs performance tests on the concrete test blocks and associates the performance test results with the batch identifier of the concrete test blocks to obtain long-term performance measurement data. The long-term performance measurement data carries the long-term performance values ​​corresponding to the target concrete design strength grade, and a unique correspondence is formed between the batch identifier and the early performance characteristic data.

[0069] Long-term performance test data will not be generated if concrete test blocks are missing, batch identification cannot be identified, curing records are incomplete, concrete test blocks have not reached the set age, performance test results cannot be interpreted, or one test result corresponds to multiple batches. Long-term performance test data will be obtained again after completing test block record verification, curing status confirmation, test data supplementation, and batch relationship correction.

[0070] The interval aggregation submodule is used to read the sulfur content detection values ​​from the raw material characteristic data and to read the same sulfur content detection value interval table as the parameter filtering submodule. The interval aggregation submodule compares the sulfur content detection values ​​with the interval boundaries in the sulfur content detection value interval table in turn to determine the sulfur content detection value interval corresponding to the current batch.

[0071] The interval aggregation submodule aggregates the long-term performance measurement data according to the sulfur content detection range. The long-term performance measurement data belonging to the same sulfur content detection range are written into the corresponding interval record to obtain the performance interval aggregation data.

[0072] The performance range data is indexed by the sulfur content detection range and retains the batch identifier, design strength grade, and source of compensation mix proportion corresponding to each long-term performance value. Therefore, the feedback correction results can correspond to the same sulfur content detection range used by the mix proportion adjustment module, preventing parameter adjustment results from one range from being written into other ranges.

[0073] The deviation calculation submodule is used to read the performance range aggregated data and the preset long-age performance threshold. The long-age performance threshold is the lower limit value of the performance corresponding to the target concrete design strength grade, and its source is the correspondence record between the strength grade and the performance lower limit value that has been confirmed in the production quality requirements.

[0074] The deviation calculation submodule reads the corresponding long-term performance threshold based on the design strength level in the performance interval aggregation data, and compares the long-term performance value in the performance interval aggregation data with the long-term performance threshold. It then forms long-term performance deviation data according to the direction and degree of deviation of the long-term performance value relative to the lower limit of performance.

[0075] When the long-term performance value is lower than the long-term performance threshold, the long-term performance deviation data forms a negative deviation record; when the long-term performance value reaches or exceeds the long-term performance threshold, a non-negative deviation record is formed. Each deviation record carries the corresponding batch identifier, design strength level, and sulfur content detection range, which allows the parameter adjustment submodule to determine the corresponding range of the addition parameters that need to be adjusted.

[0076] Long-term performance deviation data will not be generated when long-term performance thresholds are missing, the design strength level corresponding to the long-term performance thresholds is inconsistent with the measured long-term performance data, the data format cannot be compared within the same category, or the performance interval aggregation data lacks source batches. Long-term performance deviation data will be generated again after completing the supplementation of long-term performance thresholds, correction of the correspondence between design strength levels, unification of data formats, and verification of batch sources.

[0077] The parameter adjustment submodule is used to read long-term performance deviation data, preset deviation tolerance ranges, and preset parameter adjustment step sizes. The deviation tolerance range is used to determine whether the dosage parameters corresponding to the current sulfur content detection range need adjustment, and must include at least the lower deviation limit. The deviation tolerance range is derived from confirmed production control records and uses the same deviation expression method as the long-term performance deviation data.

[0078] The parameter adjustment step size includes the adjustment step size for the mineral admixture dosage and the adjustment step size for the additive dosage, which are used to limit the relationship between the changes in the mineral admixture dosage and the additive dosage during a single feedback correction process. The parameter adjustment step size is derived from the adjustment rules used for single performance deviations in existing parameter correction records.

[0079] The parameter adjustment submodule compares the deviation values ​​in the long-term performance deviation data with the allowable deviation range. When the deviation value is within the allowable deviation range, the amount of mineral admixture and the adjustment amount of additives in the corresponding sulfur content detection range remain unchanged.

[0080] When the deviation value exceeds the allowable deviation range, the parameter adjustment submodule filters the sulfur content detection range corresponding to that deviation value. When the deviation value is less than the lower limit of the allowable deviation range, the mineral admixture dosage corresponding to that sulfur content detection range is increased by the adjustment step size according to the mineral admixture dosage, and the admixture addition parameter corresponding to that sulfur content detection range is increased by the adjustment step size according to the admixture dosage, thus obtaining the adjusted mineral admixture and admixture addition parameters.

[0081] The parameter adjustment submodule writes the adjusted mineral admixture dosage and additive adjustment dosage back to the records of the same sulfur content detection range in the addition parameter correspondence table, and retains the correlation between the addition parameters before adjustment, the batches from which long-term performance deviations originate, and the addition parameters after adjustment.

[0082] When the sulfur content of subsequent batches falls within the same sulfur content range, the mix proportion adjustment module reads the adjusted dosage parameters of the mineral admixtures and additives to form a new compensating mix proportion. The early performance characteristic data and long-term performance measurement data generated in the new batch are then fed back into the feedback correction module, thus establishing a production management relationship where the dosage parameter adjustment results flow back to the mix proportion adjustment process of subsequent batches.

[0083] When long-term performance deviation data lacks sulfur content detection ranges, parameter adjustment step sizes are missing, write permission verification fails, the read / write process of the dosage parameter correspondence table is abnormal, or the adjustment result cannot uniquely correspond to the original sulfur content detection range, the original dosage parameters are not overwritten. After completing permission restoration, read / write process restoration, and range consistency verification, the adjusted dosage parameters are written again. After writing is complete, the dosage parameters of the corresponding range are read again. If the read result is consistent with the adjustment result, the adjusted dosage parameters are provided to the mix proportion adjustment module.

[0084] Please see Figure 5 Based on the above-mentioned concrete production process management system based on recycled aggregates, this embodiment also provides a concrete production process management method based on recycled aggregates.

[0085] S1: Detect the recycled aggregate entering the production line, read the characteristic X-ray signal output by the online X-ray fluorescence analyzer, extract the sulfur element peak from the characteristic X-ray signal to obtain sulfur element peak data; read the sulfur element calibration data, compare the sulfur element peak intensity with the sulfur element peak intensity range, read the corresponding sulfur element mass percentage calibration value to obtain the sulfur element content detection amount; associate the sulfur element content detection amount with the batch aggregate information to obtain raw material characteristic data.

[0086] S2: Obtain the design strength grade of the target concrete, match it with the strength grade mix proportion table according to the design strength grade, and obtain the standard mix proportion; read the sulfur content detection amount in the raw material characteristic data, compare the sulfur content detection amount with the sulfur content detection amount interval table, and determine the corresponding sulfur content detection amount interval; read the mineral admixture addition amount and admixture adjustment amount from the addition parameter correspondence table according to the sulfur content detection amount interval; adjust the cement addition amount and admixture addition amount in the standard mix proportion to obtain the compensated mix proportion, and perform metering and addition according to the compensated mix proportion to obtain the compensated mixture.

[0087] S3: Sample the compensated mixture and collect the hydration exothermic curve. Extract the exothermic peak value and peak time from the hydration exothermic curve to obtain early hydration data. Perform acoustic monitoring on the concrete test blocks formed from the compensated mixture. Extract the frequency components and energy distribution from the acoustic data. Screen acoustic signals whose frequency components are within the acoustic frequency range. Extract the occurrence time, duration, and maximum energy of acoustic signals whose energy exceeds the acoustic energy threshold to obtain acoustic characteristic data. Associate the early hydration data, acoustic characteristic data, raw material characteristic data, and compensated mix proportion according to batch identifiers to obtain early performance characteristic data.

[0088] S4: After the concrete test blocks formed from the compensated mixture are cured to the set age, performance tests are conducted. The long-term performance test data of the corresponding batch are obtained according to the batch identifier in the early performance characteristic data. The long-term performance test data are collected according to the sulfur content detection range to obtain the performance range collection data. The long-term performance values ​​are compared with the long-term performance threshold of the corresponding design strength grade to obtain the long-term performance deviation data. The deviation value is compared with the allowable deviation range. For the sulfur content detection range where the deviation value is less than the lower limit of the deviation, the corresponding mineral admixture dosage and admixture addition parameters are increased, and the adjusted addition parameters are written into the addition parameter correspondence table for subsequent batches.

[0089] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention in any other way. Any person skilled in the art may make changes or modifications to the above-disclosed technical content to create equivalent embodiments that can be applied to other fields. However, any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the protection scope of the present invention.

Claims

1. A recycled aggregate based concrete production process management system, characterized by, The system includes: The online detection module is used to detect the sulfur content of recycled aggregates entering the production line, obtain the sulfur content detection value, and associate the sulfur content detection value with batch aggregate information to obtain raw material characteristic data. The mix proportion adjustment module is used to obtain the design strength grade of the target concrete, determine the standard mix proportion based on the design strength grade of the target concrete, call the sulfur content detection amount in the raw material characteristic data, determine the addition parameters of mineral admixtures and additives based on the sulfur content detection amount, adjust the standard mix proportion based on the addition parameters of mineral admixtures and additives to obtain the compensated mix proportion, and perform metering and addition according to the compensated mix proportion to obtain the compensated mixture. An early monitoring module is used to collect the hydration exothermic curve of the compensated mixture and extract its features to obtain early hydration data. At the same time, it collects acoustic data and extracts its features to obtain acoustic feature data. The early hydration data and acoustic feature data are batch-correlated with the raw material feature data and the compensated mix ratio to obtain early performance feature data. The feedback correction module is used to perform performance tests on concrete test blocks formed from the compensated mixture after curing to a set age, obtain the measured long-term performance data of the batch corresponding to the early performance characteristic data, calculate the long-term performance deviation data based on the measured long-term performance data and the long-term performance threshold, and adjust the addition parameters of mineral admixtures and additives based on the long-term performance deviation data.

2. The recycled aggregate-based concrete production process management system according to claim 1, characterized by, The online detection module includes: The signal detection submodule is used to detect recycled aggregates entering the production line, read the characteristic X-ray signals output by the online X-ray fluorescence analyzer, extract sulfur element peak data from the characteristic X-ray signals; The content calculation submodule is used to read the preset sulfur element calibration data based on the sulfur element spectral peak data, calculate the content correspondence between the sulfur element spectral peak data and the sulfur element calibration data, and obtain the sulfur element content detection amount. The information association submodule is used to read batch aggregate information from the batch management record, associate batch identifiers based on the sulfur content detection amount and batch aggregate information, and obtain raw material characteristic data.

3. The concrete production process management system based on recycled aggregates according to claim 2, characterized in that, The specific process for obtaining the sulfur content detection amount is as follows: Read the sulfur element peak intensity in the sulfur element peak data, and read the preset sulfur element calibration data, which includes the sulfur element peak intensity range and the sulfur element mass percentage calibration value. The intensity of the sulfur element spectral peak is compared with the intensity range of the sulfur element spectral peak, and the corresponding sulfur element mass percentage calibration value is read. The corresponding sulfur element mass percentage calibration value is used as the sulfur element content detection quantity.

4. The concrete production process management system based on recycled aggregates according to claim 1, characterized in that, The proportion adjustment module includes: The mix proportion determination submodule is used to obtain the design strength grade of the target concrete, read the preset strength grade mix proportion table, match it with the strength grade mix proportion table according to the design strength grade, and obtain the standard mix proportion. The strength grade mix proportion table contains the mapping relationship between the strength grade identifier and the corresponding benchmark dosage of each component of cement, mineral admixtures, aggregates, water and admixtures. The parameter filtering submodule is used to read the sulfur content detection amount in the raw material characteristic data, read the preset sulfur content detection amount range table and the addition parameter correspondence table. The addition parameter correspondence table contains the mapping relationship between the sulfur content detection amount range and the corresponding mineral admixture addition amount and additive adjustment amount. The sulfur content detection amount is compared with the sulfur content detection amount range table to determine the sulfur content detection amount range. The addition parameters of the mineral admixture and additive are obtained by filtering the sulfur content detection amount range in the addition parameter correspondence table. The proportioning adjustment submodule is used to adjust the amount of cement and admixture added in the standard mix proportion based on the addition parameters of the mineral admixture and admixture, and write the amount of mineral admixture added in the addition parameters of the mineral admixture and admixture into the standard mix proportion to obtain the compensated mix proportion, and perform metering and addition according to the compensated mix proportion to obtain the compensated mixture.

5. The concrete production process management system based on recycled aggregates according to claim 4, characterized in that, The specific process for obtaining the compensation mix ratio is as follows: Read the cement dosage and admixture dosage in the standard mix proportion, and read the mineral admixture addition amount and admixture adjustment amount in the mineral admixture and admixture addition parameters. The mineral admixture addition amount is the amount of mineral admixture that replaces part of the cement, and the admixture adjustment amount is the increase in admixture dosage relative to the standard mix proportion. Calculate the difference between the cement dosage and the mineral admixture dosage to obtain the adjusted cement dosage; calculate the sum of the admixture dosage and the adjusted admixture dosage to obtain the adjusted admixture dosage. The adjusted cement dosage, mineral admixture dosage, and admixture dosage are written into the standard mix proportion to obtain the compensated mix proportion.

6. The concrete production process management system based on recycled aggregates according to claim 1, characterized in that, The early monitoring module includes: The hydration extraction submodule is used to sample the compensated mixture, collect the hydration exothermic curve, extract the exothermic peak value and peak time in the hydration exothermic curve, and obtain early hydration data. The acoustic extraction submodule is used to perform acoustic monitoring on concrete test blocks formed from the compensated mixture during the preset early curing stage, collect acoustic data, extract frequency components and energy distribution from the acoustic data, and obtain acoustic feature data. The feature association submodule is used to perform batch association based on the early hydration data, the acoustic feature data, the raw material feature data, and the compensation mix ratio to obtain early performance feature data.

7. The concrete production process management system based on recycled aggregates according to claim 6, characterized in that, The specific process for acquiring the acoustic feature data is as follows: Acoustic data generated by concrete test blocks formed from the compensated mixture during a preset early curing stage are monitored using acoustic sensors, and preset acoustic frequency ranges and preset acoustic energy thresholds are read. Frequency components and energy distribution are extracted from the acoustic data. Acoustic signals with frequency components within the acoustic frequency range are selected. The signal energy of the selected acoustic signals is compared with the acoustic energy threshold. The occurrence time, duration, and maximum energy of acoustic signals exceeding the acoustic energy threshold are extracted to obtain the acoustic feature data.

8. The concrete production process management system based on recycled aggregates according to claim 1, characterized in that, The feedback correction module includes: The test block testing submodule is used to perform performance tests on concrete test blocks formed from the compensated mixture after curing to a set age, read the batch identifier in the early performance characteristic data, and obtain the long-term performance test data associated with the batch identifier. The interval aggregation submodule is used to read the sulfur content detection amount in the raw material characteristic data, read the preset sulfur content detection amount interval table, compare the sulfur content detection amount with the sulfur content detection amount interval table, determine the sulfur content detection amount interval, and aggregate the long-term performance measured data according to the sulfur content detection amount interval to obtain performance interval aggregation data. The deviation calculation submodule is used to read a preset long-term performance threshold based on the performance interval aggregation data. The long-term performance threshold is the lower limit of the performance value of the corresponding intensity level. The module calculates the difference between the long-term performance value in the performance interval aggregation data and the long-term performance threshold to obtain long-term performance deviation data. The parameter adjustment submodule is used to read the preset allowable deviation range based on the long-term performance deviation data, compare the deviation in the long-term performance deviation data with the allowable deviation range, filter the sulfur content detection range where the deviation exceeds the allowable deviation range, and adjust the addition parameters of mineral admixtures and additives according to the sulfur content detection range.

9. The concrete production process management system based on recycled aggregates according to claim 8, characterized in that, The specific process for adjusting the addition parameters of the mineral admixtures and additives is as follows: Read the deviation value and sulfur content detection range in the long-term performance deviation data, and read the preset allowable deviation range and preset parameter adjustment step size. The allowable deviation range includes the lower limit of deviation, and the parameter adjustment step size includes the adjustment step size of mineral admixture dosage and the adjustment step size of additive dosage. The deviation value is compared with the lower limit of the deviation value, and the sulfur content detection range with the deviation value less than the lower limit of the deviation value is selected. The mineral admixture dosage is increased according to the adjustment step size of the mineral admixture dosage, and the additive addition parameters corresponding to the sulfur content detection range are increased according to the adjustment step size of the additive dosage, so as to obtain the adjusted mineral admixture and additive addition parameters.

10. A method for managing the concrete production process based on recycled aggregates, characterized in that, The method corresponds to the concrete production process management system based on recycled aggregates as described in any one of claims 1-9, and includes the following steps: S1: Detect the sulfur content of the recycled aggregate entering the production line, obtain the sulfur content detection amount, and correlate the sulfur content detection amount with the batch aggregate information to obtain raw material characteristic data; S2: Obtain the design strength grade of the target concrete, determine the standard mix proportion based on the design strength grade of the target concrete, call the sulfur content detection amount in the raw material characteristic data, determine the addition parameters of mineral admixtures and additives based on the sulfur content detection amount, adjust the standard mix proportion based on the addition parameters of mineral admixtures and additives to obtain the compensation mix proportion, and perform metering and addition according to the compensation mix proportion to obtain the compensated mixture; S3: Collect the hydration exothermic curve of the compensated mixture and extract its features to obtain early hydration data. At the same time, collect acoustic data and extract its features to obtain acoustic feature data. Batch-associate the early hydration data and acoustic feature data with the raw material feature data and the compensated mix ratio to obtain early performance feature data. S4: After the concrete test blocks formed from the compensated mixture are cured to a set age, performance tests are conducted to obtain the measured long-term performance data of the batch corresponding to the early performance characteristic data. The long-term performance deviation data is calculated based on the measured long-term performance data and the long-term performance threshold, and the addition parameters of mineral admixtures and additives are adjusted based on the long-term performance deviation data.