A high weather-resistant flame-retardant cable for rail transit

By employing a coaxial layered structure consisting of a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a highly weather-resistant outer sheath, combined with specific processing techniques, the problems of aging, interlayer slippage, and decreased fire resistance in rail transit flame-retardant cables during long-term use have been solved, achieving higher structural stability and fire resistance.

CN123120416APending Publication Date: 2026-11-17四川营盛线缆制造有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611352423.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-02
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing flame-retardant cables for rail transit are prone to problems such as aging of the sheath material, interlayer slippage, internal damage, and decreased fire resistance during long-term use, making them difficult to meet the needs of diverse application scenarios.

Method used

It adopts a coaxial layered structure consisting of a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a high weather-resistant outer sheath. Combined with three-layer synchronous co-extrusion molding, interlocking wrapping, and segmented gradient cross-linking curing processes, a gradient protection system is formed.

Benefits of technology

It improves the structural stability and fire resistance of the cable, enhances its adaptability to different rail transit scenarios, and extends the service life of the cable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120416A_ABST
    Figure CN123120416A_ABST
Patent Text Reader

Abstract

This invention relates to the field of flame-retardant cable technology, specifically a high-weather-resistant flame-retardant cable for rail transit. It employs a coaxial layered structure from the inside out, consisting of a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a high-weather-resistant outer sheath. Each functional layer has a clearly defined role, respectively undertaking the functions of conductive transmission, electrical insulation, buffering oxygen barrier, rigid protection, and environmental weather resistance, forming a gradient protection system from the inside out. This helps to adapt to the comprehensive performance requirements of different laying scenarios in rail transit. The manufacturing method uses a raw material grading pretreatment process, conducting quality control on the raw materials for different functional layers to unify particle size accuracy, moisture content, and dispersion uniformity. This helps to reduce defects such as porosity and filler agglomeration during the molding process, improving the uniformity of material performance in each layer and the batch stability of the product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of flame-retardant cable technology, specifically a high weather-resistant flame-retardant cable for rail transit. Background Technology

[0002] As the core carrier of urban public transportation and intercity passenger transport, the reliability of the power supply, signaling, and control systems of rail transit directly affects the operational safety and service stability of the lines. The laying scenarios for rail transit cables cover a wide range, including environments such as underground tunnels and underground substations that are in a high-humidity, enclosed state for a long time, as well as elevated sections, ground lines, and open-air depots that are directly exposed to the outdoors. Some coastal and northern lines also need to withstand the long-term effects of salt spray corrosion, extreme temperature differences, and wind and sand abrasion.

[0003] At the same time, the space of rail transit is relatively enclosed and densely populated. After a fire occurs, the smoke spreads quickly and the escape is difficult. Therefore, strict requirements are put forward for the flame retardant, low smoke and low toxicity performance of cables. Moreover, after the cables are laid, they are mostly in locations that are difficult to maintain and replace. The design life is generally not less than 30 years, which places high demands on the weather resistance and durability of the sheath, the long-term stability of the structure and the long-term flame retardant performance.

[0004] Existing flame-retardant cables for rail transit mostly use low-smoke halogen-free flame-retardant polyolefins as the main sheath material. To meet the relevant standards for bundled combustion and smoke toxicity, a large amount of inorganic hydroxide flame retardant is usually filled into the matrix resin. Although a high amount of flame retardant can ensure that the initial flame-retardant performance of the cable meets the standards, it can easily lead to a decrease in the mechanical toughness and aging resistance of the sheath material. Under the combined effects of long-term ultraviolet radiation, thermal cycling, vibration, and bending, the sheath surface is prone to aging phenomena such as powdering and micro-cracks. Aging defects not only cause the internal flame retardant to migrate and precipitate to the surface, leading to a gradual decline in the flame-retardant performance of the cable over service time, but may also provide a penetration channel for moisture and corrosive media, causing problems such as internal armor corrosion and decreased insulation performance, making it difficult to guarantee the operational reliability of the cable throughout its entire life cycle.

[0005] In terms of structural design, conventional multilayer flame-retardant cables often employ a step-by-step extrusion process, with interlayer bonding relying solely on simple adhesion during the molten state. Under the long-term vibration and temperature fluctuations of rail transit, this can easily lead to interlayer slippage and debonding, weakening the overall structural stability of the cable and further expanding the penetration path of corrosive media. In some armored cables, the metal steel strip is in direct contact with the internal insulation buffer structure. During long-term vibration operation, hard contact wear can easily occur, causing localized damage to the internal functional layers and affecting the cable's electrical and fire resistance performance. Furthermore, in continuous fire scenarios, gases generated by the thermal decomposition of the internal insulation layer tend to escape radially, eroding the outer fire-resistant structure in the early stages of ceramic formation, forming penetrating micropores, and reducing the integrity of the fire barrier and its continuous fire resistance time.

[0006] At the manufacturing process level, the production of existing flame-retardant cables mostly adopts a step-by-step extrusion and single curing mode with fixed parameters. On the one hand, it is difficult to simultaneously take into account the differentiated molding and cross-linking requirements of the inner insulation layer, the middle flame-retardant oxygen barrier layer and the outer weather-resistant protective layer. This can easily lead to problems such as insufficient cross-linking degree of the inner layer and excessive cross-linking and embrittlement of the outer layer, affecting the stable performance of each layer. On the other hand, the process parameters generally lack scenario-based adaptation logic. The same set of production parameters is difficult to match the performance emphasis of different working conditions such as tunnels, elevated roads and vehicle ends. This can easily lead to some performance redundancy and some protection shortcomings, making it difficult to fully adapt to the usage needs of diverse scenarios in rail transit. Summary of the Invention

[0007] The purpose of this invention is to provide a high weather-resistant flame-retardant cable for rail transit, addressing the aforementioned problems.

[0008] The technical solution adopted in this invention is as follows: a high weather-resistant flame-retardant cable for rail transit, which, from the inside out, includes a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a high weather-resistant outer sheath.

[0009] The conductor core is made of multiple strands of tin-plated copper single wires concentrically twisted together;

[0010] The cross-linked flame-retardant insulating layer is wrapped around the outer periphery of the conductor core to provide electrical insulation protection;

[0011] The flame-retardant and oxygen-barrier buffer layer is wrapped around the cross-linked flame-retardant insulating layer to provide mechanical cushioning;

[0012] The composite flame-retardant armor layer is wrapped around the flame-retardant oxygen-barrier buffer layer to provide rigid support;

[0013] The highly weather-resistant outer protective layer covers the outer periphery of the composite flame-retardant armor layer to resist environmental erosion.

[0014] Optionally, the outer surface of the conductor core is smooth and flat, and the stranding diameter ratio is 12 to 16.

[0015] Optionally, the inner wall of the cross-linked flame-retardant insulation layer is smooth and can fit with the conductor core, and the outer wall of the cross-linked flame-retardant insulation layer is provided with a spiral interlocking groove structure and can fit with the flame-retardant oxygen-barrier buffer layer.

[0016] Optionally, the flame-retardant oxygen-barrier buffer layer is an inorganic filler-modified flame-retardant polyolefin composite material containing oriented flake mica powder and microporous structure. The inner and outer walls of the flame-retardant oxygen-barrier buffer layer are provided with spiral interlocking groove structure, and the inner wall of the flame-retardant oxygen-barrier buffer layer can be interlocked with the cross-linked flame-retardant insulation layer.

[0017] Optionally, the composite flame-retardant armor layer includes a flexible gasket, a galvanized steel strip interlocking armor body, and a ceramicized flame-retardant coating;

[0018] The galvanized steel strip interlocking armor body is a rigid frame. The inner side of the galvanized steel strip interlocking armor body is connected to a flexible pad, and the flexible pad can be embedded with the outer wall of the flame-retardant and oxygen-barrier buffer layer. The outer side of the galvanized steel strip interlocking armor body is coated with a ceramic flame-retardant coating.

[0019] Optionally, the high weather-resistant outer sheath is embedded in the gap between the steel strips of the galvanized steel strip interlocking armor body to form a mechanical interlock. The high weather-resistant outer sheath includes weather-resistant modified low-smoke halogen-free flame-retardant polyolefin, compounded antioxidants and light stabilizers.

[0020] Optionally, the production of the high weather-resistant flame-retardant cable for rail transit includes the following steps:

[0021] S1. Raw material classification and pretreatment: The raw materials of conductor core, cross-linked flame-retardant insulation layer, flame-retardant oxygen-barrier buffer layer, composite flame-retardant armor layer and high weather-resistant outer sheath are classified and pretreated according to material properties to unify the particle size accuracy, moisture content and dispersion uniformity of each raw material.

[0022] S2. The inner three-layer co-extrusion molding adopts the three-layer co-extrusion process. The cross-linked flame-retardant insulation layer, flame-retardant oxygen-barrier buffer layer and composite flame-retardant armor layer are simultaneously extruded and formed on the outer surface of the stranded conductor core (1). The matching spiral interlocking groove structure is formed on the contact surface of the three layers to obtain the inner layer co-extrusion semi-finished product.

[0023] S3. Interlocking wrapping of composite flame-retardant armor layer: galvanized steel strips pre-coated with ceramic flame-retardant coating are interlocked around the flexible pad of the inner co-extruded semi-finished product. The wrapping tension and gap accuracy of the steel strip are controlled to form a rigid armor skeleton and obtain the armor semi-finished product.

[0024] S4. High weather-resistant outer sheath extrusion molding: A high weather-resistant outer sheath is extruded on the outside of the armored semi-finished product, so that the molten sheath material is embedded in the gap of the steel strip to form mechanical interlocking, and the coarse cable product is obtained.

[0025] S5. Segmented gradient cross-linking and curing: The crude cable is fed into a segmented curing channel and goes through three stages in sequence: preheating and pre-cross-linking, main irradiation cross-linking, and gradient slow cooling to complete the differentiated cross-linking and shaping, eliminate interlayer stress, and obtain the cured cable.

[0026] S6. Post-processing and scenario-based performance verification: The surface of the cured cable is trimmed and the dimensions are calibrated. Graded performance tests are carried out for different laying scenarios in rail transit to obtain the finished cable.

[0027] Optionally, S2 includes the following sub-steps:

[0028] S21. Conductor core stranding and forming, setting the stranding pitch ratio to 12~16 times, controlling the multiple strands of tin-plated copper single wires to be stranded at a uniform speed in the same direction and concentrically, and after stranding, the outer surface of the conductor is finely polished to remove surface burrs and protrusions, ensuring that the surface roughness Ra of the conductor is Ra≤0.8μm.

[0029] S22. Co-extrusion equipment and die head debugging: Three single-screw extruders are used to correspond to the flexible pads of the cross-linked flame-retardant insulation layer, flame-retardant oxygen-barrier buffer layer and composite flame-retardant armor layer respectively. They are matched with a three-layer co-extrusion die head with a spiral cavity structure. The inner wall of the die head is provided with continuous spiral protrusions to form the spiral interlocking groove structure of each layer contact surface.

[0030] S23. Gradient temperature extrusion molding: A gradient temperature rise curve is set along the barrel of the single screw extruder from the feeding section to the homogenization section. The extrusion temperature of the cross-linked flame-retardant insulation layer is set at 140℃~170℃, the extrusion temperature of the flame-retardant oxygen-barrier buffer layer is controlled at 135℃~165℃, and the extrusion temperature of the composite flame-retardant armor layer flexible liner is controlled at 140℃~160℃.

[0031] S24. Directional flow and structural forming: A circumferential directional flow groove is set in the die head. Through shearing action, the flake mica powder in the flame-retardant and oxygen-barrier buffer layer is oriented along the cable axis. Combined with the gradient foaming of the thermal expansion microsphere pore-forming agent, an axially connected anisotropic microporous structure is formed inside the flame-retardant and oxygen-barrier buffer layer. When the three layers of material are in a molten state in the die head, they complete the spiral interlocking and interlocking. After extrusion, an integrated inner layer structure is formed.

[0032] Optionally, step S3 includes the following sub-steps:

[0033] S31. Steel strip unwinding and tension control: galvanized steel strip with pre-coated ceramic coating is output through an active unwinding mechanism, controlling the unwinding tension fluctuation to ≤±5%;

[0034] S32. Interlocking wrapping forming, using an interlocking armored machine head, galvanized steel strip with pre-coated ceramic coating is continuously wrapped around the outside of the flexible pad in a spiral shape, and the overlap gap of the galvanized steel strip with pre-coated ceramic coating is controlled to be ≤0.2mm, and the wrapping pitch ratio is 10~14 times.

[0035] S33. Online inspection of wrapping quality: Real-time monitoring of the gap, wrapping roundness and edge curling of the galvanized steel strip with pre-coated ceramic coating, marking unqualified sections, and ensuring that the roundness tolerance of the armor layer after wrapping is ≤0.1mm.

[0036] Optionally, step S4 includes the following sub-steps:

[0037] S41. Extrusion process parameter settings: Use a single screw extruder to extrude the raw material for the high weather-resistant outer protective layer. Set the barrel temperature to 130℃~165℃ and the die temperature to 160℃~170℃. Control the melt flow rate to match the travel speed of the armored semi-finished product.

[0038] S42. Extrusion interlocking molding uses an extrusion die head to control the gap between the die core and the die sleeve, so that the molten protective layer material is fully embedded into the interlocking gap and surface texture of the galvanized steel strip under the extrusion pressure, and forms a mechanical interlocking structure after cooling;

[0039] S43. Pre-cooling and shaping: The extruded rough product is placed in a constant temperature water bath at 40℃~60℃ for pre-cooling to pre-shape the outer sheath and obtain the cable rough product.

[0040] The beneficial effects of the present invention include at least one of the following;

[0041] 1. It adopts a coaxial layered structure from the inside out, consisting of a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a high weather-resistant outer sheath. Each functional layer has a clear division of labor and can respectively undertake the functions of conductive transmission, electrical insulation, buffering and oxygen barrier, rigid protection, and environmental weather resistance, forming a gradient protection system from the inside out, which helps to adapt to the comprehensive performance requirements of different laying scenarios in rail transit.

[0042] 2. The flame-retardant oxygen-barrier buffer layer is made of flame-retardant polyolefin composite material modified with inorganic fillers. The interior is set with oriented flake mica powder and microporous structure. On the one hand, it can play a mechanical buffering role, disperse the mechanical stress transmitted from the outside, and reduce the damage of concentrated force to the internal insulation layer. On the other hand, it can guide the gas generated by the thermal decomposition of the insulation layer to diffuse along the axial and circumferential directions, reduce the local rate of radial gas escape, and alleviate the erosive effect of decomposition gas on the outer fireproof structure, which is conducive to improving the density and continuous fire resistance of the fire barrier.

[0043] 3. The contact surfaces between the cross-linked flame-retardant insulation layer and the flame-retardant oxygen-barrier buffer layer, as well as between the flame-retardant oxygen-barrier buffer layer and the flexible gasket, are all equipped with matching spiral interlocking groove structures. This can improve the bonding strength between polymer functional layers, limit the relative slippage between layers in the axial and circumferential directions, help improve the problem of interlayer debonding under long-term vibration and thermal cycling conditions, and enhance the overall structural stability of the cable.

[0044] 4. The composite flame-retardant armor layer adopts a composite structure of flexible padding, galvanized steel strip interlocking armor body and ceramic flame-retardant coating. The flexible padding can disperse the hard contact stress of the metal steel strip on the internal structure and reduce wear damage under vibration conditions. The galvanized steel strip interlocking structure can provide rigid support and improve the cable's resistance to lateral pressure, impact and biological attack. The ceramic flame-retardant coating on the outside of the steel strip can seal the gaps in the steel strip in a fire environment and form a physical fire barrier with the steel strip, which helps to enhance the overall flame-retardant and fire-resistant effect of the cable. Attached Figure Description

[0045] Figure 1 A schematic diagram of a high weather-resistant flame-retardant cable for rail transit;

[0046] Figure 2 This is a flowchart illustrating the processing of a high-weather-resistant flame-retardant cable for rail transit.

[0047] In the picture:

[0048] 1 is the conductor core, 2 is the cross-linked flame-retardant insulation layer, 3 is the flame-retardant oxygen-barrier buffer layer, 4 is the composite flame-retardant armor layer, and 5 is the high weather-resistant outer protective layer. Detailed Implementation

[0049] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The components of the embodiments of the present invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.

[0050] Therefore, the following detailed description of the embodiments of the invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art based on the embodiments of the invention without inventive effort are within the scope of protection of the invention.

[0051] It should be noted that, unless otherwise specified, the embodiments and features described in this invention can be combined with each other.

[0052] It should be noted that similar labels and letters in the following figures indicate similar items. Therefore, once an item is defined in one figure, it does not need to be further defined and explained in subsequent figures.

[0053] In the description of this invention, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product of this invention is in use, or the orientation or positional relationship commonly understood by those skilled in the art. They are only used for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention. In addition, the terms "first," "second," etc., are only used to distinguish descriptions and should not be construed as indicating or implying relative importance.

[0054] In the description of this invention, it should also be noted that, unless otherwise explicitly specified and limited, the terms "set," "install," "connect," and "link" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

[0055] like Figure 1 As shown, a high weather-resistant flame-retardant cable for rail transit includes, from the inside out, a conductor core 1, a cross-linked flame-retardant insulation layer 2, a flame-retardant oxygen-barrier buffer layer 3, a composite flame-retardant armor layer 4, and a high weather-resistant outer sheath 5.

[0056] The conductor core 1 is made of multiple strands of tin-plated copper single wires concentrically twisted together;

[0057] The cross-linked flame-retardant insulating layer 2 is wrapped around the outer periphery of the conductor core 1 to provide electrical insulation protection;

[0058] The flame-retardant and oxygen-barrier buffer layer 3 is wrapped around the outer periphery of the cross-linked flame-retardant insulating layer 2 to provide mechanical cushioning;

[0059] The composite flame-retardant armor layer 4 is wrapped around the flame-retardant oxygen-barrier buffer layer 3 to provide rigid support;

[0060] The high weather-resistant outer protective layer 5 covers the outer periphery of the composite flame-retardant armor layer 4 to resist environmental erosion.

[0061] The purpose of this design is to adopt a coaxial layered structure from the inside out, consisting of a conductor core, a cross-linked flame-retardant insulation layer, a flame-retardant oxygen-barrier buffer layer, a composite flame-retardant armor layer, and a highly weather-resistant outer sheath. Each functional layer has a clear division of labor and can respectively undertake the functions of conductive transmission, electrical insulation, buffering and oxygen barrier, rigid protection, and environmental weather resistance, forming a gradient protection system from the inside out, which helps to adapt to the comprehensive performance requirements of different laying scenarios in rail transit.

[0062] Meanwhile, in this embodiment, the outer surface of the conductor core 1 is smooth and flat, and the stranding diameter ratio is 12 to 16 times.

[0063] Meanwhile, the inner wall of the cross-linked flame-retardant insulation layer 2 is smooth and can fit with the conductor core 1, and the outer wall of the cross-linked flame-retardant insulation layer 2 is provided with a spiral interlocking groove structure and can fit with the flame-retardant oxygen-barrier buffer layer 3.

[0064] In this embodiment, the flame-retardant oxygen barrier buffer layer 3 is an inorganic filler modified flame-retardant polyolefin composite material, which contains oriented sheet mica powder and microporous structure. The inner and outer walls of the flame-retardant oxygen barrier buffer layer 3 are provided with spiral interlocking groove structure, and the inner wall of the flame-retardant oxygen barrier buffer layer 3 can be interlocked with the cross-linked flame-retardant insulation layer 2.

[0065] The purpose of this design is that the flame-retardant oxygen-barrier buffer layer is made of flame-retardant polyolefin composite material modified with inorganic fillers. The interior is set with oriented flake mica powder and microporous structure. On the one hand, it can play a mechanical buffering role, disperse the mechanical stress transmitted from the outside, and reduce the damage of concentrated force to the internal insulation layer. On the other hand, it can guide the gas generated by the thermal decomposition of the insulation layer to diffuse along the axial and circumferential directions, reduce the local rate of radial gas escape, and alleviate the erosive effect of decomposition gas on the outer fireproof structure, which is conducive to improving the density and continuous fire resistance of the fire barrier.

[0066] Furthermore, the contact surfaces between the cross-linked flame-retardant insulation layer and the flame-retardant oxygen-barrier buffer layer, as well as between the flame-retardant oxygen-barrier buffer layer and the flexible pad, are all equipped with matching spiral interlocking groove structures. This can improve the bonding strength between polymer functional layers, limit the relative slippage between layers in the axial and circumferential directions, help improve the interlayer debonding problem under long-term vibration and thermal cycling conditions, and enhance the overall structural stability of the cable.

[0067] In this embodiment, the composite flame-retardant armor layer 4 includes a flexible pad, a galvanized steel strip interlocking armor body, and a ceramic flame-retardant coating.

[0068] The galvanized steel strip interlocking armor body is a rigid frame. The inner side of the galvanized steel strip interlocking armor body is connected to a flexible pad, and the flexible pad can be embedded with the outer wall of the flame-retardant and oxygen-barrier buffer layer 3. The outer side of the galvanized steel strip interlocking armor body is coated with a ceramic flame-retardant coating.

[0069] The purpose of this design is that the composite flame-retardant armor layer adopts a composite structure of flexible padding, galvanized steel strip interlocking armor body, and ceramic flame-retardant coating. The flexible padding can disperse the hard contact stress of the metal steel strip on the internal structure and reduce wear damage under vibration conditions. The galvanized steel strip interlocking structure can provide rigid support and improve the cable's resistance to lateral pressure, impact and biological attack. The ceramic flame-retardant coating on the outside of the steel strip can seal the gaps in the steel strip in a fire environment, forming a physical fire barrier with the steel strip, which helps to enhance the overall flame-retardant and fire-resistant effect of the cable.

[0070] In this embodiment, the high weather-resistant outer sheath 5 is embedded in the gap of the steel strip of the galvanized steel strip interlocking armor body to form a mechanical interlock. The high weather-resistant outer sheath 5 includes weather-resistant modified low-smoke halogen-free flame-retardant polyolefin, compounded antioxidant and light stabilizer.

[0071] The purpose of this design is that the high weather-resistant outer sheath uses weather-modified low-smoke halogen-free flame-retardant polyolefin, and is compounded with weather-resistant additives such as antioxidants and light stabilizers. It can resist the erosion of the environment such as ultraviolet radiation, damp heat, salt spray and wind and sand to a certain extent, and slow down the aging rate of the sheath. At the same time, the outer sheath is embedded in the gap of the steel strip to form a mechanical interlock, which helps to improve the reliability of the combination between the sheath and the armor structure, and ensure the stability of the flame-retardant and protective performance of the cable during long-term service.

[0072] This application also provides a method for producing high weather-resistant flame-retardant cables for rail transit, including the following steps:

[0073] S1. Raw material classification and pretreatment: The raw materials of conductor core 1, cross-linked flame-retardant insulation layer 2, flame-retardant oxygen-barrier buffer layer 3, composite flame-retardant armor layer 4 and high weather-resistant outer sheath 5 are classified and pretreated according to their material properties to unify the particle size accuracy, moisture content and dispersion uniformity of each raw material.

[0074] S2. The inner three-layer synchronous co-extrusion molding adopts a three-layer co-extrusion process. The cross-linked flame-retardant insulation layer 2, the flame-retardant oxygen-barrier buffer layer 3 and the composite flame-retardant armor layer 4 are simultaneously extruded and formed on the outer surface of the stranded conductor core 1. The matching spiral interlocking groove structure is simultaneously formed on the contact surface of the three layers to obtain the inner layer co-extrusion semi-finished product.

[0075] S3. Interlocking wrapping of composite flame-retardant armor layer: galvanized steel strips pre-coated with ceramic flame-retardant coating are interlocked around the flexible pad of the inner co-extruded semi-finished product. The wrapping tension and gap accuracy of the steel strip are controlled to form a rigid armor skeleton and obtain the armor semi-finished product.

[0076] S4. High weather-resistant outer sheath extrusion molding: A high weather-resistant outer sheath is extruded on the outside of the armored semi-finished product, so that the molten sheath material is embedded in the gap of the steel strip to form mechanical interlocking, and the coarse cable product is obtained.

[0077] S5. Segmented gradient cross-linking and curing: The crude cable is fed into a segmented curing channel and goes through three stages in sequence: preheating and pre-cross-linking, main irradiation cross-linking, and gradient slow cooling to complete the differentiated cross-linking and shaping, eliminate interlayer stress, and obtain the cured cable.

[0078] S6. Post-processing and scenario-based performance verification: The surface of the cured cable is trimmed and the dimensions are calibrated. Graded performance tests are carried out for different laying scenarios in rail transit to obtain the finished cable.

[0079] The purpose of this design is to use a raw material classification pretreatment process in the preparation method, and to carry out quality control on the raw materials of different functional layers separately, so as to unify the particle size accuracy, moisture content and dispersion uniformity. This helps to reduce defects such as porosity and filler agglomeration during the molding process, and improve the uniformity of the material properties of each layer and the batch stability of the product.

[0080] Meanwhile, the inner three-layer synchronous co-extrusion process can complete the synchronous molding of the spiral interlocking structure of each layer in the molten state, realizing interlayer melt interlocking, which can improve the interlayer bonding strength compared with the step extrusion method; at the same time, through the directional flow guiding structure and gradient temperature control in the die head, the orientation state and microporous structure of the sheet filler in the buffer layer can be adjusted to ensure the stable realization of the air resistance flow guiding and mechanical buffering functions of the buffer layer.

[0081] In this embodiment, S2 includes the following sub-steps:

[0082] S21. Conductor core stranding and forming, setting the stranding pitch ratio to 12~16 times, controlling the multiple strands of tin-plated copper single wires to be stranded at a uniform speed in the same direction and concentrically, and after stranding, the outer surface of the conductor is finely polished to remove surface burrs and protrusions, ensuring that the surface roughness Ra of the conductor is Ra≤0.8μm.

[0083] S22. Co-extrusion equipment and die head debugging: Three single-screw extruders are used to correspond to the flexible pads of the cross-linked flame-retardant insulation layer 2, the flame-retardant oxygen-barrier buffer layer 3, and the composite flame-retardant armor layer 4, respectively. They are matched with a three-layer co-extrusion die head with a spiral cavity structure, and the inner wall of the die head is provided with continuous spiral protrusions to form the spiral interlocking groove structure of each layer contact surface.

[0084] S23. Gradient temperature extrusion molding: A gradient temperature rise curve is set along the barrel of the single screw extruder from the feeding section to the homogenization section. The extrusion temperature of the cross-linked flame-retardant insulation layer 2 is set at 140℃~170℃, the extrusion temperature of the flame-retardant oxygen-barrier buffer layer 3 is controlled at 135℃~165℃, and the extrusion temperature of the composite flame-retardant armor layer 4 flexible pad is controlled at 140℃~160℃.

[0085] S24. Directional flow and structural forming: A circumferential directional flow groove is set in the die head. Through shearing action, the flake mica powder in the flame-retardant and oxygen-barrier buffer layer 3 is oriented along the cable axis. Combined with the gradient foaming of the thermal expansion microsphere pore-forming agent, an axially connected anisotropic microporous structure is formed inside the flame-retardant and oxygen-barrier buffer layer 3. When the three layers of materials are in a molten state in the die head, they complete the spiral interlocking and interlocking. After extrusion, an integrated inner layer structure is formed.

[0086] The purpose of this design is to ensure the roundness of the armor structure and the tightness of the inner fit by using an interlocking armor wrapping process and precise control of tension and gap. Combined with the buffering effect of the flexible pad, it helps to reduce the risk of damage to the internal functional layers during armor construction.

[0087] In this embodiment, S3 includes the following sub-steps:

[0088] S31. Steel strip unwinding and tension control: galvanized steel strip with pre-coated ceramic coating is output through an active unwinding mechanism, controlling the unwinding tension fluctuation to ≤±5%;

[0089] S32. Interlocking wrapping forming, using an interlocking armored machine head, galvanized steel strip with pre-coated ceramic coating is continuously wrapped around the outside of the flexible pad in a spiral shape, and the overlap gap of the galvanized steel strip with pre-coated ceramic coating is controlled to be ≤0.2mm, and the wrapping pitch ratio is 10~14 times.

[0090] S33. Online inspection of wrapping quality: Real-time monitoring of the gap, wrapping roundness and edge curling of the galvanized steel strip with pre-coated ceramic coating, marking unqualified sections, and ensuring that the roundness tolerance of the armor layer after wrapping is ≤0.1mm.

[0091] Meanwhile, S4 includes the following sub-steps:

[0092] S41. Extrusion process parameter settings: Use a single screw extruder to extrude the raw material of the high weather-resistant outer protective layer 5. Set the barrel temperature to 130℃~165℃ and the die temperature to 160℃~170℃. Control the melt flow rate to match the travel speed of the armored semi-finished product.

[0093] S42. Extrusion interlocking molding uses an extrusion die head to control the gap between the die core and the die sleeve, so that the molten protective layer material is fully embedded into the interlocking gap and surface texture of the galvanized steel strip under the extrusion pressure, and forms a mechanical interlocking structure after cooling;

[0094] S43. Pre-cooling and shaping: The extruded rough product is placed in a constant temperature water bath at 40℃~60℃ for pre-cooling to pre-shape the outer sheath and obtain the cable rough product.

[0095] The purpose of this design is to use an extrusion process for the outer sheath, which allows the molten sheath material to be fully embedded in the gaps between the steel strips to form a mechanical interlock, thereby improving the bonding strength between the sheath and the armor. Combined with the pre-cooling and shaping steps, this helps to reduce molding defects such as uneven sheath thickness and sagging.

[0096] Meanwhile, the segmented gradient crosslinking curing process, through step-by-step control of preheating and pre-crosslinking, main irradiation crosslinking and gradient slow cooling, can take into account the differentiated crosslinking requirements of different functional layers, so that the degree of crosslinking of each layer is within an appropriate range. At the same time, it gradually releases the thermal internal stress generated during extrusion and crosslinking, which helps to reduce microcrack defects in the high-filler flame retardant system and improve the long-term weather resistance of the material.

[0097] It should also be noted that, in specific implementation, the performance verification process can be carried out in different rail transit scenarios such as tunnels, elevated roads, and vehicle ends to conduct graded testing. This can verify the performance of the cable under the corresponding working conditions, and the process parameters can be optimized in reverse based on the test results to form a process parameter package that is suitable for different scenarios, which is conducive to improving the adaptability of the product to the diverse working conditions of rail transit.

[0098] Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A high weather-resistant flame-retardant cable for rail transit, characterized in that, From the inside out, it includes a conductor core (1), a cross-linked flame-retardant insulation layer (2), a flame-retardant oxygen-barrier buffer layer (3), a composite flame-retardant armor layer (4), and a high weather-resistant outer sheath (5). The conductor core (1) is made by concentrically stranding multiple tin-plated copper single wires; The cross-linked flame-retardant insulating layer (2) is wrapped around the outer periphery of the conductor core (1) to provide electrical insulation protection; The flame-retardant oxygen-barrier buffer layer (3) is wrapped around the outer periphery of the cross-linked flame-retardant insulating layer (2) to provide mechanical cushioning; The composite flame-retardant armor layer (4) is wrapped around the flame-retardant oxygen-barrier buffer layer (3) to provide rigid support; The high weather-resistant outer protective layer (5) covers the outer periphery of the composite flame-retardant armor layer (4) to resist environmental erosion.

2. The high weather-resistant flame-retardant cable for rail transit according to claim 1, characterized in that, The outer surface of the conductor core (1) is smooth and flat, and the twisted section diameter ratio is 12 to 16 times.

3. The high weather-resistant flame-retardant cable for rail transit according to claim 1, characterized in that, The inner wall of the cross-linked flame-retardant insulation layer (2) is smooth and can fit with the conductor core (1). The outer wall of the cross-linked flame-retardant insulation layer (2) is provided with a spiral interlocking groove structure and can fit with the flame-retardant oxygen-barrier buffer layer (3).

4. The high weather-resistant flame-retardant cable for rail transit according to claim 3, characterized in that, The flame-retardant oxygen-barrier buffer layer (3) is an inorganic filler modified flame-retardant polyolefin composite material, which contains oriented sheet mica powder and microporous structure. The inner and outer walls of the flame-retardant oxygen-barrier buffer layer (3) are provided with spiral interlocking groove structure, and the inner wall of the flame-retardant oxygen-barrier buffer layer (3) can be interlocked with the cross-linked flame-retardant insulation layer (2).

5. A high weather-resistant flame-retardant cable for rail transit according to claim 4, characterized in that, The composite flame-retardant armor layer (4) includes a flexible liner, a galvanized steel strip interlocking armor body, and a ceramic flame-retardant coating; The galvanized steel strip interlocking armor body is a rigid frame. The inner side of the galvanized steel strip interlocking armor body is connected to a flexible pad, and the flexible pad can be fitted into the outer wall of the flame-retardant and oxygen-barrier buffer layer (3). The outer side of the galvanized steel strip interlocking armor body is coated with a ceramic flame-retardant coating.

6. A high weather-resistant flame-retardant cable for rail transit according to claim 5, characterized in that, The high weather-resistant outer protective layer (5) is embedded in the gap of the steel strip of the galvanized steel strip interlocking armor body to form a mechanical interlock. The high weather-resistant outer protective layer (5) includes weather-resistant modified low smoke halogen-free flame-retardant polyolefin, compound antioxidant and light stabilizer.

7. A high weather-resistant flame-retardant cable for rail transit according to any one of claims 1 to 6, characterized in that, The method for producing high weather-resistant flame-retardant cables for rail transit includes the following steps: S1. Raw material classification and pretreatment: The raw materials of conductor core (1), cross-linked flame-retardant insulation layer (2), flame-retardant oxygen-barrier buffer layer (3), composite flame-retardant armor layer (4) and high weather-resistant outer sheath layer (5) are classified and pretreated according to their material properties to unify the particle size accuracy, moisture content and dispersion uniformity of each raw material. S2. The inner three-layer co-extrusion molding adopts the three-layer co-extrusion process. The cross-linked flame-retardant insulation layer (2), flame-retardant oxygen-barrier buffer layer (3) and composite flame-retardant armor layer (4) are simultaneously extruded on the outer surface of the stranded conductor core (1). The three layers are simultaneously formed with matching spiral interlocking groove structure on the contact surface of the three layers to obtain the inner layer co-extrusion semi-finished product. S3. Interlocking wrapping of composite flame-retardant armor layer: galvanized steel strips pre-coated with ceramic flame-retardant coating are interlocked around the flexible pad of the inner co-extruded semi-finished product. The wrapping tension and gap accuracy of the steel strip are controlled to form a rigid armor skeleton and obtain the armor semi-finished product. S4. High weather-resistant outer sheath extrusion molding: A high weather-resistant outer sheath is extruded on the outside of the armored semi-finished product, so that the molten sheath material is embedded in the gap of the steel strip to form mechanical interlocking, and the coarse cable product is obtained. S5. Segmented gradient cross-linking and curing: The crude cable is fed into a segmented curing channel and goes through three stages in sequence: preheating and pre-cross-linking, main irradiation cross-linking, and gradient slow cooling to complete the differentiated cross-linking and shaping, eliminate interlayer stress, and obtain the cured cable. S6. Post-processing and scenario-based performance verification: The surface of the cured cable is trimmed and the dimensions are calibrated. Graded performance tests are carried out for different laying scenarios in rail transit to obtain the finished cable.

8. A high weather-resistant flame-retardant cable for rail transit according to claim 7, characterized in that, S2 includes the following sub-steps: S21. Conductor core stranding and forming, setting the stranding pitch ratio to 12~16 times, controlling the multiple strands of tin-plated copper single wires to be stranded at a uniform speed in the same direction and concentrically, and after stranding, the outer surface of the conductor is finely polished to remove surface burrs and protrusions, ensuring that the surface roughness Ra of the conductor is Ra≤0.8μm. S22. Co-extrusion equipment and die head debugging: Three single screw extruders are used to correspond to the flexible pads of the cross-linked flame-retardant insulation layer (2), flame-retardant oxygen-barrier buffer layer (3), and composite flame-retardant armor layer (4), respectively. They are matched with a three-layer co-extrusion die head with a spiral cavity structure, and the inner wall of the die head is provided with continuous spiral protrusions for forming the spiral interlocking groove structure of each layer contact surface. S23. Gradient temperature extrusion molding, a gradient temperature rise curve is set along the barrel of the single screw extruder from the feeding section to the homogenization section, the cross-linked flame retardant insulation layer (2) extrusion temperature is set at 140℃~170℃, the flame retardant oxygen barrier buffer layer (3) extrusion temperature is controlled at 135℃~165℃, the composite flame retardant armor layer (4) flexible pad extrusion temperature is controlled at 140℃~160℃; S24. Directional flow and structural forming: A circumferential directional flow groove is set in the die head. Through shearing action, the flake mica powder in the flame-retardant oxygen-barrier buffer layer (3) is oriented along the cable axis. Combined with the gradient foaming of the thermal expansion microsphere pore-forming agent, an axially connected anisotropic microporous structure is formed inside the flame-retardant oxygen-barrier buffer layer (3). When the three layers of materials are in a molten state in the die head, they complete the spiral interlocking and biting. After extrusion, an integrated inner layer structure is formed.

9. A high weather-resistant flame-retardant cable for rail transit according to claim 8, characterized in that, S3 includes the following sub-steps: S31. Steel strip unwinding and tension control: galvanized steel strip with pre-coated ceramic coating is output through an active unwinding mechanism, controlling the unwinding tension fluctuation to ≤±5%; S32. Interlocking wrapping forming, using an interlocking armored machine head, galvanized steel strip with pre-coated ceramic coating is continuously wrapped around the outside of the flexible pad in a spiral shape, and the overlap gap of the galvanized steel strip with pre-coated ceramic coating is controlled to be ≤0.2mm, and the wrapping pitch ratio is 10~14 times. S33. Online inspection of wrapping quality: Real-time monitoring of the gap, wrapping roundness and edge curling of the galvanized steel strip with pre-coated ceramic coating, marking unqualified sections, and ensuring that the roundness tolerance of the armor layer after wrapping is ≤0.1mm.

10. A high weather-resistant flame-retardant cable for rail transit according to claim 8, characterized in that, S4 includes the following sub-steps: S41. Extrusion process parameter setting: Use a single screw extruder to extrude the raw material of the high weather-resistant outer protective layer (5), set the barrel temperature to 130℃~165℃, set the die temperature to 160℃~170℃, and control the melt flow rate to match the travel speed of the armored semi-finished product. S42. Extrusion interlocking molding uses an extrusion die head to control the gap between the die core and the die sleeve, so that the molten protective layer material is fully embedded into the interlocking gap and surface texture of the galvanized steel strip under the extrusion pressure, and forms a mechanical interlocking structure after cooling; S43. Pre-cooling and shaping: The extruded rough product is placed in a constant temperature water bath at 40℃~60℃ for pre-cooling to pre-shape the outer sheath and obtain the cable rough product.