Medium-voltage solid-state transformer

By wrapping conductive foil around the core frame column of the medium-voltage solid-state transformer and setting an insulating structure between the core and the winding, the potential difference problem between the core and the winding is solved, the core surface is made equipotential, the risk of partial discharge and eddy current loss is reduced, and the stability and efficiency of the transformer are improved.

CN123120484APending Publication Date: 2026-11-17SHENZHEN MEGMEET ELECTRICAL CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611538239.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-30
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

A high potential difference exists between the transformer core and the windings, leading to electric field distortion and the risk of partial discharge. Furthermore, the floating potential of the core can easily cause insulation breakdown.

Method used

Design a medium-voltage solid-state transformer by using conductive foil wrapped around the outer side of the magnetic core frame column. The conductive foil makes the surface of the magnetic core equipotential, suppressing partial discharge and common-mode interference. An insulation structure is set between the magnetic core and the winding to reduce eddy current loss.

Benefits of technology

It effectively reduces the risk of partial discharge, suppresses common-mode interference, reduces eddy current losses, and improves magnetic circuit utilization efficiency and mechanical stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120484A_ABST
    Figure CN123120484A_ABST
Patent Text Reader

Abstract

This application discloses a medium-voltage solid-state transformer, which includes a magnetic core, windings, and a first conductive foil. The magnetic core includes a frame post and a center post, with the center post disposed within a frame formed by the frame post, and the windings wound around the center post. The first conductive foil is sleeved on the outer wall of the frame post facing away from the center post. Through the above scheme, the medium-voltage solid-state transformer of this application can utilize the first conductive foil to make the surface of the magnetic core equipotential, suppressing partial discharge and common-mode interference, thereby avoiding the introduction of eddy current losses and effectively reducing the risk of partial discharge.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of power electronics technology, and in particular to a medium-voltage solid-state transformer. Background Technology

[0002] In recent years, transformers, as core power devices in power electronic equipment such as switching power supplies, on-board chargers, photovoltaic inverters, energy storage converters, communication power supplies, and server power supplies, have been widely used in AI (Artificial Intelligence) computing data centers, megawatt-level electric vehicle supercharging stations, wind-solar-storage grid connection, AC-DC hybrid microgrids, and integrated source-grid-load-storage scenarios, relying on high-frequency power electronic conversion technology to achieve direct connection to medium-voltage power grids.

[0003] However, in related technologies, there is a high potential difference between the core and windings of the transformer, and the electric field distribution on the outer surface of the core (especially at the edges and end faces of the frame columns and middle columns) is severely distorted and the local field strength is concentrated, which can easily lead to partial discharge or even insulation breakdown. In addition, there is a floating core potential, which results in a high potential difference between the core and the windings and insulation structure, leading to electric field distortion and thus the risk of partial discharge. Summary of the Invention

[0004] In view of the above problems, this application provides a medium-voltage solid-state transformer that can make the surface of the magnetic core equipotential, suppress partial discharge and common-mode interference, thereby avoiding the introduction of eddy current losses and effectively reducing the risk of partial discharge.

[0005] To solve the above-mentioned technical problems, one technical solution adopted in this application is to provide a medium-voltage solid-state transformer, wherein the medium-voltage solid-state transformer includes a magnetic core, a winding and a first conductive foil; the magnetic core includes a frame post and a center post, the center post is disposed in the frame formed by the frame post, and the winding is wound on the center post; the first conductive foil is sleeved on the outer wall of the frame post away from the center post.

[0006] The frame column includes a first side plate, a second side plate, a first bottom plate, and a second bottom plate. The first side plate, the first bottom plate, the second side plate, and the second bottom plate are connected end to end to form a rectangular frame. One end of the central column is connected to the inner wall of the first bottom plate facing the second bottom plate, and an air gap is provided between the other end of the central column and the second bottom plate.

[0007] The medium-voltage solid-state transformer further includes a second conductive foil and a third conductive foil. One end of the second conductive foil and one end of the third conductive foil are both connected to the first conductive foil. The other end of the second conductive foil extends from the outer side wall of the first base plate to the inner side wall of the first base plate, and extends along the first side wall of the central column towards the air gap, so as to be spaced apart from the air gap. The first side wall is the side wall of the central column facing the first side plate. The other end of the third conductive foil extends from the outer side wall of the first base plate to the inner side wall of the first base plate, and extends along the second side wall of the central column towards the air gap, so as to be spaced apart from the air gap. The second side wall is the side wall of the central column facing the second side plate.

[0008] The dimension of the air gap along the axial direction of the central column is the air gap depth; the minimum distance between the second conductive foil and the air gap is not less than 5 times the air gap depth, and the minimum distance between the third conductive foil and the air gap is not less than 5 times the air gap depth.

[0009] The frame column and the middle column include at least two magnetic laminations, and an insulating structure is provided between each two adjacent magnetic laminations so that each two adjacent magnetic laminations are insulated from each other.

[0010] The insulating structure includes an insulating heat sink, which is disposed between each pair of adjacent magnetic stacks and is thermally connected to the two adjacent magnetic stacks.

[0011] The insulating structure includes an insulating adhesive layer, which is disposed between every two adjacent magnetic laminations, and the two adjacent magnetic laminations are bonded and fixed by the insulating adhesive layer.

[0012] The winding includes an insulating casting body, a primary winding, a first-stage winding, and a second-stage winding. The primary winding is embedded inside the insulating casting body. The first-stage winding surrounds the central column, forming a first heat dissipation channel between them. The insulating casting body surrounds the first-stage winding, forming a second heat dissipation channel between them. The second-stage winding surrounds the insulating casting body, forming a third heat dissipation channel between them. The second-stage winding is electrically connected to the first-stage winding.

[0013] The insulating casting body has at least two first support portions protruding from the outer side wall facing the secondary winding, and the at least two first support portions abut against the inner side wall of the secondary winding facing the insulating casting body, so as to separate the insulating casting body from the secondary winding; and / or, the insulating casting body has at least two second support portions protruding from the inner side wall facing the primary winding, and the at least two second support portions abut against the outer side wall of the primary winding facing the insulating casting body, so as to separate the insulating casting body from the primary winding.

[0014] The first support portion is provided with a first heat dissipation hole, which extends in a direction parallel to the center line of the central column; and / or, the second support portion is provided with a second heat dissipation hole, which extends in a direction parallel to the center line of the central column.

[0015] The winding further includes a first mounting member, which is arranged around the central column and spaced apart in the first heat dissipation duct, and the first primary winding is spirally wound on the outer side wall of the first mounting member away from the central column; and / or, the winding further includes a second mounting member, which is arranged around the insulating casting body and spaced apart in the third heat dissipation duct, and the second primary winding is spirally wound on the outer side wall of the second mounting member away from the insulating casting body.

[0016] The medium-voltage solid-state transformer further includes a mounting frame, with a center column and a first mounting component spaced apart from each other on the mounting frame to separate the primary winding from the center column; and / or, the first mounting component and an insulating casting body spaced apart from each other on the mounting frame to separate the primary winding from the insulating casting body; and / or, the insulating casting body and a second mounting component spaced apart from each other on the mounting frame to separate the insulating casting body from the secondary winding.

[0017] The second mounting component has at least two third support portions protruding from the inner wall of the insulating casting body. The at least two third support portions abut against the outer wall of the insulating casting body facing the second stage winding, so that the insulating casting body and the second stage winding are spaced apart.

[0018] The medium-voltage solid-state transformer also includes a skirt, which is connected to the insulating cast body.

[0019] The beneficial effects of this application are as follows: Unlike the prior art, the medium-voltage solid-state transformer provided by this application can make the surface of the magnetic core equipotential by using the first conductive foil to cover the outer wall of its magnetic core frame column away from the central column, thereby suppressing partial discharge and common-mode interference, thus avoiding the introduction of eddy current losses and effectively reducing the risk of partial discharge. Attached Figure Description

[0020] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0021] Figure 1 This is an assembly diagram of one embodiment of the medium-voltage solid-state transformer in this application; Figure 2 for Figure 1 A front view of a medium-voltage solid-state transformer. Figure 3 for Figure 1 An exploded schematic diagram of a medium-voltage solid-state transformer. Figure 4 for Figure 1 A schematic diagram of the structure of a magnetic core in a medium-voltage solid-state transformer; Figure 5 for Figure 1 A schematic diagram of the winding structure in an embodiment of a medium-voltage solid-state transformer.

[0022] Explanation of reference numerals in the attached figures: 100. Medium-voltage solid-state transformer; 10. Magnetic core; 11. Frame column; 111. First side plate; 112. Second side plate; 113. First base plate; 114. Second base plate; 12. Central column; 121. First side wall; 122. Second side wall; 13. Air gap; 14. Magnetic lamination; 15. Insulation structure; 151. Insulating heat sink; 152. Insulating adhesive layer; 20. Winding; 21. Insulating casting; 211. First support part; 212. Second support part; 213. First heat dissipation through hole; 214. Second heat dissipation through hole; 2101. Insulating connector; 2102. First insulation 2103, Second Insulator; 2104, First Baffle; 2105, First Guide Slot; 22, Primary Winding; 23, First Primary Winding; 24, Second Primary Winding; 25, First Mounting Component; 251, Second Baffle; 252, Second Guide Slot; 26, Second Mounting Component; 261, Third Baffle; 262, Third Guide Slot; 27, Conductive Connector; 28, Low-Voltage Side Lead-Out Terminal; 31, First Conductive Foil; 32, Second Conductive Foil; 33, Third Conductive Foil; 50, Umbrella Skirt; 61, First Heat Dissipation Channel; 62, Second Heat Dissipation Channel; 63, Third Heat Dissipation Channel. Detailed Implementation

[0023] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.

[0024] The terms "first," "second," and "third" in this application are for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first," "second," or "third" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified. All directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of this application are only used to explain the relative positional relationships and movements between components in a specific orientation (as shown in the figures). If the specific orientation changes, the directional indications also change accordingly. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or device that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products, or devices.

[0025] In this document, the term "embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment may be included in at least one embodiment of this application. The appearance of this phrase in various places throughout the specification does not necessarily refer to the same embodiment, nor is it a separate or alternative embodiment mutually exclusive with other embodiments. It will be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments.

[0026] The present application will now be described in detail with reference to the accompanying drawings and embodiments.

[0027] Please see Figures 1-3 ,in, Figure 1 This is an assembly diagram of one embodiment of the medium-voltage solid-state transformer in this application. Figure 2 for Figure 1 A front view of a medium-voltage solid-state transformer. Figure 3 for Figure 1 An exploded view of a medium-voltage solid-state transformer. In this embodiment, the medium-voltage solid-state transformer 100 includes a magnetic core 10, a winding 20, and a first conductive foil 31.

[0028] The medium-voltage solid-state transformer 100 provided in this application can be used as the isolation stage of a solid-state transformer (power electronic transformer) as its high-frequency isolation transformer; it can also be used independently as a medium-frequency isolation transformer in a medium-voltage distribution network. For example, the medium-voltage side voltage level of the medium-voltage solid-state transformer 100 is 3kV, 6kV, 10kV, 20kV or 35kV, the rated power is 50kVA to 2MVA, and the operating frequency is 500Hz to 50kHz, exemplarily 2kHz to 20kHz, which is not limited in this application.

[0029] The magnetic core 10 includes a frame post 11 and a middle post 12. The middle post 12 is disposed within the frame formed by the frame post 11, and the winding 20 is wound around the middle post 12. The first conductive foil 31 is sleeved on the outer wall of the frame post 11 away from the middle post 12.

[0030] Understandably, the magnetic core 10 forms an enclosed magnetic circuit structure of "outer frame pillar 11 + central pillar 12". The winding 20 is arranged in the window area between the central pillar 12 and the frame pillar 11. The central pillar 12, the winding 20, and the frame pillar 11 are arranged radially from the inside to the outside. This structure concentrates the magnetomotive force of the magnetic circuit in the central pillar 12. The winding 20 is partially surrounded by the outer frame pillar 11. On the one hand, it improves the utilization efficiency of the magnetic circuit and reduces outward leakage magnetic field. On the other hand, the frame pillar 11 can serve as an overall mechanical skeleton and also as a carrier of the shielding layer, making it easy to attach the first conductive foil 31 to its outer surface. This allows the first conductive foil 31 to be used to make the outer wall of the frame pillar 11 equipotential, suppressing partial discharge and common-mode interference, thereby avoiding the introduction of eddy current losses and effectively reducing the risk of partial discharge.

[0031] In addition, the term "cladding" as used herein refers to the first conductive foil 31 covering and adhering to at least a portion of the outer side wall of the frame post 11 circumferentially, forming a foil-shaped conductive layer surrounding the frame post 11.

[0032] The first conductive foil 31 mainly plays the following role in the circuit: (1) Electrostatic shielding and common-mode current collection. Due to the high voltage change rate of the isolation stage converter, there is a parasitic distributed capacitance between the winding 20 and the magnetic core 10. The high-frequency common-mode displacement current will be injected into the magnetic core 10 through this distributed capacitance. The first conductive foil 31 is attached to the outer surface of the magnetic core 10, which can collect the common-mode current on the spot and guide it to the ground potential through the ground lead-out terminal (not shown in the figure), preventing it from continuing to diffuse along the magnetic core 10 to the shell (not shown in the figure), mounting bracket (not shown in the figure), busbar (not shown in the figure), fasteners (not shown in the figure) and other adjacent metal parts, thereby suppressing common-mode electromagnetic interference, eliminating potential fluctuations on the metal surface, and reducing the risk of surface partial discharge under medium voltage environment.

[0033] (2) High-frequency leakage current shunting. The first conductive foil 31 is a conductive layer surrounding the frame post 11. The high-frequency leakage magnetic field radiating outward through the frame post 11 induces eddy currents in the foil. The magnetic potential generated by the eddy current is opposite to that of the leakage magnetic field, thereby weakening the leakage magnetic field radiating outward and reducing the eddy current heating and external electromagnetic radiation in the adjacent metal structural components.

[0034] (3) Surface heat dissipation and temperature equalization. The thermal conductivity of the first conductive foil 31 is much higher than that of the paint film and insulating material on the surface of the magnetic core 10. It has a large area, thin thickness and direct contact with air. It can quickly spread and dissipate the heat on the surface of the frame column 11 along the foil surface, playing the role of "heat dissipation skin". When the normal direction of the magnetic stack 14 is arranged radially along the central column 12, the heat conducted out of the magnetic core 10 is just dissipated from the first conductive foil 31 to the surrounding area, forming a complete heat flow path.

[0035] In some embodiments, the material of the first conductive foil 31 may be copper foil, oxygen-free copper foil, nickel-plated copper foil, aluminum foil, copper-clad aluminum foil, or a composite foil with a polyimide film, polyester film, or epoxy coating on the surface of the above metal foil. This application does not limit the specific materials used.

[0036] In some embodiments, the thickness of the first conductive foil 31 is from 0.05 mm to 1.0 mm, exemplarily from 0.1 mm to 0.5 mm. If the thickness is too thin, the current-carrying cross-section at high frequencies will be insufficient and significant heat generation will occur; if the thickness is too large, the material cost and weight will increase, and there will be no further benefits due to the skin effect limitation.

[0037] In some embodiments, the first conductive foil 31 can be directly bonded to the outer wall of the frame post 11, or a thermally conductive insulating pad (not shown in the figure) can be sandwiched between them, such as a thermally conductive silicone rubber pad, an alumina ceramic sheet, or a boron nitride coating, to prevent surface discharge between the first conductive foil 31 and the surface of the magnetic core 10 due to potential difference, while improving contact thermal resistance.

[0038] In some embodiments, the circumferential connection of the first conductive foil 31 can be achieved by a single, integral sheet, where the first conductive foil 31 is a single sheet of metal foil with its ends overlapping to form a ring structure around the frame post 11. Electrical connection is achieved at the overlap using laser welding, argon arc welding, soldering, ultrasonic welding, conductive adhesive bonding, or bolt crimping, with an overlap length of 5mm to 50mm. Alternatively, an open-ring design can be used, where an insulating spacer (e.g., a polyimide film) is placed at the overlap, making the first conductive foil 31 electrically an open ring, thus not forming a complete short-circuit turn around the frame post 11. Using an open-ring design avoids excessive circulating current and heat generation within the foil under strong leakage magnetic field; in this case, the first conductive foil 31 primarily functions as electrostatic shielding and surface heat dissipation. Alternatively, a segmented approach can be adopted, where the first conductive foil 31 is composed of multiple segmented foils arranged at intervals along the circumference of the frame post 11, with insulating gaps between adjacent segmented foils, the gap width being 0.5mm to 5mm; the segmented foils are connected by conductive connecting strips (or wires) at a position away from the magnetic core 10 and then grounded uniformly. The segmented approach can suppress leakage flux and limit the circulating current within the foil to a very small range, making it the preferred approach for high-frequency, high leakage flux conditions.

[0039] In some embodiments, the frame formed by the frame posts 11 can be a rectangular frame, a circular frame, or a polygonal frame, and this application does not limit this.

[0040] Please continue reading. Figure 4 , Figure 4 for Figure 1 A schematic diagram of the structure of a magnetic core in a medium-voltage solid-state transformer.

[0041] In some embodiments, the frame column 11 includes a first side plate 111, a second side plate 112, a first bottom plate 113, and a second bottom plate 114. The first side plate 111, the first bottom plate 113, the second side plate 112, and the second bottom plate 114 are connected end to end to form a rectangular frame. The first bottom plate 113 and the second bottom plate 114 are arranged at intervals along the axial direction of the central column 12 and are located at the two ends of the axial direction of the central column 12, respectively. The first side plate 111 and the second side plate 112 are arranged at intervals along a direction perpendicular to the axial direction and are located on the two sides of the radial direction of the central column 12, respectively. The first side plate 111 and the second side plate 112 are both perpendicular to the first bottom plate 113 and the second bottom plate 114.

[0042] In other embodiments, the frame column 11 may also include a plurality of side columns arranged at intervals along the circumference. The plurality of side columns are connected end to end to the first base plate 113 and the second base plate 114 to form a multi-column frame, thereby further reducing magnetic leakage and providing more outer surfaces for the first conductive foil 31 to be attached.

[0043] It is worth noting that in this article, "axial" refers to the direction extending along the centerline of the central column 12; "radial" refers to the direction perpendicular to the centerline of the central column 12 and pointing away from or towards the centerline; and "circumferential" refers to the annular direction around the centerline of the central column 12. "Inner wall" refers to the surface facing the interior of the frame (i.e., the side facing the central column 12); and "outer wall" refers to the surface away from the interior of the frame (i.e., the side away from the central column 12).

[0044] Furthermore, one end of the central column 12 is connected to the inner wall of the first base plate 113 facing the second base plate 114, and an air gap 13 is provided between the other end of the central column 12 and the second base plate 114. That is, the central column 12 and the first base plate 113 are directly magnetically connected (without an air gap), and the central column 12 and the second base plate 114 are magnetically coupled through the air gap 13. The path of the main magnetic flux is: central column 12, air gap 13, second base plate 114, first side plate 111 and second side plate 112, first base plate 113, central column 12, thus forming a closed magnetic circuit.

[0045] Compared to opening an air gap in the middle of the central column 12, the air gap 13 is located at the axial end of the central column 12. The magnetic flux at its edge diverges outward along the radial direction of the central column 12 in a more concentrated manner, making it easier to predict and shield. It also avoids the inconvenience of winding the winding 20 being divided into two sections axially by the air gap. In addition, the magnetostrictive vibration at the air gap 13 is concentrated at the end, which can be easily constrained by subsequent pads and mounting brackets, reducing noise.

[0046] In some embodiments, the air gap 13 has an air gap depth of 0.5 mm to 20 mm, preferably 2 mm to 5 mm. The air gap 13 can be formed by placing an air gap pad (not shown) with a thickness equal to the air gap depth d between the end face of the central column 12 facing the second base plate 114 and the inner sidewall of the second base plate 114. The air gap pad is made of a non-magnetic and heat-resistant insulating material, such as epoxy glass cloth board, polyimide board, aramid paperboard, polytetrafluoroethylene board or ceramic sheet.

[0047] In other embodiments, to further disperse the magnetomotive force and reduce the edge magnetic flux density at a single air gap, multiple second air gaps (not shown) connected in series along the axial direction can be provided between the central column 12 and the second base plate 114, with the total air gap length of the multiple second air gaps and air gap 13 remaining unchanged; small auxiliary air gaps can also be added at the connection between the first side plate 111, the second side plate 112 and the base plate of the frame column 11. In this case, the "air gap depth" is taken as the largest axial dimension among all air gaps, or the sum of the depths of all air gaps, as long as it satisfies the subsequent limiting relationship between the conductive foil and the air gap spacing, and this application does not impose any limitations on this.

[0048] It is worth noting that the "air gap depth" in this article refers to the dimension of the air gap 13 along the axial direction of the central column 12, that is, the axial distance between the magnetic end faces on both sides of the air gap 13. The "minimum spacing" refers to the minimum straight-line distance among all point pairs between two objects.

[0049] In some embodiments, the material of the magnetic core 10 can be selected according to the operating frequency and loss requirements, such as amorphous ribbon, nanocrystalline ribbon, oriented silicon steel sheet, ferrite and other high-frequency low-loss materials, metal soft magnetic powder core (iron-silicon-aluminum, iron-nickel, iron-silicon-chromium), or a composite combination of the above materials. For operating frequencies from 2kHz to 20kHz, nanocrystalline stacks or amorphous stacks can be used; for higher frequencies, ferrite can be used, and this application does not limit this.

[0050] In some embodiments, the first conductive foil 31 covers the first side plate 111, the second side plate 112, the first bottom plate 113, and the second bottom plate 114 of the frame column 11, each of which is away from the outer side wall of the central column 12, and continuously transitions at the junction edge of each side plate and the bottom plate, so that the first conductive foil 31 becomes a connected conductive layer surrounding the entire frame of the magnetic core 10.

[0051] In some embodiments, the medium-voltage solid-state transformer 100 further includes a second conductive foil 32 and a third conductive foil 33, with one end of the second conductive foil 32 and one end of the third conductive foil 33 both connected to the first conductive foil 31.

[0052] The other end of the second conductive foil 32 extends from the outer side wall of the first base plate 113 to the inner side wall of the first base plate 113, and extends along the first side wall 121 of the central column 12 toward the air gap 13, so as to be spaced apart from the air gap 13; wherein, the first side wall 121 is the side wall of the central column 12 facing the first side plate 111.

[0053] The other end of the third conductive foil 33 extends from the outer side wall of the first base plate 113 to the inner side wall of the first base plate 113, and extends along the second side wall 122 of the central column 12 toward the air gap 13, so as to be spaced apart from the air gap 13; wherein, the second side wall 122 is the side wall of the central column 12 facing the second side plate 112.

[0054] Thus, the first conductive foil 31, the second conductive foil 32, and the third conductive foil 33 are interconnected, forming a connected conductive shield that extends from the outer surface of the magnetic core 10 frame to the side wall of the central column 12 inside the window.

[0055] The shielding principle is as follows: the edge magnetic flux at the air gap 13 diverges outward from the end face of the central column 12 along the radial direction of the central column 12 and passes through the conductor of the winding 20 arranged around the central column 12. Since the second conductive foil 32 is arranged along the first side wall 121 of the central column 12 towards the first side plate 111 and the third conductive foil 33 is arranged along the second side wall 122 of the central column 12 towards the second side plate 112, that is, the two conductive foils are exactly located on the radial sides of the central column 12 and on the main path of the edge magnetic flux diverging towards the winding 20, the high-frequency edge magnetic flux induces eddy currents in the second conductive foil 32 and the third conductive foil 33 when it passes through them. The magnetic field generated by the eddy current is opposite to the direction of the edge magnetic flux, "squeezing" the edge magnetic flux to the side of each conductive foil near the central column 12, significantly weakening its penetration towards the winding 20. The high-frequency eddy current losses that would normally be generated in the thick cross-section conductor of winding 20 are transferred to a thin sheet-like conductive foil with a large surface area, low thermal resistance, and direct contact with the cooling medium. The losses are then evenly distributed through the conductive foil itself and the first conductive foil 31 connected to it, fundamentally suppressing local hot spots in the winding near the air gap 13.

[0056] In some embodiments, the second conductive foil 32 and the third conductive foil 33 can be directly attached to the surfaces of the first sidewall 121 and the second sidewall 122 of the central column 12. When the surface of the central column 12 is a cylindrical surface, the second conductive foil 32 is attached to the fan-shaped area facing the first side plate 111 on the cylindrical surface, and the third conductive foil 33 is attached to the fan-shaped area facing the second side plate 112. The central angle of the two fan-shaped areas is exemplary from 30° to 150°. A thermally conductive insulating layer can be sandwiched between the foil and the surface of the central column 12.

[0057] When the second conductive foil 32 and the third conductive foil 33 are wrapped from the outer side wall to the inner side wall of the first base plate 113, the bend should be made with an arc transition (the bending radius is exemplary not less than 10 times the foil thickness), and an insulating corner guard (not shown in the figure) is provided at the junction of the inner and outer side walls of the first base plate 113 to avoid foil damage and electric field concentration at the corners.

[0058] The connection between the second conductive foil 32, the third conductive foil 33 and the first conductive foil 31 can be welding, conductive adhesive bonding, mechanical pressing, or integral molding (e.g., formed by bending a single sheet of foil multiple times) to ensure the electrical continuity and common-mode current discharge capability of the shield. The material and thickness of the second conductive foil 32 and the third conductive foil 33 can be the same as or different from the first conductive foil 31; the thickness of the second conductive foil 32 and the third conductive foil 33 is 0.05 mm to 0.5 mm, and this application does not limit this.

[0059] In some embodiments, when the axial dimension of the air gap 13 along the central column 12 is the air gap depth d, the minimum distance L2 between the second conductive foil 32 and the air gap 13 is not less than 5 times the air gap depth d, and the minimum distance L3 between the third conductive foil 33 and the air gap 13 is not less than 5 times the air gap depth d, that is, L2≥5d and L3≥5d.

[0060] Among them, the minimum spacing L2 and L3 refer to the minimum straight-line distance between the edge point of the second conductive foil 32 and the third conductive foil 33 closest to the air gap 13 and the air gap 13, which is measured along the axial direction of the central column 12.

[0061] It is worth noting that the diffusion and attenuation range of the edge magnetic flux is directly related to the air gap depth. When the magnetic flux at air gap 13 diverges outward, its magnetopotential drop is mainly concentrated in a region centered on the air gap and with a scale comparable to the air gap depth. Finite element simulation and actual measurements show that the magnetic flux density at the air gap edge decreases radially and axially from the air gap end face according to an approximately exponential law. The range of its significant influence area is approximately 3 to 5 times the air gap depth. In areas more than 5 times the air gap depth away from the air gap, the edge magnetic flux density has attenuated to a lower proportion of the magnetic density at the air gap center. If the conductive foil is too close to air gap 13, the conductive foil will be in the region with the highest edge magnetic flux density. The induced eddy currents within the foil will be too large, causing the conductive foil to heat up severely, and the shielding layer will become a new heat source. At the same time, the conductive foil near air gap 13 is equivalent to a short-circuit turn, which will significantly reduce the excitation inductance and increase the air gap reluctance. This equivalent "short-circuit" effect will cause the transformer excitation current to rise and losses and temperature rise to worsen. Maintaining sufficient spacing also ensures that there is a necessary medium-voltage insulation distance and surface creepage distance between the air gap 13 and the winding 20, and between the air gap 13 and the conductive foil, and preserves an axial heat dissipation airflow channel to prevent the heat in the air gap 13 area from being "blocked" by the conductive foil.

[0062] Therefore, setting L2≥5d and L3≥5d can achieve a balance between shielding effectiveness and the loss, temperature rise, and insulation margin of the conductive foil itself. More preferably, 5d≤L2≤(0.3~0.6)H and 5d≤L3≤(0.3~0.6)H; where H is the total axial length of the central column 12, i.e., the winding height of the winding 20, thereby maximizing the shielding area by ensuring the conductive foil covers a larger area of ​​the central column 12 without entering the strong edge magnetic flux region. L2 and L3 can be equal or unequal; this application does not limit this.

[0063] In some embodiments, perforations or mesh foils may be formed on the second conductive foil 32 and the third conductive foil 33 to reduce eddy current losses within the foil, reduce weight, and allow the cooling medium to pass through laterally; a magnetic material layer (e.g., ferrite soft magnetic sheet, nanocrystalline composite sheet) may also be added to the side of the second conductive foil 32 and the third conductive foil 33 near the winding 20 to further improve the shunting capability of the edge magnetic flux.

[0064] It is worth noting that the insulation between the shield formed by the first conductive foil 31, the second conductive foil 32, and the third conductive foil 33 and the winding 20 is ensured by the insulation layer of the winding 20 itself, the first mounting member 25, the insulating casting body 21, and necessary insulating spacers; for example, the surfaces of the second conductive foil 32 and the third conductive foil 33 facing the winding 20 are covered with a polyimide film or epoxy coating with a thickness of 0.02 mm to 0.5 mm. After assembly, the first conductive foil 31, the second conductive foil 32, and the third conductive foil 33 should not have electrical contact with any charged conductor of the winding 20 or the magnetic surface of the magnetic core 10.

[0065] In addition, by binding the first conductive foil 31, the second conductive foil 32, and the third conductive foil 33 to parts of the frame post 11 and the middle post 12, the potential of the outer side of the magnetic core 10 can be effectively made consistent. Since the middle post 12 requires air gap adjustment of inductance, it is more complicated to handle the equipotential of the middle post 12. It is necessary to ensure that the magnetic core 10 is in contact with each conductive foil, and to ensure that the leakage flux of the air gap 13 does not cut the conductive foils and cause eddy currents. Therefore, the air gap 13 needs to be set on one side of the middle post 12, and the second conductive foil 32 and the third conductive foil 33 extend from the other side of the middle post 12 to a certain distance from the air gap 13.

[0066] In some embodiments, to reduce eddy current losses, at least one of the frame post 11 and the middle post 12 includes at least two magnetic laminations 14, with an insulating structure 15 between each pair of adjacent magnetic laminations 14 to ensure that each pair of adjacent magnetic laminations 14 are insulated from each other. Both the frame post 11 and the middle post 12 are constructed by stacking magnetic laminations 14.

[0067] In some embodiments, the thickness of the magnetic stack 14 is 0.02 mm to 0.5 mm, for example, the magnetic stack 14 is 0.025 mm (amorphous / nanocrystalline ribbon), 0.10 mm to 0.20 mm (oriented silicon steel) or 1 mm to 3 mm (ferrite plate).

[0068] In some embodiments, the insulating structure 15 includes an insulating heat sink 151, which is disposed between each two adjacent magnetic stacks 14 and is thermally connected to the two adjacent magnetic stacks 14.

[0069] Specifically, the insulating heat sink 151 is an insulator electrically and has a thermal conductivity significantly higher than that of conventional insulating paper and insulating varnish. The material of the insulating heat sink 151 can be at least one of the following: boron nitride film or boron nitride-filled polymer film, alumina ceramic sheet, alumina or boron nitride-filled epoxy fiberglass film (thermally conductive prepreg), polyimide composite thermally conductive film, thermally conductive silicone rubber sheet, or mica composite thermally conductive sheet. The thickness of the insulating heat sink 151 is 0.01 mm to 0.5 mm, preferably 0.02 mm to 0.1 mm, in order to minimize the equivalent additional air gap and superposition factor loss of the magnetic circuit while ensuring insulation and voltage withstand capability.

[0070] It is worth noting that "thermal conductive connection" means that there is surface contact and a heat conduction path between the insulating heat sink 151 and the magnetic stacks 14 on both sides. The two can be bonded, pressed, glued or coated with thermally conductive interface materials (such as thermally conductive silicone grease, thermally conductive gel, phase change thermal pad), as long as there is no significant thermal insulation gap.

[0071] By making a complete magnetic core 10 into a stacked form, and each magnetic stack 14 is insulated and bonded, the area of ​​the magnetic core 10 perpendicular to the magnetic flux direction can be effectively reduced, thereby reducing the eddy current loss of the magnetic core 10 itself.

[0072] The stacking direction of the magnetic core 10 can be selected in two ways: First, the magnetic laminations 14 are stacked in a direction perpendicular to the axis of the central column 12. In this case, the normal direction of the magnetic laminations 14 is along the axial direction of the central column 12, and the insulating heat sink 151 connects the heat along the axial direction of the central column 12. The heat inside the magnetic core 10 is conducted along the axial direction of the central column 12 to the surface of the first base plate 113 and the second base plate 114 and dissipated. Second, the normal direction of the magnetic laminations 14 is along the radial direction of the central column 12, and the heat is conducted radially to the outer surface of the frame column 11 and evenly distributed by the first conductive foil 31. Both stacking directions are acceptable, and this application does not limit them.

[0073] After adopting the insulating heat sink 151, the temperature difference between the inside of the magnetic core 10 and the outer surface of the magnetic core 10 is significantly reduced, the highest hot spot temperature of the magnetic core 10 is lowered, and the loss of the magnetic core 10 (especially the loss component that increases with temperature) decreases accordingly. Thus, the working magnetic flux density or working frequency can be increased without increasing the volume of the magnetic core 10.

[0074] In addition, the insulating heat sink 151 also has the following functions: First, it serves as a buffer and stress distribution layer during stacking to prevent the magnetic stack 14 (especially brittle amorphous / nanocrystalline ribbon) from breaking under fastening pressure; Second, an air gap pad (not shown in the figure) can be set at the location of the air gap 13; Third, a thermally conductive insulating film with a certain degree of adhesion (such as thermally conductive prepreg) can bond the magnetic stack 14 into a whole after curing.

[0075] In other embodiments, the insulating structure 15 includes an insulating adhesive layer 152 disposed between each two adjacent magnetic laminations 14, and the two adjacent magnetic laminations 14 are bonded and fixed by the insulating adhesive layer 152.

[0076] Specifically, the insulating adhesive layer 152 is formed by curing an insulating adhesive, such as epoxy adhesive, polyurethane adhesive, silicone adhesive, acrylic adhesive, or anaerobic adhesive; the thickness of the insulating adhesive layer 152 is 0.005 mm to 0.2 mm, preferably 0.01 mm to 0.05 mm. Using thin-layer bonding can minimize the additional air gap effect while ensuring interlayer insulation, and facilitates the resistance to interlayer slippage caused by magnetostriction and short-circuit electrodynamics after the laminates are bonded into a whole.

[0077] In other embodiments, an insulating heat sink 151 may be provided between two adjacent magnetic stacks 14, and at least one side surface of the insulating heat sink 151 has an adhesive layer, so that the insulating heat sink 151 and the magnetic stack 14 can be thermally connected and bonded at the same time, achieving the combined effect of "low interlayer loss, low interlayer thermal resistance, high mechanical integrity and low noise".

[0078] Please continue reading. Figure 5 , Figure 5 for Figure 1 A schematic diagram of the winding structure in an embodiment of a medium-voltage solid-state transformer.

[0079] In some embodiments, the winding 20 includes an insulating casting body 21, a primary winding 22, a first-stage winding 23, and a second-stage winding 24, with the primary winding 22 embedded inside the insulating casting body 21.

[0080] In this transformer, the primary winding 22, the first-stage winding 23, and the second-stage winding 24 constitute the two windings on either side. The primary winding 22 is a high-voltage winding that withstands medium-voltage levels and is electrically connected to the high-voltage side of the solid-state transformer isolation stage converter. The first-stage winding 23 and the second-stage winding 24 are low-voltage windings and are electrically connected to the low-voltage side of the isolation stage converter. Of course, in other embodiments, the primary winding 22 can also be a low-voltage winding, and the first-stage winding 23 and the second-stage winding 24 can be high-voltage windings. This application does not limit the voltage levels of the two windings.

[0081] The primary winding 23 is arranged around the central column 12, forming a first heat dissipation duct 61 between the primary winding 23 and the central column 12. That is, there is an axially penetrating annular gap between the primary winding 23 and the outer circumferential surface of the central column 12, and this gap is the first heat dissipation duct 61.

[0082] The insulating casting body 21 is arranged around the primary winding 23, and a second heat dissipation air duct 62 is formed between the insulating casting body 21 and the primary winding 23. That is, there is an axially penetrating annular gap between the inner circumferential surface of the insulating casting body 21 and the outer circumferential surface of the primary winding 23.

[0083] The second-stage winding 24 is arranged around the insulating casting body 21, forming a third heat dissipation duct 63 between it and the insulating casting body 21. That is, there is an axially penetrating annular gap between the inner circumferential surface of the second-stage winding 24 and the outer circumferential surface of the insulating casting body 21; and the second-stage winding 24 is electrically connected to the first-stage winding 23.

[0084] It can be seen that the following coaxial layers are formed in the radial direction from the inside to the outside: central column 12, first heat dissipation air duct 61, first primary winding 23, second heat dissipation air duct 62, insulating casting body 21 (with primary winding 22 embedded inside), third heat dissipation air duct 63, and second primary winding 24.

[0085] In some embodiments, the medium-voltage solid-state transformer 100 may be designed to lie flat, with the first heat dissipation duct 61, the second heat dissipation duct 62, and the third heat dissipation duct 63 running through the central column 12 along its axial direction, and its two ends communicating with the external space, thereby forming a natural convection "chimney-like" airflow channel; or cooling fans (not shown in the figure) may be installed at the air inlet and / or air outlet of the air duct, such as axial flow fans or centrifugal fans to form forced air cooling; and / or, a guide shroud (not shown in the figure) may be installed at the air outlet to guide the airflow through each air duct in sequence; and / or, a heat sink with ultra-high thermal conductivity (not shown in the figure) may be installed between the magnetic core 10 and each winding to assist in heat dissipation.

[0086] In some embodiments, the electrical connection between the primary winding 23 and the secondary winding 24 can be a parallel connection, that is, the number of turns of the primary winding 23 is equal to the number of turns of the secondary winding 24, one end of each is connected to a common busbar and the other end is connected to the low-voltage side terminal, forming a parallel shunt.

[0087] In some other embodiments, the winding 20 also includes a conductive connector 27. The electrical connection between the first winding 23 and the second winding 24 can also be a series connection, that is, one end of the first winding 23 and one end of the second winding 24 are connected through the conductive connector 27 to form a series winding, with its two ends serving as low-voltage side lead-out terminals 28.

[0088] The working mechanism of the above 20-layer winding arrangement is as follows: (1) Reduce leakage inductance and improve soft switching. The primary winding 23 and the secondary winding 24 are located on the inner and outer sides of the primary winding 22 and are electrically connected, forming a "sandwich" (interleaved) surround of the primary winding 22. The magnetomotive force of the primary winding 22 is balanced by the secondary magnetomotive forces on both sides in the radial direction. The leakage magnetic field is constrained in the narrow annular region between the primary winding 22 and the adjacent secondary winding, that is, in the gap between the second heat dissipation channel 62 and the third heat dissipation channel 63, thereby significantly reducing the leakage magnetic field energy and leakage inductance.

[0089] (2) Improved heat dissipation of cast-in-place high-voltage windings. The primary winding 22 is enclosed inside the insulating casting body 21, and its heat can only be conducted inward and outward through the insulating casting body 21. The second heat dissipation duct 62 and the third heat dissipation duct 63 are located outside the inner and outer surfaces of the insulating casting body 21, respectively, so that both surfaces of the insulating casting body 21 are in contact with the flowing cooling medium, forming "bidirectional heat dissipation", which solves the inherent problem of the difficulty in dissipating heat inside the cast-in-place high-voltage winding; the innermost primary winding 23 can also dissipate heat directly to the side of the central column 12 and the end through the first heat dissipation duct 61. The three ducts are axially connected, and the cooling medium forms a continuous flow under the buoyancy force or the drive of the fan.

[0090] (3) Reduce winding eddy current losses. The secondary side current is divided into inner and outer windings 23 and 24, which reduces the thickness of a single conductor. Combined with the spiral winding (see below), the conductor is oriented radially with a narrow side, which further reduces the effective thickness of the conductor in the direction of the edge magnetic flux, thereby reducing additional eddy current losses.

[0091] Furthermore, the primary winding 22, the first secondary winding 23, and the second secondary winding 24 are all single-layer coils, which can effectively reduce the parasitic capacitance of the same coil. Their input and output lines are located at different positions to avoid the problem of local electric field concentration and excessive parasitic capacitance caused by excessive voltage due to adjacent input and output lines. Moreover, the arrangement of the first secondary winding 23 and the second secondary winding 24 sandwiching the primary winding 22 from opposite sides effectively reduces the secondary leakage inductance. Therefore, when the medium-voltage solid-state transformer 100 is applied in a DC-DC (Direct Current) converter, it can effectively reduce the resonant frequency shift of the DC-DC converter.

[0092] Furthermore, in some embodiments, at least two first support portions 211 protrude from the outer sidewall of the insulating casting body 21 facing the secondary winding 24, and the at least two first support portions 211 abut against the inner sidewall of the secondary winding 24 facing the insulating casting body 21, so that the insulating casting body 21 and the secondary winding 24 are spaced apart.

[0093] In other embodiments, at least two second support portions 212 protrude from the inner wall of the insulating casting body 21 facing the primary winding 23, and the at least two second support portions 212 abut against the outer wall of the primary winding 23 facing the insulating casting body 21, so that the insulating casting body 21 is spaced apart from the primary winding 23.

[0094] Both the first support portion 211 and the second support portion 212 are integrally formed with the insulating casting body 21. For example, corresponding grooves are provided on the core of the casting mold, and the casting is completed in one step after curing. The number of first support portions 211 is exemplarily 2, 3, 4, 6 or 8, evenly distributed along the circumference of the insulating casting body 21. The number and arrangement of the second support portions 212 are similar, and the number of both can be the same or different. The first support portions 211 and the second support portions 212 can be continuous ribs or spaced bosses along the axial direction. For example, ribs that extend continuously along the axial direction are used, and their axial length is equal to or slightly less than the axial length of the insulating casting body 21. The radial protrusion height of the first support portions 211 and the second support portions 212 is equal to the gap of the corresponding heat dissipation duct, exemplarily 0.5mm to 5mm, and further exemplarily 1mm to 3mm.

[0095] The first support portion 211 and the second support portion 212 use a "point support" method to determine the air duct gap, which has the following effects: First, it ensures that the second heat dissipation air duct 62 and the third heat dissipation air duct 63 remain connected and have a uniform gap, preventing the windings 23 and 24 from sticking to the insulating casting body 21 due to their own weight or short-circuit electrodynamics, thus avoiding air duct blockage; Second, the insulating casting body 21 and the windings 23 and 24 only contact each other through the support portion, while the rest of the parts remain spaced, reducing the risk of interface heat accumulation and interface partial discharge caused by large-area contact; Third, the protruding support portion causes disturbance when the cooling medium flows through, enhancing convective heat transfer; Fourth, the support portion causes the surface creepage path to form a bypass at the support portion, extending the actual creepage distance and increasing the withstand voltage margin under the same axial insulation distance.

[0096] Furthermore, the first support portion 211 is provided with a first heat dissipation through hole 213, which extends in a direction parallel to the center line of the central column 12; and / or, the second support portion 212 is provided with a second heat dissipation through hole 214, which extends in a direction parallel to the center line of the central column 12.

[0097] The first heat dissipation through-hole 213 and the second heat dissipation through-hole 214 are through-holes opened on the support body along the axial direction. Their cross-sectional shape can be circular, elliptical, oblong, or polygonal. The hole diameter (or equivalent diameter) can be 1 mm to 10 mm. The number of through-holes provided on each support is exemplarily 1 to 5. The purpose of providing through-holes is: firstly, to allow the cooling medium to flow axially in the main air duct formed on the outer edge of the support and to flow laterally through the support body, flushing the winding surface that was originally located on the "leeward side" of the support and eliminating the heat dissipation dead zone; secondly, the inlet and outlet of the through-holes form a bypass path in the surface direction, further extending the creepage distance; and thirdly, to reduce the weight of the insulating casting 21 and reduce the shrinkage stress and cracking tendency during the casting and curing process.

[0098] In some embodiments, the winding 20 further includes a first mounting member 25, which is arranged around the central column 12 and spaced apart in the first heat dissipation duct 61, and the primary winding 23 is spirally wound on the outer side wall of the first mounting member 25 away from the central column 12.

[0099] In some embodiments, the winding 20 further includes a second mounting member 26, which is disposed around the insulating casting body 21 and spaced apart in the third heat dissipation duct 63, and the second stage winding 24 is spirally wound on the outer side wall of the second mounting member 26 away from the insulating casting body 21.

[0100] The first mounting component 25 and the second mounting component 26 are insulating frames, which are exemplary cylindrical (cylindrical or polygonal cylindrical) structures. The material is insulating and has a certain mechanical strength, such as epoxy glass cloth rolls, aramid paper rolls, polyimide rolls, polyether ether ketone, polyphenylene sulfide, or ceramic rolls. This application does not limit the specific materials used.

[0101] It is worth noting that "intermittently arranged in the first heat dissipation duct 61" and "intermittently arranged in the third heat dissipation duct 63" means that annular gaps are maintained between the first mounting component 25 and the central column 12, and between the second mounting component 26 and the insulating casting body 21. The mounting components themselves do not fill the entire duct. The duct is formed by the gaps between the mounting components and adjacent components, as well as the openings on the mounting components. For example, the inner diameter of the first mounting component 25 is larger than the outer diameter of the central column 12, and the radial gap between them is 1mm to 8mm; the inner diameter of the second mounting component 26 is larger than the outer diameter of the insulating casting body 21 (or larger than the outer edge diameter of the first support 211), and the radial gap between them is 1mm to 8mm. To further ensure the continuity of the duct, ventilation slots or through holes extending axially can be provided on the first mounting component 25 and the second mounting component 26.

[0102] Furthermore, "spiral winding" refers to the primary winding 23 and the secondary winding 24 being wound on the outer wall of the mounting component with a helical angle, with an axial spacing of one pitch between adjacent turns, thus forming continuous helical grooves on the winding surface. The advantages of helical winding are: firstly, the spaces between adjacent turns and within the helical grooves are filled with cooling medium, forming a porous heat dissipation network inside the winding. The cooling medium can directly scour the conductor surface, resulting in significantly higher heat dissipation area and efficiency than closely wound layers; secondly, helical winding typically uses copper strip, aluminum foil, or flat wire, with its narrow side facing radially, reducing the effective thickness of the conductor in the edge magnetic flux direction, thereby reducing high-frequency eddy current losses; thirdly, the mounting component provides a defined geometry for the winding, making the insulation gap between the winding and the magnetic core 10 and the insulating casting 21 stable, controllable, and reproducible; fourthly, the inter-turn voltage of the helical winding is low (each turn only bears one pitch voltage), which is beneficial for medium-voltage insulation design.

[0103] In some embodiments, the insulating casting body 21 includes an insulating connector 2101, a first insulator 2102, and a second insulator 2103. The insulating connector 2101 has at least two first baffles 2104 protruding from its outer side wall away from the central column 12. The at least two first baffles 2104 are arranged parallel to each other and spaced apart. A first guide groove 2105 is formed between each two adjacent first baffles 2104. The primary winding 22 is spirally wound in each first guide groove 2105 to facilitate the winding and forming of the corresponding coil. The first insulator 2102 and the second insulator 2103 clamp the insulating connector 2101 from opposite sides to cover the primary winding 22. That is, the insulating connector 2101 is disposed between the first insulator 2102 and the second insulator 2103.

[0104] In some embodiments, at least two second baffles 251 protrude from the outer side wall of the first mounting member 25 away from the central column 12. The at least two second baffles 251 are arranged parallel to each other and spaced apart. A second guide groove 252 is formed between each two adjacent second baffles 251. Specifically, the primary winding 23 is wound in a spiral shape in each second guide groove 252 to facilitate the winding of the corresponding coil.

[0105] In some embodiments, at least two third baffles 261 protrude from the outer side wall of the second mounting member 26 away from the central column 12. The at least two third baffles 261 are arranged parallel to each other and spaced apart. A third guide groove 262 is formed between each two adjacent third baffles 261. The second stage winding 24 is specifically wound in a spiral shape in each third guide groove 262 to facilitate the winding of the corresponding coil.

[0106] In some embodiments, the medium-voltage solid-state transformer 100 further includes a mounting frame (not shown), with the center column 12 and the first mounting member 25 spaced apart from each other on the mounting frame, so that the primary winding 23 is spaced apart from the center column 12.

[0107] In some embodiments, the first mounting member 25 is spaced apart from the insulating casting body 21 on the mounting frame so that the primary winding 23 is spaced apart from the insulating casting body 21.

[0108] In some embodiments, the insulating casting body 21 is spaced apart from the second mounting member 26 on the mounting frame so that the insulating casting body 21 is spaced apart from the secondary winding 24.

[0109] It is worth noting that "spaced connection" means that the components are not directly pressed or attached to each other, but are positioned separately by mounting brackets, maintaining a designed gap between them. Thus, the coaxiality, axial position, and radial clearance between the components are uniformly guaranteed by the mounting brackets. The gap dimensions of the first heat dissipation duct 61, the second heat dissipation duct 62, and the third heat dissipation duct 63 are precisely controllable after assembly and remain stable under long-term operation, temperature cycling, and short-circuit impacts. Simultaneously, mechanical decoupling is achieved between the magnetic core 10 and the winding 20: the magnetostrictive deformation and high-frequency vibration of the magnetic core 10 are not directly transmitted to the winding conductors, and the self-weight and short-circuit electrodynamic force of the winding 20 are borne by the mounting brackets, preventing local compression or wear of the insulation layer. During assembly, the components can be sequentially fitted and pressed against the end plate axially, resulting in good assembly processability and the ability to be repaired.

[0110] In some embodiments, the second mounting member 26 has at least two third support portions (not shown) protruding from the inner sidewall of the insulating casting body 21, and the at least two third support portions abut against the outer sidewall of the insulating casting body 21 facing the secondary winding 24, so that the insulating casting body 21 and the secondary winding 24 are spaced apart.

[0111] In other words, the third support is located on the inner wall of the second mounting member 26, rather than on the outer wall of the insulating casting body 21. This allows the third support to be integrally formed with the second mounting member 26 (e.g., prefabricated during injection molding, compression molding, or rolling), eliminating the complexity of setting a separate boss on the surface of the insulating casting body 21. Simultaneously, the circumferential position of the third support corresponds to the helical pitch of the second winding 24, ensuring the support point falls within the inter-turn groove, preventing the support from compressing the conductor. After the second mounting member 26 is positioned on the end plate, the gap of the third heat dissipation duct 63 is automatically determined.

[0112] In some embodiments, the number of third supports is 2 to 8, evenly distributed circumferentially, with a radial height of 0.5 mm to 5 mm, and the shape can be a continuous annular rib or a spaced boss.

[0113] It should be noted that when the third support and the first support 211 are provided simultaneously, either one can abut against the surface of the insulating casting 21, or they can abut against different positions in the axial direction. This application does not limit this. Similarly, the second support 212 can also be provided on the outer side wall of the first mounting member 25 and abut against the inner side wall of the first primary winding 23.

[0114] In addition, insulating spacers, insulating baffles, or insulating end rings can be installed between the insulating casting body 21 and the first mounting part 25, between the insulating casting body 21 and the second mounting part 26, and at the lead-out ends of windings 23 and 24 to further separate potentials and extend the creepage path. The electrical connection between the second stage winding 24 and the first stage winding 23 can be completed at the axial end of winding 20 through a connecting bus (copper bus, aluminum bus, or braided flexible connection). An insulating heat shrink tube or a silicone rubber sleeve can be fitted over the connecting bus.

[0115] In some embodiments, the medium-voltage solid-state transformer 100 further includes a skirt 50 connected to the insulating cast body 21. The skirt 50 protrudes radially outward from the outer surface of the insulating cast body 21 to extend the surface creepage path of the outer insulation and block the formation of a continuous water film on the surface, thereby improving the withstand voltage level of the medium-voltage solid-state transformer 100 in outdoor, humid, or polluted environments.

[0116] In summary, the medium-voltage solid-state transformer 100 provided in this application embodiment effectively shields the magnetic flux at the edge of the air gap without occupying the magnetic core window by providing a first conductive foil 31 on the outer wall of the frame column 11 of the magnetic core 10, and arranging a second conductive foil 32 and a third conductive foil 33 connected to the first conductive foil 31 along the outer periphery of the frame body and the central column 12 of the magnetic core 10, and limiting the minimum distance between the conductive foil and the air gap 13 to not less than 5 times the depth of the air gap. This significantly reduces the additional eddy current loss and local hot spots of the winding 20 near the air gap. Furthermore, by providing an insulating heat sink 151 or an insulating adhesive layer 152 with both insulation and heat conduction functions between the magnetic laminations 14, the transformer effectively shields the magnetic flux at the edge of the air gap without occupying the magnetic core window. The technical challenge of "contradictory insulation and heat conduction" in high-frequency magnetic cores has been solved. By coaxially staggering the arrangement of "central column 12, primary winding 23, insulating casting body 21 (containing primary winding 22), and secondary winding 24" and three axially connected first heat dissipation air ducts 61, second heat dissipation air ducts 62, and third heat dissipation air ducts 63, the unity of low leakage inductance and high-efficiency heat dissipation is achieved. By combining the support part and heat dissipation through holes, the first mounting part 25, the second mounting part 26 and the mounting frame, the unity of heat dissipation, insulation, mechanical support and assembly processability is achieved. By directly connecting the umbrella skirt 50 and the insulating casting body 21, the unity of medium-voltage external insulation performance and expanded heat dissipation surface is achieved.

[0117] Unlike existing technologies, the medium-voltage solid-state transformer provided in this application uses a first conductive foil to be sleeved on the outer wall of its magnetic core frame column away from the central column. This allows the magnetic core surface to be made equipotential using the first conductive foil, suppressing partial discharge and common-mode interference, thereby avoiding the introduction of eddy current losses and effectively reducing the risk of partial discharge.

[0118] In the several embodiments provided in this application, it should be understood that the disclosed medium-voltage solid-state transformer can be implemented in other ways. For example, the medium-voltage solid-state transformer embodiments described above are merely illustrative, and the division of each functional part is only a logical functional division. In actual implementation, there may be other division methods, such as multiple functional parts being combined or integrated into several modules, or each functional part existing physically separately, etc.

[0119] The above description is merely an embodiment of this application and does not limit the patent scope of this application. Any equivalent structural or principle transformations made based on the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.

Claims

1. A medium-voltage solid-state transformer, characterized in that, The medium-voltage solid-state transformer includes a magnetic core, windings, and a first conductive foil; The magnetic core includes a frame post and a middle post, the middle post is disposed within a frame formed by the frame post, and the winding is wound around the middle post; The first conductive foil is sleeved on the outer wall of the frame column opposite to the middle column.

2. The medium-voltage solid-state transformer according to claim 1, characterized in that, The frame column includes a first side plate, a second side plate, a first bottom plate, and a second bottom plate. The first side plate, the first bottom plate, the second side plate, and the second bottom plate are connected end to end to enclose and form a rectangular frame. One end of the central column is connected to the inner wall of the first base plate facing the second base plate, and an air gap is provided between the other end of the central column and the second base plate.

3. The medium-voltage solid-state transformer according to claim 2, characterized in that, The medium-voltage solid-state transformer further includes a second conductive foil and a third conductive foil, with one end of the second conductive foil and one end of the third conductive foil both connected to the first conductive foil; The other end of the second conductive foil extends from the outer side wall of the first base plate to the inner side wall of the first base plate, and extends along the first side wall of the central column toward the air gap, so as to be spaced apart from the air gap; wherein, the first side wall is the side wall of the central column facing the first side plate; The other end of the third conductive foil extends from the outer side wall of the first base plate to the inner side wall of the first base plate, and extends along the second side wall of the central column toward the air gap, so as to be spaced apart from the air gap; wherein, the second side wall is the side wall of the central column facing the second side plate.

4. The medium-voltage solid-state transformer according to claim 3, characterized in that, The dimension of the air gap along the axial direction of the central column is the air gap depth; the minimum distance between the second conductive foil and the air gap is not less than 5 times the air gap depth, and the minimum distance between the third conductive foil and the air gap is not less than 5 times the air gap depth.

5. The medium-voltage solid-state transformer according to claim 1, characterized in that, At least one of the frame column and the central column includes at least two magnetic laminations, and an insulating structure is provided between each two adjacent magnetic laminations so that each two adjacent magnetic laminations are insulated from each other.

6. The medium-voltage solid-state transformer according to claim 5, characterized in that, The insulating structure includes an insulating heat sink, which is disposed between each two adjacent magnetic stacks and is thermally connected to the two adjacent magnetic stacks.

7. The medium-voltage solid-state transformer according to claim 5, characterized in that, The insulating structure includes an insulating adhesive layer, which is disposed between each pair of adjacent magnetic laminations, and the two adjacent magnetic laminations are bonded and fixed by the insulating adhesive layer.

8. The medium-voltage solid-state transformer according to claim 1, characterized in that, The winding includes an insulating cast body, a primary winding, a first-stage winding, and a second-stage winding, wherein the primary winding is embedded inside the insulating cast body; The primary winding is arranged around the central column, forming a first heat dissipation airflow channel between it and the central column; The insulating casting body is arranged around the primary winding, forming a second heat dissipation air duct between it and the primary winding; The second-stage winding is arranged around the insulating casting body, forming a third heat dissipation air duct between the second-stage winding and the insulating casting body, and the second-stage winding is electrically connected to the first-stage winding.

9. The medium-voltage solid-state transformer according to claim 8, characterized in that, At least two first support portions protrude from the outer side wall of the insulating casting body facing the second stage winding, and the at least two first support portions abut against the inner side wall of the second stage winding facing the insulating casting body, so that the insulating casting body is spaced apart from the second stage winding; And / or, the insulating casting body has at least two second support portions protruding from the inner sidewall facing the primary winding, and the at least two second support portions abut against the outer sidewall facing the primary winding, so that the insulating casting body is spaced apart from the primary winding.

10. The medium-voltage solid-state transformer according to claim 9, characterized in that, The first support portion is provided with a first heat dissipation through hole, which extends along a direction parallel to the center line of the central column; And / or, the second support portion is provided with a second heat dissipation through hole, the second heat dissipation through hole extending in a direction parallel to the center line of the central column.

11. The medium-voltage solid-state transformer according to claim 8, characterized in that, The winding also includes a first mounting member, which is arranged around the central column and spaced apart in the first heat dissipation duct. The first primary winding is spirally wound on the outer side wall of the first mounting member away from the central column. And / or, the winding further includes a second mounting member, which is arranged around the insulating casting body and spaced apart in the third heat dissipation duct, and the second stage winding is spirally wound on the outer side wall of the second mounting member away from the insulating casting body.

12. The medium-voltage solid-state transformer according to claim 11, characterized in that, The medium-voltage solid-state transformer also includes a mounting frame, and the center column is connected to the first mounting component at a distance from the mounting frame so that the first primary winding is spaced apart from the center column; And / or, the first mounting member is spaced apart from the insulating casting body by the mounting frame, so that the first primary winding is spaced apart from the insulating casting body; And / or, the insulating casting body is spaced apart from the second mounting member by the mounting frame, so that the insulating casting body is spaced apart from the second stage winding.

13. The medium-voltage solid-state transformer according to claim 11, characterized in that, The second mounting member has at least two third support portions protruding from the inner sidewall facing the insulating casting body. The at least two third support portions abut against the outer sidewall facing the second stage winding of the insulating casting body, so that the insulating casting body is spaced apart from the second stage winding.

14. The medium-voltage solid-state transformer according to any one of claims 8-13, characterized in that, The medium-voltage solid-state transformer also includes a skirt, which is connected to the insulating cast body.