A proton exchange membrane fuel cell membrane electrode cathode catalyst layer, membrane electrode and its preparation method
By introducing amphiphilic supramolecular host compounds into the cathode catalyst layer of a proton exchange membrane fuel cell, the proton conduction and oxygen transport pathways were optimized, solving the problems of low Pt utilization and mutual constraints between conduction and diffusion, and achieving high-efficiency output performance of the fuel cell.
Patent Information
- Application Number
- CN202611315692.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-17
AI Technical Summary
The existing proton exchange membrane fuel cell cathode catalyst layer has low Pt utilization and the mutual constraints between proton conduction and oxygen diffusion make it difficult to improve output performance.
Introducing amphiphilic supramolecular host compounds, such as calixarenes, cucurbiturates, and crown ether macrocyclic compounds, into the cathode catalytic layer allows for the capture of sulfonate groups through hydrogen bond networks, constructing ordered hydrophilic and hydrophobic cavities and optimizing proton conduction and oxygen transport pathways.
Significantly improves Pt utilization, reduces oxygen transport resistance, enhances the power output performance of proton exchange membrane fuel cells, achieves efficient proton conduction and oxygen diffusion synergy, and breaks through the performance bottleneck of traditional catalyst layers.
Smart Images

Figure CN123120754A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of proton exchange membrane fuel cell technology, and particularly to a proton exchange membrane fuel cell membrane electrode cathode catalyst layer, membrane electrode, and preparation method thereof. Background Technology
[0002] As a core technology in the hydrogen energy industry, the slow kinetics of the oxygen reduction reaction (ORR) at the cathode of proton exchange membrane fuel cells (PEMFCs) have been a persistent obstacle to the development of sustainable electrochemical energy conversion technologies.
[0003] Platinum-loaded carbon (Pt / C) nanoparticles are currently the most widely used ORR catalysts. However, the high cost, scarcity, and low Pt utilization of Pt / C catalysts have become the biggest bottlenecks restricting the large-scale commercialization of PEMFCs. To improve the output performance of PEMFCs, researchers have attempted to optimize the catalyst bulk structure, such as alloying Pt with transition metals (e.g., Co, Ni) or constructing ordered intermetallic compound structures to slow down the dissolution of non-noble metals. However, these approaches focus on the activity and stability of the catalyst bulk and do not improve the ion and gas transport behavior at the three-phase interface in the catalyst layer, thus having limited effect on improving output performance.
[0004] Besides the activity of the catalyst itself, the microenvironment of the three-phase interface in the catalyst layer is equally crucial to performance. Perfluorosulfonic acid (PFSA) ionomers, acting as proton conductors, function to transport protons required for the ORR reaction. However, the sulfonic acid side chains of PFSA ionomers strongly adsorb onto the Pt surface, poisoning the active sites and resulting in low Pt utilization. Simultaneously, the hydrophobic backbone of PFSA ionomers tends to densely accumulate on the Pt surface, causing severe oxygen transport obstruction. Therefore, within the same three-phase interface, proton conduction and oxygen transport mutually restrict each other, making synergistic optimization difficult.
[0005] In recent years, some studies have attempted to introduce molecular modulators (e.g., covalent organic frameworks, functional small molecules) to block sulfonate adsorption. However, these strategies often have trade-offs: either they disrupt the proton conduction network of the ionomer, leading to a significant increase in proton transport resistance; or the molecular modulators themselves are prone to dissolution, failing to guarantee long-term stability. For example, Chinese patent application CN121885654A discloses a silanol-modified catalytic layer. While this scheme can reduce the poisoning of Pt active sites by sulfonate groups to some extent through silanol modification, there is still room for improvement in constructing cross-scale ordered mass transfer channels and balancing ultra-low oxygen transport resistance.
[0006] The statements herein provide only background information in relation to the present invention and do not necessarily constitute prior art. Summary of the Invention
[0007] The purpose of this invention is to provide a method for preparing the cathode catalyst layer of a fuel cell membrane electrode, which solves the problems of low Pt utilization and mutual restriction between proton conduction and oxygen diffusion in existing cathode catalyst layers.
[0008] To achieve the above objectives, the present invention provides a method for preparing the cathode catalyst layer of a proton exchange membrane fuel cell membrane electrode, comprising: Step 1: Provide a gas diffusion layer; Step 2: Disperse the platinum-based catalyst in an alcohol-water mixed solvent, then add the amphiphilic supramolecular host compound and perfluorosulfonic acid ionomer in sequence, mix thoroughly, and obtain the cathode slurry; The amphiphilic supramolecular host compound has a macrocyclic host skeleton that forms a hydrophobic cavity; the outer edge of the macrocyclic host skeleton has hydrogen-bonding active sites that can form hydrogen bonds with the sulfonate groups of the perfluorosulfonic acid ionomer; the platinum-based catalyst contains a carbon support, and the mass ratio of the amphiphilic supramolecular host compound to the carbon support is 0.05:1 to 0.2:1. Step 3: The cathode slurry is coated onto one side surface of the gas diffusion layer and dried to obtain the cathode catalyst layer.
[0009] Optionally, the amphiphilic supramolecular host compound comprises at least one of calixarenes, cucurbiturates, and crown ether macrocyclic compounds; the hydrogen bond active site is at least one hydrogen bond donor or hydrogen bond acceptor group selected from hydroxyl, carbonyl, or heteroatom groups.
[0010] Optionally, the mass ratio of the perfluorosulfonic acid ionomer to the carbon support is 0.6:1 to 1.2:1.
[0011] Optionally, in step 2, the alcohol-water mixed solvent is a mixture of anhydrous ethanol and ultrapure water in a volume ratio of 5:1 to 15:1; the mixing is performed by ultrasonic treatment for a time of 60 min to 120 min; and the solid concentration of the cathode slurry is 2 mg / mL to 5 mg / mL.
[0012] Optionally, in step 2, the perfluorosulfonic acid ionomer is added in the form of a perfluorosulfonic acid ionomer solution, wherein the perfluorosulfonic acid ionomer solution is at least one of DuPont Nafion solutions D520, D521, D1020, D1021, or D2020.
[0013] Optionally, in step 3, the coating method is ultrasonic spraying; the drying treatment is natural air drying or drying at 80℃~100℃.
[0014] Optionally, the platinum-based catalyst is platinum nanoparticles supported on carbon black, or platinum-based alloy nanoparticles supported on carbon black; the platinum-based alloy is a PtCo alloy, a PtNi alloy, or a PtCoCe alloy; and the platinum loading of the cathode catalyst layer is 0.05 mg / cm³. 2 ~0.4mg / cm 2 .
[0015] This invention also provides a method for preparing a membrane electrode for a proton exchange membrane fuel cell, comprising: The method described above for preparing a proton exchange membrane fuel cell membrane electrode cathode catalyst layer provides a cathode catalyst layer and another gas diffusion layer. A platinum-based catalyst is coated onto one side surface of the other gas diffusion layer and then dried to obtain an anode catalyst layer. The gas diffusion layer with the cathode catalyst layer, the proton exchange membrane, and the gas diffusion layer with the anode catalyst layer are stacked sequentially and assembled by applying contact pressure to obtain the membrane electrode assembly of the proton exchange membrane fuel cell.
[0016] Optionally, the platinum loading of the anode catalyst layer is 0.1 mg / cm³. 2 ~0.4mg / cm 2 The contact pressure is 0.5MPa to 2MPa; the assembly ambient temperature is room temperature to 80℃.
[0017] The present invention also provides a proton exchange membrane fuel cell membrane electrode, which is prepared by the above-described preparation method.
[0018] Compared with the prior art, the technical solution of the present invention has at least the following beneficial effects: In the cathode catalyst layer of this invention, amphiphilic supramolecular host compounds (calixarenes, cucurbiturates, crown ether macrocyclic compounds) are introduced. These amphiphilic supramolecular host compounds have a rigid hydrophobic cavity and hydrogen-bonded active sites distributed on their outer edges. On the one hand, the hydrogen-bonded active sites (at least one hydrogen bond donor or acceptor group among hydroxyl, carbonyl, or heteroatom groups) can form hydrogen bonds with the sulfonate groups of the perfluorosulfonic acid ionomer, preferentially capturing sulfonate groups at the molecular scale, thereby inhibiting the direct adsorption of sulfonate groups on the Pt surface, reducing the sulfonate coverage of the Pt surface to below 9%, releasing the Pt active sites that were originally poisoned by sulfonate, and significantly improving Pt utilization and intrinsic catalyst activity. On the other hand, the amphiphilic supramolecular host compounds, through the hydrogen bond network... While reducing the sulfonate coverage, the complex can induce the formation of regular hydrophilic water zones with a spacing of 4nm~4.5nm in the perfluorosulfonic acid ionomer, avoiding dense packing and improving proton conduction and oxygen transport efficiency. In addition, the inherent rigid hydrophobic cavity of the amphiphilic supramolecular host compound can accommodate oxygen molecules, forming host-guest inclusion complexes, which can construct a fast oxygen transport channel and significantly reduce oxygen transport resistance. This achieves the joint optimization of proton conduction and oxygen transport paths, breaking through the bottleneck of the trade-off between proton conduction and gas diffusion in traditional cathode catalyst layers.
[0019] Furthermore, the proton exchange membrane fuel cell fabricated using the membrane electrode of this invention exhibits excellent power output performance. Under H2-O2 (back pressure 100 kPaabs) test conditions, the peak power density of the membrane electrode fabricated according to this invention can reach 2.16 W / cm². 2 Compared to traditional membrane electrodes, the output performance is significantly improved.
[0020] Furthermore, the preparation method of this invention is simple, requires no complex nanofabrication equipment, is fully compatible with existing production processes, and is suitable for large-scale production. In addition, the preparation method of this invention is universally applicable to various catalyst systems, including commercial Pt / C catalysts and platinum-based catalysts supported on ordered supports, all of which achieve performance improvements. Attached Figure Description
[0021] Figure 1 This invention provides a flowchart of a method for preparing the cathode catalyst layer of a proton exchange membrane fuel cell.
[0022] Figure 2 The graph shows a comparison of the power density of Examples 1 to 3 and Comparative Example 1.
[0023] Figure 3 The graph shows a comparison of the power density of Examples 3 to 7 with that of Comparative Example 1.
[0024] Figure 4This is a comparison chart of the maximum power density of Examples 3 to 7.
[0025] Figure 5 This is a comparison chart of the power density of Example 3 and Example 8.
[0026] Figure 6 This is a comparison graph of the power density of Example 9 and Comparative Example 2.
[0027] Figure 7 The cyclic voltammetry curves are for Example 9 and Comparative Example 2.
[0028] Figure 8 This is a comparison diagram of the electrochemical active area of Example 9 and Comparative Example 2. Detailed Implementation
[0029] The following detailed description, in conjunction with the accompanying drawings and specific embodiments, provides a proton exchange membrane fuel cell cathode catalyst layer, membrane electrode, and its preparation method according to the present invention. The advantages and features of the present invention will become clearer from the following description. It should be noted that the accompanying drawings are in a very simplified form and use non-precise proportions, used only to facilitate and clarify the illustration of the embodiments of the present invention. Please refer to the accompanying drawings to make the objectives, features, and advantages of the present invention more apparent and understandable. It should be understood that the structures, proportions, sizes, etc., depicted in the accompanying drawings are only for illustrative purposes to aid those skilled in the art and are not intended to limit the implementation conditions of the present invention. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in proportions, or adjustments to the size, without affecting the effects and objectives achieved by the present invention, should still fall within the scope of the technical content disclosed in the present invention.
[0030] The "I / C ratio" mentioned in this article refers to the mass ratio of perfluorosulfonic acid ionomer to carbon support.
[0031] The “host-guest inclusion complex” mentioned in this article refers to a non-covalent inclusion structure formed by oxygen molecules entering the hydrophobic cavity inside the amphiphilic supramolecular host compound molecule through van der Waals forces and hydrophobic interactions. This inclusion and dissociation is a reversible process.
[0032] like Figure 1 As shown, the present invention provides a method for preparing the cathode catalyst layer of a proton exchange membrane fuel cell, comprising: Step 101: Provide a gas diffusion layer.
[0033] The gas diffusion layer serves as the carrier of the cathode catalyst layer and can be a conventional gas diffusion layer in the art, such as carbon paper or carbon cloth. In some embodiments, the gas diffusion layer is Toray TGP-H-055 carbon paper.
[0034] Step 102: Disperse the platinum-based catalyst in an alcohol-water mixed solvent, then sequentially add an amphiphilic supramolecular host compound and a perfluorosulfonic acid ionomer, and sonicate to obtain a cathode slurry; wherein, the amphiphilic supramolecular host compound has a macrocyclic host framework that forms a hydrophobic cavity; the outer edge of the macrocyclic host framework has hydrogen-bonding active sites that can form hydrogen bonds with the sulfonate groups of the perfluorosulfonic acid ionomer; the platinum-based catalyst contains a carbon support, and the mass ratio of the amphiphilic supramolecular host compound to the carbon support is 0.05:1 to 0.2:1.
[0035] The platinum-based catalyst can specifically be carbon black-supported platinum nanoparticles (e.g., a Pt / C catalyst), or carbon black-supported platinum-based alloy nanoparticles, wherein the platinum-based alloy is a PtCo alloy, a PtNi alloy, or a PtCoCe alloy. The mass fraction of platinum in the platinum-based catalyst can be a conventional content such as 40 wt%.
[0036] The amphiphilic supramolecular host compound has a macrocyclic host skeleton. Specifically, the amphiphilic supramolecular host compound includes at least one of calixaranes, cucurbiturates, and crown ether macrocyclic compounds. These compounds exhibit amphiphilic properties—externally hydrophilic and internally hydrophobic—acting on both proton conduction and oxygen transport pathways, thereby jointly improving the microscopic mass transfer environment of the cathode catalyst layer. On one hand, the macrocyclic host structure has polar groups such as hydroxyl, carbonyl, ether oxygen, and amide nitrogen distributed on its outer edge. These groups act as hydrogen bond donors or acceptors, constituting hydrogen bond active sites. These groups can form stable hydrogen bonds with the sulfonate groups of the perfluorosulfonic acid ionomer, constructing a hydrogen bond network in the cathode catalyst layer. This hydrogen bond network can preferentially capture sulfonate groups, inhibiting their migration and adsorption to the Pt surface, reducing the coverage of sulfonate groups on the Pt surface, fully releasing the Pt active sites, and improving Pt utilization. Simultaneously, the amphiphilic supramolecular host compound binds to the sulfonate groups through its outer edge hydrogen bond active sites, inducing the perfluorosulfonic acid ionomer to form regular hydrophilic waters with a spacing of 4.0 nm to 4.5 nm, which is beneficial for forming long-range continuous proton transport channels and promoting proton conduction.
[0037] On the other hand, the inner wall of the cavity formed by the macrocyclic host framework is composed of a nonpolar hydrocarbon structure, creating a hydrophobic environment. The amphiphilic supramolecular host compound can be modified with different polymerization numbers or substituents to obtain different cavity sizes to suit the size of oxygen molecules. Oxygen, being a nonpolar small molecule, tends to enter the hydrophobic cavity according to the principle of "like dissolves like," forming a host-guest inclusion structure with the amphiphilic supramolecular host compound. Thus, the hydrophobic cavity constitutes a series of oxygen-containing units within the cathode catalyst layer. Oxygen molecules can sequentially enter and exit the hydrophobic cavity, transporting to the Pt active site, thereby avoiding the obstruction of the dense coating layer formed by the perfluorosulfonic acid ionomer on the surface of the platinum-based catalyst particles and shortening the oxygen mass transfer path.
[0038] The two mass transfer channels mentioned above are independent of each other at the molecular scale and do not interfere with each other. They can improve oxygen transport while maintaining the continuity of proton conduction, which is conducive to expanding the area of the proton-oxygen-electron three-phase reaction interface in the catalyst layer, thereby improving the power density of the membrane electrode.
[0039] The mass ratio of the amphiphilic supramolecular host compound to the carbon support is 0.05:1 to 0.2:1. Controlling the added mass ratio of the amphiphilic supramolecular host compound to the carbon support to be greater than or equal to 0.05:1 aims to ensure sufficient hydrogen-bonding active sites to effectively inhibit sulfonate poisoning. However, when the mass ratio of the added amphiphilic supramolecular host compound to the carbon support is greater than 0.2:1, the amphiphilic supramolecular host compound may self-aggregate, blocking mass transfer channels. Further, the preferred mass ratio of the amphiphilic supramolecular host compound to the carbon support is 0.075:1.
[0040] In some embodiments, the mass ratio (i.e., I / C ratio) of the perfluorosulfonic acid ionomer to the carbon support is 0.6:1 to 1.2:1, in order to maintain the integrity of the proton conduction network while avoiding excessive coating of Pt active sites by the perfluorosulfonic acid ionomer. Further, the mass ratio of the perfluorosulfonic acid ionomer to the carbon support is preferably 0.8:1.
[0041] In some embodiments, in step 102, the alcohol-water mixed solvent is a mixture of anhydrous ethanol and ultrapure water at a volume ratio of 5:1 to 15:1. The amphiphilic supramolecular host compound, perfluorosulfonic acid ionomer, and platinum-based catalyst are mixed by ultrasonic treatment for 60 to 120 minutes. The solid concentration of the cathode slurry is 2 mg / mL to 5 mg / mL. Within the above solvent ratio, ultrasonic treatment time, and cathode slurry solid concentration range, the platinum-based catalyst, amphiphilic supramolecular host compound, and perfluorosulfonic acid ionomer can be sufficiently and uniformly dispersed, avoiding agglomeration.
[0042] In some embodiments, in step 102, the perfluorosulfonic acid ionomer is added in the form of a perfluorosulfonic acid ionomer solution, wherein the perfluorosulfonic acid ionomer solution is at least one of DuPont Nafion solutions D520, D521, D1020, D1021, or D2020.
[0043] In some embodiments, the platinum-based catalyst is platinum nanoparticles supported on carbon black, or platinum-based alloy nanoparticles supported on carbon black; the platinum-based alloy is a PtCo alloy, a PtNi alloy, or a PtCoCe alloy; and the platinum loading of the cathode catalyst layer is 0.05 mg / cm³. 2 ~0.4mg / cm 2 .
[0044] Step 103: The cathode slurry is coated onto one side surface of the gas diffusion layer and dried to obtain the cathode catalyst layer.
[0045] In some embodiments, in step 103, the coating method is ultrasonic spraying, resulting in a uniform and controllable thickness of the cathode catalyst layer; the drying process is natural air drying or drying at 80℃~100℃. Mild drying conditions can avoid disrupting the hydrogen bond between the amphiphilic supramolecular host compound and the sulfonate group.
[0046] This invention also provides a method for preparing a membrane electrode for a proton exchange membrane fuel cell, comprising: Step S201 provides a cathode catalyst layer prepared by the above-described method for preparing a proton exchange membrane fuel cell membrane electrode cathode catalyst layer, and another gas diffusion layer.
[0047] In step S202, a platinum-based catalyst is coated onto one side surface of the other gas diffusion layer and dried to obtain an anode catalyst layer.
[0048] In some embodiments, a platinum-based catalyst is dispersed in an alcohol-water mixed solvent, a perfluorosulfonic acid ionomer is added, and the mixture is stirred evenly to obtain an anode slurry. The anode slurry is then coated onto one side of the surface of the other gas diffusion layer and dried to obtain an anode catalyst layer. The mass ratio of the perfluorosulfonic acid ionomer to the carbon support in the platinum-based catalyst can be 0.5:1, and the total solid concentration of the anode slurry can be 2 mg / mL to 5 mg / mL.
[0049] Furthermore, the platinum loading of the anode catalyst layer is 0.1 mg / cm³. 2 ~0.4mg / cm 2 .
[0050] Step S203: The gas diffusion layer with the cathode catalyst layer, the proton exchange membrane, and the gas diffusion layer with the anode catalyst layer are stacked sequentially and assembled by applying contact pressure to obtain the proton exchange membrane fuel cell membrane electrode.
[0051] It should be noted that the entire assembly process does not involve hot pressing, thus avoiding damage to the hydrogen bond network and oxygen transport channel structure caused by the high temperature and pressure of hot pressing. In step S203, the contact pressure is 0.5 MPa to 2 MPa; the assembly ambient temperature is room temperature to 80°C.
[0052] In some embodiments, the proton exchange membrane may be a Gore PRIMEA® series proton exchange membrane.
[0053] The technical solution of the present invention will be further described below with reference to specific embodiments. The raw materials, reagents, and equipment used in the following embodiments and comparative examples are all commercially available products. The Pt / C catalyst is a 40wt% product from Johnson Matthey, the Nafion solution is a 5wt% product from DuPont D520, the gas diffusion layer is Toray TGP-H-055 carbon paper, and the proton exchange membrane is a Gore PRIMEA® series proton exchange membrane. The following embodiments and comparative examples all used a Scribner 850e fuel cell test platform to test the single-cell performance of the obtained membrane electrode assembly. The test conditions were: cell temperature 70℃, relative humidity 100%, H2 / O2 inlet (H2 and O2 flow rates were both 150 mL / min), and back pressure 100 kPa. Oxygen transport characteristics were tested using a MOCON OX-TRAN2 / 12R oxygen permeability tester.
[0054] Example 1: Cathode catalytic layer containing calixarene (calixarene to carbon support mass ratio 0.1:1) (1) Preparation of cathode slurry: 40wt% Pt / C catalyst was weighed and dispersed in anhydrous ethanol / ultrapure water mixed solvent (volume ratio of anhydrous ethanol to ultrapure water 10:1), and calixarene (CAS No.: 74568-07-3, purity 98%, Aladdin Reagent (Shanghai) Co., Ltd.) and 5wt% Nafion D520 solution were added in sequence and ultrasonically dispersed to obtain cathode slurry; wherein the I / C ratio was 0.8:1, the mass ratio of calixarene to carbon support was 0.1:1, and the total solid concentration of cathode slurry was 3mg / mL.
[0055] (2) Preparation of anode slurry: Except for the absence of amphiphilic supramolecular host compounds, the other components are the same as those of cathode slurry, the I / C ratio is controlled at 0.5:1, and the total solid concentration of anode slurry is 3 mg / mL.
[0056] (3) Coating and Drying: The cathode slurry is ultrasonically sprayed onto one side of the gas diffusion layer, and the anode slurry is ultrasonically sprayed onto one side of the other gas diffusion layer. After drying at 80°C until the solvent is completely removed, a gas diffusion layer with a cathode catalytic layer and a gas diffusion layer with an anode catalytic layer are obtained. The platinum loading of both the cathode catalytic layer and the anode catalytic layer is 0.1 mg / cm³. 2 The active area is 4cm² 2 (2cm×2cm).
[0057] (4) Membrane electrode assembly: The gas diffusion layer with cathode catalyst layer, Gore 80μm proton exchange membrane (thickness of 80μm) and gas diffusion layer with anode catalyst layer are stacked in sequence, and a contact pressure of 1MPa is applied to assemble the membrane electrode at room temperature. The whole process does not involve hot pressing.
[0058] Example 2: Cathode catalyst layer containing cucurbitacin (cucurbitacin to carbon support mass ratio 0.1:1) The difference between this embodiment and Example 1 is that, in the cathode slurry preparation step, the added amphiphilic supramolecular host compound is cucurbituril (CAS No.: 80262-44-8, purity 98%, Aladdin Reagent (Shanghai) Co., Ltd.).
[0059] Example 3: Cathode catalyst layer containing crown ether (crown ether to carbon support mass ratio 0.1:1) The difference between this embodiment and Example 1 is that, in the cathode slurry preparation step, the added amphiphilic supramolecular host compound is a crown ether (CAS No.: 17455-13-9, purity 98%, Aladdin Reagent (Shanghai) Co., Ltd.).
[0060] Comparative Example 1: Unmodified cathode catalyst layer (without added amphiphilic supramolecular compounds) The difference between this embodiment and Example 1 is that no amphiphilic supramolecular compound was added in the cathode slurry preparation steps, but the rest are the same.
[0061] Comparison of test results for Examples 1-3 and Comparative Example 1: Table 1: Performance comparison of membrane electrodes with different amphiphilic supramolecular host compounds The results are as follows Figure 2As shown in Table 1, the maximum power density of Examples 1 to 3 is greater than that of Comparative Example 1, indicating that the three macrocyclic compounds, namely calixarene, cucurbituril, and crown ether, can induce the orderly arrangement of perfluorosulfonic acid ionomers in the cathode catalyst layer through non-covalent interactions with the side chain groups of perfluorosulfonic acid ionomers, forming interconnected proton conduction channels and constructing rapid oxygen transport channels, reducing proton transport resistance and oxygen mass transfer resistance, improving the utilization rate of the three-phase reaction interface, and thus increasing the power density of the membrane electrode.
[0062] Example 4: Cathode catalyst layer containing crown ether (crown ether to carbon support mass ratio 0.05:1) The difference between this embodiment and Embodiment 3 is that, in the cathode slurry preparation step, the mass ratio of crown ether to carbon support is 0.05:1.
[0063] Example 5: Cathode catalyst layer containing crown ether (crown ether to carbon support mass ratio 0.075:1) The difference between this embodiment and Embodiment 3 is that, in the cathode slurry preparation step, the mass ratio of crown ether to carbon support is 0.075:1.
[0064] Example 6: Cathode catalyst layer containing crown ether (crown ether to carbon support mass ratio 0.15:1) The difference between this embodiment and Embodiment 3 is that, in the cathode slurry preparation step, the mass ratio of crown ether to carbon support is 0.15:1.
[0065] Example 7: Cathode catalyst layer containing crown ether (crown ether to carbon support mass ratio 0.2:1) The difference between this embodiment and Embodiment 3 is that, in the cathode slurry preparation step, the mass ratio of crown ether to carbon support is 0.2:1.
[0066] Comparison of test results for Examples 3-7 and Comparative Example 1: Table 2: Performance comparison of membrane electrodes with different crown ether addition amounts The results are as follows Figure 3 , Figure 4 As shown in Table 2, Example 5 has the highest maximum power density (949.2 mW / cm²). 2 The results show that a crown ether to carbon support mass ratio of 0.075:1 is the optimal ratio, and the maximum power density at this mass ratio is 27.77% higher than that of Example 1. The maximum power density of Example 4 is lower than that of Example 5, indicating that when the amount of crown ether added is small, its ability to suppress the poisoning effect of sulfonate groups is limited. The maximum power density of Examples 3, 6, and 7 gradually decreases, indicating that when the amount of crown ether added is high, self-aggregation may occur, blocking the mass transfer channels and resulting in performance lower than that of Example 5.
[0067] Example 8: Proton exchange membrane with a thickness of 8 μm (crown ether to carbon support mass ratio 0.1:1) The difference between this embodiment and Embodiment 3 is that the thickness of the proton exchange membrane used in the membrane electrode assembly step is different. The proton exchange membrane used in this embodiment is a Gore 8μm proton exchange membrane.
[0068] The single-cell performance test results of Examples 8 and 3 are compared for example. Figure 5 As shown, the maximum power density of Example 8 is much greater than that of Example 3. The output capability of Example 8 is improved because the thin proton exchange membrane shortens the proton conduction distance and reduces membrane resistance (ohmic loss).
[0069] Example 9: Proton exchange membrane with a thickness of 8 μm (crown ether to carbon support mass ratio 0.075:1) The difference between this embodiment and Embodiment 8 is that, in the cathode slurry preparation step, the mass ratio of crown ether to carbon support is 0.075:1.
[0070] Comparative Example 2: A proton exchange membrane with a thickness of 8 μm (without crown ether). The difference between this comparative example and Example 8 is that no amphiphilic supramolecular host compound was added in the cathode slurry preparation steps, while the other preparation steps are the same.
[0071] Example 9, Comparison of test results with Comparative Example 2: Table 3: Performance comparison of membrane electrodes under optimal modification conditions and without modification The results are as follows Figures 6-8 As shown in Table 3, the maximum power density of Example 9 is greater than that of Comparative Example 2; the electrochemical active area (ECSA) of Example 9, as measured by cyclic voltammetry, is 45.62 m². 2 / g pt Comparative Example 2 is only 35.31m 2 / g pt This demonstrates that the membrane electrode prepared under the optimal modification conditions of this invention can reduce the sulfonate coverage on the Pt surface, releasing more Pt active sites that can be used for electrochemical reactions, thereby significantly improving ECSA. At the same time, under the optimal modification conditions, the amphiphilic supramolecular host compound can overcome the bottleneck of mutual constraint between proton conduction and oxygen transport, ultimately resulting in an increase in maximum power density.
[0072] In summary, this invention solves the problems of low Pt utilization and mutual constraints between proton conduction and oxygen transport by introducing an amphiphilic supramolecular host compound into the cathode slurry. Moreover, the amphiphilic supramolecular host compound only needs to be introduced in the slurry preparation step, without the need for additional processes and complex nanofabrication equipment. The preparation method is simple and suitable for large-scale production.
[0073] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.
[0074] In the description of this invention, it should be understood that the terms "center," "height," "thickness," "upper," "lower," "vertical," "horizontal," "top," "bottom," "inner," "outer," "axial," "radial," and "circumferential," etc., indicating orientation or positional relationships, are based on the orientation or positional relationships shown in the accompanying drawings and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. In the description of this invention, unless otherwise stated, "a plurality of" means two or more.
[0075] In the description of this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0076] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0077] Although the present invention has been described in detail through the preferred embodiments above, it should be understood that the above description should not be considered as a limitation of the present invention. Various modifications and substitutions to the present invention will be apparent to those skilled in the art after reading the above description. Therefore, the scope of protection of the present invention should be defined by the appended claims.
Claims
1. A method for preparing the catalyst layer of the cathode of a proton exchange membrane fuel cell, characterized in that, include: Step 1: Provide a gas diffusion layer; Step 2: Disperse the platinum-based catalyst in an alcohol-water mixed solvent, then add the amphiphilic supramolecular host compound and perfluorosulfonic acid ionomer in sequence, mix thoroughly, and obtain the cathode slurry; The amphiphilic supramolecular host compound has a macrocyclic host skeleton that forms a hydrophobic cavity; the outer edge of the macrocyclic host skeleton has hydrogen-bonding active sites that can form hydrogen bonds with the sulfonate groups of the perfluorosulfonic acid ionomer; the platinum-based catalyst contains a carbon support, and the mass ratio of the amphiphilic supramolecular host compound to the carbon support is 0.05:1 to 0.2:
1. Step 3: The cathode slurry is coated onto one side surface of the gas diffusion layer and dried to obtain the cathode catalyst layer.
2. The preparation method according to claim 1, characterized in that, The amphiphilic supramolecular host compound comprises at least one of calixarenes, cucurbiturates, and crown ether macrocyclic compounds; the hydrogen bond active site is at least one hydrogen bond donor or acceptor group selected from hydroxyl, carbonyl, or heteroatom.
3. The preparation method according to claim 1, characterized in that, The mass ratio of the perfluorosulfonic acid ionomer to the carbon support is 0.6:1 to 1.2:
1.
4. The preparation method according to claim 1, characterized in that, In step 2, the alcohol-water mixed solvent is a mixture of anhydrous ethanol and ultrapure water in a volume ratio of 5:1 to 15:1; the mixing is performed by ultrasonic treatment for 60 min to 120 min; the solid concentration of the cathode slurry is 2 mg / mL to 5 mg / mL.
5. The preparation method according to claim 1, characterized in that, In step 2, the perfluorosulfonic acid ionomer is added in the form of a perfluorosulfonic acid ionomer solution, which is at least one of DuPont Nafion solutions D520, D521, D1020, D1021, or D2020.
6. The preparation method according to claim 1, characterized in that, In step 3, the coating method is ultrasonic spraying; the drying process is natural air drying or drying at 80℃~100℃.
7. The preparation method according to claim 1, characterized in that, The platinum-based catalyst is platinum nanoparticles supported on carbon black, or platinum-based alloy nanoparticles supported on carbon black; the platinum-based alloy is a PtCo alloy, a PtNi alloy, or a PtCoCe alloy; the platinum loading of the cathode catalyst layer is 0.05 mg / cm³. 2 ~0.4mg / cm 2 .
8. A method for preparing a membrane electrode assembly (MEA) for a proton exchange membrane fuel cell, characterized in that, include: Provides a cathode catalyst layer prepared by the method for preparing a proton exchange membrane fuel cell membrane electrode cathode catalyst layer as described in any one of claims 1 to 7, and another gas diffusion layer; A platinum-based catalyst is coated onto one side surface of the other gas diffusion layer and then dried to obtain an anode catalyst layer. The gas diffusion layer with the cathode catalyst layer, the proton exchange membrane, and the gas diffusion layer with the anode catalyst layer are stacked sequentially and assembled by applying contact pressure to obtain the membrane electrode assembly of the proton exchange membrane fuel cell.
9. The preparation method according to claim 8, characterized in that, The platinum loading of the anode catalyst layer is 0.1 mg / cm³. 2 ~0.4mg / cm 2 The contact pressure is 0.5MPa to 2MPa; the assembly ambient temperature is room temperature to 80℃.
10. A membrane electrode assembly for a proton exchange membrane fuel cell, characterized in that, It is prepared using the preparation method described in claim 8 or 9.
Citation Information
Patent Citations
Silanol-improved cathode catalyst layer of proton exchange membrane fuel cell as well as preparation method and application of silanol-improved cathode catalyst layer
CN121885654A