A Mechanism-Constrained Multi-Cell Modeling and Simulation Method for Zinc-Bromine Flow Batteries
The mechanism-constrained multi-cell modeling method for zinc-bromine flow batteries solves the problems of existing models in describing the concentration difference between the electrolyte phase and the electrode surface and the inconsistency of multi-cell parameters. It realizes dynamic simulation of stack performance and weak cell identification, and improves the accuracy and reliability of simulation.
Patent Information
- Application Number
- CN202611387236.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-08
- Publication Date
- 2026-11-17
AI Technical Summary
Existing zinc-bromine flow battery models are unable to describe the concentration differences between the electrolyte bulk phase and the electrode surface, the mass transfer limit, the inconsistency of multiple individual parameters, and the cycle degradation process within a unified framework, leading to individual cell voltage differentiation and a decrease in stack performance.
A mechanism-constrained multi-cell modeling method for zinc-bromine flow batteries is adopted. By calculating the electrochemical health baseline voltage, updating the multi-cell state and assembly terminal voltage, and combining mass transfer risk, concentration risk, etc., dynamic simulation of the stack is achieved.
It can adapt to different numbers of cells and operating conditions, dynamically describe the battery degradation process, identify weak cells and output stack statistics, thereby improving the accuracy and reliability of simulation.
Smart Images

Figure CN123120782A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of flow battery technology, and in particular to a mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries. Background Technology
[0002] During charging, zinc ions are reduced and deposited as metallic zinc on the negative electrode surface in a zinc-bromine flow battery; during discharging, the deposited zinc redissolves. Influenced by differences in electrode surface current density distribution, liquid flow rate, reactant concentration, mass transfer boundary layer, and electrode structure, zinc deposition is prone to uneven thickness, residual zinc accumulation, and localized dendrites. With increasing cycle count, residual zinc, film resistance, decrease in effective reaction area, reduced mass transfer capacity, and liquid flow blockage interact, potentially leading to individual cell voltage differentiation, discharge end-stage steps, and premature collapse, thereby affecting the stack's usable capacity and operating characteristics.
[0003] Existing equivalent circuit models for zinc-bromine flow batteries typically use fixed open-circuit voltage, fixed internal resistance, and a small number of RC branches to fit voltage curves. This makes it difficult to simultaneously characterize the concentration difference between the electrolyte bulk phase and the electrode surface, flow-related mass transfer processes, limiting current, zinc deposition accumulation, and various degradation factors. For a stack composed of multiple cells connected in series, different cells exhibit initial differences in capacity, internal resistance, mass transfer capability, and equilibrium potential, and will develop different degradation rates during cycling. Using only a single average cell model or linearly amplifying the cell voltage by quantity is insufficient to describe weak cells, voltage dispersion within the stack, and the dynamic characteristics under different numbers of cells connected in series. It also hinders simulation comparisons at different scales.
[0004] Therefore, there is a need for a zinc-bromine flow battery modeling and simulation method that can calculate the electrochemical health baseline voltage, update the state of multiple cells, assemble the terminal voltages of each cell, and output the stack statistics within a unified framework, so that the model can support different numbers of cells, different operating conditions, and multiple cycles of degradation. Summary of the Invention
[0005] To address the limitations of existing zinc-bromine flow battery models in simultaneously describing the concentration differences between the electrolyte phase and electrode surface, mass transfer limits, inconsistencies in multi-cell parameters, and cyclic degradation processes within a unified framework, and the difficulty in simulating weak-cell differentiation, residual zinc accumulation, and voltage steps at the discharge end using models based on average cells or fixed parameters, this invention provides a mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries to achieve electrochemical state calculation, multi-cell degradation evolution, voltage assembly, and multi-cycle dynamic simulation.
[0006] To solve the above-mentioned technical problems, the present invention adopts the following technical solution: A mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries includes the following steps: Step S1: Collect or set the operating condition data of the zinc-bromine redox flow battery stack, and set the model initialization parameters; The operating condition data includes stack current, liquid flow rate, temperature, operating mode, and time information, wherein the operating mode includes charging, discharging, and resting; the model initialization parameters include the number of battery cells, rated capacity, and initial difference parameters of each battery cell, wherein the initial difference parameters include capacity factor, internal resistance factor, mass transfer factor, and open circuit voltage bias. The zinc-bromine flow battery stack comprises N battery cells connected in series, where N is a positive integer; the length is N, which is the maximum number of cells. max A fixed-dimensional state vector is used to store the operating state of each battery cell, and the state is updated only for the first N valid cells in the fixed-dimensional state vector. If the charging current of a single battery cell is defined as positive and the discharging current as negative, then the state of charge is updated discretely according to the following formula: ; Among them, SOC k Let I be the state of charge at time k. k Let be the stack current at time k. To account for dynamic available capacity after capacity degradation, and These are the charging coulombic efficiency and the discharging coulombic efficiency, respectively. To calculate the step size for discrete calculations, (.) indicates a limit operation, which means that when the input value is less than 0, it takes 0; when it is greater than 1, it takes 1; and when it is between 0 and 1, it retains the original value. Step S2: Update the state of charge, the bulk concentration of zinc ion species and bromine active species and the electrode surface concentration based on the operating condition data, determine the flow-related mass transfer coefficient based on the liquid flow rate, and calculate the mass transfer ratio, mass transfer risk and limiting current.
[0007] The update specifically involves updating the electrode surface concentration of electrolyte species j based on the difference between the mass transfer from the bulk electrolyte to the electrode surface and the species consumption or generation caused by the electrochemical reaction. ; Where j represents a zinc ion species or a bromine-active species; and These are the bulk concentration and electrode surface concentration of species j at time k, respectively; For traffic The mass transfer coefficient of species j under the given conditions; For the operating mode The reaction direction coefficient is determined, taking the value 1 when species j is consumed and 1 when species j is generated. 1; These are stoichiometric coefficients; Where is the electron transfer number; F is the Faraday constant; This represents the effective electrolyte volume of the corresponding reaction region.
[0008] Furthermore, the ratio of the electrode surface concentration of electrolyte species j to its corresponding bulk concentration is determined as the mass transfer ratio. : ; The smaller of the mass transfer ratios of zinc ion species and bromine active species was determined as the overall mass transfer ratio. : ; in, and These represent the mass transfer ratios of zinc ion species and bromine active species, respectively. A very small positive number set to prevent the denominator from being zero.
[0009] Any species participating in the electrode reaction The corresponding limiting current is calculated according to the following formula. : ; in, For the first The effective reaction area at any given time; the smaller of the limiting currents corresponding to each reactant species is determined as the battery limiting current. : ; The mass transfer load ratio is determined based on the ratio of the actual current to the battery's limiting current. ; in Let be the mass transfer load ratio at time k. The current at time k is the stack operating current. The limiting current is calculated based on the electrode mass transfer state; sat [0,1] ( ) indicates a limit operation that restricts the calculation result to the range of 0 to 1.
[0010] And determine the mass transfer margin based on the mass transfer loading ratio: ; in Let be the mass transfer margin at time k, representing the margin remaining between the current operating current and the ultimate mass transfer capability.
[0011] Further determine the mass transfer risk based on the mass transfer loading ratio and electrolyte mass transfer state: ; in, To normalize mass transfer risk, The risk component is determined based on the mass transfer load ratio. The risk component is determined based on the species concentration deficit on the electrode surface and the flow rate in the liquid path. and The weights are non-negative. The mass transfer risk is limited to the range of 0 to 1. The closer the actual current is to the limiting current, or the more significantly the species concentration on the electrode surface deviates from the bulk concentration, the higher the mass transfer risk. Step S3: Calculate the concentration-related open-circuit voltage based on the electrode surface concentration and temperature, calculate the activation polarization, ohmic polarization, concentration polarization and dynamic RC polarization respectively, and combine them according to the charging, discharging or static operation mode. After continuous smoothing and finite gain processing, the electrochemical health baseline voltage is obtained.
[0012] The concentration-related open-circuit voltage Calculated based on the reaction quotient formed by the activities of zinc ion species and bromine active species: ; Among them, E 0 Where R is the standard electrode potential, and T is the gas constant. k Let be the temperature at time k, and F be the Faraday constant. The reaction quotient is composed of the electrode surface activities of zinc ion species and bromine active species at time k, where n is the number of electrons transferred in the corresponding electrode reaction. The activation polarization Ohmic polarization and concentration polarization Calculate according to the following formulas respectively: ; ; ; Where α is the charge transfer coefficient and i0 is the exchange current density. Basic ohmic resistor, For membrane resistance, Let A be the limiting current, T be the absolute temperature of the battery at the current moment, and A be the limiting current. eff The effective reaction area of the electrode is asinh( ) is an inverse hyperbolic sine function; I is the actual current flowing through the fuel cell stack; The dynamic RC polarization Update according to the following formula: ; in, For the first Dynamic polarization resistance at any given time. For the first The time constant at any given moment; The concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization are combined according to the current operating mode to obtain the electrochemically calculated voltage. Limiting and finite gain corrections are applied to the deviation between the electrochemically calculated voltage and the continuous reference voltage. ; in, The electrochemical voltage at time k is obtained by combining the concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization according to the current operating mode. The target healthy baseline voltage after finite gain correction. This is a continuous reference voltage determined based on the current operating mode and state of charge, where m represents the current operating mode, including charging mode, discharging mode, and idle mode. For the finite gain coefficient corresponding to the operating mode, sat( ) is the amplitude limiting function; Further, first-order dynamic smoothing was employed to obtain the electrochemical healthy baseline voltage: ; in, The electrochemical health baseline voltage output at time k; The first-order dynamic smoothing coefficient at time k is determined according to the following formula: ; in, To simulate the discrete calculation step size, The smoothing time constant is determined based on the charging mode, discharging mode, and resting mode; Step S4: Update the degradation state of each cell based on at least one of residual zinc content, membrane resistance state, effective reaction area state, mass transfer capacity, liquid path blockage state, capacity state, and cyclic stress, and obtain the terminal voltage of each cell based on the electrochemical health baseline voltage. The specific steps for updating the degradation state of each battery cell are as follows: The first... The degradation state of each battery cell includes at least the residual zinc state. Membrane resistance state Effective reaction area status Liquid circuit blockage Mass transfer capability status and capacity status Any degenerate state Discrete updates are performed according to the following formula: ; in, This represents the degenerate state at time k+1. This is the accumulation or recovery function corresponding to the degradation state in charging, discharging, or idle operation modes. This represents the upper and lower bound constraints corresponding to the degradation state.
[0013] No. The combined degradation driving force D of each battery cell i Determined according to the following formula: ; in, For low flow stress, to Non-negative weights; The comprehensive aging-related polarization voltage drop of the i-th cell is obtained based on the comprehensive degradation driving force. The degradation correction voltage drop was determined based on the residual zinc state and the local mass transfer state. ; The terminal voltage of the i-th battery cell at time k. Calculate according to the following formula: ; in, For the first Open-circuit voltage bias of each battery cell; Step S5: Calculate the total stack voltage, lowest single-cell voltage, average single-cell voltage, and highest single-cell voltage based on the terminal voltage of each battery cell, and use at least one of the following as the simulation termination judgment parameter for the current charging and discharging stage: lowest single-cell voltage, total stack voltage, state of charge, or preset simulation time.
[0014] The total voltage of the fuel cell stack Minimum unit voltage Average cell voltage and highest single-cell voltage Calculate according to the following formulas respectively: ; ; ; ; During the discharge process, when the lowest single-cell voltage satisfies the following formula, the simulation of the current discharge stage ends or an over-discharge risk flag is output: ; in, This is the preset discharge cutoff voltage for a single cell; Step S6: Calculate the comprehensive state characterization quantity based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk, and perform gain correction on the comprehensive state characterization quantity based on at least one of low flow rate state, minimum monomer voltage, or number of cycles.
[0015] The comprehensive state characterization quantity H is calculated according to the following formula: ; in, , , , , and These are the normalized mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk; to The weights are non-negative and satisfy: ; Step S7: According to the preset simulation step size and cycle conditions, iteratively update the state of charge, electrolyte species concentration, dynamic RC polarization and degradation state of each cell, and output the simulation results of each cell terminal voltage, stack statistics, comprehensive state characterization, and the changes of each state quantity with time and cycle number.
[0016] On the other hand, a mechanism-constrained multi-cell modeling and simulation system for zinc-bromine flow batteries is provided to implement the aforementioned mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries. The system includes: a simulation condition and parameter initialization module, a state of charge and electrolyte species balance module, an electrochemical health baseline voltage calculation module, a multi-cell initial difference configuration module, a multi-cell state update module, a cell terminal voltage assembly and stack statistics module, a comprehensive state characterization module, and a simulation iteration and data recording module. The simulation operating condition and parameter initialization module is used to acquire operating condition data and set the number of battery cells, rated capacity and initial difference parameters. The state of charge and electrolyte species balance module is used to update the bulk concentration and electrode surface concentration of the state of charge, zinc ion species, and bromine active species. The electrochemical health baseline voltage calculation module is used to calculate concentration-related open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, dynamic RC polarization, mass transfer ratio, mass transfer risk, and limiting current, and to obtain the electrochemical health baseline voltage. The multi-cell initial differential configuration module is used to configure the capacity factor, internal resistance factor, mass transfer factor and open-circuit voltage bias for each cell. The multi-cell state update module is used to update the residual zinc state, membrane resistance state, effective reaction area state, mass transfer capacity state, liquid path blockage state, and capacity state of each battery cell. The single-cell terminal voltage assembly and stack statistics module is used to obtain the terminal voltage of each battery cell and calculate the total stack voltage, the lowest single-cell voltage, the average single-cell voltage, and the highest single-cell voltage. The comprehensive state characterization module is used to calculate the comprehensive state characterization quantity based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk. The simulation iteration and data recording module is used to iteratively update the model state according to the preset simulation step size and cyclic working conditions, and output and save the multi-cycle dynamic simulation results. The beneficial effects of adopting the above technical solution are as follows: This invention provides a mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries, which has the following beneficial effects: 1. This invention constrains the voltage calculation process by using bulk concentration, electrode surface concentration, flow-related mass transfer coefficient and limiting current, so that the open-circuit voltage, concentration polarization and mass transfer state can change dynamically with the operating conditions, reducing parameter distortion caused by relying solely on data voltage curve fitting.
[0017] 2. This invention uses a configurable number of cells and a fixed-dimensional state vector, which is applicable to different numbers of series-connected battery cells without changing the model input and output interface. The initial differences between cells are characterized by capacity factor, internal resistance factor, mass transfer factor and open-circuit voltage bias.
[0018] 3. This invention combines updates to degradation states such as residual zinc, membrane resistance, effective reaction area, mass transfer capacity, liquid path blockage, and capacity, which can describe the evolution of monomer differences during cycling and identify weak monomers through the lowest monomer voltage and stack statistics.
[0019] 4. This invention performs layered calculations of electrochemical health baseline voltage, combined aging-related additional polarization, and residual zinc degradation correction, and avoids non-physical jumps through continuous functions and dynamic links.
[0020] 5. This invention integrates mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk into a comprehensive state characterization quantity, which can simultaneously output simulation results at the monomer level, stack level, and cycle level for degradation mechanism analysis, parameter calibration, and model comparison.
[0021] 6. This invention can be deployed on MATLAB / Simulink, real-time simulators or industrial computers through computer programs, function blocks, state machines or lookup tables, and is suitable for multi-cycle degradation simulation, hardware-in-the-loop simulation and offline verification of control strategies. Attached Figure Description
[0022] Figure 1 The flowchart shows the overall process of multi-cell modeling and simulation of zinc-bromine redox flow battery under mechanistic constraints in this embodiment of the invention.
[0023] Figure 2 This is a block diagram of the electrochemical health baseline, multi-monomer state correction, and voltage assembly model in an embodiment of the present invention.
[0024] Figure 3 This is a diagram showing the recursive relationship between multiple cycle operating conditions and states in an embodiment of the present invention.
[0025] Figure 4 This is a diagram showing the relationship between the model input, output, and data records in an embodiment of the present invention. Detailed Implementation
[0026] The specific implementation methods of this application will be further described in detail below with reference to the accompanying drawings and embodiments.
[0027] Example 1: like Figure 1 As shown, this invention executes the following steps in sequence: simulation conditions and parameter input, calculation of state of charge and electrolyte species balance, calculation of electrochemical health baseline voltage, initial differential configuration of multiple monomers, state update of multiple monomers, assembly of monomer terminal voltages, calculation of stack statistics, and output and recording of simulation results. Each calculation step is executed sequentially with a uniform simulation step size, and continuous dynamic updates are completed using the state variables obtained from the previous simulation step.
[0028] According to the preset charging, discharging and resting conditions, the state of charge, electrolyte species concentration, dynamic RC polarization and degradation state of each battery cell are recursively calculated with a fixed simulation step size, and the corresponding state is maintained, restored or reset when the operating mode is switched or time is rolled back. At least one of the following states—residual zinc state, membrane resistance state, effective reaction area state, mass transfer capacity state, liquid path blockage state, and capacity state—is retained between multiple cycles, so that the degraded state accumulates or recovers with the number of cycles. At the end of the discharge, a degradation correction voltage drop is continuously generated based on the residual zinc state, low charge state, low single-cell voltage, and local mass transfer state. The output should include at least the state of charge, dynamic available capacity, electrolyte species concentration, open-circuit voltage, polarization, mass transfer ratio, limiting current, degradation state of each cell, terminal voltage of each cell, and stack statistics, and record the simulation results of the first cycle, the last cycle, or a specified cycle.
[0029] A mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries includes the following steps: Step S1: Collect or set the operating condition data of the zinc-bromine redox flow battery stack, and set the model initialization parameters; The operating condition data includes stack current, liquid flow rate, temperature, operating mode, and time information, wherein the operating mode includes charging, discharging, and resting; the model initialization parameters include the number of battery cells, rated capacity, and initial difference parameters of each battery cell, wherein the initial difference parameters include capacity factor, internal resistance factor, mass transfer factor, and open circuit voltage bias. The zinc-bromine flow battery stack comprises N battery cells connected in series, where N is a configurable positive integer; the length is N, which is the maximum number of cells. max A fixed-dimensional state vector is used to store the operating state of each battery cell. The state is updated only for the first N valid cells in the fixed-dimensional state vector, so that the same model can be applied to different numbers of series-connected battery cells without changing the input and output interface dimensions.
[0030] If the charging current of a single battery cell is defined as positive and the discharging current as negative, then the state of charge is updated discretely according to the following formula: ; Among them, SOC k Let I be the state of charge at time k. k Let be the stack current at time k. To account for dynamic available capacity after capacity degradation, and These are the charging coulombic efficiency and the discharging coulombic efficiency, respectively. To calculate the step size for discrete calculations, (.) indicates a limiting operation, which means that when the input value is less than 0, it takes 0, when it is greater than 1, it takes 1, and when it is between 0 and 1, it retains the original value, which is used to ensure that the state of charge always satisfies 0≤SOC≤1.
[0031] Step S2: Update the state of charge, the bulk concentration of zinc ion species and bromine active species and the electrode surface concentration based on the operating condition data, determine the flow-related mass transfer coefficient based on the liquid flow rate, and calculate the mass transfer ratio, mass transfer risk and limiting current.
[0032] The update specifically involves updating the electrode surface concentration of electrolyte species j based on the difference between the mass transfer from the bulk electrolyte to the electrode surface and the species consumption or generation caused by the electrochemical reaction. ; Where j represents a zinc ion species or a bromine-active species; and These are the bulk concentration and electrode surface concentration of species j at time k, respectively; For traffic The mass transfer coefficient of species j under the given conditions; For the operating mode The reaction direction coefficient is determined, taking the value 1 when species j is consumed and 1 when species j is generated. 1; These are stoichiometric coefficients; Where is the electron transfer number; F is the Faraday constant; This represents the effective electrolyte volume of the corresponding reaction region.
[0033] Furthermore, the ratio of the electrode surface concentration of electrolyte species j to its corresponding bulk concentration is determined as the mass transfer ratio. : ; The smaller of the mass transfer ratios of zinc ion species and bromine active species was determined as the overall mass transfer ratio. : ; in, and These represent the mass transfer ratios of zinc ion species and bromine active species, respectively. A very small positive number set to prevent the denominator from being zero.
[0034] Any species participating in the electrode reaction The corresponding limiting current is calculated according to the following formula. : ; in, For the first The effective reaction area at any given time; the smaller of the limiting currents corresponding to each reactant species is determined as the battery limiting current. : ; The mass transfer load ratio is determined based on the ratio of the actual current to the battery's limiting current. ; in Let be the mass transfer load ratio at time k. The current at time k is the stack operating current. The limiting current is calculated based on the electrode mass transfer state; sat [0,1] ( ) indicates a limit operation that restricts the calculation result to the range of 0 to 1.
[0035] And determine the mass transfer margin based on the mass transfer loading ratio: ; in Let be the mass transfer margin at time k, representing the margin remaining between the current operating current and the ultimate mass transfer capability.
[0036] Further determine the mass transfer risk based on the mass transfer loading ratio and electrolyte mass transfer state: ; in, To normalize mass transfer risk, The risk component is determined based on the mass transfer load ratio. The risk component is determined based on the species concentration deficit on the electrode surface and the flow rate in the liquid path. and The weights are non-negative. The mass transfer risk is limited to the range of 0 to 1. The closer the actual current is to the limiting current, or the more significantly the species concentration on the electrode surface deviates from the bulk concentration, the higher the mass transfer risk. In actual calculations, the ratio of current to limiting current is limited to avoid numerical oddities.
[0037] Step S3: Calculate the concentration-related open-circuit voltage based on the electrode surface concentration and temperature, calculate the activation polarization, ohmic polarization, concentration polarization and dynamic RC polarization respectively, and combine them according to the charging, discharging or static operation mode. After continuous smoothing and finite gain processing, the electrochemical health baseline voltage is obtained.
[0038] The concentration-related open-circuit voltage Calculated based on the reaction quotient formed by the activities of zinc ion species and bromine active species: ; Among them, E 0 Where R is the standard electrode potential, and T is the gas constant. k Let be the temperature at time k, and F be the Faraday constant. Let be the reaction quotient composed of the electrode surface activities of zinc ion species and bromine active species at time k, where n is the number of electrons transferred in the corresponding electrode reaction, and is a dimensionless parameter.
[0039] The activation polarization Ohmic polarization and concentration polarization Calculate according to the following formulas respectively: ; ; ; Where α is the charge transfer coefficient and i0 is the exchange current density. Basic ohmic resistor, For membrane resistance, Let A be the limiting current, T be the absolute temperature of the battery at the current moment, and A be the limiting current.eff The effective reaction area of the electrode is asinh( ) is an inverse hyperbolic sine function; I is the actual current through the stack, which is also the operating current of each connected cell in series; each polarization represents the amplitude of the polarization voltage drop, and its direction of action in charging, discharging and resting modes is determined by the operating mode and the current direction.
[0040] The dynamic RC polarization Update according to the following formula: ; in, For the first Dynamic polarization resistance at any given time. For the first The time constant at any given moment; and Adjustments are made based on at least one of the following: state of charge, fluid flow rate, temperature, and degradation state.
[0041] The concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization are combined according to the current operating mode to obtain the electrochemically calculated voltage. To suppress non-physical voltage jumps caused by instantaneous changes in physical calculation quantities, a limiting and finite gain correction is applied to the deviation between the electrochemically calculated voltage and the continuous reference voltage. ; in, The electrochemical voltage at time k is obtained by combining the concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization according to the current operating mode. The target healthy baseline voltage after finite gain correction. This is a continuous reference voltage determined based on the current operating mode and state of charge, where m represents the current operating mode, including charging mode, discharging mode, and idle mode. For the finite gain coefficient corresponding to the operating mode, sat( ) is a limiting function used to limit the voltage deviation amplitude.
[0042] Further, first-order dynamic smoothing was employed to obtain the electrochemical healthy baseline voltage: ; in, The electrochemical health baseline voltage output at time k; The first-order dynamic smoothing coefficient at time k is used to control the rate of change of the target voltage towards the healthy baseline voltage, and is determined according to the following formula: ; in, To simulate the discrete calculation step size, The smoothing time constant is determined based on the charging mode, discharging mode, and resting mode. Through finite gain correction and continuous dynamic smoothing, the electrochemical mechanism calculation results are applied to the healthy baseline voltage in a limited manner, while suppressing non-physical voltage jumps caused by operating mode switching, concentration changes, and instantaneous changes in polarization state.
[0043] Step S4: Update the degradation state of each cell based on at least one of residual zinc content, membrane resistance state, effective reaction area state, mass transfer capacity, liquid path blockage state, capacity state, and cyclic stress, and obtain the terminal voltage of each cell based on the electrochemical health baseline voltage. The specific steps for updating the degradation state of each battery cell are as follows: The first... The degradation state of each battery cell includes at least the residual zinc state. Membrane resistance state Effective reaction area status Liquid circuit blockage Mass transfer capability status and capacity status Any degenerate state Discrete updates are performed according to the following formula: ; in, This represents the degenerate state at time k+1. This is the accumulation or recovery function corresponding to the degradation state in charging, discharging, or idle operation modes. This represents the upper and lower bound constraints corresponding to the degradation state.
[0044] No. The combined degradation driving force D of each battery cell i Determined according to the following formula: ; in, For low flow stress, to Non-negative weights; The comprehensive aging-related polarization voltage drop of the i-th cell is obtained based on the comprehensive degradation driving force. The degradation correction voltage drop was determined based on the residual zinc state and the local mass transfer state. ; The terminal voltage of the i-th battery cell at time k. Calculate according to the following formula: ; in, For the first The open-circuit voltage bias of each battery cell. The manufacturing differences and cycle evolution differences between different battery cells are characterized by a combination of capacity factor, internal resistance factor, mass transfer factor, open-circuit voltage bias, and degradation state.
[0045] Step S5: Calculate the total stack voltage, lowest single-cell voltage, average single-cell voltage, and highest single-cell voltage based on the terminal voltage of each battery cell, and use at least one of the following as the simulation termination judgment parameter for the current charging and discharging stage: lowest single-cell voltage, total stack voltage, state of charge, or preset simulation time.
[0046] The total voltage of the fuel cell stack Minimum unit voltage Average cell voltage and highest single-cell voltage Calculate according to the following formulas respectively: ; ; ; ; During the discharge process, when the lowest single-cell voltage satisfies the following formula, the simulation of the current discharge stage ends or an over-discharge risk flag is output: ; in, This is the preset discharge cutoff voltage for a single cell. By prioritizing the lowest single cell voltage and combining it with the total stack voltage, state of charge, and longest discharge time, a joint judgment is made to avoid masking the low voltage state of weak cells in the simulation based solely on the total stack voltage.
[0047] Step S6: Calculate the comprehensive state characterization quantity based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk, and perform gain correction on the comprehensive state characterization quantity based on at least one of low flow rate state, minimum monomer voltage, or number of cycles.
[0048] The comprehensive state characterization quantity H is calculated according to the following formula: ; in, , , , , and These are the normalized mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk; to The weights are non-negative and satisfy: ; In this embodiment, to The values can be set sequentially to 0.24, 0.22, 0.20, 0.15, 0.11, and 0.08; these values are for illustrative purposes only and can be adjusted based on experimental calibration results, operational data, or optimization algorithms. The comprehensive state characterization quantity can also be adjusted for gain based on low flow conditions or the lowest unit voltage to improve the model's ability to characterize decreased mass transfer capacity and weak unit degradation.
[0049] Step S7: According to the preset simulation step size and cycle conditions, iteratively update the state of charge, electrolyte species concentration, dynamic RC polarization and degradation state of each cell, and output the simulation results of each cell terminal voltage, stack statistics, comprehensive state characterization, and the changes of each state quantity with time and cycle number.
[0050] On the other hand, a mechanism-constrained multi-cell modeling and simulation system for zinc-bromine flow batteries is provided to implement the aforementioned mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries. The system includes: a simulation condition and parameter initialization module, a state of charge and electrolyte species balance module, an electrochemical health baseline voltage calculation module, a multi-cell initial difference configuration module, a multi-cell state update module, a cell terminal voltage assembly and stack statistics module, a comprehensive state characterization module, and a simulation iteration and data recording module. The simulation operating condition and parameter initialization module is used to acquire operating condition data and set the number of battery cells, rated capacity and initial difference parameters. The state of charge and electrolyte species balance module is used to update the bulk concentration and electrode surface concentration of the state of charge, zinc ion species, and bromine active species. The electrochemical health baseline voltage calculation module is used to calculate concentration-related open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, dynamic RC polarization, mass transfer ratio, mass transfer risk, and limiting current, and to obtain the electrochemical health baseline voltage. The multi-cell initial differential configuration module is used to configure the capacity factor, internal resistance factor, mass transfer factor and open-circuit voltage bias for each cell. The multi-cell state update module is used to update the residual zinc state, membrane resistance state, effective reaction area state, mass transfer capacity state, liquid path blockage state, and capacity state of each battery cell. The single-cell terminal voltage assembly and stack statistics module is used to obtain the terminal voltage of each battery cell and calculate the total stack voltage, the lowest single-cell voltage, the average single-cell voltage, and the highest single-cell voltage. The comprehensive state characterization module is used to calculate the comprehensive state characterization quantity based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk. The simulation iteration and data recording module is used to iteratively update the model state according to the preset simulation step size and cyclic working conditions, and output and save the multi-cycle dynamic simulation results. Example 2: In this embodiment, as Figure 2 As shown, the state of charge (SOC) is first calculated based on the stack current and dynamic available capacity. The bulk concentrations of zinc ions and bromine active species, as well as the electrode surface concentrations, are then updated separately. The SOC is then calculated using the aforementioned SOC update formula. Simultaneously, the bulk concentrations of zinc ions and bromine active species, as well as the electrode surface concentrations, are updated separately. When the liquid flow rate increases, the flow-dependent mass transfer coefficient increases, and the rate at which the electrode surface concentration recovers to the bulk concentration increases. Conversely, when the liquid flow rate decreases, the mass transfer capacity declines, or the discharge reaches its end, the effective concentration at the electrode surface decreases, the mass transfer ratio decreases, and the mass transfer risk increases.
[0051] Concentration-dependent open-circuit voltages were calculated based on the electrode surface concentrations of zinc ion species and bromine active species. Activation polarization, ohmic polarization, and concentration polarization were calculated by combining the effective reaction area, exchange current density, fundamental ohmic resistance, film resistance, actual current, and limiting current. Dynamic RC polarization was used to describe the double-layer effect and voltage hysteresis. The above electrochemical quantities were combined according to charging, discharging, or resting modes, and after continuous smoothing and finite gain processing, the electrochemical health baseline voltage was obtained. This electrochemical health baseline voltage is used to describe normal electrochemical reactions and the tail end of conventional discharges.
[0052] Within each control cycle and each simulation step, the residual zinc state, membrane resistance state, effective reaction area state, mass transfer capacity state, fluid path blockage state, and capacity state of each monomer are updated. During charging, low flow rate, high mass transfer risk, and cyclic stress cause residual zinc and other degradation states to gradually accumulate; during discharging and resting, the relevant states are updated according to the corresponding dissolution or recovery relationships. Therefore, the degradation states of different monomers differ with the cycling process.
[0053] No. The terminal voltage of each cell is determined by the electrochemical health baseline voltage, the cell open-circuit voltage bias, the combined aging-related additional polarization, and the residual zinc degradation correction. ; In the formula, For the first The first control cycle The terminal voltage of each individual unit; The baseline voltage for electrochemical health; This is a single-cell open-circuit voltage bias; Additional polarization due to aging is caused by a combination of factors, including increased membrane resistance, decreased effective reaction area, decreased mass transfer capacity, and blockage of the liquid path. The degradation correction voltage drop is determined based on the residual zinc state and the local mass transfer state.
[0054] Among them, the residual zinc degradation correction gradually increases during the discharge stage based on the residual zinc amount, low state of charge, low individual voltage and local mass transfer risk, and is smoothed through continuous functions or dynamic links, so that the abnormal voltage pattern gradually forms at the end of the discharge, avoiding the non-physical jump caused by directly superimposing voltage drop using instantaneous switching.
[0055] According to the previous Calculate the total voltage of the stack, the lowest individual cell voltage, the average individual cell voltage, and the highest individual cell voltage using the terminal voltage of each effective cell: ; ; During the discharge process, the lowest single-cell voltage is used as the primary judgment parameter for weak single-cell identification and simulation termination. When the lowest single-cell voltage is lower than the preset single-cell discharge cutoff voltage, the simulation of the current discharge stage ends or an over-discharge risk flag is output. The total stack voltage, state of charge, and longest discharge time are used as auxiliary judgment parameters to avoid the low voltage state of weak single cells being masked by other single cells when relying solely on the total stack voltage.
[0056] Example 3: In this embodiment, as shown Figure 3 As shown, the comprehensive state characterization quantity is calculated based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk: ; In the formula, all risk quantities are normalized, and w1 to w6 are non-negative weights with a sum of 1. These weights can be adjusted based on experimental calibration results, historical operating data, or optimization algorithms. The comprehensive state characterization quantity can also be adjusted for gain based on low flow conditions, minimum unit voltage, or number of cycles, to compare the degradation degree under different units, different cycles, and different operating conditions.
[0057] In the multi-cycle simulation, each cycle includes charging, resting, discharging, and resting phases in sequence. The state of charge, electrolyte species concentration, and dynamic RC polarization are continuously updated according to the current operating mode; residual zinc, membrane resistance, effective reaction area, mass transfer capacity, fluid path blockage, and capacity state are retained between cycles, enabling the model to describe the accumulation, partial recovery, and irreversible evolution of degradation.
[0058] During the charging phase, zinc deposition and related degradation states are updated based on current, fluid flow rate, mass transfer risk, and cyclic stress; at low flow rates or with insufficient mass transfer margins, the accumulation rate of the corresponding degradation states increases. During the resting phase, electrode surface concentration, dynamic polarization, and recoverable degradation components are relaxed according to a preset recovery time constant.
[0059] During the discharge phase, the residual zinc degradation correction voltage drop is updated based on the dissolved zinc, low charge state, low monomer voltage, and local mass transfer state. As the number of cycles increases, the residual zinc, film resistance, and effective reaction area states of different monomers differentiate, causing weaker monomers to exhibit an earlier voltage drop at the end of the discharge.
[0060] The degradation correction voltage drop is generated using a continuous gate function, dynamic element, or bounded recursive relationship, so that voltage steps, shoulder changes, and premature collapse are gradually formed at the end of discharge, instead of using instantaneous switching to directly superimpose a fixed voltage drop.
[0061] Each simulation step records the state of charge, dynamic available capacity, electrolyte species concentration, open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, dynamic RC polarization, mass transfer ratio, limiting current, degradation state of each cell, terminal voltage of each cell, and stack statistics.
[0062] After completing the preset number of cycles, extract the charge-discharge curves of the first cycle, the last cycle, or a specified cycle, and calculate the voltage start value, discharge end voltage, minimum single-cell voltage, average single-cell voltage, single-cell dispersion, state characterization quantity, and the location and amplitude of voltage anomaly.
[0063] By changing the number of battery cells, fluid flow rate, initial difference parameters, or degradation parameters, simulation results under different model scales and operating conditions can be obtained. These results can be used for model parameter calibration, degradation mechanism analysis, weak cell localization, and offline comparison of the impact of external control strategies on battery state.
[0064] Example 4: like Figure 4 As shown, this invention can be implemented through computer programs, function blocks, state machines, or lookup tables, and can be deployed on MATLAB / Simulink, real-time simulators, or industrial computers. The model's input is provided by preset operating conditions, data files, or an external test platform. The model outputs unit-level and stack-level state variables according to a uniform simulation step size, and its functional scope is limited to modeling, calculation, and simulation.
[0065] The model can continuously update the electrochemical state and multi-monomer state based on actual operating data, and use the measured stack voltage or individual unit voltage to perform bounded corrections on at least one of the open-circuit voltage bias, film resistance, effective reaction area, mass transfer capacity, residual zinc state and capacity state, so that the simulated state is consistent with the actual stack.
[0066] The state of charge, dynamic available capacity, bulk and electrode surface concentrations of zinc ions and bromine active species, open-circuit voltage, various polarizations, limiting current, mass transfer ratio, mass transfer risk, residual zinc state, membrane resistance state, effective reaction area state, liquid path blockage state, individual cell terminal voltage, total stack voltage, minimum individual cell voltage, average individual cell voltage, maximum individual cell voltage, and comprehensive state characterization parameters obtained from the model calculations can be saved to a database or data file for parameter calibration, weak cell localization, mechanism analysis, model accuracy evaluation, and offline comparison of control strategies.
[0067] Based on this understanding, the technical solution of this application, in essence, or the part that contributes to the prior art, or part of the technical solution, can be embodied in the form of a computer program product.
[0068] The various embodiments in this application are described in a progressive manner. The same or similar parts between the various embodiments can be referred to each other. Each embodiment focuses on describing the differences from other embodiments.
[0069] The scope of protection of this application is not limited to the embodiments described above. Obviously, those skilled in the art can make various modifications and variations to this disclosure without departing from the scope and spirit of this disclosure. If such modifications and variations fall within the scope of the methods disclosed herein and their equivalents, then the intent of this disclosure also includes such modifications and variations.
Claims
1. A mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries, characterized in that, Includes the following steps: Step S1: Collect or set the operating condition data of the zinc-bromine redox flow battery stack, and set the model initialization parameters; Step S2: Update the state of charge and the bulk and electrode surface concentrations of zinc ion species and bromine active species based on the operating condition data; determine the flow-related mass transfer coefficient based on the liquid flow rate; and calculate the mass transfer ratio, mass transfer risk, and limiting current. Step S3: Calculate the concentration-related open-circuit voltage based on the electrode surface concentration and temperature, calculate the activation polarization, ohmic polarization, concentration polarization and dynamic RC polarization respectively, and combine them according to the charging, discharging or static operation mode. After continuous smoothing and finite gain processing, the electrochemical healthy baseline voltage is obtained. Step S4: Update the degradation state of each cell based on at least one of residual zinc content, membrane resistance state, effective reaction area state, mass transfer capacity, liquid path blockage state, capacity state, and cyclic stress, and obtain the terminal voltage of each cell based on the electrochemical health baseline voltage. Step S5: Calculate the total stack voltage, lowest single-cell voltage, average single-cell voltage, and highest single-cell voltage based on the terminal voltage of each battery cell, and use at least one of the following as the simulation termination judgment parameter for the current charging and discharging stage: lowest single-cell voltage, total stack voltage, state of charge, or preset simulation time. Step S6: Calculate the comprehensive state characterization based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk, and perform gain correction on the comprehensive state characterization based on at least one of low flow rate state, minimum monomer voltage, or number of cycles. Step S7: According to the preset simulation step size and cycle conditions, iteratively update the state of charge, electrolyte species concentration, dynamic RC polarization and degradation state of each cell, and output the simulation results of each cell terminal voltage, stack statistics, comprehensive state characterization, and the changes of each state quantity with time and cycle number.
2. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 1, characterized in that, The operating condition data in S1 includes stack current, liquid flow rate, temperature, operating mode, and time information, wherein the operating mode includes charging, discharging, and resting; the model initialization parameters include the number of battery cells, rated capacity, and initial difference parameters of each battery cell, wherein the initial difference parameters include capacity factor, internal resistance factor, mass transfer factor, and open circuit voltage bias. The zinc-bromine flow battery stack comprises N battery cells connected in series, where N is a positive integer; the length is N, which is the maximum number of cells. max A fixed-dimensional state vector is used to store the operating state of each battery cell, and the state is updated only for the first N valid cells in the fixed-dimensional state vector. If the charging current of a single battery cell is defined as positive and the discharging current as negative, then the state of charge is updated discretely according to the following formula: ; Among them, SOC k Let I be the state of charge at time k. k Let be the stack current at time k. To account for dynamic available capacity after capacity degradation, and These are the charging coulombic efficiency and the discharging coulombic efficiency, respectively. To calculate the step size for discrete calculations, (.) indicates a limit operation, which means that when the input value is less than 0, it takes 0; when it is greater than 1, it takes 1; and when it is between 0 and 1, it retains the original value.
3. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 2, characterized in that, The update described in S2 specifically refers to the following: For electrolyte species j, its electrode surface concentration is updated based on the difference between the mass transfer from the bulk electrolyte to the electrode surface and the species consumption or generation caused by the electrochemical reaction. ; Where j represents a zinc ion species or a bromine-active species; and These are the bulk concentration and electrode surface concentration of species j at time k, respectively; For traffic The mass transfer coefficient of species j under the given conditions; For the operating mode The reaction direction coefficient is determined, taking the value 1 when species j is consumed and 1 when species j is generated. 1; These are stoichiometric coefficients; Where is the electron transfer number; F is the Faraday constant; This represents the effective electrolyte volume of the corresponding reaction region; Furthermore, the ratio of the electrode surface concentration of electrolyte species j to its corresponding bulk concentration is determined as the mass transfer ratio. : ; The smaller of the mass transfer ratios of zinc ion species and bromine active species was determined as the overall mass transfer ratio. : ; in, and These represent the mass transfer ratios of zinc ion species and bromine active species, respectively. A very small positive number set to prevent the denominator from being zero; Any species participating in the electrode reaction The corresponding limiting current is calculated according to the following formula. : ; in, For the first The effective reaction area at any given time; the smaller of the limiting currents corresponding to each reactant species is determined as the battery limiting current. : ; The mass transfer load ratio is determined based on the ratio of the actual current to the battery's limiting current. ; in Let be the mass transfer load ratio at time k. The current at time k is the stack operating current. The limiting current is calculated based on the electrode mass transfer state; sat [0,1] ( () indicates a limit operation that restricts the calculation result to the range of 0 to 1; And determine the mass transfer margin based on the mass transfer loading ratio: ; in Let be the mass transfer margin at time k, representing the margin remaining between the current operating current and the ultimate mass transfer capability. Further determine the mass transfer risk based on the mass transfer loading ratio and electrolyte mass transfer state: ; in, To normalize mass transfer risk, The risk component is determined based on the mass transfer load ratio. The risk component is determined based on the species concentration deficit on the electrode surface and the flow rate in the liquid path. and The weights are non-negative; the mass transfer risk is limited to the range of 0 to 1; the closer the actual current is to the limiting current, or the more significantly the species concentration on the electrode surface deviates from the bulk concentration, the higher the mass transfer risk.
4. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 3, characterized in that, The concentration-related open-circuit voltage mentioned in S3 Calculated based on the reaction quotient formed by the activities of zinc ion species and bromine active species: ; Among them, E 0 Where R is the standard electrode potential, and T is the gas constant. k Let be the temperature at time k, and F be the Faraday constant. The reaction quotient is composed of the electrode surface activities of zinc ion species and bromine active species at time k, where n is the number of electrons transferred in the corresponding electrode reaction. The activation polarization Ohmic polarization and concentration polarization Calculate according to the following formulas respectively: ; ; ; Where α is the charge transfer coefficient and i0 is the exchange current density. Based on the ohmic resistor, For membrane resistance, Let A be the limiting current, T be the absolute temperature of the battery at the current moment, and A be the limiting current. eff The effective reaction area of the electrode is asinh( ) is an inverse hyperbolic sine function; I is the actual current flowing through the fuel cell stack; The dynamic RC polarization Update according to the following formula: ; in, For the first Dynamic polarization resistance at any given time. For the first The time constant at any given moment; The concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization are combined according to the current operating mode to obtain the electrochemically calculated voltage. Limiting and finite gain corrections are applied to the deviation between the electrochemically calculated voltage and the continuous reference voltage. ; in, The electrochemical voltage at time k is obtained by combining the concentration-dependent open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, and dynamic RC polarization according to the current operating mode. The target healthy baseline voltage after finite gain correction. This is a continuous reference voltage determined based on the current operating mode and state of charge, where m represents the current operating mode, including charging mode, discharging mode, and idle mode. For the finite gain coefficient corresponding to the operating mode, sat( ) is the amplitude limiting function; Further, first-order dynamic smoothing was employed to obtain the electrochemical healthy baseline voltage: ; in, The electrochemical health baseline voltage output at time k; The first-order dynamic smoothing coefficient at time k is determined according to the following formula: ; in, To simulate the discrete calculation step size, This is a smoothing time constant determined based on the charging mode, discharging mode, and resting mode.
5. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 4, characterized in that, S4 describes updating the degradation state of each battery cell as follows: The degradation state of each battery cell includes at least the residual zinc state. Membrane resistance state Effective reaction area status Liquid circuit blockage Mass transfer capability status and capacity status Any degenerate state Discrete updates are performed according to the following formula: ; in, This represents the degenerate state at time k+1. This is the accumulation or recovery function corresponding to the degradation state in charging, discharging, or idle operation modes. These represent the upper and lower bound constraints corresponding to the degenerate state; No. The combined degradation driving force D of each battery cell i Determined according to the following formula: ; in, For low flow stress, to Non-negative weights; The comprehensive aging-related polarization voltage drop of the i-th cell is obtained based on the comprehensive degradation driving force. The degradation correction voltage drop was determined based on the residual zinc state and the local mass transfer state. ; The terminal voltage of the i-th battery cell at time k. Calculate according to the following formula: ; in, For the first Open-circuit voltage bias of each battery cell.
6. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 5, characterized in that, S5 The total voltage of the fuel cell stack Minimum unit voltage Average cell voltage and highest single-cell voltage Calculate according to the following formulas respectively: ; ; ; ; During the discharge process, when the lowest single-cell voltage satisfies the following formula, the simulation of the current discharge stage ends or an over-discharge risk flag is output: ; in, This is the preset discharge cutoff voltage for a single cell.
7. The method for multi-cell modeling and simulation of zinc-bromine flow batteries under mechanistic constraints according to claim 1, characterized in that, The comprehensive state characterization quantity H described in S6 is calculated according to the following formula: ; in, , , , , and These are the normalized mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk; to The weights are non-negative and satisfy: .
8. A mechanism-constrained multi-cell modeling and simulation system for zinc-bromine flow batteries, used to implement the mechanism-constrained multi-cell modeling and simulation method for zinc-bromine flow batteries as described in claim 1, characterized in that, include: The simulation conditions and parameter initialization module, the state of charge and electrolyte species balance module, the electrochemical health baseline voltage calculation module, the multi-monomer initial difference configuration module, the multi-monomer state update module, the monomer terminal voltage assembly and stack statistics module, the comprehensive state characterization module, and the simulation iteration and data recording module. The simulation operating condition and parameter initialization module is used to acquire operating condition data and set the number of battery cells, rated capacity and initial difference parameters. The state of charge and electrolyte species balance module is used to update the bulk concentration and electrode surface concentration of the state of charge, zinc ion species, and bromine active species. The electrochemical health baseline voltage calculation module is used to calculate concentration-related open-circuit voltage, activation polarization, ohmic polarization, concentration polarization, dynamic RC polarization, mass transfer ratio, mass transfer risk, and limiting current, and to obtain the electrochemical health baseline voltage. The multi-cell initial differential configuration module is used to configure the capacity factor, internal resistance factor, mass transfer factor and open-circuit voltage bias for each cell. The multi-cell state update module is used to update the residual zinc state, membrane resistance state, effective reaction area state, mass transfer capacity state, liquid path blockage state, and capacity state of each battery cell. The single-cell terminal voltage assembly and stack statistics module is used to obtain the terminal voltage of each battery cell and calculate the total stack voltage, the lowest single-cell voltage, the average single-cell voltage, and the highest single-cell voltage. The comprehensive state characterization module is used to calculate the comprehensive state characterization quantity based on mass transfer risk, concentration risk, residual zinc risk, membrane resistance risk, effective reaction area loss risk, and liquid path blockage risk. The simulation iteration and data recording module is used to iteratively update the model state according to the preset simulation step size and cyclic working conditions, and output and save the multi-cycle dynamic simulation results.