A photonic chip packaged switching module for fiber-to-wireless dual-mode communication

By integrating optical path switching, signal detection, and intelligent control within the photonic chip package, the problems of slow switching response, numerous hardware components, and poor stability in fiber-to-wireless dual-mode communication are solved. This achieves millisecond-level uninterrupted adaptive switching and highly stable communication, making it suitable for industrial applications and outdoor mobile terminal applications.

CN123122667APending Publication Date: 2026-11-17BEIJING ZIYIXIN INTEGRATED CIRCUIT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611188480.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-06
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing photonic chip packaging only has a single optical path transmission function and cannot realize fiber-to-wireless dual-mode communication. This results in long switching response time, a large number of hardware components, complex wiring, and poor communication stability, which cannot meet the real-time control and ultra-high-definition video transmission requirements of industrial equipment.

Method used

The optical path switching, signal detection, and intelligent control are integrated into the photonic chip package. The MEMS optical path switching unit, signal detection unit, and control unit are used to achieve millisecond-level uninterrupted adaptive switching of fiber-to-wireless dual-mode communication. The optical/electric composite interface unit is integrated to realize bidirectional transmission of optical signals and power, and supports local threshold discrimination and AI neural network collaborative switching.

Benefits of technology

Significantly reduces the number of hardware components and wiring complexity, lowers costs, improves communication bandwidth and transmission stability, achieves millisecond-level optical path switching response, supports dynamic optimization of communication links, meets the needs of industrial real-time control and ultra-high-definition video transmission, and adapts to complex application environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123122667A_ABST
    Figure CN123122667A_ABST
Patent Text Reader

Abstract

This invention discloses a photonic chip packaged switching module for fiber-to-wireless dual-mode communication, belonging to the field of optical communication chip functional integration packaging technology. Using an alumina ceramic substrate as the carrier, it integrates a metallized circuit layer and an integrated copper ground layer, and incorporates a photonic chip, a MEMS optical path switching unit, a signal detection unit, a control unit, and an optical / electrical composite interface unit. The signal detection unit collects dual-channel quality parameters such as optical power and signal-to-noise ratio in real time. The control unit, combined with local threshold discrimination and 6G system AI collaborative instructions, drives the MEMS unit to complete bidirectional switching between fiber optic and wireless photonic optical paths, with an overall response time ≤1ms. This invention integrates dual-mode switching within the package, eliminating the need for external hardware, reducing coupling insertion loss, and possessing millisecond-level uninterrupted switching, intelligent link optimization, and high-reliability protection characteristics, making it suitable for 6G converged communication scenarios such as intelligent manufacturing mobile devices and ultra-high-definition terminals.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of optical communication chip functional integration and packaging technology, and relates to photonic wafer integrated packaging and 6G fiber-wireless integrated communication technology. Specifically, it relates to a photonic wafer packaging switching module for fiber-wireless dual-mode communication and its preparation method. Background Technology

[0002] The 6G communication architecture, with its core of wired fiber optic transmission and wireless photonic radio frequency transmission, enables seamless communication even when equipment is moving at high speeds. Devices such as intelligent manufacturing mobile production line robots, outdoor ultra-high-definition mobile live streaming terminals, and industrial mobile sensor nodes all require frequent switching of communication links between fixed fiber optic cabling areas and wireless coverage zones, placing stringent demands on switching real-time performance, transmission stability, and device integration.

[0003] Current commercial photonic chip packages only have single-path transmission capabilities and lack a built-in fiber-to-wireless dual-mode optical path switching structure. When the device switches between wired and wireless communication, it must be connected to an external independent optical path switching device, an external RF signal detection board, and an independent control MCU, which has the following technical drawbacks: 1. The switching link is external, with multiple hardware layers and long signal transmission links. The switching response time is generally greater than 5ms. During the switching process, problems such as optical signal interruption, video stuttering, and industrial control command packet loss are very likely to occur, which cannot meet the requirements of real-time control of industrial equipment and uninterrupted transmission of 4K / 8K ultra-high-definition video. 2. External switching devices, signal detection boards, and independent control units significantly increase the number of hardware components, wiring complexity, and overall size of the device, making equipment integration more difficult and material and assembly costs significantly higher. 3. The external switching component and the optical path of the photonic chip rely on multiple fiber optic jumpers for coupling. Multiple couplings introduce additional insertion loss, reducing the overall communication bandwidth and transmission stability. 4. The external switching device lacks supporting 6G system coordination logic, only supports manual switching with fixed thresholds, and cannot dynamically and adaptively optimize communication links based on real-time channel quality, resulting in poor communication stability when the channel fluctuates.

[0004] Existing commercial single-fiber bidirectional and dual-fiber bidirectional optical modules can only achieve bidirectional data transmission within the optical fiber link, and do not have the ability to switch between the optical fiber link and the wireless photonic link, making them unsuitable for 6G fiber-wireless integrated application scenarios. Summary of the Invention

[0005] The purpose of this invention is to provide a photonic chip packaged switching module for fiber-to-wireless dual-mode communication, which integrates optical path switching, real-time signal detection, intelligent control, and dual-mode interface into the photonic chip package, eliminating the need for external switching hardware and achieving millisecond-level uninterrupted adaptive switching.

[0006] The objective of this invention is achieved through the following technical solution: A photonic chip packaging switching module for fiber-optic-wireless dual-mode communication includes an alumina ceramic substrate, on which a metallized circuit layer and an integrated copper ground layer are disposed; a photonic chip, a MEMS optical path switching unit, a signal detection unit and a control unit are disposed on the metallized circuit layer, and an optical / electrical composite interface unit is disposed on one side of the metallized circuit layer; The optical / electric composite interface unit is used to connect to an external optical fiber wired communication link and a 6G wireless photonic radio frequency communication link, respectively. At the same time, it connects to the internal optical path of the photonic chip through the optical path to realize bidirectional transmission of optical signals, power and control data. The signal detection unit is connected to the optical / electric composite interface unit via optical coupling and electrical coupling, and is used to collect multi-channel quality parameters of the optical fiber channel and the wireless photonic channel in real time. The output terminal of the signal detection unit is electrically connected to the input terminal of the control unit, and the signal output terminal of the control unit is electrically connected to the control terminal of the MEMS optical path switching unit. The MEMS optical path switching unit is disposed on the main optical path of the photonic chip and is connected to the main transmission optical path of the photonic chip, the optical fiber channel optical path and the wireless photonic channel optical path respectively. The control unit has a built-in local signal threshold discrimination program and a reserved high-speed communication interface for bidirectional data interaction with the AI ​​neural network algorithm of the 6G converged communication system. It is used to autonomously output switching drive signals based on real-time channel quality data to control the MEMS optical path switching unit to complete bidirectional switching between fiber optic path and wireless photonic path.

[0007] As a further improvement of the present invention, an optical isolation structure is provided on the alumina ceramic substrate surrounding the photonic wafer, and the optical isolation structure surrounds the photonic wafer; the refractive index of the optical isolation structure is 1.45~1.50, the gap between the photonic wafer and the optical isolation structure is 0.1~0.2μm, and the gap deviation is controlled within ±0.02μm.

[0008] As a further improvement of the present invention, the optical / electric composite interface unit includes an optical fiber coupling interface, an radio frequency interface and a BGA pad, and an epoxy sealant layer is provided at the root of each interface. The fiber optic coupling interface is fixed at one end of the optical path, and its optical path is aligned with the photonic wafer, with a docking gap ≤0.1μm; The radio frequency interface is a 6G wireless photonic radio frequency integrated sub-interface, which is fixed on the signal detection unit; The BGA pads are soldered and fixed to the electrical interconnect pins of the metallized circuit layer.

[0009] As a further improvement of the present invention, the signal detection unit integrates a photodetector, an RF acquisition chip and a 12-bit ADC analog-to-digital converter module, and is synchronously coupled to the optical / electrical composite interface unit through optical and electrical dual-path coupling; the sampling period of the signal detection unit is ≤200μs, and it is used to synchronously acquire four types of channel quality parameters: optical power, signal-to-noise ratio, RF bit error rate and channel attenuation.

[0010] As a further improvement of the present invention, the control unit is an MCU control unit, which has built-in logic for switching thresholds of optical power, signal-to-noise ratio and bit error rate, and is equipped with a high-speed serial communication interface for bidirectional interconnection with the AI ​​brain of the 6G system; the control unit supports dual verification of local threshold independent discrimination and AI neural network switching prediction instructions, and can transmit link status data back in real time after the switching is completed.

[0011] As a further improvement of the present invention, the MEMS optical path switching unit is a MEMS dual-channel optical switch, which is fixed on the metallized circuit layer by eutectic bonding.

[0012] As a further improvement of the present invention, a copper-nickel alloy electromagnetic shielding layer is provided on the alumina ceramic substrate, and the copper-nickel alloy electromagnetic shielding layer covers the photonic wafer, MEMS optical path switching unit, optical isolation structure, signal detection unit, control unit and optical path; The alumina ceramic substrate is further provided with an epoxy molding layer covering a copper-nickel alloy electromagnetic shielding layer. After molding, only the optical / electrical composite interface unit and part of the integrated copper grounding layer are exposed.

[0013] As a further improvement of the present invention, the copper-nickel alloy electromagnetic shielding layer is an alloy plating layer of 80% Cu and 20% Ni, with a thickness of 5~10μm, a thickness uniformity deviation of no more than ±0.5μm, and a connection resistance of ≤0.05Ω with the grounding pin.

[0014] A method for fabricating a photonic wafer packaged switching module for fiber-optic-wireless dual-mode communication, completed entirely in a Class 1000 cleanroom, includes the following steps: Step 1: Preparation of ceramic packaging substrate and grounding shield layer: Prepare alumina ceramic substrate green blank and sinter to densify it. Sputter to form a metallized circuit layer on it. Co-fire the copper grounding layer and grounding pin to form an integrated copper grounding layer without solder interface. Step 2: Photonic wafer and MEMS optical path switching unit eutectic coupling assembly: After the photonic wafer and MEMS optical path switching unit are precisely positioned, eutectic bonding is completed through a vacuum eutectic furnace to achieve micron-level optical path coupling; Step 3: Surface mount soldering of signal detection unit and control unit: The signal detection unit and control unit are mounted by SMT and electrically connected by lead-free reflow soldering to build the signal acquisition and intelligent control circuit. Step 4: Optical / Electrical Composite Interface Coupling Integration: Sequentially assemble the BGA pads, fiber optic coupling interface, and RF interface. After completing the coupling calibration of the optical path, RF, and electrical interconnects, apply adhesive to seal and cure. Step 5: Electromagnetic shielding coating and epoxy molding: Electroplating is used to prepare a copper-nickel alloy electromagnetic shielding layer, and then an epoxy molding layer is formed by injection molding and cured at high temperature.

[0015] As a further improvement of the present invention, in step 1, the alumina ceramic substrate green body is obtained by vacuum sintering at 1600±50℃ for 2 hours, with a heating and cooling rate not exceeding 5℃ / min; the metallized circuit layer is a Ti transition layer and a high-purity copper layer sputtered sequentially, with a copper layer thickness of 10~15μm and a purity of not less than 99.99%; the integrated copper grounding layer is formed by co-firing at 850℃ for 30 minutes. In step 2, eutectic bonding is carried out in a vacuum eutectic furnace with an oxygen content of less than 10 ppm, the eutectic temperature is 280~300℃, the holding time is 60s, and the welding pressure is 0.5~1MPa; after coupling, the optical path insertion loss increment is ≤0.08dB, and the welding adhesion of the photonic wafer is ≥5N / mm². In step 4, high-temperature resistant epoxy sealant is used for sealing and curing. The curing temperature is 80~100℃, and the heat preservation time is 30~45 minutes. After curing, the module achieves an IP67 dustproof and waterproof rating.

[0016] The above technical solution has the following beneficial effects: 1. The optical path switching, signal detection, intelligent control and dual-mode interface are all integrated into the photonic chip package, eliminating the need for external switching equipment, detection boards and independent control units, which greatly reduces the number of hardware, wiring complexity and overall size, and reduces material and assembly costs; at the same time, it avoids the additional insertion loss introduced by the coupling of multiple fiber optic patch cords, and improves communication bandwidth and transmission stability.

[0017] 2. Relying on the built-in MEMS optical path switching unit, signal detection unit and control unit, the overall optical path switching response time is ≤1ms, which is far better than the switching delay of more than 5ms of the traditional external solution. It can effectively avoid optical signal interruption, video stuttering and industrial command packet loss during the switching process, and meet the stringent requirements of industrial real-time control and uninterrupted transmission of 4K / 8K ultra-high-definition video.

[0018] 3. It supports dual verification of independent local threshold discrimination and AI neural network switching prediction of 6G system. It can dynamically select the best communication link based on real-time collected parameters such as optical power, signal-to-noise ratio, bit error rate, and channel attenuation, which significantly improves communication stability in channel fluctuation scenarios. At the same time, it supports link status feedback to realize closed-loop iterative optimization of the switching algorithm.

[0019] 4. It adopts a multi-layer protection design with ceramic encapsulation substrate, integrated copper grounding layer, copper-nickel alloy electromagnetic shielding layer and epoxy encapsulation. The shielding effectiveness in the 10~3000MHz frequency band is ≥80dB. It has IP67 dustproof and waterproof capability and wide temperature adaptability from -40℃ to 150℃. It can stably adapt to complex application environments such as industrial sites and outdoor mobile terminals.

[0020] 5. It adopts a standardized optical / electrical composite interface unit, which can be directly adapted to existing 6G fiber-wireless converged communication equipment without additional modification, making it easy to promote and apply on a large scale. Attached Figure Description

[0021] To more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings in the following description are merely exemplary, and those skilled in the art can derive other embodiments based on the provided drawings without creative effort.

[0022] The structures, proportions, sizes, etc. shown in this specification are only used to complement the content disclosed in the specification for those skilled in the art to understand and read, and are not intended to limit the conditions under which the present invention can be implemented. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in the proportional relationships, or adjustments to the size, without affecting the effects and objectives that the present invention can produce, should still fall within the scope of the technical content disclosed in the present invention.

[0023] Figure 1 This is a schematic diagram of the preparation method provided by the present invention.

[0024] Figure 2 A schematic diagram of the product structure prepared in step 1 of this invention.

[0025] Figure 3 A schematic diagram of the product structure prepared in step 2 of this invention.

[0026] Figure 4 A schematic diagram of the product structure prepared in step 3 of this invention.

[0027] Figure 5 A schematic diagram of the product structure prepared in step 4 of this invention.

[0028] Figure 6 A schematic diagram of the product structure prepared in step 5 of this invention.

[0029] In the picture: 1. Alumina ceramic substrate; 2. Metallized circuit layer; 3. Integrated copper ground layer; 4. Photonic wafer; 5. MEMS optical path switching unit; 6. Optical isolation structure; 7. Signal detection unit; 8. Control unit; 9. Optical path; 10. Fiber optic coupling interface; 11. RF interface; 12. BGA pads; 13. Copper-nickel alloy electromagnetic shielding layer; 14. Epoxy encapsulation layer. Detailed Implementation

[0030] In this invention, unless otherwise stated, directional terms such as "upper," "lower," "top," and "bottom" are generally used in relation to the direction shown in the accompanying drawings, or in relation to the vertical, perpendicular, or gravitational direction of the component itself; similarly, for ease of understanding and description, "inner" and "outer" refer to the inner and outer contours of each component itself, but the above directional terms are not intended to limit this invention.

[0031] like Figure 1 As shown, a method for fabricating a photonic chip packaged switching module for fiber-optic-wireless dual-mode communication is completed entirely in a Class 1000 cleanroom, and specifically includes the following steps: Step 1: Fabrication of ceramic packaging substrate and grounding shield layer The purpose of the ceramic packaging substrate and grounding shielding layer fabrication process is to complete the alumina ceramic substrate molding, metallized circuit layer and integrated copper grounding layer sintering, and to build the module's load-bearing substrate and grounding shielding foundation. The resulting product structure is as follows: Figure 2 As shown.

[0032] The process begins with raw material pretreatment. High thermal conductivity alumina ceramic powder is ball-milled and mixed into a slurry according to a specified ratio. Then, a ceramic casting machine is used to complete the green body casting and shaping. The green body is then processed into a standard substrate of 6.0mm × 4.0mm using a laser cutting machine, with the four corners rounded to R0.3mm to form the green body of alumina ceramic substrate 1. The green body is then sent to a vacuum sintering furnace for high-temperature debinding and sintering. The sintering temperature is controlled at 1600±50℃, the holding time is 2h, and the heating and cooling rates do not exceed 5℃ / min to prevent the substrate from cracking, thus completing the densification treatment of alumina ceramic substrate 1.

[0033] After sintering, a Ti transition layer and a high-purity copper layer are sequentially sputtered onto the surface of the alumina ceramic substrate 1 using a thin-film sputtering machine to form a metallized circuit layer 2. The thickness of the copper layer is controlled at 10~15μm, the copper purity is not less than 99.99%, and the vacuum degree of the sputtering environment must be ≤1×10⁻⁶. -3Pa. The alumina ceramic substrate 1 and the metallized circuit layer 2 are combined to form a ceramic packaging substrate.

[0034] After sputtering, the copper grounding layer and the grounding pin are kept at 850℃ for 30 minutes to complete the integrated co-firing of the copper grounding layer and the grounding pin, forming an integrated copper grounding layer 3 without a solder interface.

[0035] After being cleaned using a dust-free ultrasonic cleaner, the finished ceramic packaging substrate is dried at 120℃ for 15 minutes. Subsequently, samples are taken to test the performance of the ceramic packaging substrate. The substrate must be free of cracks, pores, and warping; flatness ≤ 0.02 mm; thermal conductivity ≥ 200 W / (m・K); surface resistance of the integrated copper grounding layer 3 ≤ 0.05 Ω / ☑; total grounding resistance ≤ 0.1 Ω; perpendicularity of the grounding pins ≤ 0.05 mm; and dimensions of 0.5~1.0 mm wide and 2~3 mm long. Qualified ceramic packaging substrates are vacuum-sealed for later use; unqualified products are individually marked and scrapped. The entire process must be carried out in a dust-free environment, and touching the ceramic working surface with bare hands is prohibited.

[0036] Step 2: Eutectic coupling assembly of photonic wafer and MEMS optical path switching unit The eutectic coupling assembly process between the photonic chip 4 and the MEMS optical path switching unit 5 is used to precisely attach the 250GHz photonic chip 4 and the MEMS optical path switching unit 5 to corresponding positions on the ceramic packaging substrate, completing the integrated optical path coupling to construct the core optical path switching path. The resulting product structure is as follows: Figure 3 As shown in the figure. Among them, the MEMS optical path switching unit 5 adopts a MEMS dual-channel optical switch.

[0037] Pre-treatment of the photonic chip 4 is completed by applying a small amount of Ni / Au thin film flux to the pads. At the same time, AuSn solder is pre-placed on the pads of the metallization layer 2 corresponding to the photonic chip 4 and the MEMS optical path switching unit 5.

[0038] During operation, the ceramic packaging substrate is first picked up by a vacuum chuck and fixed by a positioning fixture. Using an anti-static vacuum nozzle with ESD protection level of Class 0, the photonic chip 4 and the MEMS dual-channel optical switch are picked up in sequence and placed on the corresponding metallization layer 2 pads. The MEMS dual-channel optical switch is aligned with the main optical path of the photonic chip 4 to achieve precise coupling of the micron-level optical path.

[0039] In the chip bonding area where the photonic chip 4 is placed, an optical isolation structure 6 is set on the ceramic packaging substrate surrounding the chip bonding area. The refractive index of the optical isolation structure 6 is 1.45~1.50 and it is assembled without misalignment, thus surrounding the photonic chip 4. The gap between the photonic chip 4 and the optical isolation structure 6 is in the range of 0.1~0.2μm, and the deviation is controlled within ±0.02μm.

[0040] After the photonic chip 4 and the MEMS dual-channel optical switch are positioned, the workpiece is clamped by the tooling and sent into the vacuum eutectic furnace to complete the eutectic bonding. The oxygen content in the furnace must be less than 10ppm to prevent metal oxidation. The eutectic temperature is set to 280~300℃, held for 60s, and the welding pressure is controlled at 0.5~1MPa.

[0041] After the eutectic bonding is completed, the optical path is finely adjusted and calibrated again through an optical alignment stage. Then, a tensile test and 3D microscopic appearance inspection are performed. The photonic wafer is required to be free of chipping, scratches and electrode damage. The dual-channel optical path of the MEMS dual-channel optical switch is free of offset and obstruction. The eutectic solder joint is free of cold solder joints, voids and solder overflow. The insertion loss increment of the optical path after coupling is ≤0.08dB. The welding adhesion of photonic wafer 4 is ≥5N / mm². The qualified semi-finished products are transferred to the buffer station. External force is prohibited from squeezing the chip optical path area throughout the operation.

[0042] Step 3: Surface mount soldering of signal detection unit and control unit The surface mount soldering process for signal detection unit 7 and control unit 8 is used to complete the surface mount soldering of photodetector, RF acquisition chip, analog-to-digital converter module and MCU control unit, and to build signal acquisition and intelligent control circuit. The resulting product structure is as follows: Figure 4 As shown in the diagram. Control unit 8 is the MCU control unit, and signal detection unit 7 refers to the photodetector, RF acquisition chip, and 12-bit ADC analog-to-digital converter module.

[0043] During the operation, the product prepared in step 2 is first loaded and locked in place using a positioning fixture. Low-temperature solder paste is then precisely printed onto the pads of the corresponding signal detection unit 7 and control unit 8 on the metallized circuit layer 2 using a stencil. The solder paste must be used within 4 hours after opening to avoid failure. Subsequently, a fully automated SMT placement machine is used to complete high-speed placement, sequentially mounting the photodetector, RF acquisition chip, 12-bit ADC analog-to-digital converter module, and MCU control unit. The placement positioning accuracy can reach ±0.01mm.

[0044] Among them: the photodetector is responsible for splitting and collecting the optical power and signal-to-noise ratio of the optical fiber and wireless optical signals, and completing the optical-to-electric conversion; the radio frequency acquisition chip is used to collect the bit error rate and channel attenuation parameters of the wireless photonic link; the 12-bit ADC analog-to-digital conversion module is responsible for converting the analog optical / radio frequency signals into high-precision digital signals.

[0045] The photodetector, MCU control unit, MEMS dual-channel optical switch and photonic chip 4 are connected via optical path 9; the radio frequency acquisition chip, 12-bit ADC analog-to-digital conversion module and MCU control unit are electrically connected.

[0046] After mounting, the chip is sent to a lead-free reflow oven for soldering. The peak temperature of the reflow oven is 245±5℃, and the constant temperature zone is maintained for 90 seconds. During the soldering process, the RF acquisition chip must not be baked at high temperature for a long time.

[0047] After soldering, the solder joints are fully inspected by an AOI optical inspection instrument. Then, electrical performance continuity tests are performed to test the connectivity of the power supply pins and data communication pins of the MCU control unit and the signal detection unit 7. All components are required to be free from defects such as misalignment, tombstoning, insufficient solder, and solder bridging. The power supply circuit must have a 100% continuity rate and no short circuits or leakage. The optical path 9 must be unobstructed.

[0048] In this process, the overall sampling period of the signal detection unit 7 is ≤200μs; the MCU control unit realizes bidirectional data interaction with the AI ​​brain of the 6G system through a high-speed serial port, with a communication rate of up to 1Gbps. It can receive data from the signal detection unit 7 and send drive signals to control the MEMS dual-channel optical switch, while transmitting the switching status back to the host AI system.

[0049] Step 4: Optical / Electrical Composite Interface Coupling and Integration The installation of fiber optic coupling interface 10, RF interface 11, and BGA pad 12 completes the connection of optical path, RF, and electrical interconnections, and achieves IP67-level sealing protection. The resulting product structure is as follows: Figure 5 As shown. Specifically: Before starting the work, clean the interface window to remove dust and impurities. First, install the BGA pad 12. The metallized circuit layer 2 has electrical interconnect pins. Solder the BGA pad 12 to the electrical interconnect pins at a temperature of 230℃. The soldering time for a single solder joint is 3 seconds. After soldering, perform a full inspection of the electrical connection conductivity. The conductivity rate is required to be 100%, and there should be no defects such as cold solder joints or solder bridges.

[0050] Subsequently, optical path coupling is performed, fixing the fiber optic coupling interface 10 to one end of the optical path 9, aligning the optical path of the fiber optic coupling interface 10 with the photonic crystal 4, and fine-tuning the mating gap to ≤0.1μm to ensure that the fiber insertion loss is ≤0.1dB. Simultaneously, fiber optic coupling calibration is performed at the junctions of the control unit 8, signal detection unit 7, photonic crystal 4, and MEMS optical path switching unit 5 with the optical path 9 to improve the stability of optical signal transmission.

[0051] RF interface 11 is a 6G wireless photonic RF integrated sub-interface, which is fixed on the signal detection unit 7 to complete the coupling calibration of the RF optical path. After all interfaces are connected, high-temperature resistant epoxy sealant is applied to the base of the interface. The sealant has a temperature resistance range of -40℃ to 150℃, and the amount of sealant applied is strictly controlled to avoid overflow and contamination of the internal optical path.

[0052] After the dispensing is completed, the assembly is sent to a constant-temperature oven for curing. The curing temperature is set to 80~100°C, and the temperature is maintained for 30~45 minutes. Vibration of the tooling is prohibited during the curing process to prevent interface offset. After curing is completed, the optical path insertion loss and the connectivity of the radio frequency path are tested, followed by an IP67 waterproof and dustproof leak test at a test pressure of 0.5 bar. A product is qualified if no leakage occurs after 5 minutes of pressure holding; products that fail the leak test need to have the old adhesive removed before re-dispensing and curing. The final requirements are that the fiber coupling has no offset, no fiber breakage, no light leakage, the sealant completely covers the root of the interface, and there are no defects such as bubbles and missing adhesive.

[0053] Step 5: Electromagnetic shielding coating and epoxy molding compound encapsulation The electromagnetic shielding coating and epoxy molding compound encapsulation process realizes the integration of electromagnetic shielding, mechanical protection and environmental protection by depositing a copper-nickel alloy shielding layer and performing integral epoxy encapsulation, and the product structure prepared thereby is as Figure 6 shown in the figure.

[0054] A copper-nickel alloy electromagnetic shielding layer 13 with 80% Cu and 20% Ni is prepared on the alumina ceramic substrate 1 by an electroplating process. The thickness of the above copper-nickel alloy electromagnetic shielding layer 13 is controlled at 5~10 μm, with a uniform thickness deviation not exceeding ±0.5 μm. The copper-nickel alloy electromagnetic shielding layer 13 covers the photonic chip 4, the MEMS optical path switching unit 5, the optical isolation structure 6, the signal detection unit 7, the control unit 8 and the optical path 9 on the alumina ceramic substrate 1, leaving only part of the integrated copper ground layer 3 and the electrical interconnection pins on the metallized circuit layer exposed.

[0055] Before electroplating, surface oil stains and dust must be thoroughly removed to ensure the adhesion of the plating layer. The connection resistance between the copper-nickel alloy electromagnetic shielding layer 13 and the ground pin must be ≤0.05Ω. After electroplating is completed, the workpiece is cleaned with pure water and dried, and the thickness uniformity of the copper-nickel alloy electromagnetic shielding layer 13 is inspected. Products with a damaged copper-nickel alloy electromagnetic shielding layer 13 must be re-plated, and direct encapsulation is prohibited.

[0056] Subsequently, the epoxy encapsulation operation is performed. First, the low optical loss epoxy molding compound is preheated to 90°C, then the workpiece is placed into a mold for mold clamping and injection molding. After encapsulation, only the optical / electrical composite interface is exposed, and the thickness of the epoxy encapsulation layer 14 is controlled at 0.8~1.2 mm; after injection molding is completed, high-temperature curing is performed at a curing temperature of 130°C for 1.5 hours, followed by slow cooling at a rate of ≤10°C / min to prevent delamination of the epoxy encapsulation layer 14.

[0057] After curing is completed, the encapsulation flash and burrs are removed, and the appearance is polished and trimmed. Then, the shielding effectiveness and encapsulation performance are tested by sampling. The requirements are that the copper-nickel alloy electromagnetic shielding layer 13 completely covers the photonic chip 4 and the MEMS optical path switching unit 5 without exposed gaps, the shielding effectiveness is ≥80dB in the frequency band of 10~3000MHz; the epoxy encapsulation layer 14 has no defects such as bubbles, delamination, sink marks and cracks, the optical loss of the molding compound is ≤0.1dB / cm, and the insulation resistance is ≥1014 Ω·cm, the rounded corners of the plastic encapsulation shell are intact, and the dimensions are consistent with the drawing.

[0058] Step 6: Dual-mode switching, electromagnetic compatibility, high and low temperature reliability comprehensive test The dual-mode switching, electromagnetic compatibility and high and low temperature reliability comprehensive test process is used to complete full-dimensional performance testing, verify switching delay, isolation, anti-interference capability and environmental reliability, and screen qualified finished products.

[0059] The test first carries out a preliminary appearance inspection to confirm that the epoxy plastic encapsulation layer 14, interfaces and pins are complete and undamaged; then a basic electrical performance test is performed to verify whether the communication links of the power supply loop, MCU control unit and 6G AI brain are normal. The core performance test includes optical path dual-mode switching performance test, which uses a 250GHz signal analyzer and special test fixture to collect switching delay, insertion loss and dual-channel isolation. The requirements are that the total module switching response time is ≤1ms, the switching loss increment is ≤0.2dB, the dual-channel optical path isolation is ≥60dB, no optical signal interruption occurs during the switching process, and the bit error rate is <10 -6 .

[0060] Subsequently, an electromagnetic interference test is carried out in an EMC anechoic chamber, the test frequency band covers 10~3000MHz, and radio frequency interference with a field strength of 12V / m is applied to verify that there is no crosstalk in communication and the signal is stable under strong interference environment. The high and low temperature cycle test is carried out in a high and low temperature humidity heat test chamber, with a temperature range of -40℃~150℃, for a total of 100 cycles, and a single cycle duration of 120min. The sample needs to be heated and cooled slowly to avoid thermal shock damage to the optical devices, and it is qualified if the optical path and circuit performance do not degrade after the cycles. The durability test uses a million-cycle durability tester to continuously perform 1 million optical path switching operations with a single switching interval of 1s. The requirements are that there is no coupling failure or control logic fault in the whole process, and the machine must be stopped immediately for disassembly and analysis if a fault occurs midway.

[0061] After all tests are completed, complete data shall be recorded, qualified and unqualified products shall be classified and determined. Qualified finished products shall be marked with model, batch and traceability code by laser marking, and then vacuum-packed and put into storage; the test data shall be archived synchronously to realize full-process traceability with one code for one product. The test fixtures shall be calibrated regularly, and the signal analyzer shall be verified every 7 days to ensure test accuracy.

[0062] As shown in Figure 6 , a photon chip packaging and switching module for fiber-wireless dual-mode communication is prepared by the above preparation method, which includes an alumina ceramic substrate 1. A metallized circuit layer 2 and an integrated copper grounding layer 3 are arranged on the alumina ceramic substrate 1. A MEMS optical path switching unit 5, a signal detection unit 7 and a control unit 8 are arranged on the metallized circuit layer 2, and an opto-electric composite interface unit is arranged on one side of the metallized circuit layer 2; The optical / electric composite interface unit is used to connect to external fiber optic wired communication links and 6G wireless photonic radio frequency communication links, respectively, and is also connected to the internal optical path of the photonic chip 4 to realize bidirectional transmission of optical signals, power and control data. The signal detection unit 7 is connected to the optical / electric composite interface unit via optical coupling and electrical coupling, and is used to collect multi-channel quality parameters of the fiber optic channel and the wireless photonic channel in real time. The output of the signal detection unit 7 is electrically connected to the input of the control unit 8, and the signal output of the control unit 8 is electrically connected to the control of the MEMS optical path switching unit 5. MEMS optical path switching unit 5 is connected to the main transmission optical path, fiber optic channel optical path and wireless photonic channel optical path of photonic chip 4 respectively; The control unit 8 has a built-in local signal threshold discrimination program and a reserved high-speed communication interface for bidirectional data interaction with the AI ​​neural network algorithm of the 6G converged communication system. It is used to autonomously output switching drive signals based on real-time channel quality data to control the MEMS optical path switching unit 5 to complete bidirectional switching between fiber optic optical path and wireless photonic optical path. The overall optical path switching response time of the photonic chip packaged switching module is ≤1ms.

[0063] The optical / electric composite interface unit includes an optical fiber coupling interface 10, an RF interface 11, and a BGA pad 12, and is coated with high-temperature resistant epoxy sealant on the outside of the interface.

[0064] The signal detection unit 7 integrates a photodetector, an RF acquisition chip, and a 12-bit ADC analog-to-digital converter module, and is synchronously coupled to the optical / electrical composite interface unit via optical and electrical dual-path coupling. The sampling period of the signal detection unit is ≤200μs, and it is used to synchronously acquire four types of channel quality parameters: optical power, signal-to-noise ratio, RF bit error rate, and channel attenuation.

[0065] Control unit 8 is an MCU control unit with built-in switching threshold logic for optical power, signal-to-noise ratio, and bit error rate. It is equipped with a high-speed serial communication interface for bidirectional interconnection with the AI ​​brain of the 6G system. Control unit 8 supports dual verification of local threshold independent discrimination and AI neural network switching prediction instructions. After the switching is completed, it can transmit link status data back in real time to realize closed-loop iterative optimization of the switching algorithm.

[0066] This invention provides a photonic chip package switching module for fiber-to-wireless dual-mode communication. It integrates the dual-mode switching function inside the photonic chip package, eliminating the need for external switching hardware, simplifying the overall communication hardware architecture, and reducing manufacturing costs. Relying on AI collaborative intelligent discrimination, it achieves millisecond-level smooth signal switching, ensuring continuous and stable communication for intelligent manufacturing mobile robots and ultra-high-definition mobile video terminals during fiber-to-wireless scenario switching. The standardized interface of the photonic chip package switching module is compatible with existing 6G fiber-to-wireless converged communication equipment, making it highly versatile for industrial application.

[0067] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the exemplary embodiments according to this application. As used herein, the singular form is intended to include the plural form as well, unless the context clearly indicates otherwise. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof.

[0068] It should be noted that the terms "first," "second," etc., used in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in sequences other than those illustrated or described herein.

[0069] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A photonic wafer package switch module for fiber-wireless dual mode communication, characterized by, The alumina ceramic substrate (1) is provided with a metallized circuit layer (2) and an integrated copper ground layer (3); a photonic chip (4), a MEMS optical path switching unit (5), a signal detection unit (7) and a control unit (8) are provided on the metallized circuit layer (2); and an optical / electrical composite interface unit is provided on one side of the metallized circuit layer (2). The optical / electric composite interface unit is used to connect to the external optical fiber wired communication link and the 6G wireless photonic radio frequency communication link, respectively. At the same time, it is connected to the internal optical path of the photonic chip (4) through the optical path (9) to realize the bidirectional transmission of optical signals, power supply and control data. The signal detection unit (7) is connected to the optical / electric composite interface unit through optical coupling and electrical coupling, and is used to collect multi-channel quality parameters of the optical fiber channel and the wireless photonic channel in real time; The output terminal of the signal detection unit (7) is electrically connected to the input terminal of the control unit (8), and the signal output terminal of the control unit (8) is electrically connected to the control terminal of the MEMS optical path switching unit (5). The MEMS optical path switching unit (5) is disposed on the main optical path of the photonic chip (4) and is connected to the main transmission optical path, the optical fiber channel optical path and the wireless photonic channel optical path of the photonic chip (4) respectively. The control unit (8) has a built-in local signal threshold discrimination program and a reserved high-speed communication interface for bidirectional data interaction with the AI ​​neural network algorithm of the 6G converged communication system. It is used to autonomously output switching drive signals based on real-time channel quality data to control the MEMS optical path switching unit (5) to complete the bidirectional switching between the optical fiber path and the wireless photonic optical path.

2. The photonic chip package switch module of claim 1, wherein, An optical isolation structure (6) is provided on the alumina ceramic substrate (1) surrounding the photonic chip (4), and the optical isolation structure (6) surrounds the photonic chip (4); the refractive index of the optical isolation structure (6) is 1.45~1.50, the gap between the photonic chip (4) and the optical isolation structure (6) is 0.1~0.2μm, and the gap deviation is controlled within ±0.02μm.

3. The photonic chip package switch module of claim 1, wherein, The optical / electric composite interface unit includes an optical fiber coupling interface (10), an RF interface (11), and a BGA pad (12), with an epoxy sealant layer at the root of each interface. The fiber optic coupling interface (10) is fixed to one end of the optical path (9), and its optical path is aligned with the photonic wafer (4), with a docking gap ≤0.1μm; The radio frequency interface (11) is a 6G wireless photonic radio frequency integrated sub-interface, which is fixed on the signal detection unit (7); The BGA pads (12) are soldered and fixed to the electrical interconnect pins of the metallized circuit layer (2).

4. The photonic chip package switch module of claim 1, wherein, The signal detection unit (7) integrates a photodetector, a radio frequency acquisition chip and a 12-bit ADC analog-to-digital conversion module, and is synchronously coupled to the optical / electrical composite interface unit through optical and electrical dual-path coupling; the sampling period of the signal detection unit (7) is ≤200μs, and it is used to synchronously acquire four types of channel quality parameters: optical power, signal-to-noise ratio, radio frequency bit error rate and channel attenuation.

5. The photonic chip package switch module of claim 1, wherein, The control unit (8) is an MCU control unit with built-in optical power, signal-to-noise ratio and bit error rate switching threshold logic, and is equipped with a high-speed serial communication interface for bidirectional interconnection with the AI ​​brain of the 6G system; the control unit (8) supports independent local threshold discrimination and dual verification of AI neural network switching prediction instructions, and can transmit link status data back in real time after the switching is completed.

6. The photonic chip package switch module of claim 1, wherein, The MEMS optical path switching unit (5) is a MEMS dual-channel optical switch, which is fixed on the metallized circuit layer (2) by eutectic bonding.

7. The photonic chip package switch module of claim 1, wherein, A copper-nickel alloy electromagnetic shielding layer (13) is provided on the alumina ceramic substrate (1), and the copper-nickel alloy electromagnetic shielding layer (13) covers the photonic wafer (4), MEMS optical path switching unit (5), optical isolation structure (6), signal detection unit (7), control unit (8) and optical path (9). The alumina ceramic substrate (1) is further provided with an epoxy molding layer (14) covering a copper-nickel alloy electromagnetic shielding layer (13). After molding, only the optical / electric composite interface unit and part of the integrated copper grounding layer (3) are exposed.

8. The photonic chip package switch module of claim 7, wherein, The copper-nickel alloy electromagnetic shielding layer (13) is an alloy plating layer of 80% Cu and 20% Ni, with a thickness of 5~10μm, a uniform thickness deviation of no more than ±0.5μm, and a connection resistance of ≤0.05Ω with the grounding pin.

9. A method of fabricating a photonic chip package switch module for fiber- wireless dual-mode communication as claimed in any one of claims 1 to 8, characterized in that, The entire process was completed in a Class 1000 cleanroom and included the following steps: Step 1: Preparation of ceramic packaging substrate and grounding shield layer: Prepare alumina ceramic substrate (1) green blank and sinter to densify it, sputter to form metallized circuit layer (2) and co-fire copper grounding layer and grounding pin to form integrated copper grounding layer without solder interface (3). Step 2: Photonic wafer and MEMS optical path switching unit eutectic coupling assembly: After the photonic wafer (4) and MEMS optical path switching unit (5) are precisely positioned, eutectic bonding is completed through a vacuum eutectic furnace to achieve micron-level optical path coupling; Step 3: Surface mount soldering of signal detection unit and control unit: The signal detection unit (7) and control unit (8) are mounted by SMT and electrically connected by lead-free reflow soldering to build the signal acquisition and intelligent control circuit; Step 4: Optical / Electrical Composite Interface Coupling Integration: Sequentially assemble the BGA pad (12), fiber optic coupling interface (10), and RF interface (11). After completing the coupling calibration of the optical path, RF, and electrical interconnects, apply adhesive to seal and cure. Step 5: Electromagnetic shielding coating and epoxy molding: Electroplating is used to prepare a copper-nickel alloy electromagnetic shielding layer (13), and then an epoxy molding layer (14) is formed by injection molding and cured at high temperature.

10. The method of claim 9, wherein, In step 1, the alumina ceramic substrate (1) green blank is obtained by vacuum sintering at 1600±50℃ for 2h, with a heating and cooling rate not exceeding 5℃ / min; the metallized circuit layer (2) is a Ti transition layer and a high-purity copper layer sputtered sequentially, with a copper layer thickness of 10~15μm and a purity of not less than 99.99%; the integrated copper grounding layer (3) is formed by co-firing at 850℃ for 30min. In step 2, eutectic bonding is carried out in a vacuum eutectic furnace with an oxygen content of less than 10 ppm, the eutectic temperature is 280~300℃, the holding time is 60s, and the welding pressure is 0.5~1MPa; after coupling, the optical path insertion loss increment is ≤0.08dB, and the welding adhesion of the photonic wafer (4) is ≥5N / mm². In step 4, high-temperature resistant epoxy sealant is used for sealing and curing. The curing temperature is 80~100℃, and the heat preservation time is 30~45 minutes. After curing, the module achieves an IP67 dustproof and waterproof rating.