Flexible printed circuit boards and their fabrication methods

By employing a step-by-step etching and lamination process, and utilizing the thermal debonding of the carrier film for automatic debonding, the problems of etching residue and bubble delamination in thick copper + fine-pitch flexible circuit boards have been solved, achieving an efficient and reliable fabrication method.

CN123124223APending Publication Date: 2026-11-17TAISHAN JINGCHENGDA CIRCUIT TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611591073.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2026-10-10
Filing Date
2026-10-14
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies for fabricating thick copper + fine-pitch flexible circuit boards suffer from a pooling effect caused by difficulty in exchanging etching solution at the bottom of the line spacing. This results in copper layer residue at the root of the lines, and the cover film colloid cannot completely fill the deep cavity grooves formed by the thick copper, leading to bubble delamination.

Method used

A thermally descalable carrier film is used to replace the whole board dry film. The process involves step-by-step etching at the same position and stepped face-by-face lamination. The first and second circuit pattern etchings are used to etch a portion of the depth, and the cover film is immediately laminated after each etching. The thermally descalable carrier film automatically descales during high-temperature lamination, which simplifies the process and ensures that the colloid is fully filled.

Benefits of technology

It effectively reduces the risk of copper layer residue and bubble delamination at the root of the circuit, improves etching efficiency and electrical insulation reliability of the product, and reduces production costs and cycle time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124223A_ABST
    Figure CN123124223A_ABST
Patent Text Reader

Abstract

This invention discloses a flexible circuit board and its fabrication method. The fabrication method includes: obtaining a copper foil layer, a thermally adhesive carrier film, a first cover film, and a second cover film; wherein the copper foil layer has a first side and a second side located on opposite sides; attaching the thermally adhesive carrier film to the second side of the copper foil layer, and performing a first circuit pattern etching on the first side of the copper foil layer after attachment; pressing the first cover film onto the first side of the copper foil layer and removing the thermally adhesive carrier film; performing a second circuit pattern etching on the second side of the copper foil layer; wherein the pattern position of the second circuit pattern etching is the same as that of the first circuit pattern etching, and the sum of the etching depths of the two is the total thickness of the copper foil layer; attaching the second cover film to the second side of the copper foil layer and pressing and curing to obtain a flexible circuit board. Based on this, this invention can effectively reduce the root residue problem caused by the pooling effect and reduce the risk of delamination.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of circuit board technology, and in particular to a flexible circuit board and its preparation method. Background Technology

[0002] With the continuous development of the new energy vehicle sector, flexible circuit boards are facing higher performance requirements, among which flexible circuit boards with a combination of thick copper and fine pitch are particularly prominent. On the one hand, to carry large currents, flexible circuit boards need to use thicker copper foil; on the other hand, to meet the needs of high-density wiring, their line width and line spacing are constantly shrinking, and the wiring is becoming more refined.

[0003] The inventors learned that the above-mentioned method for preparing a flexible circuit board with thick copper and fine pitch involves performing a single-sided DES full etching on the exposed copper foil surface of a single-sided substrate to form the circuit, followed by laminating a cover film for protection. This processing method has two major drawbacks: first, during thick copper etching, the etching solution is difficult to exchange at the bottom of the circuit spacing, creating a pooling effect and resulting in copper layer residue at the base of the circuit; second, the cover film colloid is difficult to completely fill the deep cavities formed by the thick copper, resulting in bubble delamination. Summary of the Invention

[0004] The technical problem to be solved by the present invention is to provide a flexible circuit board and its preparation method to solve the problems of copper layer residue and bubble delamination at the root of the circuit.

[0005] In a first aspect, the present invention provides a method for fabricating a flexible circuit board. The fabrication method includes: A copper foil layer, a pyrolytic adhesive carrier film, a first cover film, and a second cover film are obtained; wherein the copper foil layer has a first side and a second side located on opposite sides; The pyrolytic adhesive carrier film is bonded to the second side of the copper foil layer, and after bonding, the first side of the copper foil layer is etched with a circuit pattern for the first time. The first covering film is pressed onto the first side of the copper foil layer, and the pyrolytic adhesive carrier film is removed; A second circuit pattern etching is performed on the second side of the copper foil layer; wherein the pattern position of the second circuit pattern etching is the same as the pattern position of the first circuit pattern etching, and the sum of the etching depths of the two is the total thickness of the copper foil layer; The second cover film is bonded to the second side of the copper foil layer and then pressed and cured to obtain a flexible circuit board.

[0006] In one implementation of the first aspect, the pyrolytic adhesive carrier film includes an adhesive layer and a substrate layer, the adhesive layer being peelably adhered to a second side of the copper foil layer, and the substrate layer being disposed on a side of the adhesive layer away from the copper foil layer.

[0007] In one implementation of the first aspect, pressing the first cover film onto the first side of the copper foil layer and peeling off the pyrolytic adhesive carrier film includes: The first covering film is attached to the first surface and vacuum-pressed under first preset conditions to obtain a product intermediate. The product intermediate is cooled to a preset temperature, and the pyrolytic adhesive carrier film on the product intermediate is removed after cooling to the preset temperature.

[0008] In one implementation of the first aspect, after obtaining the copper foil layer, the pyrolytic adhesive carrier film, the first cover film, and the second cover film, the method includes: processing an alignment reference that penetrates the board surface on the copper foil layer.

[0009] In one implementation of the first aspect, after bonding, a first circuit pattern etching is performed on the first surface of the copper foil layer, including: Obtain a first dry film and attach the first dry film to the first side of the copper foil layer; Based on the alignment reference, the first surface of the first dry film that has been attached is subjected to a first controlled-depth etching.

[0010] In one implementation of the first aspect, a second circuit pattern etching is performed on the second side of the copper foil layer, including: Obtain a second dry film and adhere the second dry film to the second side of the copper foil layer; Based on the alignment reference, a second depth-controlled etching is performed on the second side of the copper foil layer at the same pattern position as the first depth-controlled etching.

[0011] In one implementation of the first aspect, the first etching depth of the first controlled-depth etching is 50% to 70% of the total thickness of the copper foil layer, and the second etching depth of the second controlled-depth etching is 30% to 50% of the total thickness of the copper foil layer.

[0012] In one implementation of the first aspect, the vacuum pressing temperature is 170°C to 190°C, the vacuum pressing pressure is 2.5MPa to 3.5MPa, and the vacuum pressing time is 100s to 150s.

[0013] In one implementation of the first aspect, the second cover film is bonded to the second side of the copper foil layer and then pressed and cured to obtain a flexible circuit board, including: after pressing and curing, performing corresponding post-processing operations to obtain the corresponding flexible circuit board.

[0014] Secondly, the present invention provides a flexible circuit board. The flexible circuit board includes a first cover film, a copper foil layer, and a second cover film stacked sequentially. The copper foil layer has a first surface and a second surface located on opposite sides. A first circuit groove is formed on the first surface of the copper foil layer, and the first circuit groove is filled with a first colloid of the first cover film. A second circuit groove is formed on the second surface of the copper foil layer, and the second circuit groove is located at the same position as the first circuit groove and is connected to it. The second circuit groove is filled with a second colloid of the second cover film.

[0015] The beneficial effects of this invention are as follows: Compared with the conventional process of using a single substrate for full etching in one go, this invention splits the etching task of the copper foil layer into two parts. The first and second circuit pattern etchings each etch only a portion of the depth. By controlling the amount of etching per pass, the flow path of the chemical solution is greatly shortened, the exchange efficiency is significantly improved, and the bottom of the gap can always maintain contact with fresh chemical solution. The copper foil layer can be thoroughly etched clean, thereby effectively reducing the root residue problem caused by the pooling effect.

[0016] Meanwhile, since the depth of the circuit grooves (i.e., the circuit gap depth) created by the first and second circuit pattern etchings is less than the total thickness of the copper foil layer, and much less than the depth of the deep cavity produced by a single full etching, this invention performs the first cover film lamination immediately after the first circuit pattern etching on the first side, and the second cover film lamination immediately after the second circuit pattern etching on the second side, instead of waiting until both the first and second sides are fully etched before lamination. Based on this, the first colloid of the first cover film and the second colloid of the second cover film can flow smoothly and fully fill the shallower circuit gaps, reducing the problem of air bubbles trapped due to poor colloid flow or gas retention during deep cavity filling, thus lowering the risk of delamination. Attached Figure Description

[0017] Figure 1 This is a flowchart of the steps in a method for preparing a flexible circuit board according to an embodiment of the present invention.

[0018] Figure 2 This is a schematic diagram of the structure of a pyrolytic adhesive carrier membrane disclosed in an embodiment of the present invention.

[0019] Figure 3 This is a top view of the corresponding structure in the embodiment of the present invention after the first circuit pattern etching.

[0020] Figure 4 yes Figure 3 A schematic diagram of the AA cross section.

[0021] Figure 5This is a schematic diagram of the structure of the corresponding structure in the embodiment of the present invention after the first cover film is pressed and the pyrolytic adhesive bearing film is removed.

[0022] Figure 6 This is a schematic diagram of the structure of the corresponding structure in the embodiment of the present invention after the second circuit pattern etching.

[0023] Figure 7 This is a schematic diagram of the structure of a flexible circuit board disclosed in an embodiment of the present invention.

[0024] Label Explanation: 1. Copper foil layer; 11. First side; 12. Second side; 13. First circuit groove; 14. Second circuit groove; 2. Thermally disintegrating carrier film; 21. Adhesive layer; 22. Substrate layer; 23. Release layer; 3. First covering film; 31. First colloid; 4. Second covering film; 41. Second colloid; 5. Alignment reference. Detailed Implementation

[0025] To explain in detail the technical content, objectives, and effects of the present invention, the following description is provided in conjunction with the embodiments and accompanying drawings.

[0026] To facilitate understanding of the technical solutions provided in the embodiments of the present invention by those skilled in the art, the relevant technologies are described below: In the field of new energy vehicles, with the continuous iteration of battery management systems, power modules, and wireless charging technologies, higher requirements are being placed on flexible circuit boards, especially in the combination design of "thick copper + fine spacing". Specifically, on the one hand, flexible circuit boards need to carry large currents, requiring copper foil thickness to reach more than 0.05mm; on the other hand, to meet the needs of high-density wiring, the line spacing is compressed to 0.08mm or less.

[0027] The inventors learned that the typical method for fabricating a single-layer thick copper + fine-pitch flexible circuit board involves using a single-sided substrate (i.e., a composite of a copper foil layer and a PI base film layer), performing a single DES (develop-etch-remove) full etching process on the exposed copper foil surface of the single-sided substrate to form the circuitry, followed by laminating a cover film for protection. This fabrication method has two major drawbacks: (1) During thick copper etching, the etching solution has difficulty to exchange at the bottom of the line spacing, forming a pool effect, resulting in copper layer residue at the root of the line. For example, when the copper foil thickness is more than 0.05 mm and the line spacing is compressed to 0.08 mm or less, the etching solution has difficulty to flow and exchange effectively at the bottom of the narrow and deep line gap. Fresh solution cannot be replenished in time and reaction products cannot be discharged in time, forming the so-called pool effect. This results in incomplete etching and residue of copper layer at the root of the line (near the substrate interface), which in turn causes the risk of short circuit between lines.

[0028] (2) The cover film colloid is difficult to completely fill the deep cavity grooves formed by thick copper, resulting in bubble delamination. For example, the line gap depth formed after full etching is more than 0.05mm. When the cover film is laminated later, the colloid has limited fluidity and is subject to surface tension, making it difficult to completely fill the bottom of the deep cavity. The air in the groove is sealed and formed into bubbles. These bubbles expand rapidly when heated during the subsequent SMT high-temperature soldering process, eventually causing the cover film and copper foil interface to delaminate and peel off, which seriously affects the electrical insulation reliability and service life of the product.

[0029] To at least address the aforementioned problems, this invention provides a manufacturing method for flexible circuit boards with thick copper and fine pitch. In this method, a thermally disintegrating carrier film 2 replaces the traditional process of dry film application, step-by-step etching at the same location, stepped facet lamination, and precise alignment using a shared alignment hole group. This results in a three-layer composite product consisting of a first cover film 3, a single-layer copper foil circuit layer, and a second cover film 4. This effectively improves the problems of etching residue and poor filler application of the cover film under thick copper and fine pitch conditions, and solves the problem of complex processes and high quality risks caused by requiring two dry film applications on the second side 12 (i.e., the reverse side) of the copper foil layer 1.

[0030] The technical solutions according to the present invention will be described below with reference to specific embodiments and in conjunction with the accompanying drawings.

[0031] Figure 1 This is a flowchart illustrating the steps of a method for fabricating a flexible circuit board according to an embodiment of the present invention. (Refer to...) Figure 1 The preparation method includes steps 100 to 108.

[0032] Step 100: Obtain copper foil layer 1, pyrolytic adhesive carrier film 2, first cover film 3, and second cover film 4; wherein, the copper foil layer 1 has a first surface 11 and a second surface 12 located on opposite sides; Step 102: The pyrolytic adhesive carrier film 2 is bonded to the second side 12 of the copper foil layer 1, and after bonding, the first side 11 of the copper foil layer 1 is etched with the circuit pattern for the first time. Step 104: Press the first covering film 3 onto the first surface 11 of the copper foil layer 1, and remove the pyrolytic adhesive bearing film 2; Step 106: A second circuit pattern etching is performed on the second surface 12 of the copper foil layer 1; wherein the pattern position of the second circuit pattern etching is the same as the pattern position of the first circuit pattern etching, and the sum of the etching depths of the two is the total thickness of the copper foil layer. Step 108: The second cover film 4 is attached to the second surface 12 of the copper foil layer 1 and pressed and cured to obtain a flexible circuit board.

[0033] As can be seen from the above description, the beneficial effects of the present invention are as follows: Compared with the conventional process of using a single substrate for full etching in one go, the present invention splits the etching task of the copper foil layer 1 into two parts. The first and second circuit pattern etchings each etch only a portion of the depth. By controlling the amount of etching per step, the flow path of the chemical solution is greatly shortened, the exchange efficiency is significantly improved, and the bottom of the gap can always maintain contact with fresh chemical solution. The copper foil layer 1 can be thoroughly etched clean, thereby effectively reducing the root residue problem caused by the pooling effect.

[0034] Meanwhile, since the depth of the circuit grooves (i.e., the circuit gap depth) formed by the first and second circuit pattern etchings is less than the total thickness of the copper foil layer 1, and much less than the depth of the deep cavity produced by a single full etching, this invention performs the first cover film 3 pressing immediately after the first circuit pattern etching is completed on the first surface 11, and the second cover film 4 pressing immediately after the second circuit pattern etching is completed on the second surface 12, instead of waiting until the first surface 11 and the second surface 12 are completely etched before pressing. Based on this, the first colloid 31 of the first cover film 3 and the second colloid 41 of the second cover film 4 can flow smoothly and fully fill the shallower circuit gaps, reducing the problem of air bubbles trapped due to poor flow of adhesive or inability to expel gas during deep cavity filling, and reducing the risk of delamination.

[0035] The following combination Figure 1 The steps in steps 100 to 108, as well as other optional steps, are described in detail.

[0036] Step 100: Obtain copper foil layer 1, pyrolytic adhesive carrier film 2, first cover film 3 and second cover film 4; wherein, the copper foil layer 1 has a first surface 11 and a second surface 12 located on opposite sides.

[0037] The thickness of the copper foil layer 1 can be 0.05mm to 0.10mm. The thermally debonded carrier film 2 has dual functions of support and protection as well as high-temperature automatic debonding. The debonding temperature range of the thermally debonded carrier film 2 is 170℃ to 190℃. The thermally debonded carrier film 2 is used to automatically debond in response to the pressing temperature during the subsequent pressing of the first cover film 3. In practical applications, such as... Figure 2As shown, the pyrolytic adhesive carrier film 2 includes a substrate layer 22, an adhesive layer 21, and a peelable release layer 23 stacked sequentially. The substrate layer 22 can be a 50μm high-temperature resistant, low-shrinkage PET film, the adhesive layer 21 can be a high-temperature resistant acrylic pressure-sensitive adhesive, and the release layer 23 is a PET release film.

[0038] In an optional embodiment, after step 100, that is, after obtaining the copper foil layer 1, the thermal adhesive carrier film 2, the first cover film 3 and the second cover film 4, the following steps are included: processing an alignment reference 5 that penetrates the board surface on the copper foil layer 1.

[0039] In practical applications, such as Figure 3 As shown, the aforementioned alignment reference 5 can be a set of alignment holes machined through the board surface by mechanical drilling. It serves as a shared absolute reference for the subsequent first and second circuit pattern etching (such as the exposure process), and its alignment accuracy can reach within ±10μm. Based on this, by sharing the alignment reference 5, the same set of mechanical alignment holes can be used for both the first and second circuit pattern etching processes, reducing the occurrence of cumulative alignment errors.

[0040] Step 102: The pyrolytic adhesive carrier film 2 is attached to the second side 12 of the copper foil layer 1, and after attachment, the first side 11 of the copper foil layer 1 is etched with a circuit pattern for the first time.

[0041] Specifically, when bonding the aforementioned thermally adhesive carrier film 2, the release layer 23 in the thermally adhesive carrier film 2 can be peeled off, and then the exposed adhesive layer 21 is adhered to the second surface 12 of the copper foil layer 1. It should be noted that after bonding the thermally adhesive carrier film 2 to the second surface 12 of the copper foil layer 1, the adhesive layer 21 is peelably adhered to the second surface 12 of the copper foil layer 1, and the substrate layer 22 is disposed on the side of the adhesive layer 21 away from the copper foil layer 1. After bonding the thermally adhesive carrier film 2 to the second surface 12 of the copper foil layer 1, the first circuit pattern etching can be performed. The specific implementation of the first circuit pattern etching can be as follows.

[0042] In an optional embodiment, step 102, after bonding, performs a first circuit pattern etching on the first surface 11 of the copper foil layer 1, which may include the following steps: obtaining a first dry film and bonding the first dry film to the first surface 11 of the copper foil layer 1; and performing a first controlled-depth etching on the first surface 11 with the first dry film bonded to it based on the alignment reference 5.

[0043] It should be noted that since the corresponding thermally adhesive carrier film 2 is bonded to the second surface 12, the second surface 12 is protected by the thermally adhesive carrier film 2. At this time, by bonding a dry film to the first surface 11 of the copper foil layer 1, the first surface 11 can be etched separately for the first circuit pattern. Specifically, alignment reference 5 (such as alignment hole group) can be used for alignment exposure first, and then the first surface 11 can be etched with controlled depth. The etching depth of this first controlled depth etching can be 50% to 70% of the total thickness of the copper foil layer 1. Based on this first controlled depth etching, such as Figure 4 As shown, corresponding lines and the first line groove 13 can be formed. At the same time, a continuous copper layer of a certain depth will be retained at the bottom of the copper foil layer 1. For example, 30% to 50% of the bottom continuous copper layer can be retained.

[0044] Step 104: Press the first covering film 3 onto the first surface 11 of the copper foil layer 1, and remove the pyrolytic adhesive carrier film 2.

[0045] In an optional embodiment, step 104 involves pressing the first cover film 3 onto the first surface 11 of the copper foil layer 1 and removing the pyrolytic adhesive carrier film 2, including: Step 200: The first covering film 3 is attached to the first surface 11 and vacuum-pressed under the first preset conditions to obtain the product intermediate; wherein, the vacuum pressing temperature is 170℃~190℃, the vacuum pressing pressure is 2.5MPa~3.5MPa, and the vacuum pressing time is 100s~150s. Step 202: Cool the product intermediate to a preset temperature, and after cooling to the preset temperature, remove the pyrolytic adhesive carrier film 2 from the product intermediate.

[0046] It should be noted that at room temperature, the adhesive layer 21 provides fixation and support, and its peel force at room temperature is ≥0.5 N / cm. When the temperature rises above 170℃, exceeding the designed trigger threshold of the adhesive layer 21, the mobility of the adhesive molecular chain segments in the adhesive layer 21 is significantly enhanced, and the glass transition temperature is locally exceeded; the adhesive layer transitions from a highly elastic state to a viscous flow state, with a decrease in modulus and a deterioration in wettability. At this time, if a corresponding peel force is applied, the sliding resistance between molecules within the adhesive layer 21 is greatly reduced under the action of the peel force, the reversibility of the adhesive force decreases, and its surface contact area is sharply reduced, thereby achieving automatic debonding so that it can be easily peeled off from the copper foil layer 1. In practical applications, if the temperature rises to 170℃~190℃, the peel force of the adhesive layer 21 can be reduced to ≤0.05 N / cm, which can ensure that no residual adhesive is transferred to the surface of the copper foil layer 1 after peeling.

[0047] In practical applications, during the vacuum pressing process, such as Figure 5As shown, the first colloid 31 in the first cover film 3 gradually fills the first line groove 13 formed by the first controlled-depth etching. Since 30% to 50% of the continuous copper layer remains at the bottom of the copper foil layer 1, it can block the penetration of the first colloid 31 in the first cover film 3. At the same time, the vacuum pressing process will simultaneously trigger the thermal debonding reaction of the thermally debonding carrier film 2 bonded to the second side 12, causing the thermally debonding carrier film 2 to lose its adhesiveness. Automatic debonding is achieved by utilizing the high temperature of vacuum pressing. That is, the high temperature of vacuum pressing of the first cover film 3 (i.e., 170℃ to 190℃) is exactly the debonding temperature range of the thermally debonding carrier film 2. Based on this, through the above-mentioned vacuum pressing, pressing and debonding can be achieved simultaneously, so that they are completed at the same time without additional processes. Afterwards, the pressed product intermediate is cooled to ≤60℃. The thermal debonding carrier film 2 is automatically debonded by utilizing the high temperature of the pressing. At this time, the thermal debonding carrier film 2 can be easily peeled off. After the thermal debonding carrier film 2 is peeled off, the second side 12 of the copper foil layer 1 is completely exposed without any adhesive residue.

[0048] Based on this, compared to attaching a dry film to the second surface 12, the present invention attaches a thermal debonding carrier film 2 to the second surface 12, which has both support and high-temperature automatic debonding functions. This allows the second surface 12 to be protected by the thermal debonding carrier film 2. Moreover, the debonding action of the thermal debonding carrier film 2 attached to the second surface 12 can be directly triggered by the pressing process, without the need for separate debonding heating, film removal and other processes. The process is greatly simplified, thereby effectively shortening the production cycle and reducing material and labor costs.

[0049] Step 106: A second circuit pattern etching is performed on the second surface 12 of the copper foil layer 1; wherein the pattern position of the second circuit pattern etching is the same as the pattern position of the first circuit pattern etching, and the sum of the etching depths of the two is the total thickness of the copper foil layer.

[0050] In optional embodiments, such as Figure 6 As shown, in step 106, a second circuit pattern etching is performed on the second surface 12 of the copper foil layer 1, including: obtaining a second dry film and attaching the second dry film to the second surface 12 of the copper foil layer 1; and performing a second depth-controlled etching on the second surface 12 of the copper foil layer 1 at the same pattern position as the first depth-controlled etching based on the alignment reference 5.

[0051] Specifically, firstly, since the unadhesive carrier film on the second surface 12 is removed, the copper foil on the second surface 12 of the copper foil layer 1 is completely exposed without any residual adhesive, so there is no need for film removal or other operations. Based on this, the present invention can directly attach the second dry film to the second surface 12. Then, alignment is performed based on the alignment reference 5 (such as the alignment hole group), and a second depth etching is performed at the same pattern position as the first depth etching to remove the copper layer remaining at the bottom of the copper foil layer 1 (such as the bottom 30% to 50% copper layer) to form the corresponding circuit and the second circuit groove 14.

[0052] It should be noted that the sum of the first etching depth of the first controlled-depth etching and the second etching depth of the second controlled-depth etching is the total thickness of the copper foil layer 1. In practical applications, the first etching depth can be 50% to 70% of the total thickness of the copper foil layer 1, and the second etching depth can be 30% to 50% of the total thickness of the copper foil layer 1.

[0053] As described above, by superimposing the first and second controlled depth etching at the same pattern location, the etching task of the total thickness of the copper foil layer 1 is split into two parts. At the same time, the bottom copper layer remaining from the first controlled depth etching can serve as a temporary anti-etch barrier layer for the lines on the first surface 11, preventing the roots of the formed lines on the first surface 11 from being over-etched.

[0054] Step 108: The second cover film 4 is attached to the second surface 12 of the copper foil layer 1 and pressed and cured to obtain a flexible circuit board.

[0055] In an optional embodiment, in step 108, the second cover film 4 is bonded to the second surface 12 of the copper foil layer 1 and then pressed and cured to obtain a flexible circuit board. This includes performing corresponding post-processing operations after pressing and curing to obtain a flexible circuit board. Figure 7 The flexible circuit board shown.

[0056] In practical applications, the above-mentioned post-process operations can be set according to the actual situation, such as immersion gold, electrical testing, and punching.

[0057] Figure 7 This is a schematic diagram of the structure of a flexible circuit board according to an embodiment of the present invention. (Refer to...) Figure 7The flexible circuit board includes a first cover film 3, a copper foil layer 1, and a second cover film 4 stacked sequentially. The copper foil layer 1 has a first surface 11 and a second surface 12 located on opposite sides. The copper foil layer 1 has a first circuit groove 13 on the first surface 11, and the first circuit groove 13 is filled with a first colloid 31 of the first cover film 3. The copper foil layer 1 has a second circuit groove 14 on the second surface 12. The second circuit groove 14 is in the same position as the first circuit groove 13 and is connected to it. The second circuit groove 14 is filled with a second colloid 41 of the second cover film 4.

[0058] It should be noted that the aforementioned first line groove 13 is a groove (such as a half-depth line groove) formed by the first depth etching of the first surface 11 of the copper foil layer 1. After the first depth etching is completed, a continuous copper layer is retained at the bottom of the first line groove 13. Based on this, a second depth etching is performed so that the pattern position of the second depth etching is the same as that of the first depth etching. This allows the "continuous copper layer retained at the bottom of the first line groove 13" to be etched away, thereby forming a second line groove 14 on the second surface 12 of the copper foil layer 1, which is in the same position as the first line groove 13 and is interconnected with it.

[0059] To make this application easier to understand, an exemplary application is provided below. In this exemplary application, a method for fabricating a flexible circuit board with a single-layer thick copper foil and fine-pitch lines is provided, which is particularly suitable for fabricating a flexible circuit board with a single-layer thick copper double-sided cover film structure having a copper foil layer 1 thickness of 0.05mm to 0.10mm and a line spacing of ≤0.08mm.

[0060] Step S1: Substrate preparation and lamination with carrier film First, a roll of copper foil layer 1 is provided as the substrate. The thickness of the copper foil layer 1 is 0.05mm, and the line spacing can be designed to be 0.08mm.

[0061] Next, a corresponding thermally adhesive carrier film 2 is rolled up and laminated on the second side 12 of the copper foil layer 1. The thermally adhesive carrier film 2 has a debonding temperature of 170℃~190℃. After that, it is cut into working boards according to the size.

[0062] It should be noted that the above-mentioned pyrolytic adhesive carrier film 2 is a thermoplastic polyolefin or modified silicone pressure-sensitive adhesive carrier film. At room temperature, the peel force of the pyrolytic adhesive carrier film 2 bonded to the second side 12 of the copper foil layer 1 is ≥0.5N / cm, and the peel force drops to ≤0.05N / cm at 170℃~190℃.

[0063] Step S2: Drilling and establishing alignment reference 5 A set of alignment holes is machined through the copper foil layer 1 on the aforementioned work board, with the diameter of the alignment holes in the set being 1.0 mm.

[0064] Step S3: Apply the first dry film to the first surface 11 of the copper foil layer 1. The first surface 11 of the copper foil layer 1 is chemically cleaned, and after cleaning, a first dry film with a thickness of 25 μm is applied to the first surface 11.

[0065] Step S4: First circuit pattern etching, i.e., first depth etching of the first surface 11. Alignment exposure was performed based on the alignment hole group, followed by DES etching using copper chloride etchant. The etching parameters were: spray pressure 1.8~2.2kg / cm², temperature 50±2℃. The etching depth was controlled at 0.030mm (approximately 60% of the total copper thickness of copper foil layer 1), and the thickness of the remaining copper layer was approximately 0.020mm (approximately 40% of the total copper thickness of copper foil layer 1).

[0066] Step S5: First cover film lamination, i.e., step filling After the first cover film 3 is bonded to the first surface 11, vacuum pressing is performed. The vacuum pressing conditions are: temperature 180℃, pressure 3.0MPa, and time 120s. The adhesive layer thickness of the first cover film 3 is 25μm to 50μm, and can be 30μm. During the pressing process, the adhesive layer of the first cover film 3 is heated and flows, filling the first line groove 13 formed by the first depth etching, while simultaneously expelling air from the groove to avoid air bubble residue.

[0067] Step S6: Remove the pyrolysis adhesive carrier film 2 During the aforementioned vacuum pressing process, the high temperature of the pressing simultaneously triggers the debonding of the thermally adhesive carrier film 2, causing it to lose its adhesiveness. Afterwards, the vacuum-pressed intermediate product is cooled to ≤60℃, and the thermally adhesive carrier film 2 is peeled off, completely exposing the second side 12 of the copper foil layer 1 without any residue. It should be noted that after high-temperature pressing, the adhesiveness of the thermally adhesive carrier film 2 significantly decreases and largely fails. Even when restored to low-temperature conditions (e.g., ≤60℃), its adhesiveness does not recover, remaining largely in a failed state, exhibiting a loss of adhesion.

[0068] Step S7: Apply a second dry film to the second side 12 of copper foil layer 1. Chemical cleaning is performed on the second side 12 of the copper foil layer 1, and a second dry film with a thickness of 25 μm is applied after cleaning.

[0069] Step S8: Second circuit pattern etching (i.e., etching the remaining copper layer on the second side 12). Alignment is performed based on the alignment of the via group, followed by a second controlled-depth etching at the same pattern location as the first via depth etching, thereby removing the residual copper layer at the bottom. It should be noted that the same etching solution as the first circuit pattern etching is used to remove the residual copper layer at the bottom, and this residual copper layer thickness can be 0.020 mm.

[0070] It should be noted that the sum of the first etching depth of the first controlled depth etching and the second etching depth of the second controlled depth etching is equal to the total thickness of the copper foil layer 1.

[0071] Step S9: Press the second cover film 4 The second cover film 4 is attached to the second side 12 of the copper foil layer 1 and then pressed and cured.

[0072] Step S10: Subsequent Process The corresponding flexible circuit board is obtained through subsequent processes such as nickel plating, electrical testing, and punching.

[0073] The prepared flexible circuit board showed good performance after testing: no delamination or bubbles were observed under 288℃ / 10s floating soldering conditions; the insulation resistance was not less than 10¹²Ω, and the electrical insulation performance was reliable; no copper layer residue was found at the root of the circuit cross-section under a microscope, and the etching effect was good; the alignment deviation was controlled within ±8μm, and the pattern transfer accuracy met the design requirements.

[0074] To further verify the applicability of the present invention under different specifications, single bare copper foils with thicknesses of 0.07 mm and 0.10 mm were used as substrates for testing, with line spacings of 0.10 mm and 0.12 mm, respectively. Specifically, for the 0.07 mm copper foil layer 1, the initial etching depth was 55% of the total copper thickness (0.0385 mm), the residual copper thickness was 45% of the total copper thickness (0.0315 mm), and the first cover film 3 had a thickness of 40 μm. For the 0.10 mm copper foil layer 1, the initial etching depth was 50% of the total copper thickness (0.050 mm), the residual copper thickness was 50% of the total copper thickness (0.050 mm), and the first cover film 3 had a thickness of 50 μm. Other process parameters and steps for both sets of tests were consistent with those in Example 1, and the test results met the requirements. Therefore, the present invention exhibits good process compatibility and reliability under different copper foil layer 1 thicknesses and line spacing conditions.

[0075] It should be noted that, to facilitate differentiation of the corresponding structures in the accompanying drawings, some structures in some figures are distinguished by color. For example, the blue-filled portion refers to the first colloid 31 of the first cover film 3, the cyan-filled portion refers to the second colloid 41 of the second cover film 4, and the black-filled portion refers to the copper foil layer 1. Furthermore, Figure 3 The diagonal line filling part is the first line groove 13.

[0076] In summary, according to the flexible circuit board and its preparation method of the present invention: (1) The present invention uses a single copper foil layer 1 as the starting material, and the second side 12 uses a thermally debonded carrier film 2 to replace the whole board protective dry film. The automatic debonding of the thermally debonded carrier film 2 is triggered by the high temperature of the first cover film 3. Compared with the operation of "first dry film application → dry film removal → chemical cleaning → second dry film application" on the second side 12, the present invention reduces the number of dry film applications on the second side 12 from two to one. At the same time, the shared alignment hole group ensures that the two pattern positions are completely overlapped, realizing high-quality and high-efficiency manufacturing of single-layer thick copper fine-pitch circuits. (2) Compared with the operation of applying a dry film to protect the second side 12 during the first depth control etching process, the present invention can realize the high-temperature synchronous automatic debonding of the thermally debonded carrier film 2 during the pressing of the first cover film 3 by applying the thermally debonded carrier film 2 to the second side 12, without the need for a special film removal process. Moreover, there is a cumulative error in the re-alignment of the secondary film. The present invention uses a common alignment hole group to ensure that the patterns are completely overlapped. That is, the common alignment hole ensures that the positions of the two patterns are completely overlapped, with a deviation of ≤±10μm and a side etching amount of ≤5μm, which significantly improves the quality. (3) The thermally debonded carrier film 2 leaves no residue after debonding, avoiding copper surface contamination caused by incomplete film removal. At the same time, there is no need for secondary film application, avoiding the risk of bubbles and wrinkles caused by secondary film application.

[0077] It should be understood that the terms "first," "second," etc., are used in this invention to describe various types of information, but these terms are not limited to them and are only used to distinguish information of the same type from each other. For example, without departing from the scope of this invention, "first" information can also be referred to as "second" information, and similarly, "second" information can also be referred to as "first" information.

[0078] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent modifications made based on the content of the present invention specification and drawings, or direct or indirect applications in related technical fields, are similarly included within the patent protection scope of the present invention.

Claims

1. A method for fabricating a flexible circuit board, characterized in that, include: A copper foil layer, a pyrolytic adhesive carrier film, a first cover film, and a second cover film are obtained; wherein the copper foil layer has a first side and a second side located on opposite sides; The pyrolytic adhesive carrier film is bonded to the second side of the copper foil layer, and after bonding, the first side of the copper foil layer is etched with a circuit pattern for the first time. The first covering film is pressed onto the first side of the copper foil layer, and the pyrolytic adhesive carrier film is removed; A second circuit pattern etching is performed on the second side of the copper foil layer; wherein the pattern position of the second circuit pattern etching is the same as the pattern position of the first circuit pattern etching, and the sum of the etching depths of the two is the total thickness of the copper foil layer; The second cover film is bonded to the second side of the copper foil layer and then pressed and cured to obtain a flexible circuit board.

2. The preparation method according to claim 1, characterized in that, The pyrolytic adhesive carrier film includes an adhesive layer and a substrate layer. The adhesive layer is peelably adhered to the second side of the copper foil layer, and the substrate layer is disposed on the side of the adhesive layer away from the copper foil layer.

3. The preparation method according to claim 1, characterized in that, Pressing the first cover film onto the first side of the copper foil layer and peeling off the pyrolytic adhesive carrier film includes: The first covering film is attached to the first surface and vacuum-pressed under first preset conditions to obtain a product intermediate. The product intermediate is cooled to a preset temperature, and the pyrolytic adhesive carrier film on the product intermediate is removed after cooling to the preset temperature.

4. The preparation method according to claim 1, characterized in that, After obtaining the copper foil layer, the pyrolytic adhesive carrier film, the first cover film, and the second cover film, the process includes: processing an alignment reference that penetrates the board surface on the copper foil layer.

5. The preparation method according to claim 4, characterized in that, After bonding, the first surface of the copper foil layer is etched with the circuit pattern for the first time, including: Obtain a first dry film and attach the first dry film to the first side of the copper foil layer; Based on the alignment reference, the first surface of the first dry film that has been attached is subjected to a first controlled-depth etching.

6. The preparation method according to claim 5, characterized in that, A second circuit pattern etching is performed on the second side of the copper foil layer, including: Obtain a second dry film and adhere the second dry film to the second side of the copper foil layer; Based on the alignment reference, a second depth-controlled etching is performed on the second side of the copper foil layer at the same pattern position as the first depth-controlled etching.

7. The preparation method according to claim 6, characterized in that, The first etching depth of the first controlled-depth etching is 50% to 70% of the total thickness of the copper foil layer, and the second etching depth of the second controlled-depth etching is 30% to 50% of the total thickness of the copper foil layer.

8. The preparation method according to claim 3, characterized in that, The vacuum pressing temperature is 170℃~190℃, the vacuum pressing pressure is 2.5MPa~3.5MPa, and the vacuum pressing time is 100s~150s.

9. The preparation method according to claim 1, characterized in that, The process of bonding the second cover film to the second side of the copper foil layer and then pressing and curing it to obtain a flexible circuit board includes: performing corresponding post-processing operations after pressing and curing to obtain the corresponding flexible circuit board.

10. A flexible circuit board, characterized in that, The device includes a first cover film, a copper foil layer, and a second cover film stacked sequentially. The copper foil layer has a first side and a second side located on opposite sides. The copper foil layer has a first line groove on the first side, which is filled with a first colloid of the first cover film. The copper foil layer has a second line groove on the second side, which is located at the same position as the first line groove and is connected to it. The second line groove is filled with a second colloid of the second cover film.