SiGe HBT Device with Improved Current Gain and its Fabrication Method
By combining low-temperature heavy doping epitaxy and high-temperature secondary heavy doping epitaxy, the doping concentration distribution of the emitter thin film of SiGe HBT device was optimized, solving the problem of excessively slow doping gradient and achieving a significant improvement in high-frequency performance and current gain of the device.
Patent Information
- Application Number
- CN202611417712.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-14
- Publication Date
- 2026-11-17
AI Technical Summary
The doping concentration gradient at the emitter-base interface of existing SiGe HBT devices is too gentle, which leads to a decrease in emitter injection efficiency and limits further improvement of device characteristic frequency fT and current gain β.
A two-step method combining low-temperature heavy doping epitaxy and high-temperature secondary heavy doping epitaxy is adopted. By forming a high-doped emitter film at low temperature and performing thermal redistribution at high temperature, the longitudinal distribution profile of doping concentration is optimized. At the same time, rapid thermal annealing is combined to activate the doping elements.
It significantly improves the current gain β and characteristic frequency fT of SiGe HBT devices, achieving a characteristic frequency of over 260 GHz and a current gain of over 1000, while balancing high doping concentration and excellent crystal quality, making it suitable for the mass production of high-end analog integrated circuits.
Smart Images

Figure CN123124374A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor device manufacturing technology, specifically relating to a SiGe HBT device with improved current gain and its fabrication method. Background Technology
[0002] High-end, specialized analog circuit devices are fabricated using high-speed, advanced SiGe heterojunction bipolar transistor (SiGe HBT) technology with characteristic frequencies of 200 GHz and above. The characteristic frequency of SiGe HBT devices... f T Current amplification factor β The current gain is closely related to the performance of its emitter layer. In-situ heavy doping can significantly reduce the thermal load of emitter layer fabrication and subsequent processes, improving product yield and overall process stability. Currently, advanced in-situ heavy arsenic (As) emitter doping processes can produce highly doped, low-resistivity emitter single-crystal silicon, which has been widely applied in advanced SiGe BiCMOS processes.
[0003] However, existing in-situ heavily doped epitaxial processes for fabricating emitter thin films suffer from problems such as insufficient steepness of the doped atom profile, wide interface transition regions, and difficulty in balancing excessively high doping concentration with crystal quality. In particular, when the doping concentration gradient at the emitter-base interface is too gentle, it leads to a decrease in emitter implantation efficiency, directly limiting device performance. f T and β Further improvements in key electrical performance. Optimizing the longitudinal distribution profile of dopant atoms in the emitter film while maintaining a high doping concentration has become a key technical challenge for further enhancing the high-frequency performance of SiGe HBTs. Summary of the Invention
[0004] To address the shortcomings of the prior art, the technical problem to be solved by the present invention is to provide a SiGe HBT device with improved current gain and a method for fabricating the same.
[0005] To solve the above-mentioned technical problems, the present invention provides the following technical solution: A method for fabricating a SiGe HBT device with improved current gain includes the following steps: S100, Provide a first SEG front structure with a base region window; S200: An HBT base region and an EB junction isolation medium are formed in the base region window of the first SEG front structure to obtain the second SEG front structure; S300, In-situ low-temperature heavy doping epitaxy and in-situ high-temperature secondary heavy doping epitaxy are sequentially performed on the second SEG front structure to form an emitter thin film and obtain a first sample; wherein, the epitaxy temperature of the in-situ low-temperature heavy doping epitaxy is lower than the epitaxy temperature of the in-situ high-temperature secondary heavy doping epitaxy. S400. Perform rapid thermal annealing on the first sample to obtain the second sample; S500: The second sample is metallized to obtain the SiGe HBT device.
[0006] Furthermore, the first SEG front structure includes a substrate and a Si collector epitaxial layer, a TEOS layer and a polysilicon outer base region sequentially stacked on the substrate. A first window is formed in the TEOS layer, and a second window is formed above the first window in the polysilicon outer base region. The second window is connected to the first window, and the first window and the second window together constitute the base region window.
[0007] Furthermore, step S100 includes the following sub-steps: S110, Select a first SEG pre-structure; S120. Perform standard RCA cleaning on the first SEG pre-structure; S130. The first SEG pre-structure, after being cleaned by standard RCA, is placed in the reaction chamber for in-situ surface pretreatment.
[0008] Furthermore, step S200 includes the following sub-steps: S210. Selectively epitaxially extend a base region thin film in the base region window of the first SEG front structure to form the HBT base region; S220. The EB junction isolation medium is deposited on the upper surface of the first SEG front structure and on the sidewall of the base region window.
[0009] Furthermore, the base region thin film is a single-crystal SiGe thin film; and / or The EB junction isolation medium has a three-layer composite structure consisting of a silicon nitride layer, a silicon oxide layer, and a silicon nitride layer stacked sequentially.
[0010] Furthermore, in step S400, the temperature of the rapid thermal annealing process is 950–1000°C, and the annealing time is 5–15 seconds.
[0011] Furthermore, both the in-situ low-temperature heavily doped epitaxy and the in-situ high-temperature sub-heavy doped epitaxy use arsenic as the dopant, and the dopant flow rate of the in-situ low-temperature heavily doped epitaxy is greater than that of the in-situ high-temperature sub-heavy doped epitaxy.
[0012] Furthermore, the process conditions for the in-situ low-temperature heavy doping epitaxy include: using dichlorosilane as the silicon source precursor, using a mixture of arsine and hydrogen as the doping gas, a reaction pressure of 100 Torr to 120 Torr, and an epitaxial temperature of 630°C to 680°C. The process conditions for the in-situ high-temperature secondary heavy doping epitaxy include: using dichlorosilane as the silicon source precursor, using a mixture of arsine and hydrogen as the doping gas, a reaction pressure of 120 Torr to 150 Torr, and an epitaxial temperature of 800℃ to 900℃.
[0013] Furthermore, the thickness of the thin film formed by the in-situ low-temperature heavy doping epitaxy is 30% to 40% of the total thickness of the emitter thin film, and the thickness of the thin film formed by the in-situ high-temperature secondary heavy doping epitaxy is 60% to 70% of the total thickness of the emitter thin film, and the sum of the thicknesses of the two is the total thickness of the emitter thin film.
[0014] A SiGe HBT device with improved current gain is fabricated using any of the above-described methods for fabricating a SiGe HBT device with improved current gain.
[0015] In this invention, an emitter thin film is fabricated using a two-step epitaxial process combining in-situ low-temperature heavy doping epitaxy and in-situ high-temperature secondary heavy doping epitaxy. In the low-temperature stage, taking advantage of the ease of arsenic atom incorporation and limited diffusion at low temperatures, a first-level doped As-Si film with a high doping concentration is formed at the interface between the emitter and base regions, ensuring the interface doping concentration. In the high-temperature stage, the dopant flow rate is reduced and the epitaxial temperature is increased, allowing for the continued epitaxy of a second-level doped As-Si film on the surface of the first-level doped As-Si film and the EB junction isolation dielectric to form a second-level doped As-Si film. During this process, arsenic atoms undergo thermal redistribution within the two films, resulting in a steeper longitudinal distribution profile of the overall emitter film doping concentration. Simultaneously, the higher epitaxial temperature helps improve crystal quality. This effectively solves the problem of decreased implantation efficiency caused by an excessively gentle emitter doping gradient. After rapid thermal annealing, the device characteristic frequency... f T With current gain β Significant improvements. The process flow of this invention is simple and cost-controllable, making it suitable for large-scale production on advanced SiGe BiCMOS process platforms. Attached Figure Description
[0016] The accompanying drawings, which are included to provide a further understanding of this application and form part of this application, illustrate exemplary embodiments and are used to explain this application, but do not constitute an undue limitation of this application. In the drawings: Figure 1 This is a flowchart of an embodiment of the method for fabricating a SiGe HBT device to improve current gain according to the present invention.
[0017] Figure 2 This is a schematic diagram of the first SEG pre-structure.
[0018] Figure 3 This is a schematic diagram of the structure after the HBT base region is formed on the first SEG pre-structure.
[0019] Figure 4 This is a schematic diagram of the second SEG pre-structure.
[0020] Figure 5 This is a schematic diagram of the structure of the first sample.
[0021] Figure 6 This is a superimposed comparison of the longitudinal distribution profiles (SIMS) of As doping using three processes: low-temperature in-situ heavy doping one-step epitaxy, in-situ high-temperature secondary heavy doping one-step epitaxy, and low-high-temperature two-step in-situ epitaxy in this embodiment.
[0022] Figure 7 The graph shows a comparison of the measured current gain β curves of the devices corresponding to the three processes mentioned above.
[0023] The diagrams in the instruction manual are labeled as follows: First SEG front structure 100; substrate 110; Si collector epitaxial layer 120; TEOS layer 130; polysilicon outer base region 140; base region window 150; first window 151; second window 152; second SEG front structure 200; HBT base region 210; EB junction isolation dielectric 220; first sample 300; emitter thin film 310; first heavily doped As-Si thin film 311; second heavily doped As-Si thin film 312. Detailed Implementation
[0024] The following specific examples illustrate the implementation of the present invention. The illustrations provided in the following embodiments are only schematic representations of the basic concept of the present invention. Unless otherwise specified, the following embodiments and features can be combined with each other.
[0025] As semiconductor processes advance towards refinement and high performance, the advanced technology of in-situ heavy doping of emitters with arsenic (As) has gradually replaced the traditional phosphorus doping process and has been widely adopted in the manufacturing of high-end SiGe chips. This process uses As as the heavy doping element. As has high activation efficiency and high carrier concentration in silicon materials, enabling the fabrication of heavily doped, low-resistivity emitter single-crystal silicon, effectively improving the characteristic frequency of SiGe HBT devices. f T With its current driving capability, it meets the high-performance requirements of advanced SiGeBiCMOS manufacturing processes, providing technical support for the research and development and production of high-end SiGe chips.
[0026] However, controlling the longitudinal distribution of doped atoms in emitter films faces a series of fundamental challenges, the most significant of which include: First, the vertical distribution profile of doped atoms in the emitter film is not steep enough, and the doping concentration gradient at the emitter-base interface is too gentle, leading to a decrease in emitter implantation efficiency, which directly restricts the efficiency of the emitter. f T and β Further improvements.
[0027] Second, the wide interface transition region blurs the boundary of the effective doped region of the emitter, increasing the uncertainty of carrier transport.
[0028] Third, there is an inherent contradiction between high doping concentration and good crystal quality. While high-temperature epitaxy improves crystal integrity, it exacerbates the thermal diffusion of As atoms, worsening the profile steepness. Conversely, while low-temperature epitaxy suppresses diffusion and increases the doping ability of As atoms, it may introduce crystal defects such as point defects or dislocations, reducing the HBT's (high-temperature bipolar) performance. f T and β The upper limit of performance also affects the reliability and consistency of the device.
[0029] The aforementioned problems are interconnected and coupled with each other, severely limiting the optimization space of the current gain performance of SiGe HBT devices under high-frequency conditions. They have become key scientific problems and technical bottlenecks that urgently need to be solved in the process of developing advanced SiGe BiCMOS processes towards higher performance.
[0030] Please see Figure 1 , Figure 1 This is a flowchart illustrating an embodiment of the method for fabricating a SiGe HBT device with improved current gain according to the present invention. The method for fabricating a SiGe HBT device with improved current gain in this embodiment includes the following steps: S100. Provide a first SEG (Selective Epitaxial Growth) pre-structure 100 with a base region window 150. The first SEG pre-structure 100 is the basic carrier for the entire HBT device fabrication, and its surface cleanliness directly affects the fabrication quality of subsequent structures such as the HBT base region 210 and emitter film 310. The base region window 150 is the growth region of the HBT base region 210. To ensure that the first SEG pre-structure 100 meets the requirements of subsequent processes, this step may specifically include the following sub-steps: S110, please refer to Figure 2A first SEG pre-structure 100 is selected. Specifically, the first SEG pre-structure 100 includes a substrate 110 and a Si collector epitaxial layer 120, a TEOS (tetraethyl orthosilicate) layer 130, and a polycrystalline silicon outer base region 140 sequentially stacked on the substrate 110. The substrate 110 serves as the supporting foundation for the entire device and is preferably a high-purity single-crystal silicon substrate to ensure the structural stability of the device. The Si collector epitaxial layer 120 is used to subsequently form the collector of the HBT device, providing a carrier collection channel. The TEOS layer 130 is a silicon dioxide layer deposited using tetraethyl orthosilicate, used to achieve electrical isolation between the Si collector epitaxial layer 120 and the polycrystalline silicon outer base region 140, preventing leakage between them. A first window 151 is formed on the TEOS layer 130 through photolithography and etching processes. A second window 152 is formed on the polysilicon outer base region 140 at the position corresponding to the first window 151 through photolithography and etching processes. The first window 151 and the second window 152 are connected and together constitute the base region window 150, providing an accurate growth area for the subsequent selective epitaxial growth of the HBT base region 210.
[0031] S120. Perform standard RCA cleaning on the first SEG pre-structure 100. Since organic matter, metal ions, particulate impurities, and other contaminants adhere to the surface of the first SEG pre-structure 100 during fabrication, these contaminants can affect the epitaxial quality of the subsequent HBT base region 210. Therefore, a standard RCA cleaning process is required to thoroughly clean the first SEG pre-structure 100. RCA cleaning is a standard semiconductor wafer cleaning method proposed by RCA Corporation in the United States. It mainly removes organic matter, metal ions, and particulate impurities from the surface of the first SEG pre-structure 100 through a multi-step chemical cleaning process. After cleaning, it is rinsed thoroughly with high-purity deionized water and dried to ensure the interface quality of subsequent processes. This cleaning method is a conventional and mature technology in the semiconductor field, and its specific cleaning parameters and operating procedures are not detailed here.
[0032] S130. The first SEG pre-structure 100, after standard RCA cleaning, is placed in the reaction chamber for in-situ surface pretreatment. After standard RCA cleaning, although most contaminants have been removed from the surface of the first SEG pre-structure 100, residual native oxide layers and interface defects may still exist, affecting the bonding force between the subsequent HBT base region 210 and the first SEG pre-structure 100, as well as the crystal quality of the epitaxial layer. Therefore, in-situ surface pretreatment is required; for example, SICONI (Silicon Carbon Nitride Interface) can be used. This process is a conventional pretreatment process used in semiconductor device fabrication to optimize interface performance. By introducing a specific reactive gas into the reaction chamber, a thin and uniform silicon carbon nitride interface layer is formed on the surface of the first SEG pre-structure 100, thereby repairing interface defects, improving interface flatness, and enhancing the bonding force between the subsequent epitaxial layer and the substrate, laying a good foundation for the selective epitaxial growth of the HBT base region 210. The specific process and parameters are conventional techniques well known to those skilled in the art and will not be elaborated here.
[0033] S200: An HBT base region 210 and an EB (emitter-base) junction isolation dielectric 220 are formed in the base region window 150 of the first SEG pre-structure 100 to obtain the second SEG pre-structure 200. This step is a key step in the formation of the main structure of the HBT device. The HBT base region 210, as an important region for carrier transport in the device, directly affects the current gain and high-frequency performance of the device due to its crystal quality and thickness uniformity. The EB junction isolation dielectric 220 is used to achieve electrical isolation between the HBT base region 210 and the subsequent emitter film 310, avoiding leakage between them and ensuring the electrical stability of the device. To ensure the fabrication quality of the HBT base region 210 and the EB junction isolation dielectric 220, this step may specifically include the following sub-steps: S210, please refer to Figure 3 In the base region window 150 (specifically the first window 151) of the first SEG front structure 100, an HBT base region 210 is formed by selectively epitaxially growing a base region thin film. The selective epitaxy process can precisely control the growth area of the base region thin film, ensuring the positional accuracy and structural integrity of the HBT base region 210. In this embodiment, the base region thin film is a single-crystal SiGe thin film. SiGe material has excellent heterojunction characteristics, and compared with traditional Si-based base regions, it can effectively improve the current gain and cutoff frequency of the HBT device, meeting the high-performance requirements of the HBT device.
[0034] S220, please refer to Figure 4An EB junction isolation dielectric 220 is deposited on the upper surface of the first SEG front structure 100 (i.e., the surface of the polysilicon outer base region 140) and the sidewall of the base region window 150 (i.e., the sidewall of the second window 152). The deposition process can employ chemical vapor deposition (CVD) to ensure that the EB junction isolation dielectric 220 has uniform coverage and consistent thickness, thereby effectively forming isolation and avoiding electrical short circuits or leakage. In this embodiment, the structure of the EB junction isolation dielectric 220 is a three-layer composite structure consisting of a silicon nitride layer, a silicon oxide layer, and a silicon nitride layer stacked sequentially, namely: a SIN / OX / SIN three-layer composite structure. The SIN (silicon nitride) layer has good insulation performance and the ability to block impurity diffusion, while the OX (silicon dioxide) layer serves as an intermediate buffer layer, which can enhance the bonding force of the three-layer structure. Compared with a single insulating layer, the three-layer composite structure has better insulation performance and structural stability, and can better guarantee the electrical performance and long-term reliability of the HBT device.
[0035] S300, please refer to Figure 5 In-situ low-temperature heavy doping epitaxy and in-situ high-temperature secondary heavy doping epitaxy are sequentially performed on the second SEG front structure 200 to form an emitter thin film 310, resulting in a first sample 300. The in-situ epitaxy refers to a continuous epitaxial growth process performed within the reaction chamber without removing the sample; the epitaxial temperature of the in-situ low-temperature heavy doping epitaxy is lower than the epitaxial temperature of the in-situ high-temperature secondary heavy doping epitaxy. Secondary heavy doping refers to the doping concentration of the second heavily doped As-Si thin film 312 being lower than the doping concentration of the first heavily doped As-Si thin film 311.
[0036] The emitter film 310 is used to inject carriers into the HBT base region 210. Its doping concentration distribution and crystal quality affect the switching speed and current driving capability of the device. The emitter fabricated by in-situ low-temperature heavy doping epitaxy and in-situ high-temperature secondary heavy doping epitaxy can take into account the maintenance of the EB junction doping concentration in the emitter film 310, the optimization of the emitter doping profile, and the fabrication of a high crystal quality emitter film 310.
[0037] In this embodiment, both the in-situ low-temperature heavily doped epitaxy and the in-situ high-temperature sub-heavily doped epitaxy use arsenic as the dopant, and the dopant flux of the in-situ low-temperature heavily doped epitaxy is greater than that of the in-situ high-temperature sub-heavily doped epitaxy. The emitter film 310 is a heavily doped As-Si film. Using As as the heavily doping element can effectively increase the carrier concentration of the emitter film 310 and reduce the emitter resistivity. The total thickness of the emitter film 310 can be approximately 100 nm. This thickness balances the electrical performance of the emitter and the integration density of the device, avoiding an increase in device size due to excessive thickness or a decrease in carrier transport efficiency due to excessive thinness.
[0038] The emitter film 310 may specifically include a first heavily doped As-Si film 311 formed on the surface of the HBT base region 210, and a second heavily doped As-Si film 312 covering the first heavily doped As-Si film 311 and the surface of the EB junction isolation medium 220.
[0039] The principle of this step is as follows: First, at a lower epitaxial temperature and with a larger dopant flow rate, a first heavily doped As-Si film 311 is epitaxially formed on the single-crystal SiGe surface of the HBT base region 210. Taking advantage of the characteristic that N-type doping is easy to incorporate into the film at low temperatures, the doping content of As at the initial EB junction interface is increased to meet the carrier injection requirements of HBT for high doped ion concentration at the EB junction interface and high gain electrical characteristics of the device. Then, the epitaxial temperature is increased and the AsH3 flow rate is reduced to continue to rapidly deposit a second heavily doped As-Si film 312 on the first heavily doped As-Si film 311 and the surface of the EB junction isolation medium 220. During this process, the high temperature will cause the As atoms in the first heavily doped As-Si film 311 and the second heavily doped As-Si film 312 to undergo thermal redistribution, making the longitudinal distribution profile of the doping concentration of the emitter film 310 tend to be steeper.
[0040] The doping gas is 1% AsH3 mixed with H2 gas, the epitaxial pressure is 100 Torr to 120 Torr, the temperature is stable at 630℃ to 680℃, and the epitaxial thickness is about 30% to 40% of the total thickness of the emitter film.
[0041] In step S300, an in-situ high-temperature secondary heavy doping epitaxial process forms a second heavily doped As-Si thin film 312. This is achieved by epitaxy on the first heavily doped As-Si thin film 311 using a reduced flow rate of the doping precursor AsH3 and an increased deposition temperature. The Si source precursor gas source remains DCS (SiH2Cl2), and the doping gas is a mixture of 1% AsH3 and H2. The epitaxial pressure is 120 Torr to 150 Torr, and the temperature is stabilized at 800℃ to 900℃, approximately 60%-70% of the total thickness of the emitter film.
[0042] In this step, the process parameters are strictly controlled during epitaxy: the epitaxial pressure of the first-doped As-Si film 311 is 100 Torr to 120 Torr, the temperature is stabilized at 630℃ to 680℃, and the AsH3 flow rate is 400 sccm to 500 sccm. For example, the epitaxial pressure can be approximately 100 Torr, 105 Torr, 110 Torr, 115 Torr, 120 Torr, etc., and the temperature can be stabilized at approximately 630℃, 640℃, 650℃, 660℃, 670℃, 680℃, etc. The epitaxial pressure of the second-doped As-Si film 312 is 120 Torr to 150 Torr, the temperature is stabilized at 800℃ to 900℃, and the AsH3 flow rate is 150 sccm to 200 sccm. For example, the pressure of the epitaxial layer can be approximately 120 Torr, 130 Torr, 140 Torr, 150 Torr, etc., and the temperature can be approximately stable at 800℃, 810℃, 820℃, 830℃, 840℃, 850℃, 860℃, 870℃, 880℃, 890℃, 900℃, etc.
[0043] (1) Low-temperature in-situ heavy doping epitaxy to form the first heavily doped As-Si thin film 311 This step utilizes the characteristic that As atoms are easily incorporated under low temperature conditions to form a first-fold doped As-Si thin film 311 with high As content at the EB junction interface to ensure the implantation efficiency of the emitter. The epitaxial thickness is about 30% to 40% of the total thickness of the emitter film.
[0044] (2) In-situ high-temperature secondary doping epitaxy to form a second-doped As-Si thin film 312 After the formation of the first-doped As-Si thin film 311, the AsH3 flow rate is reduced to 30%–50% of that in the low-temperature step, the epitaxial pressure is increased to 120–150 Torr, and the epitaxial temperature is stabilized at 800–900℃. The resulting film thickness is approximately 60%–70% of the total thickness of the emitter film 310. During the high-temperature epitaxy process, As atoms in the first-doped As-Si thin film 311 and the second-doped As-Si thin film 312 undergo thermal redistribution, forming a steep longitudinal distribution profile of doping concentration. Simultaneously, crystal quality is improved, interface defects are reduced, and the As doping profile and crystal quality of the emitter film 310 are further optimized. The sum of the thicknesses of the first-doped As-Si thin film 311 and the second-doped As-Si thin film 312 is the total thickness of the emitter film 310.
[0045] S400. The first sample 300 is subjected to rapid thermal annealing (RTP) to obtain the second sample. During the epitaxial growth process, the emitter film 310 in the first sample 300 generates a small number of lattice defects, and the doped arsenic element is not fully activated, which may result in the electrical performance of the emitter film 310 not reaching its optimal state. Therefore, the first sample 300 needs to be treated with rapid thermal annealing to fully activate the arsenic element and repair some of the lattice defects. In this embodiment, the temperature of the rapid thermal annealing process is controlled between 950 and 1000°C, for example, the temperature can be controlled at approximately 950°C, 960°C, 970°C, 980°C, 990°C, 1000°C, etc., preferably about 970°C; the annealing time is controlled between 5 and 15 seconds, for example, the annealing time can be controlled at 5 seconds, 6 seconds, 7 seconds, 8 seconds, 9 seconds, 10 seconds, 11 seconds, 12 seconds, 13 seconds, 14 seconds, 15 seconds, etc., preferably about 10 seconds. These process parameters can fully activate the arsenic doping, improve the carrier concentration and conductivity of the emitter film 310, effectively repair lattice defects generated during epitaxy, optimize the crystal quality of the emitter film 310, and avoid excessive diffusion of arsenic due to excessive temperature or time, thus ensuring the junction depth accuracy between the HBT base region 210 and the emitter film 310 and guaranteeing the stability of the device's electrical performance.
[0046] S500: Perform a metallization process compatible with standard CMOS procedures on the second sample to obtain a SiGe HBT device. The purpose of the metallization process is to form metal electrodes on the surface of the second sample, enabling electrical connection between the device and external circuits. To reduce the difficulty and cost of device integration manufacturing and facilitate the integration of HBT devices with other CMOS devices, this step adopts a metallization process compatible with standard CMOS procedures. For example, it may include sub-steps such as metal layer deposition, photolithography, etching, and annealing, thereby ultimately completing the fabrication of the SiGe HBT device. This embodiment is compatible with standard CMOS procedures, has simple process steps, and is easy to implement on advanced SiGe BiCMOS process platforms.
[0047] Please see Figure 6 This is a superimposed comparison of the longitudinal distribution profiles (SIMS) of As doping using three emitter doping processes: low-temperature in-situ heavy doping one-step epitaxy, in-situ high-temperature secondary heavy doping one-step epitaxy, and the low--high-temperature two-step in-situ epitaxy of this embodiment. The horizontal axis represents depth, and the vertical axis represents As atom concentration. Figure 6As can be seen, the peak concentration is highest at the emitter-base interface when using the low-temperature in-situ heavy doping one-step epitaxy method, but the concentration decreases rapidly with increasing depth, and there are more crystal defects. When using the in-situ high-temperature secondary heavy doping one-step epitaxy method, the peak concentration at the interface is lower, and the transition region is significantly widened with the worst steepness. When using the low-high temperature two-step in-situ epitaxy method of this embodiment, a high peak concentration similar to that of the low-temperature in-situ heavy doping one-step epitaxy method is maintained at the interface, while the steepness of the transition region is significantly better than that of the in-situ high-temperature secondary heavy doping one-step epitaxy method, achieving a balance between high concentration and steep profile.
[0048] Please see Figure 7 To improve the device current gain using three emitter doping processes: low-temperature in-situ heavy doping one-step epitaxy, in-situ high-temperature secondary heavy doping one-step epitaxy, and the low--high-temperature two-step in-situ epitaxy of this embodiment. β The measured curves show the base-emitter voltage on the horizontal axis and the voltage on the vertical axis. β Value. From Figure 7 As can be seen from the data, the relative heights of the three curves are: low-temperature in-situ heavy doping one-step epitaxy method. β Medium value, in-situ high-temperature secondary heavy doping one-step epitaxial method β The lowest value is achieved by the low-high temperature two-step in-situ epitaxy method in this embodiment. β The highest value indicates that this embodiment effectively improves the emitter injection efficiency and current gain. However, devices using the low-temperature in-situ heavy doping one-step epitaxial emitter doping process suffer from lattice defects, resulting in limitations at characteristic frequencies. f T The frequency response is less than 200 GHz, which does not meet the frequency characteristics requirements of high-frequency HBT devices.
[0049] This embodiment addresses the technical challenge of balancing insufficient doping profile steepness and crystal quality in in-situ heavily doped emitter processes by creatively proposing a two-step emitter fabrication scheme combining low-temperature heavy doping epitaxy and high-temperature secondary heavy doping epitaxy. By using high-flow-rate AsH3 for heavy doping epitaxy in the low-temperature stage, a sufficiently high As doping concentration at the EB junction interface is ensured, guaranteeing emitter implantation efficiency. Subsequently, the AsH3 flow rate is reduced for secondary heavy doping epitaxy in the high-temperature stage, utilizing the high-temperature thermal redistribution effect to optimize the vertical doping profile of As atoms in the emitter film, significantly narrowing the transition region and greatly improving the steepness. Simultaneously, the high-temperature environment effectively repairs lattice defects introduced by low-temperature epitaxy, achieving a balance between high doping concentration and excellent crystal quality. Combined with subsequent rapid thermal annealing for full activation and profile optimization of doped atoms, this embodiment effectively solves the dual problems of excessively slow doping profile and decreased implantation efficiency in traditional single-step high-temperature processes, and increased crystal defects and limited gain in single-step low-temperature processes. Experimental verification shows that the SiGe HBT device fabricated using this method achieves excellent performance at its characteristic frequency. f TWhile exceeding 260GHz, current gain β It can stably reach over 1000, and its overall performance is significantly better than traditional process solutions. In addition, the process flow of this embodiment is simple, has good compatibility with standard CMOS processes, and is cost-controllable. It is suitable for the mass production of advanced SiGeBiCMOS process platforms and is of great significance for the self-development and domestic substitution of high-end analog integrated circuits.
[0050] This invention also provides a SiGe HBT device with improved current gain, fabricated using the SiGe HBT device fabrication method of any of the above embodiments. The emitter film of this SiGe HBT device has a high doping concentration and a steep longitudinal doping profile at the EB junction interface, with a significantly narrowed interface transition region, effectively improving emitter injection efficiency. Simultaneously, the combined low-temperature and high-temperature epitaxial process ensures good crystal quality of the emitter film, reducing interface defects and leakage current. After rapid thermal annealing activation, the device can operate at its characteristic frequency. f T Achieving current gain while exceeding 260 GHz β It reaches over 1000, possessing both excellent high-frequency characteristics and current amplification capability.
[0051] The above embodiments merely illustrate preferred embodiments of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention should be determined by the appended claims.
Claims
1. A method of fabricating a SiGe HBT device with improved current gain, comprising: Includes the following steps: S100, Provide a first SEG front structure with a base region window; S200: An HBT base region and an EB junction isolation medium are formed in the base region window of the first SEG front structure to obtain the second SEG front structure; S300, In-situ low-temperature heavy doping epitaxy and in-situ high-temperature secondary heavy doping epitaxy are sequentially performed on the second SEG front structure to form an emitter thin film and obtain a first sample; wherein, the epitaxy temperature of the in-situ low-temperature heavy doping epitaxy is lower than the epitaxy temperature of the in-situ high-temperature secondary heavy doping epitaxy. S400. Perform rapid thermal annealing on the first sample to obtain the second sample; S500: The second sample is metallized to obtain the SiGe HBT device.
2. The method of claim 1, wherein the SiGe HBT device is a current gain improved SiGe HBT device. The first SEG front structure includes a substrate and a Si collector epitaxial layer, a TEOS layer and a polysilicon outer base region sequentially stacked on the substrate. A first window is formed in the TEOS layer, and a second window is formed above the first window in the polysilicon outer base region. The second window is connected to the first window, and the first window and the second window together constitute the base region window.
3. The method of claim 1, wherein the SiGe HBT device is fabricated with a current gain of 100 or more. Step S100 includes the following sub-steps: S110, Select a first SEG pre-structure; S120. Perform standard RCA cleaning on the first SEG pre-structure; S130. The first SEG pre-structure, after being cleaned by standard RCA, is placed in the reaction chamber for in-situ surface pretreatment.
4. The method of claim 1, wherein the SiGe HBT device is a current gain improved SiGe HBT device. Step S200 includes the following sub-steps: S210. Selectively epitaxially extend a base region thin film in the base region window of the first SEG front structure to form the HBT base region; S220. The EB junction isolation medium is deposited on the upper surface of the first SEG front structure and on the sidewall of the base region window.
5. The method of fabricating a SiGe HBT device with improved current gain as claimed in claim 4, wherein: The base region thin film is a single-crystal SiGe thin film; and / or The EB junction isolation medium has a three-layer composite structure consisting of a silicon nitride layer, a silicon oxide layer, and a silicon nitride layer stacked sequentially.
6. The method of claim 1, wherein the SiGe HBT device is a current gain improved SiGe HBT device. In step S400, the temperature of the rapid thermal annealing process is 950–1000°C, and the annealing time is 5–15 seconds.
7. The method for fabricating a SiGe HBT device with improved current gain as described in any one of claims 1 to 6, characterized in that: The dopant used in both the in-situ low-temperature heavily doped epitaxy and the in-situ high-temperature sub-heavy doped epitaxy is arsenic, and the dopant flow rate of the in-situ low-temperature heavily doped epitaxy is greater than that of the in-situ high-temperature sub-heavy doped epitaxy.
8. The method for fabricating a SiGe HBT device with improved current gain as described in claim 7, characterized in that: The process conditions for the in-situ low-temperature heavy doping epitaxy include: using dichlorosilane as the silicon source precursor, using a mixture of arsine and hydrogen as the doping gas, a reaction pressure of 100 Torr to 120 Torr, and an epitaxial temperature of 630°C to 680°C. The process conditions for the in-situ high-temperature secondary heavy doping epitaxy include: using dichlorosilane as the silicon source precursor, using a mixture of arsine and hydrogen as the doping gas, a reaction pressure of 120 Torr to 150 Torr, and an epitaxial temperature of 800℃ to 900℃.
9. The method for fabricating a SiGe HBT device with improved current gain as described in claim 8, characterized in that: The thickness of the thin film formed by the in-situ low-temperature heavy doping epitaxy is 30% to 40% of the total thickness of the emitter thin film, and the thickness of the thin film formed by the in-situ high-temperature secondary heavy doping epitaxy is 60% to 70% of the total thickness of the emitter thin film, and the sum of the thicknesses of the two is the total thickness of the emitter thin film.
10. A SiGe HBT device with improved current gain, characterized in that: The SiGe HBT device is fabricated using the method for improving current gain as described in any one of claims 1 to 9.