Methods for forming metal gates and semiconductor devices

By distinguishing between large and small trenches during the metal gate formation process and forming a protective layer on the large trench, the problem of load effect in chemical mechanical polishing of metal gates is solved, thus achieving dimensional stability of metal gates and reliability of device function.

CN123124420APending Publication Date: 2026-11-17SHANGHAI INTEGRATED CIRCUIT EQUIPMENT & MATERIALS INDUSTRY INNOVATION CENTER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510634081.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-16
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing technology, large-size metal gates have a loading effect in the chemical mechanical polishing process, which leads to excessive loss in the longitudinal dimension of the metal gate, affecting the MOSFET function. Moreover, the improvement effect of the existing process is limited, which restricts the design flexibility.

Method used

Before forming the metal gate, large and small trenches are distinguished and a protective layer is formed on the large trench. The metal gate is thinned by chemical mechanical polishing. The protective layer buffers the load effect of the large metal gate area during the polishing process.

Benefits of technology

It reduces the height loss of large-size metal gates, narrows the height difference between large and small-size metal gates, reduces the probability of device failure, and improves design flexibility.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124420A_ABST
    Figure CN123124420A_ABST
Patent Text Reader

Abstract

This invention provides a method for forming a metal gate and a semiconductor device structure. By depositing a protective layer to protect the large-size metal gate area before performing the final chemical mechanical polishing process on the metal gate, the protective layer above the large-size metal gate area acts as a buffer when the gate metal layer is polished by the chemical mechanical polishing process, which can reduce the load effect of the large-size metal gate area, thereby reducing the height loss of the large-size metal gate, reducing the height difference between the large-size metal gate and the small-size metal gate, and reducing the probability of device failure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing technology, and in particular to a method for forming a metal gate and a semiconductor device. Background Technology

[0002] The metal gate (MG) is an indispensable structural layer for forming MOSFETs (Metal-Oxide-Semiconductor Field-Effect Transistors) in the HKMG (High-K Metal Gate) process. During process verification, it was discovered that large-area metal gates with widths greater than 2µm exhibit a significant loading effect during MG CMP (Chemical Mechanical Polishing) processes. This results in the gate height (GH) of the large metal gate being much smaller than that of smaller metal gates (e.g., the minimum design size of 0.027µm) after CMP. This leads to excessive losses in the large metal gate and can even cause losses in the work function layer (WF), ultimately causing MOSFET malfunction.

[0003] Current HKMG process methods include PREB (Photoresist Etching Back), which eliminates differences in photoresist thickness on large and small metal gates. However, PREB's effect on reducing loading effects is limited and cannot prevent the loading effects of subsequent MG CMP processes; the larger the metal gate, the lower the height (GH). Therefore, the current practice is to establish DR (Design Rule) regulations specifying the maximum designable size and maximum placement density of the metal gate to mitigate process risks. However, this also limits the metal gate size and density that can be selected at the design stage, thus restricting more flexible and diverse design and development requirements. Summary of the Invention

[0004] The purpose of this invention is to provide a method for forming a metal gate to solve one or more problems in the prior art.

[0005] To solve the above-mentioned technical problems, the present invention provides a method for forming a metal gate, comprising:

[0006] A substrate is provided, the substrate having a first type of trench and a second type of trench, wherein the width of the first type of trench is greater than or equal to a preset threshold, and the width of the second type of trench is less than the preset threshold;

[0007] A gate metal layer is formed, which fills the first type of trench and the second type of trench;

[0008] A protective layer is formed, which at least covers the gate metal layer filling the first type of trench, while exposing the gate metal layer filling the second type of trench; and,

[0009] A chemical mechanical polishing process is performed to thin the gate metal layer.

[0010] Optionally, in the method for forming the metal gate, before forming the protective layer, the gate metal layer fills the first type of trench and the second type of trench, and also extends to the surface covering the substrate;

[0011] After the protective layer is formed, when the gate metal layer is thinned by performing the chemical mechanical polishing process, the gate metal layer is thinned to remain only in the first type of trench and the second type of trench.

[0012] Optionally, in the method for forming the metal gate, before forming the protective layer, the gate metal layer is filled only in the first type of trench and the second type of trench.

[0013] Optionally, in the method for forming the metal gate, the method for forming the protective layer includes:

[0014] An initial protective layer is deposited, the initial protective layer covering the gate metal layer and the exposed surface of the substrate; and,

[0015] The region of the initial protective layer above the first type of trench is defined as the region where the photomask is not exposed, while the region of the initial protective layer above the second type of trench is defined as the region where the photomask is exposed. A photolithography process is then performed to etch the initial protective layer to obtain the protective layer.

[0016] Optionally, in the method for forming the metal gate, the substrate has a plurality of first-type trenches arranged in an array, and the projection of the non-disclosed area of ​​the photomask onto the substrate covers the array area formed by the plurality of first-type trenches.

[0017] Optionally, in the method for forming the metal gate, the first type of trench is set independently, and the projection of the non-disclosed area of ​​the photomask onto the substrate covers the area where the first type of trench is located.

[0018] Optionally, in the method for forming the metal gate, the protective layer comprises one or more film layers, and the material of each film layer includes one or more of silicon nitride, silicon oxide, and silicon carbonitride.

[0019] Optionally, in the method for forming the metal gate, the preset threshold is greater than or equal to 2 μm.

[0020] Optionally, in the method for forming the metal gate, the material of the gate metal layer includes Al.

[0021] The present invention also provides a semiconductor device structure, wherein the metal gate of the semiconductor device structure is formed by the method described in any of the preceding claims.

[0022] In summary, the method for forming a metal gate and the semiconductor device structure provided by the present invention include: providing a substrate having a first type of trench and a second type of trench, wherein the trench width of the first type of trench is greater than or equal to a preset threshold, and the trench width of the second type of trench is less than the preset threshold; forming a gate metal layer filling the first type of trench and the second type of trench; forming a protective layer at least covering the gate metal layer filling the first type of trench and exposing the gate metal layer filling the second type of trench; and performing a chemical mechanical polishing process to thin the gate metal layer. By depositing a protective layer to protect the large-size metal gate region before performing the final chemical mechanical polishing process to polish the metal gate, the protective layer above the large-size metal gate region acts as a buffer when the gate metal layer is polished by the chemical mechanical polishing process, which can reduce the load effect of the large-size metal gate region, thereby reducing the height loss of the large-size metal gate, reducing the height difference between the large-size metal gate and the small-size metal gate, and reducing the probability of device failure. Attached Figure Description

[0023] Figure 1 A flowchart illustrating a method for forming a metal gate according to an embodiment of the present invention;

[0024] Figures 2-4 This is a schematic diagram of the partial structure of the device corresponding to each step in forming the protective layer in Embodiment 1 of the present invention;

[0025] Figures 5-7 This is a schematic diagram of the device structure corresponding to each step in forming the protective layer in Embodiment 2 of the present invention;

[0026] The labels in the accompanying drawings are explained as follows:

[0027] 11-Substrate; 12-First sidewall; 13-Second sidewall; 14-Dielectric layer; 15-Work function layer; 16-Gate metal layer; 17a-Initial protective layer; 17-Protective layer. Detailed Implementation

[0028] To make the objectives, advantages, and features of this invention clearer, the invention will be described in detail below with reference to the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to facilitate and clearly illustrate the objectives of the embodiments of this invention. Furthermore, the structures shown in the drawings are often part of the actual structures. In particular, different figures may emphasize different aspects and sometimes use different scales. It should also be understood that, unless specifically stated or indicated, the terms "first," "second," "third," etc., in the specification are only used to distinguish the various components, elements, steps, etc., in the specification, and are not used to indicate the logical or sequential relationships between the various components, elements, steps, etc.

[0029] Example 1

[0030] Please see Figure 1 This embodiment provides a method for forming a metal gate, the method comprising the following steps:

[0031] S1, providing a substrate, the substrate having a first type of trench and a second type of trench, the width of the first type of trench being greater than or equal to a preset threshold, and the width of the second type of trench being less than the preset threshold;

[0032] S2, forming a gate metal layer, the gate metal layer filling the first type of trench and the second type of trench;

[0033] S3, forming a protective layer that at least covers the gate metal layer filling the first type of trench and exposes the gate metal layer filling the second type of trench; and,

[0034] S4, Perform a chemical mechanical polishing process to thin the gate metal layer.

[0035] The method provided in this embodiment deposits a protective layer to protect the large-size metal gate area before performing the final chemical mechanical polishing process to polish the metal gate. In this way, when the gate metal layer is polished by the chemical mechanical polishing process, the protective layer above the large-size metal gate area plays a buffering role, which can reduce the load effect of the large-size metal gate area, thereby reducing the height loss of the large-size metal gate, reducing the height difference between the large-size metal gate and the small-size metal gate, and reducing the probability of device failure.

[0036] The following is in conjunction with the appendix Figures 2-4 The method for forming the metal gate provided in this embodiment will be described in further detail.

[0037] First, perform step S1, please refer to [link / reference]. Figure 2A substrate is provided, the substrate having a first type of trench and a second type of trench, wherein the first type of trench is a large-size trench with a width greater than or equal to a preset threshold, and the second type of trench is a small-size trench with a width less than the preset threshold. Accordingly, in subsequent steps, the metal grid filling the first type of trench is a large-size metal grid, and the metal grid filling the second type of trench is a small-size metal grid.

[0038] The preset threshold value can range from 0.1 to 10 μm, preferably from 0.5 to 2 μm. When the width of the large-size trench is greater than or equal to the preset threshold, a height difference between the large-size and small-size metal grids can easily occur after chemical mechanical polishing due to the load effect. In this embodiment, a protective layer is first formed on the metal grids corresponding to trench widths greater than or equal to the preset threshold before chemical mechanical polishing to improve the load effect. Therefore, the height difference between the large-size and small-size metal grids after chemical mechanical polishing can be reduced. In other embodiments, the value of the preset threshold can also be adjusted according to the actual situation. For trenches forming metal grids, they are generally strip trenches, and their width direction is the minimum width direction of the strip trench. Multiple strip trenches are arranged sequentially along a set direction. That is, in common application scenarios, both the first type of trench and the second type of trench are strip trenches, and they are arranged sequentially along a set direction. The first type of trench and the second type of trench have a minimum width in the set direction. Therefore, the width direction of the first type of trench and the second type of trench is consistent with the set direction. In other application scenarios, there may be multiple trenches that are not arranged according to a certain rule or that do not have the same shape, making it difficult to distinguish the size of the trenches by the width in the same direction. In this case, an area threshold can also be used to distinguish whether the trench is a first type of trench or a second type of trench. For example, when the trench area is greater than or equal to 3~30um... 2 When the trench area is less than 3–30 μm, it is considered a Class I trench. 2 If the trench area is greater than or equal to 20 μm, it is considered a second-type trench. Further preferred, if the trench area is greater than or equal to 20 μm... 2 When the trench area is less than 20 μm, it is considered a Class I trench. 2 If so, the trench is considered to be a second type of trench.

[0039] Since the metal gate formation method provided in this embodiment is mainly an improvement made for the region where a large-size metal gate is located, therefore Figure 2 The diagram only shows the large-sized grooves, without illustrating the small-sized grooves. Figure 3 and Figure 4 Similarly, only the large-sized groove portion is shown.

[0040] As an example, the metal gate formation method provided in this embodiment is used to form the gate of a MOSFET (metal-oxide-semiconductor field-effect transistor). The substrate in this embodiment includes a substrate 11, a source / drain region (not shown) formed in the substrate 11, a gate sidewall (including a first sidewall 12 and a second sidewall 13), a dielectric layer 14, a work function layer 15, etc.

[0041] When the metal gate formation method provided in this embodiment is applied to the formation of a MOSFET, the process steps prior to performing steps S1 and S2 may include:

[0042] (1) Preparation of substrate 11;

[0043] (2) Forming pseudo-gates includes forming pseudo-gates corresponding to large-size metal gates and small-size metal gates respectively;

[0044] (3) Deposit a first sidewall material on the sidewall of the pseudo gate, such as Si3N4 or SiO2, and form the first sidewall 12 by etching.

[0045] (4) Forming source and drain regions: Source and drain regions are formed in the substrate 11 on both sides of the dummy gate by ion implantation and annealing processes.

[0046] (5) Deposit a second sidewall material on the outside of the first sidewall 12, such as Si3N4 or SiO2, which is generally different from the material used in the first sidewall 12, and form the second sidewall 13 by etching.

[0047] (6) Remove the dummy gate by selective etching to expose the trench;

[0048] (7) A dielectric layer 14 is deposited at the bottom of the trench, and a work function material layer 15 is deposited at the bottom and sidewalls of the trench for adjusting the threshold voltage.

[0049] The execution order of some steps in steps (1) to (7) above can be adjusted according to the actual situation, and this application does not impose any restrictions on this.

[0050] Next, proceed to step S2. Please continue to see... Figure 2 A gate metal layer 16 is formed. In this embodiment, the gate metal layer 16 fills the first type of trench and the second type of trench, and extends to the surface covering the substrate.

[0051] In this embodiment, the gate metal layer 16 is made of aluminum (Al). In other embodiments, the gate metal layer 16 may also be made of other conductive metal materials, such as copper (Cu).

[0052] Then, proceed to step S3, please refer to [link / reference]. Figure 4A protective layer 17 is formed, which at least covers the gate metal layer 16 filled in the first type of trench, while exposing the gate metal layer 16 filled in the second type of trench.

[0053] The protective layer 17 comprises one or more film layers, and the material of each film layer may be one or more of silicon nitride (Si3N4), silicon oxide (SiO2), and silicon carbonitride (SiCN). This application does not limit the thickness of the protective layer 17; optionally, the thickness of the protective layer 17 may be [missing information]. Preferred options are available

[0054] Please see Figure 3 Optionally, the method for forming the protective layer 17 includes: depositing an initial protective layer 17a, the initial protective layer 17a covering the gate metal layer 16 and the exposed surface of the substrate; defining the region of the initial protective layer 17a above the first type of trench as a photomask-unexposed region, and the region of the initial protective layer 17a above the second type of trench as a photomask-exposed region; and performing a photolithography process to etch the initial protective layer 17a to obtain the protective layer 17. It should be understood that, in this embodiment, since the gate metal layer 16 extends beyond filling the first type of trench and the second type of trench to cover the surface of the substrate, there is no exposed area on the substrate surface; therefore, the initial protective layer 17a only needs to cover the gate metal layer 16.

[0055] In this embodiment, the non-disclosed area of ​​the photomask in the protective layer 17 can be designed with gradients based on the groove width, area, and density of the large-size metal grid. For example, if the method provided in this embodiment is applied to a scenario where large-size trenches are arranged in an array, that is, when the substrate has multiple first-type trenches arranged in an array, the projection of the non-disclosed area of ​​the photomask on the substrate covers the array area formed by the multiple first-type trenches. As another example, if the method provided in this embodiment is applied to a scenario where large-size trenches are independently set, that is, when the first-type trenches in the substrate are independently set, the projection of the non-disclosed area of ​​the photomask on the substrate only needs to cover the area where the first-type trenches are located. For the exposed area of ​​the photomask, its projection on the substrate can overlap with the second-type trenches, but preferably, the projected area of ​​the exposed area of ​​the photomask on the substrate is larger than the area of ​​the area where the second-type trenches are located. In other words, except for the area above the first-type trenches or the area above the array area formed by the first-type trenches, the remaining areas can all be exposed areas.

[0056] Finally, step S4 is executed, performing a chemical mechanical polishing (CMP) process to thin the gate metal layer 16. During this CMP process, the gate metal layer 16 is thinned until it is only retained within the first type of trench and the second type of trench, i.e., thinned until the upper surface of the gate metal layer 16 is flush with the upper surface of the substrate. At this point, there is no height difference between the large-size metal gate located in the first type of trench and the small-size metal gate located in the second type of trench, and the upper surfaces of both the large-size and small-size metal gates can be flush with the upper surface of the substrate.

[0057] This embodiment also provides a semiconductor device structure, wherein the metal gate of the semiconductor device structure is formed by the method described in this embodiment. The semiconductor device structure may, for example, be a MOSFET device as described in the preceding section.

[0058]

Example 2

[0059] Unlike Embodiment 1, in this embodiment, before the protective layer 17 is formed, the gate metal layer 16 is only filled in the first type of trench and the second type of trench.

[0060] Please see Figures 5-7 In this embodiment, the method of forming the gate metal layer 16 may include: forming an initial gate metal layer, the initial gate metal layer filling the first type of trench and the second type of trench and covering the surface of the substrate; and removing the initial gate metal layer on the substrate by a chemical mechanical polishing process, the initial gate metal layer remaining in the first type of trench and the second type of trench constituting the gate metal layer 16.

[0061] Since the gate metal layer 16 formed in this embodiment only fills the first type of trench and the second type of trench, after the protective layer 17 is formed and then a chemical mechanical polishing process is performed to thin the gate metal layer 16, the upper surface of the gate metal layer 16 is lower than the surface of the substrate. In Embodiment 1, only one chemical mechanical polishing process is performed on the gate metal layer 16, while in this embodiment, one chemical mechanical polishing process is performed before the formation of the protective layer 17 and another after the formation of the protective layer 17. Using the method provided in this embodiment, the height difference of a large-size metal gate can also be reduced, thus reducing the probability of device malfunction.

[0062] In summary, the method for forming a metal gate and the semiconductor device structure provided by the embodiments of the present invention include: providing a substrate having a first type of trench and a second type of trench, wherein the trench width of the first type of trench is greater than or equal to a preset threshold, and the trench width of the second type of trench is less than the preset threshold; forming a gate metal layer, wherein the gate metal layer fills the first type of trench and the second type of trench; forming a protective layer, wherein the protective layer at least covers the gate metal layer filled in the first type of trench and exposes the gate metal layer filled in the second type of trench; and performing a chemical mechanical polishing process to thin the gate metal layer. By depositing a protective layer to protect the large-size metal gate region before performing the final chemical mechanical polishing process to polish the metal gate, the protective layer above the large-size metal gate region acts as a buffer when the gate metal layer is polished by the chemical mechanical polishing process, which can reduce the load effect of the large-size metal gate region, thereby reducing the height loss of the large-size metal gate, reducing the height difference between the large-size metal gate and the small-size metal gate, and reducing the probability of device failure.

[0063] It should be noted that the various embodiments in this specification are described in a progressive manner, with each embodiment focusing on the differences from other embodiments. Similar or identical parts between embodiments can be referred to mutually. In addition, different parts between embodiments can also be combined with each other, and this invention does not limit this.

[0064] The above description is merely a description of preferred embodiments of the present invention and is not intended to limit the scope of the present invention in any way. Any changes or modifications made by those skilled in the art based on the above disclosure shall fall within the protection scope of the claims.

Claims

1. A method for forming a metal gate, characterized in that, include: A substrate is provided, the substrate having a first type of trench and a second type of trench, wherein the width of the first type of trench is greater than or equal to a preset threshold, and the width of the second type of trench is less than the preset threshold; A gate metal layer is formed, which fills the first type of trench and the second type of trench; A protective layer is formed, which at least covers the gate metal layer filling the first type of trench, while exposing the gate metal layer filling the second type of trench; as well as, A chemical mechanical polishing process is performed to thin the gate metal layer.

2. The method for forming a metal gate as described in claim 1, characterized in that, Before the protective layer is formed, the gate metal layer fills the first type of trench and the second type of trench, and also extends to the surface covering the substrate; After the protective layer is formed, when the gate metal layer is thinned by performing the chemical mechanical polishing process, the gate metal layer is thinned to remain only in the first type of trench and the second type of trench.

3. The method for forming a metal gate as described in claim 1, characterized in that, Before the protective layer is formed, the gate metal layer is filled only in the first type of trench and the second type of trench.

4. The method for forming a metal gate as described in claim 1, characterized in that, The method for forming the protective layer includes: An initial protective layer is deposited, the initial protective layer covering the gate metal layer and the exposed surface of the substrate; and, The region of the initial protective layer above the first type of trench is defined as the region where the photomask is not exposed, while the region of the initial protective layer above the second type of trench is defined as the region where the photomask is exposed. A photolithography process is then performed to etch the initial protective layer to obtain the protective layer.

5. The method for forming a metal gate as described in claim 4, characterized in that, The substrate has a plurality of first-type trenches arranged in an array, and the projection of the non-disclosed area of ​​the photomask onto the substrate covers the array area formed by the plurality of first-type trenches.

6. The method for improving the loading effect of a metal gate as described in claim 4, characterized in that, The first type of trench is set independently, and the projection of the non-disclosed area of ​​the photomask onto the substrate covers the area where the first type of trench is located.

7. The method for forming a metal gate as described in claim 1, characterized in that, The protective layer comprises one or more film layers, and the material of each film layer includes one or more of silicon nitride, silicon oxide, and silicon carbonitride.

8. The method for forming a metal gate as described in claim 1, characterized in that, The preset threshold value ranges from 0.1 to 10 μm.

9. The method for forming a metal gate as described in claim 1, characterized in that, The material of the gate metal layer includes Al.

10. A semiconductor device structure, characterized in that, The metal gate of the semiconductor device structure is formed by the method described in any one of claims 1 to 9.