A method for fabricating a light-emitting element and the light-emitting element itself.
By using a metal conductive layer to form a Schottky contact with a semiconductor layer of the second conductivity type in the light-emitting element, the lateral distribution of charge carriers is adjusted, the problem of charge carrier transport mismatch is solved, the current uniformity and luminous efficiency are improved, and the device life is extended.
Patent Information
- Application Number
- CN202611447528.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-17
- Publication Date
- 2026-11-17
AI Technical Summary
In nitride semiconductor materials, the electron mobility is much higher than the hole mobility, which leads to carrier transport mismatch, resulting in current crowding effect, affecting luminous efficiency and device reliability. Existing technologies that add an insulating current blocking layer increase process complexity and light absorption loss.
By using a metal conductive layer to form a Schottky contact with a semiconductor layer of the second conductivity type in the light-emitting element, the lateral distribution of charge carriers is adjusted, forming a differentiated contact mechanism, which suppresses the excessive accumulation of charge carriers at the electrode edge, thereby achieving current uniformity and improving device performance.
Without adding an additional insulating mask process, it improves current uniformity, enhances luminous efficiency and device reliability, eliminates local hot spot phenomenon, and extends device life.
Smart Images

Figure CN123124534A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, and specifically to a method for preparing a light-emitting element and the light-emitting element itself. Background Technology
[0002] In semiconductor lighting technology, flip-chip light-emitting diodes (LEDs) are widely used due to their high light extraction efficiency and good heat dissipation. However, because the electron mobility in nitride semiconductor materials is much higher than that of holes, a severe mismatch in carrier transport occurs. During operation, rapidly injected electrons tend to accumulate around the first electrode contact area (such as an N-type via) and undergo high-probability radiative recombination with the accumulated holes, leading to a severe current congestion effect. This localized excessive recombination not only results in weaker light emission and reduced luminous efficiency in the chip's central region but also subjects the area around the first electrode contact area to extremely high current loads for extended periods, accelerating material aging and reducing device reliability. To address this issue, existing technologies typically employ the method of adding a current blocking layer (CBL) to suppress edge currents. However, this requires additional photolithography masking processes, increasing process complexity and production costs. Furthermore, the introduction of the insulating layer may cause light absorption losses, affecting overall light extraction efficiency. Summary of the Invention
[0003] The purpose of this invention is to overcome the shortcomings of the prior art. This invention provides a method for fabricating a light-emitting element and a light-emitting element. By utilizing the Schottky contact formed in a specific region between a metal conductive layer and a semiconductor layer of the second conductivity type, the lateral distribution of charge carriers is adjusted, thereby achieving the goal of improving current uniformity and enhancing device performance without adding an additional insulating mask process.
[0004] This invention provides a method for fabricating a light-emitting element, the method comprising: A first semiconductor layer, an active layer, and a second semiconductor layer are sequentially deposited on a substrate to form an epitaxial structure. The epitaxial structure is etched to form a first electrode contact area that exposes a portion of the first semiconductor layer and a dicing channel that penetrates into the substrate. A transparent conductive layer is formed on the surface of the second semiconductor layer, and an annular opening is formed on the transparent conductive layer based on patterned etching, surrounding the first electrode contact area, and the annular opening area exposes the surface of the second semiconductor layer. A first passivation layer is deposited on the surface of the epitaxial structure, and the first passivation layer is etched by opening a window to expose the transparent conductive layer and the second semiconductor layer of the annular opening region; A metal conductive layer is deposited on the transparent conductive layer and the annular opening region. The metal conductive layer forms a Schottky contact with the second semiconductor layer in the annular opening region and an ohmic contact with the second semiconductor layer in the area covered by the transparent conductive layer. A second passivation layer is deposited on the metal conductive layer, and the second passivation layer is etched by opening a window to expose the metal conductive layer at the location of the first electrode contact area and the area covered by the transparent conductive layer, and a patterned first pad metal layer is formed in the window area. A third passivation layer is deposited on the first pad metal layer, and the third passivation layer is etched by opening a window to expose a portion of the first pad metal layer, and a second pad metal layer is formed in the windowed area.
[0005] Furthermore, etching the epitaxial structure to form a first electrode contact region exposing a portion of the first semiconductor layer and a dicing path extending into the substrate includes: The epitaxial structure is etched using a dry etching process to remove a portion of the second conductivity type semiconductor layer and the active layer until a portion of the first conductivity type semiconductor layer is exposed, forming the stepped groove. The etching depth of the stepped groove is 1.0 μm to 1.4 μm, and the diameter of the first electrode contact area is 30 μm to 80 μm.
[0006] Furthermore, etching the epitaxial structure to form a first electrode contact region exposing a portion of the first semiconductor layer and a dicing path extending into the substrate further includes: The etch channel region of the epitaxial structure is etched using a dry etching process to remove a portion of the second conductivity type semiconductor layer, the active layer, and the first conductivity type semiconductor layer in the etch channel region until the substrate is exposed, thus forming the etch channel. The width of the cutting channel is 12μm~18μm, and the etching depth is 3.5μm~4.5μm.
[0007] Furthermore, the step of forming a transparent conductive layer on the surface of the second semiconductor layer, and forming an annular opening around the first electrode contact area on the transparent conductive layer based on patterned etching, wherein the annular opening area exposes the surface of the second semiconductor layer includes: A 10nm~100nm thick indium tin oxide layer is deposited on the surface of the second semiconductor layer using a magnetron sputtering process to form a transparent conductive layer; High-temperature annealing is performed in a nitrogen atmosphere, with the annealing temperature set at 500°C to 600°C and the annealing time at 5 to 10 minutes, to activate the dopants in the second conductivity type semiconductor layer.
[0008] Furthermore, the step of forming a transparent conductive layer on the surface of the second semiconductor layer, and forming an annular opening around the first electrode contact area on the transparent conductive layer based on patterned etching, wherein the annular opening area exposes the surface of the second semiconductor layer includes: The transparent conductive layer is etched using a wet etching process to remove the transparent conductive layer in the annular opening area and the first electrode contact area, and the etching over-etching is controlled to be 5%~30%, so that the surface of the second conductive type semiconductor layer is exposed in the annular opening area to form the annular opening. The wet etching temperature is 25°C, the time is 100 to 200 seconds, the distance between the edge of the annular opening and the edge of the first electrode contact area is 5 μm to 40 μm, and the aperture of the annular opening is 5 μm to 20 μm.
[0009] Furthermore, the deposition of a metal conductive layer on the transparent conductive layer and the annular opening region includes: A reflective layer is deposited on the annular opening area and the transparent conductive layer using a magnetron sputtering process, and then a protective layer is deposited on the reflective layer to form the metallic conductive layer.
[0010] Furthermore, the reflective layer is one or more of a silver layer or an aluminum layer, and the deposition thickness of the reflective layer is 50nm~200nm; The protective layer is one or more of TiW, Ni, or Ti layers, and the deposition thickness of the protective layer is 90 nm to 400 nm.
[0011] The present invention also provides a light-emitting element, which is prepared based on the preparation method described above, and the light-emitting element comprises: An epitaxial structure includes a substrate and a first semiconductor layer, an active layer, and a second semiconductor layer sequentially stacked on the substrate; The first electrode contact area is a stepped groove that penetrates the second semiconductor layer and the active layer and exposes a portion of the first semiconductor layer; A transparent conductive layer is disposed on the side surface of the second semiconductor layer opposite to the active layer. The transparent conductive layer has an annular opening surrounding the first electrode contact area, and the annular opening area exposes a portion of the second semiconductor layer. A metal conductive layer covers the surface of the transparent conductive layer and the annular opening area. The metal conductive layer forms a Schottky contact with the second semiconductor layer in the annular opening area and an ohmic contact with the second semiconductor layer in the area covered by the transparent conductive layer.
[0012] Furthermore, the distance between the edge of the annular opening and the edge of the first electrode contact area is 5μm~40μm, and the aperture of the annular opening is 5μm~20μm; The metallic conductive layer includes a reflective layer and a protective layer stacked together, with the protective layer located on the side of the reflective layer away from the transparent conductive layer.
[0013] Furthermore, the second semiconductor layer is a P-type gallium nitride layer, the valence band top work function of the P-type gallium nitride layer is 6.7eV~7.0eV, and the valence band top work function of the P-type gallium nitride layer is greater than the work function of the metal conductive layer.
[0014] This invention provides a method for fabricating a light-emitting element and the same element. By creating a locally exposed region in the current-spreading layer surrounding the first electrode contact area, and allowing a conductive metal layer to directly contact a second-type semiconductor layer in this region to form a Schottky contact, while maintaining an ohmic contact in the current-spreading layer-covered area, a differentiated contact mechanism is constructed. Utilizing the rectifying characteristics of the Schottky barrier increases the equivalent series resistance around the first electrode contact area, thereby effectively suppressing excessive carrier accumulation at the electrode edge without completely blocking the current. This forces carriers to diffuse laterally towards the chip's center, achieving uniform recombination of carriers throughout the entire region, eliminating local hot spots and dark core phenomena, and improving luminous efficiency and device reliability. Attached Figure Description
[0015] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a schematic flowchart of the method for fabricating a light-emitting element according to an embodiment of this application; Figure 2 This is a schematic cross-sectional view of the stepped groove of the extension structure according to an embodiment of this application; Figure 3 This is a cross-sectional schematic diagram of the current spreading layer after deposition according to an embodiment of this application; Figure 4 This is a cross-sectional schematic diagram of the metal conductive layer after deposition according to an embodiment of this application; Figure 5 This is a cross-sectional schematic diagram of the passivation layer and electrode window after their formation according to an embodiment of this application; Figure 6 This is a schematic cross-sectional view of the final structure of the light-emitting element according to an embodiment of this application; Figure 7This is a comparison diagram of current distribution with and without locally exposed areas in the embodiments of this application; Figure 8 This is a comparison curve of I-LOP characteristics of embodiments of this application; Figure 9 This is a comparison curve of VI characteristics in an embodiment of this application. Detailed Implementation
[0017] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0018] Example 1: like Figures 1 to 5 As shown, this embodiment provides a method for fabricating a light-emitting element. This method optimizes carrier distribution by constructing a differentiated contact mechanism. The fabrication method includes the following steps: Step S100: Sequentially deposit a first semiconductor layer 2, an active layer 4, and a second semiconductor layer 3 on a substrate 1 to form an epitaxial structure. Etch the epitaxial structure to form a first electrode contact area that exposes a portion of the first semiconductor layer 2 and a dicing channel that penetrates into the substrate 1. Combination Figure 2 As shown, the epitaxial structure constitutes the functional core of the light-emitting element. In this embodiment, a buffer layer, a first semiconductor layer 2, an active layer 4, and a second semiconductor layer 3 are sequentially grown on a substrate 1. The substrate 1 can be a sapphire substrate, the buffer layer can be a low-temperature GaN layer, the first semiconductor layer 2 can be an N-type gallium nitride layer, the active layer 4 can be a multiple quantum well layer, and the second semiconductor layer 3 can be a P-type gallium nitride layer. The active layer 4 serves as the core region for radiative recombination luminescence, and its luminous efficiency depends on the degree of matching between injected electrons and holes. The first semiconductor layer 2 and the second semiconductor layer 3 are used to inject carriers of different polarities into the active layer 4.
[0019] A first electrode contact region is formed in the second semiconductor layer 3. The main function of this first electrode contact region is to establish a low-resistance electrical connection channel between the external circuit and the internal semiconductor layer, enabling efficient carrier injection. In this embodiment, the first electrode contact region is a stepped groove structure that extends through a portion of the epitaxial layer, providing physical space for subsequent metal electrode filling or contact. This three-dimensional contact structure helps to shorten the longitudinal transport path of carriers and reduce bulk resistance loss.
[0020] Specifically, the wafer is opened and acid-washed to remove organic matter, particles, and oxide layers from the surface of the epitaxial wafer, ensuring the cleanliness of subsequent processes. A pattern is defined using positive photoresist lithography, and a portion of the second semiconductor layer 3 and active layer 4 in the central region and dicing area are etched using ICP dry etching until the underlying N-type first semiconductor layer 2 is exposed, thus forming a stepped groove. The etching depth of the dry etching is 1.0 μm to 1.4 μm, and the diameter of the first electrode contact area is 30 μm to 80 μm. In this embodiment, the diameter of the first electrode contact area is preferably 40 μm to meet the etching requirements of the epitaxial structure.
[0021] In the above steps, negative photoresist lithography is used, with a photoresist thickness of 9μm~10μm. After exposure and development, the dicing pattern is defined, with a dicing width of 12μm~18μm to ensure dicing yield. ICP etching is used to etch to the sapphire substrate 1, with an etching depth of approximately 3.5μm~4.5μm and an etching angle of 80°~90°. The steeper angle helps to reduce the etching linewidth and can expand the effective mesa area, thereby maximizing the chip brightness within a limited size. Subsequently, a photoresist removal process is used to remove the photoresist.
[0022] Specifically, forming a first electrode contact region in the second semiconductor layer 3 includes: etching the second semiconductor layer 3 and the active layer 4 to form a stepped groove that penetrates the second semiconductor layer 3 and the active layer 4 and exposes a portion of the first semiconductor layer 2, serving as the first electrode contact region. Figure 1 and Figure 2As shown, the stepped groove is formed using an inductively coupled plasma (ICP) dry etching process. Unlike the isotropic wet etching used for the transparent conductive layer 5, the etching of the semiconductor epitaxial layer here must employ a highly anisotropic dry etching technique to ensure precise control of the etching depth and obtain steep sidewall morphology. This ensures electrical continuity while minimizing thermal damage and lattice disruption to the surrounding active layer 4. In practice, the etching depth is typically controlled between 1.0 μm and 1.4 μm to ensure complete penetration of the second semiconductor layer 3 and the active layer 4, and to a certain depth into the first semiconductor layer 2, thereby providing a stable low-resistance ohmic contact interface for subsequent metal electrode filling. For example, in a preferred embodiment, when the total thickness of the second semiconductor layer 3 and the active layer 4 in the epitaxial structure is approximately 1.2 μm, the etching depth can be set to 1.3 μm to ensure sufficient exposure of the surface of the first semiconductor layer 2 without excessive depth that could damage the substrate 1. Meanwhile, the opening diameter of the stepped groove can be adjusted according to the chip size and current capacity requirements. For example, in conventional high-power flip chips, its diameter can be set to 30μm to 80μm, preferably 40μm. This size provides sufficient current injection area to reduce current density without sacrificing the effective light-emitting area due to excessive mesa area. In addition, by adjusting the gas flow rate ratio and bias power during the ICP etching process, the sidewall angle of the stepped groove can be controlled between 80° and 90°. The steeper sidewalls not only help to reduce the etching linewidth and expand the effective light-emitting mesa area, but also improve the conformal coverage of the subsequent passivation layer and metal layer at the step, reducing the risk of leakage or short circuit due to poor coverage.
[0023] Step S200: A transparent conductive layer 5 is formed on the surface of the second semiconductor layer 3, and an annular opening surrounding the first electrode contact area is formed on the transparent conductive layer 5 based on patterned etching, and the annular opening area exposes the surface of the second semiconductor layer 3. refer to Figure 3 and Figure 4 A transparent conductive layer 5 is deposited on the surface of the second semiconductor layer 3 opposite to the active layer 4. Subsequently, the transparent conductive layer 5 is patterned to form an annular opening exposing the surface of the underlying second semiconductor layer 3. Crucially, the annular opening is spatially positioned around the first electrode contact region. This "surrounding" arrangement constitutes the core control structure of this application: since the first electrode contact region is typically the source of carrier injection and the area most prone to current congestion, setting an annular opening around this region effectively pre-defines a high-impedance modulation band along the path where current is most likely to accumulate. When carriers attempt to diffuse directly outward from the edge of the first electrode contact region, they first encounter the interface corresponding to the annular opening, thus being forced to change their transport behavior.
[0024] Specifically, a 10nm~100nm thick indium tin oxide layer is deposited on the surface of the second semiconductor layer 3 using magnetron sputtering technology to form a transparent conductive layer 5. Subsequently, a high-temperature annealing treatment is performed in a nitrogen (N2) atmosphere at a temperature of 500℃~600℃ for 5~10 minutes to activate Mg acceptors in the second semiconductor layer 3 and reduce the sheet resistance of the transparent conductive layer 5, laying the foundation for the subsequent formation of ohmic contacts. Then, a positive photoresist with a thickness of 2μm~3μm is coated. After exposure and development, an annular opening pattern surrounding the first electrode contact area is defined: the distance between the edge of the annular opening and the edge of the first electrode contact area is 5μm~40μm, and the aperture of the annular opening is 5μm~20μm. In this embodiment, the aperture of the annular opening is preferably 5μm, and the distance between the edge of the annular opening and the edge of the first electrode contact area is 8μm. Appropriate spacing can prevent the connection between the annular opening and the first electrode contact area after etching, as well as the interconnection between the annular openings. A wet etching process is used at 25°C for 100-200 seconds to completely remove the transparent conductive layer 5 in the annular opening area and the first electrode contact area. A slight over-etch of 5%-30% is applied to expose the surface of the second semiconductor layer 3, while maintaining good ohmic contact between the transparent conductive layer 5 and the second semiconductor layer 3 in the remaining areas. Simultaneously, the transparent conductive layer 5 is etched through at the first electrode contact area to expose the first semiconductor layer 2. The photoresist is then removed using a photoresist stripping process.
[0025] Furthermore, when the chip is powered on, holes are injected from the P electrode and electrons are injected from the N electrode through the first electrode contact area. Since the electron mobility is much higher than that of holes, electrons tend to diffuse rapidly to the area surrounding the first electrode contact area. At this time, the Schottky barrier at the bottom of the annular opening structure around the first electrode contact area increases the equivalent series resistance around the first electrode contact area, suppressing excessive accumulation of electrons near the first electrode contact area; it forces electrons to change their original path and diffuse laterally towards the center of the chip, extending the electron transport path; electrons and holes achieve more uniform matching and recombination throughout the entire area, eliminating the "bright ring" or "hot spot" around the first electrode contact area, and improving light efficiency and reliability.
[0026] Step S300: Deposit a first passivation layer 6 on the surface of the epitaxial structure, and perform window etching on the first passivation layer 6 to expose the transparent conductive layer 5 and the second semiconductor layer 3 in the annular opening region; Specifically, a first passivation layer 6 is deposited using PECVD to cover the chip surface and sidewalls, protecting the sidewalls of the first electrode contact area and separating the N electrode from the P electrode. The material of the first passivation layer 6 can be one or more combinations of silicon dioxide (SiO2), SiNx (silicon nitride thin film), and Al2O3 (aluminum oxide), with a thickness of 50nm~500nm. In this embodiment, SiO2 with a thickness of 350nm is preferred. Subsequently, a negative photoresist photolithography and wet etching process is used to perform BOE wet etching in the non-first electrode contact area to remove the first passivation layer 6 in the non-first electrode contact area and slightly over-etch by 10%~30% to ensure that the first passivation layer 6 is completely removed, exposing the underlying transparent conductive layer 5 and the second semiconductor layer 3 in the annular opening area without the transparent conductive layer 5.
[0027] Step S400: Deposit a metal conductive layer on the transparent conductive layer 5 and the annular opening area. The metal conductive layer directly contacts the second semiconductor layer 3 in the annular opening area to form a Schottky contact, and forms an ohmic contact with the second semiconductor layer 3 in the area covered by the transparent conductive layer 5. Specifically, a reflective layer, which can be a silver layer or an aluminum layer, is deposited on the annular opening area and the transparent conductive layer 5 using magnetron sputtering technology. A protective layer is also deposited, which can be a TiW (titanium-tungsten alloy), Ni (nickel), or Ti (titanium) thin film. In this embodiment, a silver layer and a TiW layer are preferred. The Ag film thickness is 50nm~200nm, and the TiW film thickness is 90nm~400nm. In this embodiment, the Ag film thickness is preferably 150nm, and the TiW film thickness is 300nm. The thicker TiW layer can block subsequent BOE etching of Ag, while the metal conductive layer can improve current spread. The photoresist is then removed using a photoresist stripping process.
[0028] Furthermore, at the annular opening, the metal conductive layer is in direct contact with the second semiconductor layer 3. The work function at the valence band top of the P-type gallium nitride layer is as high as approximately 6.7 eV to 7 eV, while the work functions of commonly used metals are much lower than this value, such as Au (approximately 5.1 eV), Ni (approximately 5.2 eV), Pt (approximately 5.6 eV), Ti (approximately 4.3 eV), Al (approximately 4.2 eV), and Ag (approximately 4.2 eV to 4.8 eV). When the metal conductive layer is in direct contact with the second semiconductor layer 3, due to the severe mismatch in work functions, a significant hole barrier is formed at the interface, exhibiting nonlinear rectification characteristics, i.e., a Schottky contact is naturally formed. The transparent conductive layer 5 in other areas forms an ohmic contact through the synergistic effect of high-temperature annealing and tunneling enhancement of the second semiconductor layer 3.
[0029] Specifically, a metal conductive layer is continuously deposited above the patterned transparent conductive layer 5 and the exposed annular aperture region. Since the metal conductive layer simultaneously covers two different interface media, two distinct electrical contact states are formed in situ within the same deposition process. Specifically, in the area covered by the transparent conductive layer 5, the metal conductive layer forms a low-resistance ohmic contact with the second semiconductor layer 3 through the transparent conductive layer 5, ensuring the current injection efficiency of the main light-emitting region. In the annular aperture region, the metal conductive layer directly contacts the second semiconductor layer 3, naturally forming a Schottky contact with rectifying characteristics based on the difference in work function or interface state characteristics between the two. This Schottky contact introduces a higher equivalent series resistance in the annular aperture region, effectively suppressing excessive accumulation of charge carriers at the edge of the contact region adjacent to the first electrode, forcing charge carriers to diffuse laterally across this high-resistance band towards the chip's center region. This differentiated contact mechanism achieves automatic current distribution balancing without adding an additional insulating layer, fundamentally alleviating the local overheating and efficiency degradation problems caused by differences in carrier mobility, and improving the overall luminous efficiency and reliability of the device.
[0030] Specifically, the step of forming the annular opening includes: patterning an annular opening around the first electrode contact area in the transparent conductive layer 5, and controlling the annular opening to maintain a preset distance from the first electrode contact area. This annular opening can form a closed impedance adjustment band around the first electrode contact area, ensuring that the charge carriers diffusing from the edge of the first electrode contact area in any direction are uniformly regulated, avoiding the current distribution distortion that may be caused by the asymmetric structure.
[0031] The design of the preset spacing has a dual technical purpose: on the one hand, the spacing acts as a safety buffer zone, which can effectively prevent the annular opening from accidentally connecting with the first electrode contact area due to the lateral drilling effect in the subsequent etching process, thereby avoiding the potential short circuit risk; on the other hand, the spacing ensures that the high-impedance Schottky contact area is precisely located at the electrode edge where the current congestion effect is most significant, rather than in the low current density area far away from the injection point, thereby maximizing the efficiency of current limiting control.
[0032] Furthermore, in some specific embodiments of this application, the preset spacing can be set to any value between 5μm and 40μm, preferably 8μm. In practical applications, it can be adaptively adjusted according to the chip size and epitaxial layer thickness.
[0033] Specifically, the process of patterning to form annular openings includes: etching the transparent conductive layer 5 using a wet etching process to form annular openings, and controlling the over-etching depth to expose the surface of the second semiconductor layer 3. Compared to dry etching, wet etching is isotropic, enabling the removal of the transparent conductive layer 5 while simultaneously creating a smoother transition morphology on the exposed surface of the second semiconductor layer 3, reducing the electric field concentration effect at sharp corners. More importantly, this application emphasizes the control of "over-etching depth." Over-etching depth here refers not only to the proportion by which the etching depth exceeds the theoretical thickness of the transparent conductive layer 5, but also, physically, to thoroughly remove any residual oxides, organic matter, or unreacted etching byproducts at the interface between the transparent conductive layer 5 and the second semiconductor layer 3 through appropriate over-etching, ensuring that the subsequently deposited metal conductive layer can directly contact the clean surface of the second semiconductor layer 3. Simultaneously, appropriate over-etching can also induce a specific interface state density on the surface of the second semiconductor layer 3, which is crucial for stabilizing the height of the subsequently formed Schottky barrier.
[0034] After completing the above etching process, before depositing the metal conductive layer, the process includes annealing the epitaxial structure to activate the second semiconductor layer 3, enabling ohmic contacts to form in the area covered by the transparent conductive layer 5, while maintaining Schottky contacts in the annular aperture area. This step is the core thermal processing step for achieving differentiated contact mechanisms under the same metal layer. During annealing, the area covered by the transparent conductive layer 5 contains transparent conductive oxides such as indium tin oxide as doping sources. The high temperature causes indium, tin, and other metal cations to diffuse to the surface of the second semiconductor layer 3, forming a highly concentrated heavily doped tunneling layer. This compresses the original Schottky barrier width to an extremely thin layer, achieving low-resistance ohmic contacts. In the annular aperture area, due to the lack of external doping sources, the annealing process only cleans the surface and repairs some lattice damage, failing to form a heavily doped layer. Therefore, the Schottky barrier between the metal conductive layer and the second semiconductor layer 3 in this area remains determined by the work function difference, exhibiting rectification characteristics. This method of using the same annealing process to generate drastically different electrical characteristics in different regions greatly simplifies the process complexity.
[0035] Specifically, the over-etching amount is 5% to 30%; the annealing temperature is 500°C to 600°C; and the annealing time is 5 to 10 minutes. Within this parameter range, for example, when the over-etching amount is controlled at 15% and the annealing temperature is set at 550°C, the device exhibits optimal overall performance. To more clearly illustrate the critical significance of this parameter range, the following is explained with a comparative example: If the over-etching amount is less than 5%, it is difficult to completely remove the residual layer at the interface, causing the Schottky barrier at the annular opening region to be shunted by parasitic resistance, resulting in unstable rectification characteristics and a significant reduction in current limiting effect; conversely, if the over-etching amount exceeds 30%, excessive chemical etching will cause irreversible lattice damage to the surface of the second semiconductor layer 3, introducing a large number of deep-level defects, leading to a significant increase in reverse leakage current of the device, and even causing early failure. Similarly, the choice of annealing temperature is also within a delicate balance window: if the annealing temperature is below 500℃, the doping diffusion below the transparent conductive layer 5 is insufficient, resulting in excessively high ohmic contact resistance, which leads to increased forward voltage and intensified heat generation; if the annealing temperature is above 600℃, excessive heat energy may cause atoms in the metal conductive layer to diffuse excessively into the annular opening region, or cause thermal decomposition on the surface of the second semiconductor layer 3, destroying the originally pure Schottky interface, resulting in a high degree of barrier degradation and loss of the proper current regulation function. Therefore, the above parameter range is not a simple choice of process window, but a necessary condition for realizing the core inventive concept of ensuring the coexistence of Schottky contacts and ohmic contacts.
[0036] Step S500: Deposit a second passivation layer 7 on the metal conductive layer, perform window etching on the second passivation layer 7 to expose the metal conductive layer at the location of the first electrode contact area and the area covered by the transparent conductive layer 5, and form a patterned first pad metal layer 8 in the window area. Specifically, a second passivation layer 7 is deposited using PECVD. The material of the second passivation layer 7 is one or more combinations of SiO2, SiNx, and Al2O3, covering the entire chip surface and separating the P electrode and N electrode. Positive photoresist is used to create openings at the first electrode contact area and the area covered by the transparent conductive layer 5. BOE wet etching is then used to etch until the metal conductive layer is exposed at the first electrode contact area and the area covered by the transparent conductive layer 5. The overetch can be set to 30%~50% to ensure that the second passivation layer 7 corresponding to the first electrode contact area and the area covered by the transparent conductive layer 5 is completely etched cleanly. Subsequently, a photoresist removal process is used to remove the photoresist.
[0037] Furthermore, a patterned first pad metal layer 8 is deposited on the above structure using negative photoresist lithography and electron beam evaporation (EBM) technology. This layer separates holes and electrons, allowing holes to be injected into the second semiconductor layer 3 and electrons to be injected into the first electrode contact area. This "splits and spreads" the current from the source, eliminating the risk of short circuits and making the brightness of the entire active area more uniform. The stacked metal is Cr / Ag / Ti / Ni / Al / Ti / Pt / Ti, where Ag acts as a supplementary reflector, adding a reflective layer to the area around the first electrode contact area where Ag is not covered, and reflecting the refracted light again to maximize light output. Subsequently, a photoresist removal process is used to remove the photoresist, forming the patterned first pad metal layer 8. It is important to note that the first pad metal layer 8 needs to cover the mesa area at the dicing track, directly contacting the first semiconductor layer 2, resulting in lower resistance, higher electron injection efficiency, and helping to reduce voltage.
[0038] Step S600: Deposit a third passivation layer 9 on the first pad metal layer 8, perform window etching on the third passivation layer 9 to expose part of the first pad metal layer 8, and form a second pad metal layer 10 in the windowed area.
[0039] Specifically, a third passivation layer 9 is deposited on the structure formed in the above steps to cover the entire chip surface. Negative photolithography is used to expose and develop the pad pattern, and the third passivation layer 9 under the pad is removed by BOE etching. Electron beam evaporation (EBM) technology is used to deposit a metal stack second pad metal layer 10, which is a stack of Ti, Ni, and AuSn. The second pad metal layer 10 is in direct contact with the first pad metal layer 8. The adhesion between the metals is much better than the contact between the metal and the passivation layer, which helps to improve the push force.
[0040] Example 2: This embodiment provides a light-emitting element, which includes an epitaxial structure comprising a first semiconductor layer 2, an active layer 4, and a second semiconductor layer 3 stacked sequentially. Figure 7 In the cross-sectional structure shown, the first semiconductor layer 2, the active layer 4, and the second semiconductor layer 3 constitute the core functional stack of the light-emitting element. The first semiconductor layer 2 is located at the bottom as an electron injection layer, the second semiconductor layer 3 is located at the top as a hole injection layer, and the active layer 4 is sandwiched between the two as a radiative recombination region.
[0041] The light-emitting element also includes a first electrode contact area disposed in the second semiconductor layer 3. Figure 7As can be seen, the first electrode contact area is embedded inside the second semiconductor layer 3 in the form of a stepped groove, extending downwards through the active layer 4 to expose part of the surface of the first semiconductor layer 2. This three-dimensional embedded structure provides a low-resistance physical channel for external circuits to access the first semiconductor layer 2, allowing charge carriers to be vertically injected from the chip surface into the underlying semiconductor layer. Compared to a planar contact structure, this stepped design effectively shortens the longitudinal transport path of charge carriers, reduces bulk resistance loss, and its sidewall morphology provides a good topological basis for the conformal coverage of subsequent film layers.
[0042] Furthermore, the light-emitting element includes a transparent conductive layer 5 disposed on the surface of the second semiconductor layer 3. The transparent conductive layer 5 has an annular opening that exposes a portion of the second semiconductor layer 3, and the annular opening surrounds the first electrode contact area. Figure 7 As shown, a transparent conductive layer 5 covers the upper surface of the second semiconductor layer 3, used to laterally expand the injected charge carriers in the horizontal direction. Crucially, the transparent conductive layer 5 is not a continuous thin film, but rather has annular openings surrounding the first electrode contact area. These annular openings spatially encircle the first electrode contact area, thus forming a specific interface control window at the edge of the first electrode contact area. This surrounding arrangement ensures that charge carriers diffusing from the edge of the first electrode contact area in any direction must pass through this control window, avoiding current distribution distortion that may be caused by asymmetric structures. It should be noted that the specific geometry of the annular openings is not limited to a single ring as shown in the figure; it can also be a ring array composed of multiple discrete openings or other patterns capable of achieving the surrounding function, as long as it can functionally exert uniform control over the current transport behavior around the first electrode contact area.
[0043] In addition, the light-emitting element also includes a metal conductive layer disposed on the transparent conductive layer 5 and the annular opening region. The metal conductive layer continuously covers the upper surface of the transparent conductive layer 5 and the surface of the second semiconductor layer 3 exposed in the annular opening region. Since the metal conductive layer is in contact with two different dielectric interfaces simultaneously, two distinct electrical contact states are formed in situ within the same structure: the metal conductive layer forms a Schottky contact with the second semiconductor layer 3 in the annular opening region and an ohmic contact with the second semiconductor layer 3 in the area covered by the transparent conductive layer 5. From a device physics perspective, in the main functional region covered by the transparent conductive layer 5, the metal conductive layer forms a low-resistance ohmic contact with the second semiconductor layer 3 through the transparent conductive layer 5. This ensures that most of the operating current can be efficiently injected into the active layer 4 for radiative recombination, maintaining the basic luminous efficiency of the device. In the annular opening region, the metal conductive layer is in direct contact with the second semiconductor layer 3. Due to the difference in work function or interface state characteristics between the two, a Schottky barrier with rectification characteristics is naturally formed at this interface. The Schottky barrier introduces a significantly higher equivalent series resistance in the annular aperture region compared to the ohmic contact region, effectively creating a high-impedance modulation band around the current injection source in the first electrode contact region. When charge carriers attempt to diffuse directly outward from the edge of the first electrode contact region, they are suppressed by this high-resistance band, forcing them to change their original transport path and diffuse laterally over a longer distance towards the chip center region, bypassing the annular aperture region. This differentiated contact mechanism achieves automatic current distribution balancing through the structure's own electrical characteristics without introducing an additional insulating barrier layer. This fundamentally alleviates local current congestion and thermal saturation effects caused by differences in carrier mobility, improving the overall optical efficiency and long-term reliability of the device.
[0044] Specifically, the annular opening has an annular structure, and a preset distance is maintained between the edge of the annular opening and the edge of the first electrode contact area. Combined with... Figure 7As shown, the annular aperture structure forms a continuous and closed impedance regulation band in the circumferential direction of the first electrode contact area, ensuring that carriers diffusing from the edge of the first electrode contact area to any direction are uniformly regulated, avoiding current distribution distortion or local hot spot shift that may be caused by asymmetric structures. The preset spacing has a dual technical purpose: firstly, this spacing acts as a process safety buffer, effectively preventing accidental connection between the annular aperture and the first electrode contact area due to photolithography alignment deviations or lateral drilling effects from wet etching during fabrication, thus avoiding potential short-circuit risks; secondly, this spacing ensures that the high-impedance Schottky contact area is precisely located at the edge of the first electrode contact area where the current congestion effect is most significant, rather than in a low-current-density area far from the injection point, thereby maximizing the efficiency of current limiting regulation. For example, in some specific embodiments of this application, the preset spacing can be set to any value between 5μm and 40μm, preferably 8μm, and can be adaptively adjusted according to chip size, epitaxial layer thickness, and photolithography capabilities in practical applications.
[0045] Furthermore, the work function of the metal conductive layer is mismatched with the valence band top work function of the second semiconductor layer 3, causing a Schottky barrier to form between the metal conductive layer and the second semiconductor layer 3 in the annular opening region, exhibiting the rectification characteristics of a Schottky contact. From a device physics perspective, this work function mismatch is the fundamental reason for the formation of a stable Schottky barrier. When the metal conductive layer is in direct contact with the second semiconductor layer 3, due to the significant difference in their Fermi levels, charge transfer occurs at the interface to reach thermal equilibrium, causing the energy bands on the semiconductor surface to bend. For a P-type semiconductor, if the metal work function is significantly lower than the semiconductor's valence band top work function, the energy bands at the interface will bend upwards, forming a barrier that hinders the flow of holes from the semiconductor to the metal—the Schottky barrier. The existence of this barrier causes carrier transport to no longer follow Ohm's law, but is instead limited by thermal emission or tunneling mechanisms, macroscopically exhibiting nonlinear rectification characteristics. By utilizing this physical property, this application successfully constructed a high-impedance channel in the annular opening region without introducing additional insulating material, forcing charge carriers to diffuse laterally towards the chip center across the region, thus achieving automatic current distribution balancing.
[0046] Specifically, the second semiconductor layer 3 is a P-type gallium nitride layer, the transparent conductive layer 5 is an indium tin oxide layer, and the metal conductive layer includes at least one of silver or aluminum. The valence band top work function of the P-type gallium nitride layer is 6.7 eV to 7.0 eV, and the valence band top work function of the P-type gallium nitride layer is greater than that of the metal conductive layer. In this material system, P-type gallium nitride (P-GaN), as a wide bandgap semiconductor, has a valence band top work function as high as 6.7 eV to 7.0 eV, while the work functions of commonly used reflective metals such as silver or aluminum are typically between 4.2 eV and 4.8 eV. The large work function difference of over 1.9 eV provides the necessary thermodynamic conditions for forming a sufficiently high and stable Schottky barrier. In contrast, although metals such as nickel or platinum can also form contacts with P-GaN, their work function difference is smaller, resulting in a lower barrier height. Under high temperature or high current operating conditions, these contacts are prone to degradation or transformation into ohmic contacts, making it difficult to maintain a long-term stable current-limiting effect. Furthermore, choosing silver or aluminum as the material for the metallic conductive layer also takes into account the high reflectivity requirement of flip-chip LEDs, allowing the metallic conductive layer to not only perform electrical control functions but also act as a back reflector to improve light extraction efficiency. Meanwhile, indium tin oxide (ITO), as the transparent conductive layer 5, not only possesses excellent light transmittance and conductivity but can also form good ohmic contacts with P-GaN through an annealing process, ensuring the current injection efficiency of the main light-emitting region.
[0047] Specifically, in this embodiment, a test sample and a comparative sample are set up for comparative testing. The test sample is prepared according to the process described in the aforementioned embodiment. The sample of the present invention has an annular opening surrounding the first electrode contact area in the transparent conductive layer 5, while the comparative sample has the same epitaxial structure, film material and process parameters except that the annular opening is not formed.
[0048] Combination Figure 9 The current distribution comparison diagrams shown visually illustrate the differences in carrier transport behavior between the two samples under a 350mA driving current. In the current distribution thermogram of the comparative sample, a distinct high-brightness annular halo appears around the first electrode contact area, indicating that a large number of electrons accumulate in this region and undergo excessive recombination with holes. The central region of the chip, however, is relatively dark, exhibiting typical current congestion and uneven light emission. In contrast, the current distribution thermogram of the present invention shows a more uniform orange-red background color, the strong halo around the first electrode contact area is significantly weakened or even disappears, and the brightness of the central region of the chip is significantly improved. This phenomenon strongly confirms that the Schottky contact formed at the annular opening region plays the expected regulatory role: the Schottky barrier introduces additional equivalent series resistance at the edge of the first electrode contact area, effectively suppressing longitudinal injection and local recombination of electrons at this location, forcing electrons to cross this high-resistance band and diffuse laterally over a longer distance towards the central region of the chip, thereby achieving uniform carrier matching and radiative recombination throughout the entire region.
[0049] Further integration Figure 8 and Figure 9 The photoelectric characteristic curves can be used to quantitatively evaluate the improvement effect of the proposed solution on the overall device performance. For example... Figure 8 As shown in the I-LOP characteristic curve, the optical output power of the sample of this invention is consistently higher than that of the comparative sample across the entire current testing range. Particularly under a high current operating condition of 1.5A, the optical output power of the sample of this invention is 3.2% higher than that of the comparative sample. From a microscopic mechanism perspective, this improvement in optical efficiency does not stem from a change in the luminous efficiency of the material itself, but rather from the mitigation of local thermal saturation and efficiency decay (Droop effect) after the current distribution is homogenized. When charge carriers are no longer concentrated in the narrow electrode edge region, the overall utilization rate of the active layer 4 is improved, enabling the device to maintain a high quantum efficiency even at high current densities.
[0050] At the same time, such as Figure 9 As shown in the VI characteristic curve, under the same driving current, the forward voltage of the sample of this invention is slightly lower than that of the comparative sample. Specifically, under the test condition of 1.5A, the forward voltage of the sample of this invention is reduced by about 0.03V. This seemingly small voltage improvement actually reflects the optimization of the carrier transport path inside the device. Although the annular opening region introduces a Schottky barrier, which theoretically increases the local resistance, the structure promotes the uniform distribution of current over a wider active area, effectively reducing Joule heat loss in the transparent conductive layer 5 and the semiconductor bulk resistance. The resulting global resistance reduction benefits outweigh the impedance increment introduced by the local Schottky contact. In addition, the uniform current distribution also avoids the generation of local hot spots, which helps to improve the long-term reliability and anti-static capability of the device.
[0051] In summary, based on the comparative test data above, it can be seen that this application, by setting an annular opening around the first electrode contact area in the transparent conductive layer 5 and using a metal conductive layer to form a Schottky contact in situ in this area, has successfully achieved precise control over the lateral distribution of charge carriers. Without adding an additional insulating mask process, it has significantly improved the current congestion problem, increased the optical output power, and reduced the forward voltage, fully verifying the inventiveness and practical value of the technical solution of this application.
[0052] Furthermore, the embodiments of the present invention have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of the present invention. The descriptions of the above embodiments are only for the purpose of helping to understand the method and core ideas of the present invention. At the same time, for those skilled in the art, there will be changes in the specific implementation methods and application scope based on the ideas of the present invention. Therefore, the content of this specification should not be construed as a limitation of the present invention.
Claims
1. A method for preparing a light-emitting element, characterized in that, The preparation method includes: A first semiconductor layer, an active layer, and a second semiconductor layer are sequentially deposited on a substrate to form an epitaxial structure. The epitaxial structure is etched to form a first electrode contact area that exposes a portion of the first semiconductor layer and a dicing channel that penetrates into the substrate. A transparent conductive layer is formed on the surface of the second semiconductor layer, and an annular opening is formed on the transparent conductive layer based on patterned etching, surrounding the first electrode contact area, and the annular opening area exposes the surface of the second semiconductor layer. A first passivation layer is deposited on the surface of the epitaxial structure, and the first passivation layer is etched by opening a window to expose the transparent conductive layer and the second semiconductor layer of the annular opening region; A metal conductive layer is deposited on the transparent conductive layer and the annular opening region. The metal conductive layer forms a Schottky contact with the second semiconductor layer in the annular opening region and an ohmic contact with the second semiconductor layer in the area covered by the transparent conductive layer. A second passivation layer is deposited on the metal conductive layer, and the second passivation layer is etched by opening a window to expose the metal conductive layer at the location of the first electrode contact area and the area covered by the transparent conductive layer, and a patterned first pad metal layer is formed in the window area. A third passivation layer is deposited on the first pad metal layer, and the third passivation layer is etched by opening a window to expose a portion of the first pad metal layer, and a second pad metal layer is formed in the windowed area.
2. The method for preparing a light-emitting element as described in claim 1, characterized in that, Etching the epitaxial structure to form a first electrode contact region exposing a portion of the first semiconductor layer and a cleavage path extending into the substrate includes: The epitaxial structure is etched using a dry etching process to remove a portion of the second conductivity type semiconductor layer and the active layer until a portion of the first conductivity type semiconductor layer is exposed, forming the stepped groove. The etching depth of the stepped groove is 1.0 μm to 1.4 μm, and the diameter of the first electrode contact area is 30 μm to 80 μm.
3. The method for preparing the light-emitting element as described in claim 2, characterized in that, Etching the epitaxial structure to form a first electrode contact region exposing a portion of the first semiconductor layer and a dicing path extending into the substrate further includes: The etch channel region of the epitaxial structure is etched using a dry etching process to remove a portion of the second conductivity type semiconductor layer, the active layer, and the first conductivity type semiconductor layer in the etch channel region until the substrate is exposed, thus forming the etch channel. The width of the cutting channel is 12μm~18μm, and the etching depth is 3.5μm~4.5μm.
4. The method for preparing a light-emitting element as described in claim 1, characterized in that, The step of forming a transparent conductive layer on the surface of the second semiconductor layer, and forming an annular opening around the first electrode contact area on the transparent conductive layer based on patterned etching, wherein the annular opening area exposes the surface of the second semiconductor layer includes: A 10nm~100nm thick indium tin oxide layer is deposited on the surface of the second semiconductor layer using a magnetron sputtering process to form a transparent conductive layer; High-temperature annealing is performed in a nitrogen atmosphere, with the annealing temperature set at 500°C to 600°C and the annealing time at 5 to 10 minutes, to activate the dopants in the second conductivity type semiconductor layer.
5. The method for preparing a light-emitting element as described in claim 1, characterized in that, The step of forming a transparent conductive layer on the surface of the second semiconductor layer, and forming an annular opening around the first electrode contact area on the transparent conductive layer based on patterned etching, wherein the annular opening area exposes the surface of the second semiconductor layer includes: The transparent conductive layer is etched using a wet etching process to remove the transparent conductive layer in the annular opening area and the first electrode contact area, and the etching over-etching is controlled to be 5%~30%, so that the surface of the second conductive type semiconductor layer is exposed in the annular opening area to form the annular opening. The wet etching temperature is 25°C, the time is 100 to 200 seconds, the distance between the edge of the annular opening and the edge of the first electrode contact area is 5 μm to 40 μm, and the aperture of the annular opening is 5 μm to 20 μm.
6. The method for preparing a light-emitting element as described in claim 1, characterized in that, The deposition of a metal conductive layer on the transparent conductive layer and the annular opening region includes: A reflective layer is deposited on the annular opening area and the transparent conductive layer using a magnetron sputtering process, and then a protective layer is deposited on the reflective layer to form the metallic conductive layer.
7. The method for preparing a light-emitting element as described in claim 6, characterized in that, The reflective layer is one or more of a silver layer or an aluminum layer, and the deposition thickness of the reflective layer is 50nm~200nm; The protective layer is one or more of TiW, Ni, or Ti layers, and the deposition thickness of the protective layer is 90 nm to 400 nm.
8. A light-emitting element, characterized in that, The light-emitting element is prepared according to the preparation method described in any one of claims 1 to 7, and the light-emitting element comprises: An epitaxial structure includes a substrate and a first semiconductor layer, an active layer, and a second semiconductor layer sequentially stacked on the substrate; The first electrode contact area is a stepped groove that penetrates the second semiconductor layer and the active layer and exposes a portion of the first semiconductor layer; A transparent conductive layer is disposed on the side surface of the second semiconductor layer opposite to the active layer. The transparent conductive layer has an annular opening surrounding the first electrode contact area, and the annular opening area exposes a portion of the second semiconductor layer. A metal conductive layer covers the surface of the transparent conductive layer and the annular opening area. The metal conductive layer forms a Schottky contact with the second semiconductor layer in the annular opening area and an ohmic contact with the second semiconductor layer in the area covered by the transparent conductive layer.
9. The light-emitting element as described in claim 8, characterized in that, The distance between the edge of the annular opening and the edge of the first electrode contact area is 5μm~40μm, and the aperture of the annular opening is 5μm~20μm; The metallic conductive layer includes a reflective layer and a protective layer stacked together, with the protective layer located on the side of the reflective layer away from the transparent conductive layer.
10. The light-emitting element as described in claim 9, characterized in that, The second semiconductor layer is a P-type gallium nitride layer, the valence band top work function of the P-type gallium nitride layer is 6.7eV~7.0eV, and the valence band top work function of the P-type gallium nitride layer is greater than the work function of the metal conductive layer.