Display module, display module manufacturing method and display device

By designing a thickness difference between the bending and non-bending areas in the cover plate body and using an adhesive layer made of a specific material, the shortcomings of OLED display products in bending performance and impact resistance are solved, thereby improving the performance and reliability of the display module.

CN123124632APending Publication Date: 2026-11-17HEFEI VISIONOX TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510629608.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing OLED display products are insufficient in terms of both bending performance and impact resistance, making it difficult to meet the needs of flexible display devices.

Method used

A display module structure is designed, wherein the cover plate body has a bending area and a non-bending area. The bending area is formed by recessing to reduce the thickness, while the non-bending area maintains a larger thickness. The cover plate body and the encapsulation layer are firmly bonded by an adhesive layer. The adhesive layer is combined with polyurethane or acrylic materials to improve the bonding strength and cushioning performance.

Benefits of technology

It improves the bending and impact resistance of the display module, extends its service life, reduces stress concentration during bending, and enhances the stability and durability of the overall structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124632A_ABST
    Figure CN123124632A_ABST
Patent Text Reader

Abstract

This application relates to the field of display technology, and more particularly to a display module, a method for manufacturing a display module, and a display device. The display module includes: a display panel, comprising a substrate and an array device layer, a light-emitting device layer, and an encapsulation layer stacked on the substrate along its thickness direction; and a cover plate assembly disposed on the side of the encapsulation layer away from the substrate, the cover plate assembly including a cover plate body, a protective film layer, and an adhesive layer disposed on the cover plate body, the protective film layer being located on the side of the cover plate body away from the substrate, and the adhesive layer being located between the cover plate body and the encapsulation layer. The cover plate body has a bending region and a non-bending region. The bending region is formed by a recess from a surface facing the substrate in a direction away from the substrate, and the adhesive layer partially fills the recess. Along the thickness direction, the thickness of the recess corresponding to the bending region is smaller than the thickness of the non-bending region, thereby improving the performance of the display module.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of display technology, and in particular to a display module, a method for manufacturing the display module, and a display device. Background Technology

[0002] Organic light-emitting diodes (OLEDs) and flat panel displays based on light-emitting diodes (LEDs) are widely used in various consumer electronics products such as mobile phones, televisions, laptops, and desktop computers due to their advantages such as high image quality, energy saving, thin body, and wide range of applications, becoming the mainstream of display devices.

[0003] However, the performance of current OLED display products needs to be improved. Summary of the Invention

[0004] This application provides a display module, a method for manufacturing the display module, and a display device, aiming to improve the performance of the display module.

[0005] In a first aspect, this application provides a display module, comprising: a display panel, including a substrate and an array device layer, a light-emitting device layer and an encapsulation layer stacked on the substrate along the thickness direction of the substrate, the array device layer including a pixel driving circuit, the light-emitting device layer including a plurality of light-emitting units, and the encapsulation layer for encapsulating the plurality of light-emitting units; a cover plate assembly disposed on the side of the encapsulation layer away from the substrate, the cover plate assembly including a cover plate body and a protective film layer and an adhesive layer disposed on the cover plate body, the protective film layer being located on the side of the cover plate body away from the substrate, and the adhesive layer being located between the cover plate body and the encapsulation layer; wherein, the cover plate body has a bending region and a non-bending region, the bending region being recessed from a surface facing the substrate in a direction away from the substrate to form a recess, the adhesive layer partially filling the recess, and along the thickness direction, the thickness dimension of the recess corresponding to the bending region is smaller than the thickness dimension of the non-bending region.

[0006] According to any of the foregoing embodiments of the first aspect of this application, on the substrate, the orthographic projection of the cover plate body is located within the orthographic projection of the protective film layer, and the orthographic projection area of ​​the cover plate body is smaller than the orthographic projection area of ​​the protective film layer.

[0007] According to any of the foregoing embodiments of the first aspect of this application, on the substrate, the minimum distance between the edge of the orthographic projection of the cover plate body and the edge of the orthographic projection of the protective film layer is greater than or equal to 0.13 mm and less than or equal to 0.33 mm.

[0008] According to any of the foregoing embodiments of the first aspect of this application, the adhesive layer includes a substrate layer and a first filling portion protruding from the substrate layer. The substrate layer is located between the cover plate body and the encapsulation layer. The first filling portion extends from the substrate layer toward the side facing the cover plate body and fills the recessed portion. And / or, the adhesive layer further includes a second filling portion located between the substrate layer and the protective film layer. The second filling portion extends along the thickness direction to the protective film layer and covers at least a portion of the edge of the cover plate body.

[0009] According to any of the foregoing embodiments of the first aspect of this application, along the thickness direction, the thickness dimension of the non-bending area is greater than or equal to 70 μm, the thickness dimension of the recessed portion corresponding to the bending area is greater than or equal to 20 μm and less than or equal to 50 μm; and / or, the width of the bending area is greater than or equal to 5 mm and less than or equal to 20 mm.

[0010] According to any of the foregoing embodiments of the first aspect of this application, the minimum thickness of the adhesive layer is greater than or equal to 25 μm and less than or equal to 50 μm; and / or, the adhesive layer comprises a polyurethane-based material or an acrylic-based material; and / or, the refractive index of the adhesive layer is greater than or equal to 1.50 and less than or equal to 1.52.

[0011] According to any of the foregoing embodiments of the first aspect of this application, the protective film layer includes an organic film layer, the thickness of which is less than or equal to 30 μm.

[0012] According to any of the foregoing embodiments of the first aspect of this application, the organic film layer includes at least one of polyimide, polyethylene terephthalate, cellulose triacetate, and polymethyl methacrylate.

[0013] According to any of the foregoing embodiments of the first aspect of this application, the organic membrane layer further includes long-chain fatty acids, wherein the content of long-chain fatty acids in the organic membrane layer is less than or equal to 5%.

[0014] According to any of the foregoing embodiments of the first aspect of this application, the cover plate body includes a glass substrate layer.

[0015] Secondly, this application provides a method for manufacturing a display module, including:

[0016] A display panel is provided, the display panel including a substrate and an array device layer, a light-emitting device layer and an encapsulation layer stacked on the substrate along the thickness direction of the substrate;

[0017] A cover plate assembly is provided, the cover plate assembly includes a cover plate body and a protective film layer and an adhesive layer disposed on the cover plate body. The cover plate body has a bending area and a non-bending area. The bending area is formed by a recess from a side surface facing the substrate in a direction away from the substrate. The adhesive layer partially fills the recess. Along the thickness direction, the thickness dimension of the recess corresponding to the bending area is smaller than the thickness dimension of the non-bending area.

[0018] The cover plate assembly is bonded to the display panel, with the adhesive layer positioned between the cover plate body and the encapsulation layer.

[0019] According to any of the foregoing embodiments of the second aspect of this application, the step of providing a cover plate assembly specifically includes:

[0020] Provide a cover plate body material layer, apply an organic material to one side of the cover plate body material layer through a coating process and then cure it to form a protective film layer on one side of the cover plate body material layer;

[0021] The outer edge region of the cover plate body material layer and the region where the recess is pre-formed are etched to form a recess, and the orthographic projection of the cover plate body material layer on the substrate is located within the orthographic projection of the protective film layer, and the orthographic projection area of ​​the cover plate body material layer is smaller than the orthographic projection area of ​​the protective film layer, so as to form a cover plate body.

[0022] An adhesive layer is formed by coating the side of the cover plate body away from the protective film layer through a coating process and then curing it to obtain the cover plate assembly.

[0023] According to any of the foregoing embodiments of the second aspect of this application, the adhesive layer includes a second filling portion, which fills at least a portion of the edge of the cover plate body, and the filling width of the second filling portion is D1, which is greater than or equal to 0.2 mm and less than or equal to 0.5 mm.

[0024] According to any of the foregoing embodiments of the second aspect of this application, after the step of bonding the cover plate assembly to the display panel, a cutting step is further included, the cutting step comprising:

[0025] The edges of the enclosure formed by the cover plate assembly and the display panel are cut according to predetermined cutting points.

[0026] According to any of the foregoing embodiments of the second aspect of this application, the vertical distance from the predetermined cutting point to the edge of the cover plate body is D2, wherein D2≥2 / 3*D1.

[0027] Thirdly, this application provides a display device that includes a display module of any of the foregoing embodiments of the first aspect, or a display device that includes a display module of any of the foregoing embodiments of the second aspect.

[0028] This application provides a display module, a method for manufacturing the display module, and a display device. The display module includes a display panel and a cover plate assembly. The display panel may include a substrate and an array device layer, a light-emitting device layer, and an encapsulation layer stacked on the substrate along its thickness direction. The array device layer includes a pixel driving circuit, and the light-emitting device layer includes multiple light-emitting units. The pixel driving circuit controls the brightness and color of the light-emitting units according to an input signal. The encapsulation layer encapsulates the multiple light-emitting units. The cover plate assembly is disposed on the side of the encapsulation layer facing away from the substrate. A protective film layer is located on the side of the cover plate body facing away from the substrate, and an adhesive layer is located between the cover plate body and the encapsulation layer. The adhesive layer is used to firmly bond the cover plate body to the encapsulation layer. The cover plate body has a bending area and a non-bending area. The bending area is formed by recessing from the side surface facing the substrate in a direction away from the substrate, so that the thickness of the recess corresponding to the bending area is smaller than the thickness of the non-bending area. Thus, while reducing the thickness of the bending area to improve bending performance, the non-bending area can maintain a larger thickness compared to the bending area to enhance impact resistance, thereby improving the performance of the display module. Attached Figure Description

[0029] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0030] Figure 1 This is a schematic diagram of the structure of the display module provided in the embodiments of this application;

[0031] Figure 2 for Figure 1 Schematic diagram of the middle cover plate assembly;

[0032] Figure 3 for Figure 2 A magnified view of a section at point A in the middle;

[0033] Figure 4 A flowchart illustrating the manufacturing method of the display module provided in this application embodiment. Figure 1 ;

[0034] Figure 5 A flowchart illustrating the manufacturing method of the display module provided in this application embodiment. Figure 2 .

[0035] Explanation of reference numerals in the attached figures:

[0036] 10-Display panel; 11-Substrate; 12-Array device layer; 13-Light-emitting device layer; 14-Encapsulation layer;

[0037] 20 - Cover plate assembly;

[0038] 100 - Cover plate body; 100a - Bending area; 100b - Non-bending area; 110 - Recess;

[0039] 200 - Protective film layer;

[0040] 300 - Adhesive layer; 310 - Substrate layer; 320 - First filler portion; 330 - Second filler portion;

[0041] X - Thickness direction.

[0042] The accompanying drawings illustrate specific embodiments of this application, which will be described in more detail below. These drawings and descriptions are not intended to limit the scope of the concept in any way, but rather to illustrate the concept of this application to those skilled in the art through reference to particular embodiments. Detailed Implementation

[0043] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions in the preferred embodiments of this application will be described in more detail below with reference to the accompanying drawings. Obviously, the described embodiments are merely some embodiments of this application, not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.

[0044] It should be noted that in the description of the embodiments of this application, the terms "upper", "lower", "inner", "outer" and other terms indicating the orientation or positional relationship are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of description, and do not indicate or imply that the device or component must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation on the embodiments of this application.

[0045] Furthermore, it should be noted that the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.

[0046] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "fixation," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection, an electrical connection, or a connection that allows communication between them; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication between two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.

[0047] In related technologies, flexible foldable display modules typically consist of components such as a cover plate, optically transparent adhesive, and a screen. Currently, the mainstream foldable cover plate solutions include colorless polyimide (CPI) and ultra-thin glass (UTG). Compared to colorless polyimide (CPI), ultra-thin glass (UTG) has become the preferred solution for high-end devices due to its higher elastic modulus and flatness. However, current ultra-thin glass (UTG) cover plates struggle to balance bending performance and impact resistance, thus affecting the performance of the display module.

[0048] In view of this, the present application provides a display module, a method for manufacturing a display module, and a display device. The display module includes a display panel and a cover plate assembly. The display panel may include a substrate and an array device layer, a light-emitting device layer, and an encapsulation layer stacked on the substrate along its thickness direction. The array device layer includes a pixel driving circuit, and the light-emitting device layer includes multiple light-emitting units. The pixel driving circuit is used to control the brightness and color of the light-emitting units according to an input signal. The encapsulation layer is used to encapsulate the multiple light-emitting units. The cover plate assembly is disposed on the side of the encapsulation layer facing away from the substrate, a protective film layer is located on the side of the cover plate body facing away from the substrate, and an adhesive layer is located between the cover plate body and the encapsulation layer. The adhesive layer is used to firmly bond the cover plate body to the encapsulation layer. The cover plate body has a bending area and a non-bending area. The bending area is formed by recessing from the side surface facing the substrate in a direction away from the substrate, so that the thickness of the recess corresponding to the bending area is smaller than the thickness of the non-bending area. Thus, while reducing the thickness of the bending area to improve bending performance, the non-bending area can maintain a larger thickness compared to the bending area to enhance impact resistance, thereby improving the performance of the display module.

[0049] The present application will now be described in detail with reference to the accompanying drawings and specific embodiments.

[0050] See Figures 1 to 3This application provides a display module, which may include a display panel 10 and a cover plate assembly 20. The display panel 10 may include a substrate 11 and an array device layer 12, a light-emitting device layer 13, and an encapsulation layer 14 stacked on the substrate 11 along its thickness direction X. The array device layer 12 includes a pixel driving circuit, the light-emitting device layer 13 includes multiple light-emitting units, and the encapsulation layer 14 encapsulates the multiple light-emitting units. The cover plate assembly 20 is disposed on the side of the encapsulation layer 14 facing away from the substrate 11. The cover plate assembly 20 includes a cover plate body 100, a protective film layer 200 disposed on the cover plate body 100, and an adhesive layer 300. The protective film layer 200 is located on the side of the cover plate body 100 facing away from the substrate 11, and the adhesive layer 300 is located between the cover plate body 100 and the encapsulation layer 14. The cover plate body 100 has a bending region 100a and a non-bending region 100b. The bending region 100a is recessed from one side surface facing the substrate 11 in a direction away from the substrate 11 to form a recess 110. The adhesive layer 300 partially fills the recess 110. Along the thickness direction X, the thickness dimension of the recess 110 corresponding to the bending region 100a is smaller than the thickness dimension of the non-bending region 100b.

[0051] It is understood that the substrate 11, as the basic supporting structure of the display panel 10, may include insulating substrates such as glass or flexible organic materials. Optionally, the substrate 11 may include flexible organic materials. Along the thickness direction X of the substrate 11, an array device layer 12, a light-emitting device layer 13, and an encapsulation layer 14 may be stacked sequentially. The array device layer 12 may include a pixel driving circuit, which can receive input signals and adjust the brightness and color of each light-emitting unit in the light-emitting device layer 13 according to the input signals. Multiple light-emitting units serve as the basic light-emitting elements for the display image; through different combinations of light emission, rich colors and clear image display can be achieved. The encapsulation layer 14 can encapsulate the light-emitting device layer 13, effectively isolating it from external moisture, oxygen, and other substances that may damage the light-emitting units, ensuring the stable operation of the display panel 10 and extending its service life.

[0052] It should be noted that the cover plate assembly 20 can be disposed on the side of the encapsulation layer 14 opposite to the substrate 11. The cover plate assembly 20 may include a cover plate body 100, a protective film layer 200, and an adhesive layer 300. The protective film layer 200 can be located on the side of the cover plate body 100 opposite to the substrate 11. The protective film layer 200 can effectively resist scratches and abrasions, thereby reducing the probability of surface damage to the cover plate body 100. This reduces the probability of reduced optical performance of the display module due to surface damage to the cover plate body 100, ensuring the clarity and color accuracy of the displayed image, and improving the durability and visual effect of the display module.

[0053] In practice, the adhesive layer 300 is disposed between the cover plate body 100 and the encapsulation layer 14 to achieve bonding between the cover plate body 100 and the encapsulation layer 14, thereby ensuring the connection stability between the cover plate assembly 20 and the display panel 10.

[0054] It should also be noted that the cover plate body 100 may include a bending region 100a and a non-bending region 100b. The bending region 100a has a recessed portion 110 formed by recessing from the side surface facing the substrate 11 in a direction away from the substrate 11. Thus, along the thickness direction X, the thickness of the recessed portion 110 corresponding to the bending region 100a can be smaller than the thickness of the non-bending region 100b. With this configuration, when the display module needs to be bent, the thinner bending region 100a, compared to the non-bending region 100b, can reduce the force required for bending, making the bending of the display module smoother. In addition, it can effectively reduce the number of microcracks per unit cross-section of the bending region 100a during the bending process, thereby effectively improving the bending performance of the display module and extending its service life. At the same time, the thicker non-bending region 100b, compared to the bending region 100a, can give the display module stronger structural rigidity and resistance to deformation. When the display module is subjected to external impact, it effectively absorbs and disperses the impact force, reducing damage to the internal structure of the display module caused by external impact, thus affecting the display effect and service life. Therefore, through the differential thickness design of the bending area 100a and the non-bending area 100b, the display module can balance bending performance and impact resistance, thereby improving the performance of the display module.

[0055] In other words, compared to the uniform thickness design of the cover plate body 100 in related technologies, the cover plate body 100 provided in this application can reduce the thickness of the bending area 100a through the recessed portion 110, thereby reducing the stress concentration during the bending process. This reduces the bending force required for the display module during bending operations, making the bending process smoother and effectively delaying the aging process of the material in the bending area 100a, thus improving the bending performance of the display module. Furthermore, compared to the uniform thickness design of the cover plate body 100 in related technologies, the cover plate body 100 provided in this application can increase the thickness of the non-bending area 100b through a thickness differentiation design between the bending area 100a and the non-bending area 100b. This allows the non-bending area 100b to effectively disperse impact energy when the display module is subjected to impact, improving the impact resistance of the display module. Therefore, the display module can meet the bending performance requirements of flexible display devices while also possessing reliable impact resistance.

[0056] See Figure 2 In some embodiments, on the substrate 11, the orthographic projection of the cover plate body 100 is located within the orthographic projection of the protective film layer 200, and the orthographic projection area of ​​the cover plate body 100 is smaller than the orthographic projection area of ​​the protective film layer 200.

[0057] It should be noted that when manufacturing the cover plate assembly 20, a cover plate body 100 can be provided first. After forming a protective film layer 200 on one side of the cover plate body 100, the edge of the cover plate body 100 is etched so that the orthographic projection of the cover plate body 100 onto the substrate 11 is within the orthographic projection of the protective film layer 200 onto the substrate 11. This arrangement allows the adhesive layer 300 to fill the periphery of the cover plate body 100, reducing the probability of edge damage to the cover plate body 100 when the display module is subjected to external forces such as side scratches or impacts. In addition, it can also enhance the overall dustproof and waterproof performance of the display module, reducing the probability of external moisture and dust entering the interior of the display module through the cover plate assembly 20, thereby improving the durability and stability of the display module.

[0058] See Figure 2 In some embodiments, on the substrate 11, the minimum distance between the edge of the orthographic projection of the cover plate body 100 and the edge of the orthographic projection of the protective film layer 200 is greater than or equal to 0.13 mm and less than or equal to 0.33 mm.

[0059] The minimum distance between the edge of the orthographic projection of the cover plate body 100 and the edge of the orthographic projection of the protective film layer 200 can be set to d1, where 0.13mm ≤ d1 ≤ 0.33mm. Optionally, d1 can be 0.15mm, 0.20mm, 0.25mm, etc. This setting ensures that the adhesive layer 300 effectively fills the periphery of the cover plate body 100. In this state, the adhesive layer 300 is evenly distributed between the edge of the cover plate body 100 and the protective film layer 200, which can fully exert its buffering and energy absorption function when the display module is subjected to external impact, effectively reducing the risk of damage to the edge of the cover plate body 100.

[0060] It should be noted that when manufacturing the display module, after the cover plate assembly 20 is attached to the display panel 10, the whole structure formed by the cover plate assembly 20 and the display panel 10 needs to be cut. The minimum vertical distance between the cutting point and the edge of the cover plate body 100 projected onto the substrate 11 can be understood as d1. Thus, by setting the minimum distance, the probability of micro-cracks appearing on the edge of the cover plate body 100 due to cutting stress can be reduced, thereby improving the cutting safety.

[0061] If d1 is too small, for example, set to 0.08mm or 0.1mm, then when the display module encounters side scratches or collisions, the edge of the cover plate body 100 is easily subjected to direct force, leading to edge damage. Furthermore, it will worsen the sealing effect of the cover plate assembly 20, allowing external moisture and dust to more easily enter the display module through gaps, affecting the normal operating performance and lifespan of the display module. In addition, it will increase the probability of cutting stress causing micro-cracks at the edge of the cover plate body 100.

[0062] If d1 is too large, for example, set to 0.35mm or 0.45mm, it will weaken the flatness, uniformity, and light transmittance of the cover plate assembly 20.

[0063] See Figure 2 and Figure 3 In some embodiments, the adhesive layer 300 includes a substrate layer 310 and a first filling portion 320 protruding from the substrate layer 310. The substrate layer 310 is located between the cover plate body 100 and the encapsulation layer 14. The first filling portion 320 extends from the substrate layer 310 toward the side facing the cover plate body 100 and fills the recess 110.

[0064] The substrate layer 310 is evenly distributed between the cover plate body 100 and the encapsulation layer 14. Through the adhesive properties of the substrate layer 310, the cover plate body 100 and the encapsulation layer 14 can be bonded together, effectively ensuring that the relative position between the display panel 10 and the cover plate assembly 20 is fixed during the use of the display module.

[0065] The first filling portion 320 fills the recessed portion 110, allowing it to fit tightly against the inner wall of the recessed portion 110, further enhancing the connection strength between the bending area 100a of the cover plate body 100 and the encapsulation layer 14. When the display module is bent, the first filling portion 320 can effectively disperse the stress in the bending area 100a, preventing stress concentration at the connection interface between the cover plate body 100 and the encapsulation layer 14, preventing problems such as delamination and cracking, thereby improving the bending reliability of the display module.

[0066] In other embodiments, the adhesive layer 300 further includes a second filler portion 330 located between the substrate layer 310 and the protective film layer 200, the second filler portion 330 extending along the thickness direction X to the protective film layer 200, and the second filler portion 330 covering at least a portion of the edge of the cover plate body 100.

[0067] It should be noted that the second filling portion 330 covering at least a portion of the edge of the cover plate body 100 can be understood as the second filling portion 330 being located on the periphery of the cover plate body 100 and abutting between the substrate layer 310 and the protective film layer 200. Therefore, when the display module is subjected to external forces such as side scratches or impacts, the flexibility and viscoelasticity of the second filling portion 330 can act as a buffer medium, evenly dispersing the external force and preventing damage to the edge of the cover plate body 100 due to excessive localized force, thus enhancing the impact resistance of the display module's edge area. Simultaneously, the sealing structure formed by the second filling portion 330, the protective film layer 200, and the substrate layer 310 can effectively prevent external moisture, dust, and other impurities from intruding into the display module through the edge gaps of the cover plate assembly 20.

[0068] In addition, when manufacturing the display module, after the cover plate assembly 20 is attached to the display panel 10, the whole formed by the cover plate assembly 20 and the display panel 10 needs to be cut. By setting the second filling part 330, the probability of micro-cracks appearing on the edge of the cover plate body 100 due to cutting stress can be reduced, thereby improving the cutting safety.

[0069] See Figure 3 In some embodiments, along the thickness direction X, the thickness dimension of the non-bending region 100b is greater than or equal to 70 μm, and the thickness dimension of the recess 110 corresponding to the bending region 100a is greater than or equal to 20 μm and less than or equal to 50 μm.

[0070] The thickness of the non-bending region 100b is h1, where h1 ≥ 70 μm. Optionally, h1 can be set to 70 μm, 75 μm, 80 μm, etc., thus ensuring the structural rigidity and impact resistance of the non-bending region 100b. When the display module encounters external impacts such as collisions or compression, the thicker non-bending region 100b can effectively buffer and disperse the impact force, thereby reducing the risk of damage to internal components and ensuring the normal operation of the display module.

[0071] If h1 is less than 70μm, for example, h1 is set to 40μm or 45μm, the impact resistance of the cover plate body 100 will decrease, thereby affecting the reliability and service life of the display module.

[0072] The thickness of the recessed portion 110 corresponding to the bending area 100a is h2, where 20μm≤h2≤50μm. Optionally, h2 can be set to 30μm, 35μm, 40μm, etc. The moderately thinned bending area 100a can effectively reduce the stress concentration during the bending process of the display module, making the bending operation smoother, while reducing material fatigue damage and improving bending performance.

[0073] If h2 is greater than 50μm, for example, h2 is set to 55μm, 60μm, 70μm, etc., it will increase the force required for bending and increase the number of microcracks in 100 unit cross-sections of the cover plate body, affecting the flexibility of the display module and making it difficult to meet the usage requirements of flexible display devices.

[0074] If h2 is less than 20μm, for example, h2 is set to 10μm, 15μm, etc., it will weaken the structural strength of the bending area 100a, making it prone to cracking during bending and shortening the bending life of the display module.

[0075] In other embodiments, the width of the bending region 100a is greater than or equal to 5 mm and less than or equal to 20 mm.

[0076] It should be noted that the width of the bending area 100a is d2, where 5mm ≤ d2 ≤ 20mm. Optionally, d2 can be set to 10mm, 15mm, 17mm, etc. This setting provides sufficient bending area 100a for the display module, ensuring smooth bending in flexible application scenarios without excessively affecting the structural strength of other areas of the cover plate body 100. During bending, the bending area 100a can evenly distribute stress, avoiding localized stress concentration that could lead to material damage, thereby improving the bending reliability and service life of the display module. At the same time, it ensures that the non-bending area 100b has sufficient area to maintain the overall rigidity of the cover plate body 100, enabling the display module to effectively absorb and disperse impact forces when facing external impacts, ensuring the safety of the internal structure of the display module.

[0077] Understandably, if d2 is less than 5mm, the bendable area 100a will be insufficient, thus limiting the bending freedom of the display module and making it difficult to meet bending requirements. Furthermore, stress is easily concentrated in a small area during bending, increasing the risk of material breakage of the cover plate body 100. On the other hand, if d2 is greater than 20mm, it will excessively weaken the structural strength of the cover plate body 100, resulting in a reduction in the area of ​​the non-bending area 100b and reducing the impact resistance of the cover plate body 100.

[0078] In some embodiments, the minimum thickness of the adhesive layer 300 is greater than or equal to 25 μm and less than or equal to 50 μm.

[0079] In practice, the minimum thickness of the adhesive layer 300 can be selected as 25μm, 35μm, 50μm, etc., so that the adhesive layer 300 can provide sufficient adhesive force to ensure that the cover plate body 100 is firmly connected to the encapsulation layer 14, and can also play a good role in buffering and stress dispersion when the display module is subjected to external impact, vibration or bending, thereby improving the reliability and service life of the display module.

[0080] Setting the minimum thickness of the adhesive layer 300 to less than 25μm, such as 10μm, 15μm, or 20μm, will reduce its adhesive strength and cushioning performance, thus affecting the normal use of the display module. Setting the minimum thickness of the adhesive layer 300 to greater than 50μm, such as 60μm, 65μm, or 70μm, will increase the overall thickness of the display module, which is not conducive to the thinner and lighter design of display products. Furthermore, an excessively thick adhesive layer 300 may result in uneven curing, residual air bubbles, and reduced assembly accuracy.

[0081] In some alternative embodiments, the adhesive layer 300 comprises a polyurethane-based material or an acrylic-based material.

[0082] Understandably, polyurethane-based materials possess excellent flexibility and high elasticity, allowing the adhesive layer 300 to deform along with the cover plate body 100 and encapsulation layer 14 during the bending of the display module. This effectively alleviates the stress generated by bending and ensures the stability of the connection between the cover plate body 100 and the encapsulation layer 14. Simultaneously, polyurethane-based materials exhibit good wear resistance and chemical corrosion resistance, resisting erosion from external moisture, dust, and other substances. This prevents the performance of the adhesive layer 300 from deteriorating due to environmental factors, thereby improving the dustproof and waterproof performance and lifespan of the display module.

[0083] Furthermore, acrylic materials possess high transparency and optical stability, which can reduce the impact on light transmission in the display panel 10, ensuring the clarity and color reproduction of the displayed image. Acrylic materials also feature rapid curing and excellent processing performance, helping to improve the production efficiency of display modules and reduce manufacturing costs.

[0084] In some embodiments, the refractive index of the adhesive layer 300 is greater than or equal to 1.50 and less than or equal to 1.52. This configuration allows light to pass more smoothly during its transmission from the display panel 10 through the encapsulation layer 14 and the adhesive layer 300 to the cover plate body 100, avoiding problems such as light scattering and haloing caused by excessive differences in refractive index, thereby improving the clarity, contrast, and color reproduction of the displayed image.

[0085] If the refractive index of the adhesive layer 300 is set to less than 1.50, light is prone to excessive refraction at the interface between the adhesive layer 300 and adjacent components (such as the encapsulation layer 14 and the cover plate body 100), resulting in light loss and uneven brightness of the displayed image. If the refractive index of the adhesive layer 300 is set to greater than 1.52, it will affect the overall optical balance of the display module and its display stability under different ambient light conditions.

[0086] In some embodiments, the protective film layer 200 includes an organic film layer with a thickness of less than or equal to 30 μm. For example, the thickness of the organic film layer can be set to 20 μm, 25 μm, 30 μm, etc. This setting can effectively protect the surface of the cover plate body 100 and reduce the probability of the bending performance of the display module being affected by an excessively thick organic film layer. In addition, a thinner organic film layer has less impact on light transmission, which helps maintain good optical performance of the display module and ensures the clarity and color accuracy of the displayed image.

[0087] In some embodiments, the organic film layer includes at least one of polyimide, polyethylene terephthalate, cellulose triacetate, and polymethyl methacrylate.

[0088] Optionally, the organic film layer may include one or more of polyimide, polyethylene terephthalate, cellulose triacetate, and polymethyl methacrylate to meet the diverse performance requirements of the protective film layer 200 in different application scenarios.

[0089] Polyimide possesses excellent high-temperature resistance and chemical corrosion resistance, along with good flexibility and mechanical strength. Applying polyimide to organic film layers enhances the impact resistance of the cured organic film due to its high strength. Furthermore, during frequent bending of the display module, polyimide effectively disperses stress, reduces crack formation, and improves the bending reliability of the display module.

[0090] Polyethylene terephthalate (PET) possesses high transparency, good dimensional stability, and abrasion resistance, which can reduce the impact on light transmission in the display panel 10, ensuring a clear and bright display image. Cellulose triacetate effectively reduces light scattering and reflection, optimizes the optical performance of the display module, and enhances image contrast and color reproduction.

[0091] Polymethyl methacrylate (PMMA) has high light transmittance and high hardness, which on the one hand ensures the display effect of the display module, and on the other hand provides strong surface impact resistance, effectively protecting the cover plate body 100 when it is hit by external objects.

[0092] In some embodiments, the organic membrane layer further includes long-chain fatty acids, wherein the content of long-chain fatty acids in the organic membrane layer is less than or equal to 5%.

[0093] Optionally, long-chain fatty acids may include dodecanoic acid. By adding long-chain fatty acids, the flexibility and ductility of the organic film layer can be effectively improved. When the display module is bent, the organic film layer containing long-chain fatty acids can better adapt to the deformation of the cover plate body 100, reducing the risk of cracking and damage caused by excessive rigidity of the organic film layer, thereby improving the bending performance and service life of the display module.

[0094] It should be noted that if the content of long-chain fatty acids in the organic membrane layer is set to be greater than 5%, the mechanical strength and stability of the organic membrane layer will decrease, making it more susceptible to damage from external forces and affecting the protective effect on the cover plate body 100.

[0095] In some embodiments, the cover body 100 includes a glass substrate layer.

[0096] Understandably, the glass substrate layer has excellent light transmittance and optical uniformity, ensuring that the light emitted by the display panel 10 passes through with high fidelity, reducing light refraction and reflection losses, and making the displayed image clear. At the same time, the glass substrate layer has excellent chemical stability, effectively resisting the corrosion of external moisture, acids, alkalis and other chemicals, avoiding the impact of material corrosion on the performance and appearance of the display module, and extending the service life of the display module.

[0097] Based on the above embodiments, see Figure 4 This application provides a method for manufacturing a display module, including:

[0098] S101: A display panel 10 is provided, the display panel 10 including a substrate 11 and an array device layer 12, a light-emitting device layer 13 and an encapsulation layer 14 stacked on the substrate 11 along the thickness direction X.

[0099] It should be noted that the array device layer 12 may include a pixel driving circuit. This circuit receives input signals and adjusts the brightness and color of each light-emitting unit in the light-emitting device layer 13 according to these signals. Multiple light-emitting units serve as the basic light-emitting elements for the display image; through different combinations of light emission, rich colors and clear image display can be achieved. The encapsulation layer 14 encapsulates the light-emitting device layer 13, effectively isolating it from external moisture, oxygen, and other substances that may damage the light-emitting units, ensuring the stable operation of the display panel 10 and extending its service life.

[0100] S102: Provide a cover plate assembly 20, which includes a cover plate body 100, a protective film layer 200 disposed on the cover plate body 100, and an adhesive layer 300. The cover plate body 100 has a bending region 100a and a non-bending region 100b. The bending region 100a is recessed from a side surface facing the substrate 11 in a direction away from the substrate 11 to form a recess 110. The adhesive layer 300 partially fills the recess 110. Along the thickness direction X, the thickness dimension of the bending region 100a corresponding to the recess 110 is smaller than the thickness dimension of the non-bending region 100b.

[0101] The bending region 100a is formed by recessing the side surface facing the substrate 11 in a direction away from the substrate 11 to form a recess 110. Compared with the non-bending region 100b, the recess 110 in the bending region 100a is thinned in the thickness direction X. The thinned bending region 100a effectively reduces the stress concentration when the display module is bent, ensuring that the bending operation is smooth. At the same time, the non-bending region 100b maintains sufficient thickness to provide stable impact resistance for the display module. Thus, through the thickness difference design between the bending region 100a and the non-bending region 100b, the display module can take into account both bending performance and impact resistance, thereby improving the performance of the display module.

[0102] Understandably, the protective film layer 200 adheres to the surface of the cover plate body 100, serving a protective function to resist external scratches, wear, and environmental erosion, thus extending the service life of the cover plate body 100. The adhesive layer 300 is used to firmly bond the cover plate body 100 to the display panel 10, and can also further disperse bending stress within the recess 110.

[0103] S103: Attach the cover plate assembly 20 to the display panel 10, such that the adhesive layer 300 is located between the cover plate body 100 and the encapsulation layer 14.

[0104] In practice, the cover plate body 100 coated with adhesive layer 300 can be smoothly brought closer to the display panel 10. Using auxiliary means such as vacuum adsorption and mechanical positioning, the cover plate body 100 and the display panel 10 are aligned in the horizontal and vertical directions. During the bonding process, the adhesive layer 300's stickiness causes the cover plate body 100 and the encapsulation layer 14 to come into contact and interact with each other molecularly. As bonding pressure is applied, the adhesive layer 300 can be uniformly filled between the cover plate body 100 and the encapsulation layer 14, forming a strong bonding interface.

[0105] In some embodiments, see Figure 5 Step S102 may specifically include:

[0106] S1021: Provide a cover plate body material layer, and apply an organic material to one side of the cover plate body material layer by a coating process and then cure it to form a protective film layer 200 on one side of the cover plate body material layer.

[0107] In practice, a cover plate body material layer is first provided to serve as the supporting structure for the cover plate assembly 20. Then, an organic material is coated onto one side of the cover plate body material layer using a coating process. The coating process parameters are adjusted according to the characteristics of the organic material and the design requirements of the protective film layer 200. For example, suitable coating equipment and methods, such as spin coating, blade coating, or spray coating, are selected to ensure that the organic material uniformly and smoothly covers the surface of the cover plate body material layer. After coating, the organic material is cured. The curing process can employ high-temperature baking to form the protective film layer 200.

[0108] Understandably, by using a coating process to form the protective film layer 200, compared to the related technology that uses adhesive to connect the protective film layer 200 to the cover plate body 100, the bonding steps can be reduced, thus improving production efficiency and yield. Furthermore, it can reduce the use of adhesive, thereby reducing the thickness of the display module.

[0109] S1022: Etch the outer edge region of the cover plate body material layer and the region where the recess 110 is pre-formed to form the recess 110, and make the orthographic projection of the cover plate body material layer on the substrate 11 located within the orthographic projection of the protective film layer 200, and the orthographic projection area of ​​the cover plate body material layer is smaller than the orthographic projection area of ​​the protective film layer 200, so as to form the cover plate body 100.

[0110] In practice, the outer edge region of the cover plate body material layer and the region where the pre-formed recess 110 is formed can be etched using dry etching or wet etching. This allows for the thinning of the pre-formed bending region of the cover plate body material layer, so that the thickness of the recess 110 corresponding to the bending region 100a of the subsequently obtained cover plate body 100 is smaller than the thickness of the non-bending region 100b, thus balancing bending performance and impact resistance.

[0111] Furthermore, by adjusting the etching range and depth, the orthographic projection of the cover plate body material layer on the substrate 11 is located within the orthographic projection of the protective film layer 200, and the orthographic projection area of ​​the cover plate body material layer is smaller than the orthographic projection area of ​​the protective film layer 200, thereby forming the cover plate body 100. This ensures that the adhesive layer 300 formed subsequently effectively wraps and protects the edge of the cover plate body 100, reducing the risk of damage to the edge of the cover plate body 100.

[0112] S1023: An adhesive is applied to the side of the cover plate body 100 away from the protective film layer 200 by a coating process and cured to form an adhesive layer 300, thereby obtaining the cover plate assembly 20.

[0113] An adhesive is applied to the side of the cover plate body 100 opposite to the protective film layer 200 using a coating process. During the coating process, the adhesive also needs to fill the recesses 110 and edge areas of the cover plate body 100. For the recesses 110, it is necessary to ensure that the adhesive is fully filled so that the adhesive layer 300 can effectively disperse stress when the display module is bent, avoiding cracking or delamination in the bending area 100a. After coating, the adhesive is cured. Optionally, the adhesive can be cured by ultraviolet curing or high-temperature heat curing to form the adhesive layer 300, thereby obtaining the cover plate assembly 20.

[0114] In some embodiments, the adhesive layer 300 includes a second filler portion 330, which fills at least a portion of the edge of the cover body 100. The filler portion 330 has a filler width of D1, which is greater than or equal to 0.2 mm and less than or equal to 0.5 mm.

[0115] Understandably, by setting the filling width between 0.2mm and 0.5mm, including both 0.2mm and 0.5mm, the adhesive layer 300 can effectively protect the edges of the cover plate body 100. On one hand, the second filling portion 330 can effectively disperse impact force, reducing damage to the edges of the cover plate body 100 caused by excessive localized stress. On the other hand, the second filling portion 330 can also prevent the intrusion of external moisture, dust, and other impurities, thereby improving the dustproof and waterproof performance and lifespan of the display module.

[0116] In other embodiments, the outer edge region of the cover plate body material layer and the region where the recessed portion 110 is pre-formed can be etched first to form the cover plate body 100. Then, the cover plate body 100 is placed in a corresponding mold to coat both sides of the cover plate body 100 to form a protective film layer 200 and an adhesive layer 300, thereby obtaining the cover plate assembly 20. The protective film layer 200 can be formed first, followed by the adhesive layer 300, or vice versa. This embodiment does not limit the specific application.

[0117] In some embodiments, see Figure 4 After step S103, a cutting step is also included, which may include: S104: cutting the edge of the community formed by the cover plate assembly 20 and the display panel 10 according to a predetermined cutting point.

[0118] Understandably, by cutting the edges of the community formed by the cover plate assembly 20 and the display panel 10, excess material during the bonding process can be removed, so that the display module has the shape and size that meets the design requirements and optimizes the fit with other external components.

[0119] In some embodiments, the vertical distance from the predetermined cutting point to the edge of the cover plate body 100 is D2, where D2 ≥ 2 / 3 * D1.

[0120] The vertical distance between the predetermined cutting point and the edge of the cover plate body 100 can also be understood as the minimum distance between the edge of the cover plate body 100 projected onto the substrate 11 and the edge of the protective film layer 200 projected onto the substrate 11. Thus, by setting D2 to be greater than or equal to 2 / 3*D1, the probability of microcracks appearing at the edge of the cover plate body 100 due to cutting stress can be reduced, thereby improving cutting safety.

[0121] Based on the above embodiments, this application provides a display device including the display module of any of the above embodiments.

[0122] The specific details of the display module can be found in the relevant descriptions in the above embodiments, and will not be repeated here. The display device can be a mobile phone, computer, tablet computer, television, electronic paper, or other device with display function, and is not limited thereto.

[0123] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A display module, characterized in that, include: The display panel includes a substrate and an array device layer, a light-emitting device layer and an encapsulation layer stacked on the substrate along the thickness direction of the substrate. The array device layer includes a pixel driving circuit, the light-emitting device layer includes a plurality of light-emitting units, and the encapsulation layer is used to encapsulate the plurality of light-emitting units. A cover plate assembly is disposed on the side of the encapsulation layer opposite to the substrate. The cover plate assembly includes a cover plate body, a protective film layer disposed on the cover plate body, and an adhesive layer. The protective film layer is located on the side of the cover plate body opposite to the substrate, and the adhesive layer is located between the cover plate body and the encapsulation layer. The cover plate body has a bending area and a non-bending area. The bending area is formed by a recessed portion formed by a side surface facing the substrate and extending away from the substrate. The adhesive layer partially fills the recessed portion. Along the thickness direction, the thickness dimension of the bending area corresponding to the recessed portion is smaller than the thickness dimension of the non-bending area.

2. The display module according to claim 1, characterized in that, On the substrate, the orthographic projection of the cover plate body is located within the orthographic projection of the protective film layer, and the orthographic projection area of ​​the cover plate body is smaller than the orthographic projection area of ​​the protective film layer. Preferably, on the substrate, the minimum distance between the edge of the orthographic projection of the cover plate body and the edge of the orthographic projection of the protective film layer is greater than or equal to 0.13 mm and less than or equal to 0.33 mm.

3. The display module according to claim 2, characterized in that, The adhesive layer includes a base layer and a first filling portion protruding from the base layer. The base layer is located between the cover plate body and the encapsulation layer. The first filling portion extends from the base layer toward the side facing the cover plate body and fills the recessed portion. And / or, the adhesive layer further includes a second filler portion located between the substrate layer and the protective film layer, the second filler portion extending along the thickness direction to the protective film layer, and the second filler portion covering at least a portion of the edge of the cover plate body.

4. The display module according to claim 1, characterized in that, Along the thickness direction, the thickness dimension of the non-bending area is greater than or equal to 70 μm, and the thickness dimension of the bending area corresponding to the recess is greater than or equal to 20 μm and less than or equal to 50 μm; And / or, the width of the bending area is greater than or equal to 5 mm and less than or equal to 20 mm.

5. The display module according to claim 1, characterized in that, The minimum thickness of the adhesive layer is greater than or equal to 25 μm and less than or equal to 50 μm; And / or, the adhesive layer comprises a polyurethane-based material or an acrylic-based material; And / or, the refractive index of the adhesive layer is greater than or equal to 1.50 and less than or equal to 1.

52.

6. The display module according to claim 5, characterized in that, The protective film layer includes an organic film layer, and the thickness of the organic film layer is less than or equal to 30 μm; Preferably, the organic film layer comprises at least one of polyimide, polyethylene terephthalate, cellulose triacetate, and polymethyl methacrylate; Preferably, the organic membrane layer further includes long-chain fatty acids, wherein the content of the long-chain fatty acids in the organic membrane layer is less than or equal to 5%; Preferably, the cover plate body includes a glass substrate layer.

7. A method for manufacturing a display module, characterized in that, include: A display panel is provided, the display panel including a substrate and an array device layer, a light-emitting device layer and an encapsulation layer stacked on the substrate along the thickness direction of the substrate; A cover plate assembly is provided, the cover plate assembly including a cover plate body and a protective film layer and an adhesive layer disposed on the cover plate body, the cover plate body having a bending region and a non-bending region, the bending region being formed by a recessed portion formed by a side surface facing the substrate and extending away from the substrate, the adhesive layer partially filling the recessed portion, and the thickness dimension of the bending region corresponding to the recessed portion being smaller than the thickness dimension of the non-bending region along the thickness direction; The cover plate assembly is attached to the display panel such that the adhesive layer is located between the cover plate body and the encapsulation layer.

8. The manufacturing method according to claim 7, characterized in that, The step of providing the cover plate assembly specifically includes: A cover plate body material layer is provided, and an organic material is coated on one side of the cover plate body material layer by a coating process and then cured to form the protective film layer on one side of the cover plate body material layer. The outer edge region of the cover plate body material layer and the region where the recess is pre-formed are etched to form the recess, and the orthographic projection of the cover plate body material layer on the substrate is located within the orthographic projection of the protective film layer, and the orthographic projection area of ​​the cover plate body material layer is smaller than the orthographic projection area of ​​the protective film layer, so as to form the cover plate body. The adhesive layer is formed by coating the cover plate body on the side opposite to the protective film layer through a coating process and then curing it to obtain the cover plate assembly. Preferably, the adhesive layer includes a second filler portion that fills at least a portion of the edge of the cover plate body, the filler portion having a filler width of D1, the filler width being greater than or equal to 0.2 mm and less than or equal to 0.5 mm.

9. The manufacturing method according to claim 8, characterized in that, Following the step of attaching the cover plate assembly to the display panel, a cutting step is further included, the cutting step comprising: The edges of the community formed by the cover plate assembly and the display panel are cut according to predetermined cutting points; Preferably, the vertical distance from the predetermined cutting point to the edge of the cover plate body is D2, where D2 ≥ 2 / 3 * D1.

10. A display device, characterized in that, The display device includes the display module as described in any one of claims 1 to 6, or the display device includes the display module formed by claims 7 to 9.