Semiconductor device and method of manufacturing the same
By designing trench isolation structures in semiconductor devices and applying tensile or compressive stress to NMOS and PMOS respectively, the problem of limited effect of shallow trench isolation structures at the edge of the active region is solved, thus improving the performance of the devices.
Patent Information
- Application Number
- CN202611347446.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-01
- Publication Date
- 2026-11-17
AI Technical Summary
In radio frequency or analog circuit devices, due to the large area of the active region, shallow trench isolation structures can only act on the edge of the active region, resulting in limited performance improvement of the device.
The design employs a trench isolation structure, including a first trench isolation structure and a second trench isolation structure, to apply tensile stress and compressive stress to the NMOS and PMOS respectively, thereby improving the stress distribution in the active region and enhancing device performance.
By applying appropriate tensile or compressive stress to the active region, the electron or hole mobility of NMOS and PMOS is improved, thereby enhancing the overall performance of the devices.
Smart Images

Figure CN123124775A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a semiconductor device and its manufacturing method. Background Technology
[0002] The compressive or tensile stress generated by shallow trench isolation (STI) acts on the active region it defines, which can help improve device performance. However, in RF or analog circuit devices, the active region is relatively large, and the compressive or tensile stress generated by shallow trench isolation can only act on the edge of the active region, resulting in a limited effect on improving device performance. Summary of the Invention
[0003] The purpose of this invention is to provide a semiconductor device and a method for manufacturing the same, which can improve the performance of the device.
[0004] To achieve the above objectives, the present invention provides a semiconductor device comprising:
[0005] Substrate;
[0006] A trench isolation structure is formed in the substrate, the trench isolation structure defining a plurality of active regions spaced apart along a second direction, each active region extending along a first direction; the trench isolation structure includes a first trench isolation structure and a second trench isolation structure, the first trench isolation structure being located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure being located on both sides of each active region in the second direction;
[0007] A MOS device is formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
[0008] Optionally, the first trench isolation structure is further used to define a plurality of virtual active regions, the plurality of virtual active regions being spaced apart along the second direction, and each of the virtual active regions extending along the first direction.
[0009] Optionally, the substrate includes at least two device regions arranged sequentially along the first direction, each device region including the trench isolation structure, the plurality of active regions and the MOS device, the first trench isolation structures of two adjacent device regions being connected to each other; the MOS devices of two adjacent device regions may be of the same or different types.
[0010] Optionally, a first trench and a second trench are formed in the substrate; when the MOS device is an NMOS, the first trench isolation structure includes a pad layer formed on the inner wall of the first trench and an insulating layer filled in the first trench, and the second trench isolation structure includes a pad layer formed on the inner wall of the second trench and an insulating layer filled in the second trench; when the MOS device is a PMOS, the first trench isolation structure includes a first pad layer formed on the inner wall of the first trench and a first insulating layer filled in the first trench, and the second trench isolation structure includes a second pad layer formed on the inner wall of the second trench and a second insulating layer filled in the second trench.
[0011] Optionally, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are made of the same material; when the MOS device is a PMOS, the first trench isolation structure and the second trench isolation structure are made of different materials.
[0012] Optionally, the MOS device includes:
[0013] Multiple gates extend along the second direction from the multiple active regions on one side of the second trench isolation structure in the second direction to the multiple active regions on the other side of the second trench isolation structure in the second direction, and the multiple gates are spaced apart along the first direction;
[0014] Source / drain, formed on both sides of the gate, in the active region.
[0015] Optionally, the semiconductor device further includes:
[0016] Multiple virtual gates are located at both ends of the multiple active regions in the first direction, and the multiple virtual gates extend from one side of the multiple active regions in the second direction to the other side in the second direction.
[0017] Optionally, the semiconductor device further includes:
[0018] Contact plugs are formed on the source / drain and the gate.
[0019] The present invention also provides a method for manufacturing a semiconductor device, comprising:
[0020] Provide a substrate;
[0021] A trench isolation structure is formed in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, and each active region extending along a first direction; the trench isolation structure includes a first trench isolation structure and a second trench isolation structure, the first trench isolation structure being located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure being located on both sides of each active region in the second direction;
[0022] A MOS device is formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
[0023] Optionally, when the MOS device is an NMOS, the step of forming a trench isolation structure in the substrate includes:
[0024] Simultaneously, a first trench and a second trench are formed in the substrate;
[0025] A liner layer is formed on the inner walls of the first trench and the second trench;
[0026] An insulating layer is filled in the first trench and the second trench. The first trench isolation structure includes the padding layer and the insulating layer in the first trench, and the second trench isolation structure includes the padding layer and the insulating layer in the second trench.
[0027] When the MOS device is a PMOS, the step of forming a trench isolation structure in the substrate includes:
[0028] A first trench is formed in the substrate;
[0029] A first liner layer is formed on the inner wall of the first trench;
[0030] A first insulating layer is filled in the first trench, and the first trench isolation structure includes the first liner layer and the first insulating layer;
[0031] A second trench is formed in the substrate;
[0032] A second liner layer is formed on the inner wall of the second trench;
[0033] A second insulating layer is filled into the second trench, and the second trench isolation structure includes the second liner layer and the second insulating layer.
[0034] Optionally, when the MOS device is an NMOS, the insulating layer is formed using a HARP deposition process; when the MOS device is a PMOS, the first insulating layer is formed using an HDP deposition process, and the second insulating layer is formed using a HARP deposition process.
[0035] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0036] 1. The semiconductor device of the present invention includes: a substrate; a trench isolation structure formed in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, each of the active regions extending along a first direction; the trench isolation structure including a first trench isolation structure and a second trench isolation structure, the first trench isolation structure being located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure being located on both sides of each of the active regions in the second direction; and a MOS device formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction. This enables improved device performance.
[0037] 2. The semiconductor device manufacturing method of the present invention includes: providing a substrate; forming a trench isolation structure in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, each of the active regions extending along a first direction; the trench isolation structure including a first trench isolation structure and a second trench isolation structure, the first trench isolation structure being located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure being located on both sides of each of the active regions in the second direction; forming a MOS device in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction. This enables the device performance to be improved. Attached Figure Description
[0038] Figure 1 This is a layout of the semiconductor device according to Embodiment 1 of the present invention;
[0039] Figure 2 This is a layout of the semiconductor device according to Embodiment 2 of the present invention;
[0040] Figure 3 yes Figure 2 The diagram shows a cross-sectional view of the semiconductor device along the AA' direction;
[0041] Figure 4 yes Figure 2 The diagram shows a cross-sectional view of the semiconductor device along the BB' direction;
[0042] Figure 5 This is a flowchart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;
[0043] Figures 6a-6g yes Figure 5 A schematic diagram of the semiconductor device manufacturing method shown.
[0044] Among them, the appendix Figures 1-6g The annotations in the attached figures are explained as follows:
[0045] 10-Substrate; 101-Lower substrate; 102-Buried insulating layer; 103-Semiconductor layer; 111-Active region; 112-Virtual active region; 121-First trench isolation structure; 1211-First trench; 1212-First insulating layer; 122-Second trench isolation structure; 1221-Second trench; 1222-Second insulating layer; 123-Mask layer; 131-Gate; 132-Virtual gate; 141-Source / drain; 15-Contact plug; X-First direction; Y-Second direction; A1-First device region; A2-Second device region. Detailed Implementation
[0046] To make the objectives, advantages, and features of the present invention clearer, the semiconductor device and its manufacturing method proposed in this invention will be further described in detail below with reference to the accompanying drawings. It should be noted that the drawings are all in a very simplified form and use non-precise proportions, and are only used to facilitate and clarify the illustration of the embodiments of the present invention.
[0047] An embodiment of the present invention provides a semiconductor device, comprising: a substrate; a trench isolation structure formed in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, each of the active regions extending along a first direction; the trench isolation structure including a first trench isolation structure and a second trench isolation structure, the first trench isolation structure being located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure being located on both sides of each of the active regions in the second direction; and a MOS device formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
[0048] See below. Figures 1-4 The semiconductor device provided in this embodiment will be described in more detail.
[0049] like Figure 3 and Figure 4 In the illustrated embodiment, the substrate 10 is an SOI (Semiconductor-On-Insulator) substrate, which includes a stacked lower substrate 101, an insulating buried layer 102, and a semiconductor layer 103; or, the substrate 10 is a bulk substrate.
[0050] The lower substrate 101, the semiconductor layer 103, and the bulk substrate can be made of semiconductor materials such as silicon, and the insulating buried layer 102 can be made of insulating materials such as silicon oxide.
[0051] A trench isolation structure is formed in the substrate 10, the trench isolation structure is used to define a plurality of active regions 111, the plurality of active regions 111 are spaced apart along a second direction Y, and each active region 111 extends along a first direction X; the trench isolation structure includes a first trench isolation structure 121 and a second trench isolation structure 122, the first trench isolation structure 121 is located on both sides of the plurality of active regions 111 in the first direction X, and the second trench isolation structure 122 is located on both sides of each active region 111 in the second direction Y.
[0052] Multiple active regions 111 are defined in the substrate 10, dividing the large active regions into multiple smaller active regions 111, so that the first trench isolation structure 121 and the second trench isolation structure 122 are closer to each active region 111, so that stress can be better transferred to the MOS device.
[0053] In one embodiment, the first direction X is perpendicular to the second direction Y, where the first direction X is the channel length direction and the second direction Y is the channel width direction. Both the first direction X and the second direction Y are parallel to the top surface of the substrate 10.
[0054] In one embodiment, the first trench isolation structure 121 is also located on both sides of the second trench isolation structure 122 in the first direction X, such as... Figure 2 As shown, the first trench isolation structure 121 is also used to define a plurality of virtual active regions 112 corresponding to the plurality of active regions 111. The plurality of virtual active regions 112 are spaced apart along the second direction Y, and each virtual active region 112 extends along the first direction X.
[0055] Each of the active regions 111 and each of the virtual active regions 112 on both sides of the active region 111 are aligned one by one in the first direction X.
[0056] In one embodiment, the length of the active region 111 in the first direction X is greater than the length of the virtual active region 112 in the first direction X, the width of the active region 111 in the second direction Y is equal to the width of the virtual active region 112 in the second direction Y, and the distance between two adjacent active regions 111 is equal to the distance between two adjacent virtual active regions 112 (that is, the width of the second trench isolation structure 122 between two adjacent active regions 112 in the second direction Y is equal to the width of the first trench isolation structure 121 between two adjacent virtual active regions 112 in the second direction Y).
[0057] In one embodiment, the top surface of the trench isolation structure is higher than the top surface of the substrate 10, or the top surface of the trench isolation structure is flush with the top surface of the substrate 10.
[0058] In one embodiment, the substrate 10 is an SOI substrate, and the trench isolation structure penetrates at least through the semiconductor layer 103. Specifically, the SOI substrate is a PDSOI (Partially Depleted Semiconductor-On-Insulator) substrate, and the trench isolation structure penetrates the semiconductor layer 103; or, the SOI substrate is an FDSOI (Fully Depleted Semiconductor-On-Insulator) substrate, and the trench isolation structure penetrates the semiconductor layer 103, the buried insulating layer 102, and extends into the lower substrate 101.
[0059] The MOS device is formed in the plurality of active regions 111. When the MOS device is an NMOS, the first trench isolation structure 121 and the second trench isolation structure 122 are used to apply tensile stress to the plurality of active regions 111. That is, the plurality of active regions 111 are subjected to tensile stress in both the first direction X and the second direction Y, so that electrons are redistributed to the energy valley with smaller effective mass, thereby improving the electron mobility of the NMOS. When the MOS device is a PMOS, the first trench isolation structure 121 is used to apply compressive stress to the plurality of active regions 111, and the second trench isolation structure 122 is used to apply tensile stress to the plurality of active regions 111. That is, the plurality of active regions 111 are subjected to compressive stress in the first direction X and tensile stress in the second direction Y, so that the effective mass of holes can be reduced, making holes easier to accelerate, thereby improving the hole mobility of the PMOS.
[0060] In one embodiment, the first direction X is the channel length direction, and the second direction Y is the channel width direction. The channel is the channel in the MOS device.
[0061] In one embodiment, the material type, material density, crystal structure, etc. of the first trench isolation structure 121 and the second trench isolation structure 122 are adjusted so that the first trench isolation structure 121 and the second trench isolation structure 122 can provide the required stress.
[0062] In one embodiment, when the MOS device is an NMOS, the first trench isolation structure 121 and the second trench isolation structure 122 are made of the same material and are formed simultaneously; when the MOS device is a PMOS, the first trench isolation structure 121 and the second trench isolation structure 122 are made of different materials and are formed separately.
[0063] In one embodiment, a first trench and a second trench are formed in the substrate 10; when the MOS device is an NMOS, the first trench isolation structure 121 includes a pad layer formed on the inner wall of the first trench and an insulating layer filled in the first trench, and the second trench isolation structure 122 includes a pad layer formed on the inner wall of the second trench and an insulating layer filled in the second trench; when the MOS device is a PMOS, the first trench isolation structure 121 includes a first pad layer formed on the inner wall of the first trench and a first insulating layer filled in the first trench, and the second trench isolation structure 122 includes a second pad layer formed on the inner wall of the second trench and a second insulating layer filled in the second trench.
[0064] In one embodiment, when the MOS device is an NMOS, the insulating layer can provide tensile stress; when the MOS device is a PMOS, the first insulating layer can provide compressive stress, and the second insulating layer can provide tensile stress.
[0065] In one embodiment, the padding layer is used to protect the inner walls of the first trench and the second trench when the insulating layer is formed. The first padding layer and the second padding layer are respectively used to protect the inner walls of the first trench and the second trench when the first insulating layer and the second insulating layer are formed. The padding layer, the first padding layer and the second padding layer can play a buffering role.
[0066] In one embodiment, the first pad layer and the second pad layer are made of silicon nitride, and the first insulating layer and the second insulating layer are made of silicon oxide.
[0067] In one embodiment, the substrate 10 includes at least two device regions arranged sequentially along the first direction X. Each device region includes the trench isolation structure, the plurality of active regions 111, and the MOS device. The first trench isolation structures 121 of adjacent two device regions are connected to each other. The MOS devices of adjacent two device regions are of the same type (both are NMOS or both are PMOS) or different types (NMOS and PMOS, respectively).
[0068] exist Figure 1 In the illustrated embodiment, the substrate 10 includes a device region; Figure 2 In the embodiment shown, the substrate 10 includes two device regions arranged sequentially along the first direction X, namely a first device region A1 and a second device region A2.
[0069] When the substrate 10 includes at least two device regions sequentially arranged along the first direction X, the virtual active regions 112 are arranged on both sides of the active region 111 in the first direction X. This allows the sum of the length of the active region 111 in the first direction X, the length of the virtual active regions 112 on both sides of the active region 111 in the first direction X, and the distance between the active region 111 and the virtual active regions 112 (i.e., ...) to be equal to the sum of the lengths of the active region 111 in the first direction X, the lengths ... in the first direction X, and the distance between the active region 111 and the virtual active regions 112 (i.e., ...) to be equal to the sum of the lengths of the active region 111 in the first direction X, the lengths of the virtual active regions 112 in the first direction X, and the distance between the active region 111 and the virtual active regions 112 in the first direction X, to be equal to Figure 2 With the length L1 shown remaining unchanged, the distance between the active regions 111 in two adjacent device regions is increased, thereby reducing the impact of the first trench isolation structure 121 in one device region on the active region 111 in the other adjacent device region when the types of MOS devices in the two adjacent device regions are different (NMOS and PMOS, respectively) and the first trench isolation structure 121 connected in the two adjacent device regions provides different types of stress (tensile stress and compressive stress). That is, the virtual active region 112 can play a buffering role.
[0070] exist Figure 2 In the illustrated embodiment, two sets of virtual active regions 112 are provided between the active region 111 of the first device region A1 and the active region 111 of the second device region A2. In another embodiment, one set of virtual active regions 112 can be provided between the active region 111 of the first device region A1 and the active region 111 of the second device region A2, which can save device area. In one embodiment, the MOS device includes:
[0071] A plurality of gates 131 extend along the second direction Y from the second trench isolation structure 122 on one side of the plurality of active regions 111 in the second direction Y to the second trench isolation structure 122 on the other side of the plurality of active regions 111 in the second direction Y, and the plurality of gates 131 are spaced apart along the first direction X.
[0072] Source / drain 141 is formed in the active regions 111 on both sides of the gate 131, located in or on the substrate 10 (RSD, Raised Source / Drain). The source / drain 141 of the active region 111 on one side of the gate 131 is the source, and the source / drain 141 of the active region 111 on the other side of the gate 131 is the drain; between two adjacent gates 131, the drain of one gate 131 is shared with the source of the other gate 131.
[0073] In one embodiment, a gate dielectric layer (not shown) is further formed between the gate 131 and the substrate 10.
[0074] The region located below the gate 131 between the source and the drain is a channel.
[0075] In one embodiment, the semiconductor device further includes:
[0076] Multiple virtual gates 132 are respectively located at both ends of the multiple active regions 111 in the first direction X, and the multiple virtual gates 132 extend from one side of the multiple active regions 111 in the second direction Y to the other side in the second direction Y.
[0077] In one embodiment, the plurality of virtual active regions 112 also have virtual gates 132 formed at both ends of the first direction X, and the virtual gates 132 extend from one side of the plurality of virtual active regions 112 in the second direction Y to the other side in the second direction Y.
[0078] In one embodiment, the virtual gates 132 at both ends of the plurality of active regions 111 in the first direction X extend from the plurality of active regions 111 and the second trench isolation structure 122 to the first trench isolation structure 121; the virtual gates 132 at both ends of the plurality of virtual active regions 112 in the first direction X extend from the plurality of virtual active regions 112 to the first trench isolation structure 121.
[0079] Since the virtual gates 132 are formed at both ends of the plurality of active regions 111 in the first direction X, when the plurality of gates 131 are formed by photolithography and etching processes, it can be ensured that the pattern density of the plurality of gates 131 remains uniform, that is, it is ensured that the shape of the gates 131 near the edge positions of the plurality of active regions 111 at both ends of the first direction X is consistent with the shape of the gates 131 at the middle positions away from the two ends of the plurality of active regions 111 in the first direction X.
[0080] When the substrate is a bulk substrate, the source / drain 141 is located in or on the bulk substrate of the active region 111; when the SOI substrate is a PDSOI substrate, the source / drain 141 is located in or on the semiconductor layer 103 of the active region 111; when the SOI substrate is an FDSOI substrate, the source / drain 141 is located on the semiconductor layer 103 of the active region 111. Figure 3 and Figure 4 In the embodiment shown, the source / drain 141 is located on the semiconductor layer 103 of the active region 111.
[0081] In one embodiment, the semiconductor device further includes:
[0082] Contact plugs 15 are formed on the source / drain electrodes 141 on both sides of the gate electrode 131.
[0083] In one embodiment, the width of the active region 111 in the second direction Y is the minimum width allowed by the process of forming the contact plug 15 on the active region 111.
[0084] In one embodiment, the contact plug 15 is also formed on the gate 131. The contact plug 15 includes a gate contact plug, a source contact plug, and a drain contact plug.
[0085] In one embodiment, the contact plug 15 may be formed on the portions of the gate 131 located on the second trench isolation structure 122 at both ends. Alternatively, the contact plug 15 may be located solely on the gate 131, or it may extend from the gate 131 to the second trench isolation structure 122 on both sides of the gate 131.
[0086] It should be noted that the contact plug 15 is not formed on the virtual gate 132 and the virtual active region 112.
[0087] In one embodiment, the semiconductor device further includes:
[0088] A metal silicide layer (not shown) is formed on the source / drain 141 and the gate 131, and the contact plug 15 is formed on the metal silicide layer.
[0089] In one embodiment, the width of the second trench isolation structure 122 between two adjacent active regions 111 in the second direction Y is the minimum width allowed by the process of filling the trench isolation structure 122 in the trench within the substrate 10. This ensures that, during the fabrication of the second trench isolation structure 122, the second trench isolation structure 122 can be filled into the trench while preventing the metal silicide layers on the two adjacent active regions 111 from becoming too close together, thus avoiding short circuits between the two adjacent active regions 111. Furthermore, the width of the plurality of active regions 111 in the second direction Y is the sum of the widths of the second trench isolation structures 122 between all adjacent active regions 111 in the second direction Y (i.e., ... Figure 1 While keeping the width W1 shown unchanged, the total width of the plurality of active regions 111 in the second direction Y is maximized, so as to avoid reducing the effective width of the channel too much and thus reducing the device performance.
[0090] In one embodiment, the width of the active region 111 in the second direction Y is the minimum width allowed by the process of forming the contact plug 15 on the active region 111, so as to minimize the width of each active region 111 in the second direction Y, thereby allowing the stress provided by the second trench isolation structure 122 to be applied more evenly to the entire area of each active region 111, avoiding the active region 111 being too wide in the second direction Y, which would result in the stress on the middle area of the active region 111 in the second direction Y being too small.
[0091] One embodiment of the present invention provides a method for manufacturing a semiconductor device, see reference. Figure 5 , Figure 5 This is a flowchart of a method for manufacturing a semiconductor device according to an embodiment of the present invention, the method comprising:
[0092] Step S1: Provide a substrate;
[0093] Step S2: Form a trench isolation structure in the substrate. The trench isolation structure defines a plurality of active regions. The plurality of active regions are spaced apart along a second direction, and each active region extends along a first direction. The trench isolation structure includes a first trench isolation structure and a second trench isolation structure. The first trench isolation structure is located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure is located on both sides of each active region in the second direction.
[0094] Step S3: Form a MOS device in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
[0095] See below. Figures 1-4 , Figures 6a-6g The manufacturing method of the semiconductor device provided in this embodiment will be described in more detail. It should be noted that for structures with the same names in the manufacturing method of the semiconductor device as those in the semiconductor device itself, please refer to the description of the semiconductor device described above.
[0096] According to step S1, a substrate 10 is provided.
[0097] like Figure 3 , Figure 4 and Figures 6a-6g In the illustrated embodiment, the substrate 10 is an SOI (Semiconductor-On-Insulator) substrate, which includes a stacked lower substrate 101, an insulating buried layer 102, and a semiconductor layer 103; or, the substrate 10 is a bulk substrate.
[0098] Following step S2, as Figures 1-4 , Figure 6g As shown, a trench isolation structure is formed in the substrate 10. The trench isolation structure defines a plurality of active regions 111, which are spaced apart along a second direction Y. Each active region 111 extends along a first direction X. The trench isolation structure includes a first trench isolation structure 121 and a second trench isolation structure 122. The first trench isolation structure 121 is located on both sides of the plurality of active regions 111 in the first direction X, and the second trench isolation structure 122 is located on both sides of each active region 111 in the second direction Y.
[0099] In one embodiment, the first direction X is perpendicular to the second direction Y, where the first direction X is the channel length direction and the second direction Y is the channel width direction.
[0100] In one embodiment, the first trench isolation structure 121 is also located on both sides of the second trench isolation structure 122 in the first direction X, such as... Figure 2 As shown, the first trench isolation structure 121 is also used to define a plurality of virtual active regions 112 corresponding to the plurality of active regions 111. The plurality of virtual active regions 112 are spaced apart along the second direction Y, and each virtual active region 112 extends along the first direction X.
[0101] In one embodiment, when the subsequently formed MOS device is an NMOS, the step of forming a trench isolation structure in the substrate 10 includes:
[0102] Simultaneously, a first trench 1211 and a second trench 1221 are formed in the substrate 10;
[0103] A liner layer (not shown) is formed on the inner walls of the first trench 1211 and the second trench 1221;
[0104] An insulating layer (not shown) is filled in the first trench 1211 and the second trench 1221. The first trench isolation structure 121 includes the padding layer and the insulating layer in the first trench 1211, and the second trench isolation structure 122 includes the padding layer and the insulating layer in the second trench 1221.
[0105] In the above embodiments, the insulating layer can provide tensile stress such that both the first trench isolation structure 121 and the second trench isolation structure 122 can be used to apply tensile stress to the plurality of active regions 111.
[0106] In one embodiment, when the subsequently formed MOS device is a PMOS, the step of forming a trench isolation structure in the substrate 10 includes:
[0107] like Figure 6a As shown, a first trench 1211 is formed in the substrate 10;
[0108] A first liner layer (not shown) is formed on the inner wall of the first trench 1211;
[0109] like Figure 6c As shown, the first insulating layer 1212 is filled in the first trench 1211, and the first trench isolation structure 121 includes the first padding layer and the first insulating layer 1212.
[0110] like Figure 6d As shown, a second trench 1221 is formed in the substrate 10;
[0111] A second liner layer (not shown) is formed on the inner wall of the second trench 1221;
[0112] like Figure 6f As shown, a second insulating layer 1222 is filled in the second trench 1221, and the second trench isolation structure 122 includes the second padding layer and the second insulating layer 1222.
[0113] In the above embodiments, the first insulating layer 1212 and the second insulating layer 1222 have different material types, material density, crystal structure and other properties. The first insulating layer 1212 can provide compressive stress, and the second insulating layer 1222 can provide tensile stress, so that the first trench isolation structure 121 can be used to apply compressive stress to the plurality of active regions 111, and the second trench isolation structure 122 can be used to apply tensile stress to the plurality of active regions 111.
[0114] In one embodiment, the step of forming the first trench 1211 and the second trench 1221 includes: as follows Figure 6a As shown, a mask layer 123 is formed on the substrate 10; as Figure 6a and Figure 6d As shown, the mask layer 123 and the substrate 10 are etched to form the first trench 1211 and the second trench 1221.
[0115] In one embodiment, the mask layer 123 may comprise a single-layer structure or a structure of at least two stacked layers. For example, the mask layer 123 may comprise a stacked silicon oxide layer and a silicon nitride layer.
[0116] In one embodiment, such as Figure 6b As shown, when the first insulating layer 1212 is filled into the first trench 1211, the first insulating layer 1212 is also formed on the mask layer 123; as Figure 6c As shown, the first insulating layer 1212 above the top surface of the mask layer 123 is removed.
[0117] In one embodiment, such as Figure 6e As shown, when the second insulating layer 1222 is filled into the second trench 1221, the second insulating layer 1222 is also formed on the mask layer 123; as Figure 6f As shown, the second insulating layer 1222 above the top surface of the mask layer 123 is removed.
[0118] In one embodiment, such as Figure 6gAs shown, after forming the first trench isolation structure 121 and the second trench isolation structure 122, the mask layer 123 is removed. The mask layer 123 can be removed using a wet etching process. The top corners of the first trench isolation structure 121 and the second trench isolation structure 122 are also partially etched away, causing the top width of the first trench isolation structure 121 and the second trench isolation structure 122 to gradually widen from top to bottom.
[0119] It should be noted that, Figures 6a-6g This is only used to illustrate the formation steps of the first trench isolation structure 121 and the second trench isolation structure 122. Figures 6a-6g The first trench isolation structure 121 and the second trench isolation structure 122 that are finally formed do not represent their relative positional relationship in the substrate 10.
[0120] In one embodiment, when the MOS device is an NMOS, the insulating layer is formed using a HARP (High Aspect Ratio Process) deposition process; when the MOS device is a PMOS, the insulating layer 1212 is formed using an HDP (High Density Plasma) deposition process, and the second insulating layer 1222 is formed using a HARP deposition process. The lattice structure, density, and other properties of the insulating layer, the insulating layer 1212, and the second insulating layer 1222 are adjusted by modifying the process parameters (e.g., temperature) of the HARP and HDP deposition processes, thereby enabling the first trench isolation structure 121 and the second trench isolation structure 122 to provide the required type of stress.
[0121] Following step S3, as follows Figures 1-4 As shown, a MOS device is formed in the plurality of active regions 111; wherein, when the MOS device is an NMOS, the first trench isolation structure 121 and the second trench isolation structure 122 are used to apply tensile stress to the plurality of active regions 111; when the MOS device is a PMOS, the first trench isolation structure 121 is used to apply compressive stress to the plurality of active regions 111, and the second trench isolation structure 122 is used to apply tensile stress to the plurality of active regions 111.
[0122] When the MOS device is an NMOS, the plurality of active regions 111 are subjected to tensile stress in the first direction X and the second direction Y, which causes electrons to redistribute to energy valleys with smaller effective mass, thereby improving the electron mobility of the NMOS. When the MOS device is a PMOS, the plurality of active regions 111 are subjected to compressive stress in the first direction X and tensile stress in the second direction Y, which reduces the effective mass of holes and makes holes easier to accelerate, thereby improving the hole mobility of the PMOS.
[0123] In one embodiment, the substrate 10 includes at least two device regions arranged sequentially along the first direction X. Each device region includes the trench isolation structure, the plurality of active regions 111, and the MOS device. The first trench isolation structures 121 of adjacent two device regions are connected to each other. The MOS devices of adjacent two device regions are of the same type (both are NMOS or both are PMOS) or different types (NMOS and PMOS, respectively).
[0124] In one embodiment, the step of forming the MOS device in the plurality of active regions 111 includes:
[0125] A plurality of gates 131 are formed, the plurality of gates 131 extending from the plurality of active regions 111 on one side of the second trench isolation structure 122 in the second direction Y to the plurality of active regions 111 on the other side of the second direction Y in the second trench isolation structure 122, and the plurality of gates 131 are spaced apart along the first direction X.
[0126] Source / drain electrodes 141 are formed in the active regions 111 on both sides of the gate 131, and the source / drain electrodes 141 are located in or on the substrate 10 (RSD, Raised Source / Drain). Specifically, the source / drain electrode 141 in the active region 111 on one side of the gate 131 is the source, and the source / drain electrode 141 in the active region 111 on the other side of the gate 131 is the drain; between two adjacent gates 131, the drain of one gate 131 is shared with the source of the other gate 131.
[0127] In one embodiment, the method for manufacturing the semiconductor device further includes:
[0128] Multiple virtual gates 132 are formed, which are respectively located at both ends of the multiple active regions 111 in the first direction X. The multiple virtual gates 132 extend from one side of the multiple active regions 111 in the second direction Y to the other side in the second direction Y.
[0129] In one embodiment, the plurality of virtual active regions 112 also have virtual gates 132 formed at both ends of the first direction X, and the virtual gates 132 extend from one side of the plurality of virtual active regions 112 in the second direction Y to the other side in the second direction Y.
[0130] In one embodiment, the plurality of gates 131 and the plurality of dummy gates 132 can be formed by first depositing gate material on the trench isolation structure, the active region 111, and the dummy active region 112, and then etching the gate material. The gate material may be planarized or left unplanarized before etching.
[0131] Since the virtual gates 132 are formed at both ends of the plurality of active regions 111 in the first direction X, when the plurality of gates 131 are formed by photolithography and etching processes, it can be ensured that the pattern density of the plurality of gates 131 remains uniform, that is, it is ensured that the shape of the gates 131 near the edge positions of the plurality of active regions 111 at both ends of the first direction X is consistent with the shape of the gates 131 at the middle positions away from the two ends of the plurality of active regions 111 in the first direction X.
[0132] When the substrate is a bulk substrate, the source / drain 141 is located in or on the bulk substrate of the active region 111; when the SOI substrate is a PDSOI substrate, the source / drain 141 is located in or on the semiconductor layer 103 of the active region 111; when the SOI substrate is an FDSOI substrate, the source / drain 141 is located on the semiconductor layer 103 of the active region 111. Figure 3 and Figure 4 In the embodiment shown, the source / drain 141 is located on the semiconductor layer 103 of the active region 111.
[0133] When the source / drain 141 is located in the bulk substrate or in the semiconductor layer 103, the source / drain 141 can be formed by ion implantation; when the source / drain 141 is located on the bulk substrate or on the semiconductor layer 103, the source / drain 141 can be formed by epitaxial growth.
[0134] In one embodiment, the method for manufacturing the semiconductor device further includes:
[0135] Contact plugs 15 are formed on the source / drain 141 and the gate 131. The contact plugs 15 include a gate contact plug, a source contact plug, and a drain contact plug.
[0136] In one embodiment, prior to forming the contact plug 15, the method of manufacturing the semiconductor device further includes:
[0137] A metal silicide layer (not shown) is formed on the source / drain 141 and the gate 131.
[0138] As can be seen from the above, in the semiconductor device and its manufacturing method provided by the present invention, the trench isolation structure is used to define a plurality of active regions, the plurality of active regions are spaced apart along a second direction, and each active region extends along a first direction; the trench isolation structure includes a first trench isolation structure and a second trench isolation structure, the first trench isolation structure is located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure is located on both sides of each active region in the second direction; the MOS device is formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions. By modifying the layout, a large active area is divided into multiple smaller active areas extending along a first direction and spaced apart along a second direction. This allows the stress provided by the trench isolation structure to be applied more evenly across the entire area of each active area (including the central and edge areas in the second direction), increasing the stress effect on the central area of the large active area. Furthermore, depending on the type of MOS device, different types of first and second trench isolation structures are designed in the first and second directions of the multiple active areas to provide different types of stress. Therefore, the carrier mobility of the MOS device can be improved, thereby enhancing the device's performance (e.g., the on-current I in the FoM quality factor). dsat and transconductance G m (It) has been improved.
[0139] Furthermore, due to the increased carrier mobility, while maintaining or increasing the transconductance Gm, the large active region is divided into multiple smaller active regions extending along a first direction and spaced apart along a second direction. A second trench isolation structure is provided between adjacent active regions. This allows the total width of the multiple active regions in the second direction to decrease while maintaining the sum of the widths of the second trench isolation structures between all adjacent active regions in the second direction. This, in turn, reduces the parasitic capacitance between the gate and the active region, thereby significantly improving the device's RF performance (e.g., the cutoff frequency F in the quality factor FoM specification).t and maximum oscillation frequency F max ).
[0140] The above description is merely a description of preferred embodiments of the present invention and is not intended to limit the scope of the present invention in any way. Any changes or modifications made by those skilled in the art based on the above disclosure shall fall within the protection scope of the claims.
Claims
1. A semiconductor device, characterized in that, include: Substrate; A trench isolation structure is formed in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, and each of the active regions extending along a first direction; The trench isolation structure includes a first trench isolation structure and a second trench isolation structure. The first trench isolation structure is located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure is located on both sides of each of the active regions in the second direction. A MOS device is formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
2. The semiconductor device as claimed in claim 1, characterized in that, The first trench isolation structure is also used to define a plurality of virtual active regions, which are spaced apart along the second direction, and each virtual active region extends along the first direction.
3. The semiconductor device as described in claim 1, characterized in that, The substrate includes at least two device regions arranged sequentially along the first direction. Each device region includes the trench isolation structure, the plurality of active regions, and the MOS device. The first trench isolation structures of two adjacent device regions are connected to each other. The MOS devices of two adjacent device regions may be of the same or different types.
4. The semiconductor device as claimed in claim 1, characterized in that, The substrate has a first trench and a second trench formed therein; when the MOS device is an NMOS, the first trench isolation structure includes a pad layer formed on the inner wall of the first trench and an insulating layer filled in the first trench, and the second trench isolation structure includes a pad layer formed on the inner wall of the second trench and an insulating layer filled in the second trench; when the MOS device is a PMOS, the first trench isolation structure includes a first pad layer formed on the inner wall of the first trench and a first insulating layer filled in the first trench, and the second trench isolation structure includes a second pad layer formed on the inner wall of the second trench and a second insulating layer filled in the second trench.
5. The semiconductor device as claimed in claim 1, characterized in that, When the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are made of the same material; when the MOS device is a PMOS, the first trench isolation structure and the second trench isolation structure are made of different materials.
6. The semiconductor device as claimed in claim 1, characterized in that, The MOS device includes: Multiple gates extend along the second direction from the multiple active regions on one side of the second trench isolation structure in the second direction to the multiple active regions on the other side of the second trench isolation structure in the second direction, and the multiple gates are spaced apart along the first direction; Source / drain, formed on both sides of the gate, in the active region.
7. The semiconductor device as claimed in claim 1, characterized in that, The semiconductor device further includes: Multiple virtual gates are located at both ends of the multiple active regions in the first direction, and the multiple virtual gates extend from one side of the multiple active regions in the second direction to the other side in the second direction.
8. The semiconductor device as claimed in claim 6, characterized in that, The semiconductor device further includes: Contact plugs are formed on the source / drain and the gate.
9. A method for manufacturing a semiconductor device, characterized in that, include: Provide a substrate; A trench isolation structure is formed in the substrate, the trench isolation structure defining a plurality of active regions, the plurality of active regions being spaced apart along a second direction, and each of the active regions extending along a first direction; The trench isolation structure includes a first trench isolation structure and a second trench isolation structure. The first trench isolation structure is located on both sides of the plurality of active regions in the first direction, and the second trench isolation structure is located on both sides of each of the active regions in the second direction. A MOS device is formed in the plurality of active regions; wherein, when the MOS device is an NMOS, the first trench isolation structure and the second trench isolation structure are used to apply tensile stress to the plurality of active regions; when the MOS device is a PMOS, the first trench isolation structure is used to apply compressive stress to the plurality of active regions, and the second trench isolation structure is used to apply tensile stress to the plurality of active regions; wherein, the first direction is perpendicular to the second direction, the first direction is the channel length direction, and the second direction is the channel width direction.
10. The method for manufacturing a semiconductor device as described in claim 9, characterized in that, When the MOS device is an NMOS, the step of forming a trench isolation structure in the substrate includes: Simultaneously, a first trench and a second trench are formed in the substrate; A liner layer is formed on the inner walls of the first trench and the second trench; An insulating layer is filled in the first trench and the second trench. The first trench isolation structure includes the padding layer and the insulating layer in the first trench, and the second trench isolation structure includes the padding layer and the insulating layer in the second trench. When the MOS device is a PMOS, the step of forming a trench isolation structure in the substrate includes: A first trench is formed in the substrate; A first liner layer is formed on the inner wall of the first trench; A first insulating layer is filled in the first trench, and the first trench isolation structure includes the first liner layer and the first insulating layer; A second trench is formed in the substrate; A second liner layer is formed on the inner wall of the second trench; A second insulating layer is filled into the second trench, and the second trench isolation structure includes the second liner layer and the second insulating layer.
11. The method for manufacturing a semiconductor device as described in claim 10, characterized in that, When the MOS device is an NMOS, the insulating layer is formed using the HARP deposition process; when the MOS device is a PMOS, the first insulating layer is formed using the HDP deposition process, and the second insulating layer is formed using the HARP deposition process.