A method and semiconductor structure for suppressing metal diffusion in through-silicon vias during thinning processes.
By forming a porous metal adsorption layer on the surface of through-silicon vias (TSVs), the leakage current problem caused by metal diffusion in TSVs was solved, thus improving device yield.
Patent Information
- Application Number
- CN202511736049.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-24
- Publication Date
- 2026-11-17
AI Technical Summary
During wafer thinning, the metal material in the through-silicon via is exposed on the back side of the wafer due to process reasons. This causes metal atoms to diffuse along lattice defects to the active region of the device, resulting in leakage current and reducing device yield.
After wafer thinning, a porous metal adsorption layer is formed on the surface of the through-silicon via (TSV). The diffused metal atoms or ions are fixed by physical and chemical adsorption, preventing them from migrating to the active region of the device.
This effectively reduces the risk of metal diffusion into the active region of the device, improves device performance, and increases product yield.
Smart Images

Figure CN123124780A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, and more specifically to a method and semiconductor structure for suppressing metal diffusion in through-silicon vias during thinning processes. Background Technology
[0002] In the manufacturing process of memory chips (such as 3D stacked memory devices), wafer bonding and through-silicon via (TSV) technologies are typically used to achieve vertical interconnects between multiple wafers. This process involves thinning a wafer that has completed its front-end fabrication, and then stacking and bonding multiple thinned wafers together. The TSV structure runs through the wafer and is responsible for transmitting electrical signals between different layers, making it one of the key technologies for achieving high-density integration and high-performance memory.
[0003] However, during wafer thinning, the metal material filled in the TSV is partially exposed on the back side of the wafer due to processes such as grinding, polishing, or etching. Because the thinning process introduces numerous lattice defects, such as dislocations, microcracks, and other types of crystal damage, into the back side and near-surface regions of the wafer, these defects provide pathways for rapid diffusion of metal atoms. Metal atoms diffuse along these lattice defects into the active region of the device, particularly into the depletion region of the PN junction (e.g., the depletion region between the N-type well and the P-type substrate), introducing deep-level defect centers in the semiconductor band gap. These deep-level defects enhance carrier generation and recombination rates, leading to a significant amount of additional leakage current in the depletion region under reverse bias. This leakage phenomenon causes severe degradation of device performance and reduces device yield. Summary of the Invention
[0004] The summary section introduces a series of simplified concepts, which will be further explained in detail in the detailed description section. The summary section of this invention is not intended to limit the key features and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution.
[0005] To address the existing problems, one embodiment of the present invention provides a method for suppressing metal diffusion in through-silicon vias during the thinning process, the method comprising: A first wafer is provided, the first wafer including a semiconductor substrate of a first doping type, at least one through-silicon via embedded in the semiconductor substrate, and at least one well region of a second doping type formed in the semiconductor substrate, the well region being formed on the front side of the first wafer; The back side of the first wafer is subjected to a substrate thinning process so that the end of the through-silicon via protrudes from the thinned back side. An insulating liner layer is formed on the thinned back side, and the insulating liner layer conformally covers the surface of the semiconductor substrate and the through silicon via; A conformal metal adsorption layer is formed on the surface of the insulating liner layer. The metal adsorption layer is made of a porous material and is used to adsorb and diffuse metal atoms or ions. A bonding dielectric layer is formed covering the metal adsorption layer, wherein the lowest height of the upper surface of the bonding dielectric layer is greater than or equal to the end face height of the through silicon via; A planarization process is used to remove portions of the bonding dielectric layer, the metal adsorption layer, and the insulating liner layer to expose the ends of the through-silicon vias.
[0006] In one embodiment, the porous material comprises alumina.
[0007] In one embodiment, the thickness of the metal adsorption layer is 68 Å-118 Å.
[0008] In one embodiment, the through-silicon via includes a barrier layer and a conductive pillar formed within the space enclosed by the barrier layer, and the planarization process further includes removing a portion of the barrier layer and exposing the conductive pillar.
[0009] In one embodiment, providing the first wafer includes: Provide a semiconductor substrate of the first doping type; The front side of the semiconductor substrate is subjected to global ion implantation of the first doping type; At least one well region of a second doping type is formed on the front side of the semiconductor substrate, wherein the implantation depth of the global ion implantation of the first doping type is greater than the depth of the well region of the second doping type, and the implantation dose of the global ion implantation of the first doping type is less than the implantation dose of the well region of the second doping type.
[0010] In one embodiment, at least one well region of a first doping type is further formed on the front side of the semiconductor substrate, wherein the implantation dose of the first doping type global ion implantation is less than the implantation dose of the first doping type well region, and the implantation depth of the first doping type global ion implantation is greater than the depth of the first doping type well region.
[0011] In one embodiment, the first doping type is P-type, the second doping type is N-type, and the implanted ion for global ion implantation of the first doping type is boron ion.
[0012] In one embodiment, the implantation energy of the first doped type of global ion implantation is 250K-800K, and the implantation dose of the first doped type of global ion implantation is 5E11 ion / cm². 2-6E12 ion / cm 2 .
[0013] In one embodiment, the insulating liner layer is formed using atomic layer deposition (ALD), the metal adsorption layer is formed using ALD, and the bonding medium layer is formed using chemical vapor deposition (CVD). Both the insulating liner layer and the bonding dielectric layer are made of silicon oxide.
[0014] Another aspect of this invention provides a semiconductor structure, the semiconductor structure comprising: The first wafer after back-side thinning includes a semiconductor substrate of a first doping type, wherein at least one well region of a second doping type is formed in the semiconductor substrate, and the well region of the second doping type is located on the front side of the first wafer; wherein the first wafer also includes at least one through-silicon via embedded in the semiconductor substrate, and the end of the through-silicon via protrudes from the surface of the semiconductor substrate of the first wafer after back-side thinning. A bonding dielectric layer is formed on the back side of the first wafer, and the surface of the bonding dielectric layer is flush with the end face of the through silicon via. An insulating liner and a metal adsorption layer are located between the through-silicon via and the bonding dielectric layer, wherein the insulating liner is located between the metal adsorption layer and the through-silicon via; wherein the metal adsorption layer is made of a porous material for adsorbing and diffusing metal atoms or ions.
[0015] The method and semiconductor structure for suppressing metal diffusion in through-silicon vias (TSVs) during the wafer thinning process provided by the present invention introduce a porous metal adsorption layer to actively adsorb and fix metal ions or metal atoms diffused from the TSV after wafer thinning, effectively reducing the risk of their migration to the active region of the device, thereby helping to improve the device leakage problem caused by metal contamination and improve product yield. Attached Figure Description
[0016] The following drawings, which are incorporated herein by reference as part of this invention, are provided for understanding the invention. The drawings illustrate embodiments of the invention and their descriptions, serving to explain the principles of the invention.
[0017] In the attached image: Figures 1A to 1I A cross-sectional schematic diagram of the device obtained by sequentially performing each step of the manufacturing method of the semiconductor structure in the related art is shown; Figure 2 A schematic flowchart of a method for suppressing metal diffusion in through-silicon vias during a thinning process, according to a specific embodiment of the present invention, is shown. Figures 3A to 3JThe diagram shows a cross-sectional view of a device obtained by sequentially implementing each step of a method for suppressing metal diffusion in a through-silicon via (TSV) thinning process according to a specific embodiment of the present invention. Detailed Implementation
[0018] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of the invention. However, it will be apparent to those skilled in the art that the invention can be practiced without one or more of these details. In other instances, certain technical features well-known in the art have not been described in order to avoid obscuring the invention.
[0019] It should be understood that the invention can be embodied in various forms and should not be construed as being limited to the embodiments set forth herein. Rather, providing these embodiments will make the disclosure thorough and complete, and will fully convey the scope of the invention to those skilled in the art. In the drawings, for clarity, the dimensions and relative dimensions of layers and regions may be exaggerated. The same reference numerals denote the same elements throughout.
[0020] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this invention, the first element, component, area, layer, or portion discussed below may be referred to as the second element, component, area, layer, or portion.
[0021] Spatial relation terms such as “below,” “under,” “below,” “below,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “below” other elements or features will be oriented “above” other elements or features. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.
[0022] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the invention. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0023] Reference Figures 1A-1I One method for manufacturing a semiconductor device in related technologies includes: firstly, as shown in the figure... Figure 1A As shown, a first wafer is provided, the first wafer including a semiconductor substrate 100 of a first doping type, and a shallow trench isolation structure 101 is formed on the front side of the semiconductor substrate 100; then as... Figure 1B As shown, ion implantation of a first doping type is performed on the front side of the semiconductor substrate 100 to form a first doping type well region 102; then as... Figure 1C As shown, ion implantation of a second doping type is performed on the front side of the semiconductor substrate 100 to form a second doping type well region 103. Next, a through-silicon via is formed through the semiconductor substrate 100.
[0024] After the front-end processes are completed, the back side of the first wafer undergoes a thinning process. Firstly, as... Figure 1D As shown, the back side of the first wafer is rapidly thinned using processes such as wet etching and polishing. It should be noted that before rapid thinning, the back side of the first wafer is first heavily doped, and the resulting doped layer serves as a stop layer in the thinning process, such as wet etching. Then, as... Figure 1E As shown, a chemical mechanical polishing process is performed to expose the end face of the through-silicon via 104, and finally as... Figure 1FAs shown, a portion of the substrate material around the through-silicon via 104 is removed using a wet etching process until the end of the through-silicon via 104 protrudes beyond the back surface of the thinned first wafer. Then, as... Figure 1G As shown, an insulating liner layer 105 is formed on the back side of the thinned first wafer. Then, as... Figure 1H As shown, a bonding dielectric layer 106 is formed covering the insulating liner layer 105. Finally, as... Figure 1I The bonding dielectric layer 106 is planarized to expose the through-silicon via 104.
[0025] After the back side of the first wafer is thinned, there are defects on the back side of the first wafer. Metal atoms or ions exposed on the end face of the through-silicon via 104 will diffuse along the defects on the back side. When the diffused metal atoms or ions enter the depletion region of the PN junction between the second doped type well region 103 and the semiconductor substrate 100 (e.g., the depletion region between the N-type well region and the P-type substrate), a deep energy level will be introduced in the middle of the energy band, thereby providing a large number of charge carriers through recombination-generation, causing the device leakage current to increase exponentially and reducing the device yield.
[0026] In view of the aforementioned technical problems, embodiments of the present invention propose a method for suppressing metal diffusion in through-silicon vias during the thinning process. The following refers to... Figures 2 to 3J The manufacturing method of the present invention will be described in detail below, wherein, Figure 2 A schematic flowchart of a method for suppressing metal diffusion in through-silicon vias during a thinning process, according to a specific embodiment of the present invention, is shown. Figures 3A to 3J The diagram shows a cross-sectional view of a device obtained by sequentially implementing each step of a method for suppressing metal diffusion in a through-silicon via (TSV) thinning process according to a specific embodiment of the present invention.
[0027] First, step S201 is executed, providing the first wafer 300, such as... Figure 3A As shown.
[0028] The first wafer includes a semiconductor substrate 300. The semiconductor substrate 300 is made of at least one of the following materials: silicon (Si), germanium (Ge), silicon germanium (SiGe), silicon carbide (SiC), silicon germanium carbide (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP), or other III / V compound semiconductors; or it is silicon-on-dielectric (SOI), silicon-on-dielectric (SSOI), silicon-on-dielectric (S-SiGeOI), silicon-on-dielectric (SiGeOI), and germanium-on-dielectric (GeOI). The semiconductor substrate 300 is doped with a first doping type, which in this embodiment is p-type, i.e., doped with a trivalent element (such as boron).
[0029] For example, a shallow trench isolation structure 301 is formed on the front side of the semiconductor substrate 300 to define the active region. In forming the shallow trench isolation structure 301, a masking film layer is first formed on the semiconductor substrate 300. Trenches are then etched on the front side of the semiconductor substrate 300 using photolithography and etching processes. The trenches are filled with an insulating dielectric, and then excess insulating dielectric is removed by chemical mechanical polishing, thereby forming the shallow trench isolation structure 301. The region surrounded by the shallow trench isolation structure 301 is the active region.
[0030] Next, as Figure 3A As shown, a first type of doping, blanket implantation, is performed on the front side of the semiconductor substrate 300, meaning it does not distinguish between N-type and P-type regions. This step aims to form a lower concentration but deeper doped region inside the semiconductor substrate 300, thereby shortening the PN junction between the second type of doped well region and the first type of doped substrate, reducing the possibility of metal diffusion into the depletion region. Blanket implantation can also be applied to the PN junction between the deep N-well (DNW) and the P-type substrate, avoiding leakage caused by the exposure of the DNW after thinning, and enhancing the compatibility of 3D thinning processes and DNW.
[0031] To achieve deeper junction depths, boron (B) ions are preferred for global ion implantation. Due to their light weight and small atomic radius, boron ions have a lower probability of large-angle collisions with silicon lattice atoms during implantation, resulting in slower energy loss and thus enabling deeper implantation depths. For example, the specific process parameters for ion implantation are: implantation energy ranging from 250 keV to 800 keV, and implantation dose ranging from 5E11 ions / cm². 2 Up to 6E12 ion / cm 2 between.
[0032] After global ion implantation, a well region is formed on the front side of the semiconductor substrate 300. Specifically, as... Figure 3C As shown, at least one well region 303 of the second doped type is formed, and optionally a well region 302 of the first doped type is formed, as shown. Figure 3BAs shown. The second-doped well region 303 is, for example, an N-type well region (NW), whose main function is to form a local N-type region on the P-type substrate for manufacturing devices such as NMOS transistors; similarly, the first-doped well region 302 is, for example, a P-type well region (PW) for manufacturing PMOS transistors. The depth of the second-doped well region 303 is less than the implantation depth of the first-doped global ion implantation, and the implantation dose of the second-doped well region 303 is greater than the implantation dose of the first-doped global ion implantation. Similarly, the depth of the first-doped well region 302 is less than the implantation depth of the first-doped global ion implantation, and the implantation dose of the first-doped well region 302 is greater than the implantation dose of the first-doped global ion implantation. Under the action of global ion implantation, the concentration of the first-doped ions in the semiconductor substrate 300 is increased, which reduces the width of the depletion region between the second-doped well region 303 and the semiconductor substrate 300, thereby reducing the possibility of metal atoms or ions diffusing into the depletion region between the second-doped well region 303 and the semiconductor substrate 300.
[0033] At least one through-silicon via 304 penetrating the semiconductor substrate 300 is also formed in the first wafer, such as Figure 3D As shown. Through-silicon vias (TSVs) 304 are used to achieve three-dimensional integration. Their manufacturing process may include: etching vias on a semiconductor substrate 300; depositing a barrier layer 304B, such as TiN or TaN, within the vias; then filling the vias with a conductive material (such as tungsten or copper) through processes such as electroplating to form conductive pillars 304A; and finally removing excess metal from the surface of the semiconductor substrate 300 through surface planarization treatment (such as chemical mechanical polishing (CMP)) to achieve planarization. Therefore, a TSV 304 typically includes a barrier layer 304B and conductive pillars 304A formed within the space enclosed by the barrier layer 304B.
[0034] Next, step S202 is performed to perform a substrate thinning process on the back side of the first wafer so that the end of the through-silicon via 304 protrudes from the thinned back side.
[0035] The purpose of substrate thinning is to reduce the thickness of the wafer to meet the dimensional requirements of vertical interconnects and improve heat dissipation. Thinning processes typically involve a combination of multiple processes; for example, a substrate thinning process includes: firstly, as... Figure 3D As shown, a rapid, high-thickness removal process is performed on the back side of the first wafer using a heavily doped wet etching and grinding method; then, as... Figure 3E As shown, a chemical mechanical polishing (CMP) process is performed to expose the end face of the through-silicon via 304, and finally as... Figure 3FAs shown, a portion of the substrate material around the through-silicon via 304 is removed by a wet etching process until the end of the through-silicon via 304 protrudes from the back side of the thinned first wafer.
[0036] Then, step S203 is executed, as follows: Figure 3G As shown, an insulating liner layer 305 is formed on the back side of the thinned first wafer, and the insulating liner layer 305 conformally covers the surface of the semiconductor substrate 300 and the through silicon via 304.
[0037] Here, conformal coverage refers to the ability of the deposited insulating liner layer 305 to uniformly and conformally cover the patterned structure on the back side of the first wafer. The insulating liner layer 305 maintains a substantially consistent thickness on the top, sidewalls, and back side of the exposed semiconductor substrate 300 of the through-silicon via 304. The material of the insulating liner layer 305 includes, but is not limited to, silicon oxide, and it is formed using atomic layer deposition (ALD) technology. ALD technology, with its self-limiting surface reaction mechanism, can achieve pore-free, highly conformal thin film coverage on hole structures with large aspect ratios.
[0038] Then, step S204 is performed to form a conformal metal adsorption layer 306 covering the surface of the insulating liner layer 305. The metal adsorption layer 306 is made of a porous material and is used to adsorb metal atoms or ions diffused from the silicon through-hole 304.
[0039] In traditional approaches, attempts are typically made to block metal diffusion by fabricating a dense, defect-free barrier layer. However, after wafer thinning, the metal in the TSV is exposed on the back side of the wafer, and diffusion occurs along lattice defects and stress lines generated by the thinning process. A single dense film is insufficient to completely block all diffusion paths.
[0040] In contrast, this embodiment of the invention uses a porous material as the metal adsorption layer 306. The porous material contains numerous nanoscale pores and channels, giving it a larger specific surface area and thus providing orders of magnitude more adsorption sites for capturing diffused metal atoms or ions. Metal atoms or ions diffuse under concentration gradients or stress-driven conditions. When they enter the channels of the porous material, they are bound to the inner walls of the channels by van der Waals forces or electrostatic interactions, thus losing their propulsion.
[0041] The metal adsorption layer 106 is preferably porous alumina (Al2O3) formed by atomic layer deposition (ALD). Porous alumina not only physically adsorbs metal atoms or ions, but its surface also contains numerous unsaturated bonds (dangling bonds) and active functional groups (such as -OH groups). These active sites can interact with metal atoms or ions to form stable chemical bonds, thereby preventing the metal atoms or ions from escaping again and effectively capturing and adsorbing copper and other metal atoms or ions diffused from the through-silicon vias 304. Exemplarily, the thickness of the metal adsorption layer is between 68 Å and 118 Å.
[0042] Next, step S205 is performed to form a bonding dielectric layer 307 covering the metal adsorption layer 306, wherein the lowest height of the upper surface of the bonding dielectric layer 307 is greater than or equal to the end face height of the through silicon via 304.
[0043] The bonding dielectric layer 307 serves to encapsulate and protect the underlying structure while providing the necessary dielectric surface for bonding. The minimum height of the upper surface of the bonding dielectric layer 307 is greater than or equal to the end face height of the through-silicon via 304. This is to ensure that the conductive ends of the through-silicon via 304 are completely buried under the bonding dielectric layer 307 before subsequent chemical mechanical polishing, and to ensure that after polishing, a flat bonding surface is formed in which the ends of all through-silicon vias 304 are on the same plane as the bonding dielectric layer 307.
[0044] The material of the bonding dielectric layer 307 includes, but is not limited to, silicon oxide. Considering deposition rate and process cost, this step can employ chemical vapor deposition (CVD). The insulating liner layer 305 and metal adsorption layer 306 deposited prior to ALD provide a relatively flat substrate for the CVD process, ensuring that the bonding dielectric layer 307 can continuously cover without defects. Its deposition thickness must ensure that the minimum height of the upper surface is greater than or equal to the end face height of the protruding silicon via 304, meaning that the bonding dielectric layer 307 completely fills the recessed area between adjacent silicon vias 304.
[0045] Finally, step S206 is performed, a planarization process is carried out to remove part of the bonding dielectric layer 307, the metal adsorption layer 306 and the insulating liner layer 305 to expose the end of the through silicon via 304.
[0046] The planarization process specifically includes chemical mechanical polishing (CMP). Through the synergistic effect of chemical etching and mechanical abrasion, CMP can grind the surfaces of different materials, such as the bonding dielectric layer 307, the metal adsorption layer 306, and the insulating liner layer 305, to the same height. It also includes removing part of the barrier layer 304B and exposing the conductive pillars 304A of the through-silicon via 304. After CMP treatment, the surface of the bonding dielectric layer 307 and the end face of the conductive pillars 304A achieve global planarity, forming a flat bonding interface.
[0047] This completes the process steps for implementing the method of suppressing metal diffusion in through-silicon vias during the thinning process according to an embodiment of the present invention. The back side processing of the first wafer is now complete, and it can be used for bonding with the second wafer. It is understood that the method of suppressing metal diffusion in through-silicon vias during the thinning process of this embodiment includes not only the steps described above, but may also include other necessary steps before, during, or after the above steps, all of which are included within the scope of the manufacturing method of this embodiment.
[0048] After the wafer thinning process is completed, certain microscopic lattice defects, such as dislocations and microcracks, will form on the back side due to mechanical stress and processing damage. These defects constitute channels for metal atoms or ions escaping from the exposed through-silicon vias 304 to diffuse into the active region of the device. In this embodiment of the invention, a metal adsorption layer 306 is formed on the back side of the thinned first wafer, such that the metal adsorption layer 306 laterally penetrates around all the through-silicon vias 304. When metal atoms or ions in the through-silicon vias 304 diffuse laterally along the defects on the back side of the wafer, the metal adsorption layer 306 physically captures the metal atoms or ions through its porous structure and forms stable chemical bonds with the metal elements through surface active sites. Through this mechanism, the metal adsorption layer 306 can effectively intercept and fix metal atoms or ions in their diffusion path before they further penetrate into the semiconductor substrate 300 and reach the PN junction, thereby fundamentally avoiding metal-induced leakage.
[0049] This invention also provides a semiconductor structure, which can be prepared by the methods described in the foregoing embodiments, but is not limited thereto.
[0050] The semiconductor structure of the present invention will be described in detail below. It is worth mentioning that, in order to avoid repetition, only a brief description will be given for the same components and structures as in the foregoing embodiments. For specific explanations and descriptions, please refer to the description in Embodiment 1.
[0051] Specifically, such as Figure 3C and Figure 3JAs shown, the semiconductor structure of this embodiment includes: a first wafer after back-side thinning, the first wafer including a semiconductor substrate 300 of a first doping type, at least one well region 303 of a second doping type formed in the semiconductor substrate 300, the well region 303 of the second doping type being located on the front side of the first wafer; wherein, the first wafer also includes at least one through-silicon via 304 embedded in the semiconductor substrate 300, the end of the through-silicon via 304 protruding from the surface of the semiconductor substrate 300 of the first wafer after back-side thinning; a bonding dielectric layer 307 formed on the back side of the first wafer, and the surface of the bonding dielectric layer 307 being flush with the end face of the through-silicon via 304; an insulating liner layer 305 and a metal adsorption layer 306 located between the through-silicon via 304 and the bonding dielectric layer 307, wherein the insulating liner layer 305 is located between the metal adsorption layer 306 and the through-silicon via 304; wherein, the metal adsorption layer 306 is made of a porous material and is used to adsorb diffused metal atoms or ions from the through-silicon via 304.
[0052] In one embodiment, the porous material comprises alumina.
[0053] In one embodiment, a first-doped well region 302 is also formed in the semiconductor substrate 300, the depth of which is greater than the depth of the second-doped well region 303. The different junction depths are due to global ion implantation, as detailed above.
[0054] The semiconductor structure of this invention introduces a porous metal adsorption layer, which actively adsorbs and fixes metal ions or metal atoms diffused from the TSV after wafer thinning, effectively reducing the risk of their migration to the active region of the device. This helps to improve the device leakage problem caused by metal contamination and improve product yield.
[0055] The present invention has been described through the above embodiments. However, it should be understood that the above embodiments are for illustrative purposes only and are not intended to limit the invention to the scope of the described embodiments. Furthermore, those skilled in the art will understand that the present invention is not limited to the above embodiments, and many more variations and modifications can be made based on the teachings of the present invention, all of which fall within the scope of protection claimed by the present invention. The scope of protection of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for suppressing metal diffusion in through-silicon vias during a thinning process, characterized in that, The method includes: A first wafer is provided, the first wafer including a semiconductor substrate of a first doping type, at least one through-silicon via embedded in the semiconductor substrate, and at least one well region of a second doping type formed in the semiconductor substrate, the well region being formed on the front side of the first wafer; The back side of the first wafer is subjected to a substrate thinning process so that the end of the through-silicon via protrudes from the thinned back side. An insulating liner layer is formed on the thinned back side, and the insulating liner layer conformally covers the surface of the semiconductor substrate and the through silicon via; A conformal metal adsorption layer is formed on the surface of the insulating liner layer. The metal adsorption layer is made of a porous material and is used to adsorb and diffuse metal atoms or ions. A bonding dielectric layer is formed covering the metal adsorption layer, wherein the lowest height of the upper surface of the bonding dielectric layer is greater than or equal to the end face height of the through silicon via; A planarization process is used to remove portions of the bonding dielectric layer, the metal adsorption layer, and the insulating liner layer to expose the ends of the through-silicon vias.
2. The method according to claim 1, characterized in that, The porous material includes alumina.
3. The method according to claim 1, characterized in that, The thickness of the metal adsorption layer is 68 Å-118 Å.
4. The method according to claim 1, characterized in that, The through-silicon via includes a barrier layer and conductive pillars formed within the space enclosed by the barrier layer. The planarization process further includes removing a portion of the barrier layer and exposing the conductive pillars.
5. The method according to claim 1, characterized in that, The provision of the first wafer includes: Provide a semiconductor substrate of the first doping type; The front side of the semiconductor substrate is subjected to global ion implantation of the first doping type; At least one well region of a second doping type is formed on the front side of the semiconductor substrate, wherein the implantation depth of the global ion implantation of the first doping type is greater than the depth of the well region of the second doping type, and the implantation dose of the global ion implantation of the first doping type is less than the implantation dose of the well region of the second doping type.
6. The method according to claim 5, characterized in that, At least one well region of a first doping type is also formed on the front side of the semiconductor substrate, wherein the implantation dose of the first doping type global ion implantation is less than the implantation dose of the first doping type well region, and the implantation depth of the first doping type global ion implantation is greater than the depth of the first doping type well region.
7. The method according to claim 5, characterized in that, The first doping type is P-type, the second doping type is N-type, and the implanted ion for global ion implantation of the first doping type is boron ion.
8. The method according to claim 7, characterized in that, The implantation energy for the first type of global ion implantation is 250K-800K, and the implantation dose is 5E11 ion / cm². 2 -6E12ion / cm 2 .
9. The method according to claim 1, characterized in that, The insulating liner layer is formed using atomic layer deposition (ALD), the metal adsorption layer is formed using ALD, and the bonding medium layer is formed using chemical vapor deposition (CVD). Both the insulating liner layer and the bonding dielectric layer are made of silicon oxide.
10. A semiconductor structure, characterized in that, The semiconductor structure includes: The first wafer after back-side thinning includes a semiconductor substrate of a first doping type, wherein at least one well region of a second doping type is formed in the semiconductor substrate, and the well region of the second doping type is located on the front side of the first wafer; wherein the first wafer also includes at least one through-silicon via embedded in the semiconductor substrate, and the end of the through-silicon via protrudes from the surface of the semiconductor substrate of the first wafer after back-side thinning. A bonding dielectric layer is formed on the back side of the first wafer, and the surface of the bonding dielectric layer is flush with the end face of the through silicon via. An insulating liner and a metal adsorption layer are located between the through-silicon via and the bonding dielectric layer, wherein the insulating liner is located between the metal adsorption layer and the through-silicon via; wherein the metal adsorption layer is made of a porous material for adsorbing and diffusing metal atoms or ions.