Semiconductor devices and their manufacturing methods

By forming a first dielectric layer and a stop layer on the substrate, and then etching and filling the second dielectric layer, the problem of uneven thickness of metal interconnect structures in 3D stacking processes is solved, thereby increasing the etching process window and improving process stability.

CN123124783APending Publication Date: 2026-11-17WUHAN XINXIN SEMICON MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611415885.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-11
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In 3D stacking processes, the planarization of the metal interconnect structure leads to large differences in the thickness of the silicon oxide layer at different locations of the top metal interconnect layer, affecting the etching process window and process stability.

Method used

By forming a first dielectric layer and a stop layer on the substrate, etching to form an opening and filling the second dielectric layer, and performing a planarization process with the removal rate of the second dielectric layer being greater than the removal rate of the stop layer, the stability of the planarization process is ensured.

Benefits of technology

This increases the etching process window, improves process stability, reduces thickness differences at different locations in the metal layer, and ensures the uniformity and reliability of the conductive plug vias.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124783A_ABST
    Figure CN123124783A_ABST
Patent Text Reader

Abstract

This invention provides a semiconductor device and a method for manufacturing the same. The method includes: providing a substrate with a metal layer formed on its surface; forming a first dielectric layer and a stop layer sequentially stacked on the metal layer; etching the stop layer, the first dielectric layer, and the metal layer to form an opening exposing the substrate; forming a second dielectric layer covering the stop layer and filling the opening; performing a planarization process, stopping at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer. This invention enables an increase in the etching process window and improves process stability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a semiconductor device and its manufacturing method. Background Technology

[0002] A metal interconnect structure is formed in the substrate, and in the 3D stacking process, a conductive structure in the bonding layer or a conductive structure in the redistribution layer is further fabricated on the metal interconnect structure. Both the metal interconnect structure and the conductive structure include at least one conductive plug and at least one metal interconnect layer that are alternately electrically connected.

[0003] Taking 3D stacking technology as an example, after forming the top metal interconnect layer in the metal interconnect structure, a silicon oxide layer is formed on the top metal interconnect layer and in the openings within it, and then the silicon oxide layer is planarized. However, because the silicon oxide layer is removed very quickly during planarization, even slight differences in the planarization conditions (such as the concentration of the polishing slurry) at different locations on the top metal interconnect layer can lead to significant differences in the thickness of the silicon oxide layer removed at different locations. This results in a large variation in the remaining thickness of the silicon oxide layer at different locations after planarization, causing a narrow etching window and poor process stability when subsequently etching the remaining silicon oxide layer to form multiple vias containing multiple conductive plugs in the conductive structure. Summary of the Invention

[0004] The purpose of this invention is to provide a semiconductor device and a method for manufacturing the same, which enables an increase in the etching process window and improves process stability.

[0005] To achieve the above objectives, the present invention provides a method for manufacturing a semiconductor device, comprising:

[0006] A substrate is provided, wherein a metal layer is formed on the surface of the substrate;

[0007] A first dielectric layer and a stop layer are sequentially stacked on the metal layer;

[0008] The stop layer, the first dielectric layer, and the metal layer are etched to form an opening that exposes the substrate;

[0009] A second dielectric layer is formed to cover the stop layer and fill the opening;

[0010] A planarization process is performed and stopped at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

[0011] Optionally, a hard mask layer is formed to cover the stop layer before etching the stop layer; the opening extends through the hard mask layer.

[0012] Optionally, the steps of performing the planarization process include:

[0013] A first chemical mechanical polishing process is performed to remove a portion of the second dielectric layer;

[0014] Perform a back-etching process or a second chemical mechanical polishing process to remove the remaining thickness of the second dielectric layer on the stop layer, and stop at the stop layer.

[0015] Optionally, the thickness of the second dielectric layer removed by the first chemical mechanical polishing process is greater than the thickness of the second dielectric layer removed by the etch-back process or the second chemical mechanical polishing process, and the removal rate of the second dielectric layer during the first chemical mechanical polishing process is greater than the removal rate of the second dielectric layer during the etch-back process or the second chemical mechanical polishing process.

[0016] Optionally, the second medium layer fills the portion of the opening to form an air gap, the top of which is lower than the top surface of the stop layer.

[0017] Optionally, the material of the second dielectric layer includes silicon oxide, and the material of the stop layer includes silicon nitride or titanium nitride.

[0018] Optionally, the method for manufacturing the semiconductor device further includes:

[0019] A third dielectric layer is formed to cover the stop layer and the second dielectric layer filling the opening to form a passivation layer, the passivation layer comprising the first dielectric layer, the stop layer and the third dielectric layer located above the metal layer.

[0020] The present invention also provides a semiconductor device, comprising:

[0021] A substrate, wherein a first metal interconnect layer is provided on the surface of the substrate at intervals, and a first dielectric layer and a stop layer are sequentially covering the first metal interconnect layer;

[0022] The second dielectric layer penetrates the stop layer and the first dielectric layer, corresponding to the gap between adjacent first metal interconnect layers, and fills the gap. The top surface of the second dielectric layer is flush with the top surface of the stop layer. The removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

[0023] Optionally, an air gap is formed in the second dielectric layer, the top of which is lower than the top surface of the stop layer.

[0024] Optionally, the material of the second dielectric layer includes silicon oxide, and the material of the stop layer includes silicon nitride or titanium nitride.

[0025] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0026] 1. A method for manufacturing a semiconductor device according to the present invention includes: providing a substrate, wherein a metal layer is formed on the surface of the substrate; forming a first dielectric layer and a stop layer sequentially stacked on the metal layer; etching the stop layer, the first dielectric layer, and the metal layer to form an opening exposing the substrate; forming a second dielectric layer to cover the stop layer and fill the opening; performing a planarization process and stopping at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer. This allows for an increase in the etching process window and improves process stability.

[0027] 2. The semiconductor device of the present invention includes: a substrate, on the surface of which a first metal interconnect layer is disposed at intervals and a first dielectric layer and a stop layer sequentially covering the first metal interconnect layer; a second dielectric layer, which penetrates the stop layer and the first dielectric layer and fills the gaps between adjacent first metal interconnect layers, and the top surface of the second dielectric layer is flush with the top surface of the stop layer; and the removal rate of the second dielectric layer is greater than the removal rate of the stop layer. This allows for an increase in the etching process window and improves process stability. Attached Figure Description

[0028] Figure 1 This is a flowchart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;

[0029] Figures 2a-2g yes Figure 1 A schematic diagram of the semiconductor device manufacturing method shown.

[0030] Among them, the appendix Figures 1-2g The annotations in the attached figures are explained as follows:

[0031] 10-Substrate; 101-Substrate; 102-Interlayer dielectric layer; 103-Metal interconnect structure; 1031-Metal interconnect layer; 1032-Conductive plug; 11-Metal layer; 111-First metal interconnect layer; 112-Gap; 12-First dielectric layer; 13-Stop layer; 14-Hard mask layer; 15-Opening; 16-Second dielectric layer; 161-Air gap; 17-Third dielectric layer. Detailed Implementation

[0032] To make the objectives, advantages, and features of the present invention clearer, the semiconductor device and its manufacturing method proposed in this invention will be further described in detail below with reference to the accompanying drawings. It should be noted that the drawings are all in a very simplified form and use non-precise proportions, and are only used to facilitate and clarify the illustration of the embodiments of the present invention.

[0033] One embodiment of the present invention provides a method for manufacturing a semiconductor device, see reference. Figure 1 , Figure 1 This is a flowchart of a method for manufacturing a semiconductor device according to an embodiment of the present invention, the method comprising:

[0034] Step S1: Provide a substrate, wherein a metal layer is formed on the surface of the substrate;

[0035] Step S2: Form a first dielectric layer and a stop layer, which are sequentially stacked on the metal layer;

[0036] Step S3: Etch the stop layer, the first dielectric layer, and the metal layer to form an opening that exposes the substrate;

[0037] Step S4: Form a second dielectric layer to cover the stop layer and fill the opening;

[0038] Step S5: Perform a planarization process and stop at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

[0039] See below. Figures 2a-2g The manufacturing method of the semiconductor device provided in this embodiment will be described in more detail.

[0040] Following step S1, as follows Figure 2a As shown, a substrate 10 is provided, and a metal layer 11 is formed on the surface of the substrate 10.

[0041] In one embodiment, the substrate 10 includes a substrate 101 and an interlayer dielectric layer 102 formed on the substrate 101, wherein a metal interconnect structure 103 is formed in the interlayer dielectric layer 102.

[0042] In one embodiment, the interlayer dielectric layer 102 includes at least one insulating layer, the metal interconnect structure 103 includes at least one metal interconnect layer 1031 and at least one conductive plug 1032, the metal interconnect layer 1031 and the conductive plug 1032 are alternately electrically connected, and the metal layer 11 is electrically connected to the metal interconnect layer 1031 through the conductive plug 1032.

[0043] In one embodiment, the metal layer 11 is used to fabricate a first metal interconnect layer 111, which is part of the metal interconnect structure 103. The first metal interconnect layer 111 is either the top or middle layer of the metal interconnect structure 103.

[0044] In other embodiments, no metal interconnect structure 103 is formed in the interlayer dielectric layer 102, and the first metal interconnect layer 111 is the bottom metal interconnect layer 1031.

[0045] Following step S2, as Figure 2b As shown, a first dielectric layer 12 and a stop layer 13 are formed and sequentially cover the metal layer 11.

[0046] The material of the first dielectric layer 12 may include insulating materials such as silicon oxide or silicon oxynitride.

[0047] Following step S3, as follows Figure 2c As shown, the stop layer 13, the first dielectric layer 12 and the metal layer 11 are etched to form an opening 15 that exposes the substrate 10.

[0048] In one embodiment, after etching the metal layer 11, first metal interconnect layers 111 are formed at intervals. The first metal interconnect layers 111 are the top metal interconnect layer 1031 of the metal interconnect structure 103. In other embodiments, the first metal interconnect layers 111 are the middle or bottom metal interconnect layers 1031 of the metal interconnect structure 103. The portion of the opening 15 that penetrates the metal layer 11 corresponds to the gap 112 between adjacent first metal interconnect layers 111.

[0049] In one embodiment, such as Figure 2b As shown, a hard mask layer 14 is formed to cover the stop layer 13 before etching the stop layer 13; as Figure 2c As shown, the opening 15 penetrates the hard mask layer 14, that is, the hard mask layer 14 is used as a mask to etch the stop layer 13, the first dielectric layer 12 and the metal layer 11.

[0050] According to step S4, as Figure 2d As shown, a second dielectric layer 16 is formed, which covers the stop layer 13 and fills the opening 15.

[0051] In one embodiment, the second dielectric layer 16 fills a portion of the opening 15 to form an air gap 161, the top of which is lower than the top surface of the stop layer 13. This utilizes the extremely low dielectric constant of the air in the air gap 161 to significantly reduce the parasitic capacitance between the metal interconnect structures 103, thereby reducing chip dynamic power consumption and improving signal transmission speed. In other embodiments, the second dielectric layer 16 fills the opening 15, but no air gap 161 is formed in the portion of the second dielectric layer 16 located in the opening 15.

[0052] Taking the second dielectric layer 16 filling the portion of the opening 15 to form the air gap 161 as an example, in one embodiment, the step of forming the second dielectric layer 16 includes: forming a first silicon oxide layer on the inner wall of the opening 15 and the top surface of the stop layer 13 using an atomic layer deposition process; depositing a second silicon oxide layer on the first silicon oxide layer using TEOS (tetraethyl orthosilicate) as a silicon source, taking advantage of the faster growth of TEOS at the top and corners of the opening 15, so that the second silicon oxide layer is sealed in advance to form the air gap 161, wherein the second dielectric layer 16 includes the first silicon oxide layer and the second silicon oxide layer.

[0053] In one embodiment, a recess A1 is formed on the top surface of the second dielectric layer 16 above the opening 15.

[0054] Following step S5, as follows Figure 2e and Figure 2f As shown, a planarization process is performed and stopped at the stop layer 13; wherein, during the planarization process, the removal rate of the second dielectric layer 16 is greater than the removal rate of the stop layer 13.

[0055] During the planarization process, the hard mask layer 14 and the second dielectric layer 16 stacked on the stop layer 13 are removed, and the stop layer 13 is either partially removed or not removed at all.

[0056] In one embodiment, the removal rate of the hard mask layer 14 is greater than the removal rate of the stop layer 13.

[0057] That is, the etching selectivity ratio or polishing selectivity ratio of the second dielectric layer 16 to the stop layer 13 is high, and the etching selectivity ratio or polishing selectivity ratio of the hard mask layer 14 to the stop layer 13 is also high. In one embodiment, the etching selectivity ratio or polishing selectivity ratio of the second dielectric layer 16 and the hard mask layer 14 to the stop layer 13 is greater than or equal to 10:1.

[0058] In one embodiment, the second dielectric layer 16 is made of silicon oxide, the hard mask layer 14 is made of silicon oxide, and the stop layer 13 is made of silicon nitride or titanium nitride.

[0059] In one embodiment, the air gap 161 remains closed after the planarization process is performed.

[0060] In one embodiment, the step of performing the planarization process includes:

[0061] like Figure 2e As shown, a first chemical mechanical polishing process is performed to remove a portion of the thickness of the second dielectric layer 16;

[0062] like Figure 2f As shown, a back etching process or a second chemical mechanical polishing process is performed to remove the remaining thickness of the second dielectric layer 16 on the stop layer 13, and the process stops at the stop layer 13.

[0063] In one embodiment, the thickness of the second dielectric layer 16 removed by the first chemical mechanical polishing process is greater than the thickness of the second dielectric layer 16 removed by the etch-back process or the second chemical mechanical polishing process. The removal rate of the second dielectric layer 16 during the first chemical mechanical polishing process is greater than the removal rate of the second dielectric layer 16 during the etch-back process or the second chemical mechanical polishing process. The removal rate of the second dielectric layer 16 during the etch-back process or the second chemical mechanical polishing process is greater than the removal rate of the stop layer 13. This allows for rapid removal of the second dielectric layer 16 on the stop layer 13 while accurately stopping the process on the stop layer 13.

[0064] In other embodiments, the hard mask layer 14 is formed on the stop layer 13. The second dielectric layer 16 on the stop layer 13 is removed during the first chemical mechanical polishing process, and the hard mask layer 14 on the stop layer 13 is removed during the etch-back process or the second chemical mechanical polishing process; or, the second dielectric layer 16 and a portion of the hard mask layer 14 on the stop layer 13 are removed during the first chemical mechanical polishing process, and the remaining thickness of the hard mask layer 14 on the stop layer 13 is removed during the etch-back process or the second chemical mechanical polishing process.

[0065] In one embodiment, after performing the first chemical mechanical polishing process, the depth of the depression A1 becomes shallower, and after performing the back etching process or the second chemical mechanical polishing process, the depression A1 is removed; or, after performing the first chemical mechanical polishing process, the depression A1 is removed.

[0066] In one embodiment, such as Figure 2g As shown, the method of manufacturing the semiconductor device further includes: forming a third dielectric layer 17 to cover the stop layer 13 and the second dielectric layer 16 filled in the opening 15 to form a passivation layer, the passivation layer including the first dielectric layer 12, the stop layer 13 and the third dielectric layer 17 located above the first metal interconnect layer 111.

[0067] The material of the third dielectric layer 17 includes insulating materials such as silicon oxide, silicon oxynitride, or silicon nitride.

[0068] In one embodiment, when the first metal interconnect layer 111 is the top metal interconnect layer 1301, the method for manufacturing the semiconductor device further includes: etching the third dielectric layer 17, the stop layer 13, and the first dielectric layer 12 covering the first metal interconnect layer 111 to form a plurality of vias (not shown) exposing the first metal interconnect layer 111; and filling the vias with metal material to form a plurality of conductive plugs. The conductive plugs may be part of a bonding layer or redistribution layer that is subsequently fabricated on the metal interconnect structure 103 in a 3D stacking process.

[0069] Alternatively, in another embodiment, when the first metal interconnect layer 111 is the bottom or intermediate metal interconnect layer 1301, the method for manufacturing the semiconductor device further includes: etching the stop layer 13 and the first dielectric layer 12 covering the first metal interconnect layer 111 to form a plurality of vias (not shown) exposing the first metal interconnect layer 111, and filling the vias with metal material to form a plurality of conductive plugs. The conductive plugs may be part of the metal interconnect structure 103.

[0070] As can be seen from the above, the semiconductor device manufacturing method provided by the present invention involves forming a first dielectric layer and a stop layer sequentially stacked on the metal layer; etching the stop layer, the first dielectric layer, and the metal layer to form an opening exposing the substrate; forming a second dielectric layer to cover the stop layer and fill the opening; performing a planarization process and stopping at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer, so that even if there are slight differences in the conditions (e.g., the concentration of polishing slurry or etching slurry) of the planarization process above different locations of the etched metal layer (i.e., the first metal interconnect layer), the stop layer at different locations of the etched metal layer can be prevented from causing the stop layer to be exposed. The significant differences in the thickness of the removed stop layer reduce the remaining thickness variation of the stop layer at different locations of the etched metal layer after the planarization process. This improves the uniformity of the total thickness of the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) at different locations of the etched metal layer. Consequently, when etching the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) to form multiple vias containing multiple conductive plugs, each via can penetrate the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) simultaneously as much as possible. This increases the etching process window and improves process stability.

[0071] An embodiment of the present invention provides a semiconductor device, comprising: a substrate, wherein a first metal interconnect layer is disposed on the surface of the substrate at intervals and a first dielectric layer and a stop layer are sequentially covering the first metal interconnect layer; a second dielectric layer, wherein the stop layer and the first dielectric layer penetrate the gap between adjacent first metal interconnect layers and fill the gap, the top surface of the second dielectric layer is flush with the top surface of the stop layer; and the removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

[0072] See below. Figure 2g The semiconductor device provided in this embodiment will be described in more detail.

[0073] The substrate 10 has a first metal interconnect layer 111 spaced apart and a first dielectric layer 12 and a stop layer 13 sequentially covering the first metal interconnect layer 111.

[0074] In one embodiment, the substrate 10 includes a substrate 101 and an interlayer dielectric layer 102 formed on the substrate 101, wherein a metal interconnect structure 103 is formed in the interlayer dielectric layer 102.

[0075] In one embodiment, the interlayer dielectric layer 102 includes at least one insulating layer, and the metal interconnect structure 103 includes at least one metal interconnect layer 1031 and at least one conductive plug 1032. The metal interconnect layer 1031 and the conductive plug 1032 are alternately electrically connected, and the first metal interconnect layer 111 is electrically connected to the metal interconnect layer 1031 through the conductive plug 1032.

[0076] In one embodiment, the first metal interconnect layer 111 is part of the metal interconnect structure 103. Specifically, the first metal interconnect layer 111 is either the top or middle layer of the metal interconnect structure 103.

[0077] In other embodiments, the first metal interconnect layer 111 is used as the bottom metal interconnect layer 1031 in the metal interconnect structure 103.

[0078] The material of the first dielectric layer 12 may include insulating materials such as silicon oxide or silicon oxynitride.

[0079] The second dielectric layer 16 corresponds to the gap between the adjacent first metal interconnect layer 111 (i.e.) Figure 2c The gap 112 shown penetrates the stop layer 13 and the first dielectric layer 12, and fills the gap 112. The top surface of the second dielectric layer 16 is flush with the top surface of the stop layer 13. The removal rate of the second dielectric layer 16 is greater than the removal rate of the stop layer 13. Here, "flush" means that the height difference between the top surface of the second dielectric layer 16 and the top surface of the stop layer 13 is 0.

[0080] The etching selectivity or polishing selectivity of the second dielectric layer 16 to the stop layer 13 is high. In one embodiment, the etching selectivity or polishing selectivity of the second dielectric layer 16 to the stop layer 13 is greater than or equal to 10:1.

[0081] In one embodiment, the second dielectric layer 16 is made of silicon oxide, and the stop layer 13 is made of silicon nitride or titanium nitride.

[0082] In one embodiment, an air gap 161 is formed in the second dielectric layer 16, the top of which is lower than the top surface of the stop layer 13. This utilizes the extremely low dielectric constant of the air in the air gap 161 to significantly reduce the parasitic capacitance between the metal interconnect structures 103, thereby reducing dynamic power consumption and improving signal transmission speed. In other embodiments, no air gap 161 is formed in the second dielectric layer 16, and the second dielectric layer 16 fills the opening 15.

[0083] In one embodiment, the semiconductor device further includes a third dielectric layer 17 covering the stop layer 13 and the second dielectric layer 16 to form a passivation layer, the passivation layer including the first dielectric layer 12, the stop layer 13 and the third dielectric layer 17 covering the first metal interconnect layer 111.

[0084] In one embodiment, when the first metal interconnect layer 111 is the top metal interconnect layer 1301, a plurality of vias (not shown) are formed in the third dielectric layer 17, the stop layer 13, and the first dielectric layer 12 above the first metal interconnect layer 111, exposing the first metal interconnect layer 111. Conductive plugs are formed in the vias. The conductive plugs can be part of a bonding layer or redistribution layer that is subsequently fabricated on the metal interconnect structure 103 in a 3D stacking process.

[0085] Alternatively, in another embodiment, when the first metal interconnect layer 111 is the bottom or intermediate metal interconnect layer 1301, a plurality of vias (not shown) are formed in the stop layer 13 and the first dielectric layer 12 above the first metal interconnect layer 111 to expose the first metal interconnect layer 111, and conductive plugs are formed in the vias. The conductive plugs may be part of the metal interconnect structure 103.

[0086] As can be seen from the above, the semiconductor device provided by the present invention has a first metal interconnect layer spaced apart on the substrate surface, and a first dielectric layer and a stop layer sequentially covering the first metal interconnect layer; a second dielectric layer, corresponding to the gap between adjacent first metal interconnect layers, penetrates the stop layer and the first dielectric layer and fills the gap; the removal rate of the second dielectric layer is greater than the removal rate of the stop layer, so that when the planarization process is performed to make the top surface of the second dielectric layer flush with the top surface of the stop layer, even if there are slight differences in the conditions of the planarization process (e.g., the concentration of polishing slurry or etching slurry) above different positions of the first metal interconnect layer, the stop layer at different positions of the first metal interconnect layer can be prevented from being damaged. The significant differences in the thickness removed reduce the remaining thickness difference of the stop layer at different locations of the first metal interconnect layer after the planarization process. This improves the uniformity of the total thickness of the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) at different locations of the first metal interconnect layer. Consequently, when etching the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) to form multiple vias containing multiple conductive plugs, each via can penetrate the first dielectric and the stop layer (or the first dielectric, the stop layer, and the third dielectric layer) simultaneously as much as possible. This increases the etching process window and improves process stability.

[0087] The above description is merely a description of preferred embodiments of the present invention and is not intended to limit the scope of the present invention in any way. Any changes or modifications made by those skilled in the art based on the above disclosure shall fall within the protection scope of the claims.

Claims

1. A method for manufacturing a semiconductor device, characterized in that, include: A substrate is provided, wherein a metal layer is formed on the surface of the substrate; A first dielectric layer and a stop layer are sequentially stacked on the metal layer; The stop layer, the first dielectric layer, and the metal layer are etched to form an opening that exposes the substrate; A second dielectric layer is formed to cover the stop layer and fill the opening; A planarization process is performed and stopped at the stop layer; wherein, during the planarization process, the removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

2. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, Before etching the stop layer, a hard mask layer is formed to cover the stop layer; the opening extends through the hard mask layer.

3. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The steps of performing the planarization process include: A first chemical mechanical polishing process is performed to remove a portion of the second dielectric layer; Perform a back-etching process or a second chemical mechanical polishing process to remove the remaining thickness of the second dielectric layer on the stop layer, and stop at the stop layer.

4. The method for manufacturing a semiconductor device as described in claim 3, characterized in that, The thickness of the second dielectric layer removed by the first chemical mechanical polishing process is greater than the thickness of the second dielectric layer removed by the etch-back process or the second chemical mechanical polishing process, and the removal rate of the second dielectric layer during the first chemical mechanical polishing process is greater than the removal rate of the second dielectric layer during the etch-back process or the second chemical mechanical polishing process.

5. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The second medium layer fills the portion of the opening to form an air gap, the top of which is lower than the top surface of the stop layer.

6. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The material of the second dielectric layer includes silicon oxide, and the material of the stop layer includes silicon nitride or titanium nitride.

7. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The method for manufacturing the semiconductor device further includes: A third dielectric layer is formed to cover the stop layer and the second dielectric layer filling the opening to form a passivation layer, the passivation layer comprising the first dielectric layer, the stop layer and the third dielectric layer located above the metal layer.

8. A semiconductor device, characterized in that, include: A substrate, wherein a first metal interconnect layer is provided on the surface of the substrate at intervals, and a first dielectric layer and a stop layer are sequentially covering the first metal interconnect layer; The second dielectric layer penetrates the stop layer and the first dielectric layer, corresponding to the gap between adjacent first metal interconnect layers, and fills the gap. The top surface of the second dielectric layer is flush with the top surface of the stop layer. The removal rate of the second dielectric layer is greater than the removal rate of the stop layer.

9. The semiconductor device as claimed in claim 8, characterized in that, An air gap is formed in the second medium layer, and the top of the air gap is lower than the top surface of the stop layer.

10. The semiconductor device as claimed in claim 8, characterized in that, The material of the second dielectric layer includes silicon oxide, and the material of the stop layer includes silicon nitride or titanium nitride.