Selective metallization manufacturing method for glass through-holes in ultrasound brain-computer interface chips

By using dry film lithography and selective electroplating to fill holes, the problems of signal attenuation and mass production consistency in the metallization process of ultrasonic brain-computer interface chips have been solved. This has enabled efficient ultrasonic signal transmission and low-resistance interconnection, simplified the production process, and improved yield and cost-effectiveness.

CN123124819APending Publication Date: 2026-11-17BEIJING ZIYIXIN INTEGRATED CIRCUIT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611226827.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-13
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing glass through-hole metallization processes for ultrasound brain-computer interface chips suffer from problems such as indiscriminate metallization leading to ultrasound signal attenuation, poor metal masking accuracy, lengthy process flow, and insufficient mass production consistency.

Method used

Dry film photolithography is used to precisely mask the ultrasonic penetration window area. Only the outer glass vias are deposited with titanium/copper seed layers and selectively electroplated to fill the vias. Combined with femtosecond laser etching and precise photolithography patterning, a continuous conductive layer is formed, and excess seed layers are removed by micro-etching.

Benefits of technology

This technology achieves a metal-free ultrasonic penetration window, ensuring efficient ultrasonic signal transmission, low single-hole on-resistance, high batch yield, simplified process flow, and reduced production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124819A_ABST
    Figure CN123124819A_ABST
Patent Text Reader

Abstract

This invention discloses a method for selective metallization of glass vias in ultrasound brain-computer interface (BCI) chips. The method includes: providing a glass substrate with a central region serving as a high-fidelity ultrasound transmission window and a peripheral region containing glass vias; attaching a dry film photoresist and photolithographically patterning it so that the photoresist completely covers the transmission window, exposing the glass vias; sputtering a titanium / copper composite seed layer; electroplating copper to fill the glass vias while the dry film photoresist covers the transmission window; and peeling off the dry film photoresist and micro-etching to remove excess seed layer from the periphery. This invention precisely masks the transmission window with dry film photoresist and selectively electroplats TGV only on the periphery, ensuring the transmission window is free of metal plating throughout, eliminating ultrasound signal reflection attenuation, and reducing transmission loss to no more than 0.5 dB; the TGV dense filling results in a conduction resistance of no more than 0.08 ohms, achieving a mass production yield of no less than 95%, making it suitable for mass production of ultrasound BCI chips.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor packaging technology applications, specifically to a method for selective metallization of glass vias in ultrasonic brain-computer interface chips. Background Technology

[0002] Ultrasonic brain-computer interfaces (BCIs) are a cutting-edge technology that utilizes the physical properties of ultrasound to read and write brain activity signals, combining non-invasiveness, high spatial resolution, and deep penetration capabilities. The ultrasound BCI chip relies on ultrasound signals penetrating a glass substrate to acquire intracranial neural signals and transmit external stimulation signals. The substrate also integrates numerous through-glass vias (TGVs) as electrical signal interconnection channels.

[0003] Current TGV metallization processes typically employ a combination of whole-board sputtering and electroplating to simultaneously deposit a copper metal layer over the entire substrate, followed by photolithography etching to remove the metal layer from specific areas. This process suffers from the following drawbacks when applied to ultrasound brain-computer interface chips: First, the indiscriminate metallization of the entire area results in the deposition of a copper metal layer in the high-fidelity ultrasonic transmission window region. The copper layer significantly attenuates the ultrasonic transmission efficiency, leading to high ultrasonic signal loss and a reduced signal-to-noise ratio. If subsequent etching is used to remove the metal in the transmission window, defects such as over-etching, damage to the substrate glass surface, thinning of the copper layer on the sidewalls of the vias, or even open circuits are likely to occur, resulting in low yield.

[0004] Secondly, the method of using metal masks to shield the ultrasonic window suffers from poor zonal shielding accuracy. Gaps exist between the metal mask and the glass substrate, allowing electroplating solution to seep in and form impure copper plating at the edge of the penetration window, creating an ultrasonic scattering interface that interferes with ultrasonic beam focusing. Furthermore, rigid metal masks cannot adapt to the curved surfaces or microstructures of ultra-thin glass substrates, resulting in significant mask alignment deviations during mass production.

[0005] Third, the traditional step-by-step etching process for metal removal has poor compatibility, requiring multiple photolithography and etching steps after sputtering, resulting in a lengthy process and high manufacturing costs in cleanrooms. Furthermore, the micro-etching step after full coverage of the titanium-copper seed layer easily corrodes the conductive sidewalls of the vias, leading to excessive TGV on-resistance.

[0006] Fourth, the aforementioned issues lead to insufficient consistency in mass production. Ultrasonic brain-computer interface (BCI) chips require no metal residue in the ultrasound penetration window, while the surrounding TGV vias must be completely and densely filled with copper. Current processes struggle to simultaneously meet both of these requirements. Small-batch development is feasible, but mass production yields are typically below 70%. Summary of the Invention

[0007] To solve the above-mentioned technical problems, the present invention provides a The technical solution of this invention is: a method for selective metallization of glass vias in an ultrasound brain-computer interface chip, comprising the following steps: A glass substrate is provided, the glass substrate having a central region and a peripheral region, the central region being an ultrasonic high-fidelity transmission window, and the peripheral region having a glass through-hole penetrating the glass substrate; A dry film photoresist is attached to the surface of the glass substrate, and the dry film photoresist is completely covered by the ultrasonic high-fidelity transmission window by photolithography patterning, thus exposing the glass through-hole. A titanium / copper composite seed layer is sputtered onto the surface of the glass substrate, so that the seed layer covers the inner wall of the glass via and the surface of the dry film photoresist, forming a continuous conductive layer; While the dry film photoresist is covering the ultrasonic high-fidelity penetration window, copper is electroplated into the glass through-hole to fill the glass through-hole with copper. All of the dry film photoresist is stripped off, and excess seed layer in the peripheral area is removed by micro-etching.

[0008] Furthermore, the glass substrate is a symmetrical composite glass substrate, including a glass core layer and a composite buffer layer disposed on the upper and lower surfaces of the glass core layer. The composite buffer layer is made of an organosilicon composite material with a thickness of 5-15 μm and is disposed in the peripheral area.

[0009] Furthermore, the thickness of the glass core layer is 0.15-0.3 mm; The ultrasonic high-fidelity penetration window is either a circular or rectangular penetration window.

[0010] Furthermore, the dry film photoresist is a positive anti-electroplating type dry film photoresist with a thickness of 15-20μm, and is bonded by vacuum hot pressing at a bonding temperature of 85-95℃. The exposure energy for the photolithographic patterning process is 130-160 mJ / cm², the developer is a 1.5%-2% sodium carbonate solution, and the developing temperature is 29-30℃.

[0011] Furthermore, the titanium / copper composite seed layer comprises a titanium layer and a copper seed layer disposed on the surface of the titanium layer. The thickness of the titanium layer is 60-80 nm, and the thickness of the copper seed layer is 160-200 nm. The seed layer is formed by magnetron sputtering with a sputtering vacuum degree ≤3×10⁻⁶. -3 Pa.

[0012] Furthermore, the copper plating filling is performed using a copper sulfate system plating solution, which contains 200 g / L copper sulfate, 100 g / L sulfuric acid, and 65 ppm chloride ions. The plating temperature is 25°C, and the current density is 1-1.2 A / dm².

[0013] Furthermore, stripping all of the dry film photoresist and micro-etching to remove the excess seed layer in the peripheral area includes: stripping the dry film photoresist with sodium hydroxide solution, removing the excess copper seed layer with copper micro-etching solution, and rinsing to remove the titanium layer with hydrofluoric acid solution. The concentration of the sodium hydroxide solution is 3.5%-4%, and the peeling temperature is 42-45℃.

[0014] Furthermore, the glass via is formed by femtosecond laser etching, with a diameter of 15-30 μm and an aspect ratio of 3:1 to 4:1; The inner wall of the glass through-hole is roughened by hydrofluoric acid, and the surface roughness Ra is 0.3-0.5μm.

[0015] Furthermore, the alignment deviation of the pattern in the photolithographic patterning process is ≤ ±3μm.

[0016] Furthermore, it also includes the detection steps: The area of ​​the ultrasonic high-fidelity transmission window was examined under a 1000x optical microscope, confirming the absence of titanium and copper metal particles. The conductivity resistance of the glass through-hole was tested, and it was confirmed that the single-hole conductivity resistance was ≤0.08Ω; the ultrasonic transmission loss was tested to be ≤0.5dB, and the batch yield was ≥95%.

[0017] The beneficial technical effects of this invention are: 1. By precisely masking the ultrasonic transmission window area through dry film photolithography, only the exposed TGV vias on the periphery are deposited with titanium / copper seed layers and selectively electroplated to fill the vias, so that the ultrasonic transmission window is free of titanium and copper metal plating throughout, eliminating the reflection and attenuation of ultrasonic signals by the metal layer.

[0018] 2. While shielding the penetration window, dense copper filling of the TGV via is achieved, and the single-hole conduction resistance can be controlled within 0.08Ω, meeting the requirements of low resistance and high reliability for high-density micro-interconnects in brain-computer interfaces.

[0019] 3. Compared with the traditional solution of etching away metal after full metallization, it eliminates multiple photolithography and etching processes, resulting in a shorter process flow, shorter production cycle, and reduced micro-nano processing costs.

[0020] 4. The dry film photoresist adheres tightly, eliminating the problem of electroplating solution seepage at the edges, and effectively avoiding defects such as copper spurs at the electroplating edges, excessive corrosion of the glass substrate, and copper layer loss on the sidewalls of through holes.

[0021] The above description is merely an overview of the technical solution of the present invention. In order to better understand the technical means of the present invention and to implement it in accordance with the contents of the specification, the preferred embodiments of the present invention are described in detail below with reference to the accompanying drawings. Attached Figure Description

[0022] Figure 1 This is a schematic diagram of the process flow of the present invention; Figure 2 This is a schematic diagram of the structure of the glass through-hole located in the glass substrate according to the present invention; Figure 3 This is a schematic diagram of the structure of the positive anti-electroplation dry film photoresist of the present invention located on a glass substrate; Figure 4 This is a schematic diagram of the exposure and development process of the present invention; Figure 5 This is a schematic diagram of a glass substrate after sputtering of the titanium / copper composite seed layer according to the present invention; Figure 6 This is a schematic diagram of the glass substrate in the electroplated copper state according to the present invention; Figure 7 This is a schematic diagram of the product structure of the present invention; Figure 8 This is a top view of the present invention.

[0023] The attached figures are labeled as follows: 100. Glass substrate; 110. High-fidelity transmission window; 120. Upper composite buffer layer; 130. Glass core layer; 140. Lower composite buffer layer; 200. Glass through-hole; 210. Titanium layer; 220. Copper seed layer; 230. Through-hole copper plating; 300. Dry film photoresist; 400. Heating roller; 500. Soluble anode. Detailed Implementation

[0024] In order to better understand the technical means of the present invention and to implement it in accordance with the contents of the specification, the specific embodiments of the present invention will be further described in detail below with reference to the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0025] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such use of data can be interchanged where appropriate for the embodiments of this application described herein.

[0026] In the description of this invention, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship described in the embodiments and shown in the accompanying drawings, or the orientation or positional relationship that the product of this invention is usually placed in during use. They are only for the convenience of describing this invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limiting this invention. Example 1

[0027] This embodiment 1 provides a method for selective metallization of glass vias in a wearable ultrasound brain-computer interface chip, comprising: like Figure 1 and Figure 2 As shown, a symmetrical composite glass substrate 100 is selected. This substrate has a three-layer stacked structure, including a glass core layer 130, an upper composite buffer layer 120 disposed on the upper surface of the glass core layer 130, and a lower composite buffer layer 140 disposed on the lower surface of the glass core layer 130. The upper composite buffer layer 120 and the lower composite buffer layer 140 are made of silicone composite material, each with a thickness of 10 μm, and are only disposed in the peripheral area of ​​the substrate. The thickness of the glass core layer 130 is 0.3 mm, and the central area of ​​the substrate has a circular ultrasonic high-fidelity transmission window 110 with a diameter of 4 mm. An array of glass vias 200 (TGV) with a diameter of 30 μm and a depth-to-width ratio of 3:1 is formed in the peripheral area using a femtosecond laser. Then, hydrofluoric acid is used to roughen the inner wall of the vias to achieve a surface roughness Ra of 0.5 μm.

[0028] like Figure 1 and Figure 3 As shown, a 20 μm thick positive anti-plating dry film photoresist 300 was attached to the surface of the substrate after the through-hole fabrication was completed. The attachment was performed by vacuum hot pressing at a temperature of 95℃, a pressure of 0.6 MPa, and a bonding speed of 1.5 m / min. After bonding, the substrate was left to stand for 15 minutes to eliminate air bubbles.

[0029] like Figure 3 As shown, the glass substrate 100 is placed in the cavity using a vacuum adsorption stage. The positive anti-electroplating dry film photoresist 300 is fed onto one side and collected from the other. When the positive anti-electroplating dry film photoresist 300 is bonded to the glass substrate 100, it is uniformly hot-pressed by a heating roller 400 to ensure proper bonding. During this process, a vacuum is required inside the cavity.

[0030] like Figure 1 and Figure 4 As shown, the dry film photoresist 300 was then patterned using photolithography. The ultrasonic high-fidelity transmission window 110 area was masked, and ultraviolet exposure was performed at an exposure energy of 160 mJ / cm², with a 2% sodium carbonate solution as the developer and a development temperature of 30°C. After development, it was rinsed with pure water and dried. After this treatment, the dry film photoresist 300 completely covered the ultrasonic high-fidelity transmission window 110 area, while the glass vias 200 in the peripheral area were exposed, with a pattern alignment deviation of 2 μm.

[0031] like Figure 4As shown, the glass substrate is aligned and loaded, and a custom photomask is placed on it. The photomask is divided into a shielding area, corresponding to the ultrasonic high-fidelity transmission window 110, and an opening area, corresponding to all the peripheral glass vias 200. Uniform exposure with ultraviolet parallel light exposes the dry film of the peripheral glass vias 200. In addition, the ultraviolet parallel light is a single-sided horizontal exposure process.

[0032] After exposure, let stand for 5 minutes to complete the photochemical reaction; at this time, rinse with a spray-type sodium carbonate developer, which is the top rinse, to dissolve and remove the photosensitive dry film in the outer area, while the dry film through the window is completely preserved.

[0033] like Figure 1 and Figure 5 As shown, magnetron sputtering deposition of a titanium / copper composite seed layer was then performed. The glass substrate was placed in a vacuum-sealed chamber, and the sputtering vacuum level in the vacuum-sealed chamber was controlled at 3 × 10⁻⁶. -3 Pa, once everything is ready, first deposit a titanium layer 210 with a thickness of 80 nm, then deposit a copper seed layer 220 with a thickness of 200 nm. During the sputtering process, the seed layer is deposited not only on the inner wall of the exposed glass via 200, but also on the surface of the dry film photoresist 300, forming a continuous conductive film on the surface.

[0034] The primary purpose of depositing the titanium layer first is to provide adhesion for the copper seed layer.

[0035] like Figure 1 and Figure 6 As shown, the dry film photoresist 300 was kept covering the ultrasonic high-fidelity penetration window 110, and copper electroplating was performed directly on the exposed glass vias 200. The electroplating solution used a copper sulfate system, with a copper sulfate content of 200 g / L, a sulfuric acid content of 100 g / L, and a chloride ion content of 65 ppm. The electroplating temperature was 25℃. The current density was set to 1.2 A / dm², and after continuous electroplating for 60 minutes, all glass vias 200 were completely filled with copper, forming a copper-plated via 230 without voids or depressions.

[0036] like Figure 6 As shown, the glass substrate 100 is placed in an electroplating tank by a carrier. The electroplating tank also contains a soluble anode 500 and is filled with copper sulfate electroplating solution. A constant current is provided by a power supply. During the electroplating process, the copper sulfate electroplating solution is continuously circulated and filtered. The glass through holes are filled with copper sulfate electroplating solution, and finally, through-hole copper 230 is formed.

[0037] like Figure 1 and Figure 7As shown, after electroplating, the residual copper sulfate plating solution on the surface of the glass substrate 100 is removed, and it is dried with nitrogen. After drying, all the dry film photoresist 300 is peeled off. Then, the peripheral area is micro-etched: first, the dry film photoresist 300 is peeled off by spraying with a 4% sodium hydroxide solution at 45°C, then copper micro-etching solution is used to etch for 60 seconds to remove the excess copper seed layer 220 in the non-through-hole areas of the peripheral area, and finally, the titanium layer 210 is removed by rinsing with dilute hydrofluoric acid.

[0038] like Figure 7 and Figure 8 As shown, the performance of the finished product obtained in this embodiment was tested: no titanium or copper metal particles were found in the ultrasonic high-fidelity transmission window 110 area under a 1000x optical microscope, and the ultrasonic transmission loss was 0.38dB; the single-hole conduction resistance in the glass through-hole 200 was 0.06Ω; the batch yield was 96.2%; after 1000 cycles of high and low temperature from -40℃ to 125℃, the copper layer showed no peeling or breakage. Example 2

[0039] This embodiment provides a method for selective metallization of glass vias in the fabrication of a miniature implantable ultrasound brain-computer interface chip.

[0040] The difference from Example 1 is as follows: Regarding the substrate, the thickness of the glass core layer 130 is 0.15 mm, the thickness of the upper composite buffer layer 120 and the lower composite buffer layer 140 are each 6 μm, the ultrasonic high-fidelity transmission window 110 is rectangular with dimensions of 2 mm × 2 mm, the glass via 200 formed by femtosecond laser etching has a diameter of 15 μm and an aspect ratio of 4:1, and the surface roughness Ra of the inner wall of the via is 0.3 μm after roughening. The dry film photoresist 300 is a 15 μm thick positive ultrathin anti-electroplating dry film. The vacuum hot pressing temperature is adjusted to 85℃, the pressure to 0.5 MPa, the bonding speed to 1.2 m / min, and the resting time to 10 min. The exposure energy for photolithography patterning is 130 mJ / cm², the developer is a 1.5% sodium carbonate solution, the developing temperature is 29℃, and the pattern alignment accuracy is 2.5 μm. In the titanium / copper composite seed layer, the titanium layer 210 has a thickness of 60 nm, and the copper seed layer 220 has a thickness of 160 nm. The current density for copper plating to fill the vias was reduced to 1.0 A / dm², and the plating time was 45 min. The stripping process was performed using a 3.5% sodium hydroxide solution at 42°C, and the micro-etching time was 40 s. The remaining process steps and conditions were the same as in Example 1.

[0041] The performance of the finished product obtained in this embodiment was tested: no titanium or copper metal particles were found in the ultrasonic high-fidelity transmission window 110 area under a 1000x optical microscope, and the ultrasonic transmission loss was 0.42dB; the single-hole conduction resistance in the glass through-hole 200 was 0.07Ω; the yield of the small-size substrate was 94.8%; and no metal detachment occurred after damp heat aging.

[0042] The above embodiments are merely specific implementations of the present invention, used to illustrate the technical solutions of the present invention, and are not intended to limit it. The scope of protection of the present invention is not limited thereto. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that any person skilled in the art can still modify or easily conceive of changes to the technical solutions described in the foregoing embodiments within the scope of the technology disclosed in the present invention, or make equivalent substitutions for some of the technical features; and these modifications, changes, or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should all be covered within the scope of protection of the present invention.

Claims

1. A method for glass via selective metallization fabrication for ultrasonic brain-machine chip, characterized in that, Includes the following steps: A glass substrate is provided, the glass substrate having a central region and a peripheral region, the central region being an ultrasonic high-fidelity transmission window, and the peripheral region having a glass through-hole penetrating the glass substrate; A dry film photoresist is attached to the surface of the glass substrate, and the dry film photoresist is completely covered by the ultrasonic high-fidelity transmission window by photolithography patterning, thus exposing the glass through-hole. A titanium / copper composite seed layer is sputtered onto the surface of the glass substrate, so that the seed layer covers the inner wall of the glass via and the surface of the dry film photoresist, forming a continuous conductive layer; While the dry film photoresist is covering the ultrasonic high-fidelity penetration window, copper is electroplated into the glass through-hole to fill the glass through-hole with copper. All of the dry film photoresist is stripped off, and excess seed layer in the peripheral area is removed by micro-etching.

2. The method for glass via selective metallization manufacturing for ultrasonic brain-machine chip according to claim 1, wherein, The glass substrate is a symmetrical composite glass substrate, including a glass core layer and a composite buffer layer disposed on the upper and lower surfaces of the glass core layer. The composite buffer layer is made of an organosilicon composite material with a thickness of 5-15 μm and is disposed in the peripheral area.

3. The method for glass via selective metallization manufacturing for ultrasonic brain-machine chip according to claim 2, characterized in that, The thickness of the glass core layer is 0.15-0.3 mm; The ultrasonic high-fidelity penetration window is either a circular or rectangular penetration window.

4. The method for glass via selective metallization of an ultrasonic brain-machine chip according to claim 1, wherein, The dry film photoresist is a positive anti-electroplating type dry film photoresist with a thickness of 15-20μm, which is bonded by vacuum hot pressing at a bonding temperature of 85-95℃. The exposure energy for the photolithographic patterning process is 130-160 mJ / cm², the developer is a 1.5%-2% sodium carbonate solution, and the developing temperature is 29-30℃.

5. The method for glass via selective metallization of an ultrasonic brain-machine chip according to claim 1, wherein, The titanium / copper composite seed layer comprises a titanium layer and a copper seed layer disposed on the surface of the titanium layer. The thickness of the titanium layer is 60-80 nm, and the thickness of the copper seed layer is 160-200 nm. The seed layer is formed by magnetron sputtering with a sputtering vacuum degree ≤3×10⁻⁶. -3 Pa.

6. The method for glass via selective metallization of an ultrasonic brain-machine chip according to claim 1, wherein, The copper plating filling method uses a copper sulfate system plating solution containing 200g / L copper sulfate, 100g / L sulfuric acid, and 65ppm chloride ions. The plating temperature is 25℃ and the current density is 1-1.2A / dm².

7. The method for selective metallization of glass vias for use in ultrasonic brain-computer interface chips according to claim 1, characterized in that, The process of stripping all the dry film photoresist and micro-etching to remove the excess seed layer in the peripheral area includes: stripping the dry film photoresist with sodium hydroxide solution, removing the excess copper seed layer with copper micro-etching solution, and rinsing with hydrofluoric acid solution to remove the titanium layer. The concentration of the sodium hydroxide solution is 3.5%-4%, and the peeling temperature is 42-45℃.

8. The method for glass via selective metallization fabrication for ultrasonic brain-machine chip according to claim 1, wherein, The glass via is formed by femtosecond laser etching, with a diameter of 15-30 μm and a depth-to-width ratio of 3:1 to 4:

1. The inner wall of the glass through-hole is roughened by hydrofluoric acid, and the surface roughness Ra is 0.3-0.5μm.

9. The method for glass via selective metallization of ultrasonic brain-machine chip according to claim 1, wherein, The alignment deviation of the pattern in the photolithography patterning process is ≤ ±3μm.

10. The method for glass via selective metallization fabrication for ultrasonic brain-machine chip according to claim 1, wherein, It also includes the detection steps: The area of ​​the ultrasonic high-fidelity transmission window was examined under a 1000x optical microscope, confirming the absence of titanium and copper metal particles. The conductivity resistance of the glass through-hole was tested, and it was confirmed that the single-hole conductivity resistance was ≤0.08Ω; The ultrasonic transmission loss is ≤0.5dB, and the batch yield is ≥95%.