Manufacturing methods for one-piece molded bodies and multi-piece packaging bodies
By designing a one-piece molded body with the gate located at the center of the container forming area, and combining injection molding and stretch blow molding, the problems of thin-walled formability and material waste of multi-piece packaging bodies are solved, and the manufacturing of multi-piece packaging bodies with uniform wall thickness is realized.
Patent Information
- Application Number
- CN202480091191.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-04-25
- Filing Date
- 2024-11-15
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, the manufacturing method of multi-piece packaging has the problems of poor thin-wall injection molding and material waste. In particular, the container part of the previous multi-piece packaging was cut out from a continuous roll, resulting in the waste of the part that is not used as a container. The injection molding method is difficult to form thin-walled containers.
It adopts a one-piece molding design with multiple container forming areas, flange forming areas and connecting parts. The gate is located in the center of the container forming area. Multiple packaging parts are manufactured by injection molding and stretch blow molding to ensure excellent injection molding performance and reduce uneven wall thickness.
It achieves excellent thin-wall injection molding performance, reduces material waste, and can form multiple containers with uniform wall thickness, suitable for food and pharmaceutical packaging.
Smart Images

Figure CN123125094A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to methods for manufacturing one-piece molded bodies and multi-piece packaging bodies. Background Technology
[0002] Previously, cup-shaped containers for yogurt and the like were made of multiple packaging units formed by connecting adjacent flanges. Generally, these multiple packaging units are obtained by thermoforming extruded polystyrene resin rolls (Patent Document 1).
[0003] In addition, the applicant of this application previously proposed a manufacturing method that can efficiently form a cup-shaped container from an injection-molded sheet preform (Patent Document 2). According to this invention, a turntable is rotated to transfer the injection-molded sheet preform, while it is held in the cavity mold, to a vacuum forming and removal station, where a cup-shaped container is formed by vacuum forming or pneumatic forming in a concave container mold. Existing technical documents Patent documents
[0004] Patent Document 1: Japanese Patent Application Publication No. 2013-163356 Patent Document 2: Japanese Patent Application Publication No. 2009-220294 Summary of the Invention The problem the invention aims to solve
[0005] However, in conventional multi-piece packaging like Patent Document 1, the container portions are cut from a continuous roll, resulting in the waste of portions not used for containers. On the other hand, in the manufacturing method of Patent Document 2, since injection molding is used to form the container, no waste material is generated as in Patent Document 1. However, the method of Patent Document 2, by injection molding multiple cup body forming portions from a single gate, makes it difficult to form thin-walled preforms.
[0006] Therefore, the present invention provides a one-piece molded body that has excellent injection molding properties even when it is thin-walled, and a method for manufacturing a multi-piece package using the one-piece molded body. Solution for solving the problem
[0007] This invention was made to solve at least a part of the above-mentioned problems and can be implemented as the following solutions or application examples.
[0008] [1] One embodiment of the one-piece molded body according to the present invention is a one-piece molded body made of thermoplastic resin, comprising a plurality of container forming regions, flange forming regions located around each of the container forming regions, and connecting portions connecting adjacent flange forming regions to each other, characterized in that, The one-piece molded body extends from the center of each of the container forming regions toward the outer periphery of the flange forming region in a direction orthogonal to the thickness direction of the container forming region, i.e., in a planar direction. A gate for injection molding is provided at the center of the plane direction of each of the container forming areas.
[0009] According to one embodiment of the one-piece molded body, since gates are provided in each of the multiple container forming areas, the injection molding performance is excellent even if the one-piece molded body has thin walls.
[0010] [2] In one embodiment of the one-piece molded body, it is possible that, The container forming region has a portion with a wall thickness greater than that of the flange forming region.
[0011] According to one embodiment of the one-piece molded body, by making the container forming area thicker than the flange forming area, the required wall thickness of the portion forming the container can be ensured.
[0012] [3] In one embodiment of the one-piece molded body, it is possible that, Adjacent flange forming regions are connected to each other by a plurality of connecting portions formed by injection molding.
[0013] According to one embodiment of the one-piece molded body, by having multiple injection-molded connecting parts of a predetermined shape, the connecting parts are not easily broken even after multiple packaging body manufacturing processes, contents filling and production processes, and sales processes.
[0014] [4] In one embodiment of the one-piece molded body, it is possible that, The connecting portion has a notch that is thinner than the flange forming area. The wall thickness of the notch gradually decreases from the two surfaces of the flange forming region toward the center in the thickness direction.
[0015] According to one embodiment of the one-piece molded body, even the thin-walled notches are easy to fill with resin, which can prevent short shots.
[0016] [5] In one embodiment of the one-piece molded body, it is possible that, The thermoplastic resin is a polyester resin or a polyolefin resin.
[0017] According to one embodiment of the one-piece molded article, due to its excellent injection molding properties, even polyester resins that are not easily molded into thin walls can be molded. Furthermore, according to another embodiment of the one-piece molded article, even polyolefin resins that are prone to uneven wall thickness during blow molding can be blow molded into multi-piece packages with minimal wall thickness unevenness.
[0018] [6] One aspect of the method for manufacturing a multi-piece package according to the present invention is characterized in that... The one-piece molded body is then injection molded. At least the container-forming region of the primary molded body obtained by injection molding is heated. The pressing area, including the gate portion, of the heated primary molded body is stretched using a tension rod, and compressed air is introduced into the container forming area to perform stretch blow molding, thereby obtaining multiple packaging bodies formed by connecting multiple adjacent containers.
[0019] According to one embodiment of the method for manufacturing multiple packaging bodies, since the gate of the one-piece molded body is located at the center of each container forming area, it is possible to form multiple containers with less uneven wall thickness. Invention Effects
[0020] The one-piece molded body according to the present invention exhibits excellent injection molding properties even with thin walls. Furthermore, the method for manufacturing multiple packaging bodies according to the present invention enables the molding of multiple containers with minimal wall thickness variation. Attached Figure Description
[0021] Figure 1 This is a perspective view of the one-piece molded body and the multi-piece packaging body involved in this embodiment. Figure 2 This is a top view of a one-piece molded body according to this embodiment. Figure 3 yes Figure 2 The front view of the one-piece molded body is shown. Figure 4 This is a schematic longitudinal cross-sectional view of the injection molding process in the manufacturing method of a multi-piece package according to this embodiment. Figure 5 This is a front view illustrating the heating process in the manufacturing method of multi-piece packaging according to this embodiment. Figure 6 This is a longitudinal cross-sectional view illustrating the stretch blow molding process in the manufacturing method of multi-piece packaging according to this embodiment. Detailed Implementation
[0022] The preferred embodiments of the present invention will now be described in detail with reference to the accompanying drawings. Furthermore, the embodiments described below are not intended to unduly limit the scope of the invention as defined in the claims. Additionally, not all components described below are necessarily essential elements of the present invention.
[0023] 1. Multipack use Figure 1 The description of the multiple package 20 is as follows. Figure 1 This is a perspective view of the one-piece molded body 10 and the multi-piece packaging body 20 involved in this embodiment. Figure 1 A perspective view of cover 30 is also shown.
[0024] The multi-pack 20 is a packaging container that is filled with contents while multiple containers 21 are connected by connecting parts 15, and then the containers 21 are sealed with caps 30 before being distributed in the market. The multi-pack 20 can be divided into individual containers 21 by bending the connecting parts 15 by the consumer. The contents filled into the multi-pack 20 are food products such as yogurt, tofu, seaweed, and pudding, and can also be used for pharmaceuticals, cosmetics, etc.
[0025] The multi-piece packaging body 20 includes multiple containers 21, multiple flanges 23, and multiple connecting parts 15. Figure 1 The image shows a multi-package 20 consisting of four containers 21 connected together, but the number of containers 21 connected is not limited to this. The multi-package 20 can also consist of two or three containers 21 connected together, or even five or more containers 21 connected together.
[0026] Container 21 has a cylindrical portion extending downward from the opening edge 22 that opens into the flange portion 23, and a bottom that closes the lower end. Each container 21 is a so-called cup-shaped container. The cylindrical portion is, for example, generally circular, but is not limited thereto, and may also have an elliptical, polygonal, or other cross-sections. There is no limitation on the capacity of the container 21, but if it is for food use, it may be, for example, 30ml to 300ml.
[0027] The flange 23 extends outward from the opening edge 22 of the container 21 in the horizontal direction (XY direction). The flange 23 is a plate-like structure with a generally flat front and back, but slight variations in texture or wall thickness are possible. The flange 23 is generally quadrilateral in shape, but other shapes may be used depending on the application of the container. Furthermore, the X-axis, Y-axis, and Z-axis are orthogonal to each other.
[0028] The cap 30, a thin sheet, seals the opening of the container 21. The cap 30 is manufactured in a separate process from the manufacturing process of the multi-piece packaging 20, and is bonded to the flange 23 after the contents of the container 21 have been filled. A cutting line 31 is formed on the cap 30 so that it is cut off along with the container 21 when the container 21 is separated. The cap 30 can be made of paper, thermoplastic resin, or the like.
[0029] 2. One-piece molded body use Figures 1-3 The one-piece molded body 10 according to this embodiment will be described. Figure 2 This is a top view of the one-piece molded body 10 according to this embodiment. Figure 3 yes Figure 2 The front view of the one-piece molded body 10 shown. Figure 2 Shaded lines were used to clearly indicate the different areas.
[0030] The one-piece molded body 10 is made of thermoplastic resin. The one-piece molded body 10 is formed by injection molding. The one-piece molded body 10 includes a plurality of container forming regions 11, flange forming regions 13 located around each container forming region 11, and connecting portions 15 connecting adjacent flange forming regions 13 to each other. The one-piece molded body 10 extends from the center of each container forming region 11 toward the outer periphery of the flange forming region 13 in a direction orthogonal to the thickness direction of the container forming region 11, i.e., in a planar direction. Here, in this embodiment, the thickness direction is along the Z-axis, and the planar direction is along a plane passing through the X and Y axes. The one-piece molded body 10 is formed, for example, entirely along an imaginary plane 18. The imaginary plane 18 is a plane that readily illustrates the shape extending in the planar direction, and is an imaginary plane parallel to the plane passing through the X and Y axes.
[0031] Each container forming region 11 and each flange forming region 13 extends in a planar direction, for example, along an imaginary plane 18. For example, one surface of the container forming region 11 and the flange forming region 13 may lie on the imaginary plane 18, or the imaginary plane 18 may be located at any position in the thickness direction of the container forming region 11 and the flange forming region 13. By injection molding, the container forming region 11 and the flange forming region 13 can have a predetermined shape. Furthermore, the injection molding process will be described later.
[0032] The container forming region 11 and the flange forming region 13 can be flat plates with a specified wall thickness. The specified wall thickness of the container forming region 11 and the flange forming region 13 is preferably as thin as possible within the range required by the specifications of the multi-piece package 20, for example, it can be 0.5 mm to 2.0 mm, further, it can be 0.5 mm to 1.5 mm, and particularly, it can be 0.5 mm to 0.8 mm. Furthermore, "flat plate" means that the shape is approximately flat overall. One or both surfaces of the container forming region 11 and the flange forming region 13 can be flat. If at least one surface of the primary molded body 10 is flat, it is easy to mechanically transport it to the heating process after injection molding or the stretch blow molding process. In addition, if the primary molded body 10 is flat, even if many primary molded bodies 10 are stacked, they will be compact, thus saving space during storage or transportation. The container forming region 11 and the flange forming region 13, which may have slight variations in undulation or wall thickness depending on the specifications required by the multi-piece package 20, are also included in the flat plate shape.
[0033] Figures 1-3The container forming region 11 and the flange forming region 13 are shown as examples with the same wall thickness, but the container forming region 11 may also have a portion with a wall thickness greater than that of the flange forming region 13. The thickness of the container forming region 11 in the Z-axis direction can be, for example, 1.1 to 4.0 times the thickness of the flange forming region 13, and more specifically, 1.1 to 3.0 times the thickness of the flange forming region 13. By making the container forming region 11 thicker than the flange forming region 13, the required wall thickness for the portion forming the container 21 can be ensured. Conventional roll sheets, as shown in Patent Document 1, have the same wall thickness, making it difficult to adjust the wall thickness of the container 21. However, in this embodiment, a container forming region 11 matching the wall thickness of the container 21 can be injection molded. Furthermore, the flange forming region 13 may also have a portion with a different wall thickness. For example, the flange forming region 13 may have a step along its inner periphery, having an annular portion along its inner periphery that is thinner than its outer periphery. Furthermore, in Figure 2 In the illustration, the area indicated by the shaded line is the container forming area 11 (including the pressing area 12), and the outer side of it is the flange forming area 13.
[0034] The outer edge of the flange forming region 13 is approximately square when viewed from above. Adjacent flange forming regions 13 are spaced slightly apart and are disposed on the same imaginary plane 18. The spacing between adjacent flange forming regions 13 (the length of the connecting portion 15) can be 0.2 mm to 1.0 mm. A connecting portion 15 is provided to connect the adjacent two sides of each flange forming region 13 in a manner that bridges the spacing. The flange forming region 13 is the part that holds the one-piece molded body 10 in the mold during the stretch blow molding process described later. In addition, the flange forming region 13 is the part that attaches the cap 30 after the contents of the multi-piece package 20 have been filled. For example, thin walls or steps may be provided at the corners of the flange forming region 13 for consumers to rest their fingers when peeling off the cap 30.
[0035] The connecting portion 15 is the part that connects adjacent flange forming regions 13 to each other. The connecting portion 15 can extend in a planar direction together with the container forming region 11 and the flange forming region 13, for example, formed along an imaginary plane 18. The connecting portion 15 is the part that consumers who purchase multiple packages 20 divide into individual containers 21. The connecting portion 15 can be easily bent and broken by the consumer. There is no limitation on the number and shape of the connecting portions 15, but it is preferable that adjacent flange forming regions 13 are connected to each other by multiple connecting portions 15 formed by injection molding. By using injection molding to form the connecting portions 15 of a predetermined shape, the additional post-processing of cutting as in the past is not required. Post-processing can also be performed to make the connecting portions 15 easy to break. In addition, by using injection molding to form the connecting portions 15, the connecting portions 15 are not easy to break even after the manufacturing process of multiple packages 20, the filling and production process of the contents, and the sales process. One or more connecting portions 15 are provided between adjacent flange forming regions 13. When there is only one connecting portion 15, the length of the connecting portion 15 in plan view may, for example, be the same as the length of the straight portion of the adjacent flange forming region 13. When there are one or more connecting portions 15, the length of each connecting portion 15 in plan view may also be shorter than the straight portion. When multiple connecting portions 15 are provided, such as... Figure 2 In this way, they are arranged with gaps between each other. When there is an odd number of connecting parts 15, it is preferable to arrange one connecting part 15 on an imaginary straight line connecting adjacent gate parts 14. This is because, during injection molding, the material enters the cavity 43 from the gate part 14. Figure 4 The molten resin inside will first reach the connecting part 15 located on the imaginary straight line, which can reliably shape the connecting part 15.
[0036] like Figure 3 As shown, the preferred connecting portion 15 has a notch portion 150 with a thinner wall than the flange forming region 13. The notch portion 150 is formed such that the wall thickness gradually decreases from both surfaces of the flange forming region 13 toward the center in the thickness direction. Through the notch portion 150, consumers can easily bend the multi-piece package 20 to prevent breakage. The notch portion 150 includes: a thinnest portion 151 located approximately at the center of the interval between adjacent flange forming regions 13; and a wall thickness reduction portion 152 whose wall thickness gradually decreases from both surfaces of the flange forming region 13 toward the thinnest portion 151 located near the center in the thickness direction (along the Z-axis). The notch portion 150 may also be formed as follows: Figure 3 It is formed by a V-shaped inclined surface as shown. Since the wall thickness gradually thins towards the center in the thickness direction where the molten resin flows fastest during injection molding, even the thinner notch 150 is easy to fill with resin, thus preventing short shots.
[0037] The container forming region 11 is formed as part of the container 21 by stretch blow molding, described later. The container forming region 11 is located inside the flange forming region 13. The outer edge of the container forming region 11 forms the opening edge 22 of the multi-piece packaging body 20. The container forming region 11 includes a pressing region 12 on its central side, which is pressed by the stretching rod 64, described later. By pressing the pressing region 12 by the stretching rod 64, the container forming region 11 can be stretched in the direction along the Z-axis. Depending on the required specifications of the container 21, it may also include a portion with a thicker wall compared to the flange forming region 13.
[0038] A gate 14 for injection molding is provided at the center of each container forming region 11. The gate 14 is a gate mark used during the injection molding of the primary molded body 10. The gate 14 is the portion where molten resin flows into the mold during the injection molding of the primary molded body 10, as described later. Generally, thin-walled injection molded articles are prone to short shots during injection molding. However, since each of the multiple container forming regions 11 has a gate 14, the injection molding performance is excellent even if the primary molded body 10 is thin-walled. Moreover, since the molten resin expands circumferentially from the gate 14 toward the outer periphery of the flange forming region 13 during injection molding, there is less circumferential flow unevenness by placing the gate 14 approximately at the center of the container forming region 11. As a result, when the container 21 is molded as thin-walled, the wall thickness unevenness is reduced. Furthermore, for illustration purposes, the gate 14 is depicted as protruding from the container forming region 11, but it may not protrude.
[0039] Furthermore, if the gate is placed in the middle of the two container forming areas as in the aforementioned Patent Document 1, it would be difficult to handle three-container containers. However, since the gate 14 is located in each container forming area 11, the one-piece molded body 10 can be applied to multiple packaging bodies 20 with an odd number of containers 21, such as three-container or five-container containers.
[0040] The thermoplastic resin used in the molding of the one-piece molded body can be either crystalline or amorphous, and there are no restrictions as long as the resin can be injection molded and stretch blow molded. However, from a recyclability point of view, polyester resin or polyolefin resin is preferred. In particular, polyester resin can be recycled as a container, resulting in a low environmental impact. Since the one-piece molded body 10 has excellent injection moldability, even polyester resin, which is not easy to injection mold into thin walls, can be molded. In addition, since the gate 14 is located approximately at the center of the container forming region 11, even polyolefin resin, which is prone to uneven wall thickness during blow molding, can be blow molded into multi-piece packaging bodies 20 with less uneven wall thickness.
[0041] Polyester resins include, but are not limited to, polyethylene terephthalate (PET), polylactic acid (PLA), polyethylene furanate (PEF), polyethylene naphthalate (PEN), and blends / mixtures of these polymers.
[0042] Polyolefin resins include, but are not limited to, polyethylene (PE), polypropylene (PP), olefin elastomers, and blends / mixtures of these polymers.
[0043] 3. Manufacturing method of multi-piece packaging use Figures 4-6 This embodiment will now describe the manufacturing method of the multi-piece packaging body 20. Figure 4 This is a schematic longitudinal cross-sectional view illustrating the injection molding process in the manufacturing method of the multi-piece packaging body 20 according to this embodiment. Figure 5 This is a front view illustrating the heating process in the manufacturing method of the multi-piece packaging body 20 according to this embodiment. Figure 6 This is a longitudinal cross-sectional view illustrating the stretch blow molding process in the manufacturing method of the multi-piece packaging body 20 according to this embodiment. Furthermore, in Figure 6 In the middle, the left side shows the state in which the primary molded body 10 is placed in the blow molding mold 60, and the right side shows the state in which the primary molded body 10 is stretched and blow molded to form the container 21.
[0044] The manufacturing method of the multi-piece packaging body 20 includes an injection molding process, a heating process, and a stretch blow molding process.
[0045] 3-1. Injection Molding Process like Figure 4 As shown, in the injection molding process, 40 pairs of injection molding molds are used. Figures 1-3 The one-piece molded body 10 shown is injection molded. The injection molding mold 40 includes: a movable mold 41 that can move forward and backward in the direction of the arrow; and a fixed mold 42, which, together with the hot runner 44, is fixed to an injection molding apparatus (not shown). As shown, when the movable mold 41 is closed relative to the fixed mold 42, a cavity 43 is formed.
[0046] Cavity 43 is formed for use Figures 1-3 The space of the outer shape of the one-piece molded body 10 as described.
[0047] With the injection molding mold 40 closed, molten resin, through an injection device (not shown), is filled into the cavity 43 via the hot runner 44 and nozzle 45. The cavity 43 is a space extending in a planar direction. Figure 4In this example, molten resin injected into the cavity 43 from nozzles 45 extending in the Z-axis direction expands radially in the planar direction within the cavity 43 corresponding to the container forming region 11. Furthermore, the molten resin expands radially in the planar direction and fills the cavity 43 corresponding to the flange forming region 13 located around the container forming region 11, and the cavity 43 corresponding to the connecting portion 15. After holding until the filled resin solidifies to a removable state, the movable mold 41 is opened, and the primary molded body 10 is ejected from the mold.
[0048] Since the one-piece molded body 10 is formed into the shape of the multi-piece package 20 through a heating process and stretch blow molding, the waste generated in the conventional thermoforming of sheets is eliminated. Therefore, compared with conventional styrene-based multi-piece packages (Patent Document 1), the environmental impact is reduced.
[0049] Furthermore, the distance from the gate 14 to the connecting portion 15 is preferably equal in the two container forming regions 11 adjacent to the connecting portion 15. This is because the molten resin filled from the gate 14 will arrive at the connecting portion 15 at almost the same time and merge at the connecting portion 15.
[0050] like Figure 4 As shown in the enlarged view, the molten resin flowing within the cavity 43 flows in the connecting portion 15 from both sides of the adjacent flange forming region 13 in the direction of the arrows. The molten resin... Figure 4 As shown by the dashed line, the resin flows fastest near the center in the height direction of the cavity 43. Therefore, even though the height of the cavity 43 gradually decreases due to the inclined surface of the wall thickness reduction section 152, the resin will fill to the thinnest part 151, preventing short shots. In addition, since the resin flow is limited by the wall thickness reduction section 152, even if the filling to the adjacent flange forming region 13 is slightly delayed, the resin will converge at the joint 15, forming a weld line that is easy to break when bent.
[0051] 3-2. Heating process like Figure 5 As shown, in the heating process, at least the container forming region 11 of the primary molded body 10 obtained by injection molding is heated. The container forming region 11 is heated to a temperature suitable for stretch blow molding by the heating process. The heating process can be performed using a known heater 50. The heating process can be performed, for example, while the primary molded body 10 is being transported toward the stretch blow molding process.
[0052] 3-3. Stretch blow molding process like Figure 6As shown on the left, in the stretch blow molding process, the heated primary molded part 10 is placed in a predetermined position on the blow molding mold 60. The blow molding mold 60 includes, for example: a blow mold 61 and a bottom mold 62, which form a cavity 63 having the shape of a container 21; a pressure plate 65, which holds the flange forming area 13 between itself and the blow mold 61; and a stretch rod 64. The stretch rod 64 can press the pressing area 12 (in...) Figure 2 The area marked with fine dots and shaded lines is pushed towards the bottom mold 62. This configuration allows the tension rod 64 to form area 11 with the container. Figure 2 Compressed air is introduced between the entire area (with the shaded lines drawn).
[0053] Next, as Figure 6 As shown on the right, the pressing area 12, including the gate portion 14, of the heated one-piece molded body 10 is stretched using a tension rod 64, and compressed air is introduced into the container forming area 11 for stretch blow molding, resulting in a plurality of adjacent containers 21 connected by connecting portions 15. Figure 1 The multi-component packaging body 20 is shown. Since the gate portion 14 of the one-piece molded body 10 is located at the center of each container forming area 11, it is possible to form multiple containers 21 with less uneven wall thickness.
[0054] This invention is not limited to the embodiments described above and can be further modified in various ways, including configurations that are substantially the same as those described in the embodiments (configurations with the same function, method, and result, or configurations with the same purpose and effect). Furthermore, this invention includes configurations in which non-essential parts of the configurations described in the embodiments are replaced. Additionally, this invention includes configurations that have the same effect as those described in the embodiments or that can achieve the same purpose. Furthermore, this invention includes configurations in which known techniques are added to the configurations described in the embodiments. Explanation of reference numerals in the attached figures
[0055] 10…One-piece molded body, 11…Container forming area, 12…Pressing area, 13…Flange forming area, 14…Gate, 15…Connecting part, 150…Notch, 151…Thinnest part, 152…Wall thickness reduction part, 18…Imaginary plane, 20…Multi-piece package, 21…Container, 22…Opening edge, 23…Flange, 30…Lid, 31…Cutting line, 40…Injection molding mold, 41…Modible mold, 42…Fixed mold, 43…Cavity, 44…Hot runner, 45…Nozzle, 50…Heater, 60…Blow molding mold, 61…Blow mold, 62…Bottom mold, 63…Cavity, 64…Tie bar, 65…Pressure plate.
Claims
1. A one-piece molded body, made of thermoplastic resin, comprising a plurality of container forming regions, flange forming regions surrounding each of the container forming regions, and connecting portions connecting adjacent flange forming regions to each other, characterized in that, The one-piece molded body extends from the center of each of the container forming regions toward the outer periphery of the flange forming region in a direction orthogonal to the thickness direction of the container forming region, i.e., in a planar direction. A gate for injection molding is provided at the center of the plane direction of each of the container forming areas.
2. The one-piece molded article according to claim 1, characterized in that, The container forming region has a portion with a wall thickness greater than that of the flange forming region.
3. The one-piece molded article according to claim 1, characterized in that, Adjacent flange forming regions are connected to each other by a plurality of connecting portions formed by injection molding.
4. The one-piece molded article according to claim 2, characterized in that, The connecting portion has a notch that is thinner than the flange forming area. The wall thickness of the notch gradually decreases from the two surfaces of the flange forming region toward the center in the thickness direction.
5. The one-piece molded article according to claim 1, characterized in that, The thermoplastic resin is a polyester resin or a polyolefin resin.
6. A method for manufacturing a multi-piece packaging unit, characterized in that, The one-piece molded article according to any one of claims 1 to 5 is injection molded. At least the container-forming region of the primary molded body obtained by injection molding is heated. The pressing area, including the gate portion, of the heated primary molded body is stretched using a tension rod, and compressed air is introduced into the container forming area to perform stretch blow molding, thereby obtaining multiple packaging bodies formed by connecting multiple adjacent containers.
Citation Information
Patent Citations
Manufacturing method of cup-shaped container
JP2009220294A
Thermoplastic multilayer resin sheet and molded container
JP2013163356A