Device for producing electrolytic copper foil with uniform weight
By using spring rotating shafts, buffer roller components and damping rotating shafts in the electrolytic copper foil production device, combined with semi-arc rods and tension springs, the problem of being too loose or too tight during the copper foil bundling process is solved, and the uniformity of the copper foil is achieved Heavy weight and tight bundling improve production quality.
Patent Information
- Application Number
- CN202420524641.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-19
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2034-03-19
AI Technical Summary
Existing electrolytic copper foil production equipment can easily cause the copper foil to be too loose or too tight during the bundling process, resulting in creases or deformation, which affects production quality.
A device including a spring rotating shaft, a buffering Kun assembly and a damping rotating shaft is designed. The buffering Kun assembly changes the angle and speed during the bundling process to uniformly control the tension of the copper foil, and avoids the copper foil through the semi-arc rod and tension spring. Contact the edges and corners to ensure a flat bundle of copper foil.
It effectively avoids creases and deformation of copper foil during the bundling process, improves production quality and functionality of the device, and ensures uniform weight and tight bundling of copper foil.
Smart Images

Figure CN221810146U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of electrolytic copper foil production and manufacturing, in particular to a device for producing electrolytic copper foil with uniform mass and weight. Background Art
[0002] Electrolytic copper foil is an important material for copper clad laminate (CCL), printed circuit board (PCB) and lithium-ion battery manufacturing. The production process of electrolytic copper foil is simple, with three main processes: solution foil production, surface treatment and product slitting. The production process seems simple, but it integrates electronics, mechanics and electrochemistry, and is a production process with particularly strict requirements on the production environment. Therefore, the electrolytic copper foil industry does not have a set of standard universal production equipment and technology, and the existing devices for producing electrolytic copper foil have certain shortcomings.
[0003] As described in Publication No. CN115305527B, "A copper foil production device comprises a mounting frame and a winding assembly, a cutting assembly and a pre-cutting assembly arranged on the mounting frame; the winding assembly comprises a bearing seat, a winding roller and a driving motor, the winding roller is arranged on the mounting frame through the bearing seat, and the driving motor is used to drive the winding roller to rotate to wind up the copper foil; a cutting edge is arranged on the upper surface of the mounting frame, and the cutting assembly comprises a cutting machine rotatably arranged inside the mounting frame, and a driving device for driving the blade of the cutting machine to expose or retract the cutting edge; the pre-cutting The assembly includes a first slide rail and a second slide rail respectively arranged on both sides of the cutting edge, a first sliding clamp plate and a second sliding clamp plate are respectively arranged on the first slide rail and the second slide rail, and a protective cover is connected between the first sliding clamp plate and the second sliding clamp plate. When the copper foil is produced and bundled, the speed difference of the roller used to bundle the copper foil may cause the copper foil to be bundled too loosely or too tightly. The copper foil itself is very thin. If it is bundled too loosely, it may cause creases in the copper foil. If it is bundled too tightly, the copper foil may be stretched and thinned due to its ductility, affecting the production quality. Utility Model Content
[0004] The utility model aims to provide a device for producing electrolytic copper foil of uniform weight, so as to solve the problem that the copper foil may generate creases or deformations when being rolled up, as mentioned in the above background technology.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solution: a device for producing electrolytic copper foil of uniform weight, comprising a processing chamber, a conveying roller is installed on one side of the processing chamber, the bottom of the processing chamber is fixedly connected to a load-bearing base, one side of the load-bearing base is fixedly connected to a load-bearing plate, one side of the top of the load-bearing plate is fixedly connected to a first load-bearing column, the other side of the top of the load-bearing plate is fixedly connected to a second load-bearing column, the top of one side of the first load-bearing column is rotatably connected to a buffer roller assembly via a spring shaft, and one end of the buffer roller assembly is rotatably connected to the top of one side of the second load-bearing column via a damping shaft.
[0006] Preferably, the buffer roller assembly includes a first support block and a second support block, the first support block is installed on the top of one side of the first load-bearing column through a spring shaft, and the second support block is rotatably connected to the top of one side of the second load-bearing column through a damping shaft.
[0007] Preferably, one side of each of the first support block and the second support block is fixedly connected with a fixed slider, the inner wall of the fixed slider is movably connected with a movable slider, and a sliding groove is provided on the surface of the movable slider.
[0008] Preferably, a first connection block is plugged into the top end of the movable slide bar, and a second connection block is plugged into the bottom end of the movable slide bar.
[0009] Preferably, the inner top wall of the first connecting block and the inner bottom wall of the second connecting block are both provided with tension springs, and the two groups of tension springs are respectively fixedly connected to the top end and the bottom end of the movable slide bar.
[0010] Preferably, a first semi-arc rod is fixedly connected to one side of the first connecting block, and a second semi-arc rod is fixedly connected to one side of the second connecting block.
[0011] Preferably, both ends of the first semi-arc rod and both ends of the second semi-arc rod are fixedly connected to a support frame, and one end of the support frame is rotatably connected to a support roller via a connecting shaft.
[0012] Compared with the prior art, the beneficial effects of the utility model are as follows:
[0013] 1. The utility model, through the arrangement of a spring shaft, a buffer roll assembly and a damping shaft, allows the manufactured copper foil to pass through the middle of the buffer roll assembly and be connected to the bundling assembly for bundling. When a group of bundling assemblies is completed and replaced, the replacement process may cause the pulling force of the copper foil to change. At this time, the buffer roll assembly changes the angle through the rotation of the spring shaft, and the tension on the copper foil can be maintained within a certain range. When the bundling assembly is installed, the bundling speed is adjusted to rotate the buffer roll assembly to the original angle, which can ensure the uniformity of the force of the copper foil bundling, ensure the tightness of the bundling, reduce the possibility of damage to the copper foil due to improper force, improve production quality, and increase the functionality of the device.
[0014] 2. The utility model fixes the slider, moves the slide bar, stretches the spring, and arranges the first semi-arc rod and the second semi-arc rod. The copper foil passes between the first semi-arc rod and the second semi-arc rod. When the buffer roller assembly rotates, the copper foil adheres to the arc surface of the first semi-arc rod and the second semi-arc rod, so that the copper foil does not contact the edges of the corners, thereby ensuring the production quality of the copper foil and improving the functionality of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0016] Figure 2 This is a schematic diagram of the structure of the buffer roller assembly of the utility model;
[0017] Figure 3 This is a schematic diagram of the structure of the first load-bearing column of the utility model;
[0018] Figure 4 This is a schematic diagram of the first half arc rod structure of the utility model;
[0019] Figure 5 It is a schematic diagram of the support roller structure of the utility model.
[0020] In the figure: 1, processing chamber; 2, conveying roller; 3, load-bearing base; 4, load-bearing plate; 5, first load-bearing column; 6, second load-bearing column; 7, spring shaft; 8, buffer roller assembly; 801, first support block; 802, second support block; 803, fixed slider; 804, movable slider; 805, slide groove; 806, first connecting block; 807, second connecting block; 808, tension spring; 809, first semi-arc rod; 810, second semi-arc rod; 811, support frame; 812, connecting shaft; 813, support roller; 9, damping shaft. DETAILED DESCRIPTION
[0021] See also Figure 1 , Figure 2 and Figure 3 A device for producing electrolytic copper foil of uniform weight includes a processing chamber 1, a conveying roller 2 is installed on one side of the processing chamber 1, a load-bearing base 3 is fixedly connected to the bottom of the processing chamber 1, a load-bearing plate 4 is fixedly connected to one side of the load-bearing base 3, a first load-bearing column 5 is fixedly connected to one side of the top of the load-bearing plate 4, a second load-bearing column 6 is fixedly connected to the other side of the top of the load-bearing plate 4, a buffer roller assembly 8 is rotatably connected to the top of one side of the first load-bearing column 5 through a spring shaft 7, and one end of the buffer roller assembly 8 is rotatably connected to the top of one side of the second load-bearing column 6 through a damping shaft 9.
[0022] When in use, through the arrangement of the spring shaft 7, the buffer roll assembly 8 and the damping shaft 9, a gap is provided in the middle of the buffer roll assembly 8, through which the copper foil can pass, and the two ends of the buffer roll assembly 8 are rotatably connected between the first load-bearing column 5 and the second load-bearing column 6. When the buffer roll assembly 8 is not affected by external force, it is statically placed between the first load-bearing column 5 and the second load-bearing column 6 through the spring shaft 7. When the buffer roll assembly 8 is affected by external force, the spring in the spring shaft 7 is deformed by the elastic pressure of rotation, and the buffer roll assembly 8 rotates itself. When the external force is removed, the buffer roll assembly 8 is affected by the rebound force of the spring in the spring shaft 7 and rotates in the opposite direction. The damping shaft 9 can slow down the rotation speed of the buffer roll assembly 8 affected by the rebound force of the spring shaft 7. When the copper foil is produced and bundled, the speed difference of the roller used for bundling the copper foil may cause the copper foil to be bundled too loosely. Or too tight, the copper foil itself is very thin, if the bundling is too loose, it may cause creases in the copper foil, if the bundling is too tight, due to the ductility of the copper foil, it may be stretched and thinned, affecting the production quality. When the device produces copper foil, the manufactured copper foil passes through the middle of the buffer roll assembly 8 and is connected to the bundling assembly for bundling. When a group of bundling assemblies are bundled and replaced, the replacement process may cause the pulling force of the copper foil to change. At this time, the buffer roll assembly 8 changes the angle through the spring shaft 7, which can maintain the tension on the copper foil within a certain range. When the bundling assembly is installed, the bundling speed is adjusted to rotate the buffer roll assembly 8 to the original angle, which can ensure the uniformity of the force of the copper foil bundling, ensure the tightness of the bundling, and reduce the possibility of damage to the copper foil due to improper force, thereby improving the production quality and increasing the functionality of the device.
[0023] See also Figure 1 , Figure 3 , Figure 4 and Figure 5 The buffer roller assembly 8 includes a first support block 801 and a second support block 802. The first support block 801 is installed on the top of one side of the first load-bearing column 5 through a spring shaft 7. The second support block 802 is rotatably connected to the top of one side of the second load-bearing column 6 through a damping shaft 9. One side of the first support block 801 and the second support block 802 is fixedly connected to a fixed slider 803. The inner wall of the fixed slider 803 is movably connected to a moving slider 804. The surface of the moving slider 804 is provided with a slide groove 805. A first connecting block 806 is inserted at the top of the movable slide bar 804, and a second connecting block 807 is inserted at the bottom of the movable slide bar 804. Tension springs 808 are provided on the inner top wall of the first connecting block 806 and the inner bottom wall of the second connecting block 807. The two groups of tension springs 808 are respectively fixedly connected to the top and bottom ends of the movable slide bar 804. A first semi-arc rod 809 is fixedly connected to one side of the first connecting block 806, and a second semi-arc rod 810 is fixedly connected to one side of the second connecting block 807.
[0024] When in use, by setting the fixed slider 803, the movable slide bar 804, the tension spring 808, the first semi-arc rod 809 and the second semi-arc rod 810, the movable slide bar 804 can slide on one side of the fixed slider 803, the first semi-arc rod 809 and the second semi-arc rod 810 have arc-shaped surfaces without edges and corners, and the first semi-arc rod 809 and the second semi-arc rod 810 are close to each other by the tension of the tension spring 808 when no external force is applied. Since the copper foil itself is very thin and is easy to be creased, if the copper foil contacts with the copper foil during movement, the copper foil will be easily creased. When the edges have an angular structure, it is easy to leave marks on the surface of the copper foil, affecting the production quality of the copper foil. When the device is processing and producing copper foil, the copper foil passes between the first semi-arc rod 809 and the second semi-arc rod 810. At this time, the first semi-arc rod 809 and the second semi-arc rod 810 are separated, and the tension spring 808 is compressed and deformed. When the buffer roller assembly 8 rotates, the copper foil is attached to the arc surface of the first semi-arc rod 809 and the second semi-arc rod 810, so that the copper foil does not contact the angular edges, thereby ensuring the production quality of the copper foil and improving the functionality of the device.
[0025] See also Figure 1 , Figure 4 and Figure 5 Both ends of the first semi-arc rod 809 and both ends of the second semi-arc rod 810 are fixedly connected to a support frame 811, and one end of the support frame 811 is rotatably connected to a support roller 813 through a connecting shaft 812.
[0026] When in use, by setting the support roller 813, four groups of support rollers 813 are respectively located on both sides of the opposite surfaces of the first semi-arc rod 809 and the second semi-arc rod 810, so that the buffer roller assembly 8 can reduce the friction on the surface of the copper foil when limiting the transmission of the copper foil, thereby improving the production quality of the copper foil.
[0027] Working principle: when the device is used to produce copper foil, the produced copper foil is first output to the outside of the processing chamber 1 through the conveying roller 2, and passes through the gap in the middle of the buffer roller assembly 8, that is, between the first semi-arc rod 809 and the second semi-arc rod 810. During the copper foil bundling process, the buffer roller assembly 8 can play a certain buffering and limiting role on the copper foil. The surfaces of the first semi-arc rod 809 and the second semi-arc rod 810 are arc-shaped to prevent the edges from causing creases on the surface of the copper foil. The supporting roller 813 rotates through the connecting shaft 812 to reduce the contact area between the copper foil and the structure, while reducing friction, reducing damage to the surface of the copper foil, and improving production quality.
[0028] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
Claims
1. A device for producing uniform heavy electrolytic copper foil, comprising a processing chamber (1), characterized in that: A conveying roller (2) is installed on one side of the processing chamber (1); a load-bearing base (3) is fixedly connected to the bottom of the processing chamber (1); a load-bearing plate (4) is fixedly connected to one side of the load-bearing base (3); a first load-bearing column (5) is fixedly connected to one side of the top of the load-bearing plate (4); a second load-bearing column (6) is fixedly connected to the other side of the top of the load-bearing plate (4); a buffer roller assembly (8) is rotatably connected to the top of one side of the first load-bearing column (5) via a spring shaft (7); and one end of the buffer roller assembly (8) is rotatably connected to the top of one side of the second load-bearing column (6) via a damping shaft (9).
2. The device for producing uniform weight electrolytic copper foil according to claim 1, characterized in that: The buffer roller assembly (8) comprises a first support block (801) and a second support block (802), wherein the first support block (801) is mounted on the top of one side of the first load-bearing column (5) via a spring shaft (7), and the second support block (802) is rotatably connected to the top of one side of the second load-bearing column (6) via a damping shaft (9).
3. The device for producing uniform weight electrolytic copper foil according to claim 2, characterized in that: A fixed slider (803) is fixedly connected to one side of the first support block (801) and the second support block (802); an inner wall of the fixed slider (803) is movably connected to a movable slider (804); and a sliding groove (805) is provided on the surface of the movable slider (804).
4. The device for producing uniform weight electrolytic copper foil according to claim 3, characterized in that: The top end of the movable slide bar (804) is plugged with a first connection block (806), and the bottom end of the movable slide bar (804) is plugged with a second connection block (807).
5. The device for producing uniform weight electrolytic copper foil according to claim 4, characterized in that: The inner top wall of the first connecting block (806) and the inner bottom wall of the second connecting block (807) are both provided with tension springs (808), and the two groups of tension springs (808) are respectively fixedly connected to the top end and the bottom end of the movable slide bar (804).
6. The device for producing uniform weight electrolytic copper foil according to claim 4, characterized in that: A first semi-arc-shaped rod (809) is fixedly connected to one side of the first connecting block (806), and a second semi-arc-shaped rod (810) is fixedly connected to one side of the second connecting block (807).
7. The device for producing uniform weight electrolytic copper foil according to claim 6, characterized in that: Both ends of the first semi-arc rod (809) and both ends of the second semi-arc rod (810) are fixedly connected to a support frame (811), and one end of the support frame (811) is rotatably connected to a support roller (813) via a connecting shaft (812).