Tensile stainless steel pipe capable of reducing thermal deformation

By forming a multi-layer protective structure on the stainless steel pipe, including an internal and external high-temperature resistant adhesive layer, a coating layer and an anti-corrosion layer, the problems of thermal deformation, wear and corrosion of the stainless steel pipe are solved, and its high temperature resistance, corrosion resistance and wear resistance are improved. properties, extending service life.

CN221811094UActive Publication Date: 2024-10-08YANCHENG XINHANG STAINLESS STEEL PIPE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420559428.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-21
Publication Date
2024-10-08
Estimated Expiration
2034-03-21

AI Technical Summary

Technical Problem

Existing stainless steel pipes are prone to thermal deformation, wear and corrosion during use, resulting in reduced service life.

Method used

It adopts an inner high-temperature resistant adhesive layer, an anti-wear layer, an outer high-temperature resistant adhesive layer, a high-temperature resistant paint layer, an anti-corrosion layer and a wear-resistant layer. These layers are fixedly connected to the main body of the stainless steel pipe to form a multi-layer protection structure to improve its high temperature resistance, corrosion resistance and wear resistance.

Benefits of technology

It effectively avoids thermal deformation, wear and corrosion damage of stainless steel pipes and extends the service life of stainless steel pipes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221811094U_ABST
    Figure CN221811094U_ABST
Patent Text Reader

Abstract

The utility model discloses a tensile stainless steel pipe capable of reducing thermal deformation, which comprises a stainless steel pipe main body, an inner high-temperature-resistant adhesive layer is fixedly connected inside the stainless steel pipe main body, an anti-abrasion layer is fixedly connected inside the inner high-temperature-resistant adhesive layer, an outer high-temperature-resistant adhesive layer is fixedly connected outside the stainless steel pipe main body, and an anti-abrasion layer is fixedly connected inside the outer high-temperature-resistant adhesive layer. The exterior of the outer high-temperature-resistant adhesive layer is fixedly connected with a high-temperature-resistant coating layer, and the exterior of the high-temperature-resistant coating layer is fixedly connected with an anti-corrosion layer; the high-temperature-resistant adhesive layer, the high-temperature-resistant coating layer, the abrasion-resistant layer, the abrasion-resistant layer, the corrosion-resistant layer and the like are adopted, and the abrasion-resistant layer, the high-temperature-resistant coating layer, the corrosion-resistant layer and the abrasion-resistant layer are fixedly connected to the stainless steel pipe body through the inner high-temperature-resistant adhesive layer and the outer high-temperature-resistant adhesive layer. And the stainless steel pipe main body has high temperature resistance, corrosion resistance and wear resistance, so that the stainless steel pipe main body is prevented from being deformed by heating or damaged by wear and corrosion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of stainless steel pipes, in particular to a tensile stainless steel pipe capable of reducing thermal deformation. Background Art

[0002] Steel pipes are used to transport fluids and powdered solids, exchange heat energy, and manufacture mechanical parts and containers. They are also an economical steel material, so existing stainless steel pipes need to have properties such as resistance to thermal deformation, wear resistance, and corrosion resistance.

[0003] Existing stainless steel pipes do not have resistance to thermal deformation, wear resistance, corrosion resistance, etc., which makes the stainless steel pipes easily deformed by heat or damaged by wear and corrosion during use, resulting in a reduced service life of the stainless steel pipes. Therefore, in order to solve the above-mentioned problems, the utility model proposes a tensile stainless steel pipe that reduces thermal deformation. Utility Model Content

[0004] The utility model aims to provide a tensile stainless steel pipe with reduced thermal deformation to solve the problems raised in the above background technology.

[0005] To achieve the above-mentioned objectives, the utility model provides the following technical solutions: a tensile stainless steel pipe for reducing thermal deformation, comprising a stainless steel pipe body, an inner high-temperature resistant adhesive layer is fixedly connected to the interior of the stainless steel pipe body, an anti-wear layer is fixedly connected to the interior of the inner high-temperature resistant adhesive layer, an outer high-temperature resistant adhesive layer is fixedly connected to the exterior of the stainless steel pipe body, a high-temperature resistant coating layer is fixedly connected to the exterior of the outer high-temperature resistant adhesive layer, an anti-corrosion layer is fixedly connected to the exterior of the high-temperature resistant coating layer, and a wear-resistant layer is fixedly connected to the exterior of the anti-corrosion layer.

[0006] Preferably, the high temperature resistant coating layer is a quartz sand layer coated with refractory cement.

[0007] Preferably, an inorganic compound layer is provided inside the inner high temperature resistant adhesive layer and the outer high temperature resistant adhesive layer.

[0008] Preferably, the surface of the anti-corrosion layer is coated with acrylic polyurethane topcoat.

[0009] Preferably, the anti-wear layer and the wear-resistant layer are both corundum layers.

[0010] Compared with the prior art, the beneficial effects of the utility model are as follows: the utility model adopts a high-temperature resistant adhesive layer, a high-temperature resistant coating layer, an anti-wear layer, a wear-resistant layer, an anti-corrosion layer, etc., and the anti-wear layer and the high-temperature resistant coating layer, the anti-corrosion layer, and the wear-resistant layer are fixedly connected to the stainless steel pipe body through the inner high-temperature resistant adhesive layer and the outer high-temperature resistant adhesive layer, so that the stainless steel pipe body has high temperature resistance, corrosion resistance, and wear resistance, thereby avoiding the stainless steel pipe body from being deformed by heat or damaged by wear and corrosion. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a schematic diagram of the structure of the utility model;

[0012] Figure 2 It is a schematic diagram of the cross-sectional structure of the utility model.

[0013] In the figure: 1. Stainless steel pipe body; 2. Inner high temperature resistant adhesive layer; 3. Anti-wear layer; 4. Outer high temperature resistant adhesive layer; 5. High temperature resistant coating layer; 6. Anti-corrosion layer; 7. Wear-resistant layer. DETAILED DESCRIPTION

[0014] See also Figure 1-2 The utility model provides a technical solution: a tensile stainless steel pipe with reduced thermal deformation, comprising a stainless steel pipe body 1, an inner high-temperature resistant adhesive layer 2 is fixedly connected to the inside of the stainless steel pipe body 1, an anti-wear layer 3 is fixedly connected to the inside of the inner high-temperature resistant adhesive layer 2, an outer high-temperature resistant adhesive layer 4 is fixedly connected to the outside of the stainless steel pipe body 1, a high-temperature resistant coating layer 5 is fixedly connected to the outside of the outer high-temperature resistant adhesive layer 4, an anti-corrosion layer 6 is fixedly connected to the outside of the high-temperature resistant coating layer 5, and a wear-resistant layer 7 is fixedly connected to the outside of the anti-corrosion layer 6.

[0015] Furthermore, the high temperature resistant coating layer 5 is a quartz sand layer coated with refractory cement, which improves the high temperature resistance of the stainless steel pipe body 1 and prevents the stainless steel pipe body 1 from being deformed due to heat.

[0016] Furthermore, an inorganic compound layer is provided inside the inner high temperature resistant adhesive layer 2 and the outer high temperature resistant adhesive layer 4 to improve the bonding effect between the inner high temperature resistant adhesive layer 2 and the outer high temperature resistant adhesive layer 4 .

[0017] Furthermore, the surface of the anti-corrosion layer 6 is coated with an acrylic polyurethane topcoat to improve the corrosion resistance of the stainless steel pipe body 1 .

[0018] Furthermore, the anti-wear layer 3 and the wear-resistant layer 7 are both corundum layers, which prevent the inner wall of the stainless steel pipe body 1 from being damaged by friction and improve the wear resistance of the outer wall of the stainless steel pipe body 1 .

[0019] Specifically, when the utility model is used, the anti-wear layer 3 is first bonded to the inner wall of the stainless steel pipe body 1 through the inner high-temperature resistant adhesive layer 2, and then the high-temperature resistant coating layer 5, the anti-corrosion layer 6 and the wear-resistant layer 7 are fixedly connected to the outer wall of the stainless steel pipe body 1 in sequence through the outer high-temperature resistant adhesive layer 4, thereby preventing the inner wall of the stainless steel pipe body 1 from being damaged by friction, and making the outer wall of the stainless steel pipe body 1 have high temperature resistance, corrosion resistance and wear resistance, thereby preventing the stainless steel pipe body 1 from being deformed by heat, avoiding damage due to corrosion or friction, and improving the service life of the stainless steel pipe body 1.

Claims

1. A tensile stainless steel pipe with reduced thermal deformation, comprising a stainless steel pipe body (1), characterized in that: The interior of the stainless steel pipe body (1) is fixedly connected to an inner high-temperature resistant adhesive layer (2), the interior of the inner high-temperature resistant adhesive layer (2) is fixedly connected to an anti-wear layer (3), the exterior of the stainless steel pipe body (1) is fixedly connected to an outer high-temperature resistant adhesive layer (4), the exterior of the outer high-temperature resistant adhesive layer (4) is fixedly connected to a high-temperature resistant coating layer (5), the exterior of the high-temperature resistant coating layer (5) is fixedly connected to an anti-corrosion layer (6), and the exterior of the anti-corrosion layer (6) is fixedly connected to a wear-resistant layer (7).

2. The tensile stainless steel pipe with reduced thermal deformation according to claim 1, characterized in that: The high temperature resistant coating layer (5) is a quartz sand layer coated with refractory cement.

3. The tensile stainless steel pipe with reduced thermal deformation according to claim 1, characterized in that: The inner high temperature resistant adhesive layer (2) and the outer high temperature resistant adhesive layer (4) are both provided with an inorganic compound layer.

4. The tensile stainless steel pipe with reduced thermal deformation according to claim 1, characterized in that: The surface of the anti-corrosion layer (6) is coated with acrylic polyurethane topcoat.

5. The tensile stainless steel tube with reduced thermal deformation according to claim 1, characterized in that: The anti-wear layer (3) and the wear-resistant layer (7) are both corundum layers.